Milling and welding integrated friction plug repair welding tool and its welding method

The design of an integrated milling and welding tool for friction plug repair solves the problems of low efficiency and difficulty in ensuring coaxiality in existing technologies, enabling efficient and continuous milling and welding operations, and improving the accuracy and efficiency of friction plug repair welding.

CN123103403APending Publication Date: 2026-11-17SHANGHAI AEROSPACE EQUIPMENTS MANUFACTURER CO LTD +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202611618967.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-20
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing friction plug repair welding technology suffers from low efficiency and difficulty in ensuring coaxiality. In particular, the "milling before welding" separation process mode results in cumbersome procedures, large equipment footprint, and unresolved errors caused by multiple clamping operations.

Method used

Design a milling and welding integrated friction plug repair welding tool. The tool has a clamping section, a welding section, a transition section and a milling section distributed along the same axis. The integrated design eliminates secondary clamping deviations. The integrated tool is used for milling and welding. Combined with specific rotation and feed speed control, continuous operation of milling and repair welding can be achieved.

Benefits of technology

It significantly shortens repair time, ensures uniformity of the friction interface, improves joint quality, reduces mechanical errors, increases welding efficiency and precision, and adapts to repair needs of different hole diameters and depths.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123103403A_ABST
    Figure CN123103403A_ABST
Patent Text Reader

Abstract

This invention provides an integrated milling and welding friction plug repair tool and its welding method. The tool includes a clamping section, a welding section, a transition section, and a milling section located at the end of the tool, arranged sequentially along the same axis. The maximum radius of the transition section is smaller than both the minimum radius of the welding section and the maximum radius of the milling section. The welding section is a rotating body, with its small end radius being smaller than or equal to the maximum radius of the milling section, and its large end radius being larger than the maximum radius of the milling section. The method includes: clamping the tool on the welding machine spindle and driving it to rotate at high speed and feed axially; using the milling section to cut the defect area to form a plug hole; the transition section fully entering the plug hole without contacting the hole wall; subsequently, the welding section entering the plug hole, generating heat through interference fit friction, and completing solid-state welding under upsetting braking; finally, cutting off the tool at the transition section and grinding the remaining end face.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of friction welding technology, specifically to a milling and welding integrated friction plug repair welding tool and its welding method. Background Technology

[0002] Friction plug welding is a solid-state joining technique widely used in the repair of defects in metal components. A typical upsetting friction plug welding process requires first machining a precisely sized plug hole at the defect location through milling, drilling, or other methods. Then, the plug rod is clamped onto a spindle, rotated at high speed, and pressed into the plug hole, using frictional heat and upsetting force to complete the welding.

[0003] However, this two-step process separation of "milling before welding" has the following prominent drawbacks: Inefficient: After milling the plug hole, the tool needs to be retracted, the plug bar replaced, and a second tool setting or reclamping of the workpiece is required, which takes a long time to switch between processes.

[0004] Coaxiality is difficult to guarantee: the coaxiality deviation between the plug hole axis and the plug rod rotation axis can easily lead to uneven frictional heat generation and defects such as incomplete welding. Two independent clamping operations will inevitably introduce mechanical repetitive positioning errors.

[0005] To address the issues of cumbersome procedures, large equipment footprint, and errors caused by multiple clamping operations, related technologies have attempted to improve welding efficiency and quality by modifying the machine tool structure. For example, Chinese patent CN217122072U discloses a friction plug welding machine tool, which uses a telescopic structure built into the multi-support spindle assembly to drive the first clamping body at the output end to extend, retract, and rotate, causing the workpiece to contact the fixed workpiece and complete friction welding under the action of upsetting or pulling force.

[0006] However, this type of technical solution still has limitations: its focus is on optimizing the drive and telescopic transmission mechanism of the machine tool spindle, and it is essentially still a modification of equipment for a single welding process, failing to change the inherent pattern of "pre-milling" and "post-welding" being performed in separate steps. The secondary positioning errors of the workpiece or tool between the milling and welding stages, as well as the time-consuming changeover, have not been fundamentally resolved. Therefore, how to achieve efficient and continuous operation integrating "milling-welding" has become the key to further improving the accuracy and efficiency of friction plug welding. Summary of the Invention

[0007] To address the shortcomings of existing technologies, the purpose of this invention is to provide an integrated milling and welding friction plug repair tool and its welding method.

