A simulation calculation method for the stress-strain corrosion behavior of steel pipes

By simulating the stress corrosion behavior of steel pipes using a multiphysics coupling model, the corrosion problem of high-strength alloy steel pipes under stress and strain conditions was solved, enabling accurate prediction of corrosion behavior and design optimization, thereby improving the safety and economic benefits of oil and gas transportation.

CN123069727APending Publication Date: 2026-11-10BAOSHAN IRON & STEEL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510582757.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-07
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

Existing technologies lack in-depth research on the stress corrosion behavior of steel pipes, especially the stress corrosion cracking mechanism and protective measures for high-strength alloy steel pipes. This leads to severe corrosion failure during oil and gas transportation, threatening the safety of life and property.

Method used

A multiphysics coupling model, including elastoplastic stress field, electrochemical reaction model and corrosion morphology evolution model, is adopted. The corrosion behavior of steel pipe under stress and strain conditions is simulated by finite element algorithm, and the local crack shape propagation and its dynamic evolution characteristics are predicted.

Benefits of technology

It enables accurate simulation of stress corrosion behavior of steel pipes, identifies potential stress problems, optimizes design and improves safety, and reduces the risk of corrosion failure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123069727A_ABST
    Figure CN123069727A_ABST
Patent Text Reader

Abstract

This invention belongs to the field of numerical simulation research on corrosion, specifically involving a method for simulating the stress-strain corrosion behavior of steel pipes. Specifically, it includes: constructing a multiphysics coupled model; defining an elastoplastic stress field; establishing an electrochemical reaction model; modeling the corrosion morphology evolution; performing multiphysics coupled calculations; and solving simultaneously using a finite element algorithm. This invention demonstrates the coupled influence of elastic and plastic deformation on pipeline corrosion. In addition to numerically solving for the galvanic current density distribution, the anode surface is dissolved, and calculations are performed on the deformed surface of the steel pipe. A linear model of the polarization curve or a linear resistance model is used as the activation boundary condition for the anode and cathode surfaces, thereby calculating the deformation-potential-current density distribution over time, realizing the application of numerical simulation calculations in the field of stress corrosion behavior of pipeline steel.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of numerical simulation research on corrosion, specifically involving a method for simulating and calculating the stress-strain corrosion behavior of steel pipes. Background Technology

[0002] Pipeline steel is one of the most commonly used steels and one of the most widely applied materials. High-strength alloy steel is a common type of carbon structural steel that plays a crucial role in infrastructure construction due to its light weight, high strength, increasingly wide range of applications, formability, toughness, and ease of processing. In many engineering applications, carbon steel comes into contact with other metals, and the corrosion rate of carbon steel depends on the environmental conditions.

[0003] Current research on stress corrosion cracking (SCC) in steel pipes mainly focuses on in-depth exploration of its cracking mechanism, influencing factors, and protective measures. Currently, researchers have conducted extensive experimental and theoretical analyses on the SCC behavior of steel pipes (especially specific materials such as carbon steel, pipeline steel, and 316L stainless steel). They have reviewed the influence of material factors (such as alloying elements, microstructure, and inclusions), environmental factors (such as applied potential, pH value, temperature, and corrosive ions), and stress factors (such as residual stress, load type, and strain rate) on the SCC behavior and mechanism of steel pipes.

[0004] Regarding cracking mechanisms, researchers focused on analyzing the protective film rupture and anodic dissolution mechanisms of high-pH SCC, as well as anodic dissolution (AD), hydrogen embrittlement (HE), and AD / HE mixing mechanisms in near-neutral pH SCC. Exploring these mechanisms contributes to a deeper understanding of the SCC behavior of steel pipes under different environments.

[0005] Furthermore, researchers reviewed recent advances in improving the stress corrosion resistance of steel pipes by adjusting the pH value and solution concentration of the medium, introducing compressive stress, optimizing the microstructure, and improving coating processes, considering factors such as the influencing medium environment, materials, and surface stress state. These studies provide strong theoretical support and practical guidance for the protection of steel pipes.

