3D touch line manufacturing process of glass palm rest touch pad
By etching the entire surface of tempered glass to form an anti-glare layer, and combining screen printing of solvent ink and UV ink layers with multi-stage curing treatment, the adhesion and strength issues of the 3D touch lines on the tempered glass touch panel were solved, and the strong adhesion and structural stability of the UV ink layer were achieved.
Patent Information
- Application Number
- CN202510780500.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-06-12
- Publication Date
- 2025-10-03
AI Technical Summary
In the prior art, the 3D touch lines of tempered glass touch panels are prone to micro-cracks at the base of the raised lines formed by etching, which reduces the structural strength. In addition, UV ink cannot effectively adhere to the glass surface, and cannot meet the user's requirements for physical properties.
After the anti-glare layer is formed by full-surface etching, a combination of screen-printed solvent ink layers and UV ink layers is used, combined with anti-ink overflow gaskets and multi-stage curing treatment to ensure that the UV ink layer is firmly attached to the tempered glass and a second anti-glare layer is formed during the curing process.
It solves the problem of poor adhesion between the UV ink layer and the glass surface, ensures the touch line's stable adhesion, avoids ink overflow during the printing process, and improves the structural strength and aesthetic effect of the touch line.
Smart Images

Figure CN120736807A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of surface treatment of consumer electronic devices, and in particular to a manufacturing process for 3D touch lines of a glass palm rest touch panel. Background Art
[0002] In order to improve the integrity of the area in front of the keyboard, existing laptops will make the touchpad in the middle of the front of the keyboard and the palm rests on both sides into an integral panel, and use raised lines (tactile lines) to separate the touch area and non-touch area to facilitate blind operation. High-end laptops use tempered glass as the panel material, but the matte decorative effect of the existing tempered glass surface is an etching process, such as Figure 1 As shown, using etching to create raised lines (tactile lines) disrupts the integrity of the tempered glass surface structure, leading to microcracks at the steps formed at the base of the etched raised lines (tactile lines). This significantly reduces structural strength and causes the glass to fail the drop ball test. Furthermore, using screen printing with conventional UV inks to create raised lines (tactile lines) fails to adhere to the glass surface, failing to meet user requirements for physical properties. Summary of the Invention
[0003] The main technical problem solved by the present invention is to provide a manufacturing process for 3D touch lines of a glass palm rest touch panel, which can ensure the strength of the 3D touch line structure on the touch panel.
[0004] To solve the above technical problems, the present invention adopts a technical solution: providing a 3D touch line manufacturing process for a glass palm rest touch panel, comprising the following steps:
[0005] S1. Etching the entire surface of white glass to form a first anti-glare layer, and then cutting, tempering, and printing an ink layer on the back to obtain tempered glass;
[0006] S2, screen printing a solvent ink layer on the surface of the first anti-glare layer of the tempered glass and adhering to the first anti-glare layer;
[0007] S3, screen printing a UV ink layer on the solvent ink layer in a 1:1 ratio to form a tactile line main body, with the UV ink layer attached to the solvent ink layer;
[0008] S4. After removing the screen printing stencil, the touch sensing line body is cured. During the curing process, a second anti-glare layer is formed on the surface of the touch sensing line body, and finally a touch sensing line attached to the tempered glass is formed.
[0009] Preferably, the screen plate for screen printing the solvent ink layer and the screen plate for screen printing the UV ink layer are the same screen plate and the screen plate cannot be unlocked by the locking mechanism during the process of screen printing the solvent ink layer and the screen printing the UV ink layer.
[0010] Preferably, the screen printing screen is a polyester mesh or a steel mesh.
[0011] Preferably, after completing step S2, an anti-ink overflow gasket is laid between the screen printing screen and the tempered glass. The anti-ink overflow gasket is arranged on both sides of the solvent ink layer. The anti-ink overflow gasket is used to support the position height of the screen, reduce the deformation of the screen during screen printing, and thus reduce ink overflow caused by screen deformation when printing the UV ink layer.
[0012] Preferably, the anti-ink spill gasket is made of a paper substrate, a cloth substrate or a plastic substrate, and is a single-sided adhesive tape.
[0013] Preferably, the ink overflow prevention gasket is composed of one or more layers of adhesive tape, and the height of the ink overflow prevention gasket is matched with the required height of the touch-sensitive line body.
[0014] Preferably, both ends of the ink overflow prevention gasket in the length direction are longer than both ends of the touch line in the length direction by 10 mm or more.
[0015] Preferably, the curing process includes: first irradiating the tactile line body with a preliminary curing lamp in an inert gas chamber to preliminarily shape the tactile line body and prevent it from flowing and deforming; then irradiating it with an ultrashort-wave UV lamp to form a second anti-glare layer on the surface of the tactile line body; and finally irradiating it with a full-band curing lamp to completely cure the tactile line body into a tactile line.
