A method and equipment for automatic submerged arc welding of shrimp-shaped pipe sections
By spot welding the shrimp-shaped bend to a straight metal pipe and utilizing the rigid support ring and ceramic gasket of the submerged arc welding equipment, the problems of low welding efficiency and welding deviation of the shrimp-shaped bend pipe section were solved, achieving a high-efficiency and stable welding effect.
Patent Information
- Application Number
- CN202611331756.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2026-06-11
- Filing Date
- 2026-08-31
- Publication Date
- 2026-11-17
AI Technical Summary
In existing technologies, the welding efficiency of shrimp-shaped bends is low and it is difficult to adapt to their complex geometry, resulting in high manual welding costs and defects caused by automatic welding equipment deviating from the weld centerline.
By spot welding the two ends of the shrimp-shaped bend to a straight metal pipe to form a rigid rotating body, and combining it with submerged arc welding equipment, a rigid metal support ring and a ceramic backing are used to achieve single-sided welding and double-sided forming, and the welding parameters are adjusted in real time by monitoring the changes in the weld gap.
This technology enables efficient, continuous, and automated welding of shrimp-shaped pipe sections, improving production efficiency, reducing labor intensity, ensuring uniform weld penetration and stable mechanical properties, and avoiding welding defects.
Smart Images

Figure CN123103126A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of welding equipment technology, specifically relating to an automatic submerged arc welding method and equipment for shrimp-shaped pipe sections. Background Technology
[0002] The statements in this section are merely background information related to the present invention and do not necessarily constitute prior art.
[0003] A "shrimp bend" is a metal pipe elbow composed of multiple obliquely cut pipe sections joined together by circumferential welds. It gets its name from its resemblance to a shrimp joint and is widely used in pipeline systems in industries such as chemical, power, and petroleum. Currently, the industry commonly uses manual carbon dioxide gas shielded welding (referred to as "MAG welding") for welding shrimp bend sections. However, manual welding has low production efficiency. The welding speed of a single weld is limited by the welder's skill level and physical exertion, and the multi-segment structure of the shrimp bend requires frequent adjustments to the workpiece position or the welder's posture, further extending the work cycle. This inefficient welding method cannot meet the needs of mass production and also leads to high labor costs.
[0004] Furthermore, the "shrimp bend," as a non-smooth transition geometry composed of multiple obliquely cut pipe segments, exhibits a significant change in the axial direction between each segment. Traditional automatic welding equipment, typically designed for straight pipes or continuously curved pipe fittings, struggles to adapt to the abrupt angle changes in shrimp bends. During welding, the welding torch is prone to deviating from the weld centerline, causing serious defects such as incomplete fusion or burn-through, leading to automatic welding failure. Summary of the Invention
[0005] To address the above problems, this invention provides an automatic submerged arc welding method and equipment for shrimp-shaped bend pipe sections, which solves the problem that traditional automatic welding equipment cannot adapt to the special geometric structure of shrimp bends.
[0006] To achieve the above objectives, the present invention is implemented through the following technical solution: In a first aspect, the present invention provides an automatic submerged arc welding method for shrimp-shaped pipe sections, comprising the following steps: Assemble the straight pipe and the bend according to the design angle, and spot weld both ends of the bend to the straight metal pipe to form a bend workpiece consisting of a straight pipe and a bend. The shrimp-shaped workpiece is hoisted onto the drive roller frame. The position of the shrimp-shaped workpiece is adjusted so that the axis of the annular weld to be welded is parallel to the ground. The rotation center of the weld is then aligned with the rotation center of the auxiliary circular tube of the roller frame. In the inner cavity of the shrimp-bent workpiece, a rigid metal support ring is set at the position of the weld to be welded, and a high-temperature resistant ceramic liner is laid on the surface of the support ring so that the ceramic liner is tightly attached to the root of the weld. Align the submerged arc welding torch with the center line of the weld, start the roller frame to make the workpiece rotate at the set linear speed V, and start the submerged arc welding torch at the set welding current and arc voltage to perform welding. The flux is automatically laid in front of the arc zone to form a flux layer to cover the arc zone; the welding wire is automatically fed in and burns under the flux layer to form a molten pool. During the welding process, the changes in weld gap caused by the alteration of the shrimp-shaped structure are monitored in real time, and the welding current or wire feeding speed is adjusted through the control system to compensate for heat input fluctuations and ensure consistent weld penetration.