[0006] It is worth noting that with the vigorous development of industrialization, the global demand for oil and gas resources is increasing day by day, and steel pipe materials such as pipeline steel are widely used in the transportation of oil and natural gas due to their reliability and economy. However, steel pipes inevitably suffer corrosion failure during operation, posing a serious threat to life and property safety. Therefore, research on stress corrosion of steel pipes is not only of theoretical significance, but also of important practical application value. Summary of the Invention

[0007] In view of the above-mentioned technical problems, this invention provides a simulation calculation method for the stress-strain corrosion behavior of steel pipes. In this invention, the model consists of two parts: the first part studies the stable effect of elastoplastic stress on corrosion by parametrically studying changes in longitudinal strain. The second part performs transient simulations to study the coupling effect between the dissolution and dynamic changes of corrosion defect depth on the pipeline under constant strain. The purpose of this numerical simulation method is to predict the shape propagation and dynamic evolution characteristics of continuously growing local cracks caused by stress corrosion effects.

[0008] The technical solution of this invention:

[0009] A method for simulating the stress-strain corrosion behavior of steel pipes includes the following steps:

[0010] (1) Construct a multiphysics coupling model:

[0011] a) Establish a geometric model that includes high-strength alloy steel pipes and a soil domain;

[0012] b) Use a fine mesh to divide the model into meshes and implement model-mesh adaptive matching. Mesh adaptive matching is performed synchronously when constructing the seawater fluid model.

[0013] (2) Define the elastoplastic stress field:

[0014] Stress simulation was performed using a small-strain plasticity model. A user-defined isotropic hardening model was constructed with a hardening function based on the experimental stress-strain curve, which was realized by a piecewise cubic interpolation function.

[0015] (3) Establish an electrochemical reaction model:

[0016] Iron dissolution anodic reaction and hydrogen evolution cathodic reaction are defined on the corrosion defect surface, and the remaining surfaces are set to electrochemical inertness;

[0017] (4) Corrosion morphology evolution modeling:

[0018] a) Define the normal migration velocity of the eroded interface:

[0019] b) A transient solver was used to simulate the corrosion process over 0-30 years, with the geometry updated at each time step;

[0020] (5) Perform multiphysics coupling calculations:

[0021] The finite element method is used to simultaneously solve the coupled equations of stress field, concentration field, and electric field, and output the surface potential, current density, and stress distribution data of the pipeline.

[0022] Furthermore, step (2) hardens the function σ. yhard The definition is as follows: Where σexp It is the experimental stress-strain curve, ε p It is plastic deformation, σ e It is von Mises stress, and E is Young's modulus (207 × 10⁻⁶). 9 Pa), σ ys It is the yield strength of high-strength alloy steel (600~1000×10). 6 Pa).

[0023] Furthermore, in step (3), the formula for calculating the anode current density is: Where i 0,a It is the exchange current density (2.353 × 10⁻⁶). -3 A / m 2 ), A a It is the Tafel slope (0.118V);

[0024] Overpotential η of anodic reaction a η is calculated using the following formula: a =φ s -φ l -E eq,a ;φ s φ is the actual electrode potential. l E is the standard electrode potential. eq,a This is the anode equilibrium potential;

[0025] The equilibrium potential of the anodic reaction is calculated by the following formula: Where E eq0,a It is the standard equilibrium potential of the anodic reaction (-0.859V), ΔP m The overpressure that causes elastic deformation (2.687 × 10⁻⁶) 8 Pa), V m This is the molar volume of steel (7.13 × 10⁻⁶). -6 m 3 / mol), z is the charge number of steel (2), F is the Faraday constant, T is the absolute concentration (298.15K), R is the ideal gas constant, v is the direction correlation factor (0.1~0.6), and α is the coefficient (1.67×10). 15 m -2 N0 is the initial dislocation density (1×10⁻⁶). 12 m -2 ).

