A low-odor, long-lasting anti-fog film and its preparation method
By using porous inorganic carriers and nonionic surfactant composite particles to form a slow-release antifogging agent in BOPP film, and combining it with organically modified nanoscale mineral materials as odor adsorbents, the problems of droplet formation and odor release in BOPP film under high humidity conditions are solved, achieving long-lasting antifogging and low-odor effects.
Patent Information
- Application Number
- CN202611173537.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-04
- Publication Date
- 2026-11-17
AI Technical Summary
Existing BOPP films are prone to forming droplets in high humidity environments, leading to odor problems and the migration and precipitation of anti-fogging agents, which affects user experience and the contents of the packaging.
A slow-release antifogging agent is formed by using porous inorganic carriers and nonionic surfactant composite particles, and combined with organic modified nanoscale mineral materials as odor adsorbents to prepare a low-odor, long-lasting antifogging film.
It effectively extends the anti-fogging performance, reduces odor release, improves the compatibility and anti-fogging effect of the film, and reduces the risk of odor pollution.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] This invention belongs to the field of polymer packaging materials technology, specifically relating to a low-odor, long-lasting anti-fog film and its preparation method. Background Technology
[0002] Bis-directional polypropylene (BOPP) film is widely used in the packaging of fresh fruits and vegetables and food due to its advantages such as being colorless, odorless, non-toxic, highly transparent, and having high tensile strength. However, when BOPP film is used as packaging material in high-humidity environments or cold chain transportation, moisture in the air easily condenses on the film surface, forming tiny droplets that severely affect the product's display effect. To solve this problem, the industry commonly uses the method of adding anti-fogging agents to the film. Anti-fogging agents are usually surfactants containing hydrophilic groups, which migrate to the film surface and reduce surface tension, allowing condensate to spread into a transparent water film. However, existing technologies have a significant drawback: the odor problem of anti-fogging films. To achieve the anti-fogging function, small-molecule anti-fogging agents (such as fatty acid glycerides, ethoxylated amines, etc.) and slip agents (such as erucamide) need to be added to the film. These low-molecular-weight substances continue to migrate to the surface and precipitate during film production and subsequent storage and use, which not only easily leads to a sticky film surface and reduced printability, but also releases irritating odors, affecting the user experience and even posing a risk of contaminating the contents of the package (such as food). This "foggy smell" is especially noticeable in high-temperature, high-humidity, or enclosed packaging environments.
[0003] To address the aforementioned issues, existing technologies such as patent CN116285040A, while extending the anti-fogging effect through hydrogen bonding between modified polypropylene resin and nonionic surfactants, primarily focus on improving anti-fogging performance and do not fundamentally solve the odor problem caused by excessive precipitation of small molecule additives. Furthermore, thermal oxidative decomposition and solvent residues during processing are also potential sources of odor.
[0004] Therefore, developing a BOPP anti-fog film that can maintain excellent anti-fog performance while significantly reducing odor has important practical value. Summary of the Invention
[0005] To address the shortcomings of existing technologies, the present invention aims to provide a low-odor, long-lasting anti-fog film and its preparation method, thereby solving the problems in the prior art.
[0006] The objective of this invention can be achieved through the following technical solutions: An anti-fog film, comprising, from bottom to top: a lower surface layer, a core layer, and an upper surface layer; The upper surface layer comprises the following raw materials by weight percentage: 5%–10% slow-release anti-fog masterbatch, 0.2%–0.6% odor absorber, and 89.4%–94.8% binary copolymer polypropylene; The raw materials for the slow-release anti-fogging masterbatch include: a slow-release anti-fogging agent and homopolymer polypropylene; the slow-release anti-fogging agent is a composite particle formed by a nonionic surfactant being physically adsorbed and anchored inside the pores and on the surface of a porous inorganic carrier.
[0007] Furthermore, the porous inorganic carrier is mesoporous silica, molecular sieve, or diatomaceous earth.
[0008] Furthermore, the nonionic surfactant comprises the following raw materials by mass percentage: 50% sorbitan monostearate and 50% polyglycerol fatty acid.
