Dry drilling surface-mounted impregnated diamond drill bits for geological exploration and their manufacturing method
By using a dry drilling surface-mounted impregnated diamond drill bit with an inner conical lip and a spiral outer diameter design, combined with a special graphite mold and integrated sintering technology, the problems of poor rock powder removal, core contamination and rapid wear during dry drilling are solved. This achieves high-efficiency cutting and long-life drill bit performance, making it suitable for exploration in complex formations.
Patent Information
- Application Number
- CN202611498493.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-24
- Publication Date
- 2026-11-17
AI Technical Summary
Existing dry-drilling diamond drill bits suffer from problems such as poor rock powder removal, core contamination, rapid wear, and poor forming accuracy, making it difficult to meet the high-efficiency exploration needs of complex dry-drilling formations.
The dry-drilling surface-mounted and impregnated diamond drill bit, designed with an inner conical lip and a spiral outer diameter, combined with a special graphite mold, ensures the precision and performance of the drill bit structure. The matrix and steel body are bonded through integrated sintering, and the surface-mounted and impregnated composite matrix structure is designed to improve cutting efficiency and service life.
It effectively reduces rock dust discharge, improves dust removal efficiency, reduces core contamination, extends drill bit life, meets the needs of efficient exploration in complex formations, and is suitable for large-scale production.
Smart Images

Figure CN123109550A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of geological exploration drilling tools, and in particular to a dry drilling surface-mounted impregnated diamond drill bit for geological exploration and its manufacturing method. It is suitable for geological core exploration under dry drilling conditions such as no water or water shortage, and can solve technical problems such as rock powder accumulation, poor powder removal, excessive drill bit wear, and core contamination during dry drilling, thereby improving the efficiency of dry drilling core extraction and the service life of the drill bit. Background Technology
[0002] Dry drilling, as an important drilling method in geological exploration, is widely used in water-scarce areas, strata with low groundwater levels, strata prone to hydration and disintegration, and exploration scenarios with high requirements for water resource protection. Currently, diamond drill bits for dry drilling are mainly divided into two types: surface-mounted and impregnated. Surface-mounted drill bits have high cutting efficiency, while impregnated drill bits have a long service life. However, existing dry drilling diamond drill bits generally suffer from the following technical defects, making them difficult to adapt to the needs of high-efficiency dry drilling: 1. Drill bit lips often adopt a planar or external conical structure. During dry drilling, rock powder generated during cutting is easily scattered and discharged from the outside of the lip. On the one hand, this causes the rock powder to be unable to be discharged from the bottom of the hole in time, accumulating between the drill bit and the hole wall, increasing drilling resistance, aggravating drill bit wear, and even causing the drill to get stuck. On the other hand, the discharged rock powder is easy to mix into the core sampling channel, contaminate the core, and affect the accuracy of geological exploration data.
[0003] 2. The outer diameter and steel body of the drill bit are mostly smooth cylindrical structures without a dedicated powder removal structure. In dry drilling conditions, there is no drilling fluid to assist in powder removal. The powder removal relies solely on the centrifugal force generated by the rotation of the drill bit, resulting in extremely low powder removal efficiency. Long-term accumulation of rock powder at the bottom of the hole can lead to overheating of the drill bit lip and diamond particle shedding, severely shortening the service life of the drill bit.
[0004] 3. Existing dry drilling bits mostly adopt a single surface-mounted or single impregnated structure, which makes it difficult to balance cutting efficiency and service life: single surface-mounted drill bits are prone to diamond particle loss and are suitable for soft to medium-hard formations; single impregnated drill bits have low cutting efficiency and are suitable for hard rock formations, but cannot meet the exploration needs of complex dry drilling formations.
[0005] 4. Graphite molds, as the core tooling for drill bit sintering, must perfectly match the overall structure, lip structure, and helical structure of the drill bit to ensure its forming accuracy and performance. However, most existing graphite molds are conventional structures adapted to smooth cylindrical drill bits, and cannot adapt to the structural designs of internal conical lips and helical outer diameters / steel bodies. This results in poor drill bit forming accuracy and large structural dimensional deviations, further affecting the drill bit's powder removal performance and drilling stability.
[0006] Therefore, there is an urgent need to design a dry drilling surface-mounted diamond drill bit with a reasonable overall structure, high powder removal efficiency, low rock powder discharge, and a balance between cutting efficiency and service life, and equipped with a graphite mold. At the same time, corresponding manufacturing methods should be provided to solve the technical defects of existing dry drilling bits and meet the high-efficiency and precise requirements of dry drilling in geological exploration. Summary of the Invention
[0007] To address the aforementioned technical problems, this invention provides a dry drilling surface-mounted impregnated diamond drill bit for geological exploration and its manufacturing method. This solves issues such as excessive rock powder discharge, poor powder removal, core contamination, rapid drill bit wear, and poor forming accuracy under dry drilling conditions. By optimizing the overall drill bit structure, adopting an internal conical lip design, a spiral outer diameter, and a steel body design, and using a graphite mold perfectly compatible with the drill bit structure, it achieves less rock powder discharge and efficient powder removal, balancing cutting efficiency and service life while ensuring drill bit forming accuracy, thus adapting to the needs of complex dry drilling geological exploration.
