Continuous production unit of poly(1,4-cyclohexanedimethyl terephthalate)

By setting up multi-stage chambers and stirring devices in the production unit of polyethylene terephthalate (PET) 1,4-cyclohexanediethanol, the problems of material backmixing and insufficient heat were solved, and the stability of molecular weight distribution and consistency of product quality were achieved.

CN123102277APending Publication Date: 2026-11-17CHINA PETROLEUM ENG CORP LTD +2
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202611175972.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-04
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In the existing technology, the production process of polyethylene terephthalate (PET) 1,4-cyclohexanediethanol ester is difficult due to material backmixing and volatilization, and insufficient heat input leads to uneven molecular weight distribution, which affects product quality.

Method used

A combination device consisting of an esterification reactor, a first polycondensation reactor, and a second polycondensation reactor is used. Multiple interconnected chambers are arranged sequentially along the height of the first reactor body, and stirring devices are installed in the chambers. By controlling the material flow and heat supply through multi-stage reaction sections, back mixing is avoided and molecular weight stability is improved.

Benefits of technology

This process ensures the flow stability and heating uniformity of materials during prepolymerization, avoids backmixing, and improves the stability of the final polymer's molecular weight growth and product consistency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123102277A_ABST
    Figure CN123102277A_ABST
Patent Text Reader

Abstract

This application provides a continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate, relating to the field of polymerization reactor technology. The continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate includes an esterification reactor, a first polycondensation reactor, and a second polycondensation reactor. The first polycondensation reactor includes a reactor body and a stirring device. Multiple chambers are arranged sequentially along the height of the reactor body, with adjacent chambers connected. The stirring device is disposed within each chamber. The reactor body has a first inlet and a first outlet communicating with the chambers. The first inlet is connected to the esterification reactor. The second polycondensation reactor is connected to the first outlet. By arranging multiple interconnected chambers sequentially along the height of the first reactor body and installing stirring devices within each chamber, reverse mixing is avoided, improving the stability of the final polymer's molecular weight growth and product consistency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of polymerization reactor technology, and more particularly to a continuous production apparatus for poly(1,4-cyclohexanediethanol terephthalate). Background Technology

[0002] Poly(1,4-cyclohexanediethanol) terephthalate (PET) is a high-performance polyester material with heat resistance, high toughness, and high chemical stability, widely used in electronics, automotive manufacturing, and medical equipment. The production of PET typically involves esterification and polycondensation reactions.

[0003] In related technologies, patent application number 202520530440.1 discloses a high-efficiency and energy-saving continuous polyester production device, including an esterification reactor, a pre-polymerization reactor and a final polymerization reactor connected in sequence. The reactants undergo esterification in the esterification reactor. After esterification, the reactants are transferred to the pre-polymerization reactor for pre-polymerization. After pre-polymerization, the reactants in the pre-polymerization reactor are transferred to the final polymerization reactor for further polymerization to obtain qualified polyester melt products.

[0004] However, reverse mixing can easily occur between materials that have been reacting for a period of time and have higher molecular weights and fresh materials that have just entered the reactor and have lower molecular weights, resulting in uneven molecular weight distribution and affecting the quality of polyester products. Summary of the Invention

[0005] This application provides a continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate, which overcomes the problems in the prior art such as material backmixing, difficulty in devolvation, and uneven molecular weight distribution caused by insufficient heat input, which affect the quality of polyester products.

[0006] This application provides a continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate, comprising: an esterification reactor, wherein the esterification reactor is used to esterify the reactants to obtain the esterified product.

[0007] The first polycondensation reactor includes a first reactor body and a stirring device. Multiple chambers are arranged sequentially along the height direction within the first reactor body, and adjacent chambers are connected. The stirring device is disposed within each chamber. The first reactor body has a first inlet and a first outlet that communicate with the chambers. The first inlet is connected to the esterification reactor. The first reactor body is used to receive the esterified material and perform a pre-polycondensation reaction on the esterified material to obtain a pre-polycondensed material.

[0008] The second polycondensation reactor is connected to the first discharge port. The second polycondensation reactor is used to receive the prepolymer and perform a polycondensation reaction on the prepolymer to obtain the final polymer.

[0009] In one possible implementation, the first reactor body includes a first shell and a plurality of flow-blocking elements disposed within the first shell. The plurality of flow-blocking elements are arranged at intervals along the height direction of the first shell, and the flow-blocking elements and the first shell enclose the chamber to form the cavity. Each chamber is provided with a heating coil.

[0010] In one possible implementation, the flow deflector includes a base plate and a side plate, one end of the base plate being connected to the side plate and the other end of the base plate being connected to the first housing.

[0011] In one possible implementation, adjacent chambers are connected by a pipe along the height direction of the first reactor body, the pipe being disposed outside the first shell, and a control valve being disposed on the pipe.

[0012] An overflow port is provided on the side plate above the stirring device along the height direction of the first reactor body, and the overflow port is connected to the chamber where the stirring device is located.

[0013] In one possible implementation, the second polycondensation reactor includes a second shell, a main shaft, and a plurality of connectors. The second shell is in communication with the first outlet. The main shaft is inserted into the second shell along the extension direction of the second shell. The plurality of connectors are disposed on the main shaft and spaced apart along the extension direction of the main shaft. The connectors are configured to rotate within the second shell to stir the reactants within the second shell.

[0014] In one possible implementation, the spindle includes a first shaft and a second shaft, the second shaft being disposed outside the first shaft.

[0015] The first shaft has a main channel, and an opening is provided on the shaft wall of the first shaft for connecting the connector and the main channel.

[0016] The second shaft and the first shaft form an annular channel, which is used to connect the outlet of the connector. Both the main channel and the annular channel are used to transfer heat medium.

[0017] In one possible implementation, the connector includes a hollow disc, a ring, a first scraper, and a second scraper. The hollow disc is connected by the ring. The first scraper is disposed on the edge of the hollow disc, and the second scraper is disposed on the side of the ring. The first scraper is used to fit against the inner wall of the second housing, and the second scraper is used to fit against the side of the adjacent connector.

[0018] In one possible implementation, the hollow disk has a first channel and a second channel, the first channel communicating with the main channel and the second channel communicating with the annular channel, both the first channel and the second channel being used to transfer a heat transfer medium.

[0019] In one possible implementation, the second housing is a cylindrical body, with a second inlet at one end and a second outlet at the other end. The second inlet communicates with the first outlet, and a screw is provided at the second outlet.

