In-situ repair equipment and method for defects in the billet making process of large forgings
By integrating online inspection, machining, and arc additive repair, real-time defect repair during the billet making process of large forgings is achieved, solving the problems of high energy consumption and performance degradation of traditional repair methods, and improving production efficiency and forging quality.
Patent Information
- Application Number
- CN202611167490.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-03
- Publication Date
- 2026-11-17
AI Technical Summary
The process of defect repair in the billet making of large forgings is lengthy, energy-intensive, and deteriorates the microstructure and properties of forgings. Traditional repair methods lead to energy waste, extended production cycles, and reduced forging quality.
The system employs an online detection unit to monitor defects in real time, combines this with localized cooling from a machining unit to remove defects, and utilizes an electric arc additive manufacturing unit for in-situ filling and repair. Finally, it leverages the forging press body for forging and strengthening to achieve immediate defect repair and improved microstructure and properties.
It significantly shortens the billet preparation process cycle, reduces energy consumption, improves production efficiency, ensures the overall mechanical properties and service reliability of forgings, and avoids coarse microstructure and performance degradation.
Smart Images

Figure CN123103303A_ABST
Abstract
Description
Technical Field
[0001] This application belongs to the field of forging, and more specifically, relates to an in-situ repair device and method for defects in the billet making process of large forgings. Background Technology
[0002] Large forgings are key core components and fundamental load-bearing structures in the manufacturing of major equipment. Typical products include steam turbine rotors and generator rotors in thermal power equipment, and heavy-duty load-bearing frame beam structures and aircraft landing gear in the aerospace field. Their manufacturing level is directly related to the lifeline of the national economy and national defense security. These forgings are huge in size and can weigh tens or even hundreds of tons. They need to be formed by forging from large ingots and are characterized by single-piece and small-batch production.
[0003] The forging process for large forgings is extremely lengthy, mainly consisting of a billet preparation stage and subsequent die forging forming stage. The billet preparation stage typically involves multiple upsetting and drawing operations to improve the internal structure of the ingot and distribute material volume. However, due to the limited production volume of small batches of single pieces, the cumulative production quantity of large forgings is low. For specific materials and specifications, the selection of forging process parameters lacks sufficient practical experience and mature data support, and process planning can easily go out of control if not handled carefully. When parameters such as deformation temperature, reduction, or feed rate are not selected appropriately, folding, surface cracks, or internal layered defects can easily occur during billet preparation. If these defects are not detected and removed in time, they will affect subsequent processes and ultimately lead to the scrapping of the forging.
[0004] Traditional repair methods for defects generated during the billet preparation stage involve: after the preform has completely cooled to room temperature, offline non-destructive testing is performed to determine the location and size of the defect; then, the defective area is removed entirely by machining; and finally, the removed billet is reheated for subsequent die forging processes. This offline repair process of "cooling-testing-removal-reheating" results in the forging undergoing multiple unnecessary "heating-cooling" cycles throughout the forging process, significantly increasing the number of heating cycles. On the one hand, this leads to energy waste, extended production cycles, and increased manufacturing costs; on the other hand, repeated heating exacerbates oxidation and decarburization on the forging surface, and causes repeated grain growth and abnormal microstructure inheritance, severely damaging the surface quality, internal microstructure uniformity, and final service performance of the forging. Summary of the Invention
[0005] To address the shortcomings of existing technologies, this application provides an in-situ repair device and method for defects in the billet preparation process of large forgings, aiming to solve the problems of lengthy process flow, high energy consumption, and deterioration of forging microstructure and properties in existing large forging defect repair methods.
[0006] This application provides an in-situ repair device for defects in the billet preparation process of large forgings, specifically comprising: The main body of the forging press is used to form large forging preforms; An online detection unit is installed on the main body of the forging press for real-time monitoring of the large forging preform. A machining unit is used to locally cool and remove defects in the preform on the large forging preform. An electric arc additive manufacturing unit is used to perform electric arc additive filling and repair on the additive repair area formed by removing defects in the preform of the large forging preform. The control system is connected to the forging press body, the online detection unit, the machining unit, and the electric arc additive manufacturing unit, respectively. When the online detection unit detects a preform defect on the surface of the large forging preform, the control system controls the forging press body to stop working and controls the machining unit and the electric arc additive manufacturing unit to move sequentially to the front of the working area of the forging press body to remove defects and perform additive repair. After the repair is completed, the forging press body then performs forging strengthening.
