A method for assembling a fluid filtration assembly and the fluid filtration assembly.

By setting annular stepped grooves and recesses in the fluid filter assembly, and combining the timing control of axial preload and welding heat input, the problems of damage to the filter element and internal loosening caused by welding heat are solved, achieving tight connection and high-reliability assembly.

CN122851984BActive Publication Date: 2026-11-17NINGBO YUSHENG MASCH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202611365945.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2026-09-04
Publication Date
2026-11-17
Estimated Expiration
2046-09-04

AI Technical Summary

Technical Problem

In the existing fluid filtration assembly process, the welding heat can easily damage the filter elements and cause internal loosening after assembly, affecting filtration accuracy and reliability.

Method used

By setting an annular stepped groove and an annular groove between the pipe body and the joint, and by controlling the timing of axial preload and welding heat input, a weld is formed and axial compression deformation is performed after the annular connection is plastically softened, eliminating gaps and achieving a tight internal connection.

Benefits of technology

It effectively blocks welding heat, avoids damage to filter components, ensures a tight and secure internal structure, and improves the product yield and fluid interception reliability of fluid filtration components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN122851984B_ABST
    Figure CN122851984B_ABST
Patent Text Reader

Abstract

This invention discloses an assembly method for a fluid filtration assembly and the fluid filtration assembly itself, relating to the field of fluid filtration technology. The assembly method includes providing a tube body, a connector, and a filter element with a rigid connecting member. The tube body has an annular stepped groove on its end face with an axial depth greater than the thickness of the connecting member, and an annular groove on its outer wall to define a thin-walled annular connecting portion. During assembly, a pre-tightening force is applied to bring the tube body into contact with the connector, and an axial gap is reserved between the connector and the connector to block welding heat. After the annular connecting portion is plastically softened by welding, the weld is controlled to solidify first, and then the continuously applied pre-tightening force forces the tube body to undergo axial compression deformation, thereby eliminating the axial gap and clamping the connecting member. This invention effectively solves the problem of high-temperature welding damaging the filter element, and achieves tight internal clamping through structural deformation, resulting in high product reliability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of fluid filtration technology, and more specifically to a method for assembling a fluid filtration assembly and a fluid filtration assembly assembled by the method. Background Technology

[0002] In various fluid piping systems, fluid filtration assemblies are typically required to intercept impurities in the fluid. Common fluid filtration assemblies generally consist of a pipe body and a connector that mates with it. The internal space of both the pipe body and the connector houses filter elements for filtering the fluid. To ensure the structural strength and external sealing of the piping system when subjected to high-pressure fluids, the pipe body and connector are often fixed together using a welding process.

[0003] Existing fluid filtration assemblies face a technical contradiction during assembly: achieving tight assembly while simultaneously protecting the filter element from heat. Specifically, filter elements typically consist of filter bags made of flexible materials and connectors used to maintain the opening shape; these components are highly sensitive to high temperatures. In conventional assembly processes, to tightly clamp the filter element between the pipe and the connector before welding to prevent loosening, the connector and connector must be tightly fitted together. During welding in this state, the high heat generated during welding is rapidly conducted through the connector to the internal connectors and filter bag, easily causing thermal melting damage or deformation failure of the filter element. Conversely, if a gap is intentionally left between the connector and the filter element during welding to block heat conduction, while preventing the filter element from burning at high temperatures, this gap solidifies and remains inside the product after welding, preventing the filter element from being effectively contained within the pipeline. This internal loosening not only causes abnormal noise and wear under fluid impact but also allows some fluid to bypass and leak from the gap around the filter bag, severely affecting the filtration accuracy and reliability of the fluid filtration assembly. Summary of the Invention

[0004] The present invention aims to solve the above-mentioned technical problems existing in the welding assembly process of fluid filter components in the prior art, and provides an assembly method and a fluid filter component that can effectively block welding heat and has a tight internal structure without loosening after assembly.

