An electrowetting electronic paper device and its preparation method

By setting a mechanical locking structure of grooves and protrusions at the pixel wall contact interface of the electrowetting electronic paper, the problem of insufficient bonding force between the pixel wall and the upper electrode plate is solved, achieving higher sealing performance and stability, and enhancing the interface's ability to block electrolyte solution and water vapor.

CN123066973APending Publication Date: 2026-11-10XINLI OPTICAL RENSHOU CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611077128.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-07-20
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

In existing electrowetting electronic paper, the contact interface between the pixel wall and the upper electrode plate lacks effective bonding force, resulting in decreased sealing performance and easy separation during long-term use.

Method used

A mechanical locking structure of groove and protrusion is set at the contact interface between the upper and lower pixel walls. The protrusion is pressed into the groove to form an interference fit connection. When the upper and lower electrode plates are combined, a mechanical lock is formed to enhance the bonding force.

Benefits of technology

It improves the sealing performance and long-term stability of the pixel wall, prevents interface separation, enhances the sealing reliability against electrolyte solution and external moisture, resists thermal stress and mechanical vibration, reduces the alignment accuracy requirements, and improves manufacturing yield.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123066973A_ABST
    Figure CN123066973A_ABST
Patent Text Reader

Abstract

This invention discloses an electrowetting electronic paper device and its preparation method, which can maintain the sealing of the pixel wall during long-term use. The electrowetting electronic paper device includes an upper electrode plate and a lower electrode plate arranged opposite to each other. The upper surface of the lower electrode plate is a hydrophobic insulating layer, and there are upper and lower pixel walls. The upper pixel wall is bonded and fixed to the lower surface of the upper electrode plate, and the lower pixel wall is bonded and fixed to the upper surface of the hydrophobic insulating layer. One of the lower surface of the upper pixel wall and the upper surface of the lower pixel wall has several grooves, and the other has several protrusions. The positions of the grooves correspond one-to-one with the positions of the protrusions. When the upper electrode plate and the lower electrode plate are aligned and bonded together, each protrusion aligns and is pressed into the corresponding groove to form a mechanical locking structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to electronic paper display technology, and more particularly to an electrowetting electronic paper device and its preparation method. Background Technology

[0002] Electrowetting electronic paper is a novel reflective display technology based on the electrowetting effect. It controls the wetting properties of the display ink within the pixel by voltage, causing it to shrink and expand. This indirectly drives the expansion and contraction of the electrolyte solution, ultimately achieving image display. It has the advantages of low power consumption and easy readability.

[0003] The pixel wall is one of the core structures of electrowetting electronic paper. It is located in a sealed cavity between the upper and lower electrodes and is used to separate the display ink and electrolyte solution of adjacent pixels to prevent liquid crosstalk between different pixels. In existing electrowetting electronic paper, the pixel wall is generally fabricated as a whole on the surface of the hydrophobic insulating layer of the lower electrode using a photolithography process, and then bonded to the upper electrode to form a sealed pixel cavity.

[0004] Because the top of the pixel wall and the upper electrode plate only form frictional contact through interference fit, there is a lack of effective bonding force between them. During long-term use, the contact interface between the top of the pixel wall and the upper electrode plate is prone to separation, resulting in a decrease in the sealing performance of the pixel wall. Summary of the Invention

[0005] To address the shortcomings of the prior art, the present invention provides an electrowetting electronic paper device and its preparation method, which can maintain the sealing of the pixel wall during long-term use.

[0006] The technical problem to be solved by the present invention is achieved through the following technical solution: An electrowetting electronic paper device includes an upper electrode plate and a lower electrode plate disposed opposite to each other. The upper surface of the lower electrode plate is a hydrophobic insulating layer, and there are upper and lower pixel walls. The upper pixel wall is bonded and fixed to the lower surface of the upper electrode plate, and the lower pixel wall is bonded and fixed to the upper surface of the hydrophobic insulating layer. One of the lower surface of the upper pixel wall and the upper surface of the lower pixel wall is provided with a plurality of grooves, and the other is provided with a plurality of protrusions. The positions of the grooves correspond one-to-one with the positions of the protrusions. When the upper electrode plate and the lower electrode plate are aligned and bonded together, each protrusion aligns and is pressed into the corresponding groove to form a mechanical locking structure.

