An integrated in-situ detection device and method for simulating space environment of perovskite solar cells.

The integrated perovskite solar cell space environment simulation in-situ testing device solves the problem that existing equipment cannot achieve multi-field coupling. It realizes multi-field in-situ coupling under high vacuum, wide temperature range cycling, AM0 illumination and in-situ electrical testing, improving experimental efficiency and testing accuracy.

CN123074409APending Publication Date: 2026-11-10ZHEJIANG ZHONGNENG SEMICON TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202610938411.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-06-26
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

Existing space environment simulation testing equipment cannot achieve multi-field in-situ coupling of high vacuum, wide temperature range circulation, AM0 illumination and in-situ electrical testing in a single cavity, resulting in distorted test results and low experimental efficiency.

Method used

The integrated perovskite solar cell space environment simulation in-situ testing device includes a vacuum chamber module, a temperature control base module, a light source module, a vacuum system module, and an electrical control and data module. It realizes multi-field in-situ coupling of high vacuum, wide temperature range cycling, AMO spectral illumination, and in-situ electrical testing. It adopts technologies such as stainless steel chamber, quartz glass window, Stirling refrigerator, dynamic stress release electrical probe assembly, and Fail-Safe state machine logic.

Benefits of technology

It achieves multi-field in-situ coupling of high vacuum, wide temperature range cycling, AMO spectral illumination and in-situ electrical testing, avoiding environmental exposure and performance degradation of samples between different testing stages, improving experimental efficiency and testing accuracy, and ensuring the safety of equipment and samples.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123074409A_ABST
    Figure CN123074409A_ABST
Patent Text Reader

Abstract

This invention belongs to the field of semiconductor optoelectronic testing equipment and discloses an integrated in-situ testing device and method for simulating a space environment for perovskite solar cells. The device includes a vacuum chamber module, a temperature-controlled platform module, a light source module, a vacuum system module, and an electrical control and data module. The temperature-controlled platform module is integrated within a single-chamber structure and applies programmed temperature cycling to the sample; the light source module applies AMO spectral illumination to the sample through an optical window; the vacuum system module maintains a high-vacuum environment; and the electrical control and data module provides closed-loop control of each module and simultaneously acquires optoelectronic performance data and environmental parameters. This invention achieves multi-field in-situ coupling of high vacuum, wide temperature range, AMO illumination, and in-situ electrical testing, improving the realism of the test and experimental efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of semiconductor optoelectronic testing equipment, specifically relating to an integrated perovskite solar cell space environment simulation in-situ testing device and method. Background Technology

[0002] Perovskite solar cells are considered a key candidate for next-generation space photovoltaic devices due to their high photoelectric conversion efficiency, low cost, and flexible fabrication capabilities. The space environment features a high vacuum and atmospheric pressure lower than... Extreme temperature alternation coverage to Including characteristics such as AMO spectral solar radiation, ground verification of its environmental adaptability is a necessary step before space application. Existing ground verification methods mainly include: discrete equipment in series: using independent thermal vacuum chambers to provide high and low temperatures and vacuum environments, with an external solar simulator irradiating through a window; samples need to be transferred between different devices, making in-situ coupled testing of vacuum-temperature-light-electrical performance impossible; large-scale space environment simulators: spacecraft-grade large-scale equipment, bulky, expensive, and with long operating cycles, unable to meet the laboratory's needs for small-batch, multi-round, and rapid iterative R&D; conventional temperature control testing equipment: commercial high and low temperature chambers typically have temperature ranges limited to... to It cannot cover the extreme low temperature of space; moreover, the inner wall of the cavity is mostly a reflective metal surface, which causes serious stray light interference and is not suitable for precise testing of photoelectric performance.

[0003] The existing technology has the following main shortcomings:

[0004] Non-in-situ testing environment: Samples are transferred between vacuum, temperature control, light exposure, and electrical testing stages, and exposure to the atmosphere leads to surface oxidation, moisture absorption, phase transformation or decomposition of perovskite materials, resulting in distorted test results; Insufficient temperature range coverage: Existing laboratory-grade equipment struggles to stably achieve the required temperature range. The following deep low temperatures, and the heating and cooling rates are typically lower than It cannot simulate the rapid alternation of shadows in space; the optical path coupling efficiency is low: external light sources are incident through ordinary glass or single-sided coated windows, resulting in large optical losses, and it is difficult to balance window thermal stress with vacuum sealing; data is not synchronized: temperature, vacuum level, light intensity, - The curves are collected from different systems with asynchronous timestamps, making it difficult to establish a mapping relationship between "environmental parameters and device response"; thermo-mechanical-optical coupling failure: at deep cryogenic temperatures, the shrinkage of the cavity material leads to window sealing failure, or the thermal radiation of the light source interferes with the temperature control accuracy; existing equipment has not solved the structural stability under multi-physics coupling; stage thermal inertia bottleneck: copper or aluminum stages have large thermal inertia during wide-temperature cycling, with significant temperature differences between the edges and the center, leading to uneven local thermal stress in the perovskite film and inducing microcracks; thermal bridge effect of electrical test leads: the internal and external electrical leads of the vacuum cavity become heat conduction channels, and condensation or discharge on the leads at deep cryogenic temperatures affects test safety and accuracy; vibration transmission blind zone: If mechanical cooling such as a Stirling refrigerator is used, vibration is directly transmitted to the sample stage. Perovskite films are sensitive to micro-vibrations, leading to fluctuations in contact resistance or film peeling. There is a contradiction in maintaining vacuum for multiple sizes: changing samples of different sizes requires breaking the vacuum for disassembly and reassembly, frequently disrupting the high-vacuum environment and resulting in extremely low experimental efficiency. Vacuum outgassing contamination of the blackening layer: conventional anodizing or chemical blackening treatments have a high outgassing rate in a vacuum environment, becoming a continuous gas source, creating an inherent contradiction with the ultimate vacuum index. Furthermore, perovskite is extremely sensitive to residual water and oxygen. Infrared thermal radiation crosstalk: the full spectrum of the AM0 solar simulator contains a large amount of infrared thermal radiation, with wavelengths greater than... The quartz window has high transmittance in this wavelength band, creating an additional heat load in the deep cryogenic stage, forming a "heat source-cold source" conflict with the refrigeration unit, resulting in a sharp increase in temperature control power consumption; oxygen-free copper has a low-temperature thermal conductivity short circuit: oxygen-free copper in The thermal conductivity increases dramatically, reaching 5 to 10 times that of room temperature. The heat from the heating unit is rapidly drawn away by the refrigerator through the high thermal conductivity copper platform, resulting in a sharp drop in heating efficiency and localized overcooling. In addition, a single test cycle includes vacuuming, cooling, illumination, heating, and venting. Existing equipment lacks programmed automatic cycle capabilities, requiring significant manual intervention. Data is scattered across different software, leading to a large workload for subsequent correlation analysis. Furthermore, there is a lack of fail-safe mechanisms in case of overheating, vacuum leakage, or abnormal power failure, posing a risk of damage. Summary of the Invention

[0005] The purpose of this invention is to provide an integrated perovskite solar cell space environment simulation in-situ testing device and method, which solves the technical problem that existing space environment simulation testing equipment cannot achieve multi-field in-situ coupling of high vacuum, wide temperature range cycling, AM0 illumination and in-situ electrical testing in a single cavity, resulting in distorted test results and low experimental efficiency.

