A preheating and soldering apparatus and method for ceramic electronic components
By combining a preheating box, protective cover, support and clamping components, and a drive soldering component, the problem of heat loss and temperature control in the soldering of ceramic electronic components is solved. This achieves segmented precise temperature control and solder paste protection, thereby improving soldering quality and reliability.
Patent Information
- Application Number
- CN202611215560.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-12
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2046-08-12
AI Technical Summary
In the soldering process of ceramic electronic components, existing technologies cannot effectively isolate the external environment, resulting in large heat loss and the inability to achieve differentiated preheating temperature control, which affects the soldering quality and reliability.
The system employs a combination structure consisting of a preheating chamber, a protective cover, a support and clamping assembly, and a drive solder melting assembly to form a two-stage sealed heating chamber and a sealed inner cavity. This allows for segmented and precise temperature control preheating of ceramic electronic components and solder pads, while the sealed inner cavity isolates external air to prevent solder paste oxidation.
It achieves segmented and precise temperature control and preheating of ceramic electronic components and pads, reduces heat loss, avoids electrode oxidation or substrate cracking, ensures the wettability and fluidity of solder paste, and improves soldering quality.
Smart Images

Figure CN122746546B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of preheating solder melting technology, and more particularly to a preheating solder melting device and method for ceramic electronic components. Background Technology
[0002] Currently, in the soldering process of ceramic electronic components, it is usually necessary to solder the ceramic electronic components onto the solder pad (PCB). However, since ceramic electronic components are sensitive to temperature changes, if they are not preheated sufficiently before soldering, the thermal shock at the moment of soldering can easily cause the ceramic electronic components to crack or develop microcracks, affecting the reliability and service life of the ceramic electronic components.
[0003] Therefore, ceramic electronic components are typically preheated before soldering. However, current preheating and soldering processes are usually conducted in open or semi-open environments, resulting in significant heat loss and making it impossible to differentiate the preheating temperature control for ceramic electronic components and solder pads. This leads to the following problems: 1) Ceramic electronic components and solder pads require different preheating temperatures, but currently, a single heating mode with the same preheating temperature is used for both, which cannot simultaneously meet the low-temperature preheating protection requirements of ceramic electronic components and the sufficient high-temperature preheating requirements of solder pads. In other words, excessively high preheating temperatures can cause electrode oxidation or thermal stress cracking of the ceramic electronic components, while insufficient preheating can lead to inadequate flux activation and moisture residue on the solder pads, affecting subsequent soldering efficiency. 2) Because current preheating and soldering processes are usually conducted in open or semi-open environments, it is impossible to effectively isolate the air in the external environment, causing the solder paste to oxidize easily during heating, affecting the wettability and flowability of the solder paste, and reducing the final soldering quality. Summary of the Invention
[0004] The purpose of this invention is to provide a preheating solder melting device and method for ceramic electronic components, which can reasonably preheat according to the large temperature resistance difference between the ceramic electronic components and the solder pads, realize segmented and precise temperature control preheating in two stages, and prevent the solder paste from oxidizing during the heating process, which is beneficial to improving the soldering quality.
[0005] To achieve this objective, the present invention adopts the following technical solution: A preheating and soldering device for ceramic electronic components, comprising: Preheating box; A protective cover is installed on top of the preheating box; A sealing baffle is slidably connected to the preheating box along the X-axis. The protective cover is provided with a sealing baffle on each of its opposite sides along the X-axis. When the two sealing baffles slide close together along the X-axis, a sealed heating cavity is formed between the preheating box, the protective cover and the two sealing baffles. A support clamping assembly is slidably connected to the preheating box along the X-axis and spaced below the protective cover. The support clamping assembly is used to support and clamp the solder pads, and the support clamping assembly is provided with a heating element for heating the sealed heating chamber. A solder melting assembly is provided, with its fixed end connected to the top of the protective cover. The output end of the solder melting assembly passes through the protective cover downward along the Z-axis and is placed inside the sealed heating cavity. Ceramic electronic components are pre-positioned in the internal cavity of the output end of the solder melting assembly and located above the pads before the output end of the solder melting assembly moves downward along the Z-axis. The output end of the solder melting assembly can move downward along the Z-axis to seal against the pads, thereby forming a local sealed inner cavity within the sealed heating cavity. The sealed inner cavity is a local space formed by the internal cavity and the pads. When the heating element heats the temperature inside the sealed heating cavity to the first preheating temperature of the ceramic electronic component, the output end of the drive solder melting assembly moves downward along the Z-axis to seal and adhere to the pad on the support clamping assembly to form a sealed inner cavity; then the heating element continues to heat the sealed heating cavity until the temperature inside reaches the second preheating temperature of the pad, and the second preheating temperature is higher than the first preheating temperature.
[0006] As an optional solution, a first screw is connected to the outer side of the sealing baffle facing the protective cover; the preheating box includes: The base plate and two side plates are provided. The base plate is horizontally connected between the two side plates. Each of the two side plates has a first sliding groove extending along the X-axis. The first screw slides through the first sliding groove along the X-axis, and the end of the first screw that extends out of the first sliding groove is threaded with a first locking ring. A fixing plate is provided with two fixing plates spaced apart from each other along the X-axis. The fixing plates are positioned between the two side plates. The bottom end of the fixing plate is connected to the base plate. The top end of the fixing plate is connected to a sealing element. The bottom end face of the sealing baffle can contact the sealing element.
[0007] As an optional solution, a first threaded shaft is rotatably connected between the two fixed plates about the X-axis; the support and clamping assembly includes: A slide block is threadedly fitted onto the first threaded shaft, and rotation of the first threaded shaft can drive the slide block to move along the X-axis on the first threaded shaft; A fixed base is slidably connected to the slide block along the Y-axis, and the heating element is mounted on the fixed base; A placement rack is installed on the fixed base. The placement rack has a through hole extending along its thickness direction. The heating element is arranged corresponding to the through hole. The placement rack is connected to two first clamping strips that are arranged at intervals along the X-axis. Both first clamping strips are arranged along the X-axis toward the heating element. The limiting plate is slidably connected to the placement frame along the Z-axis. The two limiting plates are arranged at intervals relative to each other along the X-axis. A second clamping strip is connected to one side of the limiting plate, and one second clamping strip is positioned directly above one of the first clamping strips at intervals. The limiting plate moves downward along the Z-axis to drive the second clamping strip to move downward along the Z-axis to abut against the pads placed on the two first clamping strips, so as to limit and press the pads between the first clamping strips and the corresponding second clamping strips.
[0008] As an optional solution, the support clamping assembly further includes: The second screw extends along the Z-axis, and the bottom end of the second screw rotates around the Z-axis and is axially fixedly connected to the placement frame. The limiting plate is threaded onto the second screw along the Z-axis. The second locking screw ring is threaded onto the top of the second screw that extends upward along the Z-axis to the outside of the limiting plate. Rotating the second screw can cause the limiting plate to move downward along the Z-axis on the second screw. The second locking screw ring is used to lock the limiting plate and the second screw.
[0009] As an optional solution, the support clamping assembly further includes: The second threaded shaft is rotatably connected to the slide block about the Y-axis, and the slide block has a guide groove extending along the Y-axis. The first driving member has its fixed end connected to an outer side of the slide block, and its output end is coaxially connected to the second threaded shaft. The guide block is connected to the bottom end of the fixed base. The guide block is threaded onto the second threaded shaft and can slide along the Y-axis in the guide groove.
[0010] As an optional solution, the driving solder melting component includes: The second driving component has its fixed end installed on the top of the protective cover; A telescopic rod, one end of which is connected to the output end of the second driving component; A fixed rod is provided, with the other end of the telescopic rod connected to the fixed rod, and the fixed rod is located inside the preheating box. Soldering iron tip, the bottom end of the fixing rod is connected to the soldering iron tip; A ceramic cylinder with its opening facing downwards is provided. The ceramic cylinder is sleeved on the fixing rod, and a sealing ring is sleeved at the bottom end of the ceramic cylinder. The second driving member can drive the ceramic cylinder to move downwards along the Z-axis, so as to move the sealing ring to seal against the solder pad to form the sealed inner cavity. The third screw has its bottom end passing downward along the Z-axis through the ceramic cylinder. The third screw is threadedly connected to the ceramic cylinder. The bottom end of the third screw, which passes through the ceramic cylinder, is equipped with a suction cup for adsorbing the ceramic electronic component. The ceramic electronic component is located directly below the soldering iron tip.