[0007] Furthermore, the upper electrode plate and the lower electrode plate are bonded and fixed together at the periphery of the upper and lower pixel walls by a sealing frame adhesive. The thickness of the sealing frame adhesive is less than the total thickness of the upper and lower pixel walls, so that each protrusion and the corresponding groove form an interference fit along the thickness direction.

[0008] Furthermore, the width of the protrusion is greater than the width of the groove, so that each protrusion and its corresponding groove form an interference fit along the width direction.

[0009] Furthermore, the groove is a hemispherical groove, and the protrusion is a hemispherical protrusion.

[0010] Furthermore, the diameter difference between the protrusion and the groove is 0.5~2μm.

[0011] Furthermore, the groove has a depth of 3~10μm and a diameter of 5~20μm; the protrusion has a height of 3~12μm and a diameter of 5.5~22μm.

[0012] Furthermore, the center-to-center distance between two adjacent grooves or two protrusions is 20~100μm, and the minimum edge distance between the grooves and protrusions and the upper and lower pixel walls is 8~12μm.

[0013] Furthermore, the upper pixel wall encloses and forms a plurality of pixel cavities, and the lower pixel wall encloses and forms a plurality of pixel cavities, with the pixel cavities of the upper pixel wall corresponding one-to-one with the pixel cavities of the lower pixel wall; each pixel cavity formed by the upper and lower pixel walls together is filled with immiscible display ink and electrolyte solution.

[0014] Furthermore, both the upper and lower pixel walls are made of hydrophilic materials.

[0015] A method for preparing an electrowetting electronic paper device includes the following steps: Step 1: The upper pixel wall is made on the lower surface of the upper electrode plate, and one of several grooves or several protrusions is made on the lower surface of the upper pixel wall; Step 2: The lower pixel wall is made on the upper surface of the lower electrode plate, and one of several protrusions or several grooves is made on the upper surface of the lower pixel wall; Step 3: Inject display ink into each pixel cavity formed by the lower pixel wall, and immerse the lower electrode plate in the electrolyte solution so that the electrolyte solution is higher than the upper surface of the lower pixel wall; Step 4: Immerse the upper electrode plate into the electrolyte solution and expel the air from the pixel cavities formed by the upper pixel wall. Step 5: In the immersion environment of the electrolyte solution, align and attach the upper electrode plate and the lower electrode plate, so that the protrusion is aligned and pressed into the groove to form a mechanical locking structure.

[0016] The present invention has the following beneficial effects: The electrowetting electronic paper device of the present invention provides a mechanical locking structure in which the groove and the protrusion cooperate with each other in the contact interface between the upper pixel wall and the lower pixel wall. When the upper electrode plate and the lower electrode plate are aligned and attached, the protrusion is aligned and pressed into the corresponding groove to form an interference fit physical connection. This establishes a reliable mechanical bonding force between the upper pixel wall and the lower pixel wall, effectively solving the problem that the interface of the existing integral pixel wall and the upper electrode plate is easily separated due to the lack of effective bonding force caused by frictional contact. Attached Figure Description

[0017] Figure 1 This is a schematic diagram of the stacked structure of the electrowetting electronic paper device provided by the present invention.

[0018] Figure 2 This is a three-dimensional structural diagram of the upper electrode plate and the upper pixel wall in the electrowetting electronic paper device provided by the present invention.

[0019] Figure 3 This is a three-dimensional structural diagram of the lower electrode plate and the lower pixel wall in the electrowetting electronic paper device provided by the present invention.

[0020] Figure 4 A flowchart illustrating the steps of the preparation method of the electrowetting electronic paper device provided by the present invention. Detailed Implementation

[0021] The present invention will now be described in detail with reference to the accompanying drawings and embodiments, examples of which are shown in the drawings, wherein the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and intended to explain the present invention, and should not be construed as limiting the present invention.

