A harmless treatment system and method for aluminum ash

By employing a systematic approach involving pretreatment, melting, slag powder treatment, and waste gas treatment, the pollution problems of aluminum nitride and heavy metals in aluminum ash have been solved. This approach achieves efficient and environmentally friendly harmless treatment of aluminum ash, transforming it into building material resources and reducing energy consumption and processing time.

CN120644437BActive Publication Date: 2026-11-17CHONGQING KANGQI ENVIRONMENTAL PROTECTION TECHNOLOGY CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202510979939.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2025-07-16
Publication Date
2026-11-17
Estimated Expiration
2045-07-16

AI Technical Summary

Technical Problem

Existing technologies cannot effectively treat aluminum nitride and heavy metals in aluminum ash, resulting in ammonia and heavy metal pollution. Furthermore, they are energy-intensive, have long treatment cycles, and are difficult to meet environmental emission standards.

Method used

The system employs a pretreatment module for crushing and washing, a high-temperature melting module for reacting to generate alumina and nitrogen, a slag powder treatment module for rapid cooling, crushing, acid leaching, and microwave sintering, and a waste gas treatment module for purification to meet emission standards. Combined with PLC control and wastewater treatment, it achieves automated linkage.

Benefits of technology

It achieves an aluminum nitride decomposition rate of over 98%, a heavy metal solidification rate of ≥92%, meets waste gas purification standards, allows wastewater reuse, converts slag powder into building material raw materials, reduces energy consumption, shortens the processing cycle, and complies with environmental protection standards.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120644437B_ABST
    Figure CN120644437B_ABST
Patent Text Reader

Abstract

This invention discloses a harmless treatment system for aluminum ash, comprising: a pretreatment module for crushing, removing impurities, and washing the collected aluminum ash; a high-temperature melting module for melting the washed aluminum ash, supplementing energy through the exothermic oxidation of metallic aluminum, causing aluminum nitride to react with oxygen to generate aluminum oxide and nitrogen, while simultaneously using a flux to lower the melting point, promoting the separation of metallic aluminum and slag for separate collection; a slag powder treatment module for rapidly cooling, crushing, grinding, acid leaching, and microwave sintering the molten slag after high-temperature melting to remove harmful substances, solidify heavy metals, and convert them into raw materials usable as building materials; and a waste gas treatment module for achieving purified waste gas emissions that meet standards. This invention has beneficial effects such as reducing external energy input, reducing energy consumption, achieving compliant purification of organic pollutants, reducing manual intervention, and lowering operating costs.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of harmless treatment, and more specifically, to a harmless treatment system and method for aluminum ash. Background Technology

[0002] Aluminum ash is a major solid waste generated during aluminum smelting, casting, and recycling, accounting for approximately 3%-5% of primary aluminum production. Statistics show that over 10 million tons of aluminum ash are produced globally each year, while my country, as a major aluminum producer, generates over 3 million tons annually. Aluminum ash has a complex composition, primarily containing metallic aluminum, alumina, and aluminum nitride, as well as harmful substances such as fluorides, heavy metals, and soluble salts. If improperly disposed of through direct dumping or landfilling, it not only occupies vast amounts of land resources, but the fluorides and heavy metals can also seep into the soil and groundwater through rainwater, while the ammonia gas generated from aluminum nitride reacting with water will pollute the atmosphere, posing a serious threat to the ecological environment and human health. Existing technologies, including natural stacking and simple water washing, can only remove some soluble salts and cannot effectively decompose aluminum nitride or solidify heavy metals. Aluminum nitride reacts slowly with water at room temperature to generate ammonia, and improper handling can lead to continuous ammonia release. Heavy metals exist in a free state in the slag powder and still have biological toxicity, making it difficult to meet environmental emission standards. At the same time, traditional melting methods require temperatures to be raised to over 1500℃, with energy costs accounting for more than 40% of the total treatment cost. Furthermore, the high-temperature process releases acidic gases containing fluorine and sulfur, which can easily lead to acid rain pollution if the waste gas is not properly treated. In addition, traditional slag powder treatment requires natural cooling, multiple grinding, and long-term acid leaching, with an overall treatment cycle of 10-15 hours. Moreover, traditional sintering processes require continuous high-temperature heating for 4-6 hours, and energy consumption has not been fundamentally improved.

[0003] Therefore, those skilled in the art are dedicated to providing a harmless treatment system and method for aluminum ash that can effectively solve the above-mentioned technical problems. Summary of the Invention

[0004] To achieve the above objectives, the present invention provides a harmless treatment system for aluminum ash, comprising: The pretreatment module is used to crush, remove impurities, and wash the collected aluminum ash. The high-temperature melting module is used to melt the water-washed aluminum ash. Energy is supplemented by the exothermic oxidation of metallic aluminum, which allows aluminum nitride to react with oxygen to generate aluminum oxide and nitrogen. At the same time, the melting point is lowered with the help of flux, which promotes the separation of metallic aluminum and slag and collects them separately. The slag powder processing module is used to rapidly cool, crush, grind, acid-leak, and microwave sinter the molten slag after high-temperature melting in order to remove harmful substances, solidify heavy metals, and transform them into building material raw materials. The exhaust gas treatment module is used to achieve exhaust gas purification and emission compliance.

[0005] Furthermore, the pretreatment module includes a jaw crusher, a vibrating screen, a washing tank, a stirrer, and a solid-liquid separator. The jaw crusher and the vibrating screen are used to crush the collected aluminum ash to 0.5-5mm and remove large-sized impurities. The washing tank, stirrer, and solid-liquid separator are used to wash the crushed and screened aluminum ash at a water temperature of 40-60℃ for 20-40 minutes to remove surface fluorides and soluble salts, and separate the washed aluminum ash and washing wastewater.