[0006] To solve the above-mentioned technical problems, the technical solution adopted by the present invention is as follows:

[0007] An integrated in-situ detection device for simulating space environment of perovskite solar cells includes:

[0008] A vacuum chamber module, wherein the vacuum chamber module is a single-chamber structure, and the vacuum chamber module is used to maintain a high vacuum environment;

[0009] A temperature-controlled stage module, integrated within the single-cavity structure, is used to apply pressure to a sample placed on the temperature-controlled stage module. to Programmed temperature cycling within the range;

[0010] The light source module includes a sunlight simulator, which is used to apply AMO spectral illumination to the sample through the optical window of the vacuum cavity module;

[0011] A vacuum system module, connected to the vacuum chamber module, is used to evacuate the single-chamber structure to the ultimate vacuum level;

[0012] The electrical control and data module is used to perform closed-loop control of the temperature control platform module, the light source module and the vacuum system module, and to simultaneously collect the photoelectric performance data and environmental parameters of the sample.

[0013] As a preferred embodiment of the present invention, the vacuum cavity module has a stainless steel cavity, the inner wall of which is subjected to a low outgassing rate blackening treatment, and the surface emissivity of the inner wall of the stainless steel cavity is not less than [missing information]. And the outgassing rate of the inner wall of the stainless steel cavity is not greater than .

[0014] As a preferred embodiment of the present invention, the optical window is made of quartz glass and is equipped with a double-sided anti-reflective coating. to The optical transmittance of the optical window within the specified band is not less than Furthermore, the optical window is flexibly connected to the vacuum cavity module through an elastic sealing structure.

[0015] Furthermore, a spectral filtering element is disposed between the light source module and the optical window, the spectral filtering element being used to reflect or absorb wavelengths greater than [a certain value]. Infrared thermal radiation, and only through to Spectral bands.

[0016] As a preferred embodiment of the present invention, the temperature control base module includes a stage, a heating unit and a cooling unit; the stage is made of high thermal conductivity oxygen-free copper, and the surface of the stage is blackened.

[0017] As a preferred embodiment of the present invention, the refrigeration unit is a Stirling refrigerator, and the refrigeration unit is connected to the stage through a vibration damping coupling structure to suppress the transmission of mechanical vibration to the sample.

[0018] A thermal resistance adjustment layer is provided between the back of the stage and the cold head of the refrigeration unit. The thermal resistance adjustment layer is a tungsten copper alloy gasket, which is used to introduce fixed thermal resistance and prevent the heat of the heating unit from being short-circuited away by the refrigeration unit under low temperature conditions.

[0019] As a preferred embodiment of the present invention, the stage has a built-in multi-zone independent temperature control circuit, which is used to control the temperature uniformity of the stage surface through zoned PID regulation.

[0020] As a preferred embodiment of the present invention, the electronic control and data module is used to execute a programmed temperature cycling illumination test sequence: controlling the temperature control base module to automatically raise and lower the temperature according to a preset temperature curve, and automatically turning on the light source module and simultaneously starting the photoelectric performance data acquisition of the sample after reaching the preset specified temperature node and the temperature reaches a steady state.

[0021] As a preferred technical solution of the present invention, the electronic control and data module has a fail-safe state machine logic. When the vacuum degree deterioration, temperature overshoot, light source spectral drift, or electrical noise surge in the single cavity structure is detected in real time and reaches a preset abnormal threshold, the electronic control and data module automatically switches to a safe sub-state and performs the following actions in a closed loop: cut off the power supply of the heating unit in the temperature control base module, turn off the light source module, save the currently collected data packets to a non-volatile memory, and drive the temperature control base module to start the system temperature recovery program.

[0022] As a preferred embodiment of the present invention, the vacuum system module includes a combined pumping unit of a molecular pump and a mechanical pump, and the vacuum system module is used to pump the single-chamber structure from atmospheric pressure to an ultimate vacuum level not exceeding [a certain value]. The time is no greater than .

[0023] As a preferred embodiment of the present invention, the stage is provided with vacuum adsorption holes or sample positioning grooves to physically adapt to and be backward compatible with samples of various sizes.

[0024] In addition, this invention also discloses an in-situ detection method for simulating the space environment of an integrated perovskite solar cell, comprising the following steps: using the aforementioned in-situ detection device for simulating the space environment of an integrated perovskite solar cell.

[0025] The sample is placed on the temperature-controlled base module inside the vacuum chamber module;

[0026] The vacuum system module evacuates the single-cavity structure of the vacuum chamber module to a vacuum level not exceeding [a certain threshold]. After the vacuum level stabilizes, the temperature control base module is controlled to operate according to a preset program. to Temperature changes within a certain range;

[0027] After reaching a steady state at a preset temperature node, the light source module is controlled to apply AMO spectral illumination to the sample through the optical window;

[0028] The current-voltage curve and maximum power point tracking steady-state data of the sample are acquired synchronously using the electronic control and data module.

[0029] As a preferred embodiment of the present invention, the optical window is configured with a double-sided anti-reflective coating. to The optical transmittance of the optical window within the specified band is not less than .

[0030] As a preferred embodiment of the present invention, during the cyclic temperature change process, the surface static temperature uniformity of the temperature control base module is controlled by performing zoned PID regulation through the multi-zone independent temperature control loop of the temperature control base module. Within.

[0031] As a preferred technical solution of the present invention, the method further includes the following safety protection steps: when an abnormal vacuum degree, temperature overshoot, light source spectral drift, or electrical noise surge is detected in the single cavity structure and reaches a preset abnormal threshold, the power supply of the heating unit is automatically cut off through the Fail-Safe state machine, the light source module is turned off, the currently collected data packets are saved to the non-volatile memory in real time, and the system safety recovery program is automatically started.

