Manufacturing method of pipe bend
By combining pre-bending and deep drawing with U- and O-bending processes, the wrinkling problem in tube bending manufacturing is solved, the quality of tube bending is improved, and it is suitable for applications such as vehicle dashboard reinforcement parts.
Patent Information
- Application Number
- CN202610374056.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-05-15
- Filing Date
- 2026-03-25
- Publication Date
- 2026-11-17
AI Technical Summary
In existing pipe bending manufacturing methods, the material shrinkage is large during U-bending, which easily forms wrinkles in the bent part, especially when the curvature is large, resulting in a decrease in the quality of the bent pipe.
Before pipe bending, pre-bending and deep drawing are performed. The two sides of the width direction are grasped and deep drawn, followed by U-bending and O-bending. The edges are cut or trimmed to avoid obstruction and suppress wrinkle formation.
It effectively suppresses material shrinkage in the bent section of the pipe, reduces wrinkles, and improves the quality of the bent pipe, making it suitable for applications such as vehicle dashboard reinforcement.
Smart Images

Figure CN123102797A_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to a method for manufacturing a bent pipe. Background Technology
[0002] As a method for manufacturing a bent pipe, Patent Document 1 discloses the following: When manufacturing the outer tube of a double-layered pipe, a planar plate obtained by unfolding the shape of the bent outer tube is drawn deep to form a half-pipe with a U-shaped cross-section and bent in the axial direction.
[0003] In this manufacturing method, a bent inner tube is inserted into the inside of the semi-tube body, and the semi-tube body and the inner tube are joined by welding at one end in the longitudinal direction. Then, the inner tube is bent like a mandrel so that the semi-tube body becomes a circular cross-section surrounding the inner tube.
[0004] Patent Document 1: Japanese Patent Application Publication No. 2017-100175
[0005] The method for manufacturing the outer tube described in Patent Document 1 can also be used to manufacture a bent tube that bends only in the axial direction rather than a double-layered tube by processing a half-tube formed from a planar plate, i.e., a blank, in a way that makes the cross-sectional shape O-shaped using so-called O-bending.
[0006] However, in the aforementioned manufacturing method, the planar plate obtained by unfolding and bending the tube shape through so-called U-bending is processed into a semi-tube with a U-shaped cross-section and bent in the axial direction. Therefore, the amount of material shrinkage increases during this processing, and there is a problem that the product is prone to wrinkling. Especially when the curvature of the bent part of the tube is large, wrinkles are easily formed in the bent part, which reduces the quality of the bent tube. Summary of the Invention
[0007] One aspect of this disclosure is to suppress wrinkles in the bent portion of the tube when using UO bending to manufacture a bent tube.
[0008] In one aspect of the method for manufacturing a bent tube, after pre-bending the blank into a bent shape along the tube, a deep drawing process based on stamping is performed. The pre-bent material is passed through the deep drawing process by gripping the edges on both sides in the width direction orthogonal to the central axis of the tube. Then, the deep-drawn material is U-bent in a way that the cross-sectional shape in the width direction is U-shaped, and the U-bent material is further O-bent in a way that the cross-sectional shape in the width direction is O-shaped.
[0009] In this way, according to the method for manufacturing a bent tube disclosed herein, before the blank is U-bent, the blank is pre-bent along the bending shape of the bent tube, and the edges on both sides in the width direction are grasped for deep drawing.
[0010] Therefore, in a U-shaped semi-tube formed by U-bending after deep drawing, it is possible to suppress the formation of wrinkles due to shrinkage of the material at the bent portion along the bending shape of the tube. Thus, according to the tube manufacturing method of this disclosure, it is possible to manufacture tubes with fewer wrinkles and of higher quality.
[0011] In one embodiment of this disclosure, the edges on both sides of the deep-drawn material in the width direction may be cut before U-bending. Alternatively, in another embodiment of this disclosure, the edges on both sides of the deep-drawn material in the width direction may be cut off before U-bending.
[0012] In this way, the edges that are gripped and extend outward from both sides in the width direction during deep drawing are cut or trimmed, so that the edges do not become an obstacle to U-bending, and the U-shaped half-tube can be produced more effectively through U-bending.