[0006] Furthermore, the slag powder processing module includes a rapid cooling unit, a crushing and grinding unit, an acid leaching unit, a microwave sintering unit, a mixing mixer, and a gradient field strength microwave sintering furnace unit; The rapid cooling unit is used to rapidly cool the molten slag to form a glassy body and inhibit the precipitation of harmful substances. The crushing and grinding unit is used to crush and grind the quenched slag to 50-100μm to obtain slag powder. The acid leaching unit is used to remove harmful substances from the slag powder. After solid-liquid separation, the leachate enters the heavy metal recovery system, and the leaching residue is washed and dried. In this embodiment, as a further preferred embodiment, the acid leaching unit also includes an ultrasonic vibration device, which is used to destroy the passivation film on the surface of the slag powder through cavitation effect, thereby shortening the acid leaching time to 30-45 minutes.

[0007] The microwave sintering unit includes a silane coupling agent treatment tank, an ultrasonic processor, and a dryer. The leaching residue is treated with a silane coupling agent solution of 5%-10% by mass in the silane coupling agent treatment tank, ultrasonically treated by the ultrasonic processor for 15-30 minutes, and then dried by the dryer to obtain the pretreated leaching residue. A mixing mixer is used to prepare a composite additive to enhance the curing effect of heavy metals. The composite additive contains 3%-5% silica, 1%-2% boric acid, and 0.5%-1% nano-sized components by mass fraction. Mix thoroughly; The gradient field strength microwave sintering furnace unit includes a microwave sintering furnace for sintering a mixture to form a dense building material raw material; the heavy metal solidification rate is ≥92%, and the crystal orientation growth improves the strength. The mixture is formed by mixing pretreated leaching residue and composite additives in a 9:1 ratio and stirring in a mixer for 20-30 minutes. The microwave sintering furnace is equipped with a waste heat recovery unit at the top, which introduces the sintering waste gas (80-120℃) into the preheating section of the spray tower of the waste gas treatment module to heat the 5-10% sodium hydroxide solution to 40-50℃, reducing the heating energy consumption of the spray tower by 15%-20% and increasing the fluoride removal rate by 5-8%. The waste gas treatment module includes a cyclone dust collector for removing particulate matter from the waste gas; a spray tower for removing acidic gases; and an activated carbon adsorption tower for adsorbing organic pollutants.

[0008] Furthermore, it also includes a wastewater treatment unit and a control unit: The wastewater treatment unit is used to treat washing wastewater. The washing wastewater is filtered through a ceramic membrane to remove suspended solids. The pore size of the ceramic membrane is 0.1-0.5μm. Then, fluoride ions and heavy metal ions are separated and recovered through an electrodialysis membrane. The treated wastewater is 100% reused in the washing process, and the fluoride ion recovery rate is ≥90%.

[0009] The control unit includes a PLC control cabinet, temperature sensor, pressure sensor, flow sensor, and AI intelligent control module. The AI ​​intelligent control module automatically optimizes process parameters based on real-time monitoring data (rotary furnace temperature, heavy metal content of slag powder, microwave power) through machine learning algorithms. When the lead content in the slag powder exceeds the standard, it automatically increases the proportion of boric acid in the composite additive to 2.5% and extends the microwave sintering time by 5-10 minutes.

[0010] A method for harmlessly treating aluminum ash includes the following steps: S1: Pre-treat the collected aluminum ash; S2: The pretreated aluminum ash is melted at high temperature to form slag; S3: After the slag is melted at high temperature, it is cooled, crushed, and ground to obtain slag powder; S4: Solid-liquid separation is performed on the residue powder after acid leaching; S5: The generated waste gas is treated by a cyclone dust collector to remove particulate matter; then it enters a spray tower and is sprayed and washed with a 5-10% sodium hydroxide solution to remove acidic gases such as fluorides and sulfur dioxide; finally, the waste gas is adsorbed by an activated carbon adsorption device to adsorb organic pollutants and residual harmful substances, and finally the treated waste gas is discharged.

[0011] Further, the pretreatment in step S1 specifically includes: crushing the collected aluminum ash, then sieving the crushed aluminum ash to achieve a particle size of 0.5-5mm, thereby removing larger impurities. Subsequently, the crushed and sieved aluminum ash is washed with water at a temperature of 40-60℃ for 20-40 minutes. In this invention, by setting the temperature and time, some fluorides and soluble salts adhering to the surface of the aluminum ash can be efficiently removed. After washing, a solid-liquid separation operation is performed promptly to obtain washed aluminum ash and washing wastewater, which are then purified using a wastewater treatment system. In this embodiment, preferably, the collected metallic aluminum (98% purity) is distilled and purified in a vacuum distillation furnace (pressure <10Pa, temperature 850℃), resulting in a residual impurity (Fe, Si) content of <0.1% and an aluminum purity of 99.9%, suitable for the production of 6061 aluminum alloy.

[0012] Further, step S2 specifically includes feeding the washed aluminum ash into a rotary kiln for high-temperature melting treatment. The temperature inside the rotary kiln is controlled at 1200-1400℃, and air or oxygen is introduced to oxidize the metallic aluminum in the aluminum ash, releasing heat and supplementing some of the heat. At the same time, aluminum nitride reacts with oxygen to generate aluminum oxide and nitrogen gas, with a reaction time of 1-3 hours. During the high-temperature melting process, a flux with a mass fraction of 5-10% is added. The flux is a mixture of sodium carbonate and calcium oxide. In this invention, by adding flux, the melting point of the aluminum ash is lowered, promoting the melting of the aluminum ash and the separation of impurities, forming metallic aluminum and slag. The slag is discharged through the slag discharge port, and the metallic aluminum is collected through the aluminum outlet. Preferably, this invention further includes adding a low-temperature melting section after the rotary kiln, and simultaneously turning on microwave-assisted heating (power 200-300W). By utilizing the selective heating of Na2CO3 by microwaves, the separation time of metallic aluminum and slag is shortened from 2 hours to 45 minutes, reducing energy consumption by 18%.