[0016] Preferably, the preliminary curing lamp is an LED or a mercury lamp; the ultrashort-wave UV lamp has a wavelength of 254 nm or 172 nm, and the light source is an LED lamp; the full-band curing lamp is a mercury lamp; and the inert gas in the inert gas chamber is nitrogen or argon.
[0017] The present invention provides a glass palm rest touch panel, which is manufactured using the above manufacturing process.
[0018] The beneficial effects of the present invention are:
[0019] 1. By connecting the UV ink layer and the tempered glass of the touch panel through a solvent layer, the problem of the touch cable not being able to firmly adhere to the tempered glass due to the poor adhesion of the UV ink layer to the glass surface is solved, so that the touch cable can be stably and firmly attached to the tempered glass of the touch panel;
[0020] 2. The anti-overflow gasket raises the level of the stencil and provides support for the stencil, thus avoiding the problem of UV ink overflow when printing the UV ink layer due to the pressure of the scraper on the stencil and the elastic deformation of the stencil itself, thereby reducing the problem of ink overflow when printing the UV ink layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1This is a schematic diagram of the structure of the touch line directly realized by etching process in the existing technology
[0022] Figure 2 This is a cross-sectional view of the tactile wire of the present invention combined with the tempered glass;
[0023] Figure 3 This is a top view of the tactile wire of the present invention combined with the tempered glass;
[0024] Figure 4 This is a schematic diagram of the positional relationship between the screen, the anti-ink overflow gasket and the tempered glass when printing the UV ink layer of the present invention;
[0025] Figure 5 It is a schematic diagram of the process of curing the touch-sensitive wire of the present invention.
[0026] The markings of the components in the accompanying drawings are as follows:
[0027] 1. Tempered glass; 11. Base layer; 12. First anti-glare layer;
[0028] 2. Solvent ink layer;
[0029] 3. UV ink layer; 31. Second anti-glare layer;
[0030] 4. Anti-ink spill gasket;
[0031] 5. Screen plate;
[0032] 6. Tactile line;
[0033] 7. Scraper;
[0034] 81. Preliminary curing lamp; 82. Ultra-short wave UV lamp; 83. Full-band curing lamp; 84. Inert gas chamber. DETAILED DESCRIPTION
[0035] To make the above-mentioned objects, features, and advantages of the present invention more readily apparent, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings. The following description sets forth numerous specific details to facilitate a full understanding of the present invention. However, the present invention can be implemented in many other ways than those described herein, and those skilled in the art may make similar modifications without departing from the scope of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below.
[0036] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like to indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.
[0037] Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of the technical features being referred to. Thus, a feature defined as "first" or "second" may explicitly or implicitly include at least one such feature. In the description of the present invention, "plurality" means at least two, such as two, three, etc., unless otherwise specifically defined.
[0038] In the present invention, unless otherwise specified or limited, the terms "installed," "connected," "connect," "fixed," etc. should be understood in a broad sense. For example, they can refer to fixed connection, detachable connection, or integration; mechanical connection, electrical connection; direct connection, or indirect connection through an intermediate medium; internal communication between two components, or interaction between two components, unless otherwise specified. Those skilled in the art will understand the specific meanings of the above terms in the present invention based on specific circumstances.
[0039] In the present invention, unless otherwise expressly specified or limited, when a first feature is "above" or "below" a second feature, it may mean that the first and second features are in direct contact, or that the first and second features are in indirect contact through an intermediary. Furthermore, when a first feature is "above," "above," or "above" a second feature, it may mean that the first feature is directly above or diagonally above the second feature, or simply means that the first feature is at a higher level than the second feature. When a first feature is "below," "below," or "below" a second feature, it may mean that the first feature is directly below or diagonally below the second feature, or simply means that the first feature is at a lower level than the second feature.
[0040] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it may be directly on the other element or there may be an intermediate element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be an intermediate element. The terms "vertical," "horizontal," "upper," "lower," "left," "right," and similar expressions used herein are for illustrative purposes only and do not represent the only implementation methods.
[0041] Physical quantities in formulas, unless otherwise specified, should be understood as basic quantities of the International System of Units (SI) basic units, or derived quantities derived from basic quantities through mathematical operations such as multiplication, division, differentiation or integration.