[0011] As an optional feature, the outer wall of the fixing rod is provided with a second sliding groove extending along the Z-axis; the driving solder melting assembly further includes: A slider is disposed inside the top plate of the ceramic cylinder, and the slider can slide along the Z-axis within the second groove; A sliding column extends along the Z-axis and is installed in the second sliding groove; An elastic element is sleeved on the sliding column, and both ends of the elastic element are respectively connected to the slider and the inner top wall of the second sliding groove; As the slider slides upward along the Z-axis within the second groove, the elastic element is compressed, and the soldering iron tip moves downward along the Z-axis to press the pins of the ceramic electronic component into the solder paste on the pad.
[0012] As an optional solution, the preheating and soldering device for the ceramic electronic components further includes: A flue gas suction and filtration assembly is installed on the telescopic rod and the fixed rod. The flue gas suction and filtration assembly is connected to the sealed inner cavity. The flue gas suction and filtration assembly is used to suck in the flue gas generated in the sealed inner cavity and purify the flue gas layer by layer.
[0013] Alternatively, the fixing rod is provided with a through groove extending radially therethrough; the flue gas extraction and filtration assembly includes: A suction pump, which is installed in the through groove; The first suction tube has one end connected to the inlet end of the suction pump and the other end extending downward along the Z-axis into the ceramic cylinder. The suction pump can draw the smoke generated in the sealed inner cavity into the first suction tube. The second suction tube has one end connected to the outlet end of the suction pump and the other end connected to a purification cylinder, which is sleeved on the telescopic rod and the fixed rod. The purification component is installed inside the purification cylinder and sleeved on the telescopic rod and the fixed rod. The purification component is used to purify the flue gas layer by layer.
[0014] A method for preheating and soldering ceramic electronic components, based on the preheating and soldering apparatus for ceramic electronic components as described above, includes the following steps: S1: Apply solder paste to the pad and place the pad on the support clamping assembly, so that the support clamping assembly supports and fixes the pad; S2: The ceramic electronic component is positioned above the pad, with its pins facing the solder paste on the pad. Two sealing baffles are moved along the X-axis, forming a sealed heating cavity by the preheating chamber, the protective cover, and the two sealing baffles. The heating element heats the sealed heating cavity. When the temperature inside the sealed heating cavity reaches the first preheating temperature of the ceramic electronic component, the output end of the driving solder melting assembly moves downwards along the Z-axis to seal against the pad, forming the sealed inner cavity to preheat the ceramic electronic component. The temperature continues to rise until the temperature inside the sealed heating cavity reaches the second preheating temperature of the pad, thus preheating the pad. S3: Reheat to melt the solder paste and press the pins of the ceramic electronic component into the solder paste to solder the ceramic electronic component to the pad in the sealed cavity, and open the two sealing baffles along the X-axis for heat dissipation and cooling.
[0015] The beneficial effects of this invention are: The preheating and solder melting device for ceramic electronic components of the present invention comprises a preheating box, a protective cover, a support and clamping assembly, and a driving solder melting assembly that cooperate with each other. When the heating element heats the temperature inside the sealed heating cavity formed by the preheating box, the protective cover, and two sealing baffles to the first preheating temperature of the ceramic electronic component, the output end of the driving solder melting assembly moves downward along the Z-axis to a solder pad sealed against the support and clamping assembly to form a sealed inner cavity. The heating element then continues to heat the sealed heating cavity until the temperature inside reaches the second preheating temperature of the solder pad, and the second preheating temperature is higher than the first preheating temperature. The above-mentioned structure and preheating method have the following effects: 1) The sealed heating cavity is formed by sliding the sealing baffles ( The two-stage sealing structure—the overall preheating environment and the output end of the driving solder melting component pressed down to form a local sealed cavity (soldering protection space)—allows the preheating and soldering stages to be carried out in suitable sealed environments. In other words, the sealed heating cavity provides the overall preheating environment, reducing heat loss, concentrating heat, and minimizing heat radiation and convection losses to the external environment. During the initial common heating stage of preheating, heat sharing is utilized to quickly and synchronously raise the temperature of the ceramic electronic components and solder pads from room temperature, significantly shortening the overall basic preheating time. When the temperature inside the sealed heating cavity reaches the first preheating temperature of the ceramic electronic components, the output end of the driving solder melting component moves downward along the Z-axis to seal and adhere to the solder pads, forming a sealed cavity. To effectively isolate the external air, the heating mode shifts to a pad-based heating mode. At this point, the pads can be flexibly heated to the required second preheating temperature. This is because the wall thermal resistance (solid thermal resistance) and convection thermal resistance (air thermal resistance) of the sealed cavity are directly utilized. During the continued heating of the sealed cavity to the second preheating temperature, the rate of heat transfer into the sealed cavity is slowed, ensuring that the temperature of the ceramic electronic components within the sealed cavity rises only slowly. This avoids electrode oxidation or substrate cracking caused by rapid heating or prolonged exposure to high temperatures. The above-mentioned reasonable preheating based on the significant temperature resistance difference between the ceramic electronic components and the pads achieves segmented and precise temperature control preheating in two stages. It not only meets the high-temperature preheating requirements for removing moisture from the solder pads and activating the flux (insufficient preheating will lead to incomplete flux activation and residual moisture, affecting subsequent soldering efficiency), but also avoids the problems of electrode oxidation or substrate thermal stress cracking caused by ceramic electronic components being in a high-temperature preheating environment for a long time (overheating). The sealed inner cavity provides local isolation protection during both the preheating and soldering stages, effectively reducing heat loss in the soldering area (located in the sealed inner cavity). This allows the two-stage sealing structure (sealed heating cavity + sealed inner cavity) to ensure thermal efficiency during the preheating stage while also providing a precise local heating environment for the soldering stage, avoiding energy waste caused by the entire sealed heating cavity operating at a continuous high temperature.2) After reaching the first preheating temperature within the sealed heating chamber, a local sealed inner cavity is formed between the internal cavity of the output end of the driving solder melting component and the solder pad. Since this sealed inner cavity is located within the sealed heating chamber, and both the ceramic electronic components and the solder paste on the solder pads are located within this sealed inner cavity, air from the external environment can be effectively isolated through this sealed inner cavity. This prevents the solder paste from oxidizing during heating, ensures the wettability and fluidity of the solder paste, and is beneficial for improving soldering quality.
[0016] The preheating and soldering method for ceramic electronic components of the present invention, based on the aforementioned preheating and soldering device for ceramic electronic components, can reasonably preheat according to the large temperature resistance difference between the ceramic electronic components and the solder pads, achieving segmented and precise temperature control preheating in two stages. This not only meets the high-temperature preheating requirements for removing moisture from the solder pads and activating the flux (insufficient preheating will lead to inadequate flux activation and residual moisture, affecting subsequent soldering efficiency), but also directly utilizes the wall thermal resistance (solid thermal resistance) and convection thermal resistance (air thermal resistance) of the sealed inner cavity to slow down the rate of heat transfer into the sealed inner cavity. This avoids the problem of electrode oxidation or substrate thermal stress cracking caused by the ceramic electronic components being in a high-temperature preheating environment for a long time (overheating). Furthermore, it can prevent the solder paste from oxidizing during the heating process, ensuring the wettability and fluidity of the solder paste, which is beneficial to improving the soldering quality. Attached Figure Description
[0017] Figure 1 This is a schematic diagram of the preheating and solder melting device for ceramic electronic components provided by the present invention (with a sliding sealing baffle to form a sealed heating chamber). Figure 1 ; Figure 2 This is a schematic diagram of the preheating and solder melting device for ceramic electronic components provided by the present invention (with the sealing baffle not sliding to form a sealed heating chamber). Figure 2 ; Figure 3 This is a schematic diagram of the preheating and solder melting device for ceramic electronic components provided by the present invention (excluding the two sealing baffles). Figure 3 ; Figure 4 This is a schematic diagram of the structure of the support and clamping assembly provided by the present invention; Figure 5 This is a partially exploded structural diagram of the support and clamping assembly provided by the present invention; Figure 6 yes Figure 5 A magnified schematic diagram of the partial structure at point A in the middle; Figure 7 This is a schematic diagram of the assembly structure of the driving solder melting component and the flue gas extraction and filtration component provided by the present invention. Figure 8This is a schematic diagram of the structure of the drive solder melting component and the flue gas extraction and filtration component provided by the present invention before they are assembled. Figure 9 yes Figure 8 A magnified schematic diagram of the local structure at point B; Figure 10 This is a partially exploded structural diagram of the molten solder driving assembly provided by the present invention; Figure 11 This is a schematic diagram of the internal structure of the ceramic cylinder provided by the present invention; Figure 12 This is a schematic diagram of the structure of the flue gas extraction and filtration assembly (the purification component is not installed inside the purification cylinder) provided by the present invention; Figure 13 This is a schematic diagram of the main process of the preheating and soldering method for ceramic electronic components provided by the present invention.