[0008] According to the present invention, a milling and welding integrated friction plug repair welding tool includes a clamping section, a welding section, a transition section, and a milling section located at the end of the tool, which are arranged sequentially along the same axis. The maximum radius of the transition section is smaller than both the minimum radius of the welding section and the maximum radius of the milling section. The welding section is a rotating body, and the radius of its end near the transition section is smaller than or equal to the maximum radius of the milling section, while the radius of its end away from the transition section is larger than the maximum radius of the milling section.

[0009] Preferably, the transition section and the milling section are detachably connected.

[0010] Preferably, one end of the transition section is provided with an external thread, and the center of the upper end face of the milling section is provided with an internal thread hole, and the transition section is threadedly connected to the milling section.

[0011] Preferably, the outer periphery of the transition section has a V-shaped annular groove on its surface.

[0012] Preferably, the clamping section has a cylindrical structure.

[0013] Preferably, the section of the welding segment closest to the transition section is a guide cone surface, and the taper of the guide cone surface is greater than the taper of the section of the welding segment furthest from the transition section.

[0014] Preferably, the milling section is provided with multiple helical cutting edges to form an end mill structure.

[0015] Preferably, the axial length of the transition section is greater than the maximum depth to which the welding section is pressed into the plug hole during welding.

[0016] According to another aspect of the present invention, a welding method for a milling-welding integrated friction plug repair welding tool is provided, wherein the tool is the aforementioned milling-welding integrated friction plug repair welding tool, and the axial length of the transition section is greater than the maximum depth to which the welding section is pressed into the plug hole during welding, the method comprising: Step S1: Clamp the clamping section onto the welding machine spindle; Step S2: The spindle drives the tool to rotate at high speed and feed along the axial direction. The milling section first contacts the workpiece surface and cuts the defect area to form a plug hole. Step S3: Maintain the rotation and feed of the spindle so that the transition section is fully inserted into the plug hole along the axial direction, wherein the transition section does not contact the hole wall during this process; Step S4: The welding section is continuously fed into the plug hole by the spindle. The welding section enters the plug hole with its front end near the transition section before the rest of the section, and is guided and squeezed into the plug hole by the rotation of the spindle and the axial feed. The outer peripheral surface of the welding section is pressed into the plug hole wall to generate frictional heat, so that the material in the contact area reaches a plasticized state. When the welding section reaches the preset pressing depth, the spindle is braked and stops rotating. At the same time, an axial forging force is applied to forge the welding section, so that the welding section completes solid-state welding with the hole wall under the forging pressure. Step S5: After welding is completed, cut the tool at the transition section to separate the milling section and the transition section from the welding section, and grind the end face of the welding section remaining on the workpiece surface smooth.

[0017] Preferably, in step S2, the spindle rotates at a first speed n1 and is fed axially at a first feed speed v1; in step S3, the spindle rotates at a second speed n2 and is fed axially at a second feed speed v2; in the friction stage of step S4, the spindle rotates at a third speed n3 and is fed axially at a third feed speed v3; wherein, v2 > v1, v3 < v1, and n3 < n1.

[0018] Preferably, n1 is 2000–4000 r / min, v1 is 100–800 mm / min; n2 is 1500–3000 r / min, v2 is 150–900 mm / min; n3 is 1000–2500 r / min, v3 is 20–250 mm / min.

[0019] Preferably, in the upsetting braking stage of step S4, the spindle is braked from n3 to 0 within the braking time Δt, where Δt is 0.1 to 1.0 s, and the applied axial upsetting force F is 5 to 50 kN.

[0020] Preferably, in step S5, the transition section is broken by striking the location of the annular groove on the outer peripheral surface of the transition section.