[0020] In one possible implementation, the esterification reactor includes a first esterification reactor and a second esterification reactor.

[0021] The first esterification reactor is used to perform a preliminary esterification reaction on the reactants to obtain a first esterified product, and the esterification rate of the first esterification reactor is controlled to be greater than or equal to 86% and less than or equal to 92%.

[0022] The second esterification reactor is connected to the first esterification reactor, and the esterification rate of the second esterification reactor is controlled to be greater than or equal to 96.5% and less than or equal to 99.5%.

[0023] In one possible implementation, the first polycondensation reactor is connected to the second esterification reactor, and a pre-polycondensation reaction is carried out in the first polycondensation reactor to obtain a pre-polymer with a molecular weight greater than or equal to 1500 and less than or equal to 3500.

[0024] The final polymer obtained by polycondensation reaction in the second polycondensation reactor has a molecular weight greater than or equal to 16,000 and less than or equal to 18,000.

[0025] This application provides a continuous production apparatus for poly(1,4-cyclohexanedimethyl terephthalate). By setting up an esterification reactor, a first polycondensation reactor connected to the esterification reactor, and a second polycondensation reactor connected to a first discharge port, and by arranging multiple interconnected chambers along the height direction in the first reactor body of the first polycondensation reactor, and installing a stirring device in each chamber, the esterification can achieve continuous transfer and staged reaction in the pre-polycondensation stage. This enhances the flow stability, heating uniformity, and by-product removal effect of the material in the pre-polycondensation process, thereby facilitating the continuous and stable progress of the subsequent polycondensation reaction, avoiding backmixing, and improving the stability of the final polymer molecular weight growth and product consistency. Attached Figure Description

[0026] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with this application and, together with the description, serve to explain the principles of this application.

[0027] Figure 1 A schematic diagram of the continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate provided in this application;

[0028] Figure 2 for Figure 1 A schematic diagram of the structure of the first polycondensation reactor in the continuous production unit of poly(1,4-cyclohexanediethanol) terephthalate.

[0029] Figure 3 for Figure 1 A schematic diagram of the structure of the second polycondensation reactor in the continuous production unit of poly(1,4-cyclohexanediethanol) terephthalate.

[0030] Figure 4 for Figure 3 A schematic diagram of the connecting components in the second polycondensation reactor is provided.

[0031] Explanation of reference numerals in the attached figures:

[0032] 100 - Esterification reactor; 110 - First esterification reactor; 120 - Second esterification reactor; 121 - Reactor body; 122 - Mixing device; 123 - Reaction chamber;

[0033] 200 - First polycondensation reactor; 210 - First reactor body; 211 - First inlet; 212 - First outlet; 220 - Pipeline; 230 - Chamber; 240 - Control valve; 250 - Stirring device; 260 - Baffle; 261 - Bottom plate; 262 - Side plate; 263 - Overflow port; 270 - First shell;

[0034] 300 - Second polycondensation reactor; 310 - Second shell; 311 - Second feed inlet; 312 - Second discharge outlet; 320 - Main shaft; 321 - First shaft; 3211 - Main channel; 322 - Second shaft; 3221 - Annular channel; 330 - Connector; 331 - Disc; 332 - First scraper; 333 - Second scraper; 334 - First channel; 335 - Reinforcing column; 336 - Annulus; 337 - Second channel;

[0035] 400 - Heating Jacket;

[0036] 500 - Slurry preparation structure;

[0037] 600 - Pelletizing unit; 610 - Pelletizer; 620 - Dryer; 630 - Classifier;

[0038] 710 - Slurry transfer pump; 720 - Esterification transfer pump; 730 - Prepolymer transfer pump; 740 - Condensation polymer transfer pump;

[0039] 800-Filter.

[0040] The accompanying drawings illustrate specific embodiments of this application, which will be described in more detail below. These drawings and descriptions are not intended to limit the scope of the concept in any way, but rather to illustrate the concept of this application to those skilled in the art through reference to particular embodiments. Detailed Implementation

[0041] Exemplary embodiments will now be described in detail, examples of which are illustrated in the accompanying drawings. When the following description relates to the drawings, unless otherwise indicated, the same numbers in different drawings denote the same or similar elements. The embodiments described in the following exemplary embodiments do not represent all embodiments consistent with this application. Rather, they are merely examples of apparatuses and methods consistent with some aspects of this application.

[0042] The terms "first," "second," "third," etc. (if present) in the specification, claims, and accompanying drawings of this application are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data can be interchanged where appropriate so that the embodiments of this application described herein can be implemented in orders other than those illustrated or described herein.

[0043] Secondly, it should be noted that in the description of this application, the terms "inner", "outer", "first direction", "second direction", etc., indicating the direction or positional relationship are based on the direction or positional relationship shown in the drawings. This is only for the convenience of description and does not indicate or imply that the device or component must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, it should not be construed as a limitation of this application.

[0044] Furthermore, it should be noted that, in the description of this application, unless otherwise expressly specified and limited, the terms "connected" and "linked" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection between two components. Those skilled in the art can understand the specific meaning of the above terms in this application according to the specific circumstances.

[0045] The continuous production unit for poly(1,4-cyclohexanediethanol) terephthalate is mainly used in the industrial production of high-performance polyesters using terephthalic acid and 1,4-cyclohexanediethanol as raw materials. This type of production typically requires sequential completion of esterification, pre-condensation, and condensation, and relies on continuous conveying and connection between multi-stage reaction equipment to achieve stable reaction and continuous discharge in the molten state.

[0046] In related technologies, the direct esterification method is usually adopted. After the polyester raw material is esterified in the esterification reactor, it continues to undergo pre-condensation and condensation in the polycondensation reactor, so that the oligomers are further polycondensed under high temperature conditions. At the same time, by-products generated during the reaction are continuously removed, the molecular weight is gradually increased and the final polymer is formed.

[0047] However, during the reaction, the viscosity of the materials increases rapidly, the surface renewal of the materials is slow, and the flow path control is insufficient. Back-mixing of reactants in the polycondensation reactor with newly added materials is likely, or uneven residence time distribution may occur. Furthermore, PCT prepolymers and polymers are prone to crystallization. If the heat supply to the reaction system is insufficient or the heat exchange efficiency is low during synthesis, the prepolymers and polymers are extremely prone to rapid crystallization and solidification. 1,4-Cyclohexanediethanol has a large molecular weight and low saturated vapor pressure, making its volatilization and removal from high-viscosity polymers difficult. The volatilization process itself is a strongly endothermic process; if the equipment cannot provide sufficient heat, the vaporization rate of 1,4-cyclohexanediethanol will be severely limited, resulting in its residue in the melt, hindering the polycondensation reaction, and ultimately failing to achieve the required molecular weight and product quality. In summary, how to balance the stable transport of materials after esterification, the orderly reaction during pre-polycondensation and polycondensation stages, continuous polymerization, and heat supply in continuous production processes has become an urgent technical problem to be solved.