[0007] Compared with the prior art, the technical solution conceived in this application adopts a full-process in-situ online linkage scheme that integrates defect detection, removal, additive repair, and forging strengthening on the same forging press body. This scheme involves real-time monitoring of surface defects on large forging preforms by an online detection unit to trigger a shutdown, local cooling removal of defects by a machining unit, in-situ filling and repair by an arc additive manufacturing unit, and forging strengthening of the repair area by the forging press body. Defect detection, removal, additive repair, and forging strengthening can be continuously completed on-site by the same forging press equipment. There is no need to remove the preform from the production line for offline welding or reforging, which significantly shortens the billet preparation process cycle, avoids redundant processes of repeated heating and transfer of preforms, and significantly reduces energy consumption. At the same time, forging strengthening is performed immediately after additive repair, using force-thermal coupling to break columnar crystals, refine grains, and close micropores, so that the microstructure and properties of the repair area are close to those of the matrix. This avoids the problems of coarse microstructure and performance degradation caused by traditional welding, and ensures the overall mechanical properties and service reliability of large forgings.
[0008] As a further preferred embodiment, the online detection unit includes an infrared thermal imager, and a third six-axis robot is fixedly installed on the forging press body. The infrared thermal imager is installed at the front end of the arm of the third six-axis robot, and the third six-axis robot drives the infrared thermal imager to move in multiple degrees of freedom to monitor the temperature field changes on the surface of the large forging preform.
[0009] As a further preferred embodiment, the online detection unit further includes a first laser profile scanner and a second laser profile scanner, which are respectively disposed on the left and right sides of the main working area of the forging press, for synchronously scanning the three-dimensional shape of the large forging preform from both sides.
[0010] As a further preferred embodiment, the machining unit includes a machining unit conveying device, a second six-axis robot, and a machining head. The second six-axis robot is mounted on the machining unit conveying device, and the machining head is mounted on the front end of the arm of the second six-axis robot. The machining unit conveying device is used to convey the second six-axis robot and the machining head to the front of the working area of the forging press body.
[0011] As a further preferred embodiment, the machining head includes an integrated hydraulic motor, a power head, and a cooling air nozzle. The hydraulic motor is connected to an external hydraulic station, the power head is connected to an external tool cooling hydraulic pump, and the cooling air nozzle is connected to an external air cooling device.
[0012] As a further preferred embodiment, the front end of the power head is equipped with an indexable corn milling cutter, the multiple blades of which are staggered along the circumferential and axial directions to divide wide chips into narrow and thick segments to reduce single-edge cutting force.
[0013] As a further preferred embodiment, the cooling air nozzle is a forced cooling nozzle array distributed around the indexable corn milling cutter, used for targeted local cooling of the defects in the preform.
[0014] As a further preferred embodiment, the electric arc additive manufacturing unit includes an additive manufacturing unit conveying device, a first six-axis robot, and an electric arc additive manufacturing device. The first six-axis robot is mounted on the additive manufacturing unit conveying device, and the electric arc additive manufacturing device is mounted on the front end of the arm of the first six-axis robot. The additive manufacturing unit conveying device is used to convey the first six-axis robot and the electric arc additive manufacturing device to the front of the working area of the forging press body.
[0015] As a further preferred embodiment, the electric arc additive manufacturing equipment includes a multi-arc welding torch, which is mounted on the first six-axis robot and is used to perform electric arc additive filling repair on the additive repair area. The multi-arc welding torch is connected to an external wire feeding device and a welding torch power supply. The wire feeding device is used to simultaneously feed multiple metal wires into the multi-arc welding torch, and the welding torch power supply is used to supply power to the multi-arc welding torch.
[0016] This application provides an in-situ repair method for defects in the billet preparation process of large forgings, which uses the aforementioned in-situ repair equipment and includes the following steps: S1. The forging press body forms the large forging preform. The online detection unit monitors the large forging preform in real time. When a defect is detected in the preform, the control system controls the forging press body to stop. S2. The control system controls the machining unit to move to the front of the working area of the forging press body, and locally cools and removes the defects of the preform to form an additive repair area. S3. The control system controls the machining unit to reset and controls the arc additive manufacturing unit to move to the front of the working area of the forging press body. The arc additive manufacturing unit performs arc additive manufacturing repair on the additive repair area. S4. The forging press body forges and strengthens the additive repair area after the electric arc additive repair, completing the in-situ repair of the defect.
[0017] In summary, compared with the prior art, the technical solutions conceived in this application have the following main technical advantages: 1. This application integrates defect detection, removal, additive repair, and forging strengthening into the main forging process, realizing online real-time repair of forging defects within the production cycle. This completely eliminates the lengthy process of "shutting down for cooling, offline transfer, and repeated heating" in traditional methods, significantly shortens the production cycle, and eliminates the need for additional heating cycles, preheating before welding, and post-weld heat treatment required for independent repair. This significantly reduces energy consumption and manufacturing costs, and improves production efficiency.