[0009] Furthermore, the slow-release antifogging masterbatch comprises the following raw materials in weight percentages: 30% to 35% slow-release antifogging agent and 65% to 70% homopolymer polypropylene.
[0010] Furthermore, the odor adsorbent is an organically surface-modified nanoporous mineral material.
[0011] Furthermore, the lower surface layer is a heat-sealing layer, which comprises the following raw materials by mass percentage: 1% to 3% anti-adhesion masterbatch and 97% to 99% ternary copolymer polypropylene; The anti-adhesion masterbatch comprises the following raw materials in weight percentages: 96%–98% homopolymer polypropylene and 2%–4% anti-adhesion agent. The anti-adhesion agent is irregularly shaped silica with a particle size of 3–5 μm.
[0012] Furthermore, the core layer comprises the following raw materials by weight percentage: 1% to 3% antistatic masterbatch and 97% to 99% homopolymer polypropylene; The antistatic masterbatch comprises the following raw materials by mass percentage: 70%–75% homopolymer polypropylene and 25%–30% antistatic agent; the antistatic agent is composed of glyceryl stearate and oleamide in a mass ratio of 1:(1–3).
[0013] A method for preparing a sustained-release antifogging agent includes the following steps: The porous inorganic carrier was placed in a vacuum oven and activated at 120°C to remove adsorbed water. The activated porous inorganic support is dispersed in an ethanol solution, a nonionic surfactant is added, and the reaction is carried out by heating and stirring, so that the nonionic surfactant molecules are anchored inside the pores and on the surface of the porous inorganic support. The reaction product was washed, filtered and dried to obtain a powdered slow-release antifogging agent; Furthermore, the porous inorganic support is mesoporous silica, molecular sieve, or diatomaceous earth; The nonionic surfactant comprises the following raw materials by weight percentage: 50% sorbitan monostearate and 50% polyglycerol fatty acid.
[0014] The above-mentioned method for preparing the anti-fog film includes: The raw materials for the lower surface layer, core layer, and upper surface layer are fed into an extruder and combined at the die head to form a thick sheet. After longitudinal stretching, transverse stretching, shaping and cooling, corona treatment, and slitting, an anti-fog film is obtained.
[0015] The beneficial effects of this invention are: 1. The invention uses the nanopores of porous materials to confine surfactants, preventing them from volatilizing or decomposing prematurely during processing. During use, the surfactants are slowly released by changes in humidity, resulting in a slow-release composite anti-fogging agent. This not only prolongs the anti-fogging performance but also effectively reduces the concentration of single-molecule free surfactants, thereby reducing odor. In addition, the silica carrier has an opening effect.
[0016] 2. This invention utilizes a suitable adsorbent-type odor inhibitor as an organically surface-modified nanoporous mineral material. This not only improves its compatibility with organic matter, such as at least one of nano-hydrotalcite, organomontmorillonite, or β-cyclodextrin derivatives, but also captures free small molecules (such as unreacted antifogging agent monomers, oligomers, or oxidation products) remaining in the molten state and inside the film, forming stable inclusion complexes. These complexes work synergistically with the slow-release composite antifogging agent to further suppress odor. Simultaneously, the modified adsorbent improves its compatibility with the surface PP layer.
[0017] 3. The anti-adhesion particles used in this invention are irregularly shaped large particles, which provide good opening properties for the heat-sealing layer after corona treatment. Detailed Implementation
[0018] The technical solution of the present invention will be clearly and completely described below with reference to the embodiments of the present invention. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0019] A low-odor, long-lasting anti-fog film comprises, from bottom to top: a lower surface layer, a core layer, and an upper surface layer; The bottom layer is a heat-sealing layer, which includes the following raw materials by weight percentage: 1% to 3% anti-sticking masterbatch and 97% to 99% ternary copolymer polypropylene; The core layer comprises the following raw materials by weight percentage: 1%–3% antistatic masterbatch and 97%–99% homopolymer polypropylene. The upper surface layer is a low-odor anti-fog layer, which includes the following raw materials by weight percentage: 5% to 10% slow-release anti-fog masterbatch, 0.2% to 0.6% odor absorbent, and 89.4% to 94.8% binary copolymer polypropylene.