[0048] To address the aforementioned issues, this application provides a continuous production apparatus for poly(1,4-cyclohexanediethanol terephthalate), comprising: an esterification reactor, a first polycondensation reactor, and a second polycondensation reactor.

[0049] An esterification reactor is used to carry out esterification reactions on reactants to obtain esterified products.

[0050] The first polycondensation reactor includes a first reactor body and a stirring device. Multiple chambers are arranged sequentially along the height direction in the first reactor body, and two adjacent chambers are connected. The stirring device is located in the chamber. The first reactor body has a first inlet and a first outlet connected to the chamber. The first inlet is connected to the esterification reactor. The first reactor body is used to receive esterified products and perform a pre-polycondensation reaction on the esterified products to obtain pre-polycondensed products.

[0051] The second polycondensation reactor is connected to the first discharge port. The second polycondensation reactor is used to receive the prepolymer and carry out the polycondensation reaction of the prepolymer to obtain the final polymer.

[0052] By setting up an esterification reactor, a first polycondensation reactor connected to the esterification reactor, and a second polycondensation reactor connected to the first discharge port, and by arranging multiple interconnected chambers along the height direction in the first reactor body of the first polycondensation reactor and installing stirring devices in the chambers, the esterified material can be continuously transferred and reacted in stages during the pre-polycondensation stage. This enhances the flow stability, heating uniformity, and by-product removal effect of the material during the pre-polycondensation process, which is conducive to the continuous and stable progress of the subsequent polycondensation reaction. Moreover, it avoids the phenomenon of reverse mixing between the material that has reacted for a period of time and the fresh material that has just entered the reactor, thereby improving the stability of the final polymer molecular weight growth and product consistency.

[0053] The technical solution of this application and how the technical solution of this application solves the above-mentioned technical problems are described in detail below with specific embodiments. These specific embodiments can be combined with each other, and the same or similar concepts or processes may not be described again in some embodiments. The embodiments of this application will now be described with reference to the accompanying drawings.

[0054] This application provides a continuous production apparatus for poly(1,4-cyclohexanedimethyl terephthalate), such as... Figure 1 and Figure 2 As shown, it includes: an esterification reactor 100, a first polycondensation reactor 200, and a second polycondensation reactor 300.

[0055] The esterification reactor 100 is used to carry out the esterification reaction of the reactants to obtain the esterified products.

[0056] The first polycondensation reactor 200 includes a first reactor body 210 and a stirring device 250. Multiple chambers 230 are arranged sequentially along the height direction inside the first reactor body 210. Two adjacent chambers 230 are connected. The stirring device 250 is disposed in the chamber 230. The first reactor body 210 has a first inlet 211 and a first outlet 212 that are connected to the chambers 230. The first inlet 211 is connected to the esterification reactor 100. The first reactor body 210 is used to receive esterified products and perform a pre-polycondensation reaction on the esterified products to obtain pre-polycondensed products.

[0057] The second polycondensation reactor 300 is connected to the first discharge port 212. The second polycondensation reactor 300 is used to receive the prepolymer and carry out the polycondensation reaction of the prepolymer to obtain the final polymer.

[0058] Esterification reactor 100 refers to a reaction unit used to receive terephthalic acid and 1,4-cyclohexanediethanol as reactants and complete the esterification reaction under heating conditions. The outlet of esterification reactor 100 is directly connected to the first feed port 211 of the first polycondensation reactor 200 so that the esterified material can immediately enter the subsequent reaction section after formation.

[0059] The esterification reactor 100 can be a vertical batch reactor, a horizontal cylindrical reactor, or a continuous flow reactor with stirring and devolatilization interfaces.

[0060] The first polycondensation reactor 200 is an intermediate reaction unit for pre-polycondensation treatment of esterified products. The first polycondensation reactor 200 is used to further remove low molecular weight by-products and increase the molecular weight of the material under higher temperature and continuous stirring conditions, so that the material forms a pre-polycondensate with suitable viscosity and reactivity before entering the final polycondensation.

[0061] The first reactor body 210 refers to the main cylindrical body that constitutes the outer shell of the first polycondensation reactor 200 and contains multiple chambers 230. The first reactor body 210 provides a closed and controllable reaction space for the pre-polycondensation reaction and provides a structural basis for material transfer, heat transfer and devolatilization between the chambers 230.

[0062] The first reactor body 210 can be in the form of a vertical cylinder, a segmented tower, or a multi-segment cylinder connected in series. The outer wall of the first reactor body 210 can be fitted with a jacket or insulation layer.

[0063] The stirring device 250 refers to the actuator installed inside the first polycondensation reactor 200, which is used to mix the materials in the chamber and renew the surface, thereby promoting the release and discharge of low-molecular-weight byproducts.

[0064] The mixing device 250 can be a single-layer or multi-layer paddle mixer, anchor mixer, ribbon mixer or frame mixer.

[0065] Multiple chambers 230 refer to the separate reaction spaces arranged sequentially and connected adjacently along the height direction within the first reactor body 210. Their function is to decompose the prepolymerization process into multiple continuous reaction stages, so that the material can complete heat transfer, devolatilization and molecular weight increase as it flows segment by segment along the height direction, thereby reducing the impact of backmixing and uneven residence time distribution in a single space.

[0066] Adjacent chambers 230 can be interconnected through appropriate connecting structures to form a top-to-bottom, independent flow path, avoiding backmixing.

[0067] like Figure 2 As shown, the first inlet 211 can be arranged in the upper or middle part near the top chamber 230 to match the flow direction of the esterified material, and the first outlet 212 can be arranged in the lower or side part near the end chamber 230, and can be used with the heat-insulated pipeline to achieve stable transfer.

[0068] The second polycondensation reactor 300 refers to a subsequent reaction unit connected to the first outlet 212 of the first polycondensation reactor 200, used to further polycondense the prepolymer to generate the final polymer.

