Automatic control method for graded golden finger production and processing
By detecting the conductivity and abnormal difference of the gold finger, and adjusting the preparation parameters in combination with the similar contour mean, the problem that the preparation parameters in the prior art fail to adapt to the detection results is solved, and the preparation efficiency and pass rate of the gold finger are improved.
Patent Information
- Application Number
- CN202510383343.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-03-28
- Publication Date
- 2025-06-20
AI Technical Summary
The prior art does not consider adaptive adjustment of the preparation parameters of the gold finger based on the detection results of the finished gold finger, which affects the preparation efficiency of the gold finger.
By detecting the conductivity and abnormal differences of the gold finger, we determine whether the preparation of the gold finger is qualified, and adjust the preparation parameters based on the similar contour mean, such as nitrogen concentration, the amount of gold plating solution added and the etching time of the microetching solution.
It improves the preparation efficiency of gold fingers and ensures the accuracy and pass rate of the preparation process.
Smart Images

Figure CN120186911A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of hardware circuit manufacturing, and particularly relates to an automatic control method for the production and processing of hierarchical gold fingers. Background Art
[0002] The gold finger connection is a commonly used hardware connection method in the computer hardware industry. For example, memory modules, PC boards, etc. all adopt this method, that is, directly making some pads on the PCB board, and then directly inserting the PCB into the connector. There are spring pieces in the connector that bite the pads to ensure electrical contact. On the pads of the PCB, in order to increase wear resistance and stability, a gold plating process is adopted, so it is called a gold finger.
[0003] In recent years, the application of gold fingers has expanded to non-computer industries such as communication. For example, the AMC standard (Advanced Mezzanine Card) standard, the ATCA standard (Advanced Telecommunications Computing Architecture), and the MicroTCA standard (Micro Telecommunications Computing Architecture) formulated by the PICMG (PCI Industrial Computer Manufacturers Group) organization all stipulate the use of gold fingers as the connection method.
[0004] Chinese Patent Publication No.: CN101521997B discloses a method for processing hierarchical gold fingers, including the production process of gold finger pads and the electroplating process of the gold finger pads. In the production process of the gold finger pads, the copper foil is directly made according to the final required length of the gold finger pads, reducing the shielding and etching processes and lowering the processing difficulty. On this basis, various methods can be used to electroplate the gold finger pads, such as the method of using conductive rubber strips, the method of using thin auxiliary wires, and the method of setting the auxiliary wires on the inner layer of the PCB board. Further, the thin auxiliary wires can be removed by means such as fusing with a large current and drilling. It can be seen that the above technical solutions have the following problems: they do not consider adaptively adjusting the preparation parameters of the gold fingers according to the detection results of the completed gold fingers, which affects the preparation efficiency of the gold fingers. Summary of the Invention
[0005] Therefore, the present invention provides an automatic control method for the production and processing of hierarchical gold fingers to overcome the problem in the prior art that the preparation parameters of the gold fingers are not adaptively adjusted according to the detection results of the completed gold fingers, which affects the preparation efficiency of the gold fingers.
[0006] To achieve the above object, the present invention provides an automatic control method for the production and processing of hierarchical gold fingers, including: S1. After copper plating and cutting the raw material of the single-sided fiberglass board into a working board, drill holes and perform chemical copper deposition on the working board. Then, sequentially cover a dry film and a photomask on the working board, irradiate with ultraviolet light, develop, etch, and clean. Coat with solder resist ink, irradiate with ultraviolet light after covering a photoresist film, then perform solder resist development, slightly etch the working board, treat with an activator, chemically deposit thin gold and electroplate to thicken to obtain a circuit board; S2. Determine the size of the gold fingers; S3. Pre-treat the circuit board. Put the circuit board into a micro-etching solution, and then put the circuit board after micro-etching treatment into a multi-stage water washing tank for cleaning; S4. Make a mask on the surface of the circuit board according to the size of the gold fingers. Put the circuit board with the mask into a nickel plating tank for pre-nickel plating, and then perform water washing after pre-nickel plating; S5. Put the circuit board into an electroplating tank filled with a gold plating solution, introduce nitrogen into the electroplating tank for gold plating. After the gold plating is completed, wash the circuit board, remove the mask on the surface of the circuit board, and clean the circuit board after removing the mask to complete the electroplating of each gold finger on the circuit board; S6. Determine the conduction rate based on whether each detected gold finger is conductive, and determine the abnormal difference amount based on the distance between the gold fingers with abnormal conduction; S7. Determine whether the preparation of the gold fingers is qualified based on the conduction rate and the abnormal difference amount, including: Determine that the preparation of the gold fingers is unqualified. Determine the average contour similarity based on the image information of each gold finger obtained, and adjust the preparation parameters for the gold fingers based on the average contour similarity, including adjusting the nitrogen concentration introduced into the electroplating tank to a corresponding value, adjusting the addition amount of the gold plating solution to a corresponding value, or adjusting the etching duration during the process of putting the circuit board into the micro-etching solution to a corresponding value; Determine that the preparation of the gold fingers is qualified, and continue to use the current preparation parameters to complete the preparation of the gold fingers on each circuit board.
