A method and system for optimizing sintering ore blending

By acquiring and transforming sintering ore blending data, constructing a linear programming model and using the GLOP solver, the problems of low efficiency and large error in traditional methods are solved, achieving cost-optimal solutions and improved accuracy under multiple constraints.

CN123117480APending Publication Date: 2026-11-17SHANXIN SOFTWARE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611524777.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-29
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Traditional sintering blending methods are inefficient, prone to errors, and difficult to precisely control alkalinity and quickly find the cost-optimal solution under multiple constraints. They also cannot effectively handle the nonlinear conversion relationship caused by material moisture and burn-off.

Method used

By acquiring data on moisture content, loss on ignition, and chemical composition of various iron-containing raw materials, calculating the dry weight coefficient and residual ignition coefficient, introducing intermediate variables for variable transformation, constructing a linear programming model, and using the GLOP solver to optimize the objective function to minimize the cost per ton of sinter, while conducting secondary verification to ensure the accuracy of the results.

Benefits of technology

It achieves efficient and stable wet blending scheme with the lowest cost per ton of sinter under multiple constraints, improves the automation and calculation accuracy of ore blending optimization, and ensures the accuracy of the results.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123117480A_ABST
    Figure CN123117480A_ABST
Patent Text Reader

Abstract

This application provides a method and system for optimizing sintering ore blending, including acquiring data on moisture content, loss on ignition, chemical composition, and price of each iron-containing raw material; calculating the dry weight coefficient and residual ignition coefficient of each material based on moisture content and loss on ignition; associating the wet blending ratio of each material with an intermediate variable and performing variable transformation; the intermediate variable being the reciprocal of the total residual ignition; constructing a linear programming model using the transformed variable and the intermediate variable as decision variables; the model including residual ignition constraints, wet blending ratio constraints, upper and lower limits constraints on chemical composition, and linearization constraints on basicity; solving the linear programming model with the objective function of minimizing the cost per ton of sintered ore; and back-calculating the wet blending ratio of each material based on the transformed variable and intermediate variable obtained from the solution. This method solves the problems in existing sintering ore blending methods, such as the difficulty in accurately modeling the nonlinear conversion relationship caused by material moisture content and loss on ignition, the inability to linearize the basicity ratio constraint, and the difficulty in quickly obtaining the cost-optimal solution under multiple constraints.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of automation technology in the metallurgical industry, and in particular to a method and system for optimizing sintering ore blending. Background Technology

[0002] Sintering and ore blending is a crucial step in the iron and steel smelting process. Its purpose is to mix various iron-containing raw materials (such as iron ore powder, return ore, and flux) in a specific ratio and then sinter them to produce qualified sinter for use in blast furnace ironmaking. Due to significant differences in the physical and chemical properties of different types of iron-containing raw materials, especially their varying moisture content and loss on ignition, different degrees of mass loss occur during the sintering process. This mass loss leads to a complex nonlinear conversion relationship between the wet blending ratio (i.e., the mass ratio before entering the furnace) and the actual composition of the produced sinter, posing considerable challenges to the formulation of blending schemes.

[0003] Currently, traditional sintering ore blending methods mainly rely on manual experience or simple spreadsheet calculations. These methods have significant shortcomings in practical applications: First, the sinter loss calculation process is cumbersome, and manual calculation is not only inefficient but also prone to errors; second, the basicity (i.e., the ratio of calcium oxide to silicon dioxide), one of the key quality indicators of sinter, is itself a non-linear ratio constraint, making it difficult to control precisely manually; furthermore, when faced with multiple raw material choices and multiple constraints, traditional methods often fail to quickly and accurately determine the cost-optimal ore blending scheme. Summary of the Invention

[0004] This application provides a sintering ore blending optimization method and system to solve the problems in existing sintering ore blending methods, such as the difficulty in accurately modeling nonlinear conversion relationships caused by material moisture and burn-off, the inability to linearize constraints such as alkalinity ratios, and the difficulty in quickly obtaining cost-optimal solutions under multiple constraints.