[0026] Furthermore, the formula for calculating the cathode current density in step (3) is: Where i 0,c It is the exchange current density, A c It is the Tafel slope (-0.207V);

[0027] Overpotential η of the cathode reactionc (Unit: V) Calculated by the following formula: η c =φ s -φ l -E eq0,c ; where E eq0,c It is the standard equilibrium potential of the cathode reaction (-0.644V);

[0028] The exchange current density of the cathode reaction is calculated by the following formula: Where i 0,c,ref The reference exchange current density for the cathode reaction under no external stress / strain is 1.457 × 10⁻⁶. -2 A / m 2 );

[0029] Furthermore, the normal movement speed in step (3) is v (unit: m / s), which is calculated by the following formula: Where i a (Unit: A / m) 2 ) is the anodic current density, M is the molar mass of iron (55.845 g / mol), and ρ is the density of iron (7870 kg / m³). 3 ).

[0030] Furthermore, in step (1), the geometric model pipe has a length of 1-3m and a wall thickness of 12-24mm, and its surface is provided with regular geometric corrosion defects with a length of 10-500mm and a depth of 8-12mm.

[0031] Furthermore, the regular geometric shape of the corrosion defect is elliptical, rectangular, circular, rhomboid, square, etc.

[0032] Furthermore, in step (1), the soil pH is 6-8, generally neutral, soil moisture content is 10-15%, temperature is 12-18℃, and chloride ion concentration is 1-3‰.

[0033] Furthermore, the electrolyte conductivity of the soil domain in step (1) is 0.07-0.12 S / m.

[0034] Detailed Description of the Invention: A method for simulating and calculating the stress-strain corrosion behavior of steel pipes, comprising the following process and steps:

[0035] 1. Model geometry: such as Figure 1As shown, a single soil domain is used. It consists of a high-strength alloy steel pipe and the surrounding soil domain. The pipe length is 1–3 m, and the wall thickness is 12–24 mm. Corrosion defects on the outer side of the pipe are elliptical, with lengths of 10–500 mm and depths of 8–12 mm. The electrolyte conductivity in the soil domain is 0.07–0.12 S / m. Mesh was created for all models using a fine mesh type, and model-mesh adaptive matching was selected. The conductivity of the simulated seawater solution was tested, and a seawater fluid model was constructed using a fine mesh, also with model-mesh adaptive matching selected. After all models were built, boundary conditions were set for calculation. (A quadrilateral mesh with side lengths of 30–80 μm was used, defined in the software. Ultra-fine meshes are used to improve computational accuracy, typically at the micrometer level, using quadrilateral meshes.)

[0036] 2. Definition of Elastoplastic Stress Model: A small-strain plastic model is used to simulate elastoplastic stress in the pipe domain. In the user-defined isotropic hardening model, the hardening function σ... yhard The definition is as follows: Where σ exp It is the experimental stress-strain curve, ε p It is plastic deformation, σ e It is von Mises stress, and E is Young's modulus (207 × 10⁻⁶). 9 Pa), σ ys It is the yield strength of high-strength alloy steel (600~1000×10). 6 The experimental stress-strain curves used in the model were specified based on a piecewise cubic interpolation function.

[0037] 3. Electrochemical Reaction Model Definition: Iron dissolution (anodine) and hydrogen evolution (cathode) are two electrochemical reactions occurring on the surface of pipeline corrosion defects. The remaining pipeline surface is considered electrochemically inert; the Tafel expression for the anodic reaction is used to simulate the iron dissolution reaction, and the local anodic current density is defined as follows: Where i 0,a It is the exchange current density (2.353 × 10⁻⁶). -3 A / m 2 ), A a It is the Tafel slope (0.118V), and the overpotential η of the anodic reaction. a η is calculated using the following formula: a =φ s -φ l -E eq,a The equilibrium potential of the anodic reaction is calculated by the following formula: Where E eq0,a It is the standard equilibrium potential of the anodic reaction (-0.859V), ΔP m The overpressure that causes elastic deformation (2.687 × 10⁻⁶) 8Pa), V m This is the molar volume of steel (7.13 × 10⁻⁶). -6 m 3 / mol), z is the charge number of steel (2), F is the Faraday constant, T is the absolute concentration (298.15K), R is the ideal gas constant, v is the direction correlation factor (0.1~0.6), and α is the coefficient (1.67×10). 15 m -2 N0 is the initial dislocation density (1×10⁻⁶). 12 m -2 The cathode Tafel expression is used to simulate the hydrogen evolution reaction, which sets the local cathode current density as follows: Where i 0,c It is the exchange current density, A c The Tafel slope (-0.207V) represents the overpotential η of the cathode reaction. c (Unit: V) Calculated by the following formula: η c =φ s -φ l -E eq0,c ; where E eq0,c This is the standard equilibrium potential of the cathode reaction (-0.644V); the exchange current density of the cathode reaction is calculated by the following formula: Where i 0,c,ref The reference exchange current density for the cathode reaction under no external stress / strain is 1.457 × 10⁻⁶. -2 A / m 2 ).