[0007] Further, in the S6, the process of determining the conduction rate based on whether each detected gold finger is conductive includes: Solve the ratio of the number of gold fingers with abnormal conduction to the total number of each gold finger to obtain the conduction rate; In the S7, the process of determining whether the preparation of the gold fingers is qualified based on the conduction rate includes: If the conduction rate is greater than a second preset conduction rate, it is determined that the preparation of the gold fingers is qualified, and continue to use the current preparation parameters to complete the preparation of the gold fingers on each circuit board; If the conduction rate is less than or equal to the second preset conduction rate and greater than the first preset conduction rate, determine whether the preparation of the gold fingers is qualified based on the abnormal difference amount; If the conduction rate is less than or equal to the first preset conduction rate, it is determined that the preparation of the gold fingers is unqualified. The contour similarity mean value is determined based on the obtained image information of each gold finger, and the preparation parameters for the gold fingers are adjusted based on the contour similarity mean value.
[0008] Further, in step S6, the process of determining the abnormal difference amount based on the distances between the gold fingers with abnormal conduction includes: Obtain the distances between the gold fingers with abnormal conduction, solve the variance of each distance, and determine the variance as the abnormal difference amount; In step S7, the process of determining whether the preparation of the gold fingers is qualified based on the abnormal difference amount includes: If the abnormal difference amount is less than or equal to the preset abnormal difference amount, the covering pressure of the photomask during the process of covering the circuit board with the photomask is adjusted to the corresponding value based on the abnormal difference amount; If the abnormal difference amount is greater than the preset abnormal difference amount, it is determined that the preparation of the gold fingers is unqualified. The contour similarity mean value is determined based on the obtained image information of each gold finger, and the preparation parameters for the gold fingers are adjusted based on the contour similarity mean value.
[0009] Further, during the process of covering the circuit board with the photomask based on the abnormal difference amount, the covering pressure of the photomask is adjusted to the corresponding value, where: The determined increase amplitude of the covering pressure of the photomask is inversely proportional to the abnormal difference amount.
[0010] Further, in step S7, the process of determining the contour similarity mean value of each gold finger includes: Obtain the image information of each gold finger. For a single gold finger, the image information of the single gold finger is compared with the corresponding preset gold finger image information for coincidence, and the ratio of the coincidence area to the area of the preset gold finger image information is obtained to get the contour similarity parameter; Solve the average value of the contour similarity parameters of each gold finger to obtain the contour similarity mean value; In step S7, adjusting the preparation parameters for the gold fingers based on the contour similarity mean value includes: If the contour similarity mean value is greater than the second preset similarity mean value, the nitrogen concentration introduced into the electroplating tank is adjusted to the corresponding value based on the total number of gold fingers on the circuit board; If the contour similarity mean value is less than or equal to the second preset similarity mean value and greater than the first preset similarity mean value, the addition amount of the gold plating solution is adjusted to the corresponding value based on the conduction rate; If the contour similarity mean value is less than or equal to the first preset similarity mean value, the etching duration during the process of putting the circuit board into the micro-etching solution is adjusted to the corresponding value based on the contour similarity mean value.
[0011] Further, adjust the nitrogen concentration introduced into the electroplating tank to the corresponding value based on the total number of gold fingers on the circuit board, where: The increase amplitude of the determined nitrogen concentration is proportional to the total number of gold fingers on the circuit board.
[0012] Further, adjust the addition amount of the gold plating solution to the corresponding value based on the conduction rate, where: The increase amplitude of the determined addition amount of the gold plating solution is inversely proportional to the conduction rate.
[0013] Further, after completing the adjustment of the addition amount of the gold plating solution, compare the adjusted addition amount of the gold plating solution with the preset maximum addition amount. If the adjusted addition amount of the gold plating solution is less than or equal to the preset maximum addition amount, use the adjusted addition amount of the gold plating solution as the preparation parameter for the gold fingers; if the adjusted addition amount of the gold plating solution is greater than the preset maximum addition amount, use the adjusted preset maximum addition amount as the preparation parameter for the gold fingers, and use the preset duration adjustment coefficient to adjust the electroplating duration when the circuit board is placed in the electroplating tank to the corresponding value.
