Salt crystallization inhibitor for preventing sodium chloride crystallization in oil well construction and preparation method thereof

By using microemulsion salt crystallization inhibitors composed of sodium polyacrylate and other compounds, the problems of easy decomposition and high cost of salt crystallization inhibitors in high-temperature acidic environments have been solved, achieving efficient and low-cost salt crystallization protection and improving oil and gas field production efficiency and equipment life.

CN120924254APending Publication Date: 2025-11-11CHANGZHOU UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510956818.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-07-11
Publication Date
2025-11-11

AI Technical Summary

Technical Problem

Existing salt crystallization inhibitors are prone to decomposition in high-temperature and acidic environments, are costly, incompatible with other chemicals, and their effectiveness is affected by oil and gas field conditions, thus failing to provide long-term and stable protection against salt crystallization.

Method used

A combination of sodium polyacrylate, sodium citrate, sodium tripolyphosphate, octadecyltrimethylammonium chloride, fatty alcohol polyoxyethylene ether, ethylene glycol, and sodium hydroxide is used to form a microemulsion liquid inhibitor through complexation reaction and surfactant action, thereby changing the crystal morphology and improving solubility.

Benefits of technology

It significantly improves the solubility of sodium chloride, reduces the aggregation of crystal particles, lowers the risk of equipment failure, extends the life of pipelines and equipment, and reduces production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FT_1
    Figure FT_1
Patent Text Reader

Abstract

The invention discloses a salt crystallization inhibitor for preventing sodium chloride crystallization in oil well construction and a preparation method thereof. The sodium tripolyphosphate, the octadecyl trimethyl ammonium chloride, the fatty alcohol-polyoxyethylene ether and the like are prepared with the sodium polyacrylate salt crystallization inhibitor, so that the salt crystallization inhibition effect of polyacrylic acid derivatives and other organic compounds is greatly improved. The inhibitor has the advantages of being simple in formula, convenient to operate, low in production cost and the like, the production efficiency of petroleum and inorganic chemical industries can be improved, and the service life of pipelines and equipment can be prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of oilfield construction materials, and particularly relates to oilfield well materials and their preparation methods, specifically to a salt crystallization inhibitor for preventing sodium chloride crystallization during oil well construction and its preparation method. Background Technology

[0002] In the field of petroleum engineering, research and application of salt crystallization inhibitors mainly focus on solving the blockage problem caused by salt crystallization during oil wells and drilling. Salt crystallization, especially sodium chloride crystallization, forms crystalline salt plugs in oil wells and drilling equipment, leading to problems such as equipment blockage, pump sticking, and wellbore collapse, seriously affecting oil extraction efficiency and safety. Traditional solutions include thermal dissolution and mechanical cleaning, but these methods are complex and costly.

[0003] Salt crystallization inhibitors prevent the formation and growth of salt crystals, thus preventing salt blockages, through chemical means. Inhibitors typically achieve this by increasing the solubility of the salt in water or altering its crystal morphology. In recent years, researchers have developed various highly effective salt crystallization inhibitors, such as urea, glycerol, and EDTA tetraammonium. These inhibitors not only effectively improve the water solubility of sodium chloride but also maintain their inhibitory effect over a wide temperature range. Furthermore, researchers have developed various compound inhibitors and specialized formulations to address different salt crystallization problems and meet the needs of various operating conditions.

[0004] As early as 1992, Zheng Ruozhi and Zhang Guozhao proposed an NTA salt recrystallization inhibitor, which effectively solves the problem of salt recrystallization caused by temperature differences in saturated brine drilling fluid systems, preventing complex downhole accidents such as wellbore enlargement and salt jamming. This inhibitor has a significant inhibitory effect on various salts such as sodium chloride, calcium chloride, and magnesium chloride, exceeding the level of similar products from Calgon Corporation in the United States. It can be compounded with various supersaturated brine drilling fluid systems without adversely affecting drilling fluid performance, and it also helps reduce filtration loss and has a certain corrosion inhibition effect.