[0005] To achieve the above objectives, the present invention provides a method for assembling a fluid filtration assembly, comprising the following steps: S1. A tube body, a connector, and a filter element are provided. The filter element includes a filter bag and a rigid ring-shaped connector disposed at the opening of the filter bag. The tube body has a first end face, and the connector has a second end face disposed opposite to the first end face. An annular stepped groove with an axial depth greater than the thickness of the connector is recessed at the inner periphery of the first end face. The outer wall of the tube body is provided with an annular groove located radially outside the annular stepped groove, and an annular connection portion is defined between the annular groove and the annular stepped groove; the cross-section of the annular groove is V-shaped. The opening edge of the filter bag is folded outward to form a folded portion, which covers the end face of the connector facing the second end face; S2. Insert the filter bag into the tube from the first end face, and insert the connector into the annular stepped groove; S3. Apply axial preload to the joint and / or the pipe body so that the first end face abuts against the second end face, and a weld seam is formed at the junction of their outer peripheries; at this time, there is an axial gap between the end face of the connector and the second end face to prevent heat from being conducted to the connector through the second end face in the subsequent welding operation. S4. While maintaining the axial preload, perform fusion welding along the seam to be welded to form a weld, and use welding heat input to bring the annular connection into a plastic softening state; and control the solidification rate of the weld to be greater than the rate at which the annular connection leaves the plastic softening state. In steps S3 and S4, the axial preload is the first-level preload. S5. When the weld has solidified and the annular connection is still in a plastic softened state, the axial preload is increased to a second preload greater than the first preload. By continuously applying the axial preload, the pipe body is forced to undergo axial compression deformation at the annular connection, and the opening of the annular groove tends to close, thereby reducing the axial depth of the annular stepped groove until the axial gap is eliminated, so that the connector is clamped by the second end face and the bottom surface of the annular stepped groove. At the same time, the second end face axially presses the folded part against the end face of the connector, so that the compressed folded part is tightly filled between the connector and the second end face. S6. After the annular connecting part has cooled and hardened, release the axial preload.

[0006] Preferably, in step S4, the step of controlling the solidification rate of the weld to be greater than the rate at which the annular joint exits the plastic softening state specifically includes: After the fusion welding is completed, a cooling medium is applied to the weld to accelerate its solidification.

[0007] Preferably, the difference between the axial depth of the annular stepped groove and the thickness of the connector is 0.1 mm to 0.5 mm.

[0008] Preferably, the connector is made of copper or a copper alloy, and the tube body is made of stainless steel.

[0009] Preferably, in step S4, the fusion welding is laser welding; the laser beam of the laser welding is axially offset towards one side of the pipe body relative to the seam to be welded.

[0010] The present invention also provides a fluid filtration assembly, which is assembled by any of the assembly methods described above.

[0011] One or more technical solutions provided in this invention have at least the following technical effects or advantages: In the assembly method of this invention, when an axial preload is applied to bring the first end face of the tube into contact with the second end face of the connector, an axial gap is left between the end face and the second end face of the connector. This axial gap effectively cuts off the physical path of welding heat input directly from the connector to the connector and filter bag. Simultaneously, the annular groove on the outer wall of the tube defines a thinner annular connecting portion. This annular connecting portion causes a sharp reduction in the axial heat-conducting cross-sectional area of ​​the tube, thus creating a physical bottleneck in the heat conduction path. This abrupt change in cross-section not only forces the heat generated by welding to be highly concentrated in this annular connecting portion and rapidly induces a plastic softening state, but also significantly increases the resistance to further downward heat conduction, effectively blocking the conduction of high temperature to the annular stepped groove inside the tube, thereby preventing damage to the filter element from high temperature.

[0012] Furthermore, this invention transforms the heat input during the welding process into favorable conditions for subsequent assembly deformation. Utilizing the crucial time difference—the weld solidification rate exceeding the rate at which the annular connection emerges from its plastically softened state—the continuously applied axial preload, while the weld has already solidified and provided external connection strength, forces the tube body into axial compression deformation at the still-softened annular connection. This localized axial compression deformation directly reduces the axial depth of the annular stepped groove inside the tube body, thereby automatically eliminating the axial gap initially reserved for heat insulation.