[0007] As a further implementation method, during the workpiece position adjustment process, a laser calibrator is used to ensure that the coaxiality offset between the weld rotation center and the roller frame rotation center is controlled within ±1mm.
[0008] As a further implementation, a 5±1° V-shaped bevel is machined on the mating end face of adjacent pipe sections in the shrimp bend, leaving a 1-2mm assembly gap during assembly.
[0009] As a further implementation, the ceramic gasket is attached to the inner side of the weld seam with high-temperature resistant and fire-resistant tape to support the molten metal during submerged arc welding, thereby achieving single-sided welding and double-sided forming.
[0010] Secondly, the present invention also provides an automatic submerged arc welding device for implementing the above method for a bent pipe section, comprising a roller frame, wherein a variable frequency speed-regulating roller is provided on the roller frame to drive the bent pipe workpiece to rotate, the variable frequency speed-regulating roller is provided with an auxiliary circular tube, the auxiliary circular tube being two sections of circular tube, and a steel connecting bracket is provided between the two sections of circular tube for supporting the bent pipe workpiece; a cantilever welding manipulator is provided on one side of the roller frame, and a submerged arc welding torch and a laser calibrator are fixedly mounted on the cantilever, the coaxiality of the rotation center of the weld to be welded and the rotation center of the auxiliary circular tube is calibrated by the laser calibrator; the weld to be welded is performed by the submerged arc welding torch; a rigid metal support ring is provided at the position of the weld to be welded in the inner cavity of the bent pipe workpiece; a high-temperature resistant ceramic liner is laid on the surface of the rigid metal support ring; the submerged arc welding torch and the roller frame are connected to a control system, which adjusts the welding current or wire feed speed in real time according to the detected changes in the weld gap.
[0011] As a further implementation, the rigid metal support ring is an adjustable structure, with an internal tightening device for adjusting according to the diameter of the pipe fitting to be welded.
[0012] As a further implementation, a small hydraulic device with remote control capability is provided between the submerged arc welding torch and the welding manipulator for fine-tuning the position of the automatic submerged arc welding head during the welding process; a wire feeding wheel is provided on the cantilever to supply welding wire to the automatic submerged arc welding head of the submerged arc welding torch; a flux filling funnel is also provided on the automatic submerged arc welding head to provide flux to the automatic submerged arc welding head.
[0013] As a further implementation, the variable frequency speed control roller includes a driving roller and a driven roller. The driving roller is directly hinged to the roller frame, and the driven roller is hinged to the roller frame through a bracket, ensuring that the axial position of the rotation center of the auxiliary round tube remains unchanged during the rotation of the shrimp-bent workpiece.
[0014] As a further implementation, the laser calibrator is fixedly connected to the submerged arc welding torch, and the position of its light beam movement is consistent with the position of the welding torch movement, both moving along the weld seam trajectory.
[0015] As a further implementation, the high-temperature resistant ceramic gasket is made of high-temperature refractory ceramic material and its surface is coated with a high-temperature resistant coating.
[0016] Compared with the prior art, the advantages and positive effects of this invention are: This invention connects the two ends of a curved pipe to a straight metal pipe by spot welding, forming a rigid rotating body of "straight pipe-curved pipe-straight pipe". This allows the curved pipe, which is normally difficult to rotate stably due to its irregular geometry, to be smoothly driven to rotate by a roller frame. Combined with the fixed centering of the submerged arc welding torch and the uniform rotation of the workpiece, continuous automatic welding of circumferential welds on multiple obliquely cut pipe sections is achieved. A rigid metal support ring is placed at the weld position inside the workpiece cavity, and a high-temperature resistant ceramic liner is laid, ensuring it fits tightly against the weld root. Due to the high current and deep penetration characteristics of submerged arc welding, the ceramic liner effectively supports the molten metal, preventing the molten pool from sagging, thus automatically forming a continuous and smooth weld on the back side when welding the front side. There is no need for root cleaning, grinding, or secondary welding on the back side of the weld, eliminating the cumbersome post-processing steps in traditional methods. Double-sided forming can be completed with a single welding pass, significantly increasing production efficiency and reducing the labor intensity of operators.
