Trench-IGBT device transition region structure and method of manufacturing the same
By designing staggered gate bus and trench structures in Trench-IGBT devices and connecting the emitter metal through oxide layer openings, the problems of transition region line integrity and uneven electric field distribution are solved, achieving a low-loss and high-reliability transition region structure.
Patent Information
- Application Number
- CN202510325225.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2025-03-19
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2045-03-19
AI Technical Summary
The lack of trench line integrity in the existing technology to improve the transition region of Trench-IGBT devices leads to high turn-off losses and excessive electric field in the transition region, which can easily cause local failures.
A transition region structure for a Trench-IGBT device is designed, comprising an interleaved gate bus structure, a transition polysilicon layer, and a trench structure. The oxide layer is connected to the emitter metal via an opening to achieve short-circuiting and uniform electric field distribution, thereby reducing turn-off losses.
It improves the integrity of the trench structure, reduces turn-off losses, avoids failure caused by excessive electric field in the transition region, and ensures uniform electric field distribution.
Smart Images

Figure CN120417410B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor technology, specifically to the structure of the transition region between the active region and the terminal and its fabrication method. Background Technology
[0002] Trench-type insulated-gate bipolar transistors (IGBTs) are a common type of power device. Current technologies focus primarily on improvements to the IGBT termination and active region, with less attention paid to the transition region between them. However, the transition region is a crucial aspect of IGBT design, affecting the gate-emitter connection, the integrity of the trench lines, and directly influencing IGBT performance.
[0003] Currently, there is a lack of transition zone structures that can improve the integrity of the groove lines in the transition zone, reduce IGBT product turn-off losses, and avoid local failures caused by excessive electric field in the transition zone. Summary of the Invention
[0004] To address the problems existing in the prior art, this invention provides a Trench-IGBT device transition region structure and its fabrication method to solve at least one of the above-mentioned technical problems.
[0005] To achieve the above objectives, the present invention provides a transition region structure for a Trench-IGBT device, characterized in that it includes a silicon wafer base layer, on which a gate BUS structure, a transition polysilicon layer, a terminal structure, and a trench structure are disposed, wherein the trench structure includes long trenches and short trenches arranged alternately.
[0006] The gate BUS structure is located between the terminal structure and the trench structure;
[0007] The gate BUS structure includes an alternating first-directional polysilicon layer and a second-directional polysilicon layer. The second-directional polysilicon layer is connected to the long trench and extends into the long trench. The region of the second-directional polysilicon layer in the long trench and its adjacent silicon substrate region are arsenic ion implantation regions.
[0008] The transition polysilicon layer is connected to the short trench and extends into the short trench, and the transition polysilicon layer is located between adjacent long trenches and adjacent second polysilicon layers.
[0009] The gate BUS structure, the transition polysilicon layer, and the trench structure are isolated from the emitter metal by an oxide layer. The oxide layer has a first opening in the region facing the transition polysilicon layer, and the emitter metal is short-circuited to the transition polysilicon layer through the first opening.
[0010] A second opening is formed on the oxide layer in the region between adjacent second-axis polycrystalline silicon layers, and the emitter metal is connected to the silicon wafer substrate through the second opening;
[0011] The oxide layer is also provided with an opening group adjacent to the trench structure. The emitter metal is connected to the silicon wafer substrate through the opening group and to the arsenic ion implantation region through the opening group.
[0012] More preferably, the terminal structure is isolated from the metal layer by the oxide layer.
[0013] There is an exposed oxide layer area between the metal layer and the emitter metal, and the exposed oxide layer area is directly opposite the oxide layer located between the terminal structure and the second opening.
[0014] More preferably, the opening group includes a third opening, a fourth opening, and a fifth opening;
[0015] The third and fourth openings are located on the right side of the long groove, and the fifth opening is located on the right side of the short groove, and the fifth opening is located adjacent to the gap between the third and fourth openings.
[0016] More preferably, the length of the fifth opening is greater than the length of the gap between the third opening and the fourth opening.
[0017] More preferably, the area of the first opening is 1-2 μm. 2 ;
[0018] The area of the second opening is 2-4 μm. 2 ;
[0019] The width of each opening group is 1.5μm-2.2μm, the length of the third and fifth openings is 10μm-30μm, and the end of the fourth opening away from the gate BUS structure is flush with the end of the long trench away from the gate BUS structure.