[0022] In the description of this invention, it should be understood that the terms "length", "width", "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this invention.

[0023] Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first," "second," or "third" may explicitly or implicitly include one or more of that feature. In the description of this invention, "multiple" means two or more, unless otherwise explicitly specified.

[0024] In this invention, unless otherwise explicitly specified and limited, the terms "installation," "connection," "linking," "fixing," and "setting," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal communication of two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.

[0025] Example 1 like Figure 1-3 As shown, an electrowetting electronic paper device includes an upper electrode plate 1 and a lower electrode plate 2 arranged opposite to each other. The upper surface of the lower electrode plate 2 is a hydrophobic insulating layer 23, and an upper pixel wall 3 and a lower pixel wall 4 are provided. The upper pixel wall 3 is bonded and fixed to the lower surface of the upper electrode plate 1, and the lower pixel wall 4 is bonded and fixed to the upper surface of the hydrophobic insulating layer 23. One of the lower surface of the upper pixel wall 3 and the upper surface of the lower pixel wall 4 is provided with a plurality of grooves 31, and the other is provided with a plurality of protrusions 41. The positions of the grooves 31 correspond one-to-one with the positions of the protrusions 41. When the upper electrode plate 1 and the lower electrode plate 2 are aligned and attached, each protrusion 41 is aligned and pressed into the corresponding groove 31 to form a mechanical locking structure.

[0026] The electrowetting electronic paper device of the present invention provides a mechanical locking structure in which the groove 31 and the protrusion 41 cooperate with each other at the contact interface between the upper pixel wall 3 and the lower pixel wall 4. When the upper electrode plate 1 and the lower electrode plate 2 are aligned and attached, the protrusion 41 is aligned and pressed into the corresponding groove 31 to form an interference fit physical connection. This establishes a reliable mechanical bonding force between the upper pixel wall 3 and the lower pixel wall 4, effectively solving the problem that the interface of the existing integral pixel wall and the upper electrode plate 1 is easily separated due to the lack of effective bonding force caused by frictional contact.

[0027] On the one hand, the gas between the two can be discharged during the process of the protrusion 41 being pressed into the groove 31, avoiding gas residue at the contact interface, eliminating the periodic stress caused by the expansion and contraction of the gas due to temperature changes, and improving the long-term stability of the interface bonding.

[0028] On the other hand, the interference fit between the protrusion 41 and the groove 31 generates continuous compressive stress, causing the outer wall of the protrusion 41 to fit tightly against the inner wall of the groove 31. The top of the protrusion 41 forms a surface contact with the bottom of the groove 31, and the side wall of the protrusion 41 forms a circumferential contact with the inner wall of the groove 31. These multiple contact interfaces constitute a dense sealing barrier, effectively blocking the penetration path of the electrolyte solution 6 and external water vapor along the contact interface between the upper pixel wall 3 and the lower pixel wall 4, significantly improving the sealing reliability between the upper pixel wall 3 and the lower pixel wall 4.

[0029] Furthermore, the mechanical interlocking structure between the protrusion 41 and the groove 31 can effectively resist the tendency of interface separation caused by external forces such as thermal stress and mechanical vibration. Even if the adhesion interface between the upper pixel wall 3 and the upper electrode plate 1, and between the lower pixel wall 4 and the hydrophobic insulating layer 23, degrades slightly due to long-term use, the interference compression force between the upper pixel wall 3 and the lower pixel wall 4 can still maintain the tight bond between the upper pixel wall 3 and the upper electrode plate 1, and between the lower pixel wall 4 and the hydrophobic insulating layer 23, providing redundant protection for sealing. In addition, the guide structure of the protrusion 41 and the guide structure of the groove 31 can automatically correct minor alignment deviations during the bonding process, reducing the alignment accuracy requirements and improving the manufacturing yield.

[0030] The upper electrode plate includes an upper substrate 11 and an upper electrode layer 12, with the upper electrode layer 12 disposed on the lower surface of the upper substrate 11; the lower electrode plate 2 includes a lower substrate 21, a lower electrode layer 22 and a hydrophobic insulating layer 23, with the lower electrode layer 22 disposed on the upper surface of the lower substrate 21 and the hydrophobic insulating layer 23 disposed on the upper surface of the lower electrode layer 22.

