A dual-mode detector based on 4H-SiC NWAs / GO heterojunction and its fabrication method
By using a dual-mode detector based on 4H-SiC NWAs/GO heterojunction, combining ultraviolet absorption and electromagnetic sensing functions, adaptive detection of ultraviolet light signals and electromagnetic pulse signals is achieved. This solves the problem of discrete device detection in existing technologies, meets the low power consumption and miniaturization requirements of smart grids, and is suitable for arc monitoring in complex environments.
Patent Information
- Application Number
- CN202611058898.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-07-16
- Publication Date
- 2026-11-10
AI Technical Summary
In existing power equipment, the separate detection scheme of ultraviolet detector and electromagnetic detector increases the system size and cost, and it is difficult to meet the requirements of smart grid for device miniaturization, low power consumption and high reliability. In particular, the detection performance degrades in optically obstructed environments such as enclosed switch cabinets.
A dual-mode detector based on 4H-SiC NWAs/GO heterojunction was constructed, combining the ultraviolet absorption characteristics of 4H-SiC nanowire array with the electromagnetic sensing function of graphene oxide film. This system enables adaptive detection of ultraviolet light signals and electromagnetic pulse signals.
It can detect ultraviolet signals with high sensitivity in unobstructed environments and automatically switch to electromagnetic pulse detection mode in optically obstructed environments. It meets the requirements of low power consumption and compactness, and has excellent repeatability and thermal stability, making it suitable for arc monitoring in complex environments.
Smart Images

Figure CN123076102A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of semiconductor optoelectronic devices and electromagnetic sensing technology, and relates to a method based on 4H Dual-mode detector of SiC NWAs / GO heterojunction and its fabrication method. Background Technology
[0002] During the operation of power equipment, factors such as insulation aging, poor contact, and partial discharge can easily induce weak arc discharge. Arc discharge not only generates deep ultraviolet radiation but is also accompanied by the release of broadband transient electromagnetic pulses. Therefore, highly sensitive detection of these two types of signals is an important technical means to achieve early warning of power equipment faults.
[0003] Currently, ultraviolet (UV) detection is widely used in arc detection due to its solar blindness and resistance to visible light interference. However, when an arc occurs in enclosed switchgear, gas-insulated metal-enclosed switchgear (GIS), or other environments with optical obstructions, UV signal transmission is hindered, and detection performance significantly degrades. In contrast, the electromagnetic pulse released by an arc has strong medium-penetrating ability, enabling non-contact detection under obstructed conditions. However, existing electromagnetic detectors typically rely on independent antennas and dedicated signal processing circuits, resulting in complex structures, low integration, and susceptibility to environmental noise interference.
[0004] Currently, most engineering projects employ a separate detection approach using ultraviolet (UV) and electromagnetic (EMI) detectors, with backend fusion. This not only increases system size and manufacturing costs but also fails to meet the requirements of smart grids for miniaturized devices, low power consumption, and high reliability. Therefore, developing an integrated dual-mode detector that combines UV and EMI detection capabilities is of great significance for improving the reliability and adaptability of arc monitoring in complex environments. Summary of the Invention
[0005] To address the aforementioned technical problems and deficiencies, this invention provides a method based on... 4H Dual-mode detector of SiC NWAs / GO heterojunction and its fabrication method.
[0006] In a first aspect, the present invention provides a method based on 4H A dual-mode detector based on a SiC NWAs / GO heterojunction, wherein the dual-mode detector is provided with an ITO transparent conductive glass substrate, and a PEDOT hole transport layer sequentially disposed on the ITO transparent conductive glass substrate. 4H -SiC nanowire array, graphene oxide film, silver electrode.
[0007] Specifically, the PEDOT hole transport layer and 4H- The SiC nanowire array forms a heterojunction with a built-in electric field to separate photogenerated carriers generated by ultraviolet light irradiation; the graphene oxide film forms a Schottky contact with the metal electrode and together with the ITO transparent conductive glass substrate, it constitutes a broadband electromagnetic sensing structure, enabling the dual-mode detector to respond to ultraviolet light signals and electromagnetic pulse signals respectively, thus achieving dual-mode adaptive detection.