[0020] A method for fabricating a transition region structure of a Trench-IGBT device, characterized by comprising the following steps:
[0021] Step 1: A terminal oxide layer is grown on the silicon wafer substrate, and then etched to form a terminal structure;
[0022] Step 2: Etch long trenches and short trenches of alternating lengths on the silicon wafer substrate, wherein the distance between the long trenches and the terminal structure is 35-60 μm;
[0023] Step 3: A polysilicon layer is deposited and grown using in-situ doping in a furnace tube. The polysilicon layer fills the long trench and the short trench. Photoresist is coated on the polysilicon layer, and the gate BUS structure and the transition polysilicon layer located at the connection between the emitter metal and the short trench are etched out. The polysilicon in the silicon plane is etched clean.
[0024] There is a gap between the gate BUS structure and the terminal structure;
[0025] Step 4: After step 3, the upper surface, except for the ion implantation area, is coated with photoresist for arsenic ion implantation. The implantation dose is between 1E15 and 1E16. The arsenic ion implantation area is located in the long trench and partially covers the long trench.
[0026] Step 5: Deposit an oxide layer formed by borosilicate glass using chemical vapor deposition, and then use a photoresist mask to etch out the first opening in the transition polysilicon layer, the second opening in the region between adjacent second polysilicon layers, and the opening group adjacent to the trench structure.
[0027] Step 6: Deposit a metal layer with a thickness of 3-6 μm by sputtering, and then use photoresist to etch and form a metal emitter.
[0028] More preferably, the thickness of the terminal oxide layer is 1.5μm-2μm.
[0029] More preferably, the width of the long trench and the short trench is 0.6μm-1.0μm, and the depth of the long trench and the short trench is 5.0μm-6μm.
[0030] More preferably, the long trench is 35-60 μm away from the terminal structure.
[0031] More preferably, the thickness of the polycrystalline silicon layer is 1.0 μm-1.3 μm.
[0032] More preferably, in step five, the thickness of the oxide layer is 0.5 μm-1.0 μm.
[0033] A method for fabricating a transition region structure of a Trench-IGBT device, characterized by comprising the following steps:
[0034] Step 1: A terminal oxide layer is grown on the silicon wafer substrate, and then etched to form a terminal structure;
[0035] Step 2: Etch long trenches and short trenches of alternating lengths on the silicon wafer substrate, wherein the distance between the long trenches and the terminal structure is 35-60 μm;
[0036] Step 3: A polysilicon layer is deposited and grown using in-situ doping in a furnace tube. The polysilicon layer fills the long trench and the short trench. Photoresist is coated on the polysilicon layer, and the gate BUS structure and the transition polysilicon layer located at the connection between the emitter metal and the short trench are etched out. The polysilicon in the silicon plane is etched clean.
[0037] There is a gap between the gate BUS structure and the terminal structure;
[0038] Step four: After step three, the upper surface, except for the ion implantation area, is coated with photoresist for arsenic ion implantation. The implantation dose is between 1E15 and 1E16, and the implantation width is between 0.8 μm and 1.8 μm. The arsenic ion implantation area is located in the long trench and partially covers the long trench.
[0039] Step 5: Deposit an oxide layer formed by borosilicate glass using chemical vapor deposition. Then, use a photoresist mask to etch the first opening in the oxide layer that is directly opposite the transition polysilicon layer, the second opening located in the region between adjacent second polysilicon layers, and the group of openings adjacent to the trench structure.
[0040] Step 6: Deposit a metal layer with a thickness of 3-6 μm by sputtering, and form a metal emitter by photoresist etching. The metal emitter is connected to the transition polysilicon layer through the first opening, and the metal emitter is connected to the silicon wafer substrate through the second opening and the opening group.
[0041] Compared with the prior art, the beneficial effects of the present invention are:
[0042] 1) There is a certain distance between the trench structure and the terminal structure to avoid the problem that the lines of the trench structure cannot be etched after photolithography due to the excessive step of the terminal structure.
[0043] 2) The polycrystalline silicon layer in the short trench is short-circuited with the emitter metal, which accelerates the ion extraction rate and reduces turn-off loss during the turn-off process.