[0008] To achieve this technical objective, the present invention adopts the following solution: In a first aspect, the present invention provides a dry drilling bit for geological exploration with surface-mounted and impregnated diamond, comprising a steel body, a surface-mounted and impregnated composite matrix, and a core-taking channel. The steel body, the surface-mounted and impregnated composite matrix, and the core-taking channel are arranged coaxially. The surface-mounted and impregnated composite matrix is fixedly disposed at the lower end of the steel body, forming an integrated structure with the steel body. The lower end of the surface-mounted and impregnated composite matrix is provided with an inner conical lip, which is a conical structure inclined towards the axis of the drill bit. The outer diameter of the steel body and the outer diameter of the surface-mounted and impregnated composite matrix are both provided with an integrated helical structure, forming an integrated helical outer diameter. The surface-mounted and impregnated composite matrix adopts a structure combining surface-mounting and impregnation. The surface of the matrix lip is provided with surface-mounted diamond particles, and the interior of the matrix is provided with impregnated diamond particles.
[0009] Furthermore, the angle between the inner conical lip and the drill bit axis is 15°~30°, the width of the conical surface is 8~15mm, and the edge of the lip is provided with a rounded transition with a radius of 1~2mm.
[0010] Furthermore, the spiral structure consists of continuous spiral protrusions with a pitch of 10-25 mm and a height of 2-5 mm. The spiral direction is consistent with the rotation direction of the drill bit during drilling. The cross-section of the spiral protrusion is trapezoidal, with an upper base width of 3-5 mm and a lower base width of 5-8 mm.
[0011] Furthermore, the diamond particles used in the surface setting are high-grade synthetic diamonds with a particle size of 20-40 mesh and a content of 5.2-6.6 carats / cm². 3 The setting depth is 1 / 3 to 1 / 2 of the diamond particle size; the impregnated diamond particles are a mixture of natural diamonds and synthetic diamonds, with a particle size of 40 to 80 mesh and a volume concentration of 80 to 100%.
[0012] The high-grade synthetic diamonds used are domestic D90 grade diamonds, with a high-temperature single-particle net pressure greater than 100N / particle.
[0013] Furthermore, the surface-mounted and impregnated composite matrix is composed of diamond particles, cemented carbide powder, binder, and sintering aid; wherein, the diamond particles include surface-mounted diamond particles and impregnated diamond particles, and the volume concentration of diamond particles is 70% to 100%; the cemented carbide powder includes WC powder, Mo2C powder, and TiC powder, accounting for 60% to 80% of the matrix powder mass; the binder is a Co-Ni-Fe binder, accounting for 5% to 15% of the matrix powder mass; and the sintering aid is a TiH2 sintering aid, accounting for 2 to 4% of the matrix powder mass.
[0014] Furthermore, a threaded joint is provided at the upper end of the steel body, and the central axis of the threaded joint coincides with the central axis of the steel body; an annular boss is provided at the lower end of the steel body, and the annular boss is wrapped around the surface-mounted and inlaid composite matrix during sintering to achieve the connection between the steel body and the surface-mounted and inlaid composite matrix.
[0015] Secondly, the present invention provides a method for preparing the aforementioned dry drilling surface-mounted impregnated diamond drill bit for geological exploration, comprising the following steps: S1. Steel body processing: Process the steel body, and process the outer diameter of the steel body into a spiral structure; process an annular boss at the lower end of the steel body and a threaded joint at the upper end; perform rust removal, degreasing and sandblasting treatment on the surface of the steel body; S2. Preparation of surface-mounted and impregnated composite matrix powder: Weigh the surface-mounted diamond particles, impregnated diamond particles, WC powder, Mo2C powder, TiC powder, Co-Ni-Fe binder and TiH2 sintering aid according to the formula to prepare the impregnated matrix mixed powder; the surface-mounted diamond particles are subjected to surface coating treatment to improve their adhesion. The coating treatment adopts existing technology, such as spray coating method; S3. Graphite mold preparation: Based on the overall structure of the drill bit, the inner conical lip structure, and the outer diameter structure of the spiral structure, design and prepare the graphite mold. The cavity of the graphite mold is completely matched with the overall shape of the drill bit. The lower end of the cavity is provided with an inner conical forming surface that matches the inner conical lip. The inner wall of the cavity is provided with a spiral groove that matches the outer diameter of the spiral. The upper part of the cavity is provided with a positioning groove that matches the steel body. The center of the cavity is provided with a mold core that matches the core extraction channel. S4. Mold installation: Place the processed steel body into the positioning groove of the graphite mold, fill it with the mixed powder of the matrix and compact it, embed the surface-mounted diamond particles on the surface of the matrix powder, and place the graphite block. S5. Sintering and forming: The graphite mold is placed in a hot press sintering furnace and sintered under a vacuum protective atmosphere using a segmented temperature control and gradient pressure sintering process to achieve the integrated bonding of the surface-mounted and impregnated composite matrix with the steel body. S6. Post-processing: After sintering, the furnace is cooled, the mold and graphite block are removed to obtain the drill bit blank; the drill bit blank is ground and polished, and the finished drill bit is obtained after passing the inspection.
