A method for controlling the power supply of marine welding with low spatter and high penetration stability

By dividing the welding current waveform into stages and combining arc state detection with adaptive compensation, the contradiction between low spatter and high penetration depth in ship welding was resolved, achieving stability and consistency in the welding process.

CN123103115APending Publication Date: 2026-11-17TIANJIN HEWEI BAICHUAN TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611532178.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-30
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing ship welding technology struggles to balance low spatter and high penetration depth, and the welding quality is unstable under external disturbances.

Method used

The welding current waveform is divided into droplet formation, necking and transition stages. By combining real-time detection and adaptive compensation of the arc state, the stability of droplet transition and the depth of penetration are improved through differentiated control of welding current and pulse energy.

Benefits of technology

It effectively reduces spatter, ensures sufficient penetration and stable welding process, and is suitable for welding medium and thick plates in ships, improving the consistency of welding quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FT_1
    Figure FT_1
Patent Text Reader

Abstract

This invention discloses a method for controlling a marine welding power supply with low spatter and high penetration stability, relating to the field of marine welding power supply control technology. The method divides the droplet transition cycle into a droplet formation stage, a droplet necking stage, and a droplet transition stage. During the droplet formation stage, a first peak current is output and periodically superimposed with pulse energy to deepen the penetration. During the droplet necking stage, the current is reduced to a base current to cause low-current necking of the liquid bridge and suppress spatter. During the droplet transition stage, a second peak current is output to accelerate droplet transition. Simultaneously, the regularity of droplet transition is detected; if it deviates from the preset rule, the first peak current and / or the first duration of the next cycle are adaptively adjusted. This application effectively balances low spatter, high penetration, and high stability, and is suitable for welding medium and thick plates in marine applications.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of marine welding power supply control technology, specifically a marine welding power supply control method with low spatter and high penetration stability. Background Technology

[0002] With the trend of ships becoming larger and lighter, the requirements for welding quality in ship structures are increasing. Not only are sufficient weld penetrations required to ensure structural strength, but also effective control of spatter, reduction of post-weld cleaning processes, and improvement of the consistency and stability of the welding process are needed while ensuring welding efficiency.

[0003] Currently, CO2 gas shielded welding and pulsed MIG / MAG welding methods are widely used in the shipbuilding welding field. Common methods for reducing welding spatter in existing technologies include: employing wire retraction feed control, which uses periodic forward and reverse feeding of the wire to utilize the contraction force generated by the current and the wire retraction force to make the droplet transition smoother, thereby reducing spatter generation; and using waveform control technology, which improves the droplet transition state by segmenting the welding current output waveform. For example, the droplet short-circuit transition period can be divided into stages such as the initial arc stage, the later arc stage, the initial short-circuit stage, and the droplet necking stage, with different current change rates and amplitudes set for each stage to reduce spatter generated during short-circuit transition. In addition, intelligent waveform control schemes are also used, which construct a correlation database by collecting historical welding data and use neural networks to output waveform adjustments to achieve closed-loop control of the welding process.

[0004] However, the existing technologies still have the following shortcomings in ship welding applications: First, while the wire retraction control method can effectively reduce spatter, the applicable current range is limited by the droplet transfer mode, and it can usually only be applied to a lower current range, making it difficult to meet the high current and high penetration requirements of thick plate welding in ships. Second, existing waveform control methods mainly focus on spatter suppression, with limited effect on improving weld penetration, easily leading to insufficient penetration in medium and thick plate welding in ships. Third, ship welding sites are subject to external disturbances such as inconsistent workpiece surface conditions and changes in assembly gaps. Existing control methods lack effective adaptive compensation mechanisms when the regularity of droplet transfer is disrupted by external disturbances, making it difficult to guarantee arc stability and consistent welding quality. Therefore, there is an urgent need for a ship welding power supply control method that can balance low spatter, high penetration, and high stability. Summary of the Invention

[0005] This application provides a method for controlling the power supply of ship welding with low spatter and high penetration depth stability. By dividing the welding current waveform into three stages within a single droplet transition cycle—droplet formation, droplet necking, and droplet transition—and implementing differentiated control for each stage, while introducing real-time arc state detection and adaptive compensation, this method can effectively solve the problems of difficulty in balancing low spatter and high penetration depth, as well as insufficient anti-disturbance capability in existing technologies. It achieves a comprehensive effect of low spatter, sufficient penetration depth, and high stability in ship welding processes.