[0005] In a first aspect, this application provides a method for optimizing sintering ore blending, the method comprising: Obtain data on moisture content, loss on ignition, chemical composition, and price of each iron-containing raw material; Calculate the dry weight coefficient and residual weight coefficient of each material based on the moisture content and loss on ignition. The wet proportions of each material are correlated with an intermediate variable, and the variable is transformed; the intermediate variable is the reciprocal of the total calcination residue. A linear programming model is constructed using the transformed variables and the intermediate variables as decision variables; the model includes residual constraints, wet ratio constraints, upper and lower limits constraints of chemical composition, and alkalinity linearization constraints. The linear programming model is solved with the objective function of minimizing the cost per ton of sinter. The wet proportions of each material are calculated back based on the transformed variables and intermediate variables obtained from the solution.

[0006] In some embodiments, the alkalinity linearization constraint includes: The first linear constraint is used to ensure that the result of subtracting the lower limit of alkalinity from the calcium oxide content and multiplying the silica content is greater than or equal to zero. The second linear constraint is used to ensure that the result of multiplying the upper limit of alkalinity by the silica content minus the calcium oxide content is greater than or equal to zero.

[0007] In some embodiments, the upper and lower limits of chemical composition constraints include sulfur content constraints, wherein the sulfur content constraints are corrected using a preset conversion factor.

[0008] In some embodiments, after back-calculating the wet mix ratio, the method further includes: Secondary verification was performed using a precise formula calculator; the secondary verification included calculating the dry weight ratio, dry weight ratio, calcination residue, unit consumption, price per ton, sulfur dioxide emissions from flue gas, and iron loss indicators.

[0009] In some implementations, the objective function is the minimization of the sum of the products of the transformed variables of each material and their prices, plus the processing cost.

[0010] In some implementations, the linear programming model is solved using the GLOP solver.

[0011] In some embodiments, the iron-containing raw material includes iron ore powder, recycled ore, and flux; the chemical composition includes at least one of iron, silicon dioxide, calcium oxide, magnesium oxide, aluminum oxide, sulfur, and phosphorus.

[0012] In some embodiments, obtaining data on the moisture content, loss on ignition, chemical composition, and price of each iron-containing raw material includes: Read pre-stored iron-containing raw material composition and price data from the database; the database supports the import and maintenance of the composition of purchased raw materials.

[0013] Secondly, this application also provides a sintering ore blending optimization system, the system being used to perform the above-described method, the system comprising: A data acquisition module is configured to acquire data on moisture content, loss on ignition, chemical composition, and price of each iron-containing raw material. The coefficient calculation module is configured to calculate the dry coefficient and the residual coefficient of each material based on the moisture content and loss on ignition, respectively. The variable transformation module is configured to associate the wet ratio of each material with an intermediate variable and perform variable transformation; the intermediate variable is the reciprocal of the total residual calcination. The model building module is configured to construct a linear programming model using the transformed variables and the intermediate variables as decision variables; the model includes residual constraints, wet ratio constraints, upper and lower limits constraints of chemical composition, and alkalinity linearization constraints. The solution module is configured to solve the linear programming model with the objective function of minimizing the cost per ton of sinter. The inverse calculation module is configured to inversely calculate the wet ratio of each material based on the transformed variables and intermediate variables obtained from the solution.

[0014] As can be seen from the above, this application has the following advantages: By transforming variables, the nonlinear ore blending problem is equivalently converted into a linear programming model, making the solution process efficient and stable. Under the premise of satisfying multiple constraints such as chemical composition and alkalinity, the wet blending scheme with the lowest cost per ton of sinter can be automatically obtained. At the same time, the accuracy of the results is ensured through a subsequent secondary verification mechanism, which replaces the traditional manual trial calculation and greatly improves the automation and calculation accuracy of ore blending optimization. Attached Figure Description

[0015] To more clearly illustrate the technical solution of this application, the drawings used in the embodiments will be briefly introduced below. Obviously, for those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0016] Figure 1 This is a flowchart of a sintering ore blending optimization method according to this application; Figure 2 This is a schematic diagram of a sintering ore blending optimization system according to this application. Detailed Implementation

[0017] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0018] It should be noted that the brief descriptions of terms in this application are only for the convenience of understanding the embodiments described below, and are not intended to limit the embodiments of this application. Unless otherwise stated, these terms should be understood in their ordinary and common meaning.