[0038] 4. Deformation Geometry Model Definition: In the second part of the model, we use deformation geometry to model the dissolution of iron in the corrosion defect. The dissolution of iron causes the electrode boundary to move, and its normal movement velocity is v (unit: m / s), calculated by the following formula: Where i a (Unit: A / m) 2 ) is the anodic current density, M is the molar mass of iron (55.845 g / mol), and ρ is the density of iron (7870 kg / m³). 3 The transient study was used to solve the model, simulating corrosion over a period of 0–30 years.

[0039] 5. COMSOL Multiphysics 6.2 is a direct-coupled analysis software suitable for any number of physical fields. Based on the finite element method (FEM), it is used for numerical simulation. When calculating secondary current distribution fields, the FEM can obtain not only the potential and current density information of the structural surface, but also the potential and current within a specific range. Furthermore, the element shape of the object under study can vary, offering great flexibility and versatility. Therefore, it is suitable for calculating the stress corrosion behavior of pipelines in this work.

[0040] This invention discloses a simulation method for the stress-strain corrosion behavior of steel pipes. In the oil and gas industry, steel pipes are frequently subjected to complex stress / strain conditions. Besides internal pressure stress, the pipes also experience significant longitudinal strain due to surrounding soil movement. The resulting stress, caused by changes in the surface energy of the pipe surface, can influence the corrosion rate. However, research on the stress corrosion behavior of steel pipes is not yet in-depth. This invention focuses on demonstrating the coupled effects of elastic and plastic deformation on pipe corrosion. In addition to numerically solving for the galvanic current density distribution, we allow the anode surface to dissolve and perform calculations on the deformed surface of the steel pipe. A linear model of the polarization curve or a linear resistance model is used as the activation boundary condition for the anode and cathode surfaces, thereby calculating the deformation-potential-current density distribution over time. This realizes the application of numerical simulation in the field of stress corrosion behavior of pipeline steel.

[0041] Beneficial technical effects:

[0042] In this invention, the model is implemented using both the "Solid Mechanics" and "Secondary Current Distribution" interfaces. In the first study, the "Solid Mechanics" model is independent of the results from the "Secondary Current Distribution" model; we use a sequential solver with parametric sweeps to investigate the effect of elastoplastic deformation on electrochemical reactions. In the second part of the model, we use "Deformation Geometry" for transient analysis to analyze the impact of different depths caused by dissolution on stress and corrosion. Pipeline stress analysis is crucial in pipeline design and maintenance, ensuring safety, optimizing design, and improving economic efficiency. Through stress analysis, potential stress problems can be identified, and corresponding measures can be taken to eliminate these safety hazards. Attached image description:

[0043] Figure 1 This is a model architecture diagram of the electrolyte domain and the test sample.

[0044] Figure 2 Electrolyte potential distribution in the soil domain and von Mises stress distribution in the pipe domain for a specified displacement of 4 mm.

[0045] Figure 3 Stress distribution along the length of the corrosion defect at specified displacements of 1 mm, 2 mm, 3 mm, and 4 mm.