[0032] As a preferred embodiment of the present invention, the temperature-controlled platform module further includes a dynamic stress-relieving electrical probe assembly; the dynamic stress-relieving electrical probe assembly includes a piezoelectric ceramic actuator, a miniature force sensor, and a four-wire Kelvin probe; the four-wire Kelvin probe is independently driven by the piezoelectric ceramic actuator along a direction perpendicular to the Z-axis of the sample; the miniature force sensor is connected in a closed loop with the electronic control and data module to monitor the actual contact pressure between the four-wire Kelvin probe and the surface electrode of the sample in real time; the electronic control and data module is used to output displacement compensation commands to the piezoelectric ceramic actuator in real time according to the actual contact pressure, so that the... to During temperature cycling, the actual contact pressure remains at the preset constant target contact pressure, and the displacement compensation amount... The control satisfies the formula:

[0033]

[0034] in, The displacement compensation amount of the piezoelectric ceramic actuator is given by [missing information - likely a unit], where the unit of displacement compensation is [missing information - likely a unit]. ; The preset constant target contact pressure, the unit of which is... ; The actual contact pressure is monitored in real time by the miniature force sensor, and the unit of actual contact pressure is... ; The equivalent stiffness coefficient of the cantilever structure containing the four-wire Kelvin probe is given by [insert value here]. The unit of the equivalent stiffness coefficient is [insert value here]. ; The coefficient of thermal expansion of the dynamic stress relief electrical probe assembly is given by [reference to a specific parameter, which is missing from the original text]. The unit of the coefficient of thermal expansion is [reference to a specific parameter, which is missing from the original text]. ; This represents the temperature difference between the current real-time temperature and the initial calibration temperature, with the unit of temperature difference being... ; The effective reference length of the dynamic stress relief electrical probe assembly along the Z-axis is given by [insert unit here]. .

[0035] As a preferred embodiment of the present invention, the single-cavity structure is further connected to an in-situ quadrupole mass spectrometer; the in-situ detection method for photovoltaic devices simulating space environment also includes a simultaneous degradation kinetics analysis step.

[0036] During the cyclic temperature change and AMO spectral illumination process, the in-situ quadrupole mass spectrometer is controlled to continuously acquire the intensity of specific mass-to-charge ratio ion currents of degradation product gases generated by the volatilization of the sample inside the single-cavity structure.

[0037] The electronic control and data module synchronizes the intensity of ion current with specific mass-to-charge ratios, real-time temperature, and maximum power point tracking steady-state data, and calculates the in-situ volatilization rate of the target degradation products. The formula for calculating the in-situ volatilization rate is:

[0038]

[0039] in, The in-situ volatilization rate of the target degradation products is calculated in real time, and the unit of the in-situ volatilization rate of the target degradation products is... ; The effective pumping speed of the vacuum system module for the specific target degradation product under the current vacuum level is given by [missing information - likely a unit of measurement]. ; This refers to the instrument sensitivity coefficient of the in-situ quadrupole mass spectrometer for a specific mass-to-charge ratio, with the unit of the instrument sensitivity coefficient being [missing information]. ; This refers to the intensity of a continuously acquired ion current with a specific mass-to-charge ratio. The unit of this intensity is... ; Let $\mathbf{a}$ be the ideal gas constant, and the unit of the ideal gas constant is $\mathbf{a}$. ; The absolute temperature of the gas inside the single-cavity structure is given by [insert unit here]. .

[0040] Compared with the prior art, the present invention has the following beneficial effects:

[0041] This invention relates to an integrated in-situ testing device for perovskite solar cells in a simulated space environment. By integrating a vacuum chamber module, a temperature-controlled platform module, a light source module, a vacuum system module, and an electrical control and data module into a single-cavity structure, it achieves multi-field in-situ coupling under high vacuum, wide-temperature-range cycling, AMO spectral illumination, and in-situ electrical testing. This avoids environmental exposure and performance degradation caused by sample transfer between different testing stages, and can accurately reflect the in-situ photoelectric performance of perovskite solar cells in a space environment. The temperature-controlled platform module uses a vibration-damping coupling structure to connect the cooling unit and the stage, effectively suppressing the transmission of mechanical vibration to the sample and reducing electrical measurement noise. Simultaneously, through multi-zone independent temperature control loops combined with zoned PID regulation, the temperature uniformity of the stage surface is significantly improved. A thermal resistance adjustment layer on the back of the stage introduces fixed thermal resistance, preventing heat from the heating unit from being short-circuited and drawn away by the cooling unit under deep cryogenic conditions, reducing steady-state maintenance power consumption and avoiding localized overcooling. A spectral filter element is configured between the light source module and the optical window to cut off infrared thermal radiation from entering the cavity, reduce the temperature control overshoot during the deep low temperature illumination test, and shorten the temperature stabilization time.

[0042] The electrical control and data module executes a programmed temperature cycling illumination test sequence, simultaneously acquiring environmental parameters and photoelectric performance data, achieving a fully automated testing process and significantly improving experimental efficiency. The dynamic stress-relief electrical probe assembly, through closed-loop feedback control, maintains constant contact pressure between the probe and sample electrodes during wide-temperature cycling, eliminating contact resistance fluctuations and electrode damage caused by thermal expansion mismatch. The introduction of an in-situ quadrupole mass spectrometer enables real-time molecular-level monitoring of perovskite degradation products, establishing a correlation between photoelectric performance degradation and material chemical decomposition. The Fail-Safe state machine logic provides multi-layered safety protection, automatically executing protective actions and saving data under abnormal operating conditions, ensuring the safety of valuable samples and equipment. Attached Figure Description

[0043] To more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings used in the embodiments will be briefly introduced below. It should be understood that the following drawings only show some embodiments of the present invention and should not be regarded as a limitation of the scope. For those skilled in the art, other related drawings can be obtained from these drawings without creative effort.

[0044] Figure 1 This is a schematic diagram of the overall structure of the device described in this invention.

[0045] Figure 2 This is a schematic diagram showing the connection relationship between the vacuum system module and the vacuum cavity module of the present invention.

[0046] Figure 3 For the present invention Figure 2 The main view.

[0047] Figure 4 For the present invention Figure 4 Sectional view of plane AA.

[0048] Figure 5 This is a comparison chart of in-situ and non-in-situ PCE tests of the present invention.

[0049] Figure 6 This is the durability test curve for 100 thermal cycles of the present invention.

[0050] Figure 7 This is a thermal imaging comparison of temperature distribution between the multi-zone PID and the single-zone PID of the present invention.

[0051] Figure 8 This is the low-temperature pumping curve of the present invention.

[0052] Figure label:

[0053] 101 Vacuum chamber module, 102 Temperature control base module, 103 Light source module, 104 Vacuum system module, 105 Stage. Detailed Implementation

[0054] In the following description, only certain exemplary embodiments are briefly described. As those skilled in the art will recognize, the described embodiments can be modified in various ways without departing from the spirit or scope of the embodiments of the invention. Therefore, the drawings and description are considered to be exemplary in nature and not restrictive.

[0055] The following is in conjunction with the appendix Figures 1-8 The embodiments of the present invention will be described in detail below.

[0056] Example 1: This example discloses an integrated perovskite solar cell space environment simulation in-situ testing device, the overall external structure of which includes a vacuum chamber module 101. The external dimensions of the vacuum chamber module 101 are approximately... The internal effective testing space is precisely planned to accommodate the temperature control base module 102 and the optical path. The vacuum chamber module 101 has a stainless steel chamber, the inner wall of which is vacuum-plated with a black nickel layer, the thickness of which is approximately... And after plating is completed Next continuum Vacuum baking and degassing treatment. The emissivity of the inner wall surface of the stainless steel cavity after treatment. It can greatly absorb internal stray light and suppress stray light reflection; at the same time, the measured vacuum degassing rate of the stainless steel cavity inner wall is... Significantly lower than The limits of performance are met to maintain high vacuum.