[0013] Further, step S3 specifically includes rapidly cooling the discharged slag with water at a rate of 50-100℃ / s, causing the slag to solidify and form a glassy substance. In this invention, this method inhibits the precipitation of harmful substances. Subsequently, the rapidly cooled slag is crushed and ground to achieve a particle size of 50-100μm, resulting in slag powder.

[0014] Further, step S4 specifically includes acid leaching of the slag powder. The acid used for leaching is a sulfuric acid solution with a mass fraction of 10-20%, the leaching temperature is 60-80℃, and the leaching time is 1-2 hours. In this invention, harmful substances in the slag powder are removed by acid leaching. After acid leaching, solid-liquid separation is performed to obtain leachate and leachate residue. The leachate enters a heavy metal recovery system for processing, and the leachate residue is washed and dried. It can be used as a raw material for building materials. Furthermore, between steps S4 and S5, the process includes mixing the dried leaching residue with silica powder and then performing microwave sintering to obtain building material raw materials, specifically including: S41: Place the dried leaching residue in a 5%-10% silane coupling agent aqueous solution, treat it with ultrasound for 15-30 minutes, and then dry it until the moisture content is <1% to obtain the pretreated leaching residue. S42: 3%-5% silicon dioxide, 1%-2% boric acid, and 0.5%-1% nano-sized components by mass fraction. Mix thoroughly to form a composite additive; S43: Mix the pretreated leaching residue with the composite additive at a ratio of 9:1, and stir for 20-30 minutes using a mixer to form a mixture; S44: Place the mixture in a gradient field strength microwave sintering furnace. The main microwave source at the bottom of the furnace cavity has a frequency of 2.45 GHz and a power density of 1.2-1.5 W / cm³, while the auxiliary microwave source on the side wall has a frequency of 1.8 GHz and a power density of 0.8-1.0 W / cm³. S45: The following three stages are performed using pulse heating mode: S45a: The first stage heating time is ten minutes and the power is 800W; in this invention, the temperature is rapidly increased to the starting temperature required for sintering in the first stage. S45b: In the second stage, after reducing the power from 800W to 500W, intermittent heating is performed. This intermittent heating specifically includes: S45b1: The microwave power is maintained at 500W, and the heating time is from 1 to 1.5 minutes to heat the mixture; S45b2: Microwave power is off for 3.5-6 minutes. At this time, the microwave is paused and the material is no longer actively heated. The material relies on its own residual heat to maintain internal heat conduction and release thermal stress. S45b3: Restart the 500W power for active heating. The active heating time at this stage is 3.5 minutes. S45b4: Turn off the power again and pause for 2-3.5 minutes; S45c: In the third stage, adjust the power to 650W and continue heating for 16.5-17.5 minutes.

[0015] The present invention has the following beneficial effects: 1. In the high-temperature melting module, the temperature is controlled to allow aluminum nitride to fully react with oxygen to generate aluminum oxide and nitrogen, with a decomposition rate of over 98%, eliminating the pollution hazard of aluminum nitride generating ammonia when it comes into contact with water; at the same time, the slag powder treatment module removes soluble heavy metals from the slag powder through acid leaching, and through composite additives and microwave sintering, the heavy metal solidification rate is ≥92%, effectively inhibiting the leaching of heavy metals. 2. The exhaust gas treatment module uses a three-stage treatment process of cyclone dust removal, alkaline spraying, and activated carbon adsorption to improve the fluoride removal rate and ensure that acidic gases and organic pollutants are purified to meet standards. The wastewater treatment unit uses ceramic membrane filtration and electrodialysis membrane separation, with a fluoride ion recovery rate of ≥90%. The treated wastewater is 100% reused in the water washing process. This invention achieves zero emissions through the above methods. 3. After microwave sintering, the slag powder is transformed into a dense building material raw material, which can be used to prepare concrete admixtures, ceramic products, etc., realizing the utilization of slag. In this way, compared with the traditional landfill method, the present invention effectively improves the economic value. At the same time, the heat released by the oxidation of metallic aluminum is used to supplement some of the heat, reducing the external energy input. The waste heat recovery unit at the top of the microwave sintering furnace uses the sintering waste gas to heat the alkaline solution in the spray tower, reducing energy consumption. 4. The PLC control cabinet, combined with temperature, pressure, and flow sensors, enables automated linkage control of each stage, including pretreatment, melting, slag powder treatment, and waste gas and wastewater treatment, reducing manual intervention and lowering operating costs. Attached Figure Description

[0016] Figure 1 This is a schematic flowchart of the method in this invention; Figure 2 This is a schematic block diagram of the aluminum ash harmless treatment system in this invention; Figure 3 This is a schematic diagram of a specific embodiment of the factory layout of the present invention; Figure 4 yes Figure 3 A magnified view of the structure at point A in the middle; Figure 5 yes Figure 3 A magnified schematic diagram of the structure at point B in the middle; Figure 6 yes Figure 3 A magnified schematic diagram of the structure at point C in the middle; Figure 7 yes Figure 3 A magnified schematic diagram of the structure at point D in the middle; Figure 8 yes Figure 3 A magnified schematic diagram of the structure at point E in the middle; Figure 9 yes Figure 3 A magnified schematic diagram of the structure at point F in the middle; Figure 10 This is a schematic diagram of the device connection logic of the preprocessing module in this invention; Figure 11 This is a schematic diagram of the microwave-assisted heating logic of the high-temperature melting module in this invention; Figure 12 This is a schematic diagram of the ultrasonic acid leaching logic of the slag powder treatment module in this invention; Figure 13 This is a schematic diagram of the waste heat utilization logic of the waste gas treatment module in this invention; Figure 14 This is a schematic diagram of the gradient field strength heating and waste heat recovery logic of the microwave sintering furnace in this invention; Figure 15 This is a schematic diagram of the membrane separation process logic of the wastewater treatment unit in this invention.