[0018] In the picture: 1. Preheating box; 11. Base plate; 12. Side plate; 121. First slide groove; 13. Fixing plate; 131. Sealing element; 132. First threaded shaft; 2. Protective cover; 3. Sealing baffle; 31. First screw; 32. First locking ring; 33. Horizontal plate; 34. Vertical plate; 341. Step surface; 4. Support clamping assembly; 40. Heating element; 41. Slide; 411. Guide groove; 42. Fixing base; 421. First plate; 422. Second plate; 43. Placement rack; 431. Through hole; 432. First clamping bar; 433. Square frame; 434. Supporting vertical plate; 4341. Second guide shaft; 44. Limiting plate; 441. Second clamping bar; 45. Second screw; 46. Second locking screw ring; 47. Second threaded shaft; 48. First driving component; 491. Guide block; 492. Drive motor; 493. First guide shaft; 5. Drive solder melting assembly; 51. Second drive component; 511. Telescopic rod; 52. Fixed rod; 521. Second slide groove; 522. Through groove; 53. Soldering tip; 54. Ceramic cylinder; 55. Sealing ring; 56. Third screw; 561. Suction cup; 57. Slider; 58. Sliding column; 59. Elastic component; 6. Seal the heating chamber; 7. Seal the inner cavity; 8. Flue gas extraction and filtration assembly; 81. Suction pump; 82. First suction pipe; 83. Second suction pipe; 84. Purification cylinder; 85. Purification components; 91. Control panel; 92. First temperature sensor; 93. Second temperature sensor. Detailed Implementation
[0019] Embodiments of the present invention are described in detail below. Examples of these embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals denote the same or similar components or components having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and intended to explain the present invention, and should not be construed as limiting the present invention.
[0020] In the description of this invention, unless otherwise explicitly specified and limited, the terms "connected," "linked," and "fixed" should be interpreted broadly. For example, they can refer to a fixed connection or a detachable connection; a mechanical connection or an electrical connection; a direct connection or an indirect connection through an intermediate medium; or the internal communication of two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.
[0021] In the description of this invention, unless otherwise expressly specified and limited, "above" or "below" the second feature can include direct contact between the first and second features, or contact between the first and second features through another feature between them. Furthermore, "above," "over," and "on top" of the second feature includes the first feature being directly above or diagonally above the second feature, or simply indicates that the first feature is at a higher horizontal level than the second feature. "Below," "below," and "under" the second feature includes the first feature being directly below or diagonally below the second feature, or simply indicates that the first feature is at a lower horizontal level than the second feature.
[0022] The technical solution of the present invention will be further described below with reference to the accompanying drawings and specific embodiments.
[0023] Example 1
[0024] This embodiment provides a preheating and soldering device for ceramic electronic components. It preheats and solders the ceramic electronic components and pads in stages to ensure a good soldering effect between them. This achieves high-quality soldering between the leads of the ceramic electronic components and the pads, while preventing damage to the ceramic electronic components and ensuring high soldering yield and reliability. In this embodiment, the ceramic electronic component is a common leaded ceramic electronic component, and the pad is a common PCB pad.
[0025] Specifically, such as Figures 1 to 11As shown, the preheating and solder melting device for ceramic electronic components includes a preheating chamber 1, a protective cover 2, a sealing baffle 3, a support and clamping assembly 4, and a driving solder melting assembly 5. The protective cover 2 covers the top of the preheating chamber 1. The sealing baffle 3 is slidably connected to the preheating chamber 1 along the X-axis. A sealing baffle 3 is provided on each opposite side of the protective cover 2 along the X-axis. When the two sealing baffles 3 slide close together along the X-axis, the preheating chamber 1, the protective cover 2, and the two sealing baffles 3 form a sealed heating cavity 6. The support and clamping assembly 4 is slidably connected to the preheating chamber 1 along the X-axis and is positioned below the protective cover 2. The support and clamping assembly 4 supports and clamps the solder pads, and a heating element 40 for heating the sealed heating cavity 6 is provided on the support and clamping assembly 4. The fixed end of the driving solder melting assembly 5 is connected to the top of the protective cover 2, and the output end of the driving solder melting assembly 5 passes downward along the Z-axis through the protective cover 2. The cover 2 is placed inside the sealed heating chamber 6. Before the output end of the driving solder melting assembly 5 moves downward along the Z-axis, the ceramic electronic component is pre-positioned in the internal cavity of the output end of the driving solder melting assembly 5 and located above the solder pad. The output end of the driving solder melting assembly 5 can move downward along the Z-axis to seal and adhere to the solder pad, thereby forming a partial sealed inner cavity 7 within the sealed heating chamber 6. The sealed inner cavity 7 is a local space formed by the internal cavity and the solder pad. Furthermore, when the heating element 40 heats the temperature inside the sealed heating chamber 6 to the first preheating temperature of the ceramic electronic component, the output end of the driving solder melting assembly 5 moves downward along the Z-axis to seal and adhere to the solder pad on the support clamping assembly 4 to form the sealed inner cavity 7. Then, the heating element 40 continues to heat the sealed heating chamber 6 until the temperature inside reaches the second preheating temperature of the solder pad, and the second preheating temperature is higher than the first preheating temperature. In this embodiment, the protective cover 2 can specifically be an outer casing with the opening facing downward.
[0026] The preheating and solder melting device for ceramic electronic components in this embodiment differs from existing technologies in its specific preheating implementation for both the ceramic electronic components and the solder pads. It comprises a preheating chamber 1, a protective cover 2, a support and clamping assembly 4, and a driving solder melting assembly 5 that work in concert. When the heating element 40 heats the temperature within the sealed heating cavity 6, formed by the preheating chamber 1, the protective cover 2, and the two sealing baffles 3, to the first preheating temperature of the ceramic electronic components, the output end of the driving solder melting assembly 5 moves downwards along the Z-axis to seal and adhere to the solder pads on the support and clamping assembly 4, forming a sealed inner cavity 7. The heating element 40 then continues to heat the sealed heating cavity 6 further into its inner cavity. The temperature reaches the second preheating temperature of the solder pad, and the second preheating temperature is higher than the first preheating temperature; the above-mentioned structure and preheating method have the following effects: 1) The two-stage sealing structure, formed by the sliding of the sealing baffle 3 to form a sealed heating cavity 6 (overall preheating environment) and the downward pressing of the output end of the driving solder melting component 5 to form a local sealed inner cavity 7 (soldering protection space), allows the preheating and soldering stages to be carried out in suitable sealed environments respectively; that is, the sealed heating cavity 6 provides an overall preheating environment, reduces heat loss, achieves heat concentration, reduces heat radiation and convection loss to the external environment, and utilizes heat sharing to quickly heat up the initial preheating stage. Simultaneous heating of the ceramic electronic components and solder pads from room temperature significantly shortens the overall preheating time. When the temperature inside the sealed heating cavity 6 reaches the first preheating temperature of the ceramic electronic components, the output end of the driving solder melting assembly 5 moves downward along the Z-axis to seal and adhere to the solder pads, forming a sealed inner cavity 7 to effectively isolate air from the external environment. The system then switches to a heating mode primarily focused on the solder pads. At this point, the solder pads can be flexibly heated to the required second preheating temperature because the wall thermal resistance (solid thermal resistance) and convection thermal resistance (air thermal resistance) of the sealed inner cavity 7 are directly utilized. This delays heat transfer into the sealed inner cavity 7 as the sealed heating cavity 6 continues to heat to the second preheating temperature. The rate of temperature increase ensures that the temperature of the ceramic electronic components located in the sealed inner cavity 7 rises only slowly, avoiding electrode oxidation or substrate cracking caused by rapid heating or prolonged exposure to high temperatures. The above-mentioned reasonable preheating based on the significant temperature resistance difference between the ceramic electronic components and the pads achieves segmented and precise temperature control preheating in two stages. This not only meets the high-temperature preheating requirements for removing moisture from the pads and activating the flux (insufficient preheating will lead to inadequate flux activation and moisture residue, affecting subsequent soldering efficiency), but also avoids the problem of electrode oxidation or substrate thermal stress cracking caused by prolonged exposure to high-temperature preheating (overheating) of the ceramic electronic components.The sealed inner cavity 7 provides localized isolation protection during both the preheating and soldering stages, effectively reducing heat loss in the soldering area (located within the sealed inner cavity 7). This allows the two-stage sealing structure (sealed heating cavity 6 + sealed inner cavity 7) to ensure thermal efficiency during the preheating stage while also providing a precise localized heating environment for the soldering stage, avoiding energy waste caused by the entire sealed heating cavity 6 operating at continuous high temperatures. 2) After reaching the first preheating temperature within the sealed heating cavity 6, a localized sealed inner cavity 7 is formed between the internal cavity of the output end of the driving solder melting component 5 and the solder pad. Since this sealed inner cavity 7 is located within the sealed heating cavity 6, and both the ceramic electronic components and the solder paste on the solder pads are located within this sealed inner cavity 7, it effectively isolates the solder paste from the external environment, preventing oxidation during heating, ensuring the wettability and fluidity of the solder paste, and improving soldering quality.