[0044] 3) The setting of the first opening, the second opening, and the opening group ensures a uniform electric field distribution and avoids failure caused by excessive local electric field in the transition zone. Attached Figure Description
[0045] Figure 1 This is a schematic diagram showing the process after step six in a specific embodiment of the present invention;
[0046] Figure 2 This is a schematic diagram showing the process after step two in a specific embodiment of the present invention;
[0047] Figure 3 This is a schematic diagram showing the process after step three in a specific embodiment of the present invention;
[0048] Figure 4 This is a schematic diagram showing the process after step four in a specific embodiment of the present invention;
[0049] Figure 5 This is a schematic diagram showing the process after step five in a specific embodiment of the present invention.
[0050] In the figure, 1 is the terminal structure, 2 is the exposed oxide layer area, 3 is the first opening, 4 is the second opening, 5 is the transition polysilicon layer, 6 is the oxide layer, 7 is the first-axis polysilicon layer, 8 is the second-axis polysilicon layer, 9 is the long trench, 10 is the short trench, 11 is the third opening, 12 is the fifth opening, 13 is the fourth opening, and 15 is the arsenic ion implantation region. Detailed Implementation
[0051] The present invention will now be further described with reference to the accompanying drawings.
[0052] See Figures 1 to 5 Specific Embodiment 1: A transition region structure for a Trench-IGBT device includes a silicon wafer substrate. A gate BUS structure, a transition polysilicon layer 5, a termination structure 1, and a trench structure are disposed on the silicon wafer substrate. The trench structure includes alternating long trenches 9 and short trenches 10. The gate BUS structure is located between the termination structure 1 and the trench structure. The gate BUS structure includes alternating first-directional polysilicon layers 7 and second-directional polysilicon layers 8. The second-directional polysilicon layer 8 is connected to and extends into the long trenches 9. A portion of the second-directional polysilicon layer 8 located in the long trenches 9 and its adjacent silicon wafer substrate region constitutes an arsenic ion implantation region 15. The transition polysilicon layer 5 is connected to and extends into the short trenches 10, and the transition polysilicon layer 5 is located in adjacent... The long trench 9 is adjacent to the second-axis polysilicon layer 8; a first opening 3 is formed in the transition polysilicon layer 5, and the polysilicon layer in the short trench 10 is short-circuited to the emitter metal; the gate BUS structure, the transition polysilicon layer 5, the terminal structure 1, and the trench structure are isolated from the emitter metal by an oxide layer. The oxide layer has a first opening 3 in the area facing the transition polysilicon layer 5, and the emitter metal is short-circuited to the transition polysilicon layer 5 through the first opening 3; a second opening 4 is formed on the oxide layer in the area between adjacent second-axis polysilicon layers 8, and the emitter metal is connected to the silicon substrate through the second opening 4; a group of openings adjacent to the trench structure is also formed on the oxide layer, and the emitter metal is connected to the silicon substrate through the group of openings, and the emitter metal is connected to the arsenic ion implantation region through the group of openings. The emitter metal is also the active region metal.
[0053] The silicon wafer substrate includes the first type of conductivity. <100> A substrate with a crystal orientation, having on the front side of a substrate of the first conductivity type. <100> The epitaxial layer is oriented in the crystal direction and is of the first conductivity type.
[0054] The terminal structure 1 is isolated from the metal layer by an oxide layer. There is an exposed oxide layer area 2 between the metal layer and the emitter metal. The exposed oxide layer area 2 is directly opposite the oxide layer located between the terminal structure 1 and the second opening 4.
[0055] The opening group includes a third opening 11, a fourth opening 13, and a fifth opening 12; the third opening 11 and the fourth opening 13 are located on the right side of the long groove 9, the fifth opening 12 is located on the right side of the short groove 10, and the fifth opening 12 is located adjacent to the gap between the third opening 11 and the fourth opening 13.
[0056] The length of the fifth opening 12 is greater than the length of the gap between the third opening 11 and the fourth opening 13.
[0057] The area of the first opening 3 is 1-2 μm. 2 The area of the second opening 4 is 2-4 μm. 2 The width of each aperture group is 1.5μm-2.2μm, the length of the third aperture 11 and the fifth aperture 12 is 10μm-30μm, and the end of the fourth aperture 13 away from the gate BUS structure is flush with the end of the long groove 9 away from the gate BUS structure.
[0058] The width of the long trench 9 and the short trench 10 is 0.6μm-1.0μm, and the depth of the long trench 9 and the short trench 10 is 5.0μm-6μm.