[0008] Furthermore, based on the present invention... 4H In the dual-mode detector of SiC NWAs / GO heterojunction, the 4H -SiC nanowire array 4H -SiC nanowires have a length of 2~6μm and a diameter of 50~200nm;
[0009] The thickness of the graphene oxide film is 100~200nm.
[0010] Furthermore, based on the present invention... 4H In the dual-mode detector of SiC NWAs / GO heterojunction, the thickness of the PEDOT hole transport layer is 100~300nm. The thickness of the silver electrode is 80~150nm.
[0011] Secondly, the present invention provides a method based on 4H The fabrication method of a dual-mode detector for SiC NWAs / GO heterojunction includes: cleaning n-type 4H -SiC single crystal wafer, after pretreatment 4H -SiC single crystal wafer; pretreated by electrochemical etching method 4H -SiC single crystal wafer, to obtain 4H -SiC nanowire array; graphene oxide dispersion was filtered by vacuum filtration to obtain graphene oxide film; ITO transparent conductive glass substrate coated with PEDOT:PSS was subjected to ultraviolet ozone treatment. 4H -SiC nanowire arrays were transferred onto the surface of PEDOT:PSS, and after hot pressing, graphene oxide films were transferred and coated onto the surface. 4H A dual-mode detector is obtained by depositing silver electrodes on a SiC nanowire array using acetone film, followed by vacuum annealing and thermal evaporation.
[0012] Furthermore, based on the present invention... 4H In the fabrication method of the dual-mode detector of SiC NWAs / GO heterojunction, the electrochemical etching method includes: using a graphite plate as the cathode, a mixture of HF, C2H5OH and H2O2 as the electrolyte, and etching with pulsed constant current.
[0013] Furthermore, based on the present invention...4H In the preparation method of the dual-mode detector of SiC NWAs / GO heterojunction, the volume ratio of HF, C2H5OH and H2O2 is 2~4:5~7:0.5~2; The etching current is 0.05~0.20A, and the etching time is 20~30min.
[0014] Furthermore, based on the present invention... 4H In the preparation method of the dual-mode detector of SiC NWAs / GO heterojunction, the mass concentration of the graphene oxide dispersion is 0.04~0.1 mg / mL.
[0015] Furthermore, based on the present invention... 4H In the fabrication method of the dual-mode detector of SiC NWAs / GO heterojunction, the hot pressing treatment is carried out at a temperature of 100~200℃, a pressure of 0.1~3MPa, and a time of 20~40min.
[0016] Furthermore, based on the present invention... 4H In the method for fabricating a dual-mode detector of SiC NWAs / GO heterojunction, the vacuum annealing temperature is 200~350℃ and the time is 2~3h.
[0017] Thirdly, the present invention provides a basis 4H The application of dual-mode detectors for SiC NWAs / GO heterojunctions, wherein the dual-mode detectors are used for fault monitoring and early warning of power equipment, the applications include at least one of the following: power equipment arc monitoring, partial discharge monitoring, electromagnetic pulse detection, fault diagnosis of enclosed switchgear, status monitoring of gas-insulated metal-enclosed switchgear, and industrial arc early warning.
[0018] Compared with the prior art, the technical solution provided by the present invention has at least the following beneficial effects or advantages: (1) The present invention will 4H -SiC nanowire array ( 4H The solar-blind ultraviolet absorption characteristics of SiC NWAs are combined with the dielectric loss characteristics of its one-dimensional structure to integrate ultraviolet detection and electromagnetic pulse detection functions in a single device. Based on this, the device can detect ultraviolet signals with high sensitivity in unobstructed environments and automatically switch to electromagnetic pulse detection mode in optically obstructed environments without the need for mechanical or electrical switches. This overcomes the limitation of discrete sensors that cannot adaptively switch, and significantly broadens the application scenarios in complex environments.