[0005] In 2015, Liu Renzhi et al. addressed the issues that conventional organic phosphonates, inorganic small molecules such as SiO2, Al2O3, and polyacrylic acid derivatives do not significantly inhibit crystallization, and that the released soluble salt particles are relatively large, easily increasing the pore stress of the stone. They proposed a new method utilizing the crystallization inhibition effect of K4Fe(CN)6 to remove NaCl soluble salts from the stone pores. K4Fe(CN)6 inhibits the crystallization of NaCl... + It has an adsorption effect, which hinders the migration of ions and inhibits the formation of crystal nuclei. During the crystallization process, NaCl changes from its original cubic crystal form to a dendritic crystal form, which promotes the uneven growth of crystals to form a dendritic structure and causes "salt rock creep". The richer the capillary structure of the stone, the more conducive it is to the occurrence of salt rock creep.

[0006] In 2016, Song Fang developed a salt recrystallization inhibitor for oil and gas wells by addressing the problem of salt recrystallization encountered during drilling, using a method to increase the solubility of sodium chloride. This inhibitor, primarily composed of organometallic complexes, inorganic complexes, corrosion inhibitors, and anti-swelling agents, alters the shape of sodium chloride crystals by masking specific metal ions, changing them from cubic to dendritic or snowflake-like structures. This reduces the adhesion of crystals to solid surfaces, thereby increasing the solubility of sodium chloride in water. Furthermore, it is unaffected by calcium and magnesium ions, effectively preventing pump jamming.

[0007] In 2016, Ma Chao et al., addressing the problems of high salinity in high-salinity formations, the generation of large amounts of salt scale during oil well production, leading to significantly increased maintenance costs, a marked decrease in production, poorer acid fracturing effects, high water squeezing pressure, and short effective lifespan, screened out three salt suppressants with good salt-suppressing effects. Based on this, they optimized the optimal composite salt suppressant formula: 160 mg / L salt suppressant A + 260 mg / L salt suppressant B + 42 mg / L salt suppressant C. These three salt suppressants are inorganic ferrocyanide salt suppressant, nitrogen-tritium salt, and polyacrylamide polymer, respectively. The presence of salt suppressant A reduces the amount of salt crystal precipitation, while the presence of salt suppressants B and C effectively alters the morphology of the precipitated crystals, making them smaller and significantly compensating for the shortcomings of salt suppressant A.

[0008] In 2019, Deng Zhaoping and others, starting from the perspective of increasing sodium chloride solubility to inhibit crystallization at its source, disclosed a salt crystallization inhibitor for oil wells, mainly composed of urea, glycerol, and EDTA tetraammonium. Its innovation lies in the solubilizing effect of the added EDTA tetraammonium and glycerol, and the addition of a selectively adsorbable soluble low-molecular-weight cationic resin, which reduces the effective concentration of sodium ions and the probability of sodium ions encountering chloride ions, thus preventing crystallization at the source of sodium chloride nucleation. The addition of surfactant OP-10 increases the miscibility of oil and water, causing sodium and chloride ions to partially transfer from the water-soluble state to the oil-soluble state, avoiding excessive concentration of sodium and chloride ions in aqueous solution. Urea acts as an anti-coagulant, reducing the viscosity of crude oil in the inhibitor system. Experimental results show that the use of this salt crystallization inhibitor can significantly increase the solubility of sodium chloride, thereby effectively preventing crystallization at its source.

[0009] After years of development, research on salt crystallization inhibitors has become relatively complete, but some problems still exist: (1) Inorganic ferrocyanide salt crystallization inhibition is easily decomposed in high temperature and acidic environment to produce toxic gas potassium cyanide. Therefore, its application range is very limited and it cannot cope well with the complex working conditions at the bottom of the well.

[0010] (2) The combination of multiple salt crystallization inhibitors has a very significant effect, but it often brings a problem: its cost is high, which increases the cost of oil and gas field exploration and production. In addition, the continuous use and replenishment of such inhibitors will further increase operating expenses.