[0059] The long trench 9 is 35-60μm away from the terminal structure.
[0060] A method for fabricating a transition region structure for a Trench-IGBT device includes the following steps:
[0061] Step 1: A terminal oxide layer with a thickness of 1.5μm-2μm is grown on the silicon wafer substrate, and after etching, a terminal structure 1 is formed;
[0062] Step two: Etching alternating long trenches 9 and short trenches 10 on the silicon wafer substrate, with the distance between the long trenches 9 and the terminal structure 1 being 35-60 μm; see [link to relevant documentation]. Figure 2 .
[0063] Step 3: A polysilicon layer with a thickness of 1.0μm-1.3μm is deposited and grown using the in-situ doping method of furnace tube. The polysilicon layer fills the long trench 9 and the short trench 10. Photoresist is coated on the polysilicon layer, and the gate BUS structure and the transition polysilicon layer 5 located at the connection position between the emitter metal and the short trench 10 are etched out. The polysilicon in the silicon plane is etched clean.
[0064] There is a gap between the gate BUS structure and terminal structure 1;
[0065] See Figure 3 .
[0066] Step four: The upper surface following step three, except for the ion implantation area, is coated with photoresist for arsenic ion implantation. The implantation dose is between 1E15 and 1E16, and the implantation width is between 0.8 μm and 1.8 μm. The arsenic ion implantation area 15 is located at the long trench 9 and partially covers the long trench 9. See [link / reference] Figure 4 .
[0067] Step 5: A layer of borosilicate glass with a thickness of 0.5 μm-1.0 μm is deposited using chemical vapor deposition. Then, a photoresist mask is used to etch the first opening 3 on the oxide layer, directly opposite the transition polysilicon layer 5; the second opening 4 located between adjacent second-direction polysilicon layers 8; and the group of openings adjacent to the trench structure. See [link to relevant documentation]. Figure 5 .
[0068] Step six: Deposit a 3-6 μm thick metal layer by sputtering, and then etch a metal emitter using photoresist. The metal emitter is connected to the transition polysilicon layer through the first opening 3. The metal emitter is connected to the silicon substrate through the second opening 4 and the opening group. See also... Figure 1 The metal layer has an exposed oxide layer area 2, which is directly opposite the oxide layer located between the terminal structure 1 and the second opening 4.
[0069] The above are merely preferred embodiments of the present invention. It should be noted that those skilled in the art can make various improvements and modifications without departing from the principle of the present invention, and these improvements and modifications should also be considered within the scope of protection of the present invention.
Claims
1. A transition region structure for a Trench-IGBT device, characterized in that, It includes a silicon wafer substrate, on which a gate BUS structure, a transition polysilicon layer, a terminal structure and a trench structure are disposed, and the trench structure includes long trenches and short trenches arranged alternately. The gate BUS structure is located between the terminal structure and the trench structure; The gate BUS structure includes an alternating first-directional polysilicon layer and a second-directional polysilicon layer. The second-directional polysilicon layer is connected to the long trench and extends into the long trench. The region of the second-directional polysilicon layer in the long trench and its adjacent silicon substrate region are arsenic ion implantation regions. The transition polysilicon layer is connected to the short trench and extends into the short trench, and the transition polysilicon layer is located between adjacent long trenches and adjacent second polysilicon layers. The gate BUS structure, the transition polysilicon layer, and the trench structure are isolated from the emitter metal by an oxide layer. The oxide layer has a first opening in the region facing the transition polysilicon layer, and the emitter metal is short-circuited to the transition polysilicon layer through the first opening. A second opening is formed on the oxide layer in the region between adjacent second-axis polycrystalline silicon layers, and the emitter metal is connected to the silicon wafer substrate through the second opening; The oxide layer is also provided with an opening group adjacent to the trench structure. The emitter metal is connected to the silicon wafer substrate through the opening group and to the arsenic ion implantation region through the opening group.
2. The Trench-IGBT device transition region structure according to claim 1, characterized in that: The opening group includes a third opening, a fourth opening, and a fifth opening; The third and fourth openings are located on the right side of the long groove, and the fifth opening is located on the right side of the short groove, and the fifth opening is located adjacent to the gap between the third and fourth openings.
3. The Trench-IGBT device transition region structure according to claim 2, characterized in that: The length of the fifth opening is greater than the length of the gap between the third and fourth openings.