[0046] Figure 4 This is a corrosion potential distribution diagram along the length of the corrosion defect at specified displacements of 1 mm, 2 mm, 3 mm, and 4 mm.

[0047] Figure 5This is a diagram showing the anodic current density distribution along the length of the corrosion defect at specified displacements of 1 mm, 2 mm, 3 mm, and 4 mm.

[0048] Figure 6 The diagram shows the cathodic current density distribution along the length of the corrosion defect at specified displacements of 1 mm, 2 mm, 3 mm, and 4 mm.

[0049] Figure 7 The graphs show corrosion defect curves at t = 0a and 20a.

[0050] Figure 8 The von Mises stress distribution along the length of the corrosion defect is shown for t = 0a and 20a.

[0051] Figure 9 The diagram shows the corrosion potential distribution along the length of the corrosion defect at t = 0a and 20a.

[0052] Figure 10 The diagram shows the anodic current density distribution along the length of the corrosion defect at t = 0a and 20a.

[0053] Figure 11 The diagram shows the cathodic current density distribution along the length of the corrosion defect at t = 0a and 20a.

[0054] Figure 12 This is a flowchart for the simulation calculation.

[0055] Figure 13 This is a corrosion potential distribution diagram for soil with an electrical conductivity of 0.07 S / m and a defect depth of 8 mm.

[0056] Figure 14 The diagram shows the anodic current density distribution at a soil conductivity of 0.07 S / m and a defect depth of 8 mm.

[0057] Figure 15 This is a corrosion potential distribution diagram for soil with an electrical conductivity of 0.12 S / m and a defect depth of 12 mm.

[0058] Figure 16 The diagram shows the anodic current density distribution at a soil conductivity of 0.12 S / m and a defect depth of 12 mm. Figure 17 The cathode current density distribution along the corrosion defect length is shown for t=0a and 20a under different parameters. Detailed Implementation

[0059] The present invention will now be described in detail with reference to the accompanying drawings, so that its features and advantages will become more apparent and understandable.

[0060] Example 1: A simulation calculation method for the stress-strain corrosion behavior of steel pipes and related calculation parameters are as follows:

[0061] 1. Model geometry: such as Figure 1 As shown, a single soil domain was used. It consisted of a high-strength alloy steel pipe and the surrounding soil domain. The pipe was 2m long and 19.1mm thick. The corrosion defect on the outside of the pipe was elliptical, 200mm long and 11.46mm deep. The electrolyte conductivity in the soil domain was 0.096S / m. The soil pH was 6–8, generally neutral, with a soil moisture content of 10–15%, a temperature of 12–18℃, and a chloride ion concentration of 1–3‰. Mesh was generated for all models using a fine mesh type, and model-mesh adaptive matching was selected. The conductivity of the simulated seawater solution was tested, and a seawater fluid model was constructed using an ultrafine mesh, also with model-mesh adaptive matching selected. After all models were built, boundary conditions were set for calculation.

[0062] 2. Definition of Elastoplastic Stress Model: A small-strain plastic model is used to simulate elastoplastic stress in the pipe domain. In the user-defined isotropic hardening model, the hardening function σ... yhard The definition is as follows: Where σ exp It is the experimental stress-strain curve, ε p It is plastic deformation, σ e It is von Mises stress, and E is Young's modulus (207 × 10⁻⁶). 9 Pa), σ ys It is the yield strength of high-strength alloy steel (806×10). 6 The experimental stress-strain curves used in the model were specified based on a piecewise cubic interpolation function.

