A method for purifying actinium-225 based on electrospun membrane separation
By optimizing the three-stage nitric acid concentration gradient and flow rate parameters of the electrospun membrane module, the problems of long purification time and low purity of traditional DGA resin columns were solved, achieving rapid and efficient separation and purification of actinium-225, thus improving purification efficiency and product purity.
Patent Information
- Application Number
- CN202611446827.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-17
- Publication Date
- 2026-11-17
AI Technical Summary
In existing methods for purifying actinium-225, traditional DGA resin columns suffer from problems such as high mass transfer resistance, long purification time, risk of ligand leakage, and low purity, making it difficult to meet the needs of large-scale production and efficient purification.
An electrospun membrane-based separation method was adopted. By constructing a diethylene glycol amide-functionalized electrospun membrane module, a suitable three-segment nitric acid concentration gradient and flow rate parameters (4M-8M for loading, 4M-6M for washing, and 9M-11M for desorption) were built. High-flow-rate adsorption and selective washing were achieved by utilizing the convective mass transfer characteristics. Combined with the collection of a narrow actinium-225 fraction during desorption, rapid and efficient purification was achieved.
The purification time was shortened to less than 2 hours, the purification efficiency was increased by more than 3 times, the impurity ratio was reduced, and the purity and recovery rate of actinium-225 were improved, meeting the purity requirements of clinical actinium-225.
Smart Images

Figure CN123102148A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of separation and purification technology, and in particular to a method for separating and purifying actinium-225 based on electrospun membrane. Background Technology
[0002] Actinide-225 ( 225 Actinium-225 (Ac, with a half-life of 9.92 days) is a promising alpha-emitting medical isotope. Its decay chain releases four alpha particles, exhibiting high linear energy transfer and short tissue penetration distance, enabling precise killing of tumor cells. It holds significant clinical value in targeted alpha therapy for malignant tumors such as prostate cancer, breast cancer, and leukemia. However, the global supply of actinium-225 is severely insufficient, with an annual production of only about 1.7 curies, enough to meet the treatment needs of only about 100-200 patients. Large-scale production and efficient purification are currently the bottlenecks restricting its clinical application.
[0003] Currently, the mainstream purification method for actinium-225 uses chromatography columns packed with diethylene glycolamide (DGA) extraction resin. For example, CN120183769A discloses a method for separating and purifying actinium-225 by sequentially passing a radium target solution through a lead resin column and a DGA resin column; another patent, CN119410921A, discloses a method for separating actinium from an irradiated thorium target using a four-stage tandem separation and purification process: a cation exchange resin column, a UTEVA or TK200 resin extraction column, a DGA resin extraction column, and an LN resin extraction column.
[0004] However, traditional DGA resin column chromatography systems have the following technical drawbacks: the resin particles are porous spherical (50-100 μm in diameter), solute molecules need to diffuse into the internal pores of the particles to bind with the ligands, resulting in high mass transfer resistance, forcing the operation to use extremely low flow rates, and the purification time for a single sample can be as long as 6 hours or more; DGA ligands are usually physically adsorbed onto the resin, and there is a risk of ligand leakage during long-term use or high-flow-rate operation, which affects the purity of the product. Summary of the Invention
[0005] To address the aforementioned problems in the prior art, this invention provides a method for separating and purifying actinium-225 based on electrospun membrane.
[0006] In a first aspect, embodiments of this application provide a method for separating and purifying actinium-225 based on an electrospun membrane, comprising: obtaining a loading solution; wherein the loading solution is a nitric acid solution containing actinium-225 prepared by a natural thorium target; the nitric acid concentration of the loading solution is 4M to 8M; passing the loading solution through a diethylene glycol amide-functionalized electrospun membrane module at a flow rate of 0.5 to 2.0 mL / min for actinium-225 adsorption; passing a first nitric acid solution through the electrospun membrane module at a flow rate of 0.5 to 2.0 mL / min for washing and impurity removal; wherein the nitric acid concentration of the first nitric acid solution is 4M to 6M; passing a second nitric acid solution through the electrospun membrane module at a flow rate of 0.2 to 0.8 mL / min for desorption, and collecting 30% to 60% of the intermediate desorbate to obtain a separated and purified actinium-225 product solution; wherein the nitric acid concentration of the second nitric acid solution is 9M to 11M.
[0007] Optionally, collecting the intermediate 30% to 60% of the desorption liquid includes: dividing the desorption liquid flowing out during the desorption process into n consecutive fractions of equal volume according to the outflow order, where n is a positive integer not less than 10; collecting each fraction separately; and combining the m1 to m2 fractions to obtain the separated and purified Actinium-225 product liquid; where m1 is a positive integer rounded up after n × 30%, and m2 is a positive integer rounded down after n × 60%.
[0008] Optionally, the volume of the loading solution is determined by the following formula: V_load=k×V_mem; where V_load represents the volume of the loading solution; where k is the membrane volume utilization factor, which takes a value of 20 to 100; the value of k is determined by measuring the dynamic adsorption capacity of the electrospun membrane under different acidity and flow rate conditions using the breakthrough curve method; V_mem represents the effective membrane volume, V_mem=A×δ×ε; where A represents the membrane area, δ represents the membrane thickness, and ε represents the porosity.
[0009] Optionally, the washing volume of the first nitric acid solution is 2 to 10 times the membrane volume in the electrospun membrane assembly.
[0010] Optionally, the washing and impurity removal stage adopts a gradient washing method, including: the first stage washing uses a first nitric acid solution with a nitric acid concentration of 4M and washing is performed at 2 to 3 times the membrane volume; the second stage washing uses a first nitric acid solution with a nitric acid concentration of 6M and washing is performed at 2 to 7 times the membrane volume.