4. The Trench-IGBT device transition region structure according to claim 2, characterized in that: The area of the first opening is 1-2 μm. 2 ; The area of the second opening is 2-4 μm. 2 ; The width of each opening group is 1.5μm-2.2μm, the length of the third and fifth openings is 10μm-30μm, and the end of the fourth opening away from the gate BUS structure is flush with the end of the long trench away from the gate BUS structure.
5. A method for fabricating a transition region structure for a Trench-IGBT device, characterized in that, Includes the following steps: Step 1: A terminal oxide layer is grown on the silicon wafer substrate, and then etched to form a terminal structure; Step 2: Etch long trenches and short trenches of alternating lengths on the silicon wafer substrate, wherein the distance between the long trenches and the terminal structure is 35-60 μm; Step 3: A polysilicon layer is deposited and grown using in-situ doping in a furnace tube. The polysilicon layer fills the long trench and the short trench. Photoresist is coated on the polysilicon layer, and the gate BUS structure and the transition polysilicon layer located at the connection between the emitter metal and the short trench are etched out. The polysilicon in the silicon plane is etched clean. There is a gap between the gate BUS structure and the terminal structure; Step 4: After step 3, the upper surface, except for the ion implantation area, is coated with photoresist for arsenic ion implantation. The implantation dose is between 1E15 and 1E16. The arsenic ion implantation area is located in the long trench and partially covers the long trench. Step 5: Deposit an oxide layer formed by borosilicate glass using chemical vapor deposition, and then use a photoresist mask to etch out the first opening in the transition polysilicon layer, the second opening in the region between adjacent second polysilicon layers, and the opening group adjacent to the trench structure. Step 6: Deposit a metal layer with a thickness of 3-6 μm by sputtering, and then use photoresist to etch and form a metal emitter.
6. The method for fabricating a transition region structure of a Trench-IGBT device according to claim 5, characterized in that: The thickness of the terminal oxide layer is 1.5μm-2μm.
7. The method for fabricating a transition region structure of a Trench-IGBT device according to claim 5, characterized in that: The width of the long trench and the short trench is 0.6μm-1.0μm, and the depth of the long trench and the short trench is 5.0μm-6μm.
8. The method for fabricating a transition region structure of a Trench-IGBT device according to claim 5, characterized in that: The long trench is 35-60 μm away from the terminal structure.
9. The method for fabricating a transition region structure of a Trench-IGBT device according to claim 5, characterized in that: In step five, the thickness of the oxide layer is 0.5 μm-1.0 μm.
10. The method for fabricating a transition region structure of a Trench-IGBT device according to claim 1, characterized in that, Includes the following steps: Step 1: A terminal oxide layer is grown on the silicon wafer substrate, and then etched to form a terminal structure; Step 2: Etch long trenches and short trenches of alternating lengths on the silicon wafer substrate, wherein the distance between the long trenches and the terminal structure is 35-60 μm; Step 3: A polysilicon layer is deposited and grown using in-situ doping in a furnace tube. The polysilicon layer fills the long trench and the short trench. Photoresist is coated on the polysilicon layer, and the gate BUS structure and the transition polysilicon layer located at the connection between the emitter metal and the short trench are etched out. The polysilicon in the silicon plane is etched clean. There is a gap between the gate BUS structure and the terminal structure; Step four: After step three, the upper surface, except for the ion implantation area, is coated with photoresist for arsenic ion implantation. The implantation dose is between 1E15 and 1E16, and the implantation width is between 0.8 μm and 1.8 μm. The arsenic ion implantation area is located in the long trench and partially covers the long trench. Step 5: Deposit an oxide layer formed by borosilicate glass using chemical vapor deposition. Then, use a photoresist mask to etch the first opening in the oxide layer that is directly opposite the transition polysilicon layer, the second opening located in the region between adjacent second polysilicon layers, and the group of openings adjacent to the trench structure. Step 6: Deposit a metal layer with a thickness of 3-6 μm by sputtering, and form a metal emitter by photoresist etching. The metal emitter is connected to the transition polysilicon layer through the first opening, and the metal emitter is connected to the silicon wafer substrate through the second opening and the opening group.
Citation Information
Patent Citations
Semiconductor device
US20220344328A1
Semiconductor device
WO2025001343A1