[0020] The anti-sticking masterbatch comprises the following raw materials in the following mass percentages: 96%–98% homopolymer polypropylene and 2%–4% anti-sticking agent. The anti-sticking agent is irregularly shaped silica with a particle size of 3–5 μm. The preparation process of the anti-sticking masterbatch is as follows: silica and homopolymer polypropylene are thoroughly mixed and then extruded through the feeding section, melting section, homogenization section, and extrusion section of a twin-screw extruder. The extruder production temperature is controlled at 230–260°C. After extrusion, the melt is dried, cooled, and pelletized to obtain the finished anti-sticking masterbatch.
[0021] The antistatic masterbatch comprises the following raw materials by mass percentage: 70%–75% homopolymer polypropylene and 25%–30% antistatic agent; the antistatic agent is composed of glyceryl stearate and oleamide in a mass ratio of 1:(1–3); the preparation process of the antistatic masterbatch is as follows: the antistatic agent and homopolymer polypropylene are thoroughly mixed and then extruded through the feeding section, melting section, homogenization section and extrusion section of a twin-screw extruder. The extruder production temperature is controlled at 230–260°C. After extrusion, the melt is dried, cooled and pelletized to obtain the finished antistatic masterbatch.
[0022] The slow-release anti-fogging masterbatch comprises the following raw materials by mass percentage: 30% to 35% slow-release anti-fogging agent and 65% to 70% homopolymer polypropylene; the slow-release anti-fogging agent and homopolymer polypropylene are fed into an extruder for granulation in proportion, and the extruded plastic is sliced to obtain the slow-release anti-fogging masterbatch.
[0023] The preparation process of the sustained-release antifogging agent includes: placing a porous inorganic carrier (such as mesoporous silica, molecular sieve or diatomaceous earth, with a particle size D90 ≤ 2μm) in a vacuum oven and activating it at 120℃ for 2 hours to remove adsorbed water; dispersing the activated porous carrier in an ethanol solution, adding a nonionic surfactant (50wt% sorbitan monostearate and 50wt% polyglycerol fatty acid), and performing ultrasonic treatment to anchor the surfactant molecules to the pores and surface of the carrier through strong physical adsorption; after ultrasonic treatment, the product is washed, filtered, and dried to obtain a powdered sustained-release antifogging agent.
[0024] The odor adsorbent is an organically surface-modified nanoporous mineral material, such as at least one of nano-hydrotalcite, organically modified montmorillonite, or β-cyclodextrin derivatives.
[0025] The ternary copolymer polypropylene is copolymerized from ethylene, propylene, and 1-butene; the binary copolymer polypropylene is copolymerized from ethylene and propylene.
[0026] The thickness of the lower surface layer is 1~2μm, the thickness of the core layer is 21~23μm, and the thickness of the upper surface layer is 1~2μm.
[0027] The preparation process of the above-mentioned low-odor, long-lasting anti-fog film includes: The raw materials for the lower surface layer, core layer, and upper surface layer are fed into the corresponding extruders in the appropriate proportions, and then converged at the die head to form a thick sheet. After longitudinal stretching, transverse stretching, shaping and cooling, corona treatment, and aging and slitting, a low-odor, low-long-lasting anti-fog film is obtained.
[0028] The technical solution of the present invention will be specifically described below through the following embodiments and comparative examples (unless otherwise stated, all percentages used in the embodiments and comparative examples are mass percentages), wherein the sources of the relevant raw materials are as follows: Homopolymer polypropylene: Grade T36F (Zhongjing Petrochemical); Ternary copolymer polypropylene: Grade KS359 (INEOS); Binary copolymer polypropylene: Grade TF1007 (Dushanzi Petrochemical); Organic modified montmorillonite: Grade XFI45 (Jiangsu Xianfeng Nano); Sorbitan monostearate: Grade SPAN60 (Shanghai Maclean Biochemical Technology Co., Ltd.); Polyglycerol fatty acids: CAS: 67784-82-1; Glyceryl stearate: CAS: 129-94-4; Oleamide: CAS: 301-02-0.