[0013] Alternatively, in one embodiment of this disclosure, the edges on both sides of the deep-drawn material can be bent inwards in the width direction before the U-bending. In this way, the edges on both sides of the half-tube formed by the U-bending bend in the width direction bend inwards, so when the half-tube is bent in the O-bending, the edges on both sides in the width direction come into face-to-face contact with each other, making it easier to move in the face direction. Therefore, it is possible to prevent the leading edges of the edges from colliding with each other and causing edge buckling.
[0014] Alternatively, in one embodiment of this disclosure, the bent tube can also be used as a dashboard reinforcement for a vehicle. This allows the dashboard reinforcement to be configured according to the bending shape of the tube, thus avoiding onboard components located below the vehicle's instrument panel or dashboard. Attached Figure Description
[0015] Figure 1 This is a front view showing the shape of the bend in the embodiment.
[0016] Figure 2 This is a flowchart illustrating the various steps of the manufacturing method for the bent pipe according to the embodiment.
[0017] Figure 3 This is an explanatory diagram illustrating the pre-bending process of the implementation method.
[0018] Figure 4 This is an explanatory diagram showing the deep drawing process of the implementation method.
[0019] Figure 5 This is an explanatory diagram showing the cutting process of the implementation method.
[0020] Figure 6This is an explanatory diagram illustrating the cutting process of the implementation method.
[0021] Figure 7 This is an explanatory diagram illustrating the U-bending process of the implementation method.
[0022] Figure 8 This is an explanatory diagram illustrating the O-bending process of the implementation method.
[0023] Figure 9 This is an explanatory diagram showing the cutting process of the first modified example.
[0024] Figure 10 This is an explanatory diagram showing the cross-sectional shape of the workpiece formed by the U-bending process in the second variation.
[0025] Figure 11 This is an explanatory diagram showing a bent pipe of a third modified example manufactured from blanks of different materials or plate thicknesses.
[0026] Figure 12 This is an explanatory diagram of a bent pipe, representing the fourth variation with an elliptical cross-section.
[0027] Figure 13 This is an explanatory diagram of a fifth modified example of a bent pipe with a flat portion provided on a part of its outer periphery.
[0028] Figure 14 This is an explanatory diagram of a sixth modified example of a bent pipe with one end reduced in diameter along its length. Detailed Implementation
[0029] Hereinafter, exemplary embodiments of the present disclosure will be described with reference to the accompanying drawings.
[0030] [constitute]
[0031] like Figure 1 As shown, the bent pipe 10 in this embodiment is a long cylindrical pipe, with multiple portions 12, 14, 16, and 18 along the central axis 10A being oriented towards... Figure 1 It bends vertically. This bend 10 is used as a dashboard reinforcement component configured along the width of the vehicle within the dashboard.
[0032] Furthermore, the dashboard reinforcement supports the steering column, dashboard, etc., and has the function of protecting occupants in the event of a collision. In addition, the bend 10 can be configured to avoid vehicle components inside the dashboard by bending as described above.
[0033] In this embodiment, the bend 10 is made by pressing... Figure 2 The processes S10 to S60 (where S represents a step) shown are performed sequentially. Figure 3The blank 20 shown in (A) is manufactured by processing. In addition, the blank 20 is a structure made by processing steel plates such as iron and stainless steel into a size corresponding to the length and thickness of the bent pipe 10.
[0034] like Figure 2 As shown, in manufacturing the bend 10, firstly, in the pre-bending process of S10, the bend is... Figure 3 The blank 20 shown in (A) is bent along the bending shape of the bend 10 in the direction of the central axis 10A of the bend 10. The result is as follows: Figure 3 As shown in (B), the blank 20 is processed into a workpiece 22 whose plate surface is bent at the above-mentioned multiple locations 12, 14, 16, 18.
[0035] Next, in the deep drawing process of S20, by using Figure 4 (A) and Figure 4 The stamping of the lower die 32 and upper die 34 shown in (B) performs deep drawing on the plate-shaped workpiece 22 that has been bent in the pre-bending process of S10.