[0018] 2. The preform after in-situ repair in this application still maintains a high forging temperature and can immediately enter the subsequent die forging process, thereby significantly reducing energy consumption and production cycle in traditional processes. Due to the reduction in the number and time of repeated heating, the oxidation loss and decarburization layer thickness on the surface of the forging are effectively controlled, avoiding the formation of thick oxide scale and surface carbon-depleted layer in the material during repeated high-temperature exposure, thus ensuring the surface hardness and fatigue performance of the forging. At the same time, it avoids the repeated grain growth and microstructure inheritance effect caused by multiple "heating-cooling" cycles, which helps to obtain a more uniform and fine grain structure after final forging, thereby comprehensively improving the overall mechanical properties of the forging.
[0019] 3. In this application, the repair area, which is still at a high temperature, is forged immediately after additive filling using the subsequent stroke of the forging equipment. This causes sufficient plastic deformation and dynamic recrystallization of the additive metal, effectively eliminating columnar crystals and internal pores in the additive structure. This results in the repair area having a fine-grained structure and density comparable to the forging body, solving the technical problems of coarse structure, lack of fusion defects, and insufficient bonding strength in traditional weld repair areas. This ensures that the repair area and the base material have equal strength and life.
[0020] 4. In this application, the preform after in-situ repair has been densified and has the same forging flow lines and plastic deformation capacity as the base material. The repaired forging can be directly transferred to the subsequent die forging process for integral forming. Since the repaired area and the base material are highly consistent in microstructure, hardness and hot deformation resistance, deformation incoordination or interface cracking will not occur due to differences in microstructure in the subsequent die forging, thus ensuring the overall quality and yield of the forging in the subsequent complex cavity filling process. Attached Figure Description
[0021] Figure 1 This is a schematic diagram of the overall structure of the in-situ repair device provided in the embodiments of this application; Figure 2 This is a schematic diagram of the overall structure of the online detection unit provided in the embodiments of this application; Figure 3 This is a schematic diagram of the overall structure of the machining unit provided in the embodiments of this application; Figure 4 This is a schematic diagram of the overall structure of the electric arc additive manufacturing unit provided in the embodiments of this application; Figure 5 This is a side view of the additive repair area on a large forging preform provided in this application embodiment.
[0022] In all the accompanying drawings, the same reference numerals are used to denote the same elements or structures, wherein: 1. Additive manufacturing unit conveyor; 2. Wire feeding device; 3. First six-axis robot; 4. Metal wire; 5. Multi-arc welding torch; 6. Forging press body; 7. Hydraulic motor; 8. Power head; 9. Second six-axis robot; 10. Hydraulic station; 11. Air cooling equipment; 12. Tool cooling hydraulic pump; 13. Indexable corn milling cutter; 14. Cooling air nozzle; 15. Machining unit conveyor; 16. Large forging preform; 17. First laser contour scanner; 18. Infrared thermal imager; 19. Third six-axis robot; 20. Second laser contour scanner; 21. Preform defect; 22. Additive repair area. Detailed Implementation
[0023] To make the objectives, technical solutions, and advantages of this application clearer, the following detailed description is provided in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the scope of this application.
[0024] This application discloses an in-situ repair device for defects in the billet-making process of large forgings. It enables an integrated closed-loop process of "online detection—instant repair—in-situ forging" for defects such as folds and surface cracks generated during the billet-making stage of large forgings. The device includes a forging press body 6, an online detection unit, a machining unit, an electric arc additive manufacturing unit, and a control system. The control system is connected to the forging press body 6, the online detection unit, the machining unit, and the electric arc additive manufacturing unit, respectively, and centrally controls the coordinated operation of these components.
[0025] Reference Figure 1 The forging press body 6, as the core station of the entire process, is used to form the large forging preform 16. It is a commonly used forging press in this field and is equipped with a forging operation area. Its forging principle and specific structure will not be described in detail. The online detection unit is set on the forging press body 6, including an infrared thermal imager 18, a first laser profile scanner 17, and a second laser profile scanner 20, for real-time monitoring of the forming quality of the large forging preform 16. The machining unit and the arc additive manufacturing unit are respectively arranged on two transmission devices in front of the forging press. The transmission devices drive the machining unit and the arc additive manufacturing unit to move to the appropriate working position. The machining unit includes a machining unit conveyor 15, a second six-axis robot 9, and a machining head. The machining head first locally cools the preform defects 21 on the large forging preform 16, and then performs machining to remove the defects. The electric arc additive manufacturing unit includes an additive manufacturing unit conveyor 1, a first six-axis robot 3, and an electric arc additive manufacturing equipment. It is used to perform electric arc additive filling and repair on the additive repair area 22 formed by removing defects 21 from the preform of a large forging preform 16. The electric arc additive manufacturing equipment utilizes the high heat input characteristic of electric arc additive manufacturing to heat the repair area, ensuring that its post-repair temperature matches the temperature of the main body of the large forging.