[0057] An optical window is provided on the front of the stainless steel cavity. The effective light-transmitting area of ​​the optical window is... The optical window is made of high-purity quartz glass, and both sides of the quartz glass are coated with [material name missing]. Anti-reflection membrane. Anti-reflection membrane in to The average optical transmittance within the band is not less than Furthermore, its anti-reflection spectral range achieves high-precision matching with the AM0 spectrum of the solar simulator in the light source module 103. In order to... to During extreme temperature changes, while ensuring high vacuum sealing performance and eliminating thermal stress damage, the optical window and the flange of the stainless steel cavity are flexibly connected by an indium wire sealing structure or a metal bellows elastic sealing structure. The elastic deformation of the material effectively compensates for the high and low temperature thermal stress caused by the mismatch of the material's thermal expansion and contraction coefficients.

[0058] Example 2: This example is a further optimization based on Example 1. In this example, the temperature control platform module 102 is integrated into the single-cavity structure of the vacuum cavity module 101. The temperature control platform module 102 includes a stage 105, a heating unit, and a cooling unit. The stage 105 is made of high thermal conductivity oxygen-free copper, and its surface is chemically blackened to avoid light reflection. The thickness of the stage 105 is designed to be... to In this embodiment, it is preferred that... This allows for extremely fast temperature response while maintaining sufficient heat capacity. The stage 105 has vacuum adsorption holes or sample positioning slots machined on its surface, with an area sufficient to physically cover... , , , It supports samples of various standard specifications and backward compatibility with small-sized devices; in this embodiment, the stage 105 can be customized to support a maximum of [missing information - likely related to device specifications]. Large-area perovskite modules of various specifications.

[0059] The heating unit employs a high-power heating wire or resistive heating film applied to the back of the stage 105. This heating unit is integrated with the cooling unit in the same temperature control base module 102. The temperature control range of the temperature control base module 102 is... to Static temperature uniformity is controlled within Within this range, the heating and cooling rates are not less than The refrigeration unit employs a high-efficiency Stirling refrigerator.

[0060] To eliminate the impact of micro-vibrations caused by mechanical cooling on the perovskite thin film and electrical contacts, the cold head of the Stirling refrigerator is not rigidly connected to the stage 105. Instead, it is thermally connected to the stage 105 via a vibration-damping coupling structure composed of vibration-damping pads and flexible heat pipes. The main body of the Stirling refrigerator is fixed to an independent vibration-damping bracket outside the stainless steel cavity. Through this structure, the measured vibration acceleration transmitted to the sample surface on the stage 105 is only [amount missing]. The stage 105 has built-in multi-zone thermocouples, which, together with the zoned PID algorithm of the control software, control the temperature uniformity of the stage surface during temperature changes and steady-state processes. Within.

[0061] In this embodiment, a thermal resistance adjustment layer is specifically designed. The thermal resistance adjustment layer is a tungsten-copper alloy gasket disposed between the back of the stage 105 and the flexible heat pipe. The gasket is made of WCu15 and has a thickness of [missing information]. Its room temperature thermal conductivity is approximately ,exist The thermal conductivity at this point is approximately This layer, acting as a fixed thermal resistance, is inserted into the heat conduction path. While maintaining the unobstructed heat conduction path, this thermal resistance adjustment layer artificially introduces a controllable thermal resistance, successfully preventing [the spread of heat]. Under deep cryogenic steady-state conditions, the heat from the heating unit is rapidly drawn away by the cooling unit via a short circuit. Actual measurements show that this structure enables the system to... The steady-state power consumption is maintained from sudden drop The decline reached This effectively avoids localized overcooling and temperature instability.

[0062] Example 3: In this example, the vacuum system module 104 includes a molecular pump, a mechanical pump, a vacuum valve, a full-range vacuum gauge, and a venting valve. The vacuum system module 104 uses a mechanical pump as the pre-evacuation unit and a molecular pump as the high-vacuum pumping unit. After system startup, the mechanical pump first pre-evacuates the gas pressure in the stainless steel cavity to... Subsequently, the valves are automatically shut off or switched, and the molecular pump is started for secondary evacuation. The internal vacuum of a single-cavity structure can be evacuated to its ultimate vacuum level. .

[0063] The stage 105 is cooled to After reaching and maintaining a steady state under cryogenic conditions, the cryogenic pumping auxiliary unit, i.e., the liquid nitrogen cold trap, configured in the vacuum system module 104, works in conjunction with the system. Through continuous... Monitoring showed that the vacuum level within the single-cavity structure was stably maintained at [value missing]. to Within the specified range, no vacuum degradation occurred due to the blackening layer on the inner wall of the stainless steel cavity releasing gas or sample volatilization at deep cryogenic temperatures, demonstrating the synergistic effectiveness of the low-release-rate blackening layer and the cryogenic pumping auxiliary unit.

[0064] The light source module 103 includes a solar simulator externally positioned in front of the stainless steel cavity, which can be a high-power xenon lamp light source or an LED array light source. When a high-power xenon lamp light source is used, an infrared cutoff filter is placed between the light source module 103 and the optical window as a spectral filtering element. This filter is effective for wavelengths greater than [insert wavelength here]. The reflectivity of infrared thermal radiation is greater than ,right to The average transmittance of the band is greater than When using an LED array light source, its emission wavelength is filtered or physically limited, and the spectrum only covers... to The above method completely cuts off the effective photoelectric response band of perovskite devices with wavelengths greater than [a certain value]. The infrared thermal radiation is eliminated, fundamentally removing the infrared thermal load from the external light source, thus ensuring that the steady-state temperature control overshoot during the deep cryogenic illumination test phase is controlled within a certain range. Within this period, the stabilization time is shortened to approximately [timeframe missing]. .

[0065] Example 4: The electrical test leads of the sample are introduced into the single cavity through the vacuum electrical feedthrough on the side wall of the stainless steel cavity and connected to the sample electrode placed on the stage 105. The host computer of the electrical control and data module runs customized control software, and the specific steps of its fully automatic execution of the programmed temperature cycle illumination test sequence are as follows:

[0066] Step S1: Enter the experimental formula into the control software interface, set the temperature cycle control parameters, and set the temperature range to [temperature range to be specified]. to Temperature change rate set to The number of loops is set to Second-rate;

[0067] Step S2: One-button start test. The mechanical pump and molecular pump of the vacuum system module 104 work together to evacuate the interior of the single-chamber structure to the ultimate vacuum level. Once the set value is met, the temperature control base module 102 automatically starts the temperature control program;

[0068] Step S3: The stage 105 cools down or heats up at a set rate, and when the temperature reaches... , , , Once the preset target temperature node for illumination testing has reached a steady state, the control software of the electronic control and data module automatically sends a trigger command through a unified timestamp synchronization engine to turn on the light source module 103.