[0036] The upper die 34 has a V-shaped protrusion 34A whose cross-sectional shape in the width direction corresponds to the width direction of the workpiece 22 and is bent into a V shape at the center. The lower die 32 has a concave portion 32A corresponding to the protrusion 34A of the upper die 34. Furthermore, the width direction of the workpiece 22 refers to the direction orthogonal to the central axis 10A of the length direction of the bent tube 10, and the cross-sectional shape in the width direction represents the shape of the cross-section obtained by cutting with a plane orthogonal to the central axis 10A.
[0037] In order to perform deep drawing on the entire length of the workpiece 22, the upper die 34 and the lower die 32 have approximately the same length as the workpiece 22. Moreover, the protrusion 34A and the concave portion 32A are continuously provided in almost the entire length of the upper die 34 and the lower die 32, and are bent upward and downward in accordance with the bending shape of the workpiece 22 (i.e., the bent tube 10).
[0038] In this deep drawing process, such as Figure 4 As shown in (A), the edges 22A and 22B on both sides of the workpiece 22 in the width direction are placed on the two ends of the lower die 32 in the width direction, and pressing members 36A and 36B are placed on them. During the deep drawing process, the pressing members 36A and 36B are subjected to force from above toward the edges 22A and 22B of the workpiece 22.
[0039] Therefore, the edges 22A and 22B of the workpiece 22 are gripped between the pressing parts 36A and 36B and the lower die 32, which can suppress wrinkles in the workpiece 22 caused by the deep drawing process using the lower die 32 and the upper die 34.
[0040] In addition, such as Figure 4As shown in (B), during the deep drawing process, the upper die 34 and the lower die 32 use the protrusion 34A and the concave portion 32A to press down the flat portion between the edge portion 22A and 22B of the workpiece 22 so that the workpiece 22 is gently recessed.
[0041] That is, the protrusion 34A of the upper mold 34 and the concave portion 32A of the mold 32 form a V-shape with the central portion of the V-shape bent, thus as... Figure 4 As shown in (D), the cross-sectional shape of the workpiece 24 in the width direction after deep drawing becomes the same V-shape as the upper die 34 and the lower die 32. Furthermore, as... Figure 4 As shown in (C), the V-shape is continuous along the length of workpiece 24.
[0042] In addition, during the deep drawing process, the edges 24A and 24B on both sides of the workpiece 24 in the width direction are sandwiched between the lower die 32 and the pressing parts 36A and 36B, so the edges 24A and 24B on both sides of the V-shape become shapes that extend outward.
[0043] In addition, Figure 4 middle, Figure 4 (A) indicates the configuration of the upper mold 34 and lower mold 32 before the workpiece 22 is processed. Figure 4 (B) indicates the configuration of the upper mold 34 and lower mold 32 after the workpiece 22 has been machined. Additionally, Figure 4 (C) is a perspective view showing the appearance of the workpiece 22 after deep drawing. Figure 4 (D) is a sectional view showing the cross-sectional shape of the workpiece 22 in the width direction. Furthermore, as described later... Figure 6 (A)~(D) Figure 7 (A) to (D) and Figure 8 (A)~(D) and Figure 4 The (A) to (D) correspond.
[0044] After the deep drawing process in S20, edges 24A and 24B remain on both ends of the workpiece 24 in the width direction, where they are gripped by the pressing parts 36A and 36B and the lower die 32. Therefore, in the cutting process in S30, as... Figure 5 (A) Figure 5 As shown in (B), the unwanted portions of the edges 24A and 24B are cut (i.e., severed).
[0045] As a result, in the cross-sectional shape of workpiece 24 in the width direction, the lengths of the edges 24A and 24B extending outward from both ends of the V-shape become shorter. Furthermore, in Figure 5 middle, Figure 5 (A) is a perspective view showing the appearance of the workpiece 24 after the cutting process. Figure 5 (B) is a sectional view showing the cross-sectional shape of the workpiece 24 in the width direction after the cutting process.
[0046] After the cutting process in S30, the process moves to the cutting-off process in S40. In this cutting-off process, the edges 24A and 24B extending outward in the width direction of the workpiece 24 are cut off in a V-shape in the width direction of the entire workpiece 24.