[0017] During the welding process, gap fluctuations are monitored in real time, and the welding current or wire feeding speed is automatically adjusted by the control system to compensate for changes in heat input. This effectively avoids local incomplete penetration or burn-through caused by linear speed or assembly deviations, ensuring that the entire circumferential weld has uniform penetration depth and stable mechanical properties throughout the circumference. It overcomes the shortcomings of traditional automatic welding in adapting to non-smooth transition structures. Attached Figure Description
[0018] The accompanying drawings, which form part of this invention, are used to provide a further understanding of the invention. The illustrative embodiments of the invention and their descriptions are used to explain the invention and do not constitute an improper limitation of the invention.
[0019] Figure 1 This is an overall structural diagram of the automatic submerged arc welding device for shrimp-shaped pipe sections according to the present invention; Figure 2 This is a side cross-sectional view of the welding position of the submerged arc automatic welding device for shrimp bend pipe sections according to the present invention. Figure 3 This is a partially enlarged schematic diagram of the automatic submerged arc welding head of the present invention.
[0020] The components include: 1. Roller frame; 2. Variable frequency speed control roller; 3. Auxiliary round tube; 4. Shrimp-shaped workpiece; 5. Cantilever welding manipulator; 6. Welding wire conveyor wheel; 7. Welding wire; 8. Automatic submerged arc welding head; 9. Laser calibrator; 10. Flux filling funnel; 11. Weld seam to be welded; 12. Steel connecting bracket; 13. Driven roller; 14. Ground wire; 15. Driven roller. Detailed Implementation
[0021] It should be noted that the following detailed description is illustrative and intended to provide further explanation of the invention. Unless otherwise specified, all technical and scientific terms used in this invention have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains.
[0022] It should be noted that the terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the scope of exemplary embodiments according to the invention. As used herein, unless otherwise expressly indicated by the invention, the singular form is also intended to include the plural form. Furthermore, it should be understood that when the terms "comprising" and / or "including" are used in this specification, they indicate the presence of features, steps, operations, devices, components, and / or combinations thereof. A "shrimp bend" is a metal pipe elbow composed of multiple obliquely cut pipe sections joined together by circumferential welds. Named for its resemblance to a shrimp joint, it is widely used in pipeline systems in industries such as chemical, power, and petroleum. Currently, manual carbon dioxide gas shielded welding is commonly used for welding shrimp bend sections. However, manual welding has low production efficiency. The welding speed of a single weld is limited by the welder's skill level and physical exertion, and the multi-segment structure of the shrimp bend requires frequent adjustments to the workpiece position or the welder's posture, further extending the work cycle. This inefficient welding method cannot meet the demands of mass production and also results in high labor costs.
[0023] Furthermore, the "shrimp bend," as a non-smooth transition geometry composed of multiple obliquely cut pipe segments, exhibits a significant change in the axial direction between each segment. Traditional automatic welding equipment, typically designed for straight pipes or continuously curved pipe fittings, struggles to adapt to the abrupt angle changes in shrimp bends. During welding, the welding torch is prone to deviating from the weld centerline, causing serious defects such as incomplete fusion or burn-through, leading to automatic welding failure.
[0024] Example 1 This embodiment proposes an automatic submerged arc welding method for shrimp-shaped pipe sections, which includes the following steps: The straight pipe and the shrimp bend are assembled at the designed angle, and their two ends are spot welded to the metal straight pipe to form a "straight pipe-shrimp bend-straight pipe" shrimp bend workpiece; so that the originally irregularly shaped shrimp bend can be effectively driven and supported by the roller frame, which facilitates continuous rotary welding. The shrimp-shaped workpiece is hoisted onto the drive roller frame. The position of the shrimp-shaped workpiece is adjusted so that the axis of the circumferential weld to be welded is parallel to the ground. The rotation center of the weld is then aligned with the rotation center of the auxiliary circular tube on the roller frame to ensure they are coaxial. This ensures that the weld is in a horizontal position, which is beneficial for the stable formation of the submerged arc welding pool. The alignment of the rotation center of the weld with the rotation center of the auxiliary circular tube ensures that the welding torch is always aligned with the same circumferential trajectory with each rotation of the workpiece, providing a basis for subsequent continuous welding. In the inner cavity of the shrimp-bending workpiece, a rigid metal support ring is set at the position of the weld to be welded, and a high-temperature resistant ceramic liner is laid on the surface of the support ring so that the ceramic liner is tightly attached to the root of the weld. By setting a combination structure of rigid metal support ring and ceramic liner in the inner cavity of the shrimp-bending workpiece, the high current deep penetration characteristics of submerged arc welding are utilized to obtain a well-formed weld back without the need for root cleaning and secondary welding on the back of the weld. This achieves single-sided welding and double-sided one-time forming, improving production efficiency and reducing labor intensity.