[0042] Example 1:
[0043] refer to Figure 1-Figure 5 A manufacturing process for a 3D touch line of a glass palm rest touch panel includes the following steps:
[0044] S1. Etching the entire surface of a white glass sheet to form a first anti-glare layer 12. The entire surface etching does not form raised lines as in the prior art. Instead, the etched front surface forms a first anti-glare layer 12 with a uniform height. After cutting, tempering, and printing an ink layer on the back surface, a tempered glass 1 is obtained. Therefore, the tempered glass 1 includes a base layer 11 and a first anti-glare layer 12.
[0045] S2, screen printing a solvent ink layer 2 on the surface of the first anti-glare layer 12 of the tempered glass 1, the solvent ink layer 2 can react with the tempered glass 1, so that the solvent ink layer 2 can be stably attached to the first anti-glare layer 12;
[0046] S3, screen printing a UV ink layer 3 on the solvent ink layer 2 in a 1:1 ratio, wherein the UV ink layer 3 reacts with the solvent ink layer 2, so that the UV ink layer 3 is stably attached to the solvent ink layer 2 and forms a tactile line body;
[0047] S4 , after removing the screen printing stencil 5 , the tactile line body is cured. During the curing process, a second anti-glare layer 31 is formed on the surface of the tactile line body, and finally the tactile line 6 attached to the tempered glass 1 is formed.
[0048] refer to Figure 4 The screen plate 5 for screen printing the solvent ink layer 2 and the screen plate 5 for screen printing the UV ink in steps S2 and S3 are the same screen plate 5. During the screen printing of the solvent ink layer 2 and the UV ink layer 3, the screen plate 5 cannot be unlocked by the locking mechanism, thereby ensuring that the UV ink layer 3 can be accurately printed on the solvent ink layer 2. The screen printing screen plate 5 is a polyester mesh with a mesh size that can be selected between 350 and 420 as needed.
[0049] refer to Figure 2 and Figure 4 After step S2 is completed, when printing the UV ink layer 3, anti-spill spacers 4 are placed between the screen printing stencil 5 and the tempered glass 1. These spacers 4 are placed on either side of the solvent ink layer 2, with the center distance between the spacers and the solvent ink layer 2 being 5-25 mm, preferably 15 mm. The anti-spill spacers 4 support the height of the screen printing stencil 5, minimizing deformation during screen printing and thus reducing ink spillage caused by deformation during printing of the UV ink layer 3. After printing the solvent ink layer 2, it already has a certain height. If the UV ink layer 3 is printed directly on the stencil 5, the pressure of the stencil 7 and the deformation of the stencil 5 will cause the solvent ink layer 2 to form a bulge at that location after multiple printings. If the UV ink is then printed directly, the deformation of the stencil 5 will cause the UV ink to overflow to both sides of the solvent ink layer 2, resulting in a jagged appearance at a microscopic level and failing to meet the desired requirements. However, the stencil 5 is elevated by the anti-overflow spacers 4, which are placed on both sides of the tactile line 6. The thickness of the anti-ink overflow gasket 4 can be 0.05-0.5mm, and it is composed of one or more layers of tape. The specific thickness and number of layers can be freely selected according to actual needs in this field, and the height of the corresponding anti-ink overflow gasket 4 is matched according to the required height of the tactile line body. In order to offset the pressure of the scraper 7 and the deformation of the screen 5, the horizontal height of the screen 5 after laying the anti-ink overflow gasket 4 is higher than the height of the solvent ink layer 2, thereby overcoming the pressure of the scraper 7 and the deformation of the screen 5, so that the horizontal position of the screen 5 just matches the height of the UV ink layer 3 during actual printing.
[0050] refer to Figure 4 The anti-ink spill gasket 4 is made of one of paper base material, cloth base material or plastic base material, and is a single-sided adhesive tape. The anti-ink spill gasket 4 is pasted on the screen plate 5 through the adhesive side, thereby ensuring the support of the screen plate 5 while ensuring the stability of the position connection between the anti-ink spill gasket 4 and the screen plate 5.
[0051] refer to Figure 3 and Figure 4 To better support the position of the stencil 5 and achieve better printing results when printing the UV ink layer 3, the two ends of the ink-spill prevention gasket 4 are at least 10 mm longer than the two ends of the tactile line 6. The width of the ink-spill prevention gasket 4 can be 3-30 mm, with 10 mm being preferred. The specific width can be freely selected by those skilled in the art.