[0014] Further, adjust the etching duration when the circuit board is placed in the micro-etching solution to the corresponding value based on the contour similarity mean value, where: The increase amplitude of the determined etching duration is inversely proportional to the contour similarity mean value.
[0015] Compared with the prior art, the beneficial effects of the present invention are as follows: prepare the gold fingers for the circuit board, detect the prepared gold fingers, determine whether the preparation of the gold fingers is qualified according to the detection parameters, and when it is determined that the preparation of the gold fingers is unqualified, adaptively adjust the preparation parameters of the gold fingers, thereby improving the preparation efficiency of the gold fingers.
[0016] Further, when the conduction rate is less than or equal to the second preset conduction rate and greater than the first preset conduction rate, there are some gold fingers with abnormal conduction. At this time, comprehensively determine whether the preparation of the gold fingers is qualified in combination with the abnormal difference amount. The abnormal difference amount characterizes the distribution of the non-conducted gold fingers. When the abnormal difference amount is less than or equal to the preset abnormal difference amount, the distribution of the non-conducted gold fingers is concentrated. In this case, due to problems in the preparation process of the circuit board, the bonding pressure of the photomask is unqualified, resulting in leakage at some positions, so that the circuit preparation in the circuit board is unqualified. This situation is caused by the abnormality of the circuit board, and the preparation of the gold fingers is qualified. Therefore, adjust the covering pressure of the photomask, which improves the accuracy of determining whether the preparation of the gold fingers is qualified and ensures the qualification rate of the circuit board after the preparation of the gold fingers is completed, further improving the preparation efficiency of the gold fingers.
[0017] Further, when it is determined that the preparation of the gold fingers is unqualified, the preparation parameters for the gold fingers are adjusted based on the contour similarity mean of each gold finger. The contour similarity mean of each gold finger characterizes whether the shape of each gold finger meets the preset requirements. When the contour similarity mean is greater than the second preset similarity mean, the shape of the gold finger is compliant at this time. In this case, during the gold plating process, if the nitrogen concentration of the nitrogen gas introduced into the plating solution is too low and the gold plating solution is not sufficiently stirred, it will cause uneven distribution of metal ions, resulting in inconsistent deposition thickness of the gold layer and local thinning and porosity. These defects increase the resistance of the gold fingers and affect the conduction performance. At this time, the nitrogen concentration introduced into the electroplating tank is adjusted; when the contour similarity mean is less than or equal to the second preset similarity mean and greater than the first preset similarity mean, local defects exist in the gold fingers due to insufficient raw material dosage of the gold plating solution. At this time, the addition amount of the gold plating solution is adjusted; when the contour similarity mean is less than or equal to the first preset similarity mean, at this time, due to the too short etching time during the micro-etching process, the etching is incomplete, and excess copper layers remain on the gold fingers, resulting in large-area morphological defects of the gold fingers. The preparation parameters of the gold fingers are adaptively adjusted according to the specific conditions of the gold fingers, improving the preparation efficiency of the gold fingers. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 FIG. is a flowchart of the steps of the automatic control method for grading gold finger production and processing according to an embodiment of the present invention; Figure 2 FIG. is a logical decision diagram for determining whether the preparation of the gold fingers is qualified based on the conduction rate according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE EMBODIMENTS
[0019] In order to make the objectives and advantages of the present invention clearer, the present invention will be further described below in conjunction with embodiments; it should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0020] The preferred embodiments of the present invention will be described below with reference to the accompanying drawings. Those skilled in the art should understand that these embodiments are only used to explain the technical principles of the present invention and do not limit the protection scope of the present invention.
[0021] It should be noted that in the description of the present invention, the terms indicating directions or positional relationships such as "upper", "lower", "left", "right", "inner", "outer", etc. are based on the directions or positional relationships shown in the drawings. This is only for convenience of description and does not indicate or imply that the device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be construed as a limitation of the present invention.