[0025] Align the submerged arc welding torch with the center line of the weld, start the roller frame to make the workpiece rotate at the set linear speed V, and start the submerged arc welding torch at the set welding current and arc voltage to perform welding. The flux is automatically laid in front of the arc zone to form a flux layer to cover the arc zone; the welding wire is automatically fed in and burns under the flux layer to form a molten pool. During the welding process, the changes in weld gap caused by the alteration of the shrimp-shaped structure are monitored in real time, and the welding current or wire feeding speed is adjusted through the control system to compensate for heat input fluctuations and ensure consistent weld penetration.
[0026] After welding is completed, turn off the submerged arc welding torch and the roller frame. After the workpiece stops rotating, adjust the welding torch head to the initial position and perform quality inspection and flaw detection on the weld.
[0027] The automatic submerged arc welding method provided in this embodiment is suitable for workpieces with complex geometries through workpiece rotation, welding torch fine-tuning, and real-time parameter compensation. By adjusting the matching relationship between the roller frame speed and the welding current and voltage, such as in the welding of large-diameter pipes, increasing the voltage and current while speeding up the roller frame speed can improve welding efficiency while ensuring basic weld formation. This mechanism can adapt to the welding needs of pipes with different diameters and bending angles, such as small bends.
[0028] During the workpiece position adjustment process, a laser calibrator is used to ensure that the coaxiality offset between the weld rotation center and the roller frame rotation center is controlled within ±1mm; through high-precision coaxial operation, the welding torch is ensured to be stably centered throughout the entire circumference, avoiding weld deviation or undercut.
[0029] The butt joints of adjacent pipe sections in the shrimp bend are all machined with a 5±1° V-shaped bevel. The appropriate bevel angle and gap are conducive to penetration and back-side forming. At the same time, considering the assembly difficulty, a 1-2mm assembly gap is reserved during assembly to provide suitable space for deep penetration of high current in submerged arc welding and reduce the risk of incomplete fusion.
[0030] The ceramic gasket is attached to the inner side of the weld by high-temperature resistant and fire-resistant tape. It is used to support the molten metal during submerged arc welding, so as to achieve single-sided welding and double-sided forming.
[0031] Example 2 This embodiment discloses an automatic submerged arc welding device for implementing the method, such as... Figures 1-3 As shown, the system includes a roller frame 1, on which a variable frequency speed-regulating roller 2 is mounted to drive the curved workpiece 4 to rotate. The variable frequency speed-regulating roller 2 is equipped with an auxiliary circular tube 3, which consists of two sections of circular tube. A steel connecting bracket 12 is installed between the two sections of circular tube to support the curved workpiece 4. A cantilever welding manipulator 5 is installed on one side of the roller frame 1. A submerged arc welding torch and a laser calibrator 9 are fixedly mounted on the cantilever. The laser calibrator 9 is used to calibrate the coaxiality between the rotation center of the weld to be welded and the rotation center of the auxiliary circular tube 3. The submerged arc welding torch is used to weld the weld to be welded. A rigid metal support ring is installed at the position of the weld to be welded 11 in the inner cavity of the curved workpiece 4. The surface of the rigid metal support ring is covered with a high-temperature resistant ceramic liner. The submerged arc welding torch and the roller frame 1 are connected to a control system, which adjusts the welding current or wire feed speed in real time according to the detected changes in the weld gap.
[0032] The auxiliary circular tube 3 is also equipped with a ground wire 14 at its end to ground the entire device.
[0033] A steel connecting bracket 12 is provided between the two sections of the auxiliary round tube 3 to support the shrimp-bent workpiece 4 and drive it to rotate. At the same time, the coaxial design of the auxiliary round tube 3 and the laser calibration solves the rotational eccentricity problem caused by the multi-section oblique cut structure of the shrimp bend, enabling the automatic welding equipment to stably track the weld seam and avoid the defects caused by the welding gun deviation in traditional automatic welding.