[0011] (3) Some inhibitors may be incompatible with other chemicals or treatment agents, leading to a decrease in the overall efficiency of the system or the generation of unnecessary side reactions, such as precipitation or corrosion.

[0012] (4) The effectiveness of inhibitors is often affected by specific oil and gas field conditions (such as temperature, pressure, salt concentration, etc.). Some inhibitors may fail or be ineffective under extreme conditions and cannot provide long-term stable protection.

[0013] Therefore, when conducting research on salt crystallization inhibitors for oil and gas fields, multiple factors must be considered comprehensively, and we must not lose sight of the bigger picture for the sake of minor details. Summary of the Invention

[0014] In view of the problems existing in the above-mentioned salt crystallization inhibitors, the main purpose of this invention is to propose a solution to the problem of pipeline and equipment blockage caused by high-concentration salt crystallization in the petroleum and inorganic chemical industries. A salt crystallization inhibitor that is easy to synthesize has been developed, which has the advantages of simple formulation, convenient operation and low production cost.

[0015] This invention first provides a salt crystallization inhibitor, comprising the following components by mass: 1-2 parts by weight of sodium polyacrylate, 1-2 parts by weight of sodium citrate, 1-2 parts by weight of sodium tripolyphosphate, 1-2 parts by weight of octadecyltrimethylammonium chloride, 1-2 parts by weight of fatty alcohol polyoxyethylene ether, 3-4 parts by weight of ethylene glycol, 83-90 parts by weight of water, and a certain amount of sodium hydroxide to adjust the pH value to 8-10.

[0016] Sodium polyacrylate has a molecular weight between 2000 and 6000 g / mol.

[0017] Furthermore, the total mass ratio of the octadecyltrimethylammonium chloride and fatty alcohol polyoxyethylene ether to the mass ratio of sodium polyacrylate is 3-4:1.

[0018] Furthermore, the mass ratio of the octadecyltrimethylammonium chloride to the fatty alcohol polyoxyethylene ether is 1:1.

[0019] This invention also provides a method for preparing the above-mentioned salt crystallization inhibitor, which is carried out according to the following steps: Step 1: Prepare 1-2 parts by weight of sodium polyacrylate, 1-2 parts by weight of sodium citrate, 1-2 parts by weight of sodium tripolyphosphate, 1-2 parts by weight of octadecyltrimethylammonium chloride, 1-2 parts by weight of fatty alcohol polyoxyethylene ether, 3-4 parts by weight of ethylene glycol, 88-90 parts by weight of water, and a certain amount of sodium hydroxide.

[0020] Step 2: Mix the prepared sodium citrate, sodium tripolyphosphate, ethylene glycol, and water, and stir with a mixer for 5-10 minutes to ensure complete dissolution. After stabilization, add a certain amount of sodium hydroxide to maintain the pH of the solution between 8 and 10, obtaining solution A.

[0021] Step 3: Add octadecyltrimethylammonium chloride and fatty alcohol polyoxyethylene ether to solution A in sequence, and stir with a mixer for 5-10 minutes to fully dissolve them, to obtain solution B.

[0022] Step 4: After solution B stabilizes, continue stirring in the Wu Yin mixer, slowly pouring in sodium polyacrylate at a stirring speed of approximately 200–400 rad / min. After the solution is fully dissolved, pour it out and let it stand for 1–2 hours to obtain the desired microemulsion liquid salt crystallization inhibitor. It is important to note that the stirring speed of the Wu Yin mixer should not be too slow or too fast during this process. Too slow a stirring speed may result in insufficient dissolution of the sodium polyacrylate, while too fast a stirring speed may introduce air bubbles into the solution, affecting its stability. Simultaneously, while slowly adding the sodium polyacrylate, pay close attention to the amount added each time to ensure that the solid powder is not added in lumps to prevent the sodium polyacrylate from clumping in the solution.

[0023] The microemulsion salt crystallization inhibitor prepared according to the present invention was used to dissolve sodium chloride. The results showed that at room temperature of 20°C, adding 3-6% by volume of the salt crystallization inhibitor to an aqueous sodium chloride solution could increase the amount of sodium chloride dissolved from 36.5g per 100g of deionized water to 59.1g per 100g of water.