[0016] Furthermore, in step S3, the graphite mold is made of high-density graphite with a hardness of HV160-200; the angle between the inner conical forming surface and the inner conical lip surface is consistent, and the surface roughness is ≤Ra0.8μm; the pitch, height, and cross-sectional dimensions of the spiral groove are completely matched with those of the spiral structure, and the surface roughness is ≤Ra1.0μm.
[0017] Furthermore, in step S5, the vacuum degree is ≤10. -3 Pa; sintering parameters are: heating rate 6~10℃ / min, hold at 750~850℃ for 30~45min, continue heating to 1150~1250℃, apply pressure of 18~28MPa, hold for 70~100min.
[0018] Furthermore, in step S6, the test indicators include: inner conical lip angle deviation ≤ ±0.5°, spiral structure pitch deviation ≤ ±0.2mm, spiral protrusion height deviation ≤ ±0.1mm, bonding strength between the carcass and the steel body ≥ 220MPa, carcass hardness ≥ HV1900, and surface-set diamond particle loss rate ≤ 1%.
[0019] Compared with the prior art, the beneficial effects of the present invention are as follows: (1) The present invention focuses on optimizing the overall structure of the drill bit. One of the core innovations is the use of an inner conical structure design for the lip surface: the inner conical lip surface is an inwardly inclined cone shape, which can greatly reduce the probability of rock powder being discharged, guide the rock powder generated by cutting to converge in the powder discharge area, avoid the accumulation at the bottom of the hole and the aggravation of drill bit wear caused by the discharge of rock powder, and at the same time reduce the mixing of rock powder into the core sampling channel, effectively reduce core pollution, and improve the accuracy of geological exploration data.
[0020] (2) The outer diameter of the drill bit and the steel body adopt an integrated spiral structure design, which is another core innovation of this invention: the spiral structure is consistent with the rotation direction of the drill bit. During dry drilling, the rock powder accumulated at the bottom of the hole can be quickly discharged upward through the guiding effect of the spiral structure. This can quickly discharge the rock powder accumulated at the bottom of the hole, fundamentally improve the problems of poor discharge of rock powder at the bottom of the hole, repeated grinding of rock powder, and excessive wear of the drill bit under dry drilling conditions, and greatly improve the stability of dry drilling.
[0021] (3) The surface-mounted and impregnated composite matrix structure is adopted. The surface-mounted diamond particles on the lip surface improve cutting efficiency, while the impregnated diamond particles inside the matrix improve wear resistance and service life. It takes into account both the high-efficiency cutting and long-term use requirements under dry drilling conditions, and is suitable for complex dry drilling formations such as soft to hard rocks, thus expanding the application range of the drill bit.
[0022] (4) A graphite mold is designed for the overall structure of the drill bit, the inner conical lip surface and the outer diameter of the spiral. The mold cavity is fully adapted to the structure of the drill bit, which is the key to the precise forming of the drill bit in this invention: the inner conical forming surface and the spiral groove of the graphite mold can ensure the accurate angle of the inner conical lip surface and the standard size of the spiral structure, which solves the problem that the existing mold cannot be adapted to this type of special structure drill bit and the forming accuracy is poor, thus ensuring the overall performance stability of the drill bit.
[0023] (5) The steel body and the surface-mounted composite matrix are sintered together in one piece, which avoids the problems of thermal stress and weak bonding caused by traditional welding, improves the overall strength of the drill bit, and reduces the risk of matrix falling off and cracking during dry drilling; at the same time, the manufacturing process is simple, suitable for large-scale production, and reduces production costs.
[0024] Comparison of experimental data: Multiple dry drilling comparison tests showed that conventional dry drilling bits without a spiral structure resulted in a bottom hole dust accumulation rate as high as 42%, with average dry drilling footage per bit less than 8 meters before blockage and slippage occurred. Using the spiral structure drill bit of this invention, the bottom hole dust accumulation rate was reduced to below 3.5%, eliminating bottom hole blockage and dust accumulation problems. The dry drilling footage per bit increased to over 25 meters, effectively solving the core dust removal pain point in dry drilling operations. For deep hole construction ranging from tens to hundreds of meters, this invention solves the most critical bottom hole dust accumulation problem in deep hole dry drilling. Combined with the conventional annular gap airflow dust removal method in exploration boreholes, it can stably achieve continuous deep hole dry drilling operations, with the technical effect and technical means perfectly matched. Attached Figure Description
[0025] Figure 1 This is a schematic diagram of the overall structure of a dry drilling bit with surface-mounted impregnated diamond for geological exploration, as described in an embodiment of the present invention.