[0017] The attached diagram lists the components represented by each number as follows: 1. Main entrance and exit of the factory area; 2. Parking lot (10 charging parking spaces, 1 accessible parking space); 3. Biochemical pool (top covered with soil and greenery); 4. Building C (frame structure, fire resistance rating: Class II); 5. Weighbridge; 6. Building B (portal steel frame structure, fire resistance rating: Class II); 7. Rotary furnace smelting workshop; 8. Aluminum ingot finished product workshop; 9. Building A; 10. Rotary kiln equipment area; 11. Aluminum ash and aluminum slag storage area; 12. Control room; 13. Dust collection and emission pipeline; 15 16. Dust collector discharge outlet; 17. Limestone stockpile; 18. Air compressor room; 19. Ball mill; 20. Raw material preparation production line; 21. Guardhouse; 22. Rainwater collection pool; 23. Emergency pool; 24. Crushing and packaging line; 25. Dust collector; 26. Aluminum ash aluminum extraction production line; 27. Secondary entrances and exits of the plant area; 28. Desulfurization tower and discharge outlet; 29. ​​Rotary furnace; 30. Centralized dust collection and discharge pipeline; 31. Multi-tube water-cooled radiator; 32. Deacidification tower; 33. Bag filter; 35. Desulfurization tower. Detailed Implementation

[0018] The present invention will be further described below with reference to the accompanying drawings and embodiments: In the description of this invention, it should be noted that the terms "upper," "lower," "left," "right," "vertical," "horizontal," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing the invention and for simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on the invention. Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.

[0019] In the description of this invention, it should be noted that, unless otherwise explicitly specified and limited, the terms "installation," "setting," and "connection" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.

[0020] like Figures 1 to 15 As shown, an aluminum ash harmless treatment system includes: The pretreatment module is used to crush, remove impurities, and wash the collected aluminum ash. A high-temperature melting module is used to melt water-washed aluminum ash. Energy is supplemented by the exothermic oxidation of metallic aluminum, which causes aluminum nitride to react with oxygen to generate aluminum oxide and nitrogen. At the same time, a flux is used to lower the melting point, promote the separation of metallic aluminum and slag, and collect them separately. In this invention, the high-temperature melting module includes a rotary kiln for high-temperature melting treatment of water-washed aluminum ash. The rotary kiln is connected to the pretreatment module, where pretreated washed aluminum ash is fed into the rotary kiln's feed end via a conveying device. The rotary kiln is also connected to the slag powder treatment module, where the molten slag discharged from the rotary kiln enters the quenching unit of the slag powder treatment module for quenching. Finally, the rotary kiln is connected to the waste gas treatment module, where the waste gas generated by the rotary kiln is connected to the cyclone dust collector (dust collector) for dust removal. In this invention, the rotary kiln of the high-temperature melting module has a rotatable furnace body with an inner diameter of 2-5 meters, a length of 10-30 meters, a furnace body tilt angle of 1-5 degrees, and a rotation speed of 0.5-2 rpm. The inner lining material of the rotary kiln is made of a high-temperature resistant and corrosion-resistant material, effectively extending its service life.

[0021] like Figure 5 As shown, a low-temperature melting section (temperature 900-1100℃) is added to the tail of the rotary kiln, and an auxiliary microwave source (power 200-300W) is turned on simultaneously. By using microwaves to selectively heat sodium carbonate, the separation time between metallic aluminum and molten slag is shortened from 2 hours to 45 minutes.

[0022] The rotary kiln can be heated by gas, oil, or electricity, depending on the specific circumstances. In practical use, to further improve energy efficiency, a waste heat recovery structure is installed at the tail end of the rotary kiln to recover the waste heat from the discharged high-temperature flue gas, which is then used to preheat the combustion air.

[0023] The slag powder processing module is used to rapidly cool, crush, grind, acid-leach, and microwave sinter the molten slag after high-temperature melting to remove harmful substances, solidify heavy metals, and transform them into building material raw materials; such as... Figure 6 As shown, the acid leaching unit has a built-in ultrasonic vibration device (frequency 20-40kHz), which destroys the passivation film on the surface of the slag powder through cavitation effect, shortening the acid leaching time to 30-45min. The leached residue is then treated with a silane coupling agent and enters the microwave sintering furnace.

[0024] The exhaust gas treatment module is used to purify exhaust gas and ensure it meets emission standards. For example... Figure 7 As shown, the sintering exhaust gas is processed through a waste heat recovery unit ( Figure 8The heated sodium hydroxide solution enters the spray tower, which is equipped with a preheating section at the bottom. The waste heat from the sintering exhaust gas is used to raise the temperature of the alkaline solution to 40-50℃, thereby improving the fluoride removal efficiency.

[0025] The pretreatment module includes a jaw crusher, a vibrating screen, a washing tank, a stirrer, and a solid-liquid separator. The jaw crusher and the vibrating screen are used to crush the collected aluminum ash to 0.5-5mm and remove large-sized impurities. The washing tank, stirrer, and solid-liquid separator are used to wash the crushed and screened aluminum ash at a water temperature of 40-60℃ for 20-40 minutes to remove surface fluorides and soluble salts, and separate the washed aluminum ash and washing wastewater.