[0022] In addition, it should be noted that in the description of the present invention, unless otherwise clearly specified and defined, the terms "installation", "connection", and "coupling" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, and it can be the communication inside two components. For those skilled in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0023] Please refer to Figure 1 and Figure 2 as shown, which are respectively the step flowchart of the automatic control method for the production and processing of graded gold fingers and the logical decision diagram for determining whether the preparation of gold fingers is qualified in the embodiments of the present invention. An automatic control method for the production and processing of graded gold fingers in an embodiment of the present invention includes: S1. Copper-clad and cut the raw material of the single-sided fiberglass board into a working board, then drill holes and perform electroless copper plating. Sequentially cover a dry film and a photomask on the working board, irradiate with ultraviolet light, develop, etch, and clean. Coat solder mask ink, irradiate with ultraviolet light after covering a photoresist film, then perform solder mask development, slightly etch the working board, treat with an activator, chemically deposit thin gold and electroplate to thicken to obtain a circuit board; S2. Determine the size of the gold fingers; S3. Pretreat the circuit board, put the circuit board into a micro-etching solution, and then put the circuit board after micro-etching treatment into a multi-stage water washing tank for cleaning; S4. Make a mask on the surface of the circuit board according to the size of the gold fingers, put the circuit board with the mask into a nickel plating tank for pre-nickel plating, and then perform water washing after pre-nickel plating; S5. Put the circuit board into an electroplating tank filled with gold plating solution, introduce nitrogen into the electroplating tank for gold plating. After gold plating is completed, wash the circuit board, remove the mask on the surface of the circuit board, and clean the circuit board after removing the mask to complete the electroplating of each gold finger on the circuit board; S6. Determine the conduction rate based on whether each gold finger is conductive detected, and determine the abnormal difference amount based on the distance between each abnormally conductive gold finger; S7. Determine whether the preparation of the gold fingers is qualified based on the conduction rate and the abnormal difference amount, including: Determine that the preparation of the gold fingers is unqualified, determine the contour similarity mean value based on the obtained image information of each gold finger, and adjust the preparation parameters for the gold fingers based on the contour similarity mean value, including adjusting the nitrogen concentration introduced into the electroplating tank to the corresponding value, adjusting the addition amount of the gold plating solution to the corresponding value, or adjusting the etching duration during the process of putting the circuit board into the micro-etching solution to the corresponding value; Determine that the preparation of the gold fingers is qualified, and continuously use the current preparation parameters to complete the preparation of the gold fingers on each circuit board.
[0024] Specifically, in the step S3, the specific composition of the micro-etching solution is not limited. It can be an acidic cupric chloride etching solution. It can be understood that the copper layer on the surface of the circuit board can be removed through a chemical reaction to form a microscopically rough surface, so as to increase the adhesion of subsequent gold deposition. The purpose of putting the circuit board after micro-etching treatment into a multi-stage water washing tank for cleaning is to remove the residual micro-etching solution on the surface. This is prior art and will not be elaborated further.
[0025] Specifically, in the step S4, the specific method of making a mask on the surface of the circuit board is not limited. The mask can be made on the surface of the circuit board by using methods such as photolithography or screen printing according to the size of the gold finger required by the design. The mask material can be photoresist or screen printing ink. It can be understood that it is only necessary to protect the areas on the circuit board that do not need to be gold-plated. This is prior art and will not be elaborated further.
[0026] Specifically, in the step S4, the circuit board with a mask is put into a nickel plating tank for pre-nickel plating to provide a bottom layer for gold deposition, so as to improve the bonding force between the gold and the circuit board and prevent the diffusion between the gold and the copper. After pre-nickel plating, water washing is carried out to remove the residual nickel plating solution on the surface.
[0027] Specifically, in the step S1, the process of obtaining the circuit board includes: S11, copper-cladding the raw material of the single-sided glass fiber board and cutting it into several working boards, and then drilling and electroless copper plating on the working boards; S12, sequentially covering a dry film and a photo mask with a circuit on the working board, irradiating with ultraviolet light to cure the dry film in the circuit area, using a developer to remove the dry film in the unexposed part to expose the copper layer to be etched, using an etching solution to etch the exposed copper layer, and cleaning the dry film in the circuit area, and obtaining the image information of the working board through a vision detector; S13, coating a solder resist ink, covering a photoresist film with a circuit on the working board, irradiating with ultraviolet light to cure the area outside the drilled holes, and removing the uncured solder resist ink through solder resist development; S14, immersion gold, mildly etching the working board to remove the oxide layer and contaminants, treating the working board with an activator, chemically depositing a thin layer of gold on the activated working board to obtain an immersion gold layer, and electroplating and thickening the immersion gold layer to obtain the circuit board. This will not be elaborated further.
[0028] Specifically, in the step S2, the specific method for determining the size of the gold finger is not limited. The size of the gold finger can be determined according to the usage requirements and design specifications of the product. The length range of the gold finger can be 5 - 50 mm, the width range can be 0.5 - 5 mm, and the thickness range can be 0.1 - 0.5 mm. It can be understood that the specific size needs to be designed and determined according to the interface type, the number of pluggings and unpluggings, and the current-carrying capacity of the electronic product. The design graphics of the gold finger can be drawn into the design file of the circuit board using circuit board design software such as Altium Designer, and the positions and size information of each gold finger are marked. This is the prior art and will not be elaborated here.