[0021] Compared with the prior art, the present invention has the following beneficial effects: This invention integrates milling and welding functions into one unit, eliminating the need for tool changing and setting, and significantly shortening repair time. The tool is an integrated design or a rigid assembly, with the milling section axis and the welding section axis being the same axis, fundamentally eliminating secondary clamping deviations, ensuring a uniform friction interface, and improving joint quality. The reduced outer diameter transition section provides space and time for chip removal and cooling in the milling section, as well as for the "delayed contact" between the welding section and the hole wall, ensuring a stable and controllable process. Combined with a detachable milling section, stress concentration grooves, and other structures, consumable replacement is convenient, adapting to repair needs for different hole diameters and depths. Attached Figure Description

[0022] Other features, objects and advantages of the present invention will become more apparent upon reading the detailed description of the non-restrictive embodiments with reference to the accompanying drawings: Figure 1 is a schematic structural diagram of the milling and welding integrated friction plug repair welding tool according to the first embodiment of the present invention.

[0023] Figure 2 is a schematic diagram of the states at each stage of the welding process using the Figure 1 tool shown in the drawing.

[0024] Figure 3 is a schematic structural diagram of the tool with a stress concentration groove according to the second embodiment.

[0025] Reference numerals of the accompanying drawings: 1. Clamping section; 2. Welding section; 2a. Guide conical surface; 3. Transition section; 3a. Stress concentration groove; 4. Milling section; 5. Workpiece; 6. Gap. Detailed Description of the Embodiments

[0026] The present invention will be described in detail below with reference to specific embodiments. The following embodiments will help those skilled in the art to further understand the present invention, but do not limit the present invention in any form. It should be noted that several variations and improvements can be made by those of ordinary skill in the art without departing from the concept of the present invention, all of which fall within the protection scope of the present invention.

[0027] Embodiment 1: This embodiment provides a milling and welding integrated friction plug repair welding tool. As shown in Figure 1 the drawing, the tool comprises a clamping section 1, a welding section 2, a transition section 3, and a milling section 4 located at the end of the tool, which are sequentially distributed along the same axis. The clamping section 1 has a cylindrical structure with a diameter of D1. The welding section 2 is the main working area for upsetting type friction plug repair welding, and its outer shape is a revolving body. The small end (the end close to the transition section 3) has a diameter of d, and the large end (the end far away from the transition section 3) has a diameter of D2, which satisfies d≤D4 and D2>D4, where D4 is the maximum diameter of the milling section 4. The front end of the welding section 2 close to the transition section 3 is provided with a guide conical surface 2a, the minimum diameter of the guide conical surface 2a is d, which satisfies d≤D4. The diameter D2 of the large end of the welding section 2 is larger than the maximum diameter D4 of the milling section 4, so as to ensure interference friction.

[0028] The milling section 4 is located at the rearmost end, on which a plurality of spiral cutting edges are directly arranged to form an end mill structure, and its maximum diameter (outer diameter of the cutting edges) is d4.

[0029] The transition section 3 is a cylinder with a significantly reduced diameter, and its diameter D3 satisfies: D3<D4 and D3<d. The length L3 of the transition section 3 is greater than the maximum depth that the welding section 2 is pressed into the plug hole during welding.

[0030] Based on the above tools, this embodiment provides a welding method, such as... Figure 2 As shown, the method includes: Step S1: Clamp section 1 onto the welding machine spindle; Step S2: The spindle drives the tool to rotate at high speed and feed along the axial direction. The milling section 4 first contacts the surface of the workpiece 5 to cut the defect area and form a plug hole. Based on the above solutions, such as Figure 2 As shown in Figure (a), the spindle drives the tool to rotate at a predetermined speed and feed downwards. The cutting edge of the milling section 4 first contacts the defect area of ​​the workpiece 5, milling it to form a circular plug hole with a diameter approximately equal to D4. At this time, since D3 is much smaller than D4, an annular gap 6 is formed between the outer circumference of the transition section 3 and the hole wall, and they do not contact each other at all, as shown in Figure (a). Figure 2 As shown in Figure (b).

[0031] Step S3: Maintain the rotation and feed of the spindle so that the transition section 3 is fully inserted into the plug hole along the axial direction, wherein the transition section 3 does not contact the hole wall during this process; Based on the above scheme, the spindle continues to feed, and after the transition section 3 is fully inserted into the plug hole, the guide cone surface 2a at the front end of the welding section 2 (its minimum diameter is d, which satisfies d≤D4) begins to contact the hole opening and is smoothly squeezed into the plug hole during rotation. Since the large end diameter D2>D4 of the welding section 2, its outer surface generates severe interference friction with the hole wall, causing the contact surface material to be rapidly plasticized.