[0019] It should be noted that, in this application, the terms "exemplary" or "for example" are used to indicate that something is being described as an example, illustration, or illustration. Any embodiment or design described as "exemplary" or "for example" in this application should not be construed as being more preferred or advantageous than other embodiments or design solutions. Specifically, the use of terms such as "exemplary" or "for example" is intended to present the relevant concepts in a concrete manner.

[0020] See Figure 1 As can be seen, this embodiment provides a method for optimizing sintering ore blending, the method comprising: S11, obtain data on moisture content, loss on ignition, chemical composition, and price of each iron-containing raw material.

[0021] Specifically, in this embodiment, pre-stored basic data of various iron-containing raw materials are read from the database. These iron-containing raw materials include, but are not limited to, iron ore powder, return ore, and flux. The acquired data specifically includes: Moisture data: Percentage of moisture content of each material in a wet state.

[0022] Burn-off data: The percentage of mass loss of each material during high-temperature sintering due to loss of water of crystallization, decomposition of carbonates, combustion of organic matter, etc.

[0023] Chemical composition data: including the percentage content of elements such as total iron (TFe), silicon dioxide (SiO2), calcium oxide (CaO), magnesium oxide (MgO), aluminum oxide (Al2O3), sulfur (S), and phosphorus (P).

[0024] Price data: The dry basis price of each material delivered to the plant, which is the basis for calculating costs.

[0025] The method further includes: S12, calculate the dry weight coefficient and burn weight coefficient of each material based on the moisture content and burn loss.

[0026] Specifically, in this embodiment, based on the obtained moisture and burn loss data, two key coefficients are calculated for each material: Dry weight conversion factor (a_i): The calculation formula is a_i = (100 - moisture_i) / 100. This factor is used to convert the mass of wet-based materials into dry-based mass excluding moisture.

[0027] Burn-off coefficient (b_i): The calculation formula is b_i = (100 - burn-off_i) / 100. This coefficient is used to convert the mass of dry-based material into the mass remaining after sintering and burn-off.

[0028] The method further includes: S13, associate the wet ratio of each material with an intermediate variable and perform variable transformation; the intermediate variable is the reciprocal of the total calcination residue.

[0029] Specifically, in this embodiment, a key variable transformation step is performed. To address the nonlinear relationship between the wet mix ratio (w_i) and the final sinter composition, this method introduces an intermediate variable t and defines a new transformation variable y_i.

[0030] The intermediate variable t is defined as the reciprocal of the total burn residue, i.e., t = 1 / total burn residue.

[0031] The transformation variable y_i is defined as the product of the wet ratio and the intermediate variable, i.e., y_i = w_i × t.

[0032] Through this transformation, the originally nonlinear ore blending problem is cleverly transformed into a linear problem concerning y_i and t.

[0033] The method further includes: S14. Using the transformed variables and the intermediate variables as decision variables, construct a linear programming model; the model includes residual constraints, wet ratio constraints, upper and lower limits constraints of chemical composition, and alkalinity linearization constraints.

[0034] Specifically, in this embodiment, a standard linear programming model is constructed using the transformed variable y_i and the intermediate variable t as decision variables. This model includes the following core constraints: Residuals and constraints: ; This constraint ensures that the sum of the residual mass of all materials after dehydration and burn-off is exactly equal to 1 ton of sinter.

[0035] Wet proportioning and constraints: ; This constraint links the transformed variables to the original sum of wet proportions.

[0036] Chemical composition upper and lower limits constraints: For example, the constraint for total iron (TFe) can be expressed as: ; This allows the chemical composition of the finished sintered ore to be controlled within the range required by the process.

[0037] Alkalinity linearization constraint: The nonlinear alkalinity ratio constraint (R=CaO / SiO2) is transformed into two linear inequalities.

[0038] The method further includes: S15, with the objective function of minimizing the cost per ton of sintered ore, solve the linear programming model.

[0039] Specifically, in this embodiment, the objective function is to minimize the cost per ton of sinter, that is: ; Calling an efficient linear programming solver (such as the GLOP solver) to solve the model will directly provide the optimal values ​​of y_i and t.

[0040] The method further includes: S16, calculate the wet ratio of each material based on the transformed variables and intermediate variables obtained from the solution.

[0041] Specifically, in this embodiment, based on the solved y_i and t, the wet proportion w_i of each material is calculated using the formula w_i=y_i / t. This wet proportion is the optimal batching scheme that minimizes the cost per ton of sinter while satisfying all process and quality constraints.