[0011] Optionally, the electrospun membrane assembly is a multi-stage series membrane stack, comprising multiple layers of diethylene glycol amide functionalized electrospun membranes arranged sequentially along the feed flow direction; each layer of diethylene glycol amide functionalized electrospun membrane has a gap of 0.5 to 2 mm, and a flow guiding support layer is provided in the gap.
[0012] Optionally, the diethylene glycol amide ligand density of each layer of diethylene glycol amide-functionalized electrospun membrane in the multi-stage tandem membrane stack decreases gradually along the direction of feed flow; the ligand density of the first layer of diethylene glycol amide-functionalized electrospun membrane is 1.0–2.0 mmol / g; and the ligand density of the last layer of diethylene glycol amide-functionalized electrospun membrane is 0.2–0.8 mmol / g.
[0013] Optionally, the fiber diameter and porosity of each layer of diethylene glycol amide functionalized electrospun membrane in the multi-stage tandem membrane stack decrease gradually along the direction of feed flow: the fiber diameter of the first layer of diethylene glycol amide functionalized electrospun membrane is 3-10 μm and the porosity is 80%-90%; the fiber diameter of the last layer of diethylene glycol amide functionalized electrospun membrane is 0.5-2 μm and the porosity is 70%-80%.
[0014] Optionally, the flow rate of the sample loading solution is 1.0 mL / min; in the washing step, the flow rate of the first nitric acid solution is 1.0 mL / min; in the desorption step, the flow rate of the second nitric acid solution is 0.4 mL / min; and the nitric acid concentration of the sample loading solution is 6 M. The first nitric acid solution has a nitric acid concentration of 4M; the second nitric acid solution has a nitric acid concentration of 10M.
[0015] Optionally, the method further includes: evaporating the separated and purified actinium-225 product solution under reduced pressure to dryness at 40–60°C; and redissolving it to the target volume with 0.01–0.1M hydrochloric acid or nitric acid to obtain an actinium-225 solution.
[0016] The beneficial effects of this invention include: First, this application, targeting the convective mass transfer characteristics of DGA functionalized electrospun membrane modules, for the first time constructs a three-stage nitric acid concentration gradient (4M~8M for loading, 4M~6M for washing, and 9M~11M for desorption) adapted to the "loading, washing, and desorption" of the electrospun membrane module, along with its corresponding flow rate parameters (adsorption / washing 0.5~2.0mL / min, desorption 0.2~0.8mL / min). Unlike traditional resin columns, which are limited by diffusion mass transfer and forced to use a single low flow rate of 0.2 mL / min, the micron-sized inter-fiber channels of electrospun membranes allow solute molecules to rapidly reach the ligand sites on the membrane surface via convective mass transfer. This enables high flow rates of 0.5–2.0 mL / min during the loading and washing stages without sacrificing adsorption efficiency. Simultaneously, the flow rate is reduced to 0.2–0.8 mL / min during the desorption stage, ensuring sufficient contact time between the desorbent and the ligands on the membrane surface, allowing for complete displacement of actinium-225 and a concentrated peak shape. This configuration reduces the total batch time to less than 2 hours, improving purification efficiency by more than three times compared to the over 6 hours required for traditional DGA resin columns.
[0017] Secondly, this application leverages the inherent characteristic of minimal axial diffusion in electrospun membrane modules to collect the middle 30%–60% of the desorbate as the product fraction. Traditional resin columns suffer from severe tailing of the desorption peak due to internal diffusion mass transfer within the particles, resulting in a wide distribution of the target analyte across a broad volume range, forcing large-volume collection (typically 15–30 mL) and low product concentration. In contrast, the inter-fiber pore structure of the electrospun membrane causes actinium-225 to exhibit a sharp, narrow elution peak during desorption. By discarding the high-acid front and low-charge impurities discharged from the dead volume of the membrane module at the front, as well as the slow-desorption kinetics of actinium-227 at the rear, only the middle 30%–60% fraction is collected. This significantly reduces the final product volume without significantly decreasing the overall recovery rate of actinium-225, eliminating the need for additional concentration steps. This aligns with the rapid separation process of electrospun membranes, simultaneously reducing the proportion of actinium-227 impurities and improving the purity of the medical isotope product. Attached Figure Description
[0018] Figure 1 This is a flowchart illustrating the steps of a method for separating and purifying actinium-225 based on an electrospun membrane, as provided in an embodiment of the present invention. Figure 2 This is a process flow diagram of a method for separating and purifying actinium-225 based on an electrospun membrane, provided in an embodiment of the present invention. Detailed Implementation
[0019] In the following description, specific details such as particular system architectures and techniques are set forth for illustrative purposes and not for limitation, in order to provide a thorough understanding of the embodiments of this application. However, those skilled in the art will understand that this application can also be implemented in other embodiments without these specific details. In other instances, detailed descriptions of well-known systems, apparatuses, circuits, and methods have been omitted so as not to obscure the description of this application with unnecessary detail.
[0020] Furthermore, in the description of this application and the appended claims, the terms "first," "second," "third," etc., are used only to distinguish descriptions and should not be construed as indicating or implying relative importance.
[0021] Please see Figure 1 This application provides a method for separating and purifying actinium-225 based on an electrospun membrane, comprising: steps 101 to 104.
[0022] Step 101: Obtain the sample loading solution.
[0023] The loading solution is a nitric acid solution containing actinium-225 prepared by a natural thorium target; the nitric acid concentration of the loading solution is 4M to 8M.