[0069] Specifically, in the polyester production process, the reactants first enter the esterification reactor 100 and complete the esterification reaction to form esters. The esters then enter the first polycondensation reactor 200 through the chamber 230 connected to the first feed port 211. After entering, they undergo a pre-polymerization process in a series of chambers 230 arranged along the height direction. Since the chambers 230 are interconnected and the stirring device 250 can turn and refresh the materials in the chambers, a relatively stable temperature and concentration distribution can be formed when the materials flow in stages. At the same time, by-products are continuously removed under the conditions of interconnected chambers 230 and heat transfer and devolatilization, so that the esters are gradually transformed into prepolymers with a suitable degree of polymerization.

[0070] Subsequently, the prepolymer is continuously fed into the second polycondensation reactor 300 through the first discharge port 212, where it continues to undergo polycondensation reaction and completes final polymerization, ultimately yielding the final polymer.

[0071] Understandably, this continuous production unit separates esterification, prepolymerization, and final polymerization into continuously connected reaction sections, and uses a multi-chamber 230 structure to segmentally control the prepolymerization process. The material forms a clear process sequence in the flow path, and the local residence state and backmixing degree are constrained. Heat input, material renewal, and by-product removal can be matched with viscosity changes, thereby suppressing problems such as flow stagnation, local solidification, and unstable reaction connection in continuous operation, and improving the stability of the molecular weight growth of the final polymer and product consistency.

[0072] It should be understood that the above examples are merely illustrative and not limiting. Without departing from the concept of this application, the specific shape of the reactor, the connection method, and the selection of materials can be replaced with equivalent ones according to the process conditions.

[0073] In one possible implementation, reference is made to Figure 2As shown, the first reactor body 210 includes a first shell 270 and a plurality of flow-blocking elements 260 disposed within the first shell 270. The plurality of flow-blocking elements 260 are arranged at intervals along the height direction of the first shell 270. The flow-blocking elements 260 and the first shell 270 enclose a chamber 230, and a heating coil is disposed in each chamber 230.

[0074] The flow deflector 260 is an internal component disposed inside the first housing 270 for separating and guiding the flow of molten material.

[0075] The heating coil is used to heat chamber 230 to promote the forward reaction.

[0076] Reference Figure 2 As shown, the flow deflector 260 is disposed inside the first housing 270 and arranged at intervals along the height direction of the first housing 270, dividing the continuous space inside the first housing 270 into multiple interconnected chambers 230, so that the esterified material entering the first housing 270 can be retained, heated and complete the pre-condensation reaction in each chamber 230 in sequence.

[0077] The flow deflector 260 can be fixedly connected to or detachably connected to the inner wall of the first housing 270.

[0078] In one possible implementation, the first housing 270 may be a cylindrical, square, or elliptical cylindrical structure to adapt to different equipment layouts and fluid distribution requirements; the flow baffle 260 may be a plate-shaped, arc-shaped, or zigzag-shaped structure to form different flow channel blocking effects and material renewal modes.

[0079] It should be understood that the flow baffle 260 is usually a fixed part, which mainly changes the flow path of the material in the first reactor body 210 by blocking, diverting and segmenting. It can also be replaced by baffles, guide plates or weirs to achieve similar separation functions without departing from the concept of this application. All of the above structures are intended to form a multi-level chamber 230 pre-condensation space.

[0080] Specifically, when the esterified product output from the esterification reactor 100 enters the first reactor body 210, the material is transferred from top to bottom between the chambers 230. In each chamber 230, it undergoes local mixing, heat transfer, and by-product escape, thereby enabling the prepolymerization reaction to proceed unidirectionally along the height direction, avoiding backmixing, and making the residence time distribution more uniform. The phenomena of local overheating and local underreaction are reduced accordingly, which is conducive to maintaining the continuous stability of the prepolymerization process.

[0081] In addition, the structure of the staged chamber 230 can extend the effective reaction path of the material in the first reactor body 210, so that the prepolymer has reached a relatively consistent reaction degree before being output to the second polycondensation reactor 300, thereby reducing the load fluctuation of the subsequent polycondensation stage and improving the stability of the molecular weight growth of the final polymer.

[0082] It should be understood that the above examples are merely illustrative and not limiting. Any scheme that uses the same or equivalent technical means to achieve chamber 230 separation, flow control and segmented reaction should fall within the protection scope of this application.

[0083] Furthermore, such as Figure 2 As shown, the flow deflector 260 includes a base plate 261 and a side plate 262. One end of the base plate 261 is connected to the side plate 262, and the other end of the base plate 261 is connected to the first housing 270.

[0084] like Figure 2 As shown, the base plate 261 can be installed on the inner wall of the first housing 270 or integrally formed with the inner wall thereon. The base plate 261 is used to withstand the forces caused by the static pressure of the polyester melt and the agitation.

[0085] Side plate 262 can be disposed at the other end of base plate 261 and form an angle or bend connection with base plate 261. The upper edge of side plate 262 can approach adjacent baffle 260 to form a suitable baffle height.

[0086] In one possible implementation, the base plate 261 can be a flat plate structure, a reinforced plate structure with folded edges, or a load-bearing plate structure with reinforcing ribs; the side plate 262 can be a straight plate structure, an arc plate structure, or a reinforced plate structure with folded edges.

[0087] In one possible implementation, reference is made to Figure 2 As shown, along the height direction of the first reactor body 210, adjacent chambers 230 are connected by pipes 220. Pipes 220 are located outside the first shell 270, and control valves 240 are installed on pipes 220.

[0088] Along the height direction of the first reactor body 210, an overflow port 263 is provided on the side plate 262 above the stirring device 250, and the overflow port 263 is connected to the chamber 230 where the stirring device 250 is located.

[0089] It is understandable that pipe 220 and overflow port 263 together constitute the directional mass transfer and directional flow structure between the internal chambers 230 of the first polycondensation reactor 200. Pipe 220 is used to establish a controlled external connection between adjacent chambers 230, and overflow port 263 is used to trigger the overflow transfer of material when the liquid level in the chamber 230 above the stirring device 250 reaches the height of overflow port 263. This allows for both step-by-step transport between chambers 230 according to process requirements and automatic compensation and buffering through liquid level differences.

[0090] Pipeline 220 can be arranged outside the first housing 270 to avoid occupying the internal space of the first housing 270 and reduce the retention of high-viscosity polyester melt near the inner wall of the first housing 270; control valve 240 can be installed on pipeline 220, and control valve 240 can adjust the on / off state and flow rate according to the pressure, liquid level and material viscosity in each chamber 230; overflow port 263 is opened on side plate 262 and located above stirring device 250, so that the material after heating and reaction in chamber 230 can overflow the side plate 262 to form a controllable overflow after reaching a certain liquid level.