[0013] Through the coupling process of the aforementioned thermodynamic state and mechanical deformation, this invention enables the connector to be firmly clamped using the second end face and the bottom surface of the annular stepped groove after the annular connection has cooled and hardened. This assembly method not only solves the industry pain point of high-temperature damage to filter elements during welding, but also eliminates the need for additional fastening parts or complex internal support fixtures. It achieves external sealing welding and gapless internal clamping in a single welding process and with continuous axial preload, significantly improving the product yield and fluid interception reliability of the fluid filter assembly. The fluid filter assembly assembled using this method has a compact internal structure and high external connection strength, possessing significant industrial practical value. Attached Figure Description

[0014] Figure 1 is a schematic diagram of the structure when the pipe body and the connector are not in contact in an embodiment of the present invention; Figure 2 is a schematic diagram of the state structure when the pipe body and the joint are in contact in an embodiment of the present invention; Figure 3 This is a schematic diagram of the structural state of the pipe body when a weld is formed between the joints in an embodiment of the present invention; Figure 4 This is a schematic diagram of the structural state of the tube body after axial compression deformation in an embodiment of the present invention.

[0015] Explanation of reference numerals in the attached drawings: 10, tube body; 11, first end face; 12, annular stepped groove; 121, bottom surface of the groove; 13, annular groove; 14, annular connecting part; 20, joint; 21, second end face; 30, filter element; 31, filter bag; 32, connecting part; 33, folded part; 40, axial clearance; 50, weld. Detailed Implementation

[0016] To make the above-mentioned objects, features and advantages of the present invention more apparent and understandable, specific embodiments of the present invention will be described in detail below with reference to the accompanying drawings.

[0017] Combination Figures 1 to 4 As shown, this embodiment provides a method for assembling a fluid filter assembly. The fluid filter assembly involved in this method is typically used in fluid pipeline systems that withstand a certain internal pressure. The fluid medium may include water, hydraulic oil, refrigerant, or chemical fluids, etc. This assembly method, by controlling the timing of welding heat input and mechanical deformation, includes the following specific assembly steps in sequence.

[0018] In step S1 of the preparation phase, a tube body 10, a connector 20, and a filter element 30 are provided for assembly. To balance fluid pressure resistance and weldability, the connector 20 is made of copper or a copper alloy, specifically brass, to utilize its thermal conductivity and machinability; alternatively, pure copper can also be used. The tube body 10 is made of stainless steel, specifically 304 stainless steel; alternatively, 316L stainless steel can be used in applications with higher corrosion requirements. The filter element 30 includes a filter bag 31 and a connector 32 located at the opening of the filter bag 31.

[0019] The filter bag 31 can be made of flexible and deformable filter materials such as polyester fiber, nylon, or polytetrafluoroethylene. The filter bag 31 is usually a bag-shaped structure with a closed bottom and an open top. The wall of the filter bag 31 has a pore structure that allows fluid to pass through. The fluid flows in from the connector 20 and enters the internal cavity of the filter bag 31. When passing through the side wall or bottom wall of the filter bag 31, solid particles or impurities larger than the pores are physically intercepted by the pore structure and collected inside the filter bag 31. The purified fluid then flows through the pore structure and out downstream, thereby achieving the function of fluid filtration and purification.

[0020] The connector 32 is in the form of a rigid ring. In specific implementation, a stainless steel stamped ring is used to maintain the structural stability of the opening of the filter bag 31. Alternatively, a high-temperature resistant engineering plastic ring can also be used.

[0021] In terms of overall structural layout, the pipe body 10 has a first end face 11, and the connector 20 has a second end face 21 opposite to the first end face 11. An annular stepped groove 12 is recessed at the inner periphery of the first end face 11, and the initial axial depth of the annular stepped groove 12 is configured to be greater than the thickness of the connector 32. An annular groove 13 is formed on the outer wall of the pipe body 10, located radially outside the annular stepped groove 12. The annular groove 13 and the annular stepped groove 12 define a thin-walled annular connecting portion 14. The cross-section of the annular groove 13 is V-shaped. In alternative technical solutions, the cross-section of the annular groove 13 can also be U-shaped or semi-circular, but the structural advantage of the V-shaped cross-section is that it is easy to machine and can provide clear structural guidance during subsequent pressure closure, making the deformation of the pipe wall more regular.

[0022] Combination Figure 1 As shown, in step S2, the tube body 10 and the connector 20 are not in contact. At this time, the filter bag 31 is inserted into the inner hole of the tube body 10 from the first end face 11, and the connector 32 is placed into the annular stepped groove 12, so that the bottom surface of the connector 32 is supported on the bottom surface 121 of the annular stepped groove 12.