[0024] Specifically, the loading solution is a nitric acid solution containing actinium-225 prepared using a natural thorium target. After proton irradiation or photonuclear reaction, the thorium in the natural thorium target undergoes a spallation reaction to generate actinium-225. The irradiated thorium target is dissolved in nitric acid, and after filtration to remove insoluble matter, a nitric acid solution containing actinium-225 is obtained. The nitric acid concentration of the loading solution is adjusted to 4M–8M. Within this acidity range, DGA ligands have a high partition coefficient for trivalent actinide ions (including actinium-225), enabling effective adsorption of actinium-225. Simultaneously, under these acidity conditions, the nitrate complexation form of thorium (Th(IV)) results in a low affinity for DGA ligands, thus achieving partial separation of actinium-225 from a large amount of the thorium matrix during the adsorption stage.
[0025] Step 102: Pass the sample solution through a diethylene glycol amide-functionalized electrospun membrane module at a flow rate of 0.5–2.0 mL / min to adsorb actinium-225.
[0026] The sample solution was passed through a diethylene glycol amide-functionalized electrospun membrane module at a flow rate of 0.5–2.0 mL / min, allowing actinium-225 to be selectively adsorbed by DGA ligands on the membrane surface. The DGA-functionalized electrospun membrane is a membrane adsorbent with electrospun polymer fibers as the matrix and diethylene glycol amide ligands covalently grafted onto its surface. As the sample solution flowed through the membrane module, actinium-225 ions rapidly reached the DGA ligand sites on the fiber surface via convective mass transfer and were retained on the membrane after coordination with the ligands. Within the flow rate range of 0.5–2.0 mL / min, the residence time of the solution in the membrane pores was sufficient to ensure that the binding reaction between actinium-225 and the ligands reached equilibrium, while avoiding excessively long processing times due to excessively low flow rates.
[0027] Step 103: Pass the first nitric acid solution through the electrospun membrane module at a flow rate of 0.5 to 2.0 mL / min for washing and impurity removal.
[0028] The nitric acid concentration of the first nitric acid solution is 4M to 6M.
[0029] A first nitric acid solution is passed through the electrospun membrane module at a flow rate of 0.5–2.0 mL / min for washing and impurity removal. The nitric acid concentration of the first nitric acid solution is 4M–6M. After adsorption, impurity ions (such as Ra, except for actinium-225) are removed. 2+ Cs + Ru 3+ MoO2 2+ Ba 2+Fission products (such as those from metal ionization) may also be retained on the membrane due to non-specific adsorption or co-precipitation. The washing step utilizes the difference in affinity of DGA ligands for different metal ions at different acidities. Under 4M to 6M nitric acid conditions, the partition coefficient of the above-mentioned impurity ions is much lower than that of actinium-225. By passing a certain volume of nitric acid solution through the membrane module, these co-adsorbed impurity ions are selectively eluted, while actinium-225 remains on the membrane due to its high partition coefficient.
[0030] Step 104: Pass the second nitric acid solution through the electrospun membrane module at a flow rate of 0.2 to 0.8 mL / min for desorption, and collect 30% to 60% of the desorbed liquid to obtain the separated and purified actinium-225 product solution.
[0031] The nitric acid concentration of the second nitric acid solution is 9M to 11M.
[0032] A second nitric acid solution is passed through the electrospun membrane module at a flow rate of 0.2–0.8 mL / min for desorption, and the intermediate 30%–60% of the eluent is collected to obtain the purified actinium-225 product solution. The nitric acid concentration of the second nitric acid solution is 9M–11M. Under high nitric acid concentration (9M–11M), the nitrate concentration increases significantly, and the coordination mode of DGA ligands with actinium-225 shifts from inner-layer coordination to outer-layer ion association. The partition coefficient of actinium-225 drops sharply to an extremely low value, thereby displacing the actinium-225 adsorbed on the membrane into the liquid phase. The desorption flow rate of 0.2–0.8 mL / min is lower than the adsorption and washing flow rates to ensure sufficient contact time between the eluent and the membrane surface, allowing for complete desorption of actinium-225. Due to the minimal axial diffusion of electrospun membranes, actinium-225 exhibits a narrow elution peak during desorption. The initial eluent (approximately the first 30%) mainly consists of a high-acid front and low-charge impurities discharged from the dead volume of the membrane module. The middle 30%–60% contains a high-concentration actinium-225 main peak, while the final 40% contains residual actinium-227 and other impurities with slower desorption kinetics. Therefore, collecting only the middle 30%–60% of the eluent as the product fraction maximizes product purity and concentration while ensuring high recovery rates.
[0033] In summary, the method for separating and purifying actinium-225 based on electrospun membranes provided in this application has the following beneficial effects: Firstly, this application, targeting the convective mass transfer characteristics of DGA functionalized electrospun membrane modules, for the first time constructs a three-stage nitric acid concentration gradient (4M–8M for loading, 4M–6M for washing, and 9M–11M for desorption) adapted to the "loading, washing, and desorption" process of actinium-225 purification and separation, along with corresponding flow rate parameters (adsorption / washing 0.5–2.0 mL / min, desorption 0.2–0.8 mL / min). Unlike traditional resin columns, which are limited by diffusion mass transfer and forced to use a single low flow rate of 0.2 mL / min, the micron-sized interfiber channels of the electrospun membrane allow solute molecules to rapidly reach the ligand sites on the membrane surface via convective mass transfer. This enables the loading and washing stages to use high flow rates of 0.5–2.0 mL / min without sacrificing adsorption efficiency. Simultaneously, the flow rate is reduced to 0.2–0.8 mL / min during the desorption stage, ensuring sufficient contact time between the desorbent and the ligands on the membrane surface, allowing actinium-225 to be completely displaced and resulting in a concentrated peak shape. The above configuration reduces the total process time for a single batch to less than 2 hours, which is more than 3 times more efficient than the purification time of more than 6 hours for traditional DGA resin columns.