[0052] refer to Figure 4 and Figure 5Before the curing process, the screen 5 will be removed. Since the anti-spill ink gasket 4 is pasted on the screen 5, it will be removed together with the screen printed screen 5. The jig carrying the touch panel is then sent to the curing device via the conveyor line for curing. The curing process includes: the touch line body is first irradiated by the preliminary curing lamp 81 in the inert gas chamber 84 of the curing device to give the touch line body a preliminary shape to prevent flow and deformation, and then irradiated by the ultra-short wave UV lamp 82 to form a second anti-glare layer 31 on the surface of the touch line body, and finally irradiated by the full-band curing lamp 83 to completely cure the touch line 6 body into a tactile line. The preliminary curing lamp 81 is an LED; the ultra-short wave UV lamp 82 has a wavelength of 254nm and the light source is an LED lamp; the full-band curing lamp 83 is a mercury lamp; and the inert gas in the inert gas chamber 84 is argon.
[0053] Example 2
[0054] The difference between Example 2 and Example 1 is that the screen printing screen 5 is a steel mesh with a mesh size of 300-500. The preliminary curing lamp 81 is a mercury lamp, the ultrashort-wave UV lamp 82 has a wavelength of 172 nm, and the inert gas in the inert gas chamber 84 is nitrogen.
[0055] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention's description and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.
Claims
1. A 3D touch line manufacturing process for a glass palm rest touch panel, characterized in that: The steps include: S1, etching the entire surface of a white glass sheet to form a first anti-glare layer (12), and then cutting, tempering, and printing an ink layer on the back to obtain a tempered glass (1); S2, a solvent ink layer (2) screen-printed on the surface of the first anti-glare layer (12) of the tempered glass (1) and attached to the first anti-glare layer (12); S3, screen printing a UV ink layer (3) on the solvent ink layer (2) in a 1:1 ratio to form a tactile line main body, wherein the UV ink layer (3) is attached to the solvent ink layer (2); S4, after removing the screen printing screen (5), curing the touch line body, forming a second anti-glare layer (31) on the surface of the touch line body during the curing process, and finally forming a touch line (6) attached to the tempered glass (1).
2. The manufacturing process for a 3D touch line of a glass palm rest touchpad according to claim 1, characterized in that: The screen plate (5) for screen printing a solvent ink layer (2) and the screen plate (5) for screen printing a UV ink layer (3) are the same screen plate (5), and the screen plate (5) cannot be unlocked by a locking mechanism during the process of screen printing the solvent ink layer (2) and the screen printing the UV ink layer (3).
3. The manufacturing process for a 3D touch line of a glass palm rest touchpad according to claim 2, characterized in that: The screen printing screen plate (5) is a polyester mesh or a steel mesh.
4. The manufacturing process for a 3D touch line of a glass palm rest touchpad according to claim 2, characterized in that: After completing step S2, an anti-ink overflow gasket (4) is laid between the screen printing screen (5) and the tempered glass (1). The anti-ink overflow gasket (4) is arranged on both sides of the solvent ink layer (2). The anti-ink overflow gasket (4) is used to support the position height of the screen (5) to reduce the deformation of the screen (5) during screen printing, thereby reducing ink overflow caused by the deformation of the screen (5) when printing the UV ink layer (3).
5. The manufacturing process for a 3D touch line of a glass palm rest touch panel according to claim 4, characterized in that: The ink overflow prevention gasket (4) is made of a paper base material, a cloth base material or a plastic base material, and is a single-sided adhesive tape.
6. The manufacturing process for a 3D touch line of a glass palm rest touch panel according to claim 5, characterized in that: The ink overflow prevention gasket (4) is composed of one or more layers of adhesive tape, and the height of the ink overflow prevention gasket (4) is matched according to the required height of the touch-sensitive line body.
7. A process for manufacturing 3D touch lines for a glass palm rest touch panel according to any one of claims 4 to 6, characterized in that: Both ends of the ink overflow prevention gasket (4) in the length direction are longer than both ends of the touch line (6) in the length direction by 10 mm or more.
8. The manufacturing process for a 3D touch line of a glass palm rest touch panel according to claim 1, characterized in that: The curing process comprises: firstly irradiating the tactile line body in an inert gas chamber (84) with a preliminary curing lamp (81) to preliminarily shape the tactile line body and prevent it from flowing and deforming; then irradiating the tactile line body with an ultrashort-wave UV lamp (82) to form a second anti-glare layer (31) on the surface of the tactile line body; and finally irradiating the tactile line body with a full-band curing lamp (83) to completely cure the tactile line body to form the tactile line (6).
9. The manufacturing process for a 3D touch line of a glass palm rest touch panel according to claim 8, characterized in that: The preliminary curing lamp (81) is an LED or a mercury lamp; the ultrashort-wave UV lamp (82) has a wavelength of 254nm or 172nm, and the light source is an LED lamp; the full-band curing lamp (83) is a mercury lamp; and the inert gas in the inert gas chamber (84) is nitrogen or argon.
10. A glass palm rest touchpad, characterized in that: The invention is manufactured by the manufacturing process described in any one of claims 1 to 9.