[0026] In the billet-making process of large forgings, an online detection unit integrated into the forging press monitors the surface of the forging in real time. Local areas where defects occur in the forging typically exhibit significant temperature field changes and three-dimensional morphological changes. Model comparison algorithms are used to monitor defects such as folds and cracks in real time. When defects such as folds or surface cracks are detected during the billet-making process, a pre-formed defect 21 is generated. Once the control system determines that the defect characteristics exceed a preset safety threshold, the system immediately locks its spatial location and triggers an alarm. Simultaneously, a defect report with precise coordinates is generated, and the forging press body 6 immediately stops operating. The machining unit and the arc additive manufacturing unit are then moved sequentially to the front of the working area of the forging press body 6 to remove defects and perform additive repair. After repair, the forging press body 6 performs forging strengthening, achieving online real-time repair of forging defects within the current production cycle. This method eliminates the lengthy process of "stopping the machine to cool down, offline transfer, and repeated heating" in traditional processes, significantly shortening the production cycle. It also eliminates the additional heating cycles and preheating / post-heating steps required for independent repair, significantly reducing energy consumption and manufacturing costs, and improving production efficiency.
[0027] During the billet preparation process of large forgings, when pre-formed billet defect 21 occurs, significant abnormal changes in the temperature field and abrupt changes in three-dimensional morphology will appear. The online detection unit can accurately monitor the temperature and morphology in real time. For details, refer to... Figure 2 A third six-axis robot 19 is fixedly installed on the main body 6 of the forging press. An infrared thermal imager 18 is fixedly installed at the front end of the arm of the third six-axis robot 19. Through the multi-degree-of-freedom movement of the third six-axis robot 19, the infrared thermal imager 18 can freely adjust its position, thereby monitoring the temperature field changes of the processing part of the large forging preform 16 from all directions. At the same time, the first laser profile scanner 17 and the second laser profile scanner 20 are symmetrically arranged on the left and right sides of the forging platform of the main body 6 of the forging press, respectively, and scan synchronously from the left and right angles to realize the three-dimensional morphology online monitoring during the large forging process. When the infrared thermal imager 18 detects an area with obvious abnormal temperature field, and the first laser profile scanner 17 and the second laser profile scanner 20 simultaneously capture the three-dimensional morphology change area from both sides, the control system comprehensively determines that the preform defect 21 has occurred, immediately issues a stop command, stops the operation of the main body 6 of the forging press, and simultaneously starts the machining unit and the arc additive manufacturing unit to enter the subsequent repair stage. This dual-mode synchronous detection scheme achieves coordinated judgment of temperature field changes and three-dimensional morphology changes, avoiding missed detections or misjudgments that may occur with a single detection method, and significantly improving the accuracy and reliability of defect identification. Simultaneously, the first laser contour scanner 17 and the second laser contour scanner 20 scan synchronously from both sides, effectively eliminating visual blind spots present in single-sided scanning and improving the completeness and accuracy of morphology detection.