[0034] Secondly, this application leverages the inherent characteristic of minimal axial diffusion in electrospun membrane modules to collect the middle 30%–60% of the desorbate as the product fraction. Traditional resin columns suffer from severe tailing of the desorption peak due to internal diffusion mass transfer within the particles, resulting in a wide distribution of the target analyte across a broad volume range, forcing large-volume collection (typically 15–30 mL) and low product concentration. In contrast, the inter-fiber pore structure of the electrospun membrane causes actinium-225 to exhibit a sharp, narrow elution peak during desorption. By discarding the high-acid front and low-charge impurities discharged from the dead volume of the membrane module at the front, as well as the slow-desorption kinetics of actinium-227 at the rear, only the middle 30%–60% fraction is collected. This significantly reduces the final product volume without significantly decreasing the overall recovery rate of actinium-225, eliminating the need for additional concentration steps. This aligns with the rapid separation process of electrospun membranes, simultaneously reducing the proportion of actinium-227 impurities and improving the purity of the medical isotope product.
[0035] In addition, this application adds a washing step for the electrospun membrane module (using a 4M to 6M first nitric acid solution). This step utilizes the principle of different affinities of DGA ligands on the electrospun membrane surface for different metal ions at different acidities to selectively elute impurity ions co-adsorbed on the membrane surface. This washing step fully leverages the convective mass transfer advantages of the electrospun membrane, effectively removing co-adsorbed impurities without losing actinium-225. Combined with subsequent desorption fractionation, this meets the stringent requirements for nuclear purity of actinium-225 used clinically.
[0036] Optionally, the above-mentioned step of collecting the intermediate 30% to 60% of the desorption liquid can specifically include: dividing the desorption liquid flowing out during the desorption process into n consecutive fractions of equal volume according to the outflow order, where n is a positive integer not less than 10; collecting each fraction separately; merging the m1 to m2 fractions to obtain the separated and purified Actinium-225 product liquid; where m1 is a positive integer rounded up after n × 30%, and m2 is a positive integer rounded down after n × 60%.
[0037] The entire desorbed liquid effluent during the desorption process is divided into n consecutive fractions of equal volume in the order of effluent flow, where n is a positive integer not less than 10. After collecting each fraction separately, the m1-m2 fractions are combined to obtain the purified actinium-225 product liquid. Here, m1 is a positive integer rounded up from n × 30%, and m2 is a positive integer rounded down from n × 60%.
[0038] The "middle 30%–60%" ratio is translated into specific segmentation and merging operations: When n=10, m1=3 (10×30%=3), m2=6 (10×60%=6), that is, merging the 3rd to 6th fractions, corresponding to 30%–60% of the total desorbate volume. When n takes a larger value, the segmentation is more refined and the cutting accuracy is higher. The constraint that n is not less than 10 ensures that the number of segments is sufficient to achieve accurate cutting of 30%–60%.
[0039] By segmenting the fractions into equal volumes and merging intermediate sections, the desorption process is standardized, allowing for accurate extraction of high-concentration actinium-225 fractions without relying on online monitoring equipment. This method is compatible with conventional automated fractionating collectors (typically 12- to 24-position rotary tables) and can be implemented without equipment modification, lowering the equipment threshold and operational complexity. It facilitates automated operation in hot chambers or isolators, reducing the radiation exposure risk for operators.
[0040] Optionally, the volume of the sample solution is determined by the following formula: V_load = k × V_mem; Where V_load represents the volume of the sample solution; where k is the membrane volume utilization factor, with a value of 20 to 100; the value of k is determined by measuring the dynamic adsorption capacity of the electrospun membrane under different acidity and flow rate conditions using the breakthrough curve method. V_mem represents the effective membrane volume, V_mem=A×δ×ε; A represents the membrane area, δ represents the membrane thickness, and ε represents the porosity.
[0041] It should be noted that the k-value is a multiple of the sample feed volume that can be processed per unit membrane volume, reflecting the proportional relationship between the membrane module's processing capacity and its own physical volume. The k-value is not randomly selected but determined using the breakthrough curve method. The breakthrough curve method involves continuously passing an actinol-225 feed solution with a known activity concentration through the membrane module at a set flow rate. The activity concentration of actinol-225 in the effluent is continuously monitored at the outlet, and a curve of effluent concentration / initial concentration versus cumulative sample loading volume is plotted. When the effluent concentration / initial concentration reaches 5%–10% (significant breakthrough occurs), the corresponding cumulative sample loading volume is the dynamic adsorption capacity of the membrane under those conditions. The upper limit of the k-value is jointly determined by the dynamic adsorption capacity and the maximum possible concentration of actinol-225 in the feed solution, ensuring that the total sample activity does not exceed the membrane loading capacity; the lower limit of the k-value is determined by economic considerations, ensuring that the processing capacity per unit time meets production requirements.
[0042] The effective membrane volume V_mem is the pore volume of the electrospun membrane itself in the membrane module, not the apparent volume of the membrane module. The membrane area A (determined by the membrane diameter, such as 25 mm or 47 mm), membrane thickness δ (typically 100–300 μm), and porosity ε (typically 70%–90%) are all inherent physical parameters of the membrane material. The product of these three is the pore volume within the membrane that allows liquid to flow through.
[0043] As can be seen, this application quantitatively correlates the sample loading volume with the inherent physical parameters (effective membrane volume) of the membrane module and scientifically determines the k value through the breakthrough curve method, making the determination of the sample loading volume a calculable engineering design. Through double conservative estimation (the upper limit of the k value is determined by the dynamic adsorption capacity, and a value of 20-100 leaves a safety margin), it ensures that under any irradiation fluctuations and changes in feed concentration, the total activity of the sample loading does not exceed the safe threshold of membrane loading, avoiding actinium-225 breakthrough loss due to excessive sample loading. This quantitative rule allows the sample loading volume of membrane modules of different specifications (different membrane areas, thicknesses, and porosities) to be calculated using a unified formula.