[0029] Example 1 A low-odor, low-long-lasting anti-fog film is composed of a lower surface layer, a core layer, and an upper surface layer, wherein the lower surface layer is a heat-sealing layer and the upper surface layer is a low-odor layer. The heat-sealing layer comprises the following raw materials in weight percentages: 1.5% anti-stick masterbatch and 98.5% copolymer polypropylene; The anti-sticking masterbatch comprises the following raw materials in the following weight percentages: 98% homopolymer polypropylene and 2% anti-sticking agent; the anti-sticking agent is irregular silica with a particle size of 5μm. The core layer comprises the following raw materials: 98% homopolymer polypropylene and 2% antistatic masterbatch; The antistatic masterbatch comprises the following raw materials in the following mass percentages: 70% homopolymer polypropylene and 30% antistatic agent; the antistatic agent is a compound of glyceryl stearate and oleamide in a mass ratio of 1:1.5. The upper layer is a low-odor anti-fog layer, comprising the following raw materials: 10% slow-release anti-fog masterbatch, 0.6% odor absorbent masterbatch, and 89.4% copolymer polypropylene; The odor adsorbent is organically modified montmorillonite; The heat-sealing layer has a thickness of 1 μm; the core layer has a thickness of 22 μm; the low-odor anti-fog layer has a thickness of 2 μm; and the low-odor long-lasting anti-fog film has a thickness of 25 μm. The preparation method of the low-odor, long-lasting anti-fog film includes the following steps; S1, Preparation of slow-release anti-fogging masterbatch 100 parts of porous silica (particle size D90 ≤ 2μm) were placed in a vacuum oven and activated at 120℃ for 2 hours to remove adsorbed water. The activated porous silica was dispersed in 200 parts of ethanol solution, and a nonionic surfactant (50wt% sorbitan monostearate and 50wt% polyglycerol fatty acid) was added. The mixture was then ultrasonically treated to anchor the surfactant molecules to the pores and surface of the carrier through hydrogen bonding and strong physical adsorption. After the ultrasonic reaction, the mixture was filtered, washed three times with ethanol, vacuum dried at 80℃ for 12 hours, and ground through a 400-mesh sieve to obtain a slow-release anti-fogging agent. 30 parts of the slow-release anti-fogging agent and 70 parts of homopolymer polypropylene were fed into an extruder for granulation. The extruded plastic was sliced to obtain a slow-release anti-fogging masterbatch.
[0030] S2, each layer is added to the extruder in the corresponding proportion for melting and plasticizing. The heating and melting temperature of the lower surface layer is 230-240℃, the heating and melting temperature of the core layer is 250-260℃, and the heating and melting temperature of the upper surface layer is 230-240℃. They are joined at the die head to form a thick sheet. After longitudinal stretching, transverse stretching, shaping and cooling, corona treatment, and aging and slitting, a low-odor, low-efficiency anti-fog film is obtained.
[0031] Example 2 A low-odor, low-long-lasting anti-fog film is composed of a lower surface layer, a core layer, and an upper surface layer, wherein the lower surface layer is a heat-sealing layer and the upper surface layer is a low-odor layer. The heat-sealing layer comprises the following raw materials in weight percentages: 1.5% anti-stick masterbatch and 98.5% copolymer polypropylene; The anti-sticking masterbatch comprises the following raw materials in the following weight percentages: 98.5% homopolymer polypropylene and 1.5% anti-sticking agent; the anti-sticking agent is random silica with a particle size of 5μm; The heat-sealing layer thickness is 1.5 μm; The core layer comprises the following raw materials: 98% homopolymer polypropylene and 2% antistatic masterbatch; The antistatic masterbatch comprises the following raw materials in the following mass percentages: 70% homopolymer polypropylene and 30% antistatic agent; the antistatic agent is a compound of glyceryl stearate and oleamide in a mass ratio of 1:1.5.