[0024] This invention innovatively incorporates agents such as sodium tripolyphosphate, octadecyltrimethylammonium chloride, and fatty alcohol polyoxyethylene ether. Sodium tripolyphosphate is a highly efficient complexing agent that can react with metal ions such as calcium and magnesium in water to form soluble complexes. This action reduces water hardness, thereby effectively inhibiting salt crystallization.

[0025] Octadecyltrimethylammonium chloride (OTAC) is a quaternary ammonium salt with antibacterial properties, preventing the growth of microorganisms that may exist in the oil well environment while maintaining solution stability. It is also a cationic surfactant, its molecular structure containing a long-chain alkyl group and a trimethylammonium cation. The long-chain alkyl group is hydrophobic, while the trimethylammonium cation is hydrophilic. This amphiphilic property allows OTC to adsorb onto crystal surfaces, forming a protective film that prevents further crystal growth and aggregation.

[0026] Fatty alcohol polyoxyethylene ethers, as surfactants, improve the fluidity and permeability of solutions, facilitating uniform distribution in oil wells and enhancing the inhibition effect. Their molecules contain hydrophilic oxyethylene groups that can form hydrogen bonds with water, thereby reducing the surface tension of water. By adsorbing onto crystal surfaces, they can alter the crystal growth morphology, thus slowing down or preventing further crystal growth. Furthermore, their addition increases the dispersibility of tiny crystal particles in the solution, preventing them from agglomerating into large deposits.

[0027] The addition of sodium hydroxide keeps the agent in an alkaline environment, enhancing the inhibitory effect on the polymer.

[0028] The addition of ethylene glycol can adjust the pH of the solution, keeping it within an appropriate range and preventing the formation of an acidic environment. An acidic environment promotes the dissolution of certain metal ions, increasing the risk of salt crystallization. By adjusting the pH, ethylene glycol can form complexes with certain metal ions, creating stable complexes. This complexation fixes the metal ions in the solution, reducing their free concentration and thus lowering the likelihood of salt crystallization. Simultaneously, the ethylene glycol molecule contains two hydroxyl groups, which are highly hydrophilic and can form hydrogen bonds with water, increasing the solution's humidity. This hydrophilicity helps inhibit the crystallization process of salts. Furthermore, the relatively high viscosity of ethylene glycol reduces the fluidity of the solution, thereby decreasing the migration and precipitation of salts. High-viscosity solutions reduce salt accumulation at the interface, further lowering the risk of salt crystallization.

[0029] The simultaneous addition of octadecyltrimethylammonium chloride and fatty alcohol polyoxyethylene ether achieves complementary effects of charge interaction and steric hindrance, as well as improved adaptability of the mixed micelles to complex environments. This compounding strategy significantly enhances the stability, salt resistance, and crystallization inhibition efficiency of the microemulsion. Furthermore, the addition of sodium tripolyphosphate effectively blocks scaling reactions and synergistically stabilizes the microcrystals with octadecyltrimethylammonium chloride and fatty alcohol polyoxyethylene ether.

[0030] The salt crystallization inhibitor provided by this invention has advantages such as simple formulation, convenient operation, and low production cost. Compared with traditional salt crystallization inhibitors, this invention can effectively inhibit the formation of salt crystals, thereby significantly reducing the risk of equipment failure and production stoppage caused by crystallization. The application of this inhibitor can not only improve the production efficiency of the petroleum and inorganic chemical industries, but also extend the service life of pipelines and equipment. Attached Figure Description

[0031] Figure 1 The diagram shows the state of solutions C (left) and D (right) after evaporation. Detailed Implementation

[0032] The present invention will be described in detail below with reference to the embodiments, but these should not be construed as limiting the scope of protection of the present invention. Example 1

[0033] A salt crystallization inhibitor is prepared according to the following steps: Prepare 1 part by weight of sodium polyacrylate, 1 part by weight of sodium citrate, 1 part by weight of sodium tripolyphosphate, 2 parts by weight of octadecyltrimethylammonium chloride, 2 parts by weight of fatty alcohol polyoxyethylene ether, 3 parts by weight of ethylene glycol, 90 parts by weight of water, and a certain amount of sodium hydroxide.