[0027] In this embodiment, the first preheating temperature of the ceramic electronic component can be 80℃~150℃, preferably 100℃~120℃; the second preheating temperature of the solder pad can be 150℃~190℃, preferably 160℃~180℃. It is understood that the first preheating temperature should be lower than the melting point of the solder alloy in the solder paste, and the second preheating temperature should be lower than the melting point of the solder alloy but higher than the first preheating temperature. In one specific embodiment, the first preheating temperature is specifically 110℃, the second preheating temperature is specifically 175℃, and the melting point of the solder alloy is specifically 183℃.
[0028] The following is a detailed description of preheating box 1: Specifically, such as Figures 1 to 3 As shown, a first screw 31 is connected to the outer side of the sealing baffle 3 facing the protective cover 2; the preheating box 1 includes a base plate 11, two side plates 12, and two fixing plates 13; wherein, the base plate 11 is horizontally connected between the two side plates 12 to form an H-shaped structure, and the two side plates 12 are respectively provided with a first sliding groove 121 extending along the X-axis, the first screw 31 slides through the first sliding groove 121 along the X-axis, and the end of the first screw 31 that extends out of the first sliding groove 121 is threadedly connected to a first locking screw ring 32; two fixing plates 13 are provided at intervals along the X-axis, the fixing plates 13 are positioned between the two side plates 12, the bottom end of the fixing plate 13 is connected to the base plate 11, and the top end of the fixing plate 13 is connected to a sealing element 131, and the bottom end face of the sealing baffle 3 can contact the sealing element 131 to seal the preheating box 1. A control panel 91 for overall control is installed on the outer side of one of the side plates 12. In this embodiment, the sealing element 131 can be a sealing strip; and a first screw 31 is symmetrically connected to two opposite outer sides of each sealing baffle 3 along the Y-axis, and a first screw 31 is correspondingly slidably inserted into a first groove 121 along the X-axis; the control panel 91 is a common control panel 91 structure in the prior art.
[0029] Specifically, when it is necessary to enclose and form a sealed heating chamber 6, first loosen the first locking ring 32, and then move the two sealing baffles 3 along the X-axis and towards the protective cover 2 respectively. At this time, a first screw 31 slides along the X-axis in a first groove 121 to provide sliding guidance and stability for the sealing baffle 3. Then, when the first screw 31 slides to the inner end wall of the first groove 121, the first screw 31 can no longer slide along the X-axis toward the protective cover 2. At this time, if Figure 1 As shown, the first screw 31 is located at the bottom end of the protective cover 2, and one end of the sealing baffle 3 extends into the bottom end of the protective cover 2 to ensure a good sealing effect between the protective cover 2, the sealing baffle 3, and the two side plates 12. At the same time, the other end of the sealing baffle 3 presses against the sealing element 131 to ensure a good sealing effect between the sealing baffle 3, the fixing plate 13, and the two side plates 12. Furthermore, when the other end of the sealing baffle 3 presses against the sealing element 131, the outer surface of the sealing baffle 3 is flush with the outer surface of the fixing plate 13 to ensure a neat and aesthetically pleasing overall structure. Finally, the first locking ring 32 is tightened to lock the first screw 31 and the corresponding side plate 12, thereby ensuring the stability of the sealing baffle 3.
[0030] The sealing baffle 3 is described in detail below: Furthermore, such as Figure 1 and Figure 3 As shown, the sealing baffle 3 has an L-shaped structure. Specifically, the sealing baffle 3 includes a horizontal plate 33 and a vertical plate 34 that are bent and connected in an arc. The horizontal plate 33 is horizontally abutted between the two side plates 12 and can extend into the bottom of the protective cover 2. A first screw 31 is symmetrically connected to the two opposite outer sides of the horizontal plate 33 along the Y-axis. The bottom end of the vertical plate 34 is provided with a stepped surface 341, and the sealing element 131 protrudes upward along the Z-axis relative to the top end of the fixed plate 13 to form a stepped structure. When the sealing baffle 3 is moved so that the bottom end of the vertical plate 34 abuts against the top end of the fixed plate 13, the stepped surface 341 abuts against the sealing element 131. The vertical plate 34 is positioned between the two side plates 12. This not only ensures a better seal between the fixed plate 13 and the sealing baffle 3, but also makes the overall structure of the sealing baffle 3 and the fixed plate 13 neat and aesthetically pleasing. Furthermore, when the vertical plate 34 moves to abut against the sealing member 131, the sealing member 131 provides abutment limit for the vertical plate 34, preventing it from moving further along the X-axis. Simultaneously, the inner end wall of the first sliding groove 121 abuts against and limits the first screw 31, thus accurately determining that the sealing baffle 3 has moved into position. In this embodiment, the horizontal plate 33 and the vertical plate 34 can be a single integrated structure.
[0031] The following is a detailed description of the support and clamping assembly 4: Specifically, such as Figures 1 to 4 As shown, a first threaded shaft 132 is rotatably connected between two fixed plates 13 around the X-axis; the support and clamping assembly 4 includes a drive motor 492, a slide 41, a fixed base 42, a placement frame 43, and a limiting plate 44; wherein, the fixed end of the drive motor 492 is installed on the outer side of one of the fixed plates 13, and the output end of the drive motor 492 is coaxially connected to the first threaded shaft 132, and the drive motor 492 is used to drive the first threaded shaft 132 to rotate around the X-axis; the slide 41 is threaded onto the first threaded shaft 132, and the rotation of the first threaded shaft 132 can drive the slide 41 to move along the X-axis on the first threaded shaft 132; the fixed base 42 is slidably connected to the slide 41 along the Y-axis, and the heating element 40 is installed on the fixed base 42; the placement frame 43 is installed on the fixed base 42, and the placement frame 43 has a through hole 431 extending along its thickness direction, and the heating element 40 corresponds to the through hole. The 431 is configured so that the heating element 40 can directly heat the pads located above it; the placement frame 43 is connected to two first clamping strips 432 arranged at intervals along the X-axis, and both first clamping strips 432 are arranged towards the heating element 40 along the X-axis; the placement frame 43 is slidably connected to two limiting plates 44 along the Z-axis, and the two limiting plates 44 are arranged at intervals along the X-axis. A second clamping strip 441 is connected to one side of the limiting plate 44, and one second clamping strip 441 is positioned directly above one of the first clamping strips 432; when the limiting plate 44 moves downward along the Z-axis, it can drive the second clamping strip 441 to move downward along the Z-axis to abut against the pads placed on the two first clamping strips 432, thereby limiting and flexibly pressing the pads between the first clamping strips 432 and the corresponding second clamping strips 441, so as to ensure the fixing effect of the pads, while not damaging the pads, and thus better protecting the pads. In this embodiment, the slide 41 can be a cuboid structure; and a first temperature sensor 92 for detecting the temperature inside the sealed heating cavity 6 is installed on one outer side of the slide 41; the first clamping strip 432 and the second clamping strip 441 can both be silicone clamping strips.
[0032] Furthermore, such as Figures 3 to 5 As shown, two first guide shafts 493 are connected between two fixed plates 13. The two first guide shafts 493 are spaced apart and symmetrically arranged on opposite sides of the first threaded shaft 132 along the Y-axis. The slide 41 is slidably sleeved on the two first guide shafts 493 along the X-axis to provide guidance and stability for the movement of the slide 41 on the X-axis.
[0033] Specifically, such as Figures 3 to 6As shown, the fixing base 42 includes a first plate 421 and two second plates 422. The two second plates 422 are respectively connected to the opposite ends of the first plate 421 along the Y-axis to form a U-shaped fixing base 42. The heating element 40 is mounted on the first plate 421. The placement frame 43 includes a square frame 433 and two supporting vertical plates 434. The square frame 433 is mounted on the two second plates 422, so that the square frame 433 is suspended relative to the first plate 421, which facilitates the setting of the heating element 40 corresponding to the through hole 431 of the square frame 433. The two supporting vertical plates 434 are arranged at intervals along the X-axis. The supporting vertical plates 434 are vertically mounted on the square frame 433. A horizontal first clamping strip 432 is installed on the inner side of one supporting vertical plate 434 facing the top of the other supporting vertical plate 434, and the top surface of the first clamping strip 432 is flush with the top surface of the corresponding supporting vertical plate 434. In this embodiment, the first plate 421 and the two second plates 422 can be an integral structure; the square frame 433, the two supporting vertical plates 434 and the two first clamping strips 432 can be an integral structure.