[0029] Specifically, the gold fingers of the circuit board are prepared, and the prepared gold fingers are detected. Whether the preparation of the gold fingers is qualified is determined based on the detection parameters. When it is determined that the preparation of the gold fingers is unqualified, the preparation parameters of the gold fingers are adaptively adjusted, which improves the preparation efficiency of the gold fingers.
[0030] Specifically, in the step S6, the process of determining the conduction rate based on whether each detected gold finger is conductive includes: Calculating the ratio of the number of gold fingers with abnormal conduction to the total number of all gold fingers to obtain the conduction rate; In the step S7, the process of determining whether the preparation of the gold fingers is qualified based on the conduction rate includes: If the conduction rate is greater than the second preset conduction rate, it is determined that the preparation of the gold fingers is qualified, and the current preparation parameters are continuously used to complete the preparation of the gold fingers of each circuit board; If the conduction rate is less than or equal to the second preset conduction rate and greater than the first preset conduction rate, it is determined whether the preparation of the gold fingers is qualified based on the abnormal difference amount; If the conduction rate is less than or equal to the first preset conduction rate, it is determined that the preparation of the gold fingers is unqualified. The contour similarity mean value is determined based on the obtained image information of each gold finger, and the preparation parameters for the gold fingers are adjusted based on the contour similarity mean value.
[0031] Specifically, the first preset conduction rate D1 is selected within the range of [0.7, 0.8], and the second preset conduction rate D2 is taken as 1.
[0032] Specifically, in the step S6, the method for detecting whether each gold finger is conducting can be to adjust the range of the multimeter to the ohm range (Ω range), and then touch the two test leads of the multimeter to the two ends of the gold finger whose conductivity needs to be detected. The gold finger that shows "OL" (overrange, i.e., open circuit) is determined as the gold finger with abnormal conductivity. Or use an automated detection device, a flying probe tester. Place the circuit board with gold fingers on the workbench of the flying probe tester. The flying probe tester will automatically touch the two ends of the gold finger through the rapidly moving probes for electrical connection detection. The tester will quickly determine whether each gold finger is conducting according to the preset determination criteria (preset qualified range of conduction resistance), and display the detection result on the device screen. Green indicates conduction, and red indicates non-conduction.
[0033] Specifically, in the step S6, the process of determining the abnormal difference amount based on the distances between the abnormally conducting gold fingers includes: Obtain the distances between the abnormally conducting gold fingers, solve the variance of each distance, and determine this variance as the abnormal difference amount; In the step S7, the process of determining whether the preparation of the gold fingers is qualified based on the abnormal difference amount includes: If the abnormal difference amount is less than or equal to the preset abnormal difference amount, then during the process of covering the circuit board with the photomask, adjust the covering pressure of the photomask to the corresponding value based on the abnormal difference amount; If the abnormal difference amount is greater than the preset abnormal difference amount, then determine that the preparation of the gold fingers is unqualified. Determine the contour similarity average value based on the obtained image information of each gold finger, and adjust the preparation parameters for the gold fingers based on the contour similarity average value.
[0034] Specifically, the preset abnormal difference amount Y0 is selected within the range [0.04L02, 0.1L02], where L0 is the average value of the distances between the gold fingers.
[0035] Specifically, when the conduction rate is less than or equal to the second preset conduction rate and greater than the first preset conduction rate, there are some abnormally conducting gold fingers. At this time, comprehensively determine whether the preparation of the gold fingers is qualified in combination with the abnormal difference amount. The abnormal difference amount characterizes the distribution of the non-conducting gold fingers. When the abnormal difference amount is less than or equal to the preset abnormal difference amount, the distribution of the non-conducting gold fingers is concentrated. In this case, due to problems in the preparation process of the circuit board, the bonding pressure of the photomask is unqualified, resulting in leakage at some positions, thus making the preparation of the circuit in the circuit board unqualified. This situation is caused by the abnormality of the circuit board, and the preparation of the gold fingers is qualified. Therefore, adjusting the covering pressure of the photomask improves the accuracy of determining whether the preparation of the gold fingers is qualified, while ensuring the qualification rate of the circuit board with the gold fingers prepared, and further improving the preparation efficiency of the gold fingers.
[0036] Specifically, during the process of covering the circuit board with a photomask, the covering pressure of the photomask is adjusted to a corresponding value based on the abnormal difference amount, where: The determined increase amplitude of the covering pressure of the photomask is inversely proportional to the abnormal difference amount.