[0026] like Figure 4 As shown, aluminum ash is coarsely crushed by a jaw crusher and then enters a vibrating screen. The material on the screen (particle size > 5 mm) is returned to the crusher, while the material under the screen (0.5-5 mm) enters a washing tank. The agitator in the washing tank maintains a water temperature of 40-60℃ and stirs for 20-40 minutes. The solid-liquid separator separates the washed aluminum ash from the wastewater.

[0027] The slag powder processing module described in this invention includes a rapid cooling unit (water cooling tank), a crushing and grinding unit, an acid leaching unit, a microwave sintering unit, and a mixing mixer; The rapid cooling unit is used to rapidly cool the molten slag to form a glassy body and inhibit the precipitation of harmful substances. The crushing and grinding unit (cone crusher, ball mill) is used to crush and grind the quenched slag to 50-100μm to obtain slag powder. The acid leaching unit (acid leaching reactor, agitator) is used to remove harmful substances from the slag powder. After solid-liquid separation, the leachate enters the heavy metal recovery system, and the leaching residue is washed and dried. In this embodiment, as a further preferred embodiment, the acid leaching unit also includes an ultrasonic vibration device (frequency 20-40kHz, power density 0.5-1W / cm³), which is used to destroy the passivation film on the surface of the slag powder through cavitation effect, thereby shortening the acid leaching time to 30-45min.

[0028] In this invention, an ultrasonic vibration device is introduced into the acid leaching unit to destroy the passivation film on the surface of the slag powder through cavitation effect, thereby shortening the acid leaching time from 1-2 hours to 30-45 minutes; the entire process cycle is reduced from 10-15 hours in the traditional process to 5-6 hours, thus increasing its production efficiency by 2-3 times.

[0029] The microwave sintering unit includes a silane coupling agent treatment tank, an ultrasonic processor, and a dryer. The leaching residue is treated with a silane coupling agent solution of 5%-10% by mass in the silane coupling agent treatment tank, ultrasonically treated by the ultrasonic processor for 15-30 minutes, and then dried by the dryer to obtain the pretreated leaching residue. A mixing mixer is used to prepare a composite additive to enhance the curing effect of heavy metals. The composite additive comprises 3%-5% silica, 1%-2% boric acid, and 0.5%-1% nano-sized components by mass fraction. Mix thoroughly; The gradient field strength microwave sintering furnace unit (microwave sintering furnace, axial magnetic field generator) is used for sintering mixed materials to form dense building material raw materials; the heavy metal solidification rate is ≥92%, and the crystal orientation growth improves the strength.

[0030] The gradient field strength microwave sintering furnace unit includes a furnace cavity, a main microwave source, an auxiliary microwave source, and a waste heat recovery unit (such as...). Figure 8 As shown in the figure, the main microwave source at the bottom of the furnace cavity has a frequency of 2.45 GHz and a power density of 1.2-1.5 W / cm³, while the auxiliary microwave source on the side wall (frequency 1.8 GHz, power density 0.8-1.0 W / cm³) forms a gradient field heating area through an axial magnetic field generator, so that the temperature field of the mixture is uniformly distributed during sintering. A waste heat recovery unit is set at the top of the furnace body, which introduces the sintering waste gas (80-120℃) into the preheating section of the spray tower of the waste gas treatment module through a pipeline to heat the 5-10% sodium hydroxide solution to 40-50℃, which can reduce the heating energy consumption of the spray tower by 15%-20% and improve the fluoride removal rate by 5-8%.

[0031] The axial magnetic field generator generates an electromagnetic field strength that decreases along the height direction in the furnace cavity by adjusting the phase difference between the main microwave source and the auxiliary microwave source (0.8W / cm³ at the top and 1.5W / cm³ at the bottom), so that the temperature difference between the upper surface and the bottom of the material is ≤50℃, thus avoiding local overheating.

[0032] The microwave sintering furnace is equipped with a waste heat recovery unit at the top, which introduces the sintering waste gas (80-120℃) into the preheating section of the spray tower of the waste gas treatment module to heat the 5-10% sodium hydroxide solution to 40-50℃, reducing the heating energy consumption of the spray tower by 15%-20% and increasing the fluoride removal rate by 5-8%. The waste gas treatment module includes a cyclone dust collector for removing particulate matter from the waste gas; a spray tower for removing acidic gases (fluorides, sulfur dioxide, etc.); and an activated carbon adsorption tower for adsorbing organic pollutants.

[0033] The present invention also includes a wastewater treatment unit and a control unit: The wastewater treatment unit treats washing wastewater, which is filtered through a ceramic membrane to remove suspended solids. The ceramic membrane has a pore size of 0.1-0.5 μm. Fluoride ions and heavy metal ions are then separated and recovered via electrodialysis. The treated wastewater is 100% reused in the washing process, with a fluoride ion recovery rate ≥90%. Figure 9As shown, after the washing wastewater is filtered through a ceramic membrane (pore size 0.1-0.5μm) to remove suspended solids, it enters an electrodialysis membrane separation device to recover fluoride ions. The qualified wastewater after electrodialysis membrane separation is connected to the bottom of the washing tank through a reuse pipe (pipe diameter DN50-80) to maintain the stability of the liquid level and water temperature in the washing tank. The qualified wastewater is returned to the washing tank through the reuse pipe.