[0032] The core layer thickness is 21.5 μm; The upper layer is a low-odor anti-fog layer, comprising the following raw materials: 10% composite anti-fog masterbatch, 0.6% odor absorbent masterbatch, and 89.4% copolymer polypropylene; The odor adsorbent is organically modified montmorillonite; The low-odor anti-fog layer is 2μm thick; The thickness of the low-odor, long-lasting anti-fog film is 25 μm; The preparation method of the low-odor, long-lasting anti-fog film includes the following steps; S1, Preparation of slow-release anti-fogging masterbatch 100 parts of porous silica (particle size D90 ≤ 4μm) were placed in a vacuum oven and activated at 120℃ for 2 hours to remove adsorbed water. The activated porous silica was dispersed in 200 parts of ethanol solution, and a nonionic surfactant (50% sorbitan monostearate and 50% polyglycerol fatty acid) was added. The mixture was then ultrasonically treated to anchor the surfactant molecules to the pores and surface of the carrier through hydrogen bonding and strong physical adsorption. After the ultrasonic reaction, the mixture was filtered, washed three times with ethanol, vacuum dried at 80℃ for 12 hours, and ground through a 400-mesh sieve to obtain a slow-release anti-fogging agent. 30 parts of the slow-release anti-fogging agent and 70 parts of homopolymer polypropylene were fed into an extruder for granulation. The extruded plastic was sliced to obtain a slow-release anti-fogging masterbatch.
[0033] S2, each layer is added to the extruder in the corresponding proportion for melting and plasticizing. The heating and melting temperature of the lower surface layer is 230-240℃, the heating and melting temperature of the core layer is 250-260℃, and the heating and melting temperature of the upper surface layer is 230-240℃. They are joined at the die head to form a thick sheet. After longitudinal stretching, transverse stretching, shaping and cooling, corona treatment, and aging and slitting, a low-odor, low-efficiency anti-fog film is obtained.
[0034] Comparative Example 1 A typical anti-fog film consists of a lower surface layer, a core layer, and an upper surface layer, wherein the lower surface layer is a heat-sealing layer and the upper surface layer is an anti-fog layer. The heat-sealing layer comprises the following raw materials in weight percentages: 1.5% anti-stick masterbatch and 98.5% copolymer polypropylene; The anti-sticking masterbatch comprises the following raw materials in the following weight percentages: 98.5% homopolymer polypropylene and 1.5% anti-sticking agent; the anti-sticking agent is irregular silica with a particle size of 5 μm. The heat-sealing layer thickness is 1.5 μm; The core layer comprises the following raw materials: 98% homopolymer polypropylene and 2% antistatic masterbatch; The antistatic masterbatch comprises the following raw materials in the following mass percentages: 70% homopolymer polypropylene and 30% antistatic agent; the antistatic agent is a compound of glyceryl stearate and oleamide in a mass ratio of 1:1.5.
[0035] The core layer thickness is 21.5 μm; The upper layer is an anti-fog layer, comprising the following raw materials: 10% ordinary anti-fog masterbatch and 90% copolymer polypropylene; The anti-fog layer is 2μm thick; Each layer is added to an extruder in the appropriate proportion for melting and plasticizing. The heating and melting temperature of the lower surface layer is 230-240℃, the heating and melting temperature of the core layer is 250-260℃, and the heating and melting temperature of the upper surface layer is 230-240℃. The layers are then joined at the die head to form a thick sheet. After longitudinal stretching, transverse stretching, shaping and cooling, corona treatment, and aging and slitting, a low-odor, low-efficiency, long-lasting anti-fog film is obtained.