[0037] In this embodiment, optionally, The abnormal difference amount is compared with a first preset difference comparison threshold and a second preset difference comparison threshold; If the abnormal difference amount is less than or equal to the first preset difference comparison threshold, the covering pressure of the photomask is adjusted to 1.29 times the initial covering pressure; If the abnormal difference amount is less than or equal to the second preset difference comparison threshold and greater than the first preset difference comparison threshold, the covering pressure of the photomask is adjusted to 1.21 times the initial covering pressure; If the abnormal difference amount is greater than the second preset difference comparison threshold, the covering pressure of the photomask is adjusted to 1.12 times the initial covering pressure; The first preset difference comparison threshold is taken as 0.4Y0, and the second preset difference comparison threshold is taken as 0.65Y0.
[0038] Specifically, in step S7, the process of determining the contour similarity mean value of each gold finger includes: Obtain the image information of each gold finger. For a single gold finger, the image information of the single gold finger is compared with the corresponding preset gold finger image information for coincidence, and the ratio of the coincidence area to the area of the preset gold finger image information is obtained to get the contour similarity parameter; Solve the average value of the contour similarity parameters of each gold finger to obtain the contour similarity mean value; In step S7, based on the contour similarity mean value, adjusting the preparation parameters for the gold finger includes: If the contour similarity mean value is greater than the second preset similarity mean value, the nitrogen concentration introduced into the electroplating tank is adjusted to a corresponding value based on the total number of gold fingers on the circuit board; If the contour similarity mean value is less than or equal to the second preset similarity mean value and greater than the first preset similarity mean value, the addition amount of the gold plating solution is adjusted to a corresponding value based on the conduction rate; If the contour similarity mean value is less than or equal to the first preset similarity mean value, the etching duration during the process of putting the circuit board into the micro-etching solution is adjusted to a corresponding value based on the contour similarity mean value.
[0039] Specifically, the first preset similarity mean value S1 is selected within the range of [0.89, 0.94], and the second preset similarity mean value S2 is selected within the range of [0.96, 1].
[0040] Specifically, when it is determined that the preparation of the gold fingers is unqualified, the preparation parameters for the gold fingers are adjusted based on the contour similarity mean value of each gold finger. The contour similarity mean value of each gold finger characterizes whether the shape of each gold finger meets the preset requirements. When the contour similarity mean value is greater than the second preset similarity mean value, the shape of the gold finger is compliant at this time. In this case, during the gold plating process, if the nitrogen concentration introduced into the plating solution is too low and the gold plating solution is not stirred sufficiently, it will cause uneven distribution of metal ions, resulting in inconsistent deposition thickness of the gold layer and local thinning and porosity. These defects increase the resistance of the gold fingers and affect the conduction performance. At this time, the nitrogen concentration introduced into the electroplating tank is adjusted; when the contour similarity mean value is less than or equal to the second preset similarity mean value and greater than the first preset similarity mean value, local defects exist in the gold fingers due to insufficient raw material dosage of the gold plating solution. At this time, the addition amount of the gold plating solution is adjusted; when the contour similarity mean value is less than or equal to the first preset similarity mean value, at this time, due to the too short etching duration during the micro-etching process, the etching is incomplete, and excess copper layer remains on the gold fingers, resulting in large-area morphological defects of the gold fingers. The preparation parameters of the gold fingers are adaptively adjusted according to the specific situation of the gold fingers, improving the preparation efficiency of the gold fingers.
[0041] Specifically, based on the total number of gold fingers in the circuit board, the nitrogen concentration introduced into the electroplating tank is adjusted to the corresponding value, where: The increase amplitude of the determined nitrogen concentration is proportional to the total number of gold fingers in the circuit board.
[0042] In this embodiment, optionally, The total number of gold fingers in the circuit board is compared with the first preset number and the second preset number; If the total number of gold fingers is less than or equal to the first preset number, the nitrogen concentration is adjusted to 1.11 times the initial nitrogen concentration; If the total number of gold fingers is less than or equal to the second preset number and greater than the first preset number, the nitrogen concentration is adjusted to 1.18 times the initial nitrogen concentration; If the total number of gold fingers is greater than the second preset number, the nitrogen concentration is adjusted to 1.27 times the initial nitrogen concentration; The first preset number is taken as 1.2M0, and the second preset number is taken as 3.8M0, where M0 is the average value of the total number of gold fingers of each circuit board in history.
[0043] Specifically, based on the conduction rate, the addition amount of the gold plating solution is adjusted to the corresponding value, where: The increase amplitude of the determined addition amount of the gold plating solution is inversely proportional to the conduction rate.
[0044] In this embodiment, optionally, The conduction rate is compared with the first preset conduction comparison threshold and the second preset conduction comparison threshold; If the conduction rate is less than or equal to the first preset conduction ratio threshold, adjust the addition amount of the gold plating solution to 1.29 times the initial addition amount; If the conduction rate is less than or equal to the second preset conduction ratio threshold and greater than the first preset conduction ratio threshold, adjust the addition amount of the gold plating solution to 1.22 times the initial addition amount; If the conduction rate is greater than the second preset conduction ratio threshold, adjust the addition amount of the gold plating solution to 1.13 times the initial addition amount; The first preset conduction ratio threshold is taken as 0.66D1, and the second preset conduction ratio threshold is taken as 0.82D1.