[0044] Optionally, the washing volume of the first nitric acid solution is 2 to 10 times the membrane volume in the electrospun membrane module.
[0045] Membrane volume refers to the sum of the apparent volumes of all membranes in an electrospun membrane module (i.e., membrane area × membrane thickness × number of membrane layers), which differs from the aforementioned effective membrane volume. Membrane volume is the total volume including the fiber skeleton, while effective membrane volume is the pore volume. Washing volume is based on membrane volume.
[0046] The selection of the washing volume needs to consider two objectives: if the volume is too small (less than twice the membrane volume), the washing solution will not be able to fully displace the co-adsorbed impurities in the membrane pores and fiber surface; if the volume is too large (more than 10 times the membrane volume), although impurities can be removed more thoroughly, it will prolong the washing time and may cause some loss of actinium-225, while also increasing the burden of waste liquid treatment.
[0047] By linking the washing volume to the membrane volume rather than the sample loading volume, the thoroughness of washing for membrane modules of different specifications is ensured to be consistent. Whether it is a small-area membrane of 25mm or a large-area membrane of 47mm, the same membrane volume multiple is used for washing, ensuring the scalability of process parameters. The range of 2 to 10 times ensures effective removal of impurities while avoiding the loss of actinium-225 and wasted time due to over-washing.
[0048] Furthermore, it should be noted that the embodiments of this application use two different physical benchmarks—effective membrane volume and apparent membrane volume—to determine the sample loading volume and washing volume, respectively. This is because the adsorption and washing steps have fundamentally different separation mechanisms. Sample loading and adsorption is a mass transfer control process, where the actual flow path of the feed solution is only the pore space between the fibers. Using the effective membrane volume as a benchmark allows for accurate calculation of the effective contact time between the solute molecules and the ligand sites, thereby ensuring that the target ion Actinium-225 is fully captured under dynamic flow conditions without breakthrough. Washing and impurity removal, on the other hand, is a displacement and dilution control process. It not only requires the displacement of the high-concentration mother liquor remaining in the pores but also requires thorough rinsing of the fiber skeleton surface to remove adsorbed impurity ions. Using the apparent membrane volume, which includes the fiber skeleton and pores, as a benchmark is equivalent to introducing a redundancy safety factor, ensuring sufficient coverage of the membrane module by the washing solution and the intensity of the cleaning. By proposing a differentiated calculation method based on the mass transfer differences between adsorption and washing in the membrane adsorption separation system, the sample loading amount is maximized to ensure adsorption safety while maximizing the throughput, and the washing amount is minimized to ensure sufficient removal of impurities while minimizing reagent consumption and operation time. Together, these two methods ensure that the total process time is less than or equal to 2 hours and the product purity meets the standards.
[0049] Optionally, the washing and impurity removal stage adopts a gradient washing method, including: the first stage washing uses a first nitric acid solution with a nitric acid concentration of 4M and washing is performed at 2 to 3 times the membrane volume; the second stage washing uses a first nitric acid solution with a nitric acid concentration of 6M and washing is performed at 2 to 7 times the membrane volume.
[0050] The first stage of washing uses a 4M nitric acid solution, applied at a volume of 2–3 times the membrane volume. Under 4M nitric acid conditions, Ra 2+ Ba 2+ The partition coefficients of divalent metal ions are extremely low, making them very easy to elute; at the same time, the thorium matrix remaining in the membrane pores also has a low affinity for DGA ligands at this acidity. Therefore, the main purpose of the first-stage washing is to rapidly displace the thorium matrix and low-affinity divalent fission product impurities remaining in the membrane pores and on the fiber surface.
[0051] The second stage of washing uses a 6M nitric acid solution, applied at a volume of 2–7 times the membrane volume. Under 6M nitric acid conditions, impurities commonly found in Zr, Mo, Ru fission products as oxygen anions (such as ZrO) are removed. 2+ MoO2 2+ Actinium (etc.) binds very weakly to DGA ligands and is forcibly removed. At this acidity, the partition coefficient of actinium-225 remains high, and no significant loss occurs.
[0052] Different impurities exhibit different elution behaviors at different acidities, making it difficult to efficiently remove all types of impurities simultaneously with a single acidity. By employing a phased washing process—first low acid (4M) followed by high acid (6M)—different types of co-adsorbed impurities can be removed more effectively. Specifically, this gradient washing strategy fully utilizes the changing affinity of DGA ligands for different metal ions with varying acidity, achieving the categorized and phased removal of complex impurity profiles. The first phase (4M) targets divalent ions and the thorium matrix, while the second phase (6M) targets oxonium anion fission products, resulting in higher impurity removal efficiency and lower actinium-225 loss compared to washing with a single acidity.
[0053] Optionally, the electrospun membrane assembly is a multi-stage series membrane stack, including multiple layers of diethylene glycol amide functionalized electrospun membranes arranged sequentially along the feed flow direction; a gap of 0.5 to 2 mm is left between each layer of diethylene glycol amide functionalized electrospun membrane, and a flow guiding support layer is provided in the gap.
[0054] The multilayer membranes are arranged sequentially along the flow direction, and each membrane adsorbs actinium-225. The total adsorption capacity of the multilayer membranes is the sum of the adsorption capacities of each membrane layer, thereby increasing the processing capacity several times without changing the specifications of a single membrane.
[0055] A 0.5–2 mm interlayer spacing ensures a certain distance between each membrane layer, preventing them from sticking together tightly. If the membrane layers stick together, the feed solution cannot be evenly distributed to the full area of each membrane layer, resulting in some membrane area not being effectively utilized. At the same time, local high flow rate zones may form at the bonding points, causing insufficient adsorption.