[0031] The lower substrate 21 can be a glass substrate or a flexible polymer substrate (such as PET or PI), and the lower electrode layer 22 can be ITO or a metal thin film (such as silver or gold), deposited on the upper surface of the lower substrate 21 by magnetron sputtering or evaporation. The hydrophobic insulating layer 23 is a fluorinated organic compound (such as polytetrafluoroethylene). The upper substrate 11 and lower substrate 21 can be made of glass substrate or flexible polymer substrate (such as PET, PI), and the upper electrode layer 12 and lower electrode layer 22 can be made of ITO or metal thin film (such as silver, gold), and are deposited on the upper substrate 11 and lower substrate 21 respectively by magnetron sputtering or evaporation. The hydrophobic insulating layer 23 is a fluorinated organic compound (such as polytetrafluoroethylene).

[0032] Both the lower pixel wall 4 and the lower pixel wall 4 are made of elastic material so that they can be tightly pressed together by their own internal elasticity during interference compression, forming a sealing structure similar to a sealing ring.

[0033] The upper electrode plate 1 and the lower electrode plate 2 are bonded and fixed to each other at the periphery of the upper pixel wall 3 and the lower pixel wall 4 by a sealing frame adhesive 7. The thickness of the sealing frame adhesive 7 is less than the total thickness of the upper pixel wall 3 and the lower pixel wall 4, so that each protrusion 41 and the corresponding groove 31 form an interference fit along the thickness direction.

[0034] The present invention uses the sealing frame adhesive 7 to limit the thickness of the box between the upper electrode plate 1 and the lower electrode plate 2, and by making the thickness of the sealing frame adhesive 7 less than the total thickness of the upper pixel wall 3 and the lower pixel wall 4, it ensures that the protrusion 41 and the groove 31 can form an interference compression in the thickness direction (box thickness direction) during bonding and pressing, while avoiding gaps between the upper pixel wall 3 and the lower pixel wall 4, so as to ensure the sealing effect.

[0035] The width of the protrusion 41 is greater than the width of the groove 31, so that each protrusion 41 and the corresponding groove 31 form an interference fit in the width direction.

[0036] The present invention uses the interference fit between the protrusion 41 and the groove 31 in the width direction (display plane) to generate continuous circumferential compressive stress between the outer wall of the protrusion 41 and the inner wall of the groove 31. The two are tightly fitted to form a sealing barrier with circumferential contact, which further blocks the penetration path of liquid along the interface.

[0037] Preferably, the groove 31 is a hemispherical groove 31, the protrusion 41 is a hemispherical protrusion 41, the diameter difference between the protrusion 41 and the groove 31 is 0.5~2μm; the center distance between two adjacent grooves 31 or two protrusions 41 is 20~100μm, and the minimum edge distance between the groove 31 and the protrusion 41 and the upper pixel wall 3 and the lower pixel wall 4 is 8~12μm.

[0038] In this embodiment, the groove 31 has a depth of 3~10μm and a diameter of 5~20μm; the protrusion 41 has a height of 3~12μm and a diameter of 5.5~22μm.

[0039] The upper pixel wall 3 encloses and forms a plurality of pixel cavities, and the lower pixel wall 4 encloses and forms a plurality of pixel cavities. The pixel cavities of the upper pixel wall 3 correspond one-to-one with the pixel cavities of the lower pixel wall 4. Each pixel cavity formed by the upper pixel wall 3 and the lower pixel wall 4 is filled with immiscible display ink 5 and electrolyte solution 6.

[0040] Preferably, both the upper pixel wall 3 and the lower pixel wall 4 are made of hydrophilic materials.