[0042] Furthermore, in some embodiments, the alkalinity linearization constraint includes: The first linear constraint is used to ensure that the result of subtracting the lower limit of alkalinity from the calcium oxide content and multiplying the silica content is greater than or equal to zero. The second linear constraint is used to ensure that the result of multiplying the upper limit of alkalinity by the silica content minus the calcium oxide content is greater than or equal to zero.

[0043] Specifically, in this embodiment, basicity R is a key quality indicator of sintered ore, defined as the ratio of calcium oxide (CaO) to silicon dioxide (SiO2), i.e., R = CaO / SiO2. This is a typical nonlinear ratio constraint, which cannot be directly handled in traditional linear programming models. To solve this problem, this embodiment decomposes the ratio constraint R ∈ [R_min, R_max] into two purely linear inequalities: The first linear constraint is used to ensure that the alkalinity does not fall below its lower limit R_min. The mathematical expression of this constraint is: CaO - R_min × SiO2 ≥ 0. Substituting this into the transformed variables, its specific form is: .

[0044] The essence of this constraint is to require that the calcium oxide content in the sinter be at least R_min times its silica content, thereby ensuring that the alkalinity is not too low.

[0045] The second linear constraint is used to ensure that alkalinity does not exceed its upper limit R_max. The mathematical expression of this constraint is: .

[0046] Substituting it into the transformed variable, its specific form is: .

[0047] The essence of this constraint is to require that the R_max multiple of the silica content in the sinter be at least equal to the calcium oxide content, thereby ensuring that the alkalinity is not too high.

[0048] Through these two linear inequalities, the originally nonlinear alkalinity range constraint is perfectly linearized and can be directly used as a standard constraint condition for solving linear programming models.

[0049] Furthermore, in some embodiments, the upper and lower limits of chemical composition constraints include sulfur composition constraints, wherein the sulfur composition constraints are corrected for sulfur content using a preset conversion factor.

[0050] Specifically, in this embodiment, sulfur is a harmful element during the sintering process, and its content needs to be strictly controlled. However, the behavior of sulfur during the sintering process is quite complex; not all sulfur remains in the final sinter, and some sulfur is discharged with the flue gas in gaseous form (such as SO2). Therefore, directly substituting the original sulfur content in the material into the model for calculation will lead to a deviation in the prediction of the sulfur content of the finished sinter.

[0051] To address this issue, this embodiment introduces a preset conversion factor to correct for the sulfur content of the material. According to the technical disclosure, this conversion factor typically has a value of 0.26. This means that when performing constrained calculations for sulfur content, the original sulfur content (S_i) from the material analysis report is not used directly; instead, the corrected sulfur content S'_i = 0.26 × S_i is used.

[0052] Therefore, when constructing the linear programming model, the upper and lower limits of the sulfur content become: ; Where S_min and S_max are the lower and upper limits of the permissible sulfur content in the finished sinter, respectively. In this way, the model can more realistically reflect the actual residual sulfur during the sintering process, thereby making more accurate batching decisions.

[0053] Furthermore, in some embodiments, the method further includes: Secondary verification was performed using a precise formula calculator; the secondary verification included calculating the dry weight ratio, dry weight ratio, calcination residue, unit consumption, price per ton, sulfur dioxide emissions from flue gas, and iron loss indicators.

[0054] Specifically, in this embodiment, the secondary verification process mainly includes the calculation and verification of the following indicators: Dry basis ratio: Based on the back-calculated wet basis ratio and the moisture content of each material, the dry basis ratio is recalculated.

[0055] Dry proportion: Calculate the mass percentage of each material in a dry basis.

[0056] Burn residue: The total burn residue is accurately calculated based on the dry proportions and burn loss of each material.

[0057] Unit consumption: Calculates the consumption of various materials (including iron-containing materials and flux) required to produce one ton of sinter.

[0058] Price per ton: This is an indicator of cost-effectiveness, calculated as sintering cost / theoretical TFe value, with the unit being yuan / ton. It reflects the cost per unit of iron grade.