[0034] Dissolve 1 part by weight of sodium citrate, 1 part by weight of sodium tripolyphosphate, and 3 parts by weight of ethylene glycol in 90 parts by weight of water using a Wu Yin mixer. Add a certain amount of sodium hydroxide to adjust the pH of the solution to 8-10, obtaining solution A. Add 2 parts by weight of octadecyltrimethylammonium chloride and 2 parts by weight of fatty alcohol polyoxyethylene ether to this solution, and stir thoroughly to dissolve, obtaining solution B. Continue stirring solution B, add 2 parts by weight of sodium polyacrylate, and after it is fully dissolved, let it stand for 1-2 hours to obtain a microemulsion liquid salt crystallization inhibitor. Example 2

[0035] Dissolve 2 parts by weight of sodium citrate, 1 part by weight of sodium tripolyphosphate, and 4 parts by weight of ethylene glycol in 87 parts by weight of water using a Wu Yin mixer. Add a certain amount of sodium hydroxide to adjust the pH of the solution to 8-10, obtaining solution A. Add 2 parts by weight of octadecyltrimethylammonium chloride and 1 part by weight of fatty alcohol polyoxyethylene ether to the solution, and stir thoroughly to dissolve, obtaining solution B. Continue stirring solution B, add 1 part by weight of sodium polyacrylate, and after it is fully dissolved, let it stand for 1-2 hours to obtain a microemulsion liquid salt crystallization inhibitor. Example 3

[0036] Dissolve 2 parts by weight of sodium citrate, 2 parts by weight of sodium tripolyphosphate, and 4 parts by weight of ethylene glycol in 83 parts by weight of water using a Wu Yin mixer. Add a certain amount of sodium hydroxide to adjust the pH of the solution to 8-10, obtaining solution A. Add 2 parts by weight of octadecyltrimethylammonium chloride and 2 parts by weight of fatty alcohol polyoxyethylene ether to this solution, and stir thoroughly to dissolve, obtaining solution B. Continue stirring solution B, add 2 parts by weight of sodium polyacrylate, and after it is fully dissolved, let it stand for 1-2 hours to obtain a microemulsion liquid salt crystallization inhibitor. Comparative Example 1

[0037] The difference between this comparative example and Example 1 is that octadecyltrimethylammonium chloride was not added. Comparative Example 2

[0038] The difference between this comparative example and Example 1 is that fatty alcohol polyoxyethylene ether was not added. Comparative Example 3

[0039] Dissolve 1 part by weight of sodium citrate, 1 part by weight of sodium tripolyphosphate, and 3 parts by weight of ethylene glycol in 90 parts by weight of water using a Wu Yin mixer. Add a certain amount of sodium hydroxide to adjust the pH of the solution to 8-10, obtaining solution A. Add 3 parts by weight of octadecyltrimethylammonium chloride and 1 part by weight of fatty alcohol polyoxyethylene ether to the solution, and stir thoroughly to dissolve, obtaining solution B. Continue stirring solution B, add 2 parts by weight of sodium polyacrylate, and after it is fully dissolved, let it stand for 1-2 hours to obtain a microemulsion liquid salt crystallization inhibitor.

[0040] The salt crystallization inhibition performance of Examples 1-3 and Comparative Examples 1-3 was tested, and the test method is as follows: Measure 200 mL of deionized water into a beaker, add 73 g of sodium chloride, place the beaker in a water bath, and heat while stirring until the sodium chloride is fully dissolved. Repeat the operation twice to obtain solution C and solution D. Measure 4 g of the salt crystallization inhibitor prepared above and add it to solution C, and stir well. After the solution evaporates to 100 mL, remove the beaker. Filter and weigh both solutions, and calculate the salt crystallization inhibition rate. The results are shown in Table 1.