[0056] The flow-guiding support layer, located in the interlayer gap (such as a screen or non-woven fabric made of polypropylene, polyethylene, or polytetrafluoroethylene), serves two purposes: first, it physically supports adjacent membrane layers to prevent them from deforming or shifting under liquid pressure; second, it guides the liquid to be evenly distributed between layers before entering the next membrane layer, ensuring that the entire surface of each membrane layer is evenly covered by the liquid.
[0057] Multi-stage tandem membrane stacks, through the stacking of multiple membranes, multiply the membrane area and adsorption capacity without changing the specifications and operating parameters of individual membranes, thereby increasing the throughput per batch. The interlayer spacing and flow-guiding support layers ensure that the flow channel gaps between each membrane layer are maintained, avoiding uneven feed distribution and sudden pressure drops caused by membrane layer adhesion, and ensuring the consistency of adsorption efficiency of each membrane layer.
[0058] Optionally, the diethylene glycol amide ligand density of each layer of diethylene glycol amide-functionalized electrospun membrane in the multi-stage tandem membrane stack decreases gradually along the direction of feed flow; the ligand density of the first layer of diethylene glycol amide-functionalized electrospun membrane is 1.0–2.0 mmol / g; and the ligand density of the last layer of diethylene glycol amide-functionalized electrospun membrane is 0.2–0.8 mmol / g.
[0059] The first layer (upstream) of ligands has a density of 1.0–2.0 mmol / g. The high-density ligands provide a high density of binding sites, enabling rapid capture of most actinium-225 in the initial stage of feed entering the membrane stack, thus achieving high-capacity adsorption.
[0060] The final (downstream) layer has a ligand density of 0.2–0.8 mmol / g. This low-density ligand provides fewer binding sites, primarily capturing trace amounts of actinium-225 remaining after penetrating the first layer. Due to the low ligand density, the non-selective adsorption capacity for impurities is correspondingly reduced, thus enabling quality control of the product at the outlet.
[0061] The ligand density in each intermediate layer is between that of the first and last layers, decreasing layer by layer or stepwise along the flow direction, forming a smooth ligand density gradient.
[0062] Ligand density refers to the amount of DGA ligands covalently grafted onto a unit mass (g) of electrospun membrane, which can be determined by methods such as elemental analysis, X-ray photoelectron spectroscopy, or thermogravimetric analysis.
[0063] The logic behind this gradient design is that the concentration of actinium-225 gradually decreases along the direction of feed flow, requiring high-density ligands upstream to provide high-capacity capture; downstream, the concentration of actinium-225 has been significantly reduced, and low-density ligands are sufficient to capture the remaining target ions. At the same time, the reduction in ligands reduces the non-selective adsorption of impurities, thereby achieving synergistic optimization of high-capacity capture at the front end and high-purity fine separation at the back end.
[0064] This application proposes a multi-stage membrane stack design with decreasing ligand density gradient. By gradually reducing the ligand density along the flow direction, it overcomes the contradiction between adsorption capacity and separation selectivity in single-density membranes. While a single high-density membrane has a large adsorption capacity, it also exhibits strong non-specific adsorption of impurities, while a single low-density membrane has good selectivity but insufficient capacity. The gradient design ensures that each membrane operates at the optimal ligand density within its respective concentration range, achieving both high recovery rate and high purity overall.
[0065] Optionally, the fiber diameter and porosity of each layer of diethylene glycol amide-functionalized electrospun membrane in the multi-stage tandem membrane stack decrease gradually along the direction of feed flow: the fiber diameter of the first layer of diethylene glycol amide-functionalized electrospun membrane is 3-10 μm and the porosity is 80%-90%; the fiber diameter of the last layer of diethylene glycol amide-functionalized electrospun membrane is 0.5-2 μm and the porosity is 70%-80%.
[0066] The first layer of fibers has a diameter of 3–10 μm and a porosity of 80%–90%. The coarse fibers and high porosity provide a larger channel size and lower flow resistance, allowing the feed liquid to pass through the first layer quickly and complete the initial capture of actinium-225 under high-flux conditions.
[0067] The final layer of fibers has a diameter of 0.5–2 μm and a porosity of 70%–80%. The fine fibers have a larger specific surface area (fiber surface area per unit volume), providing more ligand grafting sites; the lower porosity means smaller channel size, increasing the probability of contact between the feed liquid and the fiber surface, which is beneficial for capturing trace amounts of actinium-225 after penetrating upstream.
[0068] The intermediate layers have fiber diameters and porosities between the first and last layers, decreasing layer by layer or in a stepwise manner along the flow direction.
[0069] Fiber diameter and porosity are inherent physical parameters of electrospun membranes. Smaller fiber diameters result in a larger total fiber surface area per unit volume, allowing for the grafting of more ligands; however, excessively small fiber diameters lead to decreased porosity and increased flow resistance. Higher porosity results in a smaller pressure drop across the membrane and allows for higher permissible operating flow rates; however, excessively high porosity means a reduced fiber content per unit volume and a decrease in total adsorption capacity.
[0070] The logic behind this gradient design is that the upstream stage primarily operates at high throughput, requiring large-diameter fibers and high porosity to ensure flow rate; while the downstream stage focuses on fine separation, requiring small-diameter fibers and lower porosity to improve capture efficiency. The gradient design of fiber diameter and porosity further optimizes the hydrodynamic and adsorption performance of the multi-stage membrane stack. The high porosity of the upstream coarse fibers ensures high throughput capacity, while the low porosity of the downstream fine fibers improves the capture efficiency of trace amounts of actinium-225. This gradient, combined with the ligand density gradient, forms a dual gradient synergy: the high ligand density and high porosity of the upstream coarse fibers achieve high-throughput, high-capacity capture, while the low ligand density and low porosity of the downstream fine fibers achieve high-precision trace capture, jointly improving the overall separation efficiency and product purity of the membrane stack.