[0059] Sulfur dioxide emissions from flue gas: The concentration of SO2 in the sintering flue gas (mg / Nm³) is accurately estimated based on factors such as the sulfur content in the materials and desulfurization efficiency. 3 ).

[0060] Iron loss: This is a comprehensive indicator, calculated using the following formula: ; Used to evaluate the iron loss rate throughout the sintering process.

[0061] The system will compare all the indicators output by the precise formula calculator with the assumptions and constraints in the linear programming model to confirm whether all constraints are met and whether the various economic and technical indicators are reasonable.

[0062] Furthermore, in some embodiments, the objective function is the minimization of the sum of the products of the transformed variables of each material and their prices, plus the processing fee.

[0063] Specifically, in this embodiment, the objective function is the direction of optimization in the linear programming model, and the goal of this method is to minimize the cost per ton of sintered ore. The specific structure of this objective function is as follows: ; in: Z represents the final total cost per ton of sinter.

[0064] y_i is the transformation variable of the i-th material.

[0065] Price_i is the dry basis price delivered to the plant for the i-th material. Dry basis price is used here instead of wet basis price because moisture does not generate value, and using dry basis price more accurately reflects the true cost of raw materials. The sum of y_i × Price_i represents the raw material cost of all variable materials such as iron-containing raw materials and fluxes.

[0066] Processing costs are a constant term, representing fixed and variable costs other than raw material costs, such as fuel costs, electricity costs, equipment depreciation, and labor wages. This part of the cost is considered relatively fixed and does not change with variations in the ingredient mix.

[0067] Therefore, the solver's task is to find a set of values ​​for y_i such that... This part should be as small as possible to minimize the total cost Z.

[0068] Furthermore, in some embodiments, the linear programming model is solved using the GLOP solver.

[0069] Specifically, in this embodiment, the solver used is the GLOP solver. After the model is built, the system will combine all the aforementioned decision variables (y_i, t) and the objective function: All constraints (residual constraints, wet mix ratio constraints, chemical composition constraints, alkalinity linearization constraints, etc.) are encapsulated according to the input format required by the GLOP solver. Subsequently, the system calls the GLOP solver's API interface, submitting the linear programming model for solution. Internally, the GLOP solver employs advanced algorithms such as the simplex method or interior point method to search for the optimal solution that minimizes the objective function value within the given constraint space. After solving, the GLOP solver returns the optimal decision variable values ​​(i.e., the optimal y_i and t), as well as the solution status (e.g., whether an optimal solution was found, whether it is unbounded, or whether there is no feasible solution).

[0070] Furthermore, in some embodiments, the iron-containing raw material includes iron ore powder, recycled ore, and flux; the chemical composition includes at least one of iron, silicon dioxide, calcium oxide, magnesium oxide, aluminum oxide, sulfur, and phosphorus.

[0071] Specifically, in this embodiment, the types of iron-containing raw materials are clearly divided into three main categories: Iron ore powder: As the main source of iron, it is the main raw material newly purchased.

[0072] Return ore: Material generated during the sintering process that is substandard in particle size or strength and needs to be returned for re-sintering. Its composition is similar to sintered ore, but the particle size is smaller.

[0073] Flux: mainly used to adjust the basicity of sinter and improve the physicochemical properties of the sintering process. Common fluxes include limestone, dolomite, serpentine, etc., which mainly provide CaO and MgO.

[0074] Types of chemical components: The model specifies that the chemical components to be considered include at least the following: total iron (TFe), silicon dioxide (SiO2), calcium oxide (CaO), magnesium oxide (MgO), aluminum oxide (Al2O3), sulfur (S), and phosphorus (P). Among these, TFe is the core indicator for measuring iron grade; SiO2 and CaO are used to control basicity; MgO affects slag fluidity and desulfurization capacity; Al2O3 affects slag viscosity and blast furnace operation; and S and P are harmful impurities that require strict control. This implementation method indicates that these components are at least one, meaning that constraints on other trace elements can be added according to actual process requirements.

[0075] Furthermore, in some embodiments, obtaining data on the moisture content, loss on ignition, chemical composition, and price of each iron-containing raw material includes: Read pre-stored iron-containing raw material composition and price data from the database; the database supports the import and maintenance of the composition of purchased raw materials.