[0069] Step S4: Under the premise that the light source stably outputs AM0 light intensity, the data acquisition card of the electronic control and data module synchronously starts to collect the current-voltage curve of the sample and the maximum power point tracking steady-state data. The continuous recording time of single-point data is not less than [time value missing]. ;

[0070] Step S5: After the single-point electrical acquisition is completed, the control software automatically shuts down the light source module 103 and drives the temperature control base module 102 to continue to change the temperature until the cycle reaches the next preset temperature node, and repeats the control actions of steps S3 and S4.

[0071] Step S6: Setting After all temperature cycles are completed, the system automatically saves all environmental parameters and photoelectric data with a uniform timestamp, automatically generates a correlation comparison report, and drives the system to execute the safe temperature recovery and gas release procedures, thus ending the experiment.

[0072] In the aforementioned fully automated control process, the control software of the electronic control and data module incorporates fail-safe state machine logic. Throughout the entire test sequence, the system monitors the status of multiple sensors in real time.

[0073] If the full-range vacuum gauge reports a sudden deterioration in the vacuum level within the single-cavity structure... The multi-zone thermocouple feedback indicates that the surface temperature overshoot of the stage 105 exceeds [a certain value]. The photoelectric sensor feedback of the light source module 103 indicates that the spectral drift of the light source exceeds the center wavelength offset by more than [amount missing]. When the preset safety threshold is reached, or when the data acquisition card reports a sudden increase in the low-bias electrical noise of the sample exceeding a preset threshold of three times the baseline noise, the Fail-Safe state machine will instantly interrupt the current normal state flow and immediately transition to a safe sub-state. The safe closed-loop actions it executes are as follows:

[0074] Automatically cut off the power supply to the heating unit → automatically turn off the output shutter of the light source module 103 or disconnect the power supply to the light source → instantly save the currently collected data packets to non-volatile memory → forcibly drive the temperature control base module 102 to start the system reheat program, and control the stage 105 to gently return to room temperature → trigger the external audible and visual alarm to perform local and remote alarms.

[0075] In the event of a sudden power outage during the experiment, the UPS uninterruptible power supply equipped in the system will maintain the operation of the electrical control and data modules. To ensure the state machine remains intact, the current state and data are written into non-volatile memory for use after power-on. Non-destructive testing continued.

[0076] Example 5: This example is basically the same as Example 4, except that the following equivalent alternative implementation schemes are provided in this example:

[0077] The refrigeration unit in the temperature-controlled platform module 102 can be a Stirling refrigerator, a GM refrigerator, or a pulse tube refrigerator. Especially when using a pulse tube refrigerator with no moving parts, the mechanical vibration acceleration transmitted to the surface of the stage 105 can be further reduced to less than... It can completely eliminate the disturbance of micro-vibration to the contact resistance of ultrathin perovskite films.

[0078] The elastic sealing structure between the optical window and the stainless steel cavity flange can be replaced with an indium wire, or equivalently with a HelicoFlex metal sealing ring structure or an oxygen-free copper gasket knife-edge flange high-vacuum sealing structure. The replaced flexible sealing structure can extend the equipment's temperature resistance limit to [a later value]. to It can adapt to more demanding space environment simulations.

[0079] The stage 105 can be made of materials other than blackened oxygen-free copper, such as molybdenum or tungsten-copper alloys, like WCu15. Molybdenum has a coefficient of thermal expansion of only [missing information - likely a value]. Far lower than oxygen-free copper When subjected to high flow rate and temperature cycling, it can significantly reduce the thermal expansion mismatch stress between the stage 105 and the perovskite substrate, and prevent interlayer peeling of the thin film.

[0080] Example 6: In order to quantitatively verify the improvement of data authenticity by the single-cavity integrated in-situ coupling test described in this invention, a rigorous comparative experiment was conducted.

[0081] Experimental conditions: Perovskite solar cells prepared in the same batch and with identical structures were used as experimental samples. The physical structure of the device was: FTO conductive glass / TiO2 electron transport layer / FAO. 85 MA0. 15 PbI3 perovskite light-absorbing layer / Spiro-OMeTAD hole transport layer / Au metal electrode, effective area tested: .

[0082] Experimental Groups:

[0083] In-situ testing group: The sample is placed in the space environment simulation in-situ testing device for integrated perovskite solar cells described in this invention, and AMO illumination is directly turned on in-situ under fully enclosed high vacuum and programmed temperature change nodes while PCE is measured simultaneously.

[0084] Non-in-situ testing group: The sample is placed in a discrete hot vacuum chamber. After reaching a specified temperature point, the vacuum must be broken and the sample removed, then transferred to an air environment and exposed to the atmosphere for approximately [time period missing]. The photoelectric performance was tested using an external solar simulator.

[0085] Experimental data:

[0086] The measured photoelectric conversion efficiency and deviation rate data at each test temperature node are shown in Table 1 below:

[0087] Table 1:

[0088] Test temperature node In-situ test PCE (%) Non-in-situ test PCE (%) PCE deviation rate -160℃ 12.8 10.2 -20.3% -80℃ 16.5 15.1 -8.5% 25℃ 21.2 20.8 -1.9% +150℃ 14.3 13.6 -4.9%

[0089] The above comparative experimental data and conclusions show that traditional non-in-situ testing methods inevitably expose perovskite devices to external water and oxygen environments during the transfer process, leading to instantaneous degradation or hygroscopic phase transitions of sensitive interfaces and materials. This results in severely distorted test results, especially at low temperatures, where efficiency is significantly lower than expected. The in-situ testing described in this invention can truly and accurately reflect the physical performance of the device in a multi-field coupling environment in space.

[0090] Example 7: Extreme operating conditions and durability verification. The device of the present invention was driven to execute an extreme rapid temperature change program, and the control parameters were set as follows: to Temperature change rate as high as .

[0091] like Figure 7 As shown, actual measurements indicate that the temperature overshoot on the surface of the stage 105 is only [amount missing] during the heating phase. During the cooling phase, only The settling time after reaching the target value is less than The static temperature uniformity of the entire countertop is controlled within Within.

[0092] like Figure 6 As shown, the integrated perovskite solar cell space environment simulation in-situ testing device of the present invention is continuously executed. Second-rate to Extreme full-temperature thermal cycling durability test. A comparison of key performance indicators before and after the test shows:

[0093] Optical window seal leakage rate: from initial Slightly increased to It still perfectly maintains within the high vacuum sealing specifications; vacuum electrical feedthrough contact resistance: due to alternating high and low temperature stress, the contact resistance changes from the initial... Slight drift to However, the sample - The electrical measurement noise standard deviation of the curve did not show any significant degradation in the low bias region; the emissivity of the blackened layer on the inner wall of the stainless steel cavity: from the initial... Slightly decreased Its ability to absorb and suppress stray light within the cavity remains stable.