[0045] Specifically, after completing the adjustment of the addition amount of the gold plating solution, compare the adjusted addition amount of the gold plating solution with the preset maximum addition amount. If the adjusted addition amount of the gold plating solution is less than or equal to the preset maximum addition amount, use the adjusted addition amount of the gold plating solution as the preparation parameter for the gold finger; if the adjusted addition amount of the gold plating solution is greater than the preset maximum addition amount, use the adjusted preset maximum addition amount as the preparation parameter for the gold finger, and use the preset duration adjustment coefficient to adjust the electroplating duration of the circuit board in the electroplating tank to the corresponding value.
[0046] Specifically, the preset maximum addition amount is taken as 1.64T0, T0 is the average value of the addition amounts of the historical gold plating solutions, and the preset duration adjustment coefficient is taken as 1.1.
[0047] Specifically, based on the contour similarity mean value, adjust the etching duration of the circuit board in the micro-etching solution to the corresponding value, where: The determined increase amplitude of the etching duration is inversely proportional to the contour similarity mean value.
[0048] In this embodiment, optionally, Compare the contour similarity mean value with the first preset mean value comparison threshold and the second preset mean value comparison threshold; If the contour similarity mean value is less than or equal to the first preset mean value comparison threshold, adjust the etching duration to 1.26 times the initial etching duration; If the contour similarity mean value is less than or equal to the second preset mean value comparison threshold and greater than the first preset mean value comparison threshold, adjust the etching duration to 1.19 times the initial etching duration; If the contour similarity mean value is greater than the second preset mean value comparison threshold, adjust the etching duration to 1.11 times the initial etching duration; The first preset mean value comparison threshold is taken as 0.8S1, and the second preset mean value comparison threshold is taken as 0.92S1.
[0049] So far, the technical solution of the present invention has been described in conjunction with the preferred embodiments shown in the accompanying drawings. However, those skilled in the art can easily understand that the protection scope of the present invention is obviously not limited to these specific embodiments. Without departing from the principle of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will fall within the protection scope of the present invention.
[0050] The above are only the preferred embodiments of the present invention and are not intended to limit the present invention. For those skilled in the art, the present invention can have various changes and modifications. Any modification, equivalent substitution, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. An automatic control method for the production and processing of graded gold fingers, characterized in that: include: S1, copper-coating the raw material of the single-sided fiberglass board, cutting it into a working board, drilling it, chemically depositing copper, sequentially covering the working board with a dry film and a photomask, irradiating it with ultraviolet light, developing it, etching it, cleaning it, coating it with solder resist ink, irradiating it with ultraviolet light after covering it with a photoresist film, and then developing the solder resist, lightly etching the working board, treating it with an activator, chemically depositing a thin gold film, and electroplating it to obtain a circuit board; S2, determine the size of the gold finger; S3, pre-treatment of the circuit board, placing the circuit board in a micro-etching solution, and placing the micro-etched circuit board in a multi-stage water washing tank for cleaning; S4, making a mask on the surface of the circuit board according to the size of the gold finger, placing the circuit board with the mask into a nickel plating tank for pre-nickel plating, and washing after the pre-nickel plating; S5, placing the circuit board in an electroplating tank filled with gold plating solution, introducing nitrogen into the electroplating tank to perform gold plating, and after the gold plating is completed, washing the circuit board with water, removing the mask on the surface of the circuit board, and cleaning the circuit board after the mask is removed to complete the electroplating of each gold finger on the circuit board; S6, determining the conduction rate based on whether each detected golden finger is conductive, and determining the abnormal difference amount based on the distance between each abnormal conductive golden finger; S7, determining whether the preparation of the gold finger is qualified based on the conductivity and the abnormal difference, including: Determine that the preparation of the gold finger is unqualified, determine the contour similarity mean based on the image information of each gold finger obtained, and adjust the preparation parameters for the gold finger based on the contour similarity mean, including adjusting the concentration of nitrogen introduced into the electroplating tank to a corresponding value, adjusting the amount of gold plating solution added to a corresponding value, or adjusting the etching time of the circuit board in the micro-etching solution to a corresponding value; Determine that the preparation of the gold fingers is qualified, and continue to use the current preparation parameters to complete the preparation of the gold fingers of each circuit board.