[0019] (2) This invention constructs PEDOT / 4HThe synergistic system of SiC nanowire array pn heterojunction and graphene oxide / silver Schottky junction enables self-powered ultraviolet detection under zero or low bias voltage; simultaneously, non-line-of-sight detection of electromagnetic pulses is achieved through a rectified antenna mechanism. Both modes share the same device architecture; the ultraviolet mode requires no external bias voltage, while the electromagnetic mode consumes only nanowatts to microwatts, fully meeting the stringent requirements of low power consumption and compactness for distributed nodes in smart grids.
[0020] (3) The vertically arranged in this invention 4H The SiC nanowire array provides a large specific surface area and a light trapping effect, enhancing light absorption and improving ultraviolet detection efficiency while effectively attenuating incident electromagnetic waves through polarization relaxation and multiple scattering mechanisms. The graphene oxide film simultaneously serves as a charge transport layer and a key component of the antenna. This multi-interface design enables the device to operate reliably even under conditions of optical obstruction and complex electromagnetic environments, such as enclosed switchgear. Stability tests showed that the device maintained a highly consistent response signal over multiple ultraviolet / electromagnetic pulse cycles and a temperature range from room temperature to 100°C, exhibiting excellent repeatability and thermal stability.
[0021] (4) The preparation methods used in this invention (electrochemical etching, vacuum filtration, hot pressing, vacuum annealing, thermal evaporation deposition, etc.) are highly compatible with standard semiconductor processes, laying the technological foundation for device integration and miniaturization, and have good prospects for engineering transformation and promotion. Attached Figure Description
[0022] Figure 1 For based on 4H -Schematic diagram of the structure of a dual-mode detector for SiC NWAs / GO heterojunction.
[0023] Figure 2 For based on 4H A schematic diagram of the detection mechanism of the dual-mode detector of SiC NWAs / GO heterojunction. Among them, (a) is a schematic diagram of the electromagnetic signal detection mechanism; (b) is a schematic diagram of the dual-mode detection mechanism of ultraviolet light and electromagnetic signals; (c) is the response characteristics of the dual-mode detector to electric arc at different detection distances; and (d) is the detection result of dual-mode detection of ultraviolet light and electromagnetic signals. Detailed Implementation
[0024] The technical solution of the present invention will be described below with reference to embodiments. However, the present invention is not limited to the following embodiments. Unless otherwise specified, the experimental methods and detection methods described in each embodiment are conventional methods; unless otherwise specified, the reagents and materials can be purchased commercially.
[0025] Example 1 This embodiment provides a method based on 4HDual-mode detector of SiC NWAs / GO heterojunction and its fabrication method.
[0026] The embodiment described in this example is based on 4H -SiC NWAs / GO heterojunction dual-mode detector ( Figure 1 The substrate is provided with an ITO transparent conductive glass substrate, and a PEDOT hole transport layer is sequentially disposed on the ITO transparent conductive glass substrate. 4H -SiC nanowire array ( 4H -SiC NWAs), graphene oxide (GO) thin film, silver electrode.
[0027] The basis 4H The fabrication method of the dual-mode detector of SiC NWAs / GO heterojunction is as follows: S1. n-type 4H SiC single-crystal wafers were cut into 1cm × 1.5cm rectangles and ultrasonically cleaned sequentially in acetone, ethanol, and deionized water for 10 minutes each. Then, they were cleaned in a mixture of sulfuric acid and hydrogen peroxide (H₂SO₄:H₂O₂ = 3:1, v / v) for 10 minutes, followed by immersion in a 5% HF solution (volume concentration) for 2 minutes to remove the native oxide layer, yielding the pretreated wafer. 4H -SiC single crystal wafer.
[0028] S2. With pre-processed 4H Using a SiC single crystal wafer as the anode and a high-purity graphite plate as the cathode, a mixture of HF, C2H5OH, and H2O2 (HF:C2H5OH:H2O2=3:6:1, v / v / v) as the electrolyte, the pretreated substrate was etched under pulsed constant current (0.1A, pulse width 5s, interval 5s) at 25℃ and 300rpm stirring speed. 4H -SiC single crystal wafer 25 min, to obtain 4H -SiC nanowire array. After etching, rinse with deionized water. 4H -SiC nanowire arrays were then neutralized with 3wt% NaOH and dried with high-purity nitrogen to obtain vertical arrays with a length of 4μm and a diameter of 100nm. 4H -SiC nanowire array.