[0094] Furthermore, under extreme conditions where the Stirling refrigerator is running at full speed, the sampling rate is achieved using a triaxial accelerometer placed on the surface of the stage 105. The measured RMS vibration acceleration of the sample was only At this time, the sample is in The standard deviation of short-circuit current fluctuation near the bias voltage is only Compared to rigid connection schemes without vibration damping structures, its vibration acceleration reaches... The standard deviation of current fluctuation is as high as The electrical measurement noise of the present invention is reduced The above ensures the physical accuracy of precision electrical testing.

[0095] Example 8: In an area of On the blackened oxygen-free copper stage 105, according to Uniformly arranged in matrix form A high-precision thin-film thermocouple grid is used, with the physical spacing between the measuring points fixed at a certain value. The conventional single-zone PID temperature control loop and the multi-zone independent temperature control loop described in this invention were tested separately. Temperature distribution under deep cryogenic steady state.

[0096] Single-zone PID control results: When the center measuring point stabilizes at... At that time, due to heat loss through radiation and conduction to the external cavity at the edge of the stage 105, the actual temperature at the edge measuring point is only [missing information]. The maximum temperature difference on the countertop is as high as The relative standard deviation (RSD) of the table surface temperature uniformity is: This cannot meet the requirements for extremely high-precision spatial testing.

[0097] Multi-zone PID control result: On Independent temperature control loops for each zone operate in a closed-loop manner, and the central measuring point stabilizes at... At that time, the temperature of the edge measuring points was accurately compensated and maintained at... The maximum temperature difference across the entire surface suddenly dropped to The relative standard deviation (RSD) of temperature uniformity is only [value missing]. Perfectly superior to The industry's extreme indicators.

[0098] Example 9: Under the alternating low and high temperatures of space, the thermal expansion coefficients of the high thermal conductivity oxygen-free copper stage 105 and the silicon-based or glass-based perovskite samples exhibit a severe mismatch. When the temperature-controlled stage module 102 is in... to During rapid cycling, the sample undergoes micrometer-level warping deformation in the Z-axis direction, causing drastic fluctuations in the contact stress of conventional fixed probes. This not only leads to probe detachment at deep cryogenic temperatures, creating an artificial illusion of high series resistance, but also makes it highly susceptible to piercing the noble metal electrode layer, which is only a few hundred nanometers thick, during the high-temperature expansion phase. Based on the above failure mechanism, the temperature control platform module 102 also includes a dynamic stress-relieving electrical probe assembly.

[0099] The dynamic stress relief electrical probe assembly eliminates eigenvalue fluctuations in contact impedance through a closed-loop feedback topology of electromechanical coupling. The hardware architecture of the dynamic stress relief electrical probe assembly mainly consists of a piezoelectric ceramic actuator, a miniature force sensor based on the piezoresistive effect of microelectromechanical systems (MEMS), and a four-wire Kelvin probe made of gold-plated beryllium copper. The four-wire Kelvin probe is independently micro-displaced by the piezoelectric ceramic actuator along the Z-axis perpendicular to the sample surface. Physically, the cantilever of the four-wire Kelvin probe is rigidly connected to the force-bearing surface of the miniature force sensor to capture millinewton-level contact stress changes non-destructively.

[0100] During the execution of a programmed temperature cycling light test sequence, the miniature force sensor... The actual contact pressure between the four-wire Kelvin probe and the sample surface electrode is continuously acquired at a high sampling rate. The acquired analog millivolt signal is conditioned by a high-frequency chopper amplifier and then input to the electronic control and data module. The electronic control and data module internally runs a customized adaptive feedforward and PID composite servo algorithm. This algorithm uses the contact pressure error fed back by the miniature force sensor as the input to the PID controller, combined with real-time temperature difference... The calculated feedforward compensation terms are used to generate the displacement command. When the ambient temperature changes from... sudden drop At that moment, the oxygen-free copper stage 105 undergoes cooling and contraction. The miniature force sensor instantly detects that the actual contact pressure has disengaged from the target envelope region. The control software immediately calculates the displacement compensation and outputs a response time less than [time value missing]. The high-voltage analog signal is sent to the piezoelectric ceramic actuator, which drives the four-wire Kelvin probe to approach downwards to compensate for the lost contact pressure.

[0101] The deformation compensation mechanism relies on a rigorous mathematical model, and the displacement compensation amount The control satisfies the formula:

[0102]

[0103] in, The displacement compensation amount of the piezoelectric ceramic actuator is given by [missing information - likely a unit], where the unit of displacement compensation is [missing information - likely a unit]. ; The preset constant target contact pressure, the unit of which is... ; The actual contact pressure is monitored in real time by the miniature force sensor, and the unit of actual contact pressure is... ; The equivalent stiffness coefficient of the cantilever structure containing the four-wire Kelvin probe is given by [insert value here]. The unit of the equivalent stiffness coefficient is [insert value here]. ; The coefficient of thermal expansion of the dynamic stress relief electrical probe assembly is given by [reference to a specific parameter, which is missing from the original text]. The unit of the coefficient of thermal expansion is [reference to a specific parameter, which is missing from the original text]. ; This represents the temperature difference between the current real-time temperature and the initial calibration temperature, with the unit of temperature difference being... ; The effective reference length of the dynamic stress relief electrical probe assembly along the Z-axis is given by [insert unit here]. .

[0104] The first term on the right side of the formula constitutes a force-based pure feedback control logic, which is responsible for suppressing transient mechanical disturbances; the second term on the right side of the formula is a feedforward control logic based on temperature parameters, which is used to offset the slow drift caused by the inherent thermal expansion of the system in advance, thereby weakening the inherent hysteresis nonlinear effect of the piezoelectric ceramic actuator from the source.

[0105] To ensure the absolute accuracy of system control parameters, the electrical control and data module forcibly executes the system calibration subroutine before loading the sample. Static load-displacement testing is performed on the four-wire Kelvin probe cantilever using an external laser interferometer to extract... The actual physical values ​​are obtained. The temperature control base module 102 is driven to perform an unloaded full-temperature range scan, recording the thermal displacement under deformation constraint conditions, and the results are fitted to obtain... A precise baseline curve was obtained. A set of comparative peeling experiments was designed to address the electrical compensation mechanism. Perovskite solar cells from the same batch were subjected to both conventional fixed probes (static) and dynamic stress-relief electrical probe assemblies. The short-circuit current and series resistance characteristic parameters were recorded in real time during the space thermal vacuum alternating test. The data are shown in Table 3.