[0091] In one possible implementation, the pipe 220 can be a straight pipe, a bend, or a jacketed pipe with an insulation layer. A straight pipe is easier to process and install, while a bend is easier to bypass the equipment support structure and adapt to the spatial arrangement of the multi-chamber 230. A jacketed pipe can maintain the temperature of the polyester melt through a heating medium, reducing the viscosity increase and local crystallization of the polyester melt during transportation. The control valve 240 can be a ball valve, a butterfly valve, or a gate valve. The overflow port 263 can be a round hole, a strip-shaped port, or an opening with a guide groove, without specific limitations.

[0092] In addition, it should be noted that each chamber 230 may be equipped with a heating element, which can heat the material in the chamber 230 to promote the polycondensation reaction.

[0093] In one possible implementation, reference is made to Figure 3 As shown, the second polycondensation reactor 300 includes a second shell 310, a main shaft 320, and a plurality of connecting members 330. The second shell 310 is connected to the first discharge port 212. The main shaft 320 is inserted into the second shell 310 along the extending direction of the second shell 310. The plurality of connecting members 330 are disposed on the main shaft 320 and arranged at intervals along the extending direction of the main shaft 320. The connecting members 330 are configured to rotate within the second shell 310 to stir the reactants within the second shell 310.

[0094] The second shell 310 is a closed reaction shell that contains and completes the polycondensation reaction. The interior of the second shell 310 forms a reaction space for the prepolymer to stay, mix and devolatilize. The second shell 310 is connected to the first outlet 212 to receive the prepolymer output from the first polycondensation reactor 200.

[0095] The main shaft 320 is a transmission component arranged along the axial direction of the housing and rotating under driving action, used to drive multiple connecting parts 330 to move synchronously.

[0096] Multiple connectors 330 are stirring components installed on the outer periphery of the main shaft 320 for applying shearing, tumbling and scraping action to high-viscosity materials. During rotation, the connectors 330 can continuously update and disturb the material in the second shell 310, thereby maintaining the activated state of the polycondensation reaction interface.

[0097] The second shell 310 can be horizontal and connected to the first discharge port 212 via a flange, pipeline or sealing joint, so that the prepolymer can continuously enter the feed end of the second polycondensation reactor 300.

[0098] The main shaft 320 is inserted into the second housing 310 along the extending direction of the second housing 310, and the main shaft 320 and the second housing 310 are coaxially arranged to reduce rotational load and facilitate the overall agitation of the material inside the second housing 310. One or both ends of the main shaft 320 can extend out of the second housing 310 and be connected to a geared motor, coupling or other drive mechanism to achieve continuous or intermittent drive.

[0099] Multiple connectors 330 are disposed on the main shaft 320 and arranged at intervals along the extension direction of the main shaft 320. The connectors 330 can be fixed to the outer periphery of the main shaft 320 by welding, key connection, bolt connection or snap-fit. A preset working gap is maintained between each connector 330 and the inner wall of the second housing 310 so as to form a scraping film or turbulence effect when rotating, while avoiding mechanical interference due to the gap being too small.

[0100] In one possible implementation, the connector 330 may adopt a disc-shaped, frame-shaped, blade-shaped, ribbon-shaped, or scraper-shaped structure. The disc-shaped structure is suitable for enhancing radial tumbling, the blade-shaped structure is suitable for forming axial conveying and shearing, and the scraper-shaped structure is more conducive to scraping and renewing the inner wall of the housing.

[0101] Specifically, the prepolymer is discharged from the first outlet 212 of the first polycondensation reactor 200 and enters the interior of the second shell 310. The main shaft 320 rotates continuously along the extension direction of the second shell 310 under the drive mechanism. Multiple connecting parts 330 move synchronously with the main shaft 320 and cut, turn over and scrape the high-viscosity material entering the shell. Since the connecting parts 330 are arranged at intervals along the axial direction of the main shaft 320, the material is continuously pushed, turned back and redispersed during the rotation, thereby reducing local stagnation areas and backmixing, and promoting a relatively uniform state of heating and stirring of the material throughout the shell.

[0102] In addition, the working gap between the connector 330 and the inner wall of the second housing 310 allows the material surface to be continuously renewed. The thin film material is more likely to release small molecule byproducts generated during the polycondensation process under high temperature conditions, thereby enhancing the devolatilization effect and promoting the polycondensation equilibrium to move towards the formation of the final polymer. It also helps to improve the consistency of the molecular weight growth of the final polymer and the stability of the device during long-term operation.

[0103] It should be understood that the above examples are for illustrative purposes only and are not intended to be limiting.

[0104] In one possible implementation, such as Figure 3 As shown, the spindle 320 includes a first shaft 321 and a second shaft 322, with the second shaft 322 disposed outside the first shaft 321.

[0105] The first shaft 321 has a main channel 3211 inside, and an opening is provided on the shaft wall of the first shaft 321 for connecting the connector 330 and the main channel 3211.

[0106] The second shaft 322 and the first shaft 321 form an annular channel 3221. The annular channel is used to connect the outlet of the connector 330. Both the main channel 3211 and the annular channel 3221 are used to transfer heat medium.

[0107] It is understandable that the main shaft 320 forms an independent dual flow channel through the main channel 3211 inside the first shaft 321 and the annular channel 3221 formed by the first shaft 321 and the second shaft 322. It can transport heat medium separately, realize the supply and return of heat medium nearby, and avoid mutual disturbance of the medium entering and leaving the flow channel.

[0108] In one possible implementation, combining Figure 3 and Figure 4As shown, the connector 330 includes a hollow disc 331, a ring 336, a first scraper 332, and a second scraper 333. The hollow disc 331 is connected by the ring 336. The first scraper 332 is disposed on the edge of the hollow disc 331, and the second scraper 333 is disposed on the side of the ring 336. The first scraper 332 is used to fit against the inner wall of the second housing 310, and the second scraper 333 is used to fit against the side of the adjacent connector 330.

[0109] The hollow disc 331 can be coaxially fixed to the main shaft 320, or detachably connected to the main shaft 320. The disc 331 can rotate synchronously with the main shaft 320 to continuously disturb the high-viscosity polyester melt during the polycondensation reaction, thereby promoting the reaction.