[0006] To achieve the above objectives, this application provides the following technical solution: a method for controlling a low-spatter, high-penetration-depth-stability marine welding power supply, comprising the following steps:

[0007] S1. Welding parameter setting steps: Set the welding current setting value, welding voltage setting value, wire feed speed and welding shielding gas flow rate parameters according to the ship welding conditions.

[0008] S2. Droplet transition cycle detection steps: Real-time acquisition of arc voltage and welding current signals during the welding process, calculation of arc equivalent resistance, and determination of the stage switching time of droplet short-circuit transition cycle based on the differential characteristics of arc voltage and welding current signals. The droplet transition cycle is divided into droplet formation stage, droplet necking stage and droplet transition stage in sequence.

[0009] S3. Current Waveform Segmentation Control Steps: In the droplet formation stage, the welding power supply outputs a first peak current and maintains it for a first duration to promote the melting of the welding wire end and the formation of a droplet; in the droplet necking stage, the welding current is controlled to decrease from the first peak current at a first decreasing rate to the base current, so that the liquid bridge between the droplet and the welding wire completes necking under low current conditions; in the droplet transition stage, the welding current is controlled to increase from the base current at a first increasing rate to the second peak current and maintain it for a second duration, so that the necked droplet accelerates its detachment and transitions into the molten pool under the action of electromagnetic contraction force; wherein, the first peak current is greater than the second peak current, and the second duration is less than the first duration;

[0010] S4. Penetration depth enhancement control steps: During the droplet formation stage, pulse energy is periodically superimposed to increase the heat input of the welding arc to the base material during the droplet formation stage, thereby deepening the weld pool depth.

[0011] S5. Adaptive compensation step: After the droplet transition phase ends, detect whether the droplet has completed the transition according to the preset rules. If it has not completed the transition according to the preset rules, adjust the magnitude of the first peak current and / or the first duration in the next droplet transition cycle according to the detected deviation, so that the droplet transition is restored to regularity.

[0012] Furthermore, in step S3, during the droplet formation stage, the welding current rises from the base current to the first peak current at a second rising rate, where the second rising rate is less than the first rising rate.

[0013] Furthermore, in step S3, during the droplet necking stage, after the welding current is reduced to the base current, the base current is maintained for a first delay duration to fully release the liquid bridge necking energy and reduce liquid bridge explosion spatter.

[0014] Furthermore, the periodically superimposed pulse energy in step S4 is a pulse current with adjustable amplitude superimposed on the base current. The amplitude of the pulse current is 20% to 50% of the base current, and the pulse frequency is the same as the droplet transition period.

[0015] Furthermore, in step S4, the pulse energy is continuously output during the droplet formation stage, and the frequency of the pulse current is 100Hz to 500Hz.

[0016] Furthermore, the method for detecting whether the molten droplet has completed the transition according to the preset rules in step S5 is as follows: after the molten droplet transition stage ends, detect whether the instantaneous rising edge of the arc voltage appears within the preset time window. If the instantaneous rising edge of the arc voltage exceeds the preset time window, it is determined that the molten droplet transition deviates from the preset rules.

[0017] Furthermore, the specific method for adjusting the magnitude of the first peak current in the next droplet transition cycle in step S5 is as follows: when the droplet transition occurs earlier than the preset time window, the first peak current is reduced; when the droplet transition occurs later than the preset time window, the first peak current is increased.