[0028] After the forging press body 6 is shut down, the machining unit first removes the defective areas. (Refer to...) Figure 3 In the machining unit, the second six-axis robot 9 is bolted to the machining unit conveyor 15 in front of the forging press body 6, and the machining head is fixedly mounted on the front end of the arm of the second six-axis robot 9. The machining head includes an integrated hydraulic motor 7, a power head 8, and a cooling air nozzle 14. The hydraulic motor 7 is connected to an external hydraulic station 10 through three oil pipes (including an oil inlet pipe, an oil return pipe, and an oil drain pipe), which provides hydraulic power. The power head 8 is connected to an external tool cooling hydraulic pump 12 through pipes to achieve internal circulation cooling of the tool. The cooling air nozzle 14 is connected to an external air cooling device 11 through pipes, which supplies compressed cooling gas. When the online detection unit detects a preform defect 21, the forging press body 6 immediately stops working, and the machining unit conveyor 15 is then activated to convey the second six-axis robot 9 and the machining head to the front of the working area of the forging press body 6. Upon reaching the desired position, the cooling gas nozzle 14 on the machining head is activated first. The cooling gas nozzle 14 automatically adjusts the gas spray range based on the defect geometry parameters. The control system, based on the defect location, size, and morphology data transmitted by the online detection unit, controls the movement of the second six-axis robot arm 9, adjusting the cooling area of the cooling gas nozzle 14 to provide targeted localized cooling only to the preform defect 21. Simultaneously, the control system controls the coordinated movement of the third six-axis robot arm 19, enabling the infrared thermal imager 18 to monitor the temperature changes of the preform defect 21 in real time, forming a temperature feedback closed loop. The target cooling temperature for the preform defect 21 is the lower limit of the soft tissue temperature range of the metal. Taking steel as an example, this is the pearlite microstructure temperature, approximately 500℃. This ensures that the metal is in a pearlite state with low hardness and good plasticity, and that the austenite transformation has not yet occurred. This temperature range avoids the large temperature difference caused by over-cooling, which could lead to new cracks, and also achieves a hot cutting effect. Through the high-temperature softening effect, the yield strength and cutting deformation resistance of the material can be significantly reduced, making the cutting process smoother and greatly improving defect removal efficiency. Meanwhile, the improved material plasticity enhances chip morphology, reduces impact and vibration during cutting, and improves surface finish and tool life. Furthermore, the use of hot cutting completely eliminates the need for cutting fluid; the tool is cooled internally by a hydraulic pump 12 that circulates cooling to the power head 8. A central cooling channel is machined inside the tool body, allowing fluid to flow from the shank to near the front face of the tool body. This prevents cutting fluid from falling onto the forging surface and causing cracking due to rapid cooling, and also avoids contamination of the forging by the cutting fluid.
[0029] After the preform defect 21 is locally cooled to a suitable temperature, the power head 8 is activated to machine and remove the preform defect 21. Specifically, the hydraulic station 10 drives the hydraulic motor 7 through three oil pipes, and the hydraulic motor 7 drives the gear-driven power head 8, enabling the power head 8 to output high torque at low speeds, fully meeting the requirements of large-margin cutting for the main cutting force. The housing of the power head 8 is made of high-strength lightweight alloy material to balance structural rigidity and robot end-effector load-bearing limitations. The end mill installed at its front end is an indexable corn mill cutter 13. This cutter is installed at the front end of the power head 8, and its multiple inserts are staggered along the circumferential and axial directions, which can divide wide chips into narrow and thick segments, significantly reducing the single-edge cutting force from the root and effectively suppressing the low-frequency chatter that is prone to occur due to the poor rigidity of the robot's serial structure. At the same time, the inserts of this cutter can be quickly indexed or replaced after wear, without the need for overall tool removal, which is highly economical and particularly suitable for high-consumption roughing conditions. During the machining process, the cooling gas nozzle 14 continuously sprays cooling gas into the cutting area to help reduce the temperature of the cutting area and improve cutting conditions. The cooling gas nozzle 14 is a forced cooling nozzle array distributed around the indexable corn milling cutter 13. Its gas spray range can be dynamically adjusted according to the size of the defect area, and it is used to perform targeted local cooling on the preform defect 21. After machining, the preform defect 21 is completely removed, and a regular repair bevel is formed. The location of this repair bevel is the additive repair area 22, which provides good interface conditions for subsequent additive repair.
[0030] After the defects are removed and a repair bevel is formed, the arc additive manufacturing unit then fills and repairs the additive repair area 22. (Refer to...) Figure 4In the arc additive manufacturing unit, the first six-axis robot 3 is mounted on the additive manufacturing unit conveyor 1 in front of the forging press body 6. The arc additive manufacturing equipment includes multiple arc welding torches 5, which are connected to the external wire feeding device 2 and the welding torch power supply. The multiple arc welding torches 5 are integrated and mounted at the front end of the arm of the first six-axis robot 3. After the preform defect 21 is removed by machining and a repair bevel is machined, the machining unit conveyor 15 transports the second six-axis robot 9 away. The additive manufacturing unit conveyor 1 immediately transports the first six-axis robot 3 and the multiple arc welding torches 5 to the front of the working area of the forging press body 6 to perform additive repair on the additive repair area 22. The machining unit conveyor 15 and the additive manufacturing unit conveyor 1 work together to avoid interference between the second six-axis robot 9 and the first six-axis robot 3. The control system obtains the specific three-dimensional shape of the defect to be removed based on the tool path of the machining process, and then performs trajectory planning for the arc additive manufacturing unit. The first six-axis robot 3, carrying the multi-arc welding torch 5, plans the path according to the three-dimensional shape of the bevel and moves along the filling direction, while adjusting the array position of the multi-arc welding torch 5. Specifically, when the defect area to be removed is long and narrow, a single-row, multi-column array of multi-arc welding torches is used for additive repair to effectively overcome the positional limitations of the narrow space and improve additive efficiency. When the defect area to be removed is wide, a multi-row, multi-column array of multi-arc welding torches is used for additive repair to ensure uniform deposition over a large area. During the additive repair process, multiple welding torches simultaneously ignite and feed wire synchronously, allowing multiple molten droplets to converge into the same or adjacent molten pools in a short time, achieving an extremely high deposition rate and a heat input far exceeding that of a single arc. Utilizing the high heat input characteristics of the arc itself, the repair area and surrounding area are simultaneously and rapidly and uniformly heated to the same temperature as the forging matrix. Multiple metal wires 4 are simultaneously fed into the multi-arc welding torch 5 by the wire feeding device 2 and the wire feeding speed is controlled. The welding torch power supply is used to power the multi-arc welding torch 5 to achieve high-efficiency collaborative deposition.