[0041] The upper pixel wall 3 and the lower pixel wall 4 of this invention are both made of hydrophilic materials, which ensures good wettability to the electrolyte solution 6 and repulsion to the display ink 5. This prevents the display ink 5 from climbing to the contact interface between the upper pixel wall 3 and the lower pixel wall 4. At the same time, the electrolyte solution 6 preferentially wets the upper pixel wall 3 and the lower pixel wall 4 and penetrates to the contact interface between the upper pixel wall 3 and the lower pixel wall 4, which helps to further expel the gas in the interface and enhance the negative pressure at the interface.

[0042] In this embodiment, both the lower pixel wall 4 and the lower pixel wall 4 are made of hydrophilic modified elastomers (such as hydrophilic modified PDMS or hydrophilic modified PFPE), hydrophilic polyurethane or photocurable hydrogel, etc. These materials all meet the hydrophilicity and elasticity requirements of the present invention for the lower pixel wall 4 and the lower pixel wall 4.

[0043] Example 2 like Figure 4 As shown, a method for preparing an electrowetting electronic paper device includes the following steps: Step 1: The upper pixel wall is made on the lower surface of the upper electrode plate, and one of several grooves or several protrusions is made on the lower surface of the upper pixel wall.

[0044] In step 1, the upper electrode plate includes an upper substrate and an upper electrode layer disposed on the lower surface of the upper substrate. The upper substrate may be a glass substrate or a flexible polymer substrate (such as PET, PI), and the upper electrode layer may be ITO or a metal thin film (such as silver, gold), deposited on the lower surface of the upper substrate by magnetron sputtering or evaporation.

[0045] First, a hydrophilic elastic material is prepared on the lower surface of the upper electrode plate by spin coating, screen printing or roll coating. After it is cured into a hydrophilic elastic material layer, the hydrophilic elastic material layer is then processed by photolithography or plasma gas etching to form the upper pixel wall. Finally, the lower surface of the upper pixel wall is processed by laser etching to form one of the grooves or protrusions.

[0046] Step 2: Create the lower pixel wall on the upper surface of the lower electrode plate, and create one of several protrusions or several grooves on the upper surface of the lower pixel wall.

[0047] In step 2, the lower electrode plate includes a lower substrate, a lower electrode layer disposed on the upper surface of the lower substrate, and a hydrophobic insulating layer disposed on the upper surface of the lower electrode layer. The lower substrate may be a glass substrate or a flexible polymer substrate (such as PET or PI), the lower electrode layer may be ITO or a metal thin film (such as silver or gold), deposited on the upper surface of the lower substrate by magnetron sputtering or evaporation, and the hydrophobic insulating layer is a fluorinated organic compound (such as polytetrafluoroethylene).

[0048] First, a hydrophilic elastic material is prepared on the upper surface of the lower electrode plate by spin coating, screen printing or roll coating. After it is cured into another hydrophilic elastic material layer, the other hydrophilic elastic material layer is processed by photolithography or plasma gas etching to form the lower pixel wall. Finally, the upper surface of the lower pixel wall is processed by laser etching to form another type of groove or protrusion.

[0049] Step 3: Inject display ink into each pixel cavity formed by the lower pixel wall, and immerse the lower electrode plate in the electrolyte solution so that the electrolyte solution is higher than the upper surface of the lower pixel wall.

[0050] In step 3, since the density of the display ink is greater than that of the electrolyte solution, after the lower electrode plate is immersed in the electrolyte solution, the display ink will be deposited on the lower electrode plate and located in the corresponding pixel cavity. At the same time, the electrolyte solution will also fill each pixel cavity of the lower pixel wall.

[0051] Step 4: Immerse the upper electrode plate in the electrolyte solution and expel the air from the pixel cavities formed by the upper pixel wall.

[0052] In step 4, the electrolyte solution is filled into each pixel cavity of the upper pixel wall by venting air.

[0053] Step 5: In the immersion environment of the electrolyte solution, align and attach the upper electrode plate and the lower electrode plate, so that the protrusion is aligned and pressed into the groove to form a mechanical locking structure.

[0054] In step 5, the upper and lower electrode plates are aligned and bonded under the immersion environment of the electrolyte solution in order to avoid air remaining in the pixel cavity after bonding.