[0032] Step S4: The welding section 2 is continuously fed by the spindle to enter the plug hole; the welding section 2 enters the plug hole with its front end near the transition section 3 before the rest of the part, and is guided and squeezed into the plug hole under the action of spindle rotation and axial feed; the outer peripheral surface of the welding section 2 is interference-fitted with the plug hole wall to generate frictional heat, so that the material in the contact area reaches a plasticized state; when the welding section 2 reaches the preset pressing depth, the spindle brakes and stops rotating, and at the same time, an axial forging force is applied for forging, so that the welding section 2 completes solid-phase welding with the hole wall under the forging pressure.

[0033] Based on the above scheme, when the spindle reaches the preset upset position, the spindle is braked and stops rotating. At the same time, a downward upset force is applied, and the welded section 2 is completely pressed into the plug hole. Its material and the hole wall of the workpiece 5 complete solid-phase diffusion bonding under pressure, such as... Figure 2 As shown in Figure (c). At this time, the milling section 4 can extend from the back of the workpiece 5 or remain in the scrap at the bottom of the hole. The preset pressing depth can be determined according to the workpiece plate thickness and the plugging depth; in this embodiment, it is approximately 80% of the plate thickness.

[0034] Step S5: After welding is completed, cut the tool at the transition section 3 to separate the milling section 4 and the transition section 3 from the welding section 2, and grind the end face of the welding section 2 remaining on the surface of the workpiece 5 flat.

[0035] In this embodiment, the process parameters for each step can be set as follows: Step S2 Milling stage: Spindle speed n1 is 2000~4000r / min, axial feed rate v1 is 100~800mm / min; Step S3 Transition Stage: The spindle speed n2 is 1500~3000 r / min, the axial feed speed v2 is 150~900 mm / min, and v2 is greater than v1, so as to shorten the idle travel time of the transition section through the plug hole; Step S4 Welding friction stage: The spindle speed n3 is 1000~2500 r / min, the axial feed speed v3 is 20~250 mm / min, and n3 is less than n1, v3 is less than v1, so as to ensure that the welding section and the hole wall generate heat through sufficient friction. Step S4 Upsetting braking stage: The spindle is braked from n3 to 0 within the braking time Δt, where Δt is 0.1 to 1.0 s, and at the same time, an axial upsetting force F is applied, where F is 5 to 50 kN.

[0036] The above parameters can be adjusted according to the workpiece material, hole diameter, and plate thickness. In this embodiment, the workpiece is an aluminum alloy plate with a thickness of 8mm, the plug hole diameter D4 = 10mm, n1 = 3000r / min, v1 = 300mm / min, n2 = 2000r / min, v2 = 400mm / min, n3 = 1500r / min, v3 = 75mm / min, Δt = 0.3s, and F = 15kN.

[0037] Example 2: In this embodiment, the transition section 3 and the milling section 4 are detachably connected. Specifically, one end of the transition section 3 is provided with an external thread, and the center of the upper end face of the milling section 4 is provided with an internal thread hole. The transition section 3 and the milling section 4 are threadedly connected. Additionally, a V-shaped annular groove is provided on the middle section of the outer periphery of the transition section 3. Chip removal grooves may also be provided on the outer periphery of the transition section.

[0038] Based on the above scheme, see Figure 3 In this embodiment, a V-shaped annular groove is machined in the middle of the transition section 3 to form a stress concentration groove 3a. After welding, simply tapping one side of the milled section 4 will cause the tool to break precisely along the groove, resulting in a clean fracture and reducing subsequent grinding. Furthermore, the base of the milled section 4 is fixed to the lower end of the transition section 3 via a threaded connection, forming a detachable structure. Milled sections 4 of different diameters can be replaced according to the size of the defect, or worn sections 4 can be replaced individually, allowing the welded section 2 to be reused.

[0039] The above are merely preferred embodiments of the present invention and do not limit its patent protection scope. The protection scope of the present invention is determined by the claims, and any equivalent substitutions or modifications based on the concept of the present invention should fall within the protection scope of the present invention.

[0040] In the description of this application, it should be understood that the terms "upper", "lower", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this application.