[0026] Figure 2 This is an enlarged schematic diagram of the inner conical structure of the drill bit lip in an embodiment of the present invention.
[0027] Figure 3 This is a schematic diagram of the graphite mold for a dry drilling surface-mounted impregnated diamond drill bit used in geological exploration, as described in an embodiment of the present invention.
[0028] The markings in the diagram are as follows: 1. Steel body; 2. Surface-mounted and impregnated composite matrix; 3. Core extraction channel; 4. Inner conical lip; 5. Spiral structure; 6. Threaded joint; 7. Annular boss; 8. Surface-mounted diamond particles; 9. Impregnated diamond particles; 10. Graphite mold; 11. Inner conical forming surface; 12. Spiral groove; 13. Mold core; α, Angle between the inner conical lip and the drill bit axis; P, Pitch; H, Height of the spiral protrusion. Detailed Implementation
[0029] To make the objectives, technical solutions, and advantages of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the embodiments of the present invention. Obviously, the described embodiments are some embodiments of the present invention, but not all embodiments.
[0030] Unless otherwise specified, the experimental methods used in the embodiments of this invention are conventional methods. Unless otherwise specified, the materials and reagents used are commercially available.
[0031] Please see Figures 1 to 3 This invention provides a dry drilling bit for geological exploration with surface-mounted and impregnated diamond, comprising a steel body 1, a surface-mounted and impregnated composite matrix 2, and a core-taking channel 3. The steel body 1, the surface-mounted and impregnated composite matrix 2, and the core-taking channel 3 constitute the overall structure of the drill bit, and the three are arranged coaxially to ensure stability during the drilling process.
[0032] The surface-mounted and impregnated composite matrix 2 is fixedly installed at the lower end of the steel body 1, forming an integrated structure with the steel body 1. The lower end of the surface-mounted and impregnated composite matrix 2 is provided with an inner conical lip surface 4. The inner conical lip surface 4 is a conical structure inclined towards the drill bit axis. The angle between the inner conical lip surface 4 and the drill bit axis is 15°~30° (denoted as α). The width of the conical surface is 8~15mm. The edge of the lip surface is provided with a rounded transition with a radius of 1~2mm to avoid chipping of the lip surface edge. At the same time, it further guides the rock powder to gather and reduces the rock powder discharge. The design of the inner conical lip surface 4 can greatly reduce the probability of rock powder discharge and guide the rock powder to gather in the powder discharge area between the core channel 3 and the outer diameter of the drill bit, avoiding the rock powder discharge and scattering.
[0033] Both the outer diameter of the steel body 1 and the outer diameter of the surface-mounted and inlaid composite matrix 2 are equipped with an integrated spiral structure 5, forming an integrated spiral outer diameter. The spiral structure 5 is a continuous spiral protrusion with a pitch of 10~25mm (denoted as P) and a height of 2~5mm (denoted as H). The spiral direction is consistent with the rotation direction of the drill bit during drilling. The cross-section of the spiral protrusion is trapezoidal, with an upper base width of 3~5mm and a lower base width of 5~8mm, ensuring the wear resistance and powder discharge guidance of the spiral structure 5, while preventing the spiral protrusion from breaking during drilling. The spiral structure 5 extends continuously along the axial direction of the steel body 1 and the surface-mounted and inlaid composite matrix 2, and is used to guide the rock powder generated by cutting from the bottom of the hole upward through the guiding effect of the spiral appearance, achieving efficient powder discharge under dry drilling conditions.
[0034] The surface-set and impregnated diamond composite matrix 2 adopts a structure combining surface setting and impregnation. The surface of the matrix lip is set with surface-set diamond particles 8, and the interior of the matrix is set with impregnated diamond particles 9. The surface-set diamond particles 8 are used to improve cutting efficiency, and the impregnated diamond particles 9 are used to improve the wear resistance and service life of the matrix, thus achieving dual optimization of cutting efficiency and service life.
[0035] Furthermore, the surface-mounted diamond particles 8 are high-grade synthetic diamonds (using domestic D90 grade diamonds, with a single-particle net pressure greater than 100N / particle at high temperature), with a particle size of 20-40 mesh and a content of 5.2-6.6 carats / cm². 3 The diamond particles are evenly embedded on the surface of the matrix, with an embedding depth of 1 / 3 to 1 / 2 of the diamond particle diameter, to ensure the firmness of the surface-set diamond particles 8 and prevent them from falling off; the impregnated diamond particles 9 are a mixture of natural diamonds and synthetic diamonds, with a mass ratio of natural diamonds to synthetic diamonds of 2:8 to 3:7, a particle size of 40 to 80 mesh, and a volume concentration of 80 to 100%, which are evenly distributed inside the matrix and form a tight bond with the matrix powder.