[0034] It is understandable that a rigid metal support ring is provided at the weld seam 11 position in the inner cavity of the shrimp-bent workpiece 4; the surface of the rigid metal support ring is covered with a high-temperature resistant ceramic liner. Through the combination of the rigid metal support ring and the ceramic liner, combined with the high current deep penetration characteristics of submerged arc welding, the back of the weld seam can be smoothly and continuously formed without root cleaning and secondary welding, which significantly improves production efficiency and reduces labor intensity.
[0035] In addition, the auxiliary round tube 3 and the adjustable support ring can adapt to the small-diameter bending workpieces 4; the frequency conversion speed regulating roller 2 can be matched and adjusted with the welding parameters, and the speed and current can be increased when dealing with large diameters to meet the production needs of different pipe diameters and different bending angles.
[0036] As a further implementation, the rigid metal support ring is an adjustable structure with an internal tightening device for adjusting according to the diameter of the pipe fitting to be welded.
[0037] The rigid metal support ring is designed as an adjustable structure. Its main body consists of several arc-shaped metal petals or annular metal rings with openings. An internal tightening device is installed, which can be a threaded knob, lead screw, eccentric cam or bolt fastening mechanism.
[0038] Before or after placing the support ring into the inner cavity of the shrimp-bend workpiece 4, the outer diameter of the support ring is increased or decreased by rotating the tightening device according to the actual inner diameter of the pipe to be welded, until it is in close contact with the inner wall of the pipe and generates a certain radial preload.
[0039] After adjustment, the tightening device is self-locking or locked by the operator to ensure the support ring is firmly attached to the inner wall of the pipe fitting, preventing loosening or displacement due to welding vibration or workpiece rotation. Subsequently, a high-temperature resistant ceramic liner is laid on the surface of the support ring, and fire-resistant tape is used to adhere the liner to the inner side of the weld.
[0040] When welding a different diameter of the shrimp-bend workpiece 4, loosen the tightening device and readjust the outer diameter of the support ring to quickly adapt to the new pipe size without replacing the entire set of support fixtures.
[0041] A small hydraulic device with remote control capability is installed between the submerged arc welding torch and the welding manipulator. This device is used to fine-tune the position of the automatic submerged arc welding head 8 during the welding process. Specifically, when the weld trajectory of the shrimp-bend workpiece 4 deviates slightly due to its multi-section oblique cut structure, the hydraulic device corrects the welding torch head to the center of the weld in real time. A wire feeding wheel 6 is installed on the cantilever. The wire feeding wheel 6 supplies welding wire 7 to the automatic submerged arc welding head 8 of the submerged arc welding torch.
[0042] The automatic submerged arc welding head 8 is also equipped with a flux filling funnel 10 for supplying flux to the automatic submerged arc welding head 8. The upper end of the funnel is connected to a flux recovery and conveying system or a manual feeding hopper via a hose. During welding, the flux flows out of the funnel evenly by gravity or pneumatic force, laying a flux layer of a certain thickness in front of the welding wire 7, completely covering the arc area.
[0043] The variable frequency speed control roller 2 includes a driving roller 15 and a driven roller 13. The driving roller 15 is directly hinged to the roller frame 1, and the driven roller 13 is hinged to the roller frame 1 through a bracket, ensuring that the axis position of the rotation center of the auxiliary round tube 3 remains unchanged during the rotation of the shrimp-bent workpiece 4.
[0044] The laser calibrator 9 is fixedly connected to the submerged arc welding torch, and the position of its light beam is consistent with the position of the welding torch, both moving along the weld seam trajectory.
[0045] The high-temperature resistant ceramic gasket is made of high-temperature resistant refractory ceramic material and its surface is coated with a high-temperature resistant coating.
[0046] While the specific embodiments of the present invention have been described above in conjunction with the accompanying drawings, this is not intended to limit the scope of protection of the present invention. Those skilled in the art should understand that various modifications or variations that can be made by those skilled in the art without creative effort based on the technical solutions of the present invention are still within the scope of protection of the present invention.