[0047] In this cutting process, the following is used Figure 6 (A) and Figure 6 The lower die 42 and upper die 44 are shown in (B). The lower die 42 and upper die 44 have approximately the same shape as the lower die 32 and upper die 34 used in the deep drawing process, and the depth of the processed portion of the workpiece 24 is deeper. That is, the vertical length of the lower die 42's recess 32A and the upper die 44's protrusion 34A is longer than that of the lower die 32's recess 32A and the upper die 34's protrusion 34A.
[0048] In the cutting process of S40, such as Figure 6 As shown in (A), after inserting the workpiece 24 into the recess 42A of the lower mold 42 and placing the upper mold 44 thereon, as shown in (A), Figure 6 As shown in (B), the upper die 44 is moved downward to stamp the workpiece 24.
[0049] As a result, the edges 24A and 24B on both ends of the workpiece 24 in the width direction extend straight along a V-shape. Therefore, as Figure 6 (C) Figure 6 As shown in (D), the cross-sectional shape of the workpiece 26 in the width direction after the cutting process becomes a V-shape without the edges 24A and 24B.
[0050] In this way, the workpiece 26, whose cross-sectional shape in the width direction becomes a V-shape in the cutting process of S40, is processed into a workpiece 28 whose cross-sectional shape in the width direction becomes a U-shape in the U-bending process of S50.
[0051] In the U-bending process, using Figure 7 (A) and Figure 7 The lower mold 52 and the upper mold 54 are shown in (B). The upper mold 54 has a U-shaped protrusion 54A, and the lower mold 52 has a U-shaped recess 52A corresponding to the protrusion 54A.
[0052] like Figure 7 As shown in (A), in the U-bending process, the workpiece 26 after the cutting process is placed on the recess 52A of the lower die 52. Then, as... Figure 7As shown in (B), by lowering the upper die 54 above the workpiece 26, the protrusion 54A of the upper die 54 is pressed into the recess 52A of the lower die 52 while the workpiece 26 is clamped. As a result, the workpiece 26 is stamped with a U-shaped cross-section in the width direction and is processed into... Figure 7 (C) Figure 7 Workpiece 28 is shown in (D).
[0053] Next, after the U-bending process in S50, an O-bending process is performed in S60, in which a bent tube 10 with an O-shaped cross-section is formed. Furthermore, after the O-bending process, the cylindrical bent tube 10 is completed by welding the end edge portion of the workpiece 28 that has been stamped into an O-shape.
[0054] In the O-bending process, using Figure 8 (A) and Figure 8 The lower mold 62 and the upper mold 64 are shown in (B). The upper mold 64 has a recess 64A that is bent into a semi-circular shape, and the lower mold 62 has a recess 62A that is bent into a semi-circular shape corresponding to the recess 64A.
[0055] like Figure 8 As shown in (A), in the O-bending process, the bottom portion of the workpiece 28 after the U-bending process is placed on the recess 62A of the lower die 62. Then, as... Figure 8 As shown in (B), by lowering the upper die 64 above the workpiece 28, the workpiece 28 is stamped by inwardly rolling the two ends of the workpiece 28 inward using the recess 64A of the upper die 64. The result is that the workpiece 28 becomes a tube with an O-shaped cross-section, and is processed into... Figure 8 (C) Figure 8 The bend 10 shown in (D)
[0056] [Effect]
[0057] As explained above, in the manufacturing method of the bent tube 10 according to this embodiment, a pre-bending process and a deep drawing process are performed before the blank 20 is processed into the shape of the bent tube 10 by the U-bending process and the O-bending process.
[0058] Furthermore, in the pre-bending process, the blank 20 is bent in a shape corresponding to the bending shape in the length direction of the bent tube 10. In the deep drawing process, the workpiece 22 after the pre-bending process is deep drawn in a way that the cross-sectional shape in the width direction becomes a V-shape that is bent more gently than in the U-shaped process.
[0059] In this deep drawing process, the workpiece 22 is deep-drawn while its edges 22A and 22B in the width direction are gripped between the lower die 32 and the pressing parts 36A and 36B. This prevents wrinkles from forming on the workpiece 22 due to the deep drawing process. Furthermore, in the U-bending process, the workpiece 26 after the deep drawing process is U-bent, thus preventing wrinkles from forming on the workpiece 22 due to the U-bending process.