[0034] The control unit includes a PLC control cabinet, temperature sensors, pressure sensors, flow sensors, and an AI intelligent control module. Based on real-time monitoring data (rotary furnace temperature, heavy metal content in slag powder, and microwave power), the AI ​​intelligent control module automatically optimizes process parameters using machine learning algorithms. When the lead content in the slag powder exceeds the standard, it automatically increases the proportion of boric acid in the composite additive to 2.5% and extends the microwave sintering time by 5-10 minutes. This ensures stable and controllable processing results and avoids errors from manual adjustment.

[0035] A method for harmlessly treating aluminum ash includes the following steps: S1: Pre-treat the collected aluminum ash; S2: The pretreated aluminum ash is melted at high temperature to form slag; S3: After the slag is melted at high temperature, it is cooled, crushed, and ground to obtain slag powder; S4: Solid-liquid separation is performed on the residue powder after acid leaching; S5: The generated waste gas is treated by a cyclone dust collector to remove particulate matter; then it enters a spray tower and is sprayed and washed with a 5-10% sodium hydroxide solution to remove acidic gases such as fluorides and sulfur dioxide; finally, the waste gas is adsorbed by an activated carbon adsorption device to adsorb organic pollutants and residual harmful substances, and finally the treated waste gas is discharged.

[0036] The pretreatment in step S1 specifically includes: crushing the collected aluminum ash, then sieving the crushed aluminum ash to achieve a particle size of 0.5-5mm, thereby removing larger impurities. Subsequently, the crushed and sieved aluminum ash is washed with water at a temperature of 40-60℃ for 20-40 minutes. In this invention, by setting the temperature and time, some fluorides and soluble salts adhering to the surface of the aluminum ash can be efficiently removed. After washing, a solid-liquid separation operation is performed promptly to obtain washed aluminum ash and washing wastewater, which are then purified using a wastewater treatment system. In this embodiment, preferably, the collected metallic aluminum (98% purity) is distilled and purified in a vacuum distillation furnace (pressure <10Pa, temperature 850℃), resulting in a residual impurity (Fe, Si) content of <0.1% and an aluminum purity of 99.9%, suitable for the production of 6061 aluminum alloy.

[0037] Step S2 specifically includes feeding the washed aluminum ash into a high-temperature rotary furnace for high-temperature melting treatment. The temperature inside the high-temperature rotary furnace is controlled at 1200-1400℃, and air or oxygen is introduced to oxidize the metallic aluminum in the aluminum ash, releasing heat and supplementing some of the heat. At the same time, aluminum nitride reacts with oxygen to generate aluminum oxide and nitrogen gas. The reaction time is 1-3 hours. During the high-temperature melting process, a flux with a mass fraction of 5-10% is added. The flux is a mixture of sodium carbonate and calcium oxide. In this invention, by adding flux, the melting point of the aluminum ash is lowered, promoting the melting of the aluminum ash and the separation of impurities, forming metallic aluminum and slag. The slag is discharged through the slag discharge port, and the metallic aluminum is collected through the aluminum outlet. In a preferred embodiment, the present invention further includes an additional low-temperature melting section (900-1100℃) after the high-temperature rotary kiln, with simultaneous microwave-assisted heating (200-300W). By utilizing the selective heating of Na2CO3 by microwaves, the separation time between metallic aluminum and slag is shortened from 2 hours to 45 minutes, reducing energy consumption by 18%. Compared with traditional sintering, microwave sintering time is shortened from 4-6 hours to within 1 hour, further reducing energy consumption. In this embodiment, the exothermic oxidation of metallic aluminum can provide 30%-40% of the heat required for melting, reducing the rotary kiln energy consumption by 25-30 kWh / ton of aluminum ash. Combined with a flux (sodium carbonate-calcium oxide mixture), the melting temperature is reduced from 1500℃ to 1200-1400℃.

[0038] Step S3 specifically includes rapidly cooling the discharged slag with water at a rate of 50-100℃ / s. This cooling process solidifies the slag and forms a glassy substance, which, in this invention, inhibits the precipitation of harmful substances. Subsequently, the rapidly cooled slag is crushed and ground to achieve a particle size of 50-100μm, yielding slag powder.

[0039] Step S4 specifically includes acid leaching of the slag powder. The acid used for leaching is a sulfuric acid solution with a mass fraction of 10-20%, the leaching temperature is 60-80℃, and the leaching time is 1-2 hours. In this invention, harmful substances in the slag powder are removed by acid leaching. After acid leaching, solid-liquid separation is performed to obtain leachate and leachate residue. The leachate is processed in a heavy metal recovery system, and the leachate residue is washed and dried. It can be used as a raw material for building materials. Between step S4 and step S5, the process further includes mixing the dried leaching residue with silica powder and then microwave sintering it to obtain building material raw materials, specifically including: S41: Place the dried leaching residue in a 5%-10% silane coupling agent aqueous solution, treat it with ultrasound for 15-30 minutes, and then dry it until the moisture content is <1% to obtain the pretreated leaching residue. S42: 3%-5% silicon dioxide, 1%-2% boric acid, and 0.5%-1% nano-sized components by mass fraction. Mix thoroughly to form a composite additive; S43: Mix the pretreated leaching residue with the composite additive at a ratio of 9:1, and stir for 20-30 minutes using a mixer to form a mixture (three-dimensional mixer). S44: Place the mixture in a gradient field strength microwave sintering furnace. The main microwave source at the bottom of the furnace cavity has a frequency of 2.45 GHz and a power density of 1.2-1.5 W / cm³, while the auxiliary microwave source on the side wall has a frequency of 1.8 GHz and a power density of 0.8-1.0 W / cm³. S45: The following three stages are performed using pulse heating mode: S45a: The first stage heating time is ten minutes and the power is 800W; in this invention, the temperature is rapidly increased to the starting temperature required for sintering in the first stage. S45b: In the second stage, after reducing the power from 800W to 500W, intermittent heating is performed. This intermittent heating specifically includes: S45b1: The microwave power is maintained at 500W, and the heating time is from 1 to 1.5 minutes to heat the mixture; S45b2: Microwave power is off for 3.5-6 minutes. At this time, the microwave is paused and the material is no longer actively heated. The material relies on its own residual heat to maintain internal heat conduction and release thermal stress. S45b3: Restart the 500W power for active heating. The active heating time at this stage is 3.5 minutes. S45b4: Turn off the power again and pause for 2-3.5 minutes; perform active heating and pause cycles through the above steps; during the pause phase, the temperature difference between the inside and outside of the material is reduced, which can reduce microcracks caused by thermal expansion and contraction. Compared with the traditional continuous heating method, the heating method in this invention can effectively reduce the crack rate by approximately 10%. S45c: In the third stage, adjust the power to 650W and continue heating for 16.5-17.5 minutes; In this invention, by maintaining the sintering temperature at 800-1000℃ at low to medium power through this step, the slow growth of crystals and the full progress of the heavy metal solidification reaction can be effectively promoted.