[0055] In step 5, after alignment and bonding, the upper and lower electrode plates are removed from the electrolyte solution and clamped with a fixture to dry them while maintaining their bond. Finally, sealant is injected into the outer gap between the upper and lower electrode plates and the sealant is cured to form the sealing frame adhesive.

[0056] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the embodiments of the present invention and not to limit them. Although the embodiments of the present invention have been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can still be made to the technical solutions of the embodiments of the present invention, and these modifications or equivalent substitutions cannot cause the modified technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.

Claims

1. An electrowetting device for electronic paper, comprising an upper electrode plate and a lower electrode plate disposed opposite to each other, wherein the upper surface of the lower electrode plate is a hydrophobic insulating layer, characterized in that, It also includes an upper pixel wall and a lower pixel wall. The upper pixel wall is bonded and fixed to the lower surface of the upper electrode plate, and the lower pixel wall is bonded and fixed to the upper surface of the hydrophobic insulating layer. One of the lower surface of the upper pixel wall and the upper surface of the lower pixel wall is provided with a plurality of grooves, and the other is provided with a plurality of protrusions. The positions of the grooves correspond one-to-one with the positions of the protrusions. When the upper electrode plate and the lower electrode plate are aligned and fitted together, each protrusion is aligned and pressed into the corresponding groove to form a mechanical locking structure.

2. The electrowetting electronic paper device according to claim 1, characterized in that, The upper electrode plate and the lower electrode plate are bonded and fixed together at the periphery of the upper and lower pixel walls by a sealing frame adhesive. The thickness of the sealing frame adhesive is less than the total thickness of the upper and lower pixel walls, so that each protrusion and the corresponding groove form an interference fit along the thickness direction.

3. The electrowetting electronic paper device according to claim 1 or 2, characterized in that, The width of the protrusion is greater than the width of the groove, so that each protrusion and the corresponding groove form an interference fit along the width direction.

4. The electrowetting electronic paper device according to claim 1, characterized in that, The groove is a hemispherical groove, and the protrusion is a hemispherical protrusion.

5. The electrowetting electronic paper device according to claim 4, characterized in that, The diameter difference between the protrusion and the groove is 0.5~2μm.

6. The electrowetting electronic paper device according to claim 4 or 5, characterized in that, The groove has a depth of 3~10μm and a diameter of 5~20μm; the protrusion has a height of 3~12μm and a diameter of 5.5~22μm.

7. The electrowetting electronic paper device according to claim 1, characterized in that, The center-to-center distance between two adjacent grooves or two protrusions is 20~100μm, and the minimum edge distance between the grooves and protrusions and the upper and lower pixel walls is 8~12μm.

8. The electrowetting electronic paper device according to claim 1, characterized in that, The upper pixel wall encloses and forms a plurality of pixel cavities, and the lower pixel wall encloses and forms a plurality of pixel cavities. The pixel cavities of the upper pixel wall correspond one-to-one with the pixel cavities of the lower pixel wall. Each pixel cavity formed by the upper and lower pixel walls is filled with immiscible display ink and electrolyte solution.

9. The electrowetting electronic paper device according to claim 1, characterized in that, Both the upper and lower pixel walls are made of hydrophilic materials.

10. A method for preparing an electrowetting electronic paper device, characterized in that, Includes the following steps: Step 1: The upper pixel wall is made on the lower surface of the upper electrode plate, and one of several grooves or several protrusions is made on the lower surface of the upper pixel wall; Step 2: The lower pixel wall is made on the upper surface of the lower electrode plate, and one of several protrusions or several grooves is made on the upper surface of the lower pixel wall; Step 3: Inject display ink into each pixel cavity formed by the lower pixel wall, and immerse the lower electrode plate in the electrolyte solution so that the electrolyte solution is higher than the upper surface of the lower pixel wall; Step 4: Immerse the upper electrode plate into the electrolyte solution and expel the air from the pixel cavities formed by the upper pixel wall. Step 5: In the immersion environment of the electrolyte solution, align and attach the upper electrode plate and the lower electrode plate, so that the protrusion is aligned and pressed into the groove to form a mechanical locking structure.