[0034] Furthermore, such as Figures 4 to 6 As shown, the top surface of the limiting plate 44 is flush with the top surface of the second clamping strip 441, and the bottom surface of the limiting plate 44 is flush with the bottom surface of the second clamping strip 441. The limiting plate 44 and the second clamping strip 441 can be an integral structure. Furthermore, two second guide shafts 4341 extending along the Z-axis are connected to the top of the supporting vertical plate 434. The two second guide shafts 4341 are located at opposite ends of the supporting vertical plate 434 along the Y-axis. The limiting plate 44 is slidably sleeved on the two second guide shafts 4341 along the Z-axis to provide guidance and stability for the movement of the limiting plate 44 on the Z-axis.
[0035] Specifically, such as Figures 4 to 6As shown, the support clamping assembly 4 also includes a second screw 45 and a second locking screw 46; the second screw 45 extends along the Z-axis and is disposed on the outer side of the support vertical plate 434 away from the first clamping bar 432, the bottom end of the second screw 45 rotates around the Z-axis and is axially (Z-axis) fixedly connected to the square frame 433 of the placement bracket 43, that is, axial fixation means that the second screw 45 cannot move linearly on the Z-axis, but can only rotate around its own axis (Z-axis); two second guide shafts 4341 are respectively disposed on opposite sides of the second screw 45 along the Y-axis; the limiting plate 44 is provided with a first hole through which the second screw 45 passes and a locking ring 46 respectively connected to the two second guide shafts. The second hole of the shaft 4341 is slidably fitted. The limiting plate 44 is threaded onto the second screw 45 through the first hole and slidably fitted onto the two second guide shafts 4341 through the second hole. The second screw 45 extends upward along the Z-axis to the top of the limiting plate 44, where a second locking screw 46 is threadedly connected. Rotating the second screw 45 can drive the limiting plate 44 to slide downward synchronously along the Z-axis on the second screw 45 and the two second guide shafts 4341. When the limiting plate 44 slides to the second clamping strip 441 on it and the first clamping strip 432 cooperate to clamp the solder pad, the second locking screw 46 is tightened to lock the limiting plate 44 and the second screw 45.
[0036] Furthermore, such as Figure 4 and Figure 5 As shown, the support and clamping assembly 4 also includes a second threaded shaft 47, a first driving member 48, and a guide block 491. The second threaded shaft 47 is rotatably connected to the slide 41 about the Y-axis, and a guide groove 411 extending along the Y-axis is formed within the slide 41. The fixed end of the first driving member 48 is connected to an outer side of the slide 41, and the output end of the first driving member 48 is coaxially connected to the second threaded shaft 47. The first driving member 48 drives the second threaded shaft 47 to rotate about the Y-axis. A guide block 491 is connected to the bottom end of the first plate 421 of the fixed base 42. The guide block 491 is threaded onto the second threaded shaft 47 and can slide along the Y-axis within the guide groove 411, providing guidance and stability for the movement of the fixed base 42 relative to the slide 41 along the Y-axis. In this embodiment, the first driving member 48 can specifically be a motor.
[0037] In this embodiment, as Figure 5 As shown, the guide block 491 can be a dovetail block, and the guide groove 411 can be a corresponding dovetail groove. The dovetail block can slide along the Y-axis in the dovetail groove, so as to drive the fixed seat 42 and the placement frame 43 to move along the Y-axis as a whole. This can help improve the movement accuracy of the fixed seat 42 along the Y-axis and achieve stable linear guidance of the fixed seat 42 in the limited space of the slide 41.
[0038] like Figures 4 to 6As shown, by setting up the aforementioned mutually cooperating slide 41, fixed seat 42, placement frame 43, limiting plate 44, first clamping bar 432 and second clamping bar 441, on the one hand, the layout between the various components can be more reasonable and compact, occupying a small area and not taking up too much usable space in the preheating box 1, and the production cost is lower; on the other hand, the first clamping bar 432 and second clamping bar 441 can cooperate to adjust the specific positions on the X-axis and Y-axis, thereby correspondingly adjusting the specific position of the solder pad. While ensuring stable clamping and fixing of the solder pad, it can realize two-dimensional electric precision adjustment of the solder pad on the X-axis and Y-axis, thereby meeting the high-precision welding alignment requirements between the solder pad and the ceramic electronic component, and effectively improving production efficiency and welding yield.
[0039] The following is a detailed description of the drive solder melting component 5: Specifically, such as Figures 1 to 3 , Figures 7 to 11 As shown, the solder melting assembly 5 includes a second driving component 51, a telescopic rod 511, a fixed rod 52, a soldering iron tip 53, a ceramic cylinder 54, and a third screw 56. The fixed end of the second driving component 51 is mounted on the top of the protective cover 2. One end of the telescopic rod 511 is connected to the output end of the second driving component 51, and the other end of the telescopic rod 511 is connected to the fixed rod 52, which is located inside the preheating box 1. The bottom end of the fixed rod 52 is connected to the soldering iron tip 53. The ceramic cylinder 54 has its opening facing downwards, and is fitted onto the fixed rod 52, with the bottom end of the ceramic cylinder 54... A sealing ring 55 is fitted onto the ceramic cylinder 54. The second driving member 51 can drive the ceramic cylinder 54 to move downward along the Z-axis, thereby moving the sealing ring 55 to seal against the solder pad to form the aforementioned sealed inner cavity 7. That is, the sealed inner cavity 7 is a local space formed by the ceramic cylinder 54 and the solder pad together. The bottom end of the third screw 56 passes through the ceramic cylinder 54 downward along the Z-axis. The third screw 56 is threadedly connected to the ceramic cylinder 54. One end of the third screw 56 located inside the ceramic cylinder 54 is equipped with a suction cup 561 for adsorbing ceramic electronic components. The ceramic electronic components are located directly below the soldering iron tip 53. In this embodiment, the second driving member 51 can specifically be a hydraulic cylinder.
[0040] It is worth noting that the suction cup 561 can be connected to a vacuum source via a vacuum line. A control valve is installed on the vacuum line. When it is necessary to release the ceramic electronic component, the control valve switches to a depressurization state, allowing outside air to enter the suction cup 561 to disrupt its vacuum suction force and separate the suction cup 561 from the ceramic electronic component. Alternatively, in another embodiment, a retractable ejector pin can be provided below the suction cup 561. When it is necessary to release the ceramic electronic component, the ejector pin moves downward to push the ceramic electronic component off the suction cup 561, thereby releasing the adhesion.
[0041] Specifically, such as Figures 7 to 11As shown, the second driving component 51 can drive the telescopic rod 511 to extend and retract along the Z-axis. The telescopic rod 511 will drive the fixed rod 52 to move downward along the Z-axis synchronously. The fixed rod 52 will then drive the ceramic cylinder 54 and the sealing ring 55 to move downward as a whole. When the sealing ring 55 moves downward along the Z-axis to contact the pad, the ceramic cylinder 54 and the sealing ring 55 will isolate the air in the external environment to cooperate with the pad to form the aforementioned sealed inner cavity 7. In this embodiment, the ceramic cylinder 54 can specifically be an alumina ceramic cylinder 54, and the sealing ring 55 can specifically be a silicone ring.
[0042] And, as Figure 10 and Figure 11 As shown, by rotating the third screw 56 on the ceramic cylinder 54, the ceramic electronic component can be moved up and down along the Z-axis, thereby adjusting the specific height of the ceramic electronic component relative to the solder pad. This ensures that the pins of the ceramic electronic component are directly opposite the mounting position of the solder pad (with solder paste applied), and that the pins of the ceramic electronic component are directly below the soldering iron tip 53. Simultaneously, a second temperature sensor 93 is installed on the inner top wall of the ceramic cylinder 54. Before the sealed inner cavity 7 is formed, the second temperature sensor 93 is used to detect the temperature inside the sealed heating cavity 6, working in conjunction with the first temperature sensor 92 to ensure accurate temperature detection within the sealed heating cavity 6. After the sealed inner cavity 7 is formed, the second temperature sensor 93 specifically detects the temperature of the sealed inner cavity 7, while the first temperature sensor 92 continues to detect the temperature inside the sealed heating cavity 6. This allows for real-time detection of the temperature inside the sealed heating cavity 6 and the temperature of the sealed inner cavity 7, thereby obtaining the real-time temperature of the ceramic electronic component within the sealed inner cavity 7 and effectively preventing damage to the ceramic electronic component due to overheating.