[0018] Furthermore, the specific method for adjusting the first duration in the next droplet transition cycle in step S5 is as follows: when the droplet transition occurs earlier than the preset time window, the first duration is shortened; when the droplet transition occurs later than the preset time window, the first duration is extended.

[0019] Furthermore, the method for determining the stage switching time of the droplet short-circuit transition period in step S2 is as follows: when the rate of decrease of the arc equivalent resistance exceeds the first threshold, it is determined that the droplet is entering the necking stage; when the rate of increase of the arc equivalent resistance exceeds the second threshold, it is determined that the droplet is entering the transition stage.

[0020] Furthermore, in step S1, the welding shielding gas is a mixture of CO2 and Ar, with CO2 accounting for 20% to 35% of the volume.

[0021] Compared with the prior art, the beneficial effects of this application are:

[0022] 1. This application divides the droplet transition period into a droplet formation stage, a droplet necking stage, and a droplet transition stage, and sets segmented control strategies for the first peak current, the base current, and the second peak current respectively. In the droplet necking stage, the liquid bridge is necked under low current conditions, and in the droplet transition stage, the second peak current provides an electromagnetic force to accelerate the transition. This effectively reduces the amount of splash generated when the liquid bridge explodes, while ensuring the consistency and reliability of the droplet transition.

[0023] 2. This application increases the heat input to the base material by periodically superimposing pulse energy during the droplet formation stage without affecting the normal formation and transition of the droplets, thereby deepening the weld pool and resolving the contradiction between low spatter control and the requirement for large weld depth. It is particularly suitable for high weld depth welding of medium and thick plates in ships.

[0024] 3. This application uses an adaptive compensation step to monitor and adjust the regularity of droplet transition in real time. When external disturbances cause droplet transition to deviate from the preset rules, the current parameters are adjusted in a timely manner, which enhances the adaptability of the welding process to changes in working conditions and improves the stability and consistency of welding quality. Attached Figure Description

[0025] Figure 1 This is a schematic diagram of the overall structure of the welding power supply control system of this application.

[0026] In the diagram: 1. Welding power supply main circuit; 2. Rectifier and filter unit; 3. Inverter unit; 4. Transformer; 5. Output rectifier unit; 6. Current detection unit; 7. Voltage detection unit; 8. Signal conditioning circuit; 9. Central control unit; 10. Drive circuit; 11. Human-machine interface unit; 12. Wire feeding mechanism; 13. Welding torch; 14. Wire feeding speed control unit; 15. Shielding gas supply unit; 16. Gas flow control valve; 17. Workpiece; 18. Storage unit. Detailed Implementation

[0027] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments. Based on the embodiments of this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.

[0028] In the description of this application, if directional descriptions are involved, such as "up," "down," "front," "back," "left," "right," etc., indicating directional or positional relationships, they are based on the appendix. Figure 1The orientations or positional relationships shown are for the convenience of describing this application and simplifying the description only, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this application. When a feature is referred to as "set", "fixed", or "connected" to another feature, it can be directly set, fixed, or connected to the other feature, or it can be indirectly set, fixed, or connected to the other feature.

[0029] Please see Figure 1 This application provides the following technical solution: a method for controlling the power supply of marine welding with low spatter and high penetration stability.

[0030] In this embodiment, the input terminal of the welding power supply main circuit 1 is connected to a three-phase AC power grid. After rectification and filtering by the rectifier and filter unit 2, DC power is output. The DC power is inverted into high-frequency AC power by the inverter unit 3, and then stepped down by the transformer 4 before being rectified by the output rectifier unit 5 to output DC welding current. The current detection unit 6 and voltage detection unit 7 respectively collect the current and voltage signals in the welding circuit in real time. The collected signals are filtered and amplified by the signal conditioning circuit 8 and then sent to the central control unit 9. The central control unit 9 outputs a PWM control signal according to the preset control algorithm and the real-time collected welding signals. The drive circuit 10 controls the on and off of the power switching devices in the inverter unit 3, thereby adjusting the output current waveform of the welding power supply. The human-machine interaction unit 11 is used to set welding parameters and display welding status information. The wire feeding speed control unit 14 drives the wire feeding mechanism 12 to feed welding wire to the welding torch 13 according to the instructions of the central control unit 9. The shielding gas supply unit 15 supplies shielding gas to the welding area through the gas flow control valve 16. The storage unit 18 is used to store welding parameters and process data.