[0023] Combination Figure 2 As shown, in step S3, an external pressing device is used to apply an axial preload to the connector 20 and / or the pipe body 10, causing the first end face 11 to abut against the second end face 21, forming a weld seam at the junction of their outer peripheries. In a specific implementation, a servo press is used as the external pressing device to fix the pipe body 10 on the bottom clamp. The press head of the servo press holds the connector 20 and applies a unidirectional axial preload downwards. As an alternative implementation, a pneumatic-hydraulic booster cylinder or a hydraulic press can be used to provide the driving force, or a bidirectional pressing method can be used to apply pressure from both ends of the pipe body 10 and the connector 20 simultaneously. To ensure the stability of the assembly process, the applied axial preload is the first-level preload. In a specific implementation, the first-level preload can be set to 100N or 200N, and its magnitude is set to maintain the pipe body 10 and the connector 20 without relative displacement. Since the axial depth of the annular stepped groove 12 is greater than the thickness of the connector 32, an axial gap 40 is left between the end face of the connector 32 and the second end face 21. The size of this axial gap 40 ranges from 0.1 mm to 0.5 mm, for example, it can be set to 0.2 mm or 0.3 mm. This axial gap 40 can block the heat in subsequent welding operations from being conducted to the internal connector 32 through the second end face 21, providing physical thermal protection for the heat-sensitive filter element 30.

[0024] Combination Figure 3 As shown, in step S4, while maintaining the first-level pre-tightening force, fusion welding is performed along the seam to be welded to form weld 50. In this embodiment, the fusion welding process is laser welding. During the welding process, the laser beam is axially offset relative to the seam to be welded towards the tube body 10. That is, the focus of the laser beam is not completely aligned with the junction gap between the first end face 11 and the second end face 21, but is offset downwards along the axial direction of the tube body 10 by a certain distance, so that more laser energy is directly radiated onto the outer wall of the tube body 10. Since the cross-sectional area of ​​the annular connecting part 14 at the annular groove 13 is small, a large amount of offset laser heat input accumulates here, and the annular connecting part 14 enters a plastic softening state through the welding heat input. At the same time, since the wall thickness of the annular connecting part 14 is thin, the axial heat-conducting cross-sectional area of ​​the tube body 10 is drastically reduced here, increasing the resistance to the continued downward conduction of heat, effectively blocking the conduction of high temperature to the annular stepped groove 12 inside the tube body 10, ensuring that the high temperature heat accumulated on the tube body 10 is difficult to spread to the internal connector 32 and filter bag 31. To establish a time difference in structural deformation, a cooling medium is applied to weld 50 after fusion welding to accelerate its solidification. In practice, high-pressure nitrogen is used as the cooling medium, which is then concentratedly sprayed onto weld 50. Alternatively, other protective gases such as argon or liquid carbon dioxide can be used. Through forced cooling, the solidification rate of weld 50 is controlled to be greater than the rate at which the annular connection 14 emerges from its plastic softening state. This ensures that while the outer weld 50 possesses high structural strength, the inner annular connection 14 remains in a softened region prone to deformation.

[0025] Combination Figure 4 As shown, in step S5, while the weld 50 has solidified and the annular connection 14 is still in a plastically softened state, an axial preload is continuously applied using an external press-fitting device. At this time, the axial preload is increased to a second-level preload greater than the first-level preload; specifically, the second-level preload can be set to 800N or 1000N. Under the pressure of the second-level preload, the pipe body 10 undergoes axial compression deformation at the annular connection 14, where the structural strength is weakest. During the collapse of the pipe wall of the pipe body 10, the opening of the V-shaped annular groove 13 tends to close. The compression deformation of the pipe wall of the pipe body 10 causes synchronous displacement of its internal structure, resulting in a reduction in the axial depth of the annular stepped groove 12 until the reserved axial gap 40 is eliminated, allowing the connector 32 to be clamped by the second end face 21 and the bottom surface 121 of the annular stepped groove 12.