[0029] S3. Disperse 1 mL of 2 mg / mL graphene oxide aqueous solution in 50 mL of deionized water to obtain a graphene oxide dispersion; use a vacuum filtration device to filter the film through a 0.22 μm mixed cellulose ester filter membrane, and then vacuum dry for 24 h to obtain a self-supporting graphene oxide film (thickness of 150 nm).
[0030] S4. Treat the ITO transparent conductive glass coated with PEDOT:PSS (200nm thickness) with ultraviolet ozone for 10 minutes, then... 4H -SiC nanowire arrays were transferred onto the surface of PEDOT:PSS, hot-pressed at 200℃ and 0.2MPa for 20 min, and then covered with a graphene oxide film. 4H A mixed cellulose ester filter membrane was dissolved in acetone on a SiC nanowire array, then vacuum annealed at 200℃ for 2 hours (vacuum degree < 10 Pa), and a silver electrode (100 nm) was thermally evaporated and deposited on the surface of the graphene oxide film to obtain a dual-mode detector.
[0031] Example 2 This embodiment provides a method based on 4H Dual-mode detector of SiC NWAs / GO heterojunction and its fabrication method.
[0032] The embodiment described in this example is based on 4H The dual-mode detector of the SiC NWAs / GO heterojunction is provided with an ITO transparent conductive glass substrate and a PEDOT hole transport layer sequentially disposed on the ITO transparent conductive glass substrate. 4H -SiC nanowire array, graphene oxide film, silver electrode.
[0033] The basis 4H The fabrication method of the dual-mode detector of SiC NWAs / GO heterojunction is as follows: S1. n-type 4H SiC single-crystal wafers were cut into 1cm × 1.5cm rectangles and ultrasonically cleaned sequentially for 5 minutes each in acetone, ethanol, and deionized water. Then, they were cleaned for 5 minutes in a mixture of sulfuric acid and hydrogen peroxide (H₂SO₄:H₂O₂ = 3:1, v / v), followed by immersion in a 3% HF solution (volume concentration) for 5 minutes to remove the native oxide layer, yielding the pretreated wafer. 4H -SiC single crystal wafer.
[0034] S2. With pre-processed 4H Using a SiC single crystal wafer as the anode and a high-purity graphite plate as the cathode, a mixture of HF, C2H5OH, and H2O2 (HF:C2H5OH:H2O2=3:6:1, v / v / v) as the electrolyte, the pretreated substrate was etched under pulsed constant current (0.1A, pulse width 5s, interval 5s) at 25℃ and 300rpm stirring speed. 4H -SiC single crystal wafer 20 min, to obtain 4H -SiC nanowire array. After etching, rinse with deionized water. 4H -SiC nanowire array, then neutralized with 5wt% NaOH and dried with high-purity nitrogen to obtain a vertical4H -SiC nanowire array.
[0035] S3. Disperse 1 mL of 5 mg / mL graphene oxide aqueous solution in 50 mL of deionized water to obtain a graphene oxide dispersion; use a vacuum filtration device to filter the film through a 0.22 μm mixed cellulose ester filter membrane, and then vacuum dry for 24 h to obtain a self-supporting graphene oxide film (thickness of 140 nm).
[0036] S4. Treat the ITO transparent conductive glass coated with PEDOT:PSS (thickness 300nm) with ultraviolet ozone for 15 minutes, then... 4H -SiC nanowire arrays were transferred onto the surface of PEDOT:PSS, hot-pressed at 100℃ and 3.0MPa for 40 min, and then covered with a graphene oxide film. 4H A mixed cellulose ester filter membrane was dissolved in acetone on a SiC nanowire array, then vacuum annealed at 300℃ for 3h (vacuum degree <10Pa), and a silver electrode (100nm) was thermally evaporated and deposited on the surface of the graphene oxide film to obtain a dual-mode detector.
[0037] Example 3 This embodiment provides a method based on 4H Dual-mode detector of SiC NWAs / GO heterojunction and its fabrication method.