[0031] In this embodiment, the central control unit 9 uses a Siemens S7-200 PLC microcontroller as its core controller. This PLC features fast processing speed, strong anti-interference capability, and high reliability, making it suitable for use in the complex electromagnetic environment of ship welding sites. The current detection unit 6 uses a Hall current sensor, and the voltage detection unit 7 uses a voltage divider resistor network in conjunction with an isolation amplifier to acquire voltage signals. The power switching device in the inverter unit 3 is an IGBT module. IGBTs have the advantages of low on-state voltage drop, fast switching speed, and strong impact resistance, making them suitable for inverter control of high-power welding power supplies.

[0032] Its working principle is as follows:

[0033] The first step is to set the welding parameters. The operator inputs the ship welding condition parameters through the human-machine interface unit 11, including a welding current setting of 280A, a welding voltage setting of 30V, a wire feed speed of 8m / min, a shielding gas of a mixture of CO2 and Ar (with CO2 accounting for 25% by volume), and a gas flow rate of 20L / min. After receiving the above parameters, the central control unit 9 stores them in the storage unit 18 and determines the current waveform control parameters for each stage of the droplet transition cycle based on the welding parameters, including a first peak current of 420A, a base current of 60A, a second peak current of 350A, a first duration of 3ms, a second duration of 0.8ms, a first descent rate of 150A / ms, a first ascent rate of 500A / ms, a second ascent rate of 80A / ms, and a first delay duration of 0.5ms.

[0034] The second step is droplet transition cycle detection. After welding starts, the current detection unit 6 and voltage detection unit 7 collect the current and voltage signals of the welding circuit in real time at a sampling frequency of 10kHz, and send the signals to the central control unit 9. The central control unit 9 calculates the equivalent arc resistance according to the formula R=U / I, and performs time differentiation on the equivalent arc resistance to obtain the resistance change rate dR / dt. When the rate of decrease of dR / dt exceeds the first threshold (set to -8Ω / ms in this embodiment), it is determined that the droplet short-circuit transition cycle has entered the droplet necking stage; when the rate of increase of dR / dt exceeds the second threshold (set to +12Ω / ms in this embodiment), it is determined that the droplet short-circuit transition cycle has entered the droplet transition stage. The central control unit 9 switches between the droplet formation stage, the droplet necking stage, and the droplet transition stage based on the above judgment results.

[0035] The third step is segmented control of the current waveform. During the droplet formation stage, the central control unit 9 controls the welding current to rise from a base current of 60A at a second rising rate of 80A / ms to a first peak current of 420A, and maintains this current for a first duration of 3ms. This allows the welding wire tip to melt rapidly under the influence of a large arc heat, forming a uniformly sized droplet. During the droplet necking stage, the central control unit 9 controls the welding current to rapidly decrease from the first peak current of 420A to the base current of 60A at a first falling rate of 150A / ms, and maintains this current for a first delay of 0.5ms. At this time, the liquid bridge between the droplet and the welding wire completes its necking under low current conditions. Due to the extremely small current, the electromagnetic contraction force and resistive heat during the liquid bridge necking process are significantly reduced, lowering the energy at which the liquid bridge bursts, thereby effectively suppressing spatter generation. During the droplet transfer stage, the central control unit 9 controls the welding current to rapidly increase from a base current of 60A to a second peak current of 350A at a first rise rate of 500A / ms, and maintains this current for a second duration of 0.8ms. At this time, a large electromagnetic contraction force acts on the necked-out liquid bridge, causing the droplet to accelerate its detachment from the welding wire end and transition into the molten pool, achieving stable droplet transfer. It should be noted that the first peak current of 420A is greater than the second peak current of 350A in this step. This is because the main function of the first peak current is to melt the welding wire to form a droplet, while the main function of the second peak current is to provide electromagnetic force to accelerate droplet detachment. Since their functions are different, the required current amplitudes are also different.