[0110] The first scraper 332 is disposed on the edge of the hollow disc 331 and is used to form a circumferential scraping along the inner wall of the second housing 310, so that the polyester melt attached to the inner wall of the second housing 310 is continuously renewed and falls back into the reaction zone, thereby reducing the formation of thermal resistance layer and retention layer.

[0111] The second scraper 333 is disposed on the surface of the ring 336 and is used to scrape the sides of the adjacent connectors 330 to clean the polyester melt and by-products that may be deposited on the sidewalls between the discs, so that the gap between the adjacent connectors 330 remains relatively unobstructed and the problem of material accumulation and carbonization near the disc surface is reduced.

[0112] In one possible implementation, the hollow disc 331 can be a composite disc 331 with guide holes and weight reduction holes; the first scraper 332 and the second scraper 333 can respectively adopt a straight blade, a beveled blade or an arc blade structure, or they can adopt a sheet-like, elastic sheet-like or wear-resistant strip-like structure.

[0113] Specifically, during the rotation of the main shaft 320, the hollow disc 331 causes axial and radial disturbance to the material on the one hand, and on the other hand, with the help of the first scraper 332, it continuously scrapes along the inner wall of the second shell 310, timely peeling off the high-viscosity polyester melt adhering to the surface of the second shell 310 and reintroducing it into the reaction zone to continue stirring and reacting; and the second scraper 333 can simultaneously remove the residual material on the side of the adjacent connecting parts 330, so that the disc side area between the hollow discs 331 is not prone to the formation of accumulation layers and local stagnation areas.

[0114] Understandably, the inner wall and sides of the pan can be continuously renewed, allowing heat to be transferred more effectively to the interior of the reactants. Small molecule byproducts generated during the polycondensation process are also more likely to escape from the material surface and be extracted, thereby reducing the probability of local overheating, wall adhesion, and crystallization. This also keeps the material in a relatively uniform residence state within the second polycondensation reactor 300, improving heat transfer and devolatilization efficiency, reducing material adhesion, accumulation, and blockage, which is beneficial for maintaining the stable operation of the continuous polycondensation process and improving the uniformity of the final polymer molecular weight growth and the consistency of preparation.

[0115] It should be understood that the above examples are for illustrative purposes only and are not intended to be limiting.

[0116] Furthermore, in combination Figure 3 and Figure 4 As shown, the hollow disk 331 has a first channel 334 and a second channel 337. The first channel 334 is connected to the main channel 3211, and the second channel 337 is connected to the annular channel 3221. Both the first channel 334 and the second channel 337 are used to transfer heat medium.

[0117] Specifically, in combination Figure 3 and Figure 4 As shown, a first channel 334 and a second channel 337 can be provided inside the hollow disc 331. The heating medium circulates within the hollow disc 331, allowing the heating medium to exchange heat with the hollow disc 331. This provides stable heat compensation to the material in the second polycondensation reactor 300, maintaining the temperature conditions required for the polycondensation reaction. This ensures that the material can maintain good flowability and reaction uniformity even at high viscosity, reducing abnormal increases in polyester melt viscosity, surface crystallization, or flow obstruction caused by localized cooling. It also improves the heat transfer and devolatilization effect of the polyester melt and helps to improve the continuous stability of the final polymer molecular weight growth.

[0118] like Figure 3 and Figure 4 As shown, the first channel 334 is connected to the main channel 3211. The first channel 334 is used to receive fresh heat medium and perform heat exchange. After the heat exchange is completed, the heat medium can flow out of the hollow disk 331 through the second channel 337 and flow to the annular channel 3221 for discharge. The two channels independently transport the heat medium, effectively preventing the medium from mixing.

[0119] In addition, it should be noted that, such as Figure 4 As shown, a reinforcing column 335 can be provided on the hollow disc 331, which can improve the overall rigidity and fatigue resistance of the hollow disc 331 without significantly increasing its weight, disperse the fluid impact stress during the stirring process, and prevent the hollow disc 331 from deforming and cracking.

[0120] In one possible implementation, such as Figure 3 As shown, the second housing 310 is a cylindrical body. One end of the second housing 310 is provided with a second feed port 311, and the other end of the second housing 310 is provided with a second discharge port 312. The second feed port 311 is connected to the first discharge port 212, and a screw is provided at the second discharge port 312.

[0121] The second housing 310 can be arranged horizontally, with the axis of the cylindrical body aligned with the extension direction of the main shaft 320. The second feed port 311 is located near the front end cover, and the second discharge port 312 is located near the rear end cover.

[0122] Specifically, the prepolymer moves from the second inlet 311 to the second outlet 312 in the second shell 310. At the same time, the surface is continuously renewed by the stirring, scraping and turning action of the main shaft 320 and its connecting parts 330, and a suitable reaction temperature is maintained under the action of an external heat source, so that the residual oligomers further undergo condensation and gradually increase the molecular weight.

[0123] Furthermore, referring to Figure 3 As shown, a screw can be installed at the second discharge port 312. The rotation of the screw can remove the material accumulated at the second discharge port 312 and prevent blockage.

[0124] In one possible implementation, such as Figure 1 As shown, the esterification reactor 100 includes a first esterification reactor 110 and a second esterification reactor 120.

[0125] The first esterification reactor 110 is used to feed the reactants for a preliminary esterification reaction to obtain the first esterified product. The esterification rate of the first esterification reactor 110 is controlled to be greater than or equal to 86% and less than or equal to 92%.

[0126] The second esterification reactor 120 is connected to the first esterification reactor 110, and the esterification rate of the second esterification reactor 120 is controlled to be greater than or equal to 96.5% and less than or equal to 99.5%.

[0127] Understandably, the esterification rate of the first esterification reactor can be controlled within the range of 86% to 92%. This allows for the rapid conversion of most of the raw materials while maintaining good fluidity and avoiding side reactions caused by prolonged high-temperature reactions in the first esterification reactor 110.

[0128] The first esterified product after the reaction is completed can enter the second esterification reactor for deep esterification. The esterification rate can be controlled within the range of 96.5% to 99.5%, ensuring that the content of residual small molecules meets product requirements, stabilizing subsequent reaction conditions, and avoiding the need to significantly increase the reaction temperature and extend the residence time in pursuit of the ultimate conversion rate, thus preventing the material from thermally degrading and turning yellow. At the same time, it effectively controls production energy consumption and balances product quality and operating costs.