[0031] During the arc additive repair process, the infrared thermal imager 18 on the arm of the third six-axis robot 19 monitors the temperature changes of the additive repair area 22 in real time, forming a closed-loop temperature control. When the temperature is low, the control system instructs to increase the heat input of the arc additive process; when the temperature is too high, it reduces the heat input of the arc additive process to prevent local overheating and microstructural deterioration. Since the aforementioned machining is hot cutting, after the preform defect 21 is removed, the repair bevel of the additive repair area 22 still has a high temperature, about 500°C. At this time, additive repair is equivalent to achieving the effect of substrate preheating, thereby reducing energy consumption and improving work efficiency. Compared with direct additive processing without preheating the substrate, the cold substrate without preheating causes the cladding layer to cool rapidly, the interface is only mechanically interlocked and there are a large number of unfused defects. The huge tensile thermal stress is prone to warping and cracking. In the current process, substrate preheating significantly improves the metallurgical bonding quality between the substrate and the deposited layer interface. By slowing down the cooling rate of the molten pool, time is provided for the full diffusion and wetting of elements at the interface, thereby eliminating unfused defects and improving the interface bonding strength. Simultaneously, the high heat input of the electric arc rapidly raises the temperature of the repaired area, significantly reducing the temperature gradient near the interface and effectively suppressing thermal stress caused by rapid contraction, thus preventing crack initiation at the interface. Utilizing the high heat input characteristic of electric arc additive manufacturing, the repaired area is heated simultaneously with the additive repair process, ensuring its temperature matches that of the main body of the large forging. After repair, the forging can be directly transferred to subsequent forging processes without requiring reheating in the furnace.
[0032] After the arc additive repair is completed, the additive unit conveyor 1 transports the first six-axis robot 3 away, and the forging press body 6 immediately starts. The large forging preform 16 is immediately transferred to the subsequent forging process, thus eliminating the additional preheating step, eliminating additive casting defects, and ensuring the streamline integrity of the large forging. After the additive repair is completed, the deposition layer in the additive repair zone 22 is higher than the matrix of the large forging preform 16, such as... Figure 5As shown, this design prevents depressions from forming during subsequent forging. Specifically, the portion of the additive repair zone 22 that protrudes above the substrate is trapezoidal in shape, with the ratio of the length L of the top region of the trapezoid to the height H of the trapezoid being 1 to 1.5. This avoids the recurrence of folding defects during subsequent forging. The limitation of this geometric parameter ensures that the metal can flow fully and fill the additive repair zone 22 during forging, forming dense forging flow lines. Forging the additive repair zone 22 using the subsequent stroke of the forging press body 6 can eliminate casting defects such as porosity and gas bubbles that may exist in the additive structure, eliminate the anisotropy caused by the layer-by-layer accumulation of the additive deposition layer, and allow the metal in the additive repair zone 22 to undergo sufficient plastic deformation and dynamic recrystallization. Ultimately, this results in a fine-grained structure and mechanical properties comparable to the body of the large forging preform 16, while ensuring the flow line integrity of the large forging. After the additive filling is completed, the forging is immediately transferred to the subsequent forging process, thus eliminating the need for an additional preheating step. The repair area is forged using the subsequent stroke of the forging equipment to eliminate the porosity and anisotropy that may exist in the additive structure, allowing the metal in the repair area to undergo sufficient plastic deformation and dynamic recrystallization, ultimately obtaining a fine-grained structure and mechanical properties comparable to the forging body.
[0033] This application also discloses an in-situ repair method for defects in the billet preparation process of large forgings, which uses the aforementioned in-situ repair equipment and includes the following steps: S1. The forging press body 6 forms the large forging preform 16. The infrared thermal imager 18, the first laser profile scanner 17, and the second laser profile scanner 20 in the online detection unit monitor the surface temperature field and three-dimensional morphology of the large forging preform 16 in real time. When the preform defect 21 is detected, the control system controls the forging press body 6 to stop and lock the defect location.