[0043] Furthermore, such as Figures 7 to 11 As shown, a second groove 521 extending along the Z-axis is provided on the outer wall of the fixed rod 52; the driving solder melting assembly 5 also includes a slider 57, a sliding column 58, and an elastic element 59; wherein, the slider 57 is disposed inside the top plate of the ceramic cylinder 54, and the slider 57 can slide along the Z-axis in the second groove 521 under the action of external force; the sliding column 58 extends along the Z-axis and is installed in the second groove 521; the elastic element 59 is sleeved on the sliding column 58, and the two ends of the elastic element 59 are respectively connected to the inner top wall of the slider 57 and the second groove 521; when the slider 57 slides upward along the Z-axis in the second groove 521, the elastic element 59 is compressed, at which time the soldering iron tip 53 moves downward along the Z-axis to press the pins of the ceramic electronic component into the solder paste on the pad. In this embodiment, the elastic element 59 can specifically be a spring.
[0044] Specifically, after the ceramic electronic components and pads are preheated in sections, the temperature is raised again. During heating, the solder paste on the pads melts, and the second drive unit 51 is activated. At this time, because the sealing ring 55 is in contact with the pad, that is, under the abutment and limiting action of the pad, the ceramic cylinder 54 and the sealing ring 55 can no longer move downward along the Z-axis. However, under the sliding engagement of the slider 57 and the second slide groove 521, the slider 57 is driven to slide upward along the Z-axis in the second slide groove 521, and the elastic element 59 is compressed, thereby causing the fixing rod 52 and the solder paste on it to move downward. The soldering iron tip 53 moves downward along the Z-axis relative to the ceramic cylinder 54, so that the soldering iron tip 53 directly presses the pins of the ceramic electronic component into the solder paste of the pad, thereby ensuring that the solder paste fully wets the pins and the mounting position of the corresponding pads. After the solder paste cools and solidifies, the soldering between the ceramic electronic component and the pad is completed, ensuring that a reliable electrical and mechanical connection is formed between the pins of the ceramic electronic component and the pad. Then, the second drive unit 51 controls the telescopic rod 511 to move the soldering iron tip 53 upward along the Z-axis to disengage from the solder paste.
[0045] It is understood that in this embodiment, the soldering iron tip 53 is mainly used as a pressing component. The soldering iron tip 53 itself does not necessarily have an independent heating function. It only needs to move downwards along the Z-axis relative to the ceramic cylinder 54 to press the pins of the ceramic electronic component into the molten solder paste. The heat for melting the solder paste is provided by the heating element 40 inside the sealed heating chamber 6. In this embodiment, the heating element 40 can specifically be several heating plates.
[0046] Furthermore, such as Figures 7 to 11 As shown, three second sliding grooves 521 are evenly provided along the circumference of the outer wall of the fixed rod 52, and each second sliding groove 521 is provided with a sliding column 58 and an elastic element 59; correspondingly, three sliders 57 are provided inside the top plate of the ceramic cylinder 54, and one slider 57 can slide along the Z-axis in a corresponding second sliding groove 521; thereby better ensuring the guidance and stability of the fixed rod 52 and the soldering iron tip 53 moving downward along the Z-axis relative to the ceramic cylinder 54.
[0047] like Figures 7 to 10 As shown, by setting up the aforementioned mutually cooperating fixing rod 52, ceramic cylinder 54, sealing ring 55, sliding column 58, elastic element 59, second sliding groove 521, and slider 57, on the one hand, the overall structural layout of the driving solder melting assembly 5 is more reasonable and compact, occupying a small area, and will not occupy a large amount of usable space in the protective cover 2 and preheating box 1, and the production cost is low; on the other hand, it can directly complete the solder melting between ceramic electronic components and pads, making the soldering operation simple and convenient, while ensuring a high-quality soldering bond between ceramic electronic components and pads.
[0048] The following is a detailed description of the flue gas extraction and filtration assembly 8: Specifically, such as Figure 7 and Figure 8 As shown, the preheating and tin melting device for ceramic electronic components also includes a flue gas suction and filtration assembly 8. The flue gas suction and filtration assembly 8 is installed on the telescopic rod 511 and the fixed rod 52. The flue gas suction and filtration assembly 8 is connected to the sealed inner cavity 7. The flue gas suction and filtration assembly 8 is used to suck in the flue gas generated in the sealed inner cavity 7 and purify the flue gas layer by layer.
[0049] By setting up the fume extraction and filtration assembly 8, on the one hand, the fumes generated in the sealed inner cavity 7 can be extracted in a timely manner and purified layer by layer, preventing the fumes from spreading to the surrounding environment, improving the working environment of the operators, and meeting occupational health and safety requirements; and on the other hand, by continuously extracting the fumes from the sealed inner cavity 7 through the fume extraction and filtration assembly 8, the fumes can be discharged in a timely manner, maintaining a clean environment in the sealed inner cavity 7, and preventing volatiles from condensing on the surface of ceramic electronic components or solder pads, which is conducive to ensuring welding quality; on the other hand, by directly installing the fume extraction and filtration assembly 8 on the telescopic rod 511 and the fixed rod 52, installation space is saved, the overall layout is simple and compact, which is conducive to improving the overall structural compactness; moreover, by timely removing the fumes, the accumulation of fumes in the sealed inner cavity 7 is prevented, and the pollutants in the fumes are prevented from adhering to the solder paste, leads, or solder pad surfaces during the welding process, ensuring the wettability of the solder paste and the cleanliness of the welding interface, which is further conducive to improving the stability and consistency of welding quality.
[0050] Furthermore, such as Figure 7 , Figure 8 and Figure 12As shown, a through groove 522 is provided on the fixed rod 52, extending radially through it; the flue gas suction and filtration assembly 8 includes a suction pump 81, a first suction pipe 82, a second suction pipe 83, and a purification component 85; wherein, the suction pump 81 is installed in the through groove 522; one end of the first suction pipe 82 is connected to the inlet end of the suction pump 81, and the other end of the first suction pipe 82 extends downward along the Z-axis into the ceramic cylinder 54, and the suction pump 81 can suck the flue gas generated in the sealed inner cavity 7 into the first suction pipe 82; that is, the first suction pipe 82 is specifically a first U-shaped pipe with the opening facing downward, and the two vertical branches of the first U-shaped pipe are respectively inserted downward along the Z-axis into the ceramic cylinder 54. The horizontal tube of the first U-shaped tube is connected to the inlet end of the bottom of the suction pump 81; and one end of the second suction tube 83 is connected to the outlet end of the suction pump 81, and the other end of the second suction tube 83 is connected to the purification cylinder 84, which is sleeved on the telescopic rod 511 and the fixed rod 52; that is, the second suction tube 83 is specifically a second U-shaped tube with the opening facing upward, and the two vertical branches of the second U-shaped tube are respectively inserted into the purification cylinder 84 along the Z-axis. The horizontal tube of the second U-shaped tube is connected to the outlet end of the top of the suction pump 81; the purification component 85 is installed in the purification cylinder 84 and sleeved on the telescopic rod 511 and the fixed rod 52. The purification component 85 is used to purify the flue gas layer by layer. The purification cylinder 84 is interference-fitted to the upper end of the fixed rod 52. The telescopic rod 511, near the telescopic part of the fixed rod 52, can slide along the Z-axis through the purification component 85 and the purification cylinder 84 to avoid interference between the telescopic rod 511 and the purification component 85 and the purification cylinder 84. The purification component 85 includes a pre-filter, an activated carbon adsorption layer, and a high-efficiency particulate air filter (HEPA filter) arranged sequentially from bottom to top. The flue gas entering the purification cylinder 84 passes through the three layers of adsorption and filtration—the pre-filter, the activated carbon adsorption layer, and the HEPA filter—from bottom to top before being directly discharged into the external environment, meeting environmental emission requirements. The specific structural type of the purification component 85 is not limited here.