[0036] Furthermore, the surface-mounted and impregnated composite matrix 2 is composed of diamond particles, cemented carbide powder, binder, and sintering aid; the diamond particles include surface-mounted diamond particles 8 and impregnated diamond particles 9, with a diamond particle volume concentration of 70% to 100%; the cemented carbide powder includes WC powder, Mo2C powder, and TiC powder, accounting for 60% to 80% of the matrix powder mass; the binder is a Co-Ni-Fe binder, accounting for 5% to 15% of the matrix powder mass; and the sintering aid is a TiH2 sintering aid, accounting for 2% to 4% of the matrix powder mass.
[0037] The upper end of the steel body 1 is provided with a threaded joint 6 for connecting with the drill rod. The central axis of the threaded joint 6 coincides with the central axis of the steel body 1. The lower end of the steel body 1 is provided with an annular boss 7. When the surface-mounted and impregnated composite matrix 2 is sintered, it wraps around the annular boss 7 to enhance the bonding strength between the matrix and the steel body 1 and prevent the matrix from falling off during the dry drilling process.
[0038] The core sampling channel 3 runs through the center of the steel body 1 and the surface-mounted and inlaid composite matrix. The lower end of the core sampling channel 3 is connected to the inner side of the inner conical lip surface 4 to protect the core and prevent it from being scratched and broken. At the same time, it reduces the amount of rock powder entering the core sampling channel and lowers the probability of core contamination.
[0039] On the other hand, the present invention provides a method for preparing the aforementioned dry drilling surface-mounted impregnated diamond drill bit for geological exploration, comprising the following steps: S1. Steel body processing: According to the drill bit specifications, process the steel body 1 with an overall structure that is compatible. The outer diameter of the steel body 1 adopts a spiral structure 5 design. The pitch, height and cross-sectional dimensions of the spiral structure meet the design requirements. Process an annular boss 7 at the lower end of the steel body 1 and a threaded joint 6 at the upper end. Perform rust removal, degreasing and sandblasting on the surface of the steel body 1 to ensure that the surface of the steel body 1 is free of oil and rust and meets the roughness standard, thereby improving the bonding performance with the matrix.
[0040] S2. Preparation of surface-mounted and impregnated composite matrix powder: Weigh the surface-mounted diamond particles 8, impregnated diamond particles 9, WC powder, Mo2C powder, TiC powder, Co-Ni-Fe binder and TiH2 sintering aid according to the formula and put them into a mixer. Add an appropriate amount of alcohol as a dispersant, mix evenly, dry and pass through an 80-100 mesh sieve to prepare the impregnated matrix mixed powder. The surface-mounted diamond particles 8 are subjected to surface coating treatment to improve their adhesion. The coating treatment adopts existing technology, such as spray coating method. S3. Graphite mold preparation: Based on the overall structure of the drill bit, the structure of the inner conical lip 4, and the outer diameter structure of the spiral structure 5, a graphite mold 10 is designed and prepared. The cavity of the graphite mold 10 is perfectly matched with the overall shape of the drill bit. Specifically, it includes: an inner conical forming surface 11 adapted to the inner conical lip 4 is provided at the lower end of the cavity; a spiral groove 12 adapted to the outer diameter of the spiral is provided on the inner wall of the cavity; a positioning groove adapted to the steel body 1 is provided at the upper part of the cavity; and a mold core 13 adapted to the core extraction channel 3 is provided at the center of the cavity. Furthermore, the graphite mold 10 is made of high-density graphite with a hardness of HV160-200, ensuring high molding precision and resistance to deformation at high temperatures. This ensures the molding precision of the overall drill bit structure, the inner conical lip 4, and the spiral structure 5. The angle between the inner conical molding surface 11 and the inner conical lip 4 is consistent, and the surface roughness is ≤Ra0.8μm. The spiral groove 12 is perfectly matched with the pitch, height, and cross-sectional dimensions of the spiral structure 5, and the surface roughness is ≤Ra1.0μm.
[0041] S4. Mold Installation: Place the prepared steel body 1 into the positioning groove of the graphite mold 10, ensuring that the spiral structure 5 of the steel body 1 precisely matches and is firmly positioned with the spiral groove 12 on the inner wall of the mold; uniformly fill the annular boss 7 at the lower end of the steel body 1 and the gap between the graphite mold 10 and the steel body 1 with the mixed powder of the impregnated matrix; during the filling process, use vibration compaction (vibration frequency 45~55Hz, time 8~12min) to ensure that the powder is densely filled and without gaps; uniformly embed the surface-mounted diamond particles 8 at the lower surface layer of the mixed powder of the impregnated matrix according to the design density (corresponding to the position of the inner conical lip 4), ensuring that the embedding depth of the surface-mounted diamond particles 8 meets the requirements; finally, place a graphite pressure block on top of the matrix powder to ensure uniform pressure.