[0060] Therefore, according to the method for manufacturing a bent tube according to this embodiment, it is possible to suppress the shrinkage of the material at multiple locations 12, 14, 16, 18 that form the bent portion of the bent tube 10, thereby preventing the formation of wrinkles and enabling the manufacture of a high-quality bent tube 10.
[0061] In addition, after the deep drawing process and before the U-bending process, in the cutting process, the unwanted parts of the edges 24A and 24B of the workpiece 24 that has undergone deep drawing are cut off, and in the slitting process, the remaining parts of the edges 24A and 24B are cut off according to the cross-sectional shape of the workpiece 24.
[0062] Therefore, according to this embodiment, the edges 22A and 22B that are gripped during deep drawing and extend outward from both sides in the width direction will not become an obstacle to the U-bending process. In the U-bending process, a workpiece 28 with a U-shaped cross-section in the width direction can be well manufactured.
[0063] [Other Implementation Methods]
[0064] The embodiments of this disclosure have been described above, but this disclosure is not limited to the above embodiments, and various methods can be used.
[0065] [First variation]
[0066] In the above embodiment, it is assumed that the workpiece 24 is cut off at both ends in the width direction in the cutting process, with the edges 24A and 24B of the workpiece 24 extending straight along the V-shape of the cross section in the width direction of the workpiece 24.
[0067] However, if the edges 24A and 24B on both sides of the workpiece 24 in the width direction are made to extend straight, then in the O-bending process, when the workpiece 28 with a U-shaped cross section is processed into an O-shaped cross section, the front ends on both sides of the workpiece 28 in the width direction collide with each other and bend.
[0068] Therefore, it can also be used in the cutting process. Figure 9 (B) and Figure 9The lower die 46 and upper die 48 shown in (C) bend the edges 24A and 24B of the workpiece 24 inward. That is, the opening width of the recess 46A of the lower die 46 is narrower than that in the above embodiment, and the shape of the protrusion 38A of the upper die 48 matches that of the recess 46A.
[0069] The result is that in the cutting process, such as Figure 9 As shown in (A), the edges 26A and 26B on both sides of the V-shape of the workpiece 26 can be bent inward, and the front ends of both sides of the workpiece 28 in the width direction can be prevented from colliding and bending during the O-bending process.
[0070] Furthermore, in order to prevent the front ends of both ends of the workpiece 28 in the width direction from colliding and bending during the O-bending process, it is not necessary to bend the edges 24A and 24B of the workpiece 24 inward during the cutting process. For example, although one manufacturing process is added, bending the edges 24A and 24B of the workpiece 24 inward during the subsequent process of the U-bending process can achieve the same effect as described above.
[0071] [Second variation]
[0072] In the above embodiment, assuming that in the U-bending process, as follows: Figure 7 As shown in (D), the cross-sectional shape of the workpiece 28 in the width direction is described as a U-shape with the left and right sides extending in a straight line from the U-shaped bend 28A.
[0073] However, as Figure 10 As shown, the cross-sectional shape of the workpiece 28 can also be independently provided with curved portions on the left and right sides 28B and 28C extending from the curved portion 28A at the center of the U-shape, so that the left and right sides 28B and 28C are curved.
[0074] In this way, for example, in the U-shaped cross-section of workpiece 28, the central portion of the U can be made to bulge outwards. As a result, after the O-bending process, when welding is performed at the joint of workpiece 28, gaps at the joint can be suppressed, and products can be manufactured well.
[0075] [Third variation]
[0076] In the above embodiment, it is assumed that the blank 20 is a component made by processing a steel plate into a size corresponding to the length and thickness of the bent pipe 10. However, the blank 20 can also be a so-called welded blank made by joining multiple steel plates of different thicknesses and materials by welding.
[0077] Thus, as Figure 11As illustrated, in the bend 10, the plate thickness and material can be set for each region 4A, 4B along the length direction according to the application, which can improve the ease of use of the bend 10.
[0078] [Fourth variation]
[0079] In the above embodiment, the cross-sectional shape of the bend 10 is described as an O-shape formed by an O-bending process, but this shape is not limited to... Figure 8 The circular shape shown is as follows: Figure 12 As shown, it can also be elliptical in shape. Furthermore, in Figure 12 middle, Figure 12 (A) represents the XX cut surface of bend 10. Figure 12 (B) indicates the cross-sectional shape of the bend 10 at the cut surface.