[0034] S2. The control system controls the machining unit conveying device 15 to convey the second six-axis robot 9 and the machining head to the front of the working area of the forging press body 6. The second six-axis robot 9 drives the machining head to move to the preform defect 21. The cooling air nozzle 14 performs localized cooling on the preform defect 21. The hydraulic motor 7 drives the power head 8 to rotate the indexable corn milling cutter 13 to mill and remove the preform defect 21, forming the additive repair area 22. After the removal is completed, the machining unit resets and exits the working area.
[0035] S3. The control system controls the additive manufacturing unit conveying device 1 to convey the first six-axis robot 3 and the electric arc additive manufacturing equipment to the front of the working area of the forging press body 6. The first six-axis robot 3 drives the multi-arc welding torch 5 to move to the additive repair area 22. The wire feeding device 2 feeds multiple metal wires 4 into the multi-arc welding torch 5. The multi-arc welding torch 5 fills the additive repair area 22 layer by layer until it is full and slightly higher than the surface of the large forging preform 16. After the additive repair is completed, the electric arc additive unit is reset and exits the working area.
[0036] S4. The control system starts the forging press body 6. The forging press body 6 forges and strengthens the additive repair area 22, so that the surface of the additive repair area 22 is flush with the surface of the large forging preform 16, and the microstructure and properties are close to the matrix, thus completing the in-situ repair of the defect.
[0037] In this embodiment, a continuous process of "online detection → local cooling → hot cutting removal → preheated arc additive manufacturing → instant forging" is adopted. First, online instant repair is achieved, that is, the defect 21 of the preform is detected and repaired immediately during the billet making process, without stopping the machine, moving it out of the workstation, or reheating, completely eliminating all the auxiliary processes of traditional offline repair. Second, hot cutting and preheating are coordinated, that is, the residual heat of hot cutting is used as the substrate preheating of the additive repair area 22, which reduces the cutting resistance, improves the removal efficiency, and improves the metallurgical bonding quality of the additive interface. Third, closed-loop temperature field control is achieved, with the infrared thermal imager 18 running through the entire process of defect identification, cooling control, and additive monitoring to ensure that each process is executed within the optimal temperature window. Then, the forging structure is densified, and the subsequent stroke of the forging press body 6 is used to directly forge, eliminating the casting defects of the additive structure, so that the additive repair area 22 obtains a forging structure consistent with the matrix of the large forging preform 16. Finally, the integrity of the streamline is guaranteed. The scientific limitation of the trapezoidal geometric parameters of the additive repair area 22 ensures the continuity and integrity of the metal streamline after forging.
[0038] It should be understood that expressions such as "comprising" and "may include" as used in this application indicate the existence of the disclosed functions, operations, or constituent elements, and do not limit one or more additional functions, operations, and constituent elements. In this application, terms such as "comprising" and / or "having" may be interpreted as indicating a specific characteristic, number, operation, constituent element, component, or combination thereof, but should not be interpreted as excluding the existence or possibility of adding one or more other characteristics, numbers, operations, constituent elements, components, or combinations thereof.
[0039] It should be understood that the terms “center,” “upper,” “lower,” “front,” “rear,” “left,” “right,” “vertical,” “horizontal,” “inner,” “outer,” “clockwise,” “counterclockwise,” “axial,” “radial,” and “circumferential” indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this application.
[0040] Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of that feature. In the description of this application, "multiple" means two or more, unless otherwise explicitly specified.
[0041] In this application, unless otherwise expressly specified and limited, the terms "installation," "connection," "linking," and "fixing," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection between two components. Those skilled in the art can understand the specific meaning of the above terms in this application according to the specific circumstances.
[0042] Those skilled in the art will readily understand that the above description is merely a preferred embodiment of this application and is not intended to limit this application. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of this application should be included within the protection scope of this application.
Claims
1. An in-situ repair device for defects in the billet making process of large forgings, characterized in that, include: The forging press body (6) is used to form large forging preforms (16); An online detection unit is installed on the main body (6) of the forging press and is used to monitor the large forging preform (16) in real time. A machining unit is used to locally cool and remove the preform defects (21) on the large forging preform (16); An electric arc additive manufacturing unit is used to perform electric arc additive filling repair on the additive repair area (22) formed by removing defects (21) from the preform on the large forging preform (16). The control system is connected to the forging press body (6), the online detection unit, the machining unit and the electric arc additive manufacturing unit respectively. When the online detection unit detects that a preform defect (21) is generated on the surface of the large forging preform (16), the control system controls the forging press body (6) to stop working and controls the machining unit and the electric arc additive manufacturing unit to move in sequence to the front of the working area of the forging press body (6) to remove defects and perform additive repair. After the repair is completed, the forging press body (6) will perform forging strengthening.