[0038] The embodiment described in this example is based on 4H The dual-mode detector of the SiC NWAs / GO heterojunction is provided with an ITO transparent conductive glass substrate and a PEDOT hole transport layer sequentially disposed on the ITO transparent conductive glass substrate. 4H -SiC nanowire array, graphene oxide film, silver electrode.
[0039] The basis 4H The fabrication method of the dual-mode detector of SiC NWAs / GO heterojunction is as follows: S1. n-type 4H SiC single-crystal wafers were cut into 1cm × 1.5cm rectangles and ultrasonically cleaned sequentially for 5 minutes each in acetone, ethanol, and deionized water. Then, they were cleaned for 5 minutes in a mixture of sulfuric acid and hydrogen peroxide (H₂SO₄:H₂O₂ = 3:1, v / v), followed by immersion in a 5% HF solution (volume concentration) for 2 minutes to remove the native oxide layer, resulting in pretreated wafers. 4H -SiC single crystal wafer.
[0040] S2. With pre-processed 4HUsing a SiC single crystal wafer as the anode and a high-purity graphite plate as the cathode, a mixture of HF, C2H5OH, and H2O2 (HF:C2H5OH:H2O2=3:6:1, v / v / v) was used as the electrolyte. The pretreated substrate was etched under pulsed constant current (0.1A, pulse width 5s, interval 5s) at 30℃ and 500rpm stirring speed. 4H -SiC single crystal wafer 25 min, to obtain 4H -SiC nanowire array. After etching, rinse with deionized water. 4H -SiC nanowire array, then neutralized with 5wt% NaOH and dried with high-purity nitrogen to obtain a vertical 4H -SiC nanowire array.
[0041] S3. Disperse 1 mL of 3 mg / mL graphene oxide aqueous solution in 50 mL of deionized water to obtain a graphene oxide dispersion; use a vacuum filtration device to filter the film through a 0.22 μm mixed cellulose ester filter membrane, and then vacuum dry for 24 h to obtain a self-supporting graphene oxide film (thickness of 150 nm).
[0042] S4. Treat the ITO transparent conductive glass coated with PEDOT:PSS (250nm thickness) with ultraviolet ozone for 10 minutes, then... 4H -SiC nanowire arrays were transferred onto the surface of PEDOT:PSS, hot-pressed at 200℃ and 0.1MPa for 300 min, and then covered with a graphene oxide film. 4H A mixed cellulose ester filter membrane was dissolved in acetone on a SiC nanowire array, then vacuum annealed at 200℃ for 2 hours (vacuum degree < 10 Pa), and a silver electrode (100 nm) was thermally evaporated and deposited on the surface of the graphene oxide film to obtain a dual-mode detector.
[0043] 1. Detection performance under ultraviolet light: At room temperature (25℃), 254nm ultraviolet light (power density of 67mW / cm²) was used. 2 (with a bias voltage of 1V) Irradiates the dual-mode detector.
[0044] The dual-mode detector prepared in Example 1 exhibits stable ultraviolet light response performance, rapidly generating a significant photocurrent signal during ultraviolet light irradiation. The response time is approximately 0.68 s, the recovery time is approximately 1.26 s, and the detectivity reaches 10-1. 9 Jones's level ( Figure 2 (d)). The devices prepared in Examples 2 and 3 also exhibited good ultraviolet detection performance, and their response characteristics were basically the same as those in Example 1, indicating that the dual-mode detector structure provided by the present invention has good process repeatability and stability.
[0045] To evaluate the operational stability of the dual-mode detector under different ambient temperatures, the device prepared in Example 1 was placed in a temperature-controlled chamber and kept at 50 ℃, 70 ℃, and 100 ℃ for 30 min before testing. The results showed that as the ambient temperature increased, the dark current of the dual-mode detector increased slightly, but the photocurrent changed little, and the photoresponse remained stable. This indicates that the dual-mode detector provided by this invention has good thermal stability and can meet the long-term monitoring needs of power equipment under complex operating conditions. Furthermore, as... Figure 2 As shown in (a), when the dual-mode detector is illuminated by 254 nm ultraviolet light, 4H -SiC nanowire arrays absorb photons to generate electron-hole pairs. (In PEDOT:PSS / ) 4H Under the influence of the built-in electric field of the SiC nanowire array pn heterojunction, photogenerated electrons migrate toward the ITO transparent conductive glass, while photogenerated holes migrate toward PEDOT:PSS and graphene oxide, thereby forming a stable photocurrent in the external circuit and realizing the detection of ultraviolet light.