[0051] like Figure 7 , Figure 8 and Figure 12As shown, by setting up a suction pump 81, a first suction pipe 82, a second suction pipe 83, a purification cylinder 84, and a purification component 85 that work together; on the one hand, by simultaneously drawing smoke from the sealed inner cavity 7 through the two vertical branches of the first U-shaped pipe, the smoke generated in the sealed inner cavity 7 can be quickly drawn into the suction pump 81, preventing the smoke from accumulating in the sealed inner cavity 7; and when the smoke is pressurized and drawn in by the suction pump 81, it enters the purification cylinder 84 through the second U-shaped pipe, where it is purified by the purification component 85, ensuring purification efficiency; furthermore, by extending the two vertical branches of the first U-shaped pipe (opening downwards) downwards into the ceramic cylinder 54, with the horizontal pipe of the first U-shaped pipe connected to the inlet end of the suction pump 81, and extending the two vertical branches of the second U-shaped pipe (opening upwards) upwards into the purification cylinder 84, with the horizontal pipe of the second U-shaped pipe connected to the inlet end of the suction pump 81, the purification efficiency is ensured; and by extending the two vertical branches of the second U-shaped pipe (opening upwards) upwards into the purification cylinder 84, with the horizontal pipe of the second U-shaped pipe connected to the inlet end of the suction pump 81, the purification efficiency is ensured. The outlet end at the top is connected; this symmetrical double U-shaped tube layout makes full use of the free space around the telescopic rod 511 and the fixed rod 52, without occupying additional installation space; on the other hand, the purification cylinder 84 and the purification component 85 are fixed on the fixed rod 52, and the telescopic rod 511 can slide along the Z-axis through the purification component 85 and the purification cylinder 84 during movement, and the two do not interfere with each other in space, so that the flue gas suction and purification functions do not affect the normal operation of the drive soldering assembly 5; at the same time, the purification component 85 and the purification cylinder 84 are sleeved on the outer periphery of the telescopic rod 511 and the fixed rod 52, which can effectively utilize the annular space between the telescopic rod 511 and the fixed rod 52; in addition, the flue gas suction and filter assembly 8 can form a modular structure, which is convenient for disassembly and replacement of the flue gas suction and filter assembly 8, reducing maintenance difficulty and maintenance cost.
[0052] Example 2
[0053] This embodiment provides a method for preheating and soldering ceramic electronic components. This method is based on the preheating and soldering apparatus for ceramic electronic components described in Embodiment 1 above. Figure 13 As shown, the preheating and soldering method for ceramic electronic components includes the following steps: S1: Apply solder paste to the pads and place the pads on the support clamping assembly 4 so that the support clamping assembly 4 supports and fixes the pads; S2: Place the ceramic electronic component above the pad, with the pins of the ceramic electronic component facing the solder paste on the pad, and move the two sealing baffles 3 along the X-axis to form a sealed heating cavity 6 by surrounding the preheating box 1, the protective cover 2, and the two sealing baffles 3, and heat the sealed heating cavity 6 with the heating element 40; when the temperature inside the sealed heating cavity 6 reaches the first preheating temperature of the ceramic electronic component, drive the output end of the solder melting assembly 5 to move downward along the Z-axis to seal and adhere to the pad to form a sealed inner cavity 7 to preheat the ceramic electronic component; then continue to raise the temperature until the temperature inside the sealed heating cavity 6 reaches the second preheating temperature of the pad to preheat the pad; S3: Heat up again to melt the solder paste and press the leads of the ceramic electronic components into the solder paste to solder the ceramic electronic components to the pads in the sealed inner cavity 7, and open the two sealing baffles 3 along the X-axis for heat dissipation and cooling.
[0054] The specific working process of the preheating and soldering method for ceramic electronic components in this embodiment is as follows: First, solder paste is applied to the mounting position of the solder pads, and the solder pads are placed on the two first clamping strips 432. Then, two limiting plates 44 are inserted into the two second guide shafts 4341 and the second screw 45. The second screw 45 is rotated to move the limiting plates 44 downward along the Z-axis, thereby moving the two second clamping strips 441 downward along the Z-axis to cooperate with the two first clamping strips 432 to clamp and fix the solder pads. Finally, the second locking screw 46 is tightened to lock the limiting plates 44 and the second clamping strips 432. Screw 45; then, the drive motor 492 is started by the control panel 91 to drive the first threaded shaft 132 to rotate around the X-axis, thereby causing the slide 41 to slide left and right on the first threaded shaft 132; at the same time, the control panel 91 can also start the first drive component 48 to drive the second threaded shaft 47 to rotate around the Y-axis in the slide 41, thereby driving the fixed seat 42 and the placement frame 43 to move along the Y-axis as a whole through the guide block 491, so as to adjust the specific position of the solder pad on the X-axis and Y-axis.
[0055] Then, the ceramic electronic component is adsorbed onto the suction cup 561, and the third screw 56 is rotated on the ceramic cylinder 54 to adjust the specific height of the ceramic electronic component relative to the pad, so that the subsequent pressing action is within the stroke, that is, to ensure that the specific height of the ceramic electronic component matches the deformation degree of the elastic element 59; then, the two sealing baffles 3 are moved towards the protective cover 2. At this time, the first screw 31 slides in the corresponding first groove 121. When the first screw 31 slides to the inner end wall of the first groove 121, one end of the sealing baffle 3 extends into the bottom end of the protective cover 2, and the other end of the sealing baffle 3 presses against the sealing element 131, and then the first... Tighten the locking ring 32 to form a sealed heating chamber 6 by surrounding the preheating box 1, the two sealing baffles 3, and the protective cover 2. Then, control the heating element 40 to heat the sealed heating chamber 6 through the control panel 91. When the temperature values detected by the first temperature sensor 92 and the second temperature sensor 93 both reach the first preheating temperature required by the ceramic electronic component, start the second driving element 51 to drive the ceramic cylinder 54 to move downward along the Z-axis, thereby moving the sealing ring 55 to seal and adhere to the pad to form a sealed inner cavity 7. Then, continue to heat up the pad through the heating element 40 to reach the second preheating temperature required by the pad, thereby completing the staged preheating of the ceramic electronic component and the pad.
[0056] Subsequently, the heating element 40 continues to heat the sealed heating chamber 6 to melt the solder paste, and the second driving element 51 is activated again. At this time, under the abutment and limiting action of the solder pad, the ceramic cylinder 54 and the sealing ring 55 can no longer move downward along the Z-axis. Under the sliding cooperation of the slider 57 and the elastic element 59, the slider 57 slides upward along the Z-axis in the second slide groove 521, the elastic element 59 is compressed, and the fixing rod 52 and the soldering iron tip 53 on it move downward along the Z-axis relative to the ceramic cylinder 54, so that the soldering iron tip 53 directly presses the pins of the ceramic electronic component into the solder paste of the solder pad, thereby ensuring the solder... The solder paste fully wets the pins and the corresponding pads at their mounting positions. Then, the second drive unit 51 controls the telescopic rod 511 to move the soldering iron tip 53 upward along the Z-axis, separating the soldering iron tip 53 from the solder paste. At the same time, the two sealing baffles 3 are opened to allow air circulation and quickly cool the solder paste. After the solder paste cools and solidifies to form a reliable solder joint, the suction cup 561 is released from its adsorption of the ceramic electronic component. The telescopic rod 511 is then controlled again to move the fixed rod 52 upward along the Z-axis, separating the suction cup 561 from the ceramic electronic component. This completes the soldering between the ceramic electronic component and the pad.
[0057] Meanwhile, when the soldering iron tip 53 comes into contact with the solder paste and is heated, fumes are generated. At this time, the suction pump 81 is started by controlling the control panel 91. The suction pump 81 will draw the fumes generated in the sealed inner cavity 7 into the first suction pipe 82, and then blow them into the purification cylinder 84 through the second suction pipe 83. Then, the fumes are gradually adsorbed and purified through the pre-filter, activated carbon adsorption layer and HEPA filter to achieve efficient purification of harmful substances.
[0058] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the implementation of the present invention. Those skilled in the art can make other variations or modifications based on the above description. It is neither necessary nor possible to exhaustively describe all embodiments here. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention should be included within the scope of protection of the claims of the present invention.
Claims
1. A preheating and soldering device for ceramic electronic components, characterized in that, include: Preheating box (1); A protective cover (2) is installed on the top of the preheating box (1); A sealing baffle (3) is slidably connected to the preheating box (1) along the X-axis. The protective cover (2) is provided with a sealing baffle (3) on each of the opposite sides along the X-axis. When the two sealing baffles (3) slide close together along the X-axis, a sealed heating cavity (6) is formed between the preheating box (1), the protective cover (2) and the two sealing baffles (3). The support clamping assembly (4) is slidably connected to the preheating box (1) along the X-axis and located below the protective cover (2). The support clamping assembly (4) and the protective cover (2) are spaced apart. The support clamping assembly (4) is used to support and clamp the solder pads. The support clamping assembly (4) is provided with a heating element (40) for heating the sealed heating chamber (6). A drive solder melting assembly (5) has its fixed end connected to the top of the protective cover (2). The output end of the drive solder melting assembly (5) passes through the protective cover (2) along the Z-axis and is placed in the sealed heating cavity (6). Before the output end of the drive solder melting assembly (5) moves downward along the Z-axis, the ceramic electronic component is pre-set in the internal cavity of the output end of the drive solder melting assembly (5) and located above the pad. The output end of the drive solder melting assembly (5) can move downward along the Z-axis to seal and fit against the pad, so as to form a local sealed inner cavity (7) in the sealed heating cavity (6). The sealed inner cavity (7) is a local space formed by the internal cavity and the pad. When the heating element (40) heats the temperature inside the sealed heating cavity (6) to the first preheating temperature of the ceramic electronic component, the output end of the driving solder melting assembly (5) moves downward along the Z-axis to the solder pad sealed and attached to the support clamping assembly (4) to form a sealed inner cavity (7); then the heating element (40) continues to heat the sealed heating cavity (6) until the temperature inside reaches the second preheating temperature of the solder pad, and the second preheating temperature is higher than the first preheating temperature.