[0071] Optionally, the flow rate of the sample loading solution is 1.0 mL / min; in the washing step, the flow rate of the first nitric acid solution is 1.0 mL / min; in the desorption step, the flow rate of the second nitric acid solution is 0.4 mL / min; the nitric acid concentration of the sample loading solution is 6 M; the nitric acid concentration of the first nitric acid solution is 4 M; and the nitric acid concentration of the second nitric acid solution is 10 M.
[0072] At a loading acidity of 6M, the partition coefficient of actinium-225 is sufficiently high, while the partition coefficients of major impurities such as thorium and radium are relatively low. A washing acidity of 4M maximizes the elution of co-adsorbed impurities without losing actinium-225. A desorption acidity of 10M minimizes the partition coefficient of actinium-225, achieving rapid and complete desorption. A medium-to-high flow rate of 1.0 mL / min is used for loading and washing to ensure processing efficiency, while a lower flow rate of 0.4 mL / min is used for desorption to ensure complete desorption and concentrated peaks.
[0073] By combining the optimal parameters for each step, the total process time was further optimized to ≤1.5 hours, the Actinium-225 recovery rate was ≥92%, and the Actinium-227 impurity was ≤0.15%.
[0074] Optionally, the method further includes: evaporating the separated and purified actinium-225 product solution under reduced pressure to dryness at 40–60°C; and redissolving it to the target volume with 0.01–0.1M hydrochloric acid or nitric acid to obtain an actinium-225 solution.
[0075] Vacuum evaporation involves evaporating the purified actinium-225 product solution to dryness under reduced pressure at 40–60°C. This process removes nitric acid and water, leaving actinium-225 as a solid residue in the evaporation vessel. The mild conditions of 40–60°C prevent product decomposition or the spread of radioactive aerosols that could occur at higher temperatures (above 80°C); the reduced pressure environment (such as vacuum in a rotary evaporator) lowers the solvent boiling point, allowing for efficient evaporation at lower temperatures.
[0076] Reconstitute with 0.01–0.1 M hydrochloric acid or nitric acid to the target volume to obtain a high-concentration, high-purity actinium-225 solution. Reconstitution with dilute acid ensures the acidity and volume of the product solution are suitable for subsequent radiolabeling reactions (such as labeling with chelating agents like DOTA) or generator preparation. Hydrochloric acid and nitric acid are commonly used media in radiopharmaceutical preparation and can be selected based on the specific requirements of the subsequent labeling reaction.
[0077] By employing reduced-pressure evaporation and dilute acid resolution under mild conditions, the high-acidity, low-concentration actinium-225 product solution obtained from desorption is transformed into a low-acidity, high-concentration, ready-to-use product solution, realizing a process from target solution to a directly usable actinium-225 solution for labeling. The mild conditions of 40–60°C avoid radiolytic damage and volatilization loss to actinium-225 caused by high temperatures. The rotary evaporator is compatible with the hot chamber operating environment, reducing radiation exposure for operators. The final product solution can be directly used for subsequent radiopharmaceutical labeling or generator preparation without additional media conversion or concentration steps.
[0078] Please see Figure 2 The following is combined with Figure 2 The complete process flow of the method for separating and purifying actinium-225 based on electrospun membrane in this application is illustrated with an example.
[0079] Pretreatment of the sample solution: The proton-irradiated natural thorium target was dissolved, filtered, and the acidity was adjusted to obtain a nitric acid solution containing actinium-225. The HNO3 concentration of this solution was adjusted to 4M~8M and used as the sample loading solution.
[0080] Adsorption: The DGA-functionalized electrospun membrane is placed in a membrane filter or membrane module, and the resulting feed solution is pumped through the electrospun membrane at a flow rate of 0.5 to 2.0 mL / min, so that Actinium-225 is selectively adsorbed by the DGA ligands on the membrane surface; the sample loading volume is 1 to 50 mL, and the sample loading time is 5 to 60 minutes.
[0081] Washing: Wash the adsorbed electrospun membrane with 4M to 6M nitric acid solution (preferably 4M) at a flow rate of 0.5 to 2.0 mL / min, with a washing volume of 2 to 10 times the membrane volume, to remove co-adsorbed impurity ions (such as cracking products of Ra, Cs, Ru, Mo, Ba, etc.).
[0082] Desorption: Using 10M nitric acid solution as the eluent, the solution was passed through the washed electrospun membrane at a flow rate of 0.2–0.8 mL / min. The eluent was collected in fractions, one tube per 1–2 mL fraction. The peak value of actinium-225 in the eluent appeared within the 2–6 mL desorption volume, and the total desorption time did not exceed 30 minutes. The peak values containing actinium-225 were combined to obtain the purified actinium-225 product solution.
[0083] Post-processing of the product: The obtained actinium-225 product solution is evaporated to dryness under reduced pressure under mild conditions (such as 40-60℃), and then redissolved with 0.01-0.1M hydrochloric acid or nitric acid to obtain a high-concentration, high-purity actinium-225 solution, which can be directly used for subsequent labeling or generator preparation.
[0084] Optionally, the fiber diameter of the DGA functionalized electrospun membrane is 1 to 10 μm, the membrane porosity is 70% to 90%, and the membrane diameter is selected according to the filter specifications (e.g., 25 mm, 47 mm).
[0085] Optionally, the HNO3 concentration of the sample solution is 6M, the flow rate is 1.0 mL / min, and the sample loading volume per unit area of the membrane is 0.5–5 μCi / cm². 2 .