[0026] To improve the internal fluid sealing performance, the opening edge of the filter bag 31 is folded outward to form a folded portion 33, which covers the end face of the connector 32 facing the second end face 21. The folded portion 33 and the connector 32 can be fixedly connected by ultrasonic welding, hot melt pressing, or applying high-temperature resistant adhesive. During the compression process in step S5, while the connector 32 is axially clamped by the second end face 21 and the bottom surface 121 of the annular stepped groove 12, the second end face 21 axially presses the flexible folded portion 33 onto the end face of the connector 32, so that the compressed folded portion 33 tightly fills the space between the connector 32 and the second end face 21. The beneficial effect of this design is that it uses the material of the filter bag 31 itself to form a seal, which can prevent fluid from bypassing and leaking from the edge of the filter element 30.

[0027] In step S6, after the annular connecting part 14, which has undergone compression deformation, has naturally cooled and hardened, the axial preload applied by the external press-fitting equipment is released, and the assembly of the fluid filter assembly is completed.

[0028] The fluid filter assembly assembled using the above method ensures external pressure resistance through high-temperature welding while preventing internal damage to the filter element 30 due to high temperatures. Furthermore, the material deformation of the tube body 10 automatically eliminates the thermal insulation gap. The assembled assembly has no excess fitting gaps, enabling it to withstand pressure pulsations in the pipeline without component loosening.

Claims

1. A method for assembling a fluid filtration assembly, characterized in that, Includes the following steps: S1. A tube body, a connector, and a filter element are provided. The filter element includes a filter bag and a rigid ring-shaped connector disposed at the opening of the filter bag. The tube body has a first end face, and the connector has a second end face disposed opposite to the first end face. An annular stepped groove with an axial depth greater than the thickness of the connector is recessed at the inner periphery of the first end face. The outer wall of the tube body is provided with an annular groove located radially outside the annular stepped groove, and an annular connection portion is defined between the annular groove and the annular stepped groove; the cross-section of the annular groove is V-shaped. The opening edge of the filter bag is folded outward to form a folded portion, which covers the end face of the connector facing the second end face; S2. Insert the filter bag into the tube from the first end face, and insert the connector into the annular stepped groove; S3. Apply axial preload to the joint and / or the pipe body so that the first end face abuts against the second end face, and a weld seam is formed at the junction of their outer peripheries; at this time, there is an axial gap between the end face of the connector and the second end face to prevent heat from being conducted to the connector through the second end face in the subsequent welding operation. S4. While maintaining the axial preload, perform fusion welding along the seam to be welded to form a weld, and use welding heat input to bring the annular connection into a plastic softening state; and control the solidification rate of the weld to be greater than the rate at which the annular connection leaves the plastic softening state. In steps S3 and S4, the axial preload is the first-level preload. S5. When the weld has solidified and the annular connection is still in a plastic softened state, the axial preload is increased to a second preload greater than the first preload. By continuously applying the axial preload, the pipe body is forced to undergo axial compression deformation at the annular connection, and the opening of the annular groove tends to close, thereby reducing the axial depth of the annular stepped groove until the axial gap is eliminated, so that the connector is clamped by the second end face and the bottom surface of the annular stepped groove. At the same time, the second end face axially presses the folded part against the end face of the connector, so that the compressed folded part is tightly filled between the connector and the second end face. S6. After the annular connecting part has cooled and hardened, release the axial preload.

2. The assembly method according to claim 1, characterized in that, Step S4, the step of controlling the solidification rate of the weld to be greater than the rate at which the annular joint exits the plastic softening state, specifically includes: After the fusion welding is completed, a cooling medium is applied to the weld to accelerate its solidification.

3. The assembly method according to claim 1, characterized in that, The difference between the axial depth of the annular stepped groove and the thickness of the connector is 0.1 mm to 0.5 mm.

4. The assembly method according to claim 1, characterized in that, The connector is made of copper or a copper alloy, and the tube body is made of stainless steel.

5. The assembly method according to claim 4, characterized in that, In step S4, the fusion welding is laser welding; the laser beam of the laser welding is axially offset towards one side of the pipe body relative to the seam to be welded.

6. A fluid filtration assembly, characterized in that, The fluid filtration assembly is assembled by the assembly method according to any one of claims 1 to 5.

Citation Information

Patent Citations

  • Elastic longitudinal seam metal filter bag