[0046] 2. Electromagnetic Pulse Detection Performance: Under room temperature conditions (bias voltage of 1 V, distance of 1 cm), broadband transient electromagnetic pulses were generated using a standard switched arc discharge platform. The electromagnetic pulse detection performance of the dual-mode detectors prepared in Examples 1-3 was tested. The electromagnetic pulse detection time of Example 1 was 0.96 s (… Figure 2 In Example 2 (d), the electromagnetic pulse detection time was 1.2 s, and in Example 3, the electromagnetic pulse detection time was 0.98 s. During the tests, the distance between the dual-mode detector and the arc source was set to 1 cm, 5 cm, 30 cm, 60 cm, etc. Figure 2 As shown in (c), within the above detection distance range, the dual-mode detector can detect obvious electromagnetic response signals. As the detection distance increases, the amplitude of the output signal gradually decreases, but still maintains a good signal-to-noise ratio and stability.
[0047] To evaluate the anti-obstruction capability of the dual-mode detector, different obstructions, such as cardboard, plastic sheets, and metal mesh, were placed between the arc source and the detector. Test results show that under various obstruction conditions, the dual-mode detector can still stably detect the broadband transient electromagnetic pulse signal generated by the arc discharge, indicating that the dual-mode detector proposed in this invention has good anti-optical obstruction capability and is suitable for arc monitoring in enclosed switchgear and other complex environments. Figure 2As shown in (b), when ultraviolet light cannot reach the detector, the broadband transient electromagnetic pulse generated by the arc discharge is first sensed by the broadband electromagnetic receiving structure composed of an ITO transparent conductive glass substrate, a graphene oxide film and a metal electrode. Then, it is rectified at the Schottky contact formed by the graphene oxide / metal electrode and converted into a detectable electrical signal, thus realizing stable detection of the electromagnetic pulse.
[0048] 3. Dual-mode detection of ultraviolet light and electromagnetic pulse: A dual-mode detector was installed in a simulated enclosed switch cabinet to test its adaptive dual-mode performance under real optical shielding conditions. The switch cabinet was a metal enclosed cabinet without optical windows. The dual-mode detector was fixed to the inner wall of the cabinet, and the data acquisition line was led out of the cabinet. An arc discharge device was installed on the outside of the cabinet. First, the cabinet door was closed to completely block ultraviolet radiation from the metal cabinet. The arc discharge device was then activated, and the dual-mode detector was able to stably output an electromagnetic pulse response signal. Subsequently, the cabinet door was opened, and the device was irradiated with 254 nm ultraviolet light. At this time, the dual-mode detector output a clear ultraviolet light response signal. After the cabinet door was closed again, the dual-mode detector resumed its response to the electromagnetic pulse signal. Throughout the test, there was no need to replace the dual-mode detector or adjust the detection circuit. Different types of output signals could be obtained simply by changing the external excitation conditions, such as... Figure 2 As shown in (d) above. Test results show that the dual-mode detector provided by this invention can achieve deep ultraviolet detection in an unobstructed environment and electromagnetic pulse detection in an optically obstructed environment. It has good environmental adaptability and detection reliability, and can meet the needs of online monitoring of arc discharge under complex working conditions.
[0049] Based on the physical mechanism of the dual-mode detector described above, this invention also provides a working mode identification method, which monitors the output signal amplitude of the dual-mode detector in real time through a matching signal processing circuit. When the signal amplitude is higher than a preset threshold, it is determined to be in ultraviolet detection mode, indicating the presence of arc discharge in an unobstructed environment; when the signal amplitude is lower than the preset threshold, it is determined to be in electromagnetic pulse detection mode, indicating the possible presence of arc discharge under optical obstruction conditions. The output signals of both working modes can be read through the same data acquisition channel, without the need for any mechanical or electrical switches, achieving true adaptive dual-mode switching.