[0063] 3. Electrochemical Reaction Model Definition: Iron dissolution (anodine) and hydrogen evolution (cathode) are two electrochemical reactions occurring on the surface of pipeline corrosion defects. The remaining pipeline surface is considered electrochemically inert; the anodic Tafel expression is used to simulate the iron dissolution reaction, and the local anodic current density is defined as follows: Where i 0,a It is the exchange current density (2.353 × 10⁻⁶). -3 A / m 2 ), A a It is the Tafel slope (0.118V), and the overpotential η of the anodic reaction. a η is calculated using the following formula: a =φ s -φ l -E eq,a The equilibrium potential of the anodic reaction is calculated by the following formula: Where E eq0,a It is the standard equilibrium potential of the anodic reaction (-0.859V), ΔP m The overpressure that causes elastic deformation (2.687 × 10⁻⁶)8 Pa), V m This is the molar volume of steel (7.13 × 10⁻⁶). -6 m 3 / mol), z is the charge number of steel (2), F is the Faraday constant, T is the absolute concentration (298.15K), R is the ideal gas constant, v is the direction correlation factor (0.1~0.6), and α is the coefficient (1.67×10). 15 m -2 N0 is the initial dislocation density (1×10⁻⁶). 12 m -2 The cathode Tafel expression is used to simulate the hydrogen evolution reaction, which sets the local cathode current density as follows: Where i 0,c It is the exchange current density, A c This is the Tafel slope (-0.207V), and the overpotential η of the cathode reaction. c (Unit: V) Calculated by the following formula: η c =φ s -φ l -E eq0,c ; where E eq0,c This is the standard equilibrium potential of the cathode reaction (-0.644V); the exchange current density of the cathode reaction is calculated by the following formula: Where i 0,c,ref The reference exchange current density for the cathode reaction under no external stress / strain is 1.457 × 10⁻⁶. -2 A / m 2 ).

[0064] 4. Deformation Geometry Model Definition: In the second part of the model, we use deformation geometry to model the dissolution of iron in the corrosion defect. The dissolution of iron causes the electrode boundary to move, and its normal movement velocity is v (unit: m / s), calculated by the following formula: Where i a (Unit: A / m) 2 ) is the anodic current density, M is the molar mass of iron (55.845 g / mol), and ρ is the density of iron (7870 kg / m³). 3 The transient study was used to solve the model, simulating a corrosion period of 20 years.

[0065] The calculation results are as follows:

[0066] Figure 2 The electrolyte potential distribution (V) in the soil region and the von Mises stress distribution (MPa) in the pipe region are shown in the colored bars, representing a specified displacement of 4 mm in the x-direction. It can be seen that the local stress near the corrosion defects is significantly higher than that of the rest of the pipe. The uneven distribution of electrolyte potential near the corrosion defects... Figure 2The middle is also very obvious, as shown in the semi-circular area.

[0067] Figure 3 The von Mises stress distribution along the length of the corrosion defect is shown at displacements of 1 mm, 2 mm, 3 mm, and 4 mm. The von Mises stress increases with increasing tensile strain, reaching a maximum at the center of the corrosion defect. At tensile strains of 2 mm, 3 mm, and 4 mm, localized stresses are observed, particularly at the center of the corrosion defect, exceeding the yield strength of the high-strength alloy steel (806 × 10⁶ Pa). This leads to plastic deformation at the center of the corrosion defect, while deformation in other areas remains within the elastic range. At the lower tensile strain of 1 mm, the entire corrosion defect remains within the elastic deformation range.

[0068] Figure 4 The corrosion potential distribution along the length of the corrosion defect is shown at specified displacements of 1 mm, 2 mm, 3 mm, and 4 mm. At the lower tensile strain of 1 mm, a uniform variation of the corrosion potential along the length of the corrosion defect can be observed. However, at the higher tensile strains of 2 mm, 3 mm, and 4 mm, the variation of the corrosion potential is non-uniform, with the corrosion potential at the center of the corrosion defect being more negative than that on both sides.

[0069] Figure 5 The distribution of anolyte current density along the length of the corrosion defect is shown at specified displacements of 1 mm, 2 mm, 3 mm, and 4 mm. At the lower tensile strain of 1 mm, a uniform variation of anolyte current density along the length of the corrosion defect can be observed, similar to the variation characteristics of corrosion potential. However, at the higher tensile strains of 2 mm, 3 mm, and 4 mm, the variation of anolyte current density is significantly non-uniform, especially at the center of the corrosion defect. It can be seen that at higher tensile strains, the anolyte current density increases significantly at the center of the corrosion defect, while decreasing slightly at the sides. The increase in anolyte current density at tensile strains of 2 mm, 3 mm, and 4 mm is attributed to plastic deformation observed at the center of the corrosion defect (see...). Figure 3 ).