2. The in-situ repair equipment for defects in the billet making process of large forgings as described in claim 1, characterized in that, The online detection unit includes an infrared thermal imager (18). A third six-axis robot (19) is fixedly installed on the forging press body (6). The infrared thermal imager (18) is installed at the front end of the arm of the third six-axis robot (19). The third six-axis robot (19) drives the infrared thermal imager (18) to move in multiple degrees of freedom to monitor the temperature field changes on the surface of the large forging preform (16).
3. The in-situ repair equipment for defects in the billet making process of large forgings as described in claim 2, characterized in that, The online detection unit also includes a first laser profile scanner (17) and a second laser profile scanner (20). The first laser profile scanner (17) and the second laser profile scanner (20) are respectively located on the left and right sides of the working area of the forging press body (6) to simultaneously scan the three-dimensional shape of the large forging preform (16) from both sides.
4. The in-situ repair equipment for defects in the billet making process of large forgings as described in claim 1, characterized in that, The machining unit includes a machining unit conveying device (15), a second six-axis robot (9), and a machining head. The second six-axis robot (9) is mounted on the machining unit conveying device (15), and the machining head is mounted on the front end of the arm of the second six-axis robot (9). The machining unit conveying device (15) is used to convey the second six-axis robot (9) and the machining head to the front of the working area of the forging press body (6).
5. The in-situ repair equipment for defects in the billet making process of large forgings as described in claim 4, characterized in that, The machining head includes an integrated hydraulic motor (7), a power head (8), and a cooling air nozzle (14). The hydraulic motor (7) is connected to an external hydraulic station (10), the power head (8) is connected to an external tool cooling hydraulic pump (12), and the cooling air nozzle (14) is connected to an external air cooling device (11).
6. The in-situ repair equipment for defects in the billet making process of large forgings as described in claim 5, characterized in that, The power head (8) is equipped with an indexable corn milling cutter (13) at its front end. The multiple blades of the indexable corn milling cutter (13) are arranged in a staggered manner along the circumferential and axial directions to divide wide chips into narrow and thick segments to reduce single-edge cutting force.
7. The in-situ repair equipment for defects in the billet making process of large forgings as described in claim 6, characterized in that, The cooling air nozzle (14) is a forced cooling nozzle array distributed around the indexable corn milling cutter (13) for localized cooling of the preform defect (21).
8. The in-situ repair equipment for defects in the billet making process of large forgings as described in claim 1, characterized in that, The electric arc additive manufacturing unit includes an additive manufacturing unit conveying device (1), a first six-axis robot (3), and an electric arc additive manufacturing device. The first six-axis robot (3) is mounted on the additive manufacturing unit conveying device (1), and the electric arc additive manufacturing device is mounted on the front end of the arm of the first six-axis robot (3). The additive manufacturing unit conveying device (1) is used to convey the first six-axis robot (3) and the electric arc additive manufacturing device to the front of the working area of the forging press body (6).
9. The in-situ repair equipment for defects in the billet making process of large forgings as described in claim 8, characterized in that, The electric arc additive manufacturing equipment includes a multi-arc welding torch (5), which is mounted on the first six-axis robot (3) and is used to perform electric arc additive filling repair on the additive repair area (22). The multi-arc welding torch (5) is connected to an external wire feeding device (2) and a welding torch power supply. The wire feeding device (2) is used to feed multiple metal wires (4) into the multi-arc welding torch (5) at the same time. The welding torch power supply is used to supply power to the multi-arc welding torch (5).
10. A method for in-situ repair of defects in the billet-making process of large forgings, comprising using the in-situ repair equipment as described in any one of claims 1-9, characterized in that, Includes the following steps: S1. The forging press body (6) forms the large forging preform (16). The online detection unit monitors the large forging preform (16) in real time. When a defect (21) in the preform is detected, the control system controls the forging press body (6) to stop. S2. The control system controls the machining unit to move to the front of the working area of the forging press body (6) to locally cool and remove the defects (21) of the preform, forming an additive repair area (22). S3. The control system controls the machining unit to reset and controls the arc additive manufacturing unit to move to the front of the working area of the forging press body (6). The arc additive manufacturing unit performs arc additive manufacturing repair on the additive repair area (22). S4. The forging press body (6) forges and strengthens the additive repair area (22) after the electric arc additive repair is completed, and completes the in-situ repair of the defect.