[0050] The embodiments described above are some, but not all, of the embodiments of the present invention. The detailed description of the embodiments of the present invention is not intended to limit the scope of the claimed invention, but merely to illustrate selected embodiments of the invention. All other embodiments obtained by those skilled in the art through related deductions and substitutions based on the inventive concept, without inventive effort, are within the scope of protection of the present invention.
Claims
1. A method based on 4H A dual-mode detector based on a SiC NWAs / GO heterojunction, characterized in that... The dual-mode detector is provided with an ITO transparent conductive glass substrate, and a PEDOT hole transport layer sequentially disposed on the ITO transparent conductive glass substrate. 4H -SiC nanowire array, graphene oxide film, silver electrode.
2. The method based on claim 1 4H A dual-mode detector based on a SiC NWAs / GO heterojunction, characterized in that... The 4H -SiC nanowire array 4H -SiC nanowires have a length of 2~6μm and a diameter of 50~200nm; The thickness of the graphene oxide film is 100~200nm.
3. The method based on claim 1 4H A dual-mode detector based on a SiC NWAs / GO heterojunction, characterized in that... The thickness of the PEDOT hole transport layer is 100~300nm; The thickness of the silver electrode is 80~150nm.
4. A method based on any one of claims 1 to 3 4H The method for fabricating a dual-mode detector of a SiC NWAs / GO heterojunction is characterized by, include: Cleaning n-type 4H -SiC single crystal wafer, after pretreatment 4H -SiC single crystal wafer; Pre-treatment by electrochemical etching 4H -SiC single crystal wafer, to obtain 4H -SiC nanowire array; graphene oxide dispersion was filtered by vacuum filtration to obtain graphene oxide film; ITO transparent conductive glass substrate coated with PEDOT:PSS was subjected to ultraviolet ozone treatment. 4H -SiC nanowire arrays were transferred onto the surface of PEDOT:PSS, and after hot pressing, graphene oxide films were transferred and coated onto the surface. 4H A dual-mode detector is obtained by depositing silver electrodes on a SiC nanowire array using acetone film, followed by vacuum annealing and thermal evaporation.
5. The method based on claim 4 4H The method for fabricating a dual-mode detector of a SiC NWAs / GO heterojunction is characterized by, The electrochemical etching method includes: using a graphite plate as the cathode, a mixture of HF, C2H5OH and H2O2 as the electrolyte, and etching with pulsed constant current.
6. The method based on claim 5 4H The method for fabricating a dual-mode detector of a SiC NWAs / GO heterojunction is characterized by, The volume ratio of HF, C2H5OH and H2O2 is 2~4:5~7:0.5~2; The etching current is 0.05~0.20A, and the etching time is 20~30min.
7. The method based on claim 4 4H The method for fabricating a dual-mode detector of a SiC NWAs / GO heterojunction is characterized by, The mass concentration of the graphene oxide dispersion is 0.04~0.1 mg / mL.
8. The method based on claim 4 4H The method for fabricating a dual-mode detector of a SiC NWAs / GO heterojunction is characterized by, The hot pressing treatment is performed at a temperature of 100~200℃, a pressure of 0.1~3MPa, and a time of 20~40min.
9. The method based on claim 4 4H The method for fabricating a dual-mode detector of a SiC NWAs / GO heterojunction is characterized by, The vacuum annealing temperature is 200~350℃, and the time is 2~3h.
10. A method based on any one of claims 1 to 3 4H The application of dual-mode detectors in SiC NWAs / GO heterojunctions is characterized by... The dual-mode detector is used for fault monitoring and early warning of power equipment. The applications include at least one of the following: power equipment arc monitoring, partial discharge monitoring, electromagnetic pulse detection, fault diagnosis of enclosed switchgear, status monitoring of gas-insulated metal-enclosed switchgear, and industrial arc early warning.