[0040] This invention utilizes microwave sintering to achieve a pulse cycle of high-power heating, low-power holding, and medium-power curing, avoiding the problems of overheating or uneven sintering caused by traditional continuous heating. At the same time, it significantly shortens the sintering time compared to the traditional 4-6 hours, improving efficiency and reducing costs.

[0041] Compared with traditional treatment processes, this invention can reduce ammonia emissions by more than 95%, acid gas emissions by more than 80%, and reduce the risk of heavy metal leakage by 90%, effectively curbing the pollution of soil, water and air by aluminum ash; it achieves harmless and resource-based treatment of aluminum ash, which is in line with the national dual-carbon goals and solid waste resource utilization policies, and has significant environmental and social benefits.

[0042] The preferred embodiments of the present invention have been described in detail above. It should be understood that those skilled in the art can make numerous modifications and variations based on the concept of the present invention without creative effort. Therefore, all technical solutions that can be obtained by those skilled in the art based on the concept of the present invention through logical analysis, reasoning, or limited experimentation on the basis of existing technology should be within the scope of protection defined by the claims.

Claims

1. A harmless treatment system for aluminum ash, characterized in that, include: The pretreatment module is used to crush, remove impurities, and wash the collected aluminum ash. The high-temperature melting module is used to melt the water-washed aluminum ash. Energy is supplemented by the exothermic oxidation of metallic aluminum, which allows aluminum nitride to react with oxygen to generate aluminum oxide and nitrogen. At the same time, the melting point is lowered with the help of flux, which promotes the separation of metallic aluminum and slag and collects them separately. The slag powder processing module is used to rapidly cool, crush, grind, acid-leak, and microwave sinter the molten slag after high-temperature melting in order to remove harmful substances, solidify heavy metals, and transform them into building material raw materials. The exhaust gas treatment module is used to achieve exhaust gas purification and emission compliance. The pretreatment module includes a jaw crusher, a vibrating screen, a washing tank, a stirrer, and a solid-liquid separator. The jaw crusher and the vibrating screen are used to crush the collected aluminum ash to 0.5-5mm and remove large-sized impurities. The washing tank, stirrer, and solid-liquid separator are used to wash the crushed and screened aluminum ash at a water temperature of 40-60℃ for 20-40 minutes to remove surface fluorides and soluble salts, and separate the washed aluminum ash and washing wastewater. The slag powder processing module includes a rapid cooling unit, a crushing and grinding unit, an acid leaching unit, a microwave sintering unit, a mixing mixer, and a gradient field strength microwave sintering furnace unit. The rapid cooling unit is used to rapidly cool the molten slag to form a glassy body and inhibit the precipitation of harmful substances. The crushing and grinding unit is used to crush and grind the quenched slag to 50-100μm to obtain slag powder. The acid leaching unit is used to remove harmful substances from the slag powder. After solid-liquid separation, the leachate enters the heavy metal recovery system, and the leaching residue is washed and dried. The acid leaching unit also includes an ultrasonic vibration device, which is used to destroy the passivation film on the surface of the slag powder through cavitation effect, and shorten the acid leaching time to 30-45 minutes. The microwave sintering unit includes a silane coupling agent treatment tank, an ultrasonic processor, and a dryer. The leaching residue is treated with a silane coupling agent solution of 5%-10% by mass in the silane coupling agent treatment tank, ultrasonically treated by the ultrasonic processor for 15-30 minutes, and then dried by the dryer to obtain the pretreated leaching residue. The mixing mixer is used to prepare a composite additive, which is prepared by uniformly mixing 3%-5% silica, 1%-2% boric acid and 0.5%-1% nano TiO2 by mass fraction. A gradient field strength microwave sintering furnace unit includes a microwave sintering furnace, used for sintering a mixture to form a dense building material raw material. The mixture is formed by mixing pretreated leaching residue and composite additives in a 9:1 ratio and stirring with a mixer for 20-30 minutes. The microwave sintering furnace is equipped with a waste heat recovery unit at the top, which introduces sintering waste gas at 80-120℃ into the preheating section of the spray tower of the waste gas treatment module to heat a 5%-10% sodium hydroxide solution to 40-50℃, reducing the heating energy consumption of the spray tower by 15%-20% and increasing the fluoride removal rate by 5%-8%. The waste gas treatment module includes a cyclone dust collector for removing particulate matter from the waste gas; a spray tower for removing acidic gases; and an activated carbon adsorption tower for adsorbing organic pollutants.