[0086] Optionally, the washing solution is 4 M HNO3, and the washing volume is 5 times the membrane volume.
[0087] Optionally, the desorption solution is 10 M HNO3, the flow rate is 0.4 mL / min, and the first 2-5 mL of the desorption solution is collected as the product.
[0088] Alternatively, the product can be evaporated to dryness under reduced pressure in a 50°C water bath using a rotary evaporator, and then reconstituted with 0.05M HCl to the required volume.
[0089] The above-described embodiments are only used to illustrate the technical solutions of this application, and are not intended to limit them. Although this application has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of this application, and should all be included within the protection scope of this application.
Claims
1. A method for separating and purifying actinium-225 based on electrospun membrane, characterized in that, include: Obtain a sample loading solution; wherein the sample loading solution is a nitric acid solution containing actinium-225 prepared by a natural thorium target; the nitric acid concentration of the sample loading solution is 4M to 8M; The sample solution was passed through a diethylene glycol amide-functionalized electrospun membrane module at a flow rate of 0.5–2.0 mL / min to adsorb actinium-225. The first nitric acid solution is passed through the electrospun membrane assembly at a flow rate of 0.5 to 2.0 mL / min for washing and impurity removal; wherein the nitric acid concentration of the first nitric acid solution is 4M to 6M. The second nitric acid solution is passed through the electrospun membrane assembly at a flow rate of 0.2 to 0.8 mL / min for desorption, and 30% to 60% of the desorbed liquid is collected to obtain the separated and purified actinium-225 product solution; wherein the nitric acid concentration of the second nitric acid solution is 9M to 11M.
2. The method for separating and purifying actinium-225 based on electrospun membrane according to claim 1, characterized in that, Collect the intermediate 30%–60% of the eluent, including: The desorbed liquid flowing out during the desorption process is divided into n consecutive fractions of equal volume according to the outflow order, where n is a positive integer not less than 10; Collect each fraction separately; Combine the m1 to m2 fractions to obtain the separated and purified actinium-225 product liquid; Where m1 is a positive integer obtained by rounding up n × 30%, and m2 is a positive integer obtained by rounding down n × 60%.
3. The method for separating and purifying actinium-225 based on electrospun membrane according to claim 1, characterized in that, The volume of the sample liquid is determined by the following formula: V_load = k × V_mem; Wherein, V_load represents the volume of the sample solution; where k is the membrane volume utilization factor, with a value of 20 to 100; the value of k is determined by measuring the dynamic adsorption capacity of the electrospun membrane under different acidity and flow rate conditions using the breakthrough curve method. V_mem represents the effective membrane volume, V_mem=A×δ×ε; A represents the membrane area, δ represents the membrane thickness, and ε represents the porosity.
4. The method for separating and purifying actinium-225 based on electrospun membrane according to claim 1, characterized in that, The washing volume of the first nitric acid solution is 2 to 10 times the membrane volume in the electrospun membrane assembly.
5. The method for separating and purifying actinium-225 based on electrospun membrane according to claim 4, characterized in that, The washing and impurity removal stage employs a gradient washing method, including: The first stage of washing uses a 4M nitric acid solution and is performed at a volume of 2 to 3 times the membrane volume. The second stage of washing uses a 6M nitric acid solution and is performed at a volume of 2 to 7 times the membrane volume.
6. The method for separating and purifying actinium-225 based on electrospun membrane according to claim 1, characterized in that, The electrospun membrane assembly is a multi-stage series membrane stack, including multiple layers of diethylene glycol amide functionalized electrospun membranes arranged sequentially along the feed flow direction. Each layer of diethylene glycol amide functionalized electrospun membrane has a gap of 0.5 to 2 mm between it, and a flow-guiding support layer is provided in the gap.
7. The method for separating and purifying actinium-225 based on electrospun membrane according to claim 6, characterized in that, The diethylene glycolamide ligand density of each layer of diethylene glycolamide-functionalized electrospun membrane in the multi-stage tandem membrane stack decreases gradually along the direction of feed flow. The ligand density of the first layer of diethylene glycol amide-functionalized electrospun membrane is 1.0–2.0 mmol / g; The ligand density of the final layer of diethylene glycol amide-functionalized electrospun membrane is 0.2–0.8 mmol / g.
8. The method for separating and purifying actinium-225 based on electrospun membrane according to claim 7, characterized in that, In the multi-stage tandem membrane stack, the fiber diameter and porosity of each layer of diethylene glycol amide-functionalized electrospun membrane decrease gradually along the feed flow direction. The first layer of diethylene glycol amide functionalized electrospun membrane has a fiber diameter of 3–10 μm and a porosity of 80%–90%. The final layer of diethylene glycol amide functionalized electrospun membrane has a fiber diameter of 0.5–2 μm and a porosity of 70%–80%.
9. The method for separating and purifying actinium-225 based on electrospun membrane according to claim 1, characterized in that, The flow rate of the sample solution is 1.0 mL / min; During the washing step, the flow rate of the first nitric acid solution is 1.0 mL / min; In the desorption step, the flow rate of the second nitric acid solution is 0.4 mL / min; The nitric acid concentration of the sample solution is 6M; The nitric acid concentration of the first nitric acid solution is 4M; The nitric acid concentration of the second nitric acid solution is 10M.
10. The method for separating and purifying actinium-225 based on electrospun membrane according to claim 1, characterized in that, The method further includes: The purified actinide-225 product solution was evaporated to dryness under reduced pressure at 40–60°C. Redissolve the actinide-225 solution in 0.01–0.1 M hydrochloric acid or nitric acid to the target volume.
Citation Information
Patent Citations
Separation and purification method for preparing lead-212 and actinide-225 by photo-nuclear reaction method
CN120183769A