[0042] S5. Sintering and forming: The graphite mold 10 containing the steel body 1, matrix powder and graphite briquettes is placed into the hot pressing sintering furnace. Under the vacuum protective atmosphere, the sintering process of segmented temperature control and gradient pressure is adopted to achieve the integrated combination of the surface-mounted and inlaid composite matrix 2 and the steel body 1. The vacuum level of the protective atmosphere is ≤10. -3To prevent oxidation of the matrix powder and steel body 1 during high-temperature sintering, ensuring the mechanical properties and bonding strength of the matrix; the specific sintering parameters are: heating rate 6~10℃ / min, holding at 750~850℃ for 30~45min, continuing to heat to 1150~1250℃, applying a pressure of 18~28MPa, and holding for 70~100min. During sintering, the inner conical forming surface 11 and the spiral groove 12 of the graphite mold precisely shape the lip and outer diameter of the matrix, ensuring that the structural dimensions of the inner conical lip and the spiral outer diameter meet the design requirements.
[0043] S6. Post-processing: After sintering, the furnace is cooled, the mold and graphite block are removed to obtain the drill bit blank; the drill bit blank is ground and polished, the spiral structure 5 and the inner conical lip are repaired, the inner wall of the core extraction channel 3 is cleaned, and the finished drill bit is obtained after passing the inspection.
[0044] The testing indicators include: 4. Inner conical lip surface angle deviation ≤ ±0.5°; 5. Spiral structure pitch deviation ≤ ±0.2mm; 6. Spiral protrusion height deviation ≤ ±0.1mm; 7. Bond strength between the carcass and the steel body ≥ 220MPa; 8. Carcass hardness ≥ HV1900; 9. Diamond particle detachment rate ≤ 1%. Example 1
[0045] This embodiment provides a dry drilling bit for geological exploration with surface-mounted impregnated diamond. The bit has a diameter of 110mm and its overall structure consists of a steel body 1, a surface-mounted impregnated composite matrix 2, and a core extraction channel 3, all coaxially arranged. The outer diameters of the steel body 1 and the surface-mounted impregnated composite matrix 2 are integrated with a spiral structure 5. The spiral structure 5 has a pitch P = 20mm, a spiral protrusion height H = 3mm, and the spiral direction is consistent with the drilling rotation direction of the bit. The spiral protrusion has a trapezoidal cross-section (upper base 4mm, lower base 6mm). The surface-mounted and impregnated composite matrix 2 is fixedly installed at the lower end of the steel body 1. The lower end of the steel body 1 is provided with an annular boss 7. The surface-mounted and impregnated composite matrix 2 wraps around the annular boss 7 to achieve an integrated connection. The lower end of the surface-mounted and impregnated composite matrix 2 is provided with an inner conical lip surface 4. The angle α between the inner conical lip surface 4 and the drill bit axis is 20°. The width of the conical surface is 12mm and the radius of the rounded corner of the lip surface is 1.5mm. The lip surface of the surface-set matrices 2 features 8 high-grade synthetic diamonds (30 mesh, 5.72 carats / cm²). 3The diamond inlay depth is 1 / 2 the diameter of the diamond grain; the matrix contains 9 impregnated diamond particles (a mixture of natural and synthetic diamonds in a ratio of 2:8, 60 mesh, 90% concentration); the matrix components and their mass percentages are as follows: surface-mounted diamond particles 8%, impregnated diamond particles 10%, WC powder 60%, Mo2C powder 6%, TiC powder 4%, Co-Ni-Fe binder (of which Co 10%, Ni 6%, Fe 4%, and the balance Cu) 10%, and TiH2 sintering aid 2%; The coring channel 3 passes through the center of the steel body 1 and the surface-mounted and inlaid composite matrix 2; the upper end of the steel body 1 is provided with an API standard threaded connector 6 for connection with the drill pipe.
[0046] The above-mentioned method for manufacturing dry-drilling, surface-mounted, impregnated diamond drill bits for geological exploration includes the following steps: Steel body machining: Machining a steel body 1 with a diameter of 110mm, machining a spiral structure 5 (pitch 20mm, height 3mm, trapezoidal cross section) on the outer diameter of steel body 1; machining an annular boss 7 with a width of 12mm and a height of 6mm on the lower end of steel body 1, and machining an API standard threaded connector 6 on the upper end; rust removal by sandblasting, degreasing with industrial cleaning agent, drying and then setting aside for use, the surface roughness of steel body 1 is Ra1.6μm.
[0047] Preparation of matrix powder: Weigh each raw material according to the formula. The impregnated diamond particles 9 are mixed with WC, Mo2C, TiC, Co-Ni-Fe binder and TiH2 in a mixer in advance. Add alcohol and mix for 7 hours. Dry at 85℃ for 3.5 hours. Pass through a 100-mesh sieve to obtain the impregnated matrix mixed powder. The surface-mounted diamond particles 8 are coated with Mo2C (temperature 800℃, heat preservation for 2 hours) and set aside.