[0036] The fourth step is weld penetration enhancement control. During the droplet formation stage, the central control unit 9 controls the periodic superposition of pulsed current based on a base current of 60A. The amplitude of the pulsed current is 30A (i.e., 50% of the base current), and the pulse frequency is 200Hz. The superimposed pulsed energy periodically increases the instantaneous power of the arc during the droplet formation stage, increasing the heat input of the arc to the base material, thereby deepening the weld pool. Because the amplitude and duration of the pulsed energy are precisely controlled, arc instability or increased spatter is not caused. Through this step, the weld penetration in this embodiment can be increased by approximately 15% to 20% compared to the case without superimposed pulsed energy.

[0037] Step 5: Adaptive Compensation. After the droplet transition phase ends, the central control unit 9 detects whether the instantaneous rising edge of the arc voltage appears within a preset time window (in this embodiment, it is set to a time interval of 0.2ms to 0.5ms after the end of the droplet transition phase). If the instantaneous rising edge of the arc voltage appears earlier than the preset time window, it indicates that the droplet transition has occurred prematurely. At this time, the central control unit 9 controls the first peak current in the next droplet transition cycle to decrease by 20A and shorten the first duration by 0.3ms. If the instantaneous rising edge of the arc voltage appears later than the preset time window, it indicates that the droplet transition is delayed. The central control unit 9 controls the first peak current in the next droplet transition cycle to increase by 20A and extend the first duration by 0.3ms. Through the above adaptive compensation, even when external disturbances such as changes in wire extension, inconsistent workpiece surface conditions, or fluctuations in assembly gaps occur at the ship welding site, the droplet transition can still maintain good regularity, with low spatter and stable arc during the welding process.

[0038] Furthermore, regarding the welding shielding gas, this embodiment uses a CO2 and Ar mixture with a CO2 volume percentage of 25%. An appropriate CO2 ratio helps increase the heat input and penetration of the arc, while the addition of Ar gas improves arc stability and reduces spatter. When the CO2 volume percentage is too low, the weld penetration is insufficient; when the CO2 volume percentage is too high, the amount of spatter increases. Therefore, in this embodiment, it is preferable to set the CO2 gas volume percentage within the range of 20% to 35%.

[0039] It is worth noting that the core chip of the central control unit disclosed in this embodiment is a PLC microcontroller, specifically a Siemens S7-200; the current detection unit uses a Hall current sensor; the power switching device of the inverter unit is an IGBT module; and the welding shielding gas is a mixture of CO2 and Ar. The specific models and parameters of the above devices can be freely configured according to the actual application scenario. The central control unit coordinates the operation of each unit using methods commonly used in existing technologies.

[0040] Although embodiments of this application have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and variations can be made to these embodiments without departing from the principles and spirit of this application, the scope of which is defined by the appended claims and their equivalents.