Claims
1. A method for automatic submerged arc welding of shrimp-shaped pipe sections, characterized in that, Includes the following steps: Assemble the straight pipe and the bend according to the design angle, and spot weld both ends of the bend to the straight metal pipe to form a bend workpiece consisting of a straight pipe and a bend. The shrimp-shaped workpiece is hoisted onto the drive roller frame. The position of the shrimp-shaped workpiece is adjusted so that the axis of the annular weld to be welded is parallel to the ground. The rotation center of the weld is then aligned with the rotation center of the auxiliary circular tube of the roller frame. In the inner cavity of the shrimp-bent workpiece, a rigid metal support ring is set at the position of the weld to be welded, and a high-temperature resistant ceramic liner is laid on the surface of the support ring so that the ceramic liner is tightly attached to the root of the weld. Align the submerged arc welding torch with the center line of the weld, start the roller frame to make the workpiece rotate at the set linear speed V, and start the submerged arc welding torch at the set welding current and arc voltage to perform welding. The flux is automatically laid in front of the arc zone to form a flux layer to cover the arc zone; the welding wire is automatically fed in and burns under the flux layer to form a molten pool. During the welding process, the changes in weld gap caused by the alteration of the shrimp-shaped structure are monitored in real time, and the welding current or wire feeding speed is adjusted through the control system to compensate for heat input fluctuations and ensure consistent weld penetration.
2. The automatic submerged arc welding method for shrimp-shaped pipe sections according to claim 1, characterized in that, During the workpiece position adjustment process, a laser calibrator is used to ensure that the coaxiality offset between the weld rotation center and the roller frame rotation center is controlled within ±1mm.
3. The automatic submerged arc welding method for shrimp-shaped pipe sections according to claim 1, characterized in that, The mating end faces of adjacent pipe sections in the shrimp bend are all machined with a 5±1° V-shaped bevel, leaving a 1-2mm assembly gap during assembly.
4. The automatic submerged arc welding method for shrimp-shaped pipe sections according to claim 1, characterized in that, The ceramic gasket is attached to the inner side of the weld seam by high-temperature resistant and fire-resistant tape, and is used to support the molten metal during submerged arc welding to achieve single-sided welding and double-sided forming.
5. An automatic submerged arc welding device for implementing the method of any one of claims 1-4, characterized in that, The system includes a roller frame with variable frequency speed-regulating rollers that drive the bent workpiece to rotate. Each roller has an auxiliary circular tube consisting of two sections connected by a steel connecting bracket to support the bent workpiece. A cantilever welding manipulator is mounted on one side of the roller frame, with a submerged arc welding torch and a laser calibrator fixedly mounted on its cantilever. The laser calibrator calibrates the coaxiality between the rotation center of the weld to be welded and the rotation center of the auxiliary circular tube. The submerged arc welding torch is used to weld the weld. A rigid metal support ring is positioned at the weld location within the cavity of the bent workpiece. A high-temperature resistant ceramic liner is laid on the surface of the rigid metal support ring. A control system connects the submerged arc welding torch and the roller frame, adjusting the welding current or wire feed speed in real time based on detected changes in the weld gap.
6. The automatic submerged arc welding method for shrimp-shaped pipe sections according to claim 5, characterized in that, The rigid metal support ring is an adjustable structure, and its interior is equipped with a tightening device for adjusting according to the diameter of the pipe fitting to be welded.
7. The automatic submerged arc welding device for shrimp-shaped pipe sections according to claim 5, characterized in that, A small hydraulic device with remote control capability is installed between the submerged arc welding torch and the welding manipulator for fine-tuning the position of the automatic submerged arc welding head during the welding process; a wire feeding wheel is installed on the cantilever to supply welding wire to the automatic submerged arc welding head of the submerged arc welding torch; a flux filling funnel is also installed on the automatic submerged arc welding head to provide flux to the automatic submerged arc welding head.
8. The automatic submerged arc welding device for shrimp-shaped pipe sections according to claim 5, characterized in that, The variable frequency speed control roller includes a driving roller and a driven roller. The driving roller is directly hinged to the roller frame, and the driven roller is hinged to the roller frame through a bracket, ensuring that the axial position of the rotation center of the auxiliary round tube remains unchanged during the rotation of the shrimp-bent workpiece.
9. The automatic submerged arc welding device for shrimp-shaped pipe sections according to claim 5, characterized in that, The laser calibrator is fixedly connected to the submerged arc welding torch, and the position of its light beam is consistent with the position of the welding torch, both moving along the weld seam trajectory.
10. The automatic submerged arc welding device for shrimp-shaped pipe sections according to claim 5, characterized in that, The high-temperature resistant ceramic gasket is made of high-temperature refractory ceramic material and its surface is coated with a high-temperature resistant coating.