2. The automatic control method for producing and processing graded gold fingers according to claim 1 is characterized in that: In S6, the process of determining the conduction rate based on whether each gold finger is turned on or not includes: The ratio of the number of abnormally conductive golden fingers to the total number of golden fingers is solved to obtain the conductivity rate; In S7, the process of determining whether the preparation of the gold finger is qualified based on the conductivity includes: If the conductivity is greater than the second preset conductivity, it is determined that the preparation of the gold finger is qualified, and the current preparation parameters are continuously used to complete the preparation of the gold fingers of each circuit board; If the conductivity is less than or equal to the second preset conductivity and greater than the first preset conductivity, determining whether the preparation of the gold finger is qualified based on the abnormal difference amount; If the conductivity is less than or equal to the first preset conductivity, the preparation of the gold finger is determined to be unqualified, a contour similarity mean is determined based on the acquired image information of each gold finger, and preparation parameters for the gold finger are adjusted based on the contour similarity mean.
3. The automatic control method for producing and processing graded gold fingers according to claim 2 is characterized in that: In S6, the process of determining the abnormal difference amount based on the distance between the gold fingers with abnormal conduction includes: Obtain the distance between each gold finger with abnormal conduction, solve the variance of each distance, and determine the variance as the abnormal difference amount; In S7, the process of determining whether the preparation of the gold finger is qualified based on the abnormal difference amount includes: If the abnormal difference amount is less than or equal to the preset abnormal difference amount, adjusting the covering pressure of the photomask in the process of covering the circuit board with the photomask to a corresponding value based on the abnormal difference amount; If the abnormal difference is greater than the preset abnormal difference, the preparation of the gold finger is determined to be unqualified, and the contour similarity mean is determined based on the acquired image information of each gold finger, and the preparation parameters for the gold finger are adjusted based on the contour similarity mean.
4. The automatic control method for producing and processing graded gold fingers according to claim 3 is characterized in that: Based on the abnormal difference, the covering pressure of the photomask during the process of covering the circuit board with the photomask is adjusted to a corresponding value, wherein: The magnitude of the increase in cover pressure on the photomask is determined to be inversely proportional to the amount of the anomaly difference.
5. The automatic control method for producing and processing graded gold fingers according to claim 4 is characterized in that: In S7, the process of determining the mean value of the profile similarity of each golden finger includes: Obtain image information of each golden finger, and for a single golden finger, overlap and compare the image information of the single golden finger with the corresponding preset golden finger image information, obtain the ratio of the overlap area to the area of the preset golden finger image information, and obtain the contour similarity parameter; Solve the average value of the contour similarity parameters of each golden finger to obtain the contour similarity mean; In S7, adjusting the preparation parameters for the gold finger based on the profile similarity mean value includes: If the profile similarity mean is greater than the second preset similarity mean, the concentration of nitrogen introduced into the electroplating tank is adjusted to a corresponding value based on the total number of gold fingers in the circuit board; If the profile similarity mean is less than or equal to the second preset similarity mean and greater than the first preset similarity mean, adjusting the amount of gold plating solution added to a corresponding value based on the conductivity; If the profile similarity mean is less than or equal to the first preset similarity mean, the etching time of the circuit board in the process of being placed in the micro-etching solution is adjusted to a corresponding value based on the profile similarity mean.
6. The automatic control method for producing and processing graded gold fingers according to claim 5, characterized in that: The nitrogen concentration introduced into the electroplating tank is adjusted to the corresponding value based on the total number of gold fingers in the circuit board, where: The increase in nitrogen concentration was determined to be proportional to the total number of gold fingers in the circuit board.
7. The automatic control method for producing and processing graded gold fingers according to claim 6 is characterized in that: Adjust the amount of gold plating solution to the corresponding value based on the conductivity, where: The increase in the amount of gold plating solution added is inversely proportional to the conductivity.
8. The automatic control method for producing and processing graded gold fingers according to claim 7, characterized in that: After completing the adjustment of the addition amount of the gold-plating solution, compare the adjusted addition amount of the gold-plating solution with the preset maximum addition amount. If the adjusted addition amount of the gold-plating solution is less than or equal to the preset maximum addition amount, use the adjusted addition amount of the gold-plating solution as the preparation parameter of the gold finger; if the adjusted addition amount of the gold-plating solution is greater than the preset maximum addition amount, use the adjusted preset maximum addition amount as the preparation parameter of the gold finger, and use the preset time adjustment coefficient to adjust the electroplating time of the circuit board in the electroplating tank to the corresponding value.
9. The automatic control method for producing and processing graded gold fingers according to claim 8, characterized in that: Based on the mean value of profile similarity, the etching time of the circuit board in the micro-etching solution is adjusted to the corresponding value, where: The increase in the determined etching time is inversely proportional to the mean profile similarity.