2. The preheating and soldering device for ceramic electronic components according to claim 1, characterized in that, The sealing baffle (3) has a first screw (31) connected to the outer side of one end facing the protective cover (2); the preheating box (1) includes: The base plate (11) and two side plates (12) are horizontally connected between the two side plates (12). The two side plates (12) are respectively provided with a first sliding groove (121) extending along the X-axis. The first screw (31) slides through the first sliding groove (121) along the X-axis, and the end of the first screw (31) that extends out of the first sliding groove (121) is threaded with a first locking ring (32). The fixing plate (13) is provided with two fixing plates (13) spaced apart from each other along the X-axis. The fixing plate (13) is positioned between the two side plates (12). The bottom end of the fixing plate (13) is connected to the bottom plate (11). The top end of the fixing plate (13) is connected to a sealing element (131). The bottom end face of the sealing baffle (3) can contact the sealing element (131).
3. The preheating and soldering device for ceramic electronic components according to claim 2, characterized in that, A first threaded shaft (132) is rotatably connected between the two fixed plates (13) about the X-axis; the support and clamping assembly (4) includes: A slide (41) is threaded onto the first threaded shaft (132). The rotation of the first threaded shaft (132) can drive the slide (41) to move along the X-axis on the first threaded shaft (132). The fixed base (42) is slidably connected to the slide (41) along the Y-axis, and the heating element (40) is installed on the fixed base (42); A placement rack (43) is installed on the fixed base (42). The placement rack (43) has a through hole (431) extending through its thickness direction. The heating element (40) is arranged corresponding to the through hole (431). The placement rack (43) is connected to two first clamping strips (432) arranged at intervals along the X-axis. Both first clamping strips (432) are arranged along the X-axis toward the heating element (40). The limiting plate (44) is slidably connected to the placement frame (43) along the Z-axis. The two limiting plates (44) are arranged at intervals relative to each other along the X-axis. A second clamping strip (441) is connected to one side of the limiting plate (44). One second clamping strip (441) is positioned directly above one of the first clamping strips (432). The limiting plate (44) moves downward along the Z-axis to drive the second clamping bar (441) to move downward along the Z-axis to abut against the pads placed on the two first clamping bars (432), so as to limit and press the pads between the first clamping bars (432) and the corresponding second clamping bars (441).
4. The preheating and soldering device for ceramic electronic components according to claim 3, characterized in that, The support clamping assembly (4) further includes: The second screw (45) extends along the Z-axis. The bottom end of the second screw (45) rotates around the Z-axis and is axially fixedly connected to the placement frame (43). The limiting plate (44) is threaded onto the second screw (45) along the Z-axis. The second locking ring (46) is threaded onto the top of the second screw (45) which extends upward along the Z-axis to the outside of the limiting plate (44). Rotating the second screw (45) can drive the limiting plate (44) to move downward along the Z-axis on the second screw (45). The second locking ring (46) is used to lock the limiting plate (44) and the second screw (45).
5. The preheating and soldering device for ceramic electronic components according to claim 3, characterized in that, The support clamping assembly (4) further includes: The second threaded shaft (47) is rotatably connected to the slide (41) around the Y-axis, and the slide (41) has a guide groove (411) extending along the Y-axis. The first driving member (48) has its fixed end connected to an outer side of the slide (41), and its output end is coaxially connected to the second threaded shaft (47). Guide block (491), the bottom end of the fixed seat (42) is connected to the guide block (491), the guide block (491) is threaded onto the second threaded shaft (47), and the guide block (491) can slide along the Y axis in the guide groove (411).
6. The preheating and soldering apparatus for ceramic electronic components according to any one of claims 1-5, characterized in that, The driving solder melting assembly (5) includes: The second driving component (51) has its fixed end installed on the top of the protective cover (2); Telescopic rod (511), one end of which is connected to the output end of the second drive member (51); The other end of the telescopic rod (511) is connected to the fixed rod (52), and the fixed rod (52) is located inside the preheating box (1); Soldering tip (53), the bottom end of the fixing rod (52) is connected to the soldering tip (53); A ceramic cylinder (54) is provided with its opening facing downwards. The ceramic cylinder (54) is sleeved on the fixing rod (52), and a sealing ring (55) is sleeved on the bottom end of the ceramic cylinder (54). The second driving member (51) can drive the ceramic cylinder (54) to move downwards along the Z-axis, so as to move the sealing ring (55) to seal against the solder pad to form the sealing cavity (7). The third screw (56) has its bottom end passing through the ceramic cylinder (54) along the Z-axis downwards. The third screw (56) is threadedly connected to the ceramic cylinder (54). One end of the third screw (56) located inside the ceramic cylinder (54) is equipped with a suction cup (561) for adsorbing the ceramic electronic component. The ceramic electronic component is located directly below the soldering iron tip (53).
7. The preheating and soldering apparatus for ceramic electronic components according to claim 6, characterized in that, The outer wall of the fixing rod (52) is provided with a second sliding groove (521) extending along the Z-axis; the driving solder melting assembly (5) further includes: A slider (57) is disposed inside the top plate of the ceramic cylinder (54), and the slider (57) can slide along the Z-axis in the second groove (521); A sliding column (58) extends along the Z-axis and is installed in the second sliding groove (521); An elastic element (59) is sleeved on the sliding column (58), and the two ends of the elastic element (59) are respectively connected to the inner top wall of the slider (57) and the second sliding groove (521); When the slider (57) slides upward along the Z-axis in the second groove (521), the elastic element (59) is compressed, and the soldering iron tip (53) moves downward along the Z-axis to press the pins of the ceramic electronic component into the solder paste on the pad.
8. The preheating and soldering apparatus for ceramic electronic components according to claim 6, characterized in that, The preheating and soldering device for the ceramic electronic components also includes: A flue gas suction and filtration assembly (8) is installed on the telescopic rod (511) and the fixed rod (52). The flue gas suction and filtration assembly (8) is connected to the sealed inner cavity (7). The flue gas suction and filtration assembly (8) is used to suck in the flue gas generated in the sealed inner cavity (7) and purify the flue gas layer by layer.
9. The preheating and soldering apparatus for ceramic electronic components according to claim 8, characterized in that, The fixing rod (52) is provided with a through groove (522) extending radially therethrough; the flue gas extraction and filtration assembly (8) includes: A suction pump (81) is installed in the through slot (522); The first suction tube (82) has one end connected to the inlet end of the suction pump (81) and the other end extending downward along the Z-axis into the ceramic cylinder (54). The suction pump (81) can draw the smoke generated in the sealed inner cavity (7) into the first suction tube (82). The second suction tube (83) is connected at one end to the outlet end of the suction pump (81) and at the other end to a purification cylinder (84), which is sleeved on the telescopic rod (511) and the fixed rod (52). The purification component (85) is installed inside the purification cylinder (84) and sleeved on the telescopic rod (511) and the fixed rod (52). The purification component (85) is used to purify the flue gas layer by layer.
10. A method for preheating and melting solder in ceramic electronic components, characterized in that, Based on the preheating and soldering apparatus for ceramic electronic components as described in any one of claims 1-9, the preheating and soldering method for the ceramic electronic components includes the following steps: S1: Apply solder paste to the pad and place the pad on the support clamping assembly (4) so that the support clamping assembly (4) supports and fixes the pad; S2: The ceramic electronic component is placed above the pad, with the pins of the ceramic electronic component facing the solder paste on the pad. The two sealing baffles (3) are moved along the X-axis, so that the preheating box (1), the protective cover (2), and the two sealing baffles (3) form the sealed heating cavity (6), and the heating element (40) heats the sealed heating cavity (6). When the temperature inside the sealed heating cavity (6) reaches the first preheating temperature of the ceramic electronic component, the output end of the driving solder melting assembly (5) moves downward along the Z-axis to seal against the pad to form the sealed inner cavity (7) to preheat the ceramic electronic component. The temperature is then raised until the temperature inside the sealed heating cavity (6) reaches the second preheating temperature of the pad to preheat the pad. S3: Heat up again to melt the solder paste and press the pins of the ceramic electronic component into the solder paste to solder the ceramic electronic component to the pad in the sealed cavity (7), and open the two sealed baffles (3) along the X-axis for heat dissipation and cooling.
Citation Information
Patent Citations
Preheating tin melting device for ceramic electronic components
CN108031947A
Novel energy-saving wave soldering system
CN112475513A