[0041]

[0042] Where m2 is the mass of sodium chloride obtained after filtering solution D, in g; and m1 is the mass of sodium chloride obtained after filtering solution C, in g.

[0043] Figure 1 This is a comparison chart showing the effects of the salt crystallization inhibitor prepared in Example 1. It is clearly visible from the chart that after adding the salt crystallization inhibitor, the amount of sodium chloride in the solution is significantly reduced, and the crystal particles are also significantly smaller.

[0044] Table 1 Salt crystallization inhibition rate project Salt crystallization inhibition rate % Example 1 61.9 Example 2 58.1 Example 3 56.5 Comparative Example 1 57.3 Comparative Example 2 58.8 Comparative Example 3 59.8 In this invention, Example 1 showed the best application effect. Specifically, in Comparative Example 1, octadecyltrimethylammonium chloride was removed from the salt crystallization inhibitor formulation, and a salt crystallization inhibition experiment was conducted. The experiment revealed that the amount of salt crystals precipitated from the sample solution increased, and the particle size significantly increased, exhibiting aggregation. In Comparative Example 2, fatty alcohol polyoxyethylene ether was removed from the salt crystallization inhibitor formulation, and a salt crystallization inhibition experiment was conducted. The experiment revealed that the amount of salt crystals precipitated from the sample solution increased. In Comparative Example 3, the ratio of octadecyltrimethylammonium chloride and fatty alcohol polyoxyethylene ether was changed, and a salt crystallization inhibition experiment was conducted. The experiment revealed that changing the ratio did not improve the salt crystallization inhibition rate; in fact, it decreased it, indicating that the ratio in Example 1 achieved a relatively good effect.

[0045] This invention innovatively proposes a salt crystallization inhibitor formulation of sodium tripolyphosphate, octadecyltrimethylammonium chloride, fatty alcohol polyoxyethylene ether, and other agents with sodium polyacrylate, which greatly improves the salt crystallization inhibition effect of organic compounds such as polyacrylic acid derivatives.

[0046] The above description is only a preferred embodiment of the present invention. It should be noted that for those skilled in the art, several improvements and modifications can be made without departing from the principle of the present invention, and these improvements and modifications should also be considered within the scope of protection of the present invention.

Claims

1. A salt crystallization inhibitor, characterized in that, The salt comprises the following components by weight: 1-2 parts sodium polyacrylate, 1-2 parts sodium citrate, 1-2 parts sodium tripolyphosphate, 1-2 parts octadecyltrimethylammonium chloride, 1-2 parts fatty alcohol polyoxyethylene ether, 3-4 parts ethylene glycol, and 83-90 parts water; the pH value of the salt crystallization inhibitor is 8-10.

2. The salt crystallization inhibitor according to claim 1, characterized in that, The total mass ratio of the octadecyltrimethylammonium chloride and fatty alcohol polyoxyethylene ether to sodium polyacrylate is 3-4:

1.

3. The salt crystallization inhibitor according to claim 1, characterized in that, The mass ratio of the octadecyltrimethylammonium chloride to the fatty alcohol polyoxyethylene ether is 1:

1.

4. The method for preparing the salt crystallization inhibitor according to any one of claims 1-3, characterized in that, Includes the following steps: (1) Dissolve sodium citrate, sodium tripolyphosphate, and ethylene glycol in water, and adjust the pH of the solution to between 8 and 10 to obtain solution A; (2) Add octadecyltrimethylammonium chloride and fatty alcohol polyoxyethylene ether to solution A in sequence, mix well, and obtain solution B; (3) Under stirring conditions, sodium polyacrylate is added in batches. After it is fully dissolved, it is allowed to stand for 1-2 hours to obtain a microemulsion salt crystallization inhibitor.

5. The method for preparing the salt crystallization inhibitor according to claim 4, characterized in that, In step (4), the stirring speed is controlled at 200-400 rad / min.

6. The use of the salt crystallization inhibitor according to any one of claims 1-3 in preventing sodium chloride crystallization.

7. The application according to claim 6, characterized in that, The volume percentage of the added salt crystallization inhibitor is 3-6%.