[0129] In addition, it should be noted that the second esterification reactor 120 includes a reactor body 121 and a plurality of mixing devices 122. The reactor body 121 is connected to the first esterification reactor 110. The reactor body 121 has a plurality of reaction chambers 123 arranged sequentially along the extension direction. Each reaction chamber 123 is provided with a corresponding mixing device 122. The mixing device 122 is used to stir and mix the reactants in the reaction chamber 123.

[0130] The second esterification reactor 120 is a multi-chamber continuous reaction device arranged in series with the first esterification reactor 110. It is used to further mix and esterify the first ester in multiple reaction chambers 123 arranged in sequence, so as to improve the esterification depth and stabilize the discharge state.

[0131] The mixing device 122 installed in each reaction chamber 123 is used to continuously stir the material in the reaction chamber 123, so that the liquid phase components, temperature and reaction products are more uniformly distributed, reducing local concentration differences and heat transfer dead zones, thereby improving the continuity of the esterification reaction.

[0132] In one possible implementation, the first polycondensation reactor 200 is connected to the second esterification reactor 120, and the pre-polycondensation reaction is carried out in the first polycondensation reactor 200 to obtain a pre-polymer with a molecular weight greater than or equal to 1500 and less than or equal to 3500.

[0133] The polycondensation reaction is carried out in the second polycondensation reactor 300 to obtain a final polymer with a molecular weight greater than or equal to 16,000 and less than or equal to 18,000.

[0134] It is understandable that by controlling the molecular weight of the prepolymer to between 1500 and 3500 through the first polycondensation reactor 200, the molecular chain growth can be initially achieved and most small molecules can be removed. If the molecular weight is lower than 1500, a large number of small molecules will enter the subsequent system, which will easily cause foaming and entrainment. If the molecular weight is higher than 3500, the melt viscosity will be too high, increasing the energy consumption for conveying and stirring.

[0135] The prepolymer is fed into the second polycondensation reactor for deep polycondensation, controlling the final polymer molecular weight to be between 16,000 and 18,000. A final polymer molecular weight of not less than 16,000 ensures sufficient mechanical and heat resistance properties; a final polymer molecular weight of not more than 18,000 prevents excessively high melt viscosity, which could lead to processing difficulties, and avoids thermal degradation and color deterioration of the material caused by prolonged high-temperature polymerization, thus reducing production energy consumption while meeting product quality requirements.

[0136] In addition, it should be noted that heating jackets 400 are provided on the outer periphery of the esterification reactor 100, the first polycondensation reactor 200 and the second polycondensation reactor 300. The heating jackets 400 are used to heat the temperature inside the esterification reactor 100, the first polycondensation reactor 200 and the second polycondensation reactor 300.

[0137] Understandably, both esterification and polycondensation reactions require heating. The heating jacket 400 completely covers the outer perimeter of the reactor, allowing the heat medium to exchange heat evenly along the circumference and axial direction of the cylinder wall. Compared to internal coil heating, there are no local low-temperature blind spots on the cylinder wall, and the melt and slurry inside the reactor are heated evenly, which can maintain the exclusive reaction temperature range of each process and ensure the continuous and stable progress of esterification and polycondensation reactions.

[0138] The heating jacket 400 is arranged on the outside of the reactor, which does not occupy the material residence volume, does not hinder the operation of the stirring structure inside the reactor, avoids short circuits and material accumulation caused by the heat exchange components blocking the material flow, and improves the effective processing capacity of the reactor.

[0139] like Figure 1 As shown, the continuous production unit also includes a slurry preparation structure 500 and a pelletizing unit 600.

[0140] The slurry preparation structure 500 is connected to the inlet of the esterification reactor 100. The slurry preparation structure 500 is used to melt and mix the reactants to form the reactants.

[0141] The pelletizing unit 600 includes a pelletizer 610, a dryer 620, and a slice classifier 630 connected in sequence. The pelletizer 610 is connected to the outlet of the second polycondensation reactor 300. The pelletizer 610 is used to receive the polycondensate produced in the second polycondensation reactor 300 and pelletize it. The dryer 620 is used to dry the pellets. The slice classifier 630 is used to receive the dried pellets and slice them.

[0142] The slurry mixing structure 500 can stir and mix the liquid and solid phase materials of polyester raw materials to form the reactants, stabilize the feed ratio, prevent powder agglomeration and blockage, and improve the esterification reaction efficiency.

[0143] The pelletizing unit 600 consists of a pelletizer 610, a dryer 620, and a slice classifier 630 connected in sequence. The pelletizer 610 receives the high-viscosity condensate produced by the second condensation reactor 300 and completes online pelletizing. The dryer 620 removes moisture and low-molecular-weight impurities from the particles. The slice classifier 630 screens and sized qualified slices and separates broken particles and irregularly shaped materials.

[0144] Furthermore, a filter 800 can be installed between the second polycondensation reactor 300 and the pelletizing unit 600. It is understandable that the high-temperature, high-viscosity polyester melt in the second polycondensation reactor 300 is subjected to prolonged heating, which easily produces impurities such as coke particles, carbonized carbon deposits, metal wear debris, coking slough-off lumps, and inorganic additive agglomerates. The filter 800 can trap these impurities, preventing them from entering the pelletizer 610 with the melt, thus eliminating black spots, coke particles, and hard particles in the finished chips from the source, improving the appearance quality of the chips, and avoiding filament breakage, mold blockage, and product defects in downstream spinning and injection molding.

[0145] In one possible implementation, such as Figure 1 As shown, it also includes a slurry delivery pump 710, an esterification delivery pump 720, a prepolymer delivery pump 730, and a condensation polymer delivery pump 740.

[0146] The slurry delivery pump 710 is located between the slurry preparation structure 500 and the esterification reactor 100. The slurry delivery pump 710 is used to regulate the supply flow rate of slurry to the esterification reactor 100.

[0147] An esterification transfer pump 720 is disposed between the esterification reactor 100 and the first polycondensation reactor 200. The esterification transfer pump 720 is used to regulate the supply flow rate to the first polycondensation reactor 200.

[0148] A prepolymer transfer pump 730 is disposed between the first polycondensation reactor 200 and the second polycondensation reactor 300. The prepolymer transfer pump 730 is used to regulate the supply flow rate to the second polycondensation reactor 300.

[0149] A condensate transfer pump 740 is disposed between the second condensation reactor 300 and the pelletizing unit 600. The condensate transfer pump 740 is used to regulate the supply flow rate to the pelletizing unit 600.