[0036] Comparative Example 2 A low-odor, low-long-lasting anti-fog film is composed of a lower surface layer, a core layer, and an upper surface layer, wherein the lower surface layer is a heat-sealing layer and the upper surface layer is a low-odor layer. The heat-sealing layer comprises the following raw materials in weight percentages: 1.5% anti-stick masterbatch and 98.5% copolymer polypropylene; The anti-sticking masterbatch comprises the following raw materials in the following weight percentages: 98% homopolymer polypropylene and 2% anti-sticking agent; the anti-sticking agent is random silica with a particle size of 5μm; The heat seal layer thickness is 1μm; The core layer comprises the following raw materials: 98% homopolymer polypropylene and 2% antistatic masterbatch; The antistatic masterbatch comprises the following raw materials in the indicated weight percentages: 70% homopolymer polypropylene and 30% antistatic agent; the antistatic agent is a mixture of glyceryl stearate and oleamide in a weight ratio of 1:1.5. The core layer thickness is 22 μm; The upper layer is a low-odor anti-fog layer, comprising the following raw materials: 10% composite anti-fog masterbatch and 90% copolymer polypropylene; The low-odor anti-fog layer is 2μm thick; The thickness of the low-odor, long-lasting anti-fog film is 2 μm; The preparation method of the low-odor, long-lasting anti-fog film includes the following steps; Preparation of slow-release anti-fogging masterbatch: 100 parts of porous silica (particle size D90 ≤ 4μm) were placed in a vacuum oven and activated at 120℃ for 2 hours to remove adsorbed water. The activated porous silica was dispersed in 200 parts of ethanol solution, and a nonionic surfactant (50% sorbitan monostearate and 50% polyglycerol fatty acid) was added. The mixture was then ultrasonically treated to anchor the surfactant molecules to the pores and surface of the carrier through hydrogen bonding and strong physical adsorption. After the ultrasonic reaction, the mixture was filtered, washed three times with ethanol, vacuum dried at 80℃ for 12 hours, and ground through a 400-mesh sieve to obtain a slow-release anti-fogging agent. 30 parts of the slow-release anti-fogging agent and 70 parts of homopolymer polypropylene were fed into an extruder for granulation. The extruded plastic was sliced to obtain the slow-release anti-fogging masterbatch.
[0037] Each layer is added to an extruder in the appropriate proportion for melting and plasticizing. The heating and melting temperature of the lower surface layer is 230-240℃, the heating and melting temperature of the core layer is 250-260℃, and the heating and melting temperature of the upper surface layer is 230-240℃. The layers are then joined at the die head to form a thick sheet. After longitudinal stretching, transverse stretching, shaping and cooling, corona treatment, and aging and slitting, a low-odor, low-efficiency, long-lasting anti-fog film is obtained.
[0038] Comparative Example 3 The difference between this comparative example and Example 1 is that the anti-fog layer uses "anti-fog masterbatch without porous silica treatment + odor adsorbent", while the other raw materials and preparation methods are exactly the same as in Example 1.
[0039] Comparative Example 4 The difference between this comparative example and Example 1 is that the odor adsorbent in the anti-fog layer is replaced with ordinary natural montmorillonite, while the other raw materials and preparation methods are exactly the same as in Example 1.
[0040] Experimental Test The thin films prepared in Examples 1-2 and Comparative Examples 1-4 were subjected to performance tests. The test items and procedures are as follows: 1. Anti-fogging performance test; conducted according to GB / T 31726 Rapid Thermal Fogging Method. 2. Heat seal strength test; tested according to GB / T 10003. 3. Haze test; conducted in accordance with GB / T 2410. 4. Odor Test: Sensory olfaction methods commonly use a 0-6 rating scale, where 0 represents no odor and 6 represents an unbearably strong odor. Table 1. Performance test results of the products from the examples and comparative examples. As shown in Table 1, the odor level is 0 after adding odor adsorbent and slow-release anti-fogging agent, and the anti-fogging level is still 1 after 30 days. By adding slow-release anti-fogging masterbatch and gas adsorbent in combination, not only can the anti-fogging level be extended, but the odor of the film can also be reduced.
[0041] Based on the data in Table 1, the analysis is as follows: 1) By comparing the data of Comparative Example 1 and Examples 1-2, it can be seen that the anti-fogging level of ordinary anti-fogging material decreased significantly after aging, and the odor was stronger; thus, it can be seen that the anti-fogging performance of the slow-release anti-fogging agent is durable, and the odor adsorbent plays a role in suppressing odor. 2) By comparing the data of Comparative Example 2 and Examples 1-2, it can be seen that although the anti-fogging level is good when using slow-release anti-fogging agent alone, the odor still exists. This shows that an odor adsorbent is still needed for synergistic effect.
[0042] 3) By comparing the data of Comparative Example 3 and Examples 1-2, it can be seen that: using only ordinary surfactants without porous silica carriers still produces a noticeable odor; thus, it is shown that porous silica carriers have a physical adsorption effect on surfactants, which helps them to be released slowly and reduce odor.