[0070] Figure 6 The cathode current density distribution along the length of the corrosion defect is shown at specified displacements of 1 mm, 2 mm, 3 mm, and 4 mm. It can be seen that the cathode current density increases negatively with increasing tensile strain, especially in corrosion defects. Figure 6The cathodic current density distribution along the length of the corrosion defect is shown at specified displacements of 1 mm, 2 mm, 3 mm, and 4 mm. It can be seen that the cathodic current density increases negatively with increasing tensile strain, reaching its maximum at the center of the corrosion defect. The non-uniformity of the cathodic current density also becomes more pronounced with increasing tensile strain. Therefore, the cathodic current density distribution is most non-uniform at a tensile strain of 4 mm.

[0071] Figure 7 The corrosion defect curves are shown at t=0a and 20a. It can be seen that after 20 years, the depth of the corrosion defects increases, especially at the center of the corrosion defects.

[0072] Figure 8 The von Mises stress distribution along the length of the corrosion defect is shown at t=0a and 20a. It can be seen that after 20 years, the von Mises stress at the center of the corrosion defect is higher than the von Mises stress on both sides of the corrosion defect.

[0073] Figure 9 This shows the corrosion potential distribution along the length of the corrosion defect at t=0a and 20a. It can be seen that after 20 years, in the entire...

[0074] Along the length of a corrosion defect, the corrosion potential is more negative.

[0075] Figure 10 The anodic current density distribution along the length of the corrosion defect is shown at t=0a and 20a. It can be seen that after 20 years, the anodic current density at the center of the corrosion defect is slightly higher than that at t=0a.

[0076] Figure 11 The distribution of cathodic current density along the length of the corrosion defect is shown at t=0a and 20a. It can be seen that after 20 years, the cathodic current density at the center of the corrosion defect is more negative than the values ​​on both sides, and slightly more negative than the value at t=0a.

[0077] Verify the anode current density (2.353 × 10⁻⁶). -3 In the electrochemistry of metal corrosion, the Tafel equation is often used to describe the relationship between the overpotential η and the current density i of an electrode reaction. For the anodic reaction, the Tafel equation is:

[0078] η = a + blogi

[0079] Where: η is the anodic overpotential (V); a is a constant (V) related to the electrode material, reaction temperature, and solution composition; b is the anodic Tafel slope (V / dec); and i is the anodic current density (A / cm²). 2In this invention, the polarization curves used for simulation calculations yield the following values: η = -0.073, b = 0.05, a = 0.2. Substituting these values ​​into the formula, we obtain i = 2.884 × 10⁻⁶. -3 A / cm 2 The results are close to the actual values, and the calculation results are basically accurate.

[0080] Example 2: A simulation calculation method for stress-strain corrosion behavior of steel pipes:

[0081] The soil electrical conductivity was 0.07 S / m, the defect depth was 8 mm, and other conditions were the same as in Example 1.

[0082] The calculation results are shown below. Figure 13 and Figure 14 .

[0083] Corrosion potential and anodic current density are the most important parameters in electrochemical corrosion. The accuracy of these values ​​directly reflects the rationality and accuracy of the model establishment and calculation results.

[0084] Example 3: A simulation calculation method for stress-strain corrosion behavior of steel pipes:

[0085] The soil electrical conductivity was 0.12 S / m, the defect depth was 12 mm, and other conditions were the same as in Example 1.

[0086] The calculation results are shown below. Figure 15 and Figure 16 It can only calculate the current anode current diagram. If the defect depth and conductivity are too large, the maximum value within the limited range is beyond the calculation scope, and the prediction results will be distorted.

[0087] In conclusion, the calculation method based on COMSOL for the stress corrosion behavior of steel pipes in soil is feasible. It can effectively characterize the influence of different depths of steel pipes in soil on their stress and corrosion.