[0150] The slurry conveying pump 710, ester conveying pump 720, prepolymer conveying pump 730 and condensate conveying pump 740 are all mechanical conveying components used for continuous material transfer.

[0151] Among them, the slurry delivery pump 710 is used to quantitatively pressurize and deliver the reactants output from the slurry preparation structure 500, the esterification delivery pump 720 is used to stably transfer the esterification output from the esterification reactor 100, the prepolymer delivery pump 730 is used to transfer the prepolymer output from the first polycondensation reactor 200 in an intermediate manner, and the polycondensation delivery pump 740 is used to transfer the polycondensation output from the second polycondensation reactor 300 at the end.

[0152] This setup, through segmented pumping and flow regulation, enables a continuous and controllable material connection between each reaction unit, thereby maintaining the feed balance at each stage of esterification, pre-condensation, and condensation, and reducing pressure fluctuations and uneven residence of high-viscosity polyester melt during the conveying process.

[0153] Finally, it should be noted that other embodiments of this application will readily conceive of by those skilled in the art upon consideration of the specification and practice of the application disclosed herein. This application is intended to cover any variations, uses, or adaptations of this application that follow the general principles of this application and include common knowledge or customary techniques in the art not disclosed herein, and is not limited to the precise structures described above and shown in the accompanying drawings, and various modifications and changes may be made without departing from its scope.

Claims

1. A continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate, characterized in that, include: An esterification reactor (100) is used to esterify the reactants to obtain esters; A first polycondensation reactor (200) includes a first reactor body (210) and a stirring device (250). A plurality of chambers (230) are arranged sequentially along the height direction in the first reactor body (210). Two adjacent chambers (230) are connected. The stirring device (250) is disposed in the chamber (230). The first reactor body (210) has a first inlet (211) and a first outlet (212) connected to the chamber (230). The first inlet (211) is connected to the esterification reactor (100). The first reactor body (210) is used to receive the esterified material and perform a pre-polycondensation reaction on the esterified material to obtain a pre-polycondensate. The second polycondensation reactor (300) is connected to the first discharge port (212). The second polycondensation reactor (300) is used to receive the prepolymer and perform a polycondensation reaction on the prepolymer to obtain the final polymer.

2. The continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate according to claim 1, characterized in that, The first reactor body (210) includes a first shell (270) and a plurality of flow-blocking elements (260) disposed in the first shell (270). The plurality of flow-blocking elements (260) are arranged at intervals along the height direction of the first shell (270). The flow-blocking elements (260) and the first shell (270) enclose the chamber (230), and each chamber (230) is provided with a heating coil.

3. The continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate according to claim 2, characterized in that, The flow deflector (260) includes a base plate (261) and a side plate (262). One end of the base plate (261) is connected to the side plate (262), and the other end of the base plate (261) is connected to the first housing (270).

4. The continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate according to claim 3, characterized in that, Along the height direction of the first reactor body (210), adjacent chambers (230) are connected by a pipe (220), the pipe (220) is located outside the first shell (270), and a control valve (240) is provided on the pipe (220). Along the height direction of the first reactor body (210), an overflow port (263) is provided on the side plate (262) above the stirring device (250), and the overflow port (263) is connected to the chamber (230) where the stirring device (250) is located.

5. The continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate according to claim 1, characterized in that, The second polycondensation reactor (300) includes a second shell (310), a main shaft (320), and a plurality of connectors (330). The second shell (310) is connected to the first discharge port (212). The main shaft (320) is inserted into the second shell (310) along the extension direction of the second shell (310). The plurality of connectors (330) are disposed on the main shaft (320) and spaced apart along the extension direction of the main shaft (320). The connectors (330) are configured to rotate within the second shell (310) to stir the reactants within the second shell (310).

6. The continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate according to claim 5, characterized in that, The main shaft (320) includes a first shaft (321) and a second shaft (322), wherein the second shaft (322) is disposed outside the first shaft (321); The first shaft (321) has a main channel (3211) inside, and an opening is provided on the shaft wall of the first shaft (321) for connecting the connector (330) and the main channel (3211). The second shaft (322) and the first shaft (321) form an annular channel (3221), which is used to connect the outlet of the connector (330). Both the main channel (3211) and the annular channel (3221) are used to transfer heat medium.

7. The continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate according to claim 6, characterized in that, The connector (330) includes a hollow disc (331), a ring (336), a first scraper (332), and a second scraper (333). The hollow disc (331) is connected by the ring (336). The first scraper (332) is disposed on the edge of the hollow disc (331), and the second scraper (333) is disposed on the side of the ring (336). The first scraper (332) is used to fit against the inner wall of the second housing (310), and the second scraper (333) is used to fit against the side of the adjacent connector (330).

8. The continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate according to claim 7, characterized in that, The hollow disk (331) has a first channel (334) and a second channel (337). The first channel (334) is connected to the main channel (3211), and the second channel (337) is connected to the annular channel (3221). Both the first channel (334) and the second channel (337) are used to transfer heat medium.

9. The continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate according to claim 5, characterized in that, The second housing (310) is a cylindrical body. One end of the second housing (310) is provided with a second inlet (311), and the other end of the second housing (310) is provided with a second outlet (312). The second inlet (311) is connected to the first outlet (212), and a screw is provided at the second outlet (312).

10. The continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate according to any one of claims 1-9, characterized in that, The esterification reactor (100) includes a first esterification reactor (110) and a second esterification reactor (120). The first esterification reactor (110) is used to perform a preliminary esterification reaction on the reactants to obtain a first esterified product, and the esterification rate of the first esterification reactor (110) is controlled to be greater than or equal to 86% and less than or equal to 92%. The second esterification reactor (120) is connected to the first esterification reactor (110), and the esterification rate of the second esterification reactor (120) is controlled to be greater than or equal to 96.5% and less than or equal to 99.5%.

11. The continuous production apparatus for poly(1,4-cyclohexanediethanol) terephthalate according to claim 10, characterized in that, The first polycondensation reactor (200) is connected to the second esterification reactor (120). The pre-polycondensation reaction is carried out in the first polycondensation reactor (200) to obtain a pre-polymer with a molecular weight greater than or equal to 1500 and less than or equal to 3500. The final polymer obtained by polycondensation reaction in the second polycondensation reactor (300) has a molecular weight greater than or equal to 16,000 and less than or equal to 18,000.

Citation Information

Patent Citations