[0043] 4) Comparison of the data from Comparative Example 4 and Examples 1-2 shows that using unmodified montmorillonite as an odor adsorbent significantly improves haze. This indicates that adding organically surface-modified montmorillonite has good compatibility with polypropylene and is beneficial to film haze.
[0044] In the description of this specification, references to terms such as "an embodiment," "example," "specific example," etc., indicate that a specific feature, structure, material, or characteristic described in connection with that embodiment or example is included in at least one embodiment or example of the invention. In this specification, illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more embodiments or examples.
[0045] The foregoing has shown and described the basic principles, main features, and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The embodiments and descriptions in the specification are merely illustrative of the principles of the invention. Various changes and modifications can be made to the invention without departing from its spirit and scope, and all such changes and modifications fall within the scope of the claimed invention.
Claims
1. An anti-fog film, characterized by, From bottom to top, it includes: lower surface layer, core layer, and upper surface layer; The upper surface layer comprises the following raw materials by weight percentage: 5%–10% slow-release anti-fog masterbatch, 0.2%–0.6% odor absorber, and 89.4%–94.8% binary copolymer polypropylene; The raw materials for the slow-release anti-fogging masterbatch include: a slow-release anti-fogging agent and homopolymer polypropylene; the slow-release anti-fogging agent is a composite particle formed by a nonionic surfactant being physically adsorbed and anchored inside the pores and on the surface of a porous inorganic carrier.
2. The anti-fog film according to claim 1, wherein The porous inorganic carrier is mesoporous silica, molecular sieve, or diatomaceous earth.
3. The anti-fog film according to claim 1, wherein The nonionic surfactant comprises the following raw materials by weight percentage: 50% sorbitan monostearate and 50% polyglycerol fatty acid.
4. The anti-fog film according to claim 1, wherein The slow-release anti-fogging masterbatch comprises the following raw materials by weight percentage: 30% to 35% slow-release anti-fogging agent and 65% to 70% homopolymer polypropylene.
5. The anti-fog film according to claim 1, wherein The odor adsorbent is an organically surface-modified nanoporous mineral material.
6. The anti-fog film according to claim 1, wherein The lower surface layer is a heat-sealing layer, which comprises the following raw materials by mass percentage: 1% to 3% anti-sticking masterbatch and 97% to 99% ternary copolymer polypropylene; The anti-adhesion masterbatch comprises the following raw materials in weight percentages: 96%–98% homopolymer polypropylene and 2%–4% anti-adhesion agent. The anti-adhesion agent is irregularly shaped silica with a particle size of 3–5 μm.
7. The anti-fog film according to claim 1, wherein The core layer comprises the following raw materials by weight percentage: 1% to 3% antistatic masterbatch and 97% to 99% homopolymer polypropylene; The antistatic masterbatch comprises the following raw materials by mass percentage: 70%–75% homopolymer polypropylene and 25%–30% antistatic agent; the antistatic agent is composed of glyceryl stearate and oleamide in a mass ratio of 1:(1–3).
8. A method for producing a slow-release antifogging agent, characterized by, Includes the following steps: The porous inorganic carrier was placed in a vacuum oven and activated at 120°C to remove adsorbed water. The activated porous inorganic support is dispersed in an ethanol solution, a nonionic surfactant is added, and the reaction is carried out by heating and stirring, so that the nonionic surfactant molecules are anchored inside the pores and on the surface of the porous inorganic support. The reaction product was washed, filtered, and dried to obtain a powdered slow-release anti-fogging agent.
9. The method for preparing a sustained-release antifogging agent according to claim 8, characterized in that, The porous inorganic support is mesoporous silica, molecular sieve, or diatomaceous earth. The nonionic surfactant comprises the following raw materials by weight percentage: 50% sorbitan monostearate and 50% polyglycerol fatty acid.
10. The method of producing an anti-fog film according to any one of claims 1 to 7, characterized in that, include: The raw materials for the lower surface layer, core layer, and upper surface layer are fed into an extruder and converge at the die head to form a thick sheet. After longitudinal stretching, transverse stretching, shaping and cooling, corona treatment, and slitting, an anti-fog film is obtained.