[0080] [Fifth variation]
[0081] In addition, such as Figure 13 As shown, a flat portion 6 can also be provided on the outer periphery of the bend 10. In this way, the flat portion 6 can be used, for example, as a fixing portion when fixing other components to the bend 10 or fixing the bend 10 to a vehicle, etc.
[0082] [Sixth variation]
[0083] In the above embodiment, the diameter of the bend 10 is described as constant along its entire length, but as... Figure 14 As illustrated, it is also possible that the diameter of one end 8 in the length direction is smaller than that of the other parts, and that end 8 is tapered to the point of being narrowed from the other parts.
[0084] [Other variations]
[0085] In the above embodiment, it is assumed that the bend 10 is used as a dashboard reinforcement for a vehicle, but the bend 10 may also be used for other purposes.
[0086] Furthermore, the function of one component in the above embodiments can be distributed among multiple components, or the functions of multiple components can be integrated into one component. Additionally, a portion of the structure in the above embodiments can be omitted. Furthermore, at least a portion of the structure in the above embodiments can be added to, substituted, or otherwise modified relative to the structures of other above embodiments.
[0087] [The technical concepts disclosed in this specification]
[0088] [Project 1]
[0089] A method for manufacturing a bent pipe, characterized by comprising:
[0090] The blank is pre-bent in a manner that follows the bending shape of the tube;
[0091] By grasping the edges on both sides of the width direction orthogonal to the central axis of the aforementioned bend, a deep drawing process based on stamping is performed on the pre-bent material.
[0092] The material that has undergone the above deep drawing process is U-bent in a manner that forms a U-shaped cross-section in the width direction; and
[0093] The material that has undergone the above-mentioned U-bending is then O-bent in such a way that the cross-sectional shape in the width direction becomes O-shaped.
[0094] [Project 2]
[0095] According to the manufacturing method of the bent pipe described in Project 1, it includes:
[0096] Before the aforementioned U-bending, the edges on both sides of the aforementioned width direction of the material that has undergone the aforementioned deep drawing process are cut.
[0097] [Project 3]
[0098] The manufacturing method of the bent pipe as described in item 1 or 2 includes:
[0099] Before the aforementioned U-bending, the aforementioned edges on both sides of the aforementioned width direction of the material that has undergone the aforementioned deep drawing process are cut off.
[0100] [Project 4]
[0101] The manufacturing method of the bent pipe described in any of Items 1 to 3 includes:
[0102] Before the aforementioned U-bending, the aforementioned edges on both sides of the aforementioned width direction of the material that has undergone the aforementioned deep drawing process are bent inward.
[0103] [Project 5]
[0104] According to the manufacturing method of the bent pipe described in any of items 1 to 4, among which,
[0105] The aforementioned bends are used in the dashboard reinforcement of vehicles.
[0106] Explanation of reference numerals in the attached figures
[0107] 10…bend; 20…blank; 22, 24, 26, 28…workpiece; 22A, 22B…edge.
Claims
1. A method for manufacturing a bent pipe, characterized in that, include: The blank is pre-bent in a manner that follows the bending shape of the tube; The pre-bent material is subjected to a deep drawing process based on stamping by gripping the edges on both sides of the width direction orthogonal to the central axis of the bend. The material that has undergone the deep drawing process is U-bent in such a way that the cross-sectional shape in the width direction becomes U-shaped; and The material that has undergone the U-bending is then O-bent so that its cross-sectional shape in the width direction becomes O-shaped.
2. The method for manufacturing a bent pipe according to claim 1, characterized in that, include: Before the U-bending, the edges on both sides of the material that has undergone the deep drawing process are cut.
3. The method for manufacturing a bent pipe according to claim 1 or 2, characterized in that, include: Before the U-bending, the edges on both sides of the material that has undergone the deep drawing process are cut off in the width direction.
4. The method for manufacturing a bent pipe according to claim 1 or 2, characterized in that, include: Before the U-bending, the edges on both sides of the material that has undergone the deep drawing process are bent inward in the width direction.
5. The method for manufacturing a bent pipe according to claim 1 or 2, characterized in that, The bent tube is used as a reinforcement for the vehicle's dashboard.