Claims

1. A method for controlling a marine welding power source with low spatter and high penetration stability, characterized in that, Includes the following steps: S1. Welding parameter setting steps: Set the welding current setting value, welding voltage setting value, wire feed speed and welding shielding gas flow rate parameters according to the ship welding conditions. S2. Droplet transition cycle detection steps: Real-time acquisition of arc voltage and welding current signals during the welding process, calculation of arc equivalent resistance, and determination of the stage switching time of droplet short-circuit transition cycle based on the differential characteristics of arc voltage and welding current signals. The droplet transition cycle is divided into droplet formation stage, droplet necking stage and droplet transition stage in sequence. S3. Current Waveform Segmentation Control Steps: In the droplet formation stage, the welding power supply outputs a first peak current and maintains it for a first duration to promote the melting of the welding wire end and the formation of a droplet; in the droplet necking stage, the welding current is controlled to decrease from the first peak current at a first decreasing rate to the base current, so that the liquid bridge between the droplet and the welding wire completes necking under low current conditions; in the droplet transition stage, the welding current is controlled to increase from the base current at a first increasing rate to the second peak current and maintain it for a second duration, so that the necked droplet accelerates its detachment and transitions into the molten pool under the action of electromagnetic contraction force; wherein, the first peak current is greater than the second peak current, and the second duration is less than the first duration; S4. Penetration depth enhancement control steps: During the droplet formation stage, pulse energy is periodically superimposed to increase the heat input of the welding arc to the base material during the droplet formation stage, thereby deepening the weld pool depth. S5. Adaptive compensation step: After the droplet transition phase ends, detect whether the droplet has completed the transition according to the preset rules. If it has not completed the transition according to the preset rules, adjust the magnitude of the first peak current and / or the first duration in the next droplet transition cycle according to the detected deviation, so that the droplet transition is restored to regularity.

2. The method for controlling the low-spatter, high-penetration-depth stability marine welding power supply according to claim 1, characterized in that, In step S3, during the droplet formation stage, the welding current rises from the base current to the first peak current at a second rising rate, where the second rising rate is less than the first rising rate.

3. The method for controlling the low-splash, high-penetration-depth stability marine welding power supply according to claim 1, characterized in that, In step S3, during the droplet necking stage, after the welding current is reduced to the base current, the base current is maintained for the first delay duration to fully release the liquid bridge necking energy and reduce liquid bridge explosion spatter.

4. The method for controlling the low-spatter, high-penetration-depth stability marine welding power supply according to claim 1, characterized in that, In step S4, the periodically superimposed pulse energy is a pulse current with adjustable amplitude superimposed on the base current. The amplitude of the pulse current is 20% to 50% of the base current, and the pulse frequency is the same as the droplet transition period.

5. The method for controlling the low-splash, high-penetration-depth stability marine welding power supply according to claim 1, characterized in that, In step S4, the pulse energy is continuously output during the droplet formation stage, and the frequency of the pulse current is 100Hz to 500Hz.

6. The method for controlling the low-spatter, high-penetration-depth stability marine welding power supply according to claim 1, characterized in that, The method for detecting whether the molten droplet has completed the transition according to the preset rules in step S5 is as follows: after the molten droplet transition stage is completed, it is detected whether the instantaneous rising edge of the arc voltage appears within the preset time window. If the instantaneous rising edge of the arc voltage exceeds the preset time window, it is determined that the molten droplet transition deviates from the preset rules.

7. The method for controlling the low-splash, high-penetration-depth stability marine welding power supply according to claim 1, characterized in that, The specific method for adjusting the magnitude of the first peak current in the next droplet transition cycle in step S5 is as follows: when the droplet transition occurs earlier than the preset time window, the first peak current is reduced; when the droplet transition occurs later than the preset time window, the first peak current is increased.

8. The method for controlling the low-splash, high-penetration-depth stability marine welding power supply according to claim 1, characterized in that, The specific method for adjusting the first duration in the next droplet transition cycle in step S5 is as follows: when the droplet transition occurs earlier than the preset time window, the first duration is shortened; when the droplet transition occurs later than the preset time window, the first duration is extended.

9. The method for controlling the low-splash, high-penetration-depth stability marine welding power supply according to claim 1, characterized in that, The method for determining the stage switching time of the droplet short-circuit transition period in step S2 is as follows: when the rate of decrease of the arc equivalent resistance exceeds the first threshold, it is determined that the droplet is entering the necking stage; when the rate of increase of the arc equivalent resistance exceeds the second threshold, it is determined that the droplet is entering the transition stage.

10. The method for controlling the low-splash, high-penetration-depth stability marine welding power supply according to claim 1, characterized in that, In step S1, the welding shielding gas is a mixture of CO2 and Ar, with CO2 accounting for 20% to 35% of the volume.