[0048] Graphite mold preparation: Design and prepare a graphite mold 10 that is compatible with the overall structure of the drill bit. The lower end of the mold cavity is provided with an inner conical forming surface 11 (angle α is 20°, surface roughness Ra0.8μm), and the inner wall of the cavity is provided with a spiral groove 12 (pitch 20mm, depth 3mm, trapezoidal cross section). The mold material is high-density graphite with a hardness of HV180.
[0049] Mold installation: Place the steel body 1 into the positioning groove of the graphite mold 10 to ensure that the spiral structure 5 of the steel body 1 and the spiral groove 12 of the graphite mold 10 are precisely matched; fill with the mixed powder of the inlaid matrix and vibrate to compact (50Hz, 10min); evenly embed the surface-mounted diamond particles 8 on the lower surface of the matrix powder and place the graphite pressing block to compact.
[0050] Sintering and shaping: Place the mold into a hot press sintering furnace and evacuate it to 10°C. -3Pa, heat to 800℃ at 8℃ / min, hold for 40min; continue heating to 1200℃, apply 25MPa pressure, hold for 85min, and complete integrated sintering.
[0051] Post-processing: Cool to room temperature in the furnace, peel off the mold and pressure block to obtain the drill bit blank; grind and polish the spiral structure 5 and the inner conical lip surface 4; inspection indicators: lip surface angle deviation ±0.3°, pitch deviation ±0.15mm, protrusion height deviation ±0.08mm, bonding strength 230MPa, matrix hardness HV1950, surface-set diamond loss rate 0.5%. If the requirements are met, it is a finished drill bit.
[0052] Multi-stratum dry drilling test data: ① Soft rock (mudstone, shale) strata: The drilling efficiency of this composite drill bit is 38% higher than that of ordinary impregnated drill bits, and on par with that of ordinary surface-mounted drill bits; ② Medium-hard rock (sandstone, limestone) strata: Drilling efficiency is increased by 25%, and service life is increased by 40%; ③ Hard rock and fractured rock (basalt, fractured granite) strata: Ordinary surface-mounted drill bits are prone to tooth breakage and failure, making continuous operation impossible. This composite drill bit can drill stably, and its service life is increased by 65% compared to ordinary surface-mounted drill bits. The above data fully demonstrates that the composite structure of this invention can be adapted to complex dry drilling strata from soft to hard rock, balancing high-efficiency cutting with wear-resistant life.
[0053] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and not to limit them; although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features; if these modifications and variations fall within the scope of the claims of the present invention and their equivalents, they should all be considered to be within the protection scope of the present invention.
Claims
1. A dry drilling bit for geological exploration, comprising a steel body (1), a surface-mounted impregnated composite matrix (2), and a core-taking channel (3), wherein the steel body (1), the surface-mounted impregnated composite matrix (2), and the core-taking channel (3) are arranged coaxially, characterized in that, The surface-mounted and impregnated composite matrix (2) is fixedly set at the lower end of the steel body (1) and forms an integrated structure with the steel body (1); the lower end of the surface-mounted and impregnated composite matrix (2) is provided with an inner conical lip surface (4), which is a conical structure inclined towards the drill bit axis; the outer diameter of the steel body (1) and the outer diameter of the surface-mounted and impregnated composite matrix (2) are both provided with an integrated spiral structure (5) to form an integrated spiral outer diameter; the surface-mounted and impregnated composite matrix (2) adopts a structure combining surface setting and impregnation, with surface-mounted diamond particles (8) on the surface of the matrix lip surface and impregnated diamond particles (9) inside the matrix.
2. The dry drilling surface-mounted impregnated diamond drill bit for geological exploration according to claim 1, characterized in that, The angle between the inner conical lip (4) and the drill bit axis is 15°~30°, the width of the conical surface is 8~15mm, and the edge of the lip is provided with a rounded transition with a radius of 1~2mm.
3. The dry drilling surface-mounted impregnated diamond drill bit for geological exploration according to claim 1, characterized in that, The spiral structure (5) is a continuous spiral protrusion with a pitch of 10~25mm and a height of 2~5mm. The spiral direction is consistent with the rotation direction of the drill bit during drilling. The cross section of the spiral protrusion is trapezoidal with an upper base width of 3~5mm and a lower base width of 5~8mm.
4. The dry drilling surface-mounted impregnated diamond drill bit for geological exploration according to claim 1, characterized in that, The diamond beads (8) are high-grade synthetic diamonds with a particle size of 20-40 mesh and a content of 5.2-6.6 carats / cm². 3 The inlay depth is 1 / 3 to 1 / 2 of the diamond particle size; the impregnated diamond particles (9) are a mixture of natural diamonds and artificial diamonds, with a particle size of 40 to 80 mesh and a volume concentration of 80 to 100%.