[0106] Table 3 Comparison of contact resistance and device performance of conventional fixed probe and dynamic stress relief electrical probe assemblies under wide temperature range alternation;

[0107] Test loop node probe mode Contact pressure (mN) Measured value of series resistance ( ) Maximum power point efficiency deviation rate (%) 1st cycle ( ) Conventional fixed probe (static) 12.4 18.5 -15.2 1st cycle ( ) Dynamic stress relief electrical probe assembly 50.1 3.2 -1.1 50th cycle ( ) Conventional fixed probe (static) 145.8 (Electrode puncture occurred) 45.6 -42.8 50th cycle ( ) Dynamic stress relief electrical probe assembly 49.8 3.5 -2.3 100th cycle ( ) Conventional fixed probe (static) 0 (Disconnection) Polarization Opening Test failed 100th cycle ( ) Dynamic stress relief electrical probe assembly 50.0 3.8 -3.5

[0108] A conventional fixed probe (static) punctured the surface electrode due to extremely high contact stress during the 50th high-temperature cycle and completely lost electrical connection during the 100th low-temperature cycle. The dynamic stress-relieving electrical probe assembly uses micron-level servo technology to converge the contact pressure dead zone within... The nearby location ensures that the extracted photoelectric data fully reflects the physical nature of the device material's attenuation.

[0109] Parallel to the mechanical damage to the probe is the breaking of chemical bonds induced by vacuum photothermal stress, which is the core microscopic lesion leading to the decomposition of perovskite in the space environment. To extend the degradation kinetics from macroscopic electrical characterization to molecular-scale mass tracking, an in-situ quadrupole mass spectrometer was connected to the flange sidewall of the single-chamber structure.

[0110] A conical sampling funnel, wound with armored heating wire, was added to the front end of the in-situ quadrupole mass spectrometer. Due to the vapor pressure characteristics of common degradation products such as iodides, these products readily undergo irreversible sublimation on the cold surface near the water-cooled wall. The conical sampling funnel physically approaches the sample surface to within only [distance missing]. At the location, and maintained at throughout the experiment. In an isothermal state, the heating power of the armored heating wire is PID-regulated by the electronic control and data module based on feedback from the thermocouple integrated on the sampling funnel, establishing a dedicated collection channel for molecular flow that repels condensation. The in-situ quadrupole mass spectrometer is internally equipped with... An electron bombardment ionization source is connected in series with a Faraday cup detector to achieve highly sensitive capture of trace components.

[0111] Throughout the experiment, the electronic control and data modules used a timestamp clock generator to force the synchronization of photoelectric testing and mass spectrometry data. When the light source module 103 projected the AMO spectrum onto the sample, the in-situ quadrupole mass spectrometer simultaneously started continuous scanning mode, focusing on the mass-to-charge ratio. hydrogen iodide molecules and mass-to-charge ratio Characteristic fragment peaks such as methyl iodide. Due to the long-term state of the single-cavity structure... In the molecular flow region, the mean free path of gas molecules desorbing from the sample surface to the ion source is much larger than the geometric dimensions of the single-cavity structure, thus eliminating secondary recombination interference caused by gas phase collisions.

[0112] The electronic control and data module incorporates a degradation kinetics solver to extract the ion current intensity of the characteristic mass-to-charge ratio and calculate the in-situ volatilization rate of the target degradation products. The calculation formula is:

[0113]

[0114] in, The in-situ volatilization rate of the target degradation products is calculated in real time, and the unit of the in-situ volatilization rate of the target degradation products is... ; The effective pumping speed of the vacuum system module 104 for the specific target degradation product under the current vacuum level is given by [missing information - likely a unit of measurement]. ; This refers to the instrument sensitivity coefficient of the in-situ quadrupole mass spectrometer for a specific mass-to-charge ratio, with the unit of the instrument sensitivity coefficient being [missing information]. ; This refers to the intensity of a continuously acquired ion current with a specific mass-to-charge ratio. The unit of this intensity is... ; Let $\mathbf{a}$ be the ideal gas constant, and the unit of the ideal gas constant is $\mathbf{a}$. ; The absolute temperature is the temperature of the gas inside the single-cavity structure. This absolute temperature is approximately taken as the real-time temperature output by the temperature control base module 102, and the unit of absolute temperature is... Effective pumping speed Obtained by interpolation of the compression ratio curve of a specific gas using a molecular pump. Instrument sensitivity coefficient. Before the equipment was put into operation, calibration was completed by injecting a standard gas with a known leak rate into the vacuum chamber module 101, thus eliminating the interference of geometric topography factors on the conductance calculation.

[0115] For the use of FA0. 85 MA0. 15 Perovskite samples in a PbI3 mixed cation system were subjected to [further processing]. Steady-state light irradiation and thermal vacuum coupled aging test. The ambient reference temperature was kept constant at... The electronic control and data module not only outputs macroscopic data... - The decay curve trend is further mapped to the loss flux of organic cations and halogen anions with a microsecond delay. The corresponding decay relationships are extracted and shown in Table 4.

[0116] Table 4 Mixed cationic perovskites in Multidimensional degradation mapping data under high vacuum conditions / AM0 /

[0117] Aging time (h) - Efficiency retention rate (%) hydrogen iodide ( ) (mol / s) Methyl iodine ( ) (mol / s) Integrated photoelectric-volatile correlation characteristics 10 98.2 The residual solvent adsorbed on the surface desorbed slowly, and PCE did not show a trend of decline. 40 85.5 Localized dehalogenation occurs at the grain boundaries, and the short-circuit current begins to roll off. 70 68.3 The surge in iodine vacancies within the crystal lattice leads to an exponential deterioration in the in-situ volatilization rate. 100 45.1 #imgpt255# <![CDATA[The perovskite phase undergoes macroscopic phase separation into PbI₂, leading to severe device failure]]>

[0118] The correlation data between microscopic gas generation rate and macroscopic photoelectric efficiency show that, at the 40-hour aging stage, the evaporation rate of the mass-to-charge ratio (#imgpt256#) exceeds the order of magnitude of #imgpt257#, at which point the efficiency retention rate (#imgpt258#-#imgpt259#) transitions from a stable period to a steep decline. The halogen escape events detected by the in-situ quadrupole mass spectrometer are perfectly time-sequential and slightly precede the significant deterioration of electrical parameters. This forward-looking molecular-level detection capability compensates for the technical blind spot of relying solely on current-voltage curves, which can only obtain lagging data.

[0119] During rapid temperature transitions from extreme cold to high temperatures, the aerodynamic balance within the single-chamber structure is highly sensitive. The in-situ quadrupole mass spectrometer and its internal Fail-Safe state machine logic within the electrical control and data modules construct a deep safety interlock system. In addition to monitoring the macroscopic total pressure signal from the full-range vacuum gauge, the Fail-Safe state machine continuously scans the partial pressure derivatives of each component calculated by the mass analyzer. If a localized hot spot induced by the heating unit causes explosive decomposition of the sample, the in-situ evaporation rate of the target degradation product will undergo a step-like change within tens of milliseconds, exceeding the preset abnormal threshold. Upon detecting the abnormal rising edge, the system immediately bypasses the conventional temperature change waiting sequence and directly triggers the microsecond-level self-locking of the vent valve within the vacuum system module 104. Simultaneously, it instructs the piezoelectric ceramic actuator to rise along the Z-axis to physically disengage the electrical contact. The response speed of this microscopic ion flow-triggered safety defense mechanism is at least two orders of magnitude faster than conventional macroscopic total pressure leak detection and warning systems.