[0041] Specific embodiments of the present invention have been described above. It should be understood that the present invention is not limited to the specific embodiments described above, and those skilled in the art can make various changes or modifications within the scope of the claims, which do not affect the essence of the present invention. Unless otherwise specified, the embodiments and features described in this application can be arbitrarily combined with each other.

Claims

1. A milling and welding integrated friction plug repair welding tool, characterized in that, It includes a clamping section, a welding section, a transition section, and a milling section located at the end of the tool, which are distributed sequentially along the same axis. The maximum radius of the transition section is smaller than both the minimum radius of the welding section and the maximum radius of the milling section; The welding section is a rotating body, with the radius of the end closest to the transition section being less than or equal to the maximum radius of the milling section, and the radius of the end of the welding section furthest from the transition section being greater than the maximum radius of the milling section.

2. The milling and welding integrated friction plug repair welding tool according to claim 1, characterized in that, The transition section and the milling section are detachably connected. One end of the transition section is provided with an external thread, and the center of the upper end face of the milling section is provided with an internal thread hole. The transition section and the milling section are threadedly connected.

3. The milling and welding integrated friction plug repair welding tool according to claim 1, characterized in that, The outer periphery of the transition section has a V-shaped annular groove on its middle section surface, and the clamping section has a cylindrical structure.

4. The milling and welding integrated friction plug repair tool according to claim 1, characterized in that, The section of the welding segment closest to the transition section is a guide cone surface, and the taper of the guide cone surface is greater than the taper of the section of the welding segment furthest from the transition section.

5. The milling and welding integrated friction plug repair tool according to claim 1, characterized in that, The milling section is provided with multiple helical cutting edges to form an end mill structure, and the axial length of the transition section is greater than the maximum depth to which the welding section is pressed into the plug hole during welding.

6. A welding method for an integrated milling and welding friction plug repair welding tool, characterized in that, include: Step S1: Clamp the clamping section onto the welding machine spindle; Step S2: The spindle drives the tool to rotate at high speed and feed along the axial direction. The milling section first contacts the workpiece surface and cuts the defect area to form a plug hole. Step S3: Maintain the rotation and feed of the spindle so that the transition section is fully inserted into the plug hole along the axial direction, wherein the transition section does not contact the hole wall during this process; Step S4: The welding section is continuously fed into the plug hole by the spindle. The welding section enters the plug hole with its front end near the transition section before the rest of the section, and is guided and squeezed into the plug hole by the rotation of the spindle and the axial feed. The outer peripheral surface of the welding section is pressed into the plug hole wall to generate frictional heat, so that the material in the contact area reaches a plasticized state. When the welding section reaches the preset pressing depth, the spindle is braked and stops rotating. At the same time, an axial forging force is applied to forge the welding section, so that the welding section completes solid-state welding with the hole wall under the forging pressure. Step S5: After welding is completed, cut the tool at the transition section to separate the milling section and the transition section from the welding section, and grind the end face of the welding section remaining on the workpiece surface smooth.

7. The welding method of the milling and welding integrated friction plug repair welding tool according to claim 6, characterized in that, In step S2, the spindle rotates at a first speed n1 and is fed axially at a first feed rate v1; in step S3, the spindle rotates at a second speed n2 and is fed axially at a second feed rate v2; in the friction stage of step S4, the spindle rotates at a third speed n3 and is fed axially at a third feed rate v3. Where v2 > v1, v3 < v1, and n3 < n1.

8. The welding method of the milling and welding integrated friction plug repair welding tool according to claim 7, characterized in that, n1 is 2000–4000 r / min, v1 is 100–800 mm / min; n2 is 1500–3000 r / min, v2 is 150–900 mm / min; n3 is 1000–2500 r / min, v3 is 20–250 mm / min.

9. The welding method of the milling and welding integrated friction plug repair welding tool according to claim 7, characterized in that, In the upsetting braking stage of step S4, the spindle is braked from n3 to 0 within the braking time Δt, where Δt is 0.1 to 1.0 s, and the applied axial upsetting force F is 5 to 50 kN.

10. The welding method of the milling and welding integrated friction plug repair welding tool according to claim 6, characterized in that, The tool also includes a V-shaped annular groove on the outer periphery of the transition section; in step S5, the transition section is broken by striking the location of the annular groove.

Citation Information

Patent Citations

  • Friction plug repair welding machine tool

    CN217122072U