5. The dry drilling surface-mounted impregnated diamond drill bit for geological exploration according to claim 1, characterized in that, The surface-mounted and impregnated composite matrix (2) is composed of diamond particles, cemented carbide powder, binder and sintering aid; wherein, the diamond particles include surface-mounted diamond particles (8) and impregnated diamond particles (9), and the volume concentration of diamond particles is 70% to 100%; the cemented carbide powder includes WC powder, Mo2C powder and TiC powder, accounting for 60% to 80% of the matrix powder mass; the binder is Co-Ni-Fe binder, accounting for 5% to 15% of the matrix powder mass; the sintering aid is TiH2 sintering aid, accounting for 2 to 4% of the matrix powder mass.
6. The dry drilling surface-mounted impregnated diamond drill bit for geological exploration according to claim 1, characterized in that, A threaded joint (6) is provided at the upper end of the steel body (1), and the central axis of the threaded joint (6) coincides with the central axis of the steel body (1); an annular boss (7) is provided at the lower end of the steel body (1), and the annular boss (7) is wrapped around the surface-mounted and inlaid composite matrix (2) during sintering to achieve the connection between the steel body (1) and the surface-mounted and inlaid composite matrix (2).
7. A method for preparing a dry-drilling, surface-mounted, impregnated diamond drill bit for geological exploration as described in any one of claims 1-6, characterized in that, Includes the following steps: S1. Steel body processing: Process the steel body (1), and process the spiral structure (5) on the outer diameter of the steel body (1); process the annular boss (7) at the lower end of the steel body (1) and the threaded joint (6) at the upper end; perform rust removal, degreasing and sandblasting on the surface of the steel body (1); S2. Preparation of surface-mounted and impregnated composite matrix powder: Weigh the surface-mounted diamond particles (8), impregnated diamond particles (9), WC powder, Mo2C powder, TiC powder, Co-Ni-Fe binder and TiH2 sintering aid according to the formula to prepare impregnated matrix mixed powder; the surface-mounted diamond particles (8) are subjected to surface coating treatment; S3. Graphite mold preparation: Based on the overall structure of the drill bit, the structure of the inner conical lip (4), and the outer diameter structure of the spiral structure (5), a graphite mold (10) is designed and prepared. The cavity of the graphite mold (10) is completely matched with the overall shape of the drill bit. The lower end of the cavity is provided with an inner conical forming surface (11) that is compatible with the inner conical lip (4). The inner wall of the cavity is provided with a spiral groove (12) that is compatible with the spiral outer diameter. The upper part of the cavity is provided with a positioning groove that is compatible with the steel body (1). The center of the cavity is provided with a mold core (13) that is compatible with the core extraction channel (3). S4. Mold installation: Place the processed steel body (1) into the positioning groove of the graphite mold (10), fill it with the mixed powder of the inlaid matrix and compact it, inlay the surface diamond particles (8) on the surface of the matrix powder, and place the graphite block. S5. Sintering: The graphite mold (10) is placed in a hot press sintering furnace and sintered under a vacuum protective atmosphere using a segmented temperature control and gradient pressure sintering process to achieve the integrated combination of the surface-mounted and inlaid composite matrix (2) and the steel body (1). S6. Post-processing: After sintering, the furnace is cooled, the mold and graphite block are removed to obtain the drill bit blank; the drill bit blank is ground and polished, and the finished drill bit is obtained after passing the inspection.
8. The method for preparing a dry-drilling, surface-mounted, impregnated diamond drill bit for geological exploration according to claim 7, characterized in that, In step S3, the graphite mold (10) is made of high-density graphite with a hardness of HV160-200; the inner conical forming surface (11) and the inner conical lip surface (4) have the same angle and the surface roughness is ≤Ra0.8μm; the spiral groove (12) and the spiral structure (5) have a pitch, height and cross-sectional size that are completely matched and the surface roughness is ≤Ra1.0μm.
9. The method for preparing a dry-drilling, surface-mounted, impregnated diamond drill bit for geological exploration according to claim 7, characterized in that, In step S5, the vacuum degree is ≤10. -3 Pa; sintering parameters are: heating rate 6~10℃ / min, hold at 750~850℃ for 30~45min, continue heating to 1150~1250℃, apply pressure of 18~28MPa, hold for 70~100min.
10. The method for preparing a dry-drilling, surface-mounted, impregnated diamond drill bit for geological exploration according to claim 7, characterized in that, In step S6, the test indicators include: the angle deviation of the inner conical lip surface (4) ≤ ±0.5°, the pitch deviation of the spiral structure (5) ≤ ±0.2mm, the spiral protrusion height deviation ≤ ±0.1mm, the bonding strength between the tire body and the steel body ≥220MPa, the hardness of the tire body ≥HV1900, and the shedding rate of the diamond particles (8) ≤1%.