[0120] Because both power outages and protective actions are time-stamped at the atomic clock level, retrieving instantaneous data packets stored in the non-volatile memory allows for the reconstruction of the entire logical chain from the initiation of internal material decomposition, surface electrode rupture, to macroscopic failure with frame-level precision. The safety defense mechanism protects the optical window of the core of the integrated perovskite solar cell space environment simulation in-situ testing device from severe contamination by high-concentration iodine vapor, and transforms failed tests into experimental specimens reflecting ultimate stress responses. The testing architecture decouples multiple physics fields, utilizes the feedback network of the dynamic stress release electrical probe assembly to suppress contact distortion caused by mechanical deformation, and then uses the fluid channel of the in-situ quadrupole mass spectrometer to establish a monitoring model for chemical decomposition.

[0121] Although preferred embodiments of the invention have been described, those skilled in the art, upon learning the basic inventive concept, can make other changes and modifications to these embodiments. Therefore, the appended claims are intended to be interpreted as including both the preferred embodiments and all changes and modifications falling within the scope of the invention.

[0122] The above description is merely a preferred embodiment of the present invention and is not intended to limit the present invention. It should be noted that any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention should be included within the protection scope of the present invention.

Claims

1. An integrated perovskite solar cell space environment simulation in-situ detection device, characterized in that, include: A vacuum chamber module, wherein the vacuum chamber module is a single-chamber structure, and the vacuum chamber module is used to maintain a high vacuum environment; A temperature-controlled stage module, integrated within the single-cavity structure, is used to apply pressure to a sample placed on the temperature-controlled stage module. to Programmed temperature cycling within the range; The light source module includes a sunlight simulator, which is used to apply AMO spectral illumination to the sample through the optical window of the vacuum cavity module; A vacuum system module, connected to the vacuum chamber module, is used to evacuate the single-chamber structure to the ultimate vacuum level. The electrical control and data module is used to perform closed-loop control of the temperature control platform module, the light source module and the vacuum system module, and to simultaneously collect the photoelectric performance data and environmental parameters of the sample.

2. The integrated perovskite solar cell space environment simulation in-situ detection device according to claim 1, characterized in that, The vacuum chamber module has a stainless steel chamber, the inner wall of which is treated with a low outgassing rate blackening process, and the surface emissivity of the inner wall of the stainless steel chamber is not less than [value missing]. And the outgassing rate of the inner wall of the stainless steel cavity is not greater than .

3. The integrated perovskite solar cell space environment simulation in-situ detection device according to claim 1, characterized in that, The optical window is made of quartz glass and is equipped with a double-sided anti-reflective coating. to The optical transmittance of the optical window within the specified band is not less than Furthermore, the optical window is flexibly connected to the vacuum cavity module through an elastic sealing structure.

4. The integrated perovskite solar cell space environment simulation in-situ detection device according to claim 1, characterized in that, A spectral filter element is disposed between the light source module and the optical window. The spectral filter element is used to reflect or absorb wavelengths greater than [a certain value]. Infrared thermal radiation, and only through to Spectral bands.

5. The integrated perovskite solar cell space environment simulation in-situ detection device according to claim 1, characterized in that, The temperature control base module includes a stage, a heating unit, and a cooling unit; the stage is made of high thermal conductivity oxygen-free copper, and the surface of the stage is blackened.

6. The integrated perovskite solar cell space environment simulation in-situ detection device according to claim 5, characterized in that, The refrigeration unit is a Stirling refrigerator, and the refrigeration unit is connected to the stage through a vibration damping coupling structure to suppress the transmission of mechanical vibration to the sample.

7. The integrated perovskite solar cell space environment simulation in-situ detection device according to claim 5, characterized in that, A thermal resistance adjustment layer is provided between the back of the stage and the cold head of the refrigeration unit. The thermal resistance adjustment layer is a tungsten copper alloy gasket, which is used to introduce fixed thermal resistance and prevent the heat of the heating unit from being short-circuited away by the refrigeration unit under low temperature conditions.

8. The integrated perovskite solar cell space environment simulation in-situ detection device according to claim 5, characterized in that, The stage has a built-in multi-zone independent temperature control loop, which is used to control the temperature uniformity of the stage surface through zoned PID regulation.

9. A method for in-situ detection of integrated perovskite solar cells in space environment simulation, comprising using an integrated perovskite solar cell in-situ detection device for space environment simulation as described in any one of claims 1-8, characterized in that, Includes the following steps: The sample is placed on the temperature-controlled base module inside the vacuum chamber module; The vacuum system module evacuates the single-cavity structure of the vacuum chamber module to a vacuum level not exceeding [a certain threshold]. After the vacuum level stabilizes, the temperature control base module is controlled to operate according to a preset program. to Temperature changes within a certain range; After reaching a steady state at a preset temperature node, the light source module is controlled to apply AMO spectral illumination to the sample through the optical window; The current-voltage curve and maximum power point tracking steady-state data of the sample are acquired synchronously using the electronic control and data module.

10. The method for in-situ detection of integrated perovskite solar cells in space environment simulation according to claim 9, characterized in that, The temperature control platform module also includes a dynamic stress relief electrical probe assembly; the dynamic stress relief electrical probe assembly includes a piezoelectric ceramic actuator, a miniature force sensor, and a four-wire Kelvin probe; the four-wire Kelvin probe is independently driven by the piezoelectric ceramic actuator along the Z-axis direction perpendicular to the sample; the miniature force sensor is connected in a closed loop with the electrical control and data module to monitor the actual contact pressure between the four-wire Kelvin probe and the surface electrode of the sample in real time; The electrical control and data module is used to output displacement compensation commands to the piezoelectric ceramic actuator in real time according to the actual contact pressure, so that in the to During temperature cycling, the actual contact pressure remains at the preset constant target contact pressure, and the displacement compensation amount... The control satisfies the formula: in, The displacement compensation amount of the piezoelectric ceramic actuator is given by [missing information - likely a unit], where the unit of displacement compensation is [missing information - likely a unit]. ; The preset constant target contact pressure, the unit of which is... ; The actual contact pressure is monitored in real time by the miniature force sensor, and the unit of actual contact pressure is... ; The equivalent stiffness coefficient of the cantilever structure containing the four-wire Kelvin probe is given by [formula missing]. The unit of the equivalent stiffness coefficient is [formula missing]. ; The coefficient of thermal expansion of the dynamic stress relief electrical probe assembly is given by [reference to a specific parameter, which is missing from the original text]. The unit of the coefficient of thermal expansion is [reference to a specific parameter, which is missing from the original text]. ; This represents the temperature difference between the current real-time temperature and the initial calibration temperature, with the unit of temperature difference being... ; The effective reference length of the dynamic stress relief electrical probe assembly along the Z-axis is given by [reference length unit]. .