[0088] The steps and accompanying drawings described above are preferred embodiments of the present invention. Other embodiments within the scope of protection can also achieve the above-mentioned beneficial effects, and will not be described in detail here. It should be noted that those skilled in the art can make several improvements and modifications without departing from the concept of the present invention, and these improvements and modifications should also be considered within the scope of protection of the present invention.

Claims

1. A method for simulating and calculating the stress-strain corrosion behavior of steel pipes, characterized in that, Includes the following steps: (1) Construct a multiphysics coupling model: a) Establish a geometric model that includes high-strength alloy steel pipes and a soil domain; b) Use a fine mesh to divide the model into meshes and implement model-mesh adaptive matching. Mesh adaptive matching is performed synchronously when constructing the seawater fluid model. (2) Define the elastoplastic stress field: Stress simulation was performed using a small-strain plasticity model. A user-defined isotropic hardening model was constructed with a hardening function based on the experimental stress-strain curve, which was realized by a piecewise cubic interpolation function. (3) Establish an electrochemical reaction model: Iron dissolution anodic reaction and hydrogen evolution cathodic reaction are defined on the corrosion defect surface, and the remaining surfaces are set to electrochemical inertness; (4) Corrosion morphology evolution modeling: a) Define the normal migration velocity of the eroded interface: b) A transient solver was used to simulate the corrosion process over 0-30 years, with the geometry updated at each time step; (5) Perform multiphysics coupling calculations: The finite element method is used to simultaneously solve the coupled equations of stress field, concentration field, and electric field, and output the surface potential, current density, and stress distribution data of the pipeline.

2. The simulation calculation method for stress-strain corrosion behavior of steel pipes according to claim 1, characterized in that, The hardening function σ in step (2) yhard The definition is as follows: Where σ exp It is the experimental stress-strain curve, ε p It is plastic deformation, σ e It is von Mises stress, E is Young's modulus, σ ys It is the yield strength of high-strength alloy steel.

3. The simulation calculation method for stress-strain corrosion behavior of steel pipes according to claim 1, characterized in that, In step (3), The formula for calculating anode current density is: Where i 0,a It is the exchange current density, A a It is the Tafel slope; Overpotential η of anodic reaction a η is calculated using the following formula: a =φ s -φ l -E eq,a ;φ s φ is the actual electrode potential. l E is the standard electrode potential. eq,a This is the anode equilibrium potential.

4. The simulation calculation method for stress-strain corrosion behavior of steel pipes according to claim 1, characterized in that, In step (3), The equilibrium potential of the anodic reaction is calculated by the following formula: Where E eq0,a It is the standard equilibrium potential of the anodic reaction, ΔP m It is the overpressure that causes elastic deformation, V m is the molar volume of steel, z is the charge number of steel (2), F is the Faraday constant, T is the absolute concentration, R is the ideal gas constant, v is the direction correlation factor, α is the coefficient, and N0 is the initial dislocation density.

5. The simulation calculation method for stress-strain corrosion behavior of steel pipes according to claim 1, characterized in that, The formula for calculating the cathode current density in step (3) is: Where i 0,c It is the exchange current density, A c It is the Tafel slope; Overpotential η of the cathode reaction c η is calculated using the following formula: c =φ s -φ l -E eq0c ; where E eq0,c It is the standard equilibrium potential of the cathode reaction; The exchange current density of the cathode reaction is calculated by the following formula: Where i 0,c,ref It is the reference exchange current density of the cathode reaction under no external stress / strain.

6. The simulation calculation method for stress-strain corrosion behavior of steel pipes according to claim 1, characterized in that, The normal movement speed in step (3) is v, which is calculated by the following formula: Where i a ρ is the anode current density, M is the molar mass of iron, and ρ is the density of iron.

7. The simulation calculation method for stress-strain corrosion behavior of steel pipes according to claim 1, characterized in that, The surface of the geometric model described in step (1) has regular geometric corrosion defects with a depth of 8-12mm.