2. The aluminum ash harmless treatment system as described in claim 1, characterized in that, It also includes wastewater treatment units and control units: The wastewater treatment unit is used to treat washing wastewater, which is filtered through a ceramic membrane to remove suspended solids. The ceramic membrane has a pore size of 0.1-0.5 μm, and then fluoride ions and heavy metal ions are separated and recovered through an electrodialysis membrane. The control unit includes a PLC control cabinet, temperature sensor, pressure sensor, flow sensor, and AI intelligent control module. The AI ​​intelligent control module automatically optimizes process parameters based on real-time monitoring data and machine learning algorithms. When the lead content in the slag powder exceeds the standard, it automatically increases the proportion of boric acid in the composite additive to 2.5% and extends the microwave sintering time by 5-10 minutes.

3. A method for harmlessly treating aluminum ash, characterized in that, The aluminum ash harmless treatment system described in claim 2 is used for treatment, including the following steps: S1: Pre-treat the collected aluminum ash; S2: The pretreated aluminum ash is melted at high temperature to form slag; specifically, the washed aluminum ash is fed into a rotary kiln for high-temperature melting treatment. The temperature inside the rotary kiln is controlled at 1200-1400℃, and air or oxygen is introduced to oxidize the metallic aluminum in the aluminum ash and release heat, supplementing some of the heat. At the same time, aluminum nitride reacts with oxygen to generate aluminum oxide and nitrogen gas. The reaction time is 1-3 hours. During the high-temperature melting process, a flux with a mass fraction of 5%-10% is added. The flux is a mixture of sodium carbonate and calcium oxide to form metallic aluminum and slag. The slag is discharged through the slag discharge port, and the metallic aluminum is collected through the aluminum outlet. S3: Cooling, crushing, and grinding the slag discharged after high-temperature melting treatment to obtain slag powder; specifically, the discharged slag is rapidly cooled by water at a rate of 50-100℃ / s, which causes the slag to solidify and form a glassy body. Then, the rapidly cooled slag is crushed and ground to achieve a particle size of 50-100μm to obtain slag powder. S4: Solid-liquid separation is performed after acid leaching of the slag powder; S4 specifically includes acid leaching of the slag powder, the acid used for acid leaching is a sulfuric acid solution with a mass fraction of 10%-20%, the acid leaching temperature is 60-80℃, the acid leaching time is 1-2h, and solid-liquid separation is performed after acid leaching to obtain leachate and leachate residue. The leachate enters the heavy metal recovery system for processing, and the leachate residue is washed and dried. This also includes mixing dried leaching residue with silica powder and then microwave sintering it to obtain building material raw materials, specifically including: S41: Place the dried leaching residue in an aqueous solution of 5%-10% silane coupling agent by mass, treat it with ultrasound for 15-30 minutes, and then dry it until the moisture content is <1% to obtain the pretreated leaching residue. S42: Mix 3%-5% silica, 1%-2% boric acid, and 0.5%-1% nano-TiO2 by mass to form a composite additive; S43: Mix the pretreated leaching residue with the composite additive at a ratio of 9:1, and stir for 20-30 minutes using a mixer to form a mixture; S44: Place the mixture in a microwave sintering furnace. The main microwave source at the bottom of the furnace cavity has a frequency of 2.45 GHz and a power density of 1.2-1.5 W / cm³, while the auxiliary microwave source on the side wall has a frequency of 1.8 GHz and a power density of 0.8-1.0 W / cm³. S45: The following three stages are performed using pulse heating mode: S45a: The first stage heating time is ten minutes, and the power is 800W; S45b: In the second stage, after reducing the power from 800W to 500W, intermittent heating is performed. This intermittent heating specifically includes: S45b1: The microwave power is maintained at 500W, and the heating time is from 1 to 1.5 minutes to heat the mixture; S45b2: Microwave power is turned off for 3.5-6 minutes. At this time, the mixture is in a paused state and is no longer actively heated. The mixture relies on its own residual heat to maintain internal heat conduction and release thermal stress. S45b3: Reactivate the 500W power for active heating. The active heating time at this stage is 3.5 minutes. S45b4: Power off again for a pause of 2-3.5 minutes; S45c: In the third stage, adjust the power to 650W and continue heating for 16.5-17.5 minutes; S5: The generated waste gas is treated by a cyclone dust collector to remove particulate matter; then it enters a spray tower and is sprayed and washed with a 5%-10% sodium hydroxide solution to remove fluorides and sulfur dioxide; finally, the waste gas is adsorbed by an activated carbon adsorption device to adsorb organic pollutants and residual harmful substances, and finally the treated waste gas is discharged.

4. The method for harmless treatment of aluminum ash as described in claim 3, characterized in that, The pretreatment in S1 specifically includes: crushing the collected aluminum ash, then sieving the crushed aluminum ash to achieve a particle size of 0.5-5mm, thereby removing larger impurities; then washing the crushed and sieved aluminum ash with water at a temperature of 40-60℃ for 20-40 minutes; after washing, performing solid-liquid separation to obtain washed aluminum ash and washed wastewater, and purifying the washed wastewater through a wastewater treatment system.

5. The method for harmless treatment of aluminum ash as described in claim 4, characterized in that, it further... include: The collected aluminum metal with a purity of 98% is sent to a vacuum distillation furnace for distillation purification. After this distillation purification, the purity of the aluminum metal is increased to 99.9%, and the residual silicon impurity in the aluminum metal is less than 0.1%. This aluminum metal can be used in the production of 6061 aluminum alloy.

6. The method for harmless treatment of aluminum ash as described in claim 5, characterized in that, The distillation furnace operates at a pressure of less than 10 Pa and a temperature of 850 °C.

Citation Information

Patent Citations

  • Harmless treatment and recycling process for aluminum ash

    CN116408329A