[0076] Specifically, in this embodiment, the database is a specially designed central data warehouse for storing and managing information on iron-containing raw materials. Its key features are: Pre-storage: All data on moisture content, loss on ignition, chemical composition, and price of iron-containing raw materials are pre-stored in the database.

[0077] Dynamic Maintenance: This database supports the import and maintenance of the composition of incoming raw materials. This means that whenever a new batch of raw materials arrives, the quality control department can import the latest composition data (such as TFe, SiO2, CaO, etc.) into the database in batches through the system interface after completing the testing. Similarly, when market prices change, purchasing personnel can also update the price information of raw materials in the database. This dynamic maintenance mechanism ensures that the data used by the optimization model is always the latest and most accurate.

[0078] When performing optimization calculations, the system only needs to initiate a database query request to obtain the latest data of all candidate raw materials without any manual intervention.

[0079] See Figure 2 It is understood that this embodiment also provides a sintering ore blending optimization system, the system comprising: The data acquisition module is configured to acquire data on moisture content, loss on ignition, chemical composition, and price of each iron-containing raw material.

[0080] Specifically, in this embodiment, the data acquisition module serves as the system's data entry point, configured to automatically retrieve moisture, loss on ignition, chemical composition, and price data for each iron-containing raw material from a designated database. It is responsible for communicating with the underlying database to ensure the real-time nature and accuracy of the data, providing reliable input for subsequent calculations.

[0081] The system also includes: The coefficient calculation module is configured to calculate the dry coefficient and the residual coefficient of each material based on the moisture content and loss on ignition, respectively.

[0082] Specifically, in this embodiment, the coefficient calculation module receives raw data from the data acquisition module and calculates two key coefficients for each material according to the built-in formulas: the dry matter coefficient a_i and the ignition loss coefficient b_i. The calculation logic strictly follows a_i = (100 - moisture_i) / 100 and b_i = (100 - ignition loss_i) / 100, preparing for subsequent variable transformations.

[0083] The system also includes: The variable transformation module is configured to associate the wet ratio of each material with an intermediate variable and perform variable transformation; the intermediate variable is the reciprocal of the total calcination residue.

[0084] Specifically, in this embodiment, the variable transformation module is the core innovation of the entire system. It receives the output of the coefficient calculation module and executes the crucial variable transformation logic. Specifically, it defines an intermediate variable t (the reciprocal of the total burn residue), then associates the original wet ratio w_i with t to generate a new decision variable y_i = w_i × t. Through this step, it transforms the basis of all subsequent calculations from the nonlinear wet ratio space to the linear y_i and t space.

[0085] The system also includes: The model building module is configured to construct a linear programming model using the transformed variables and the intermediate variables as decision variables; the model includes residual constraints, wet ratio constraints, upper and lower limits constraints of chemical composition, and alkalinity linearization constraints.

[0086] Specifically, in this embodiment, the model building module is responsible for converting all process requirements and quality indicators into a mathematical model. Using y_i and t generated by the variable transformation module as decision variables, it automatically constructs a complete linear programming model. This model includes: residual constraints, wet ratio constraints, upper and lower limits of chemical composition constraints (including sulfur composition constraints with conversion factors), and alkalinity constraints after linearization. This module encodes all business rules into mathematical equations and inequalities.

[0087] The system also includes: The solution module is configured to solve the linear programming model with the objective function of minimizing the cost per ton of sinter.

[0088] Specifically, in this embodiment, the solver module receives the linear programming model output by the model building module and calls its internal linear programming solver (such as the GLOP solver) to solve it. It uses minimizing the cost per ton of sinter as the objective function and seeks the optimal values ​​of y_i and t while satisfying all constraints. After solving, it passes the result to the next module.

[0089] The system also includes: The inverse calculation module is configured to inversely calculate the wet ratio of each material based on the transformed variables and intermediate variables obtained from the solution.

[0090] Specifically, in this embodiment, the inverse calculation module receives the optimal y_i and t values ​​output by the solution module, and uses the formula w_i=y_i / t to calculate the optimal proportion w_i of each material under wet conditions. This w_i is the final batching scheme that can be directly used to guide production.

[0091] For ease of explanation, the above description has been provided in conjunction with specific embodiments. However, the discussion in some embodiments is not intended to be exhaustive or to limit the embodiments to the specific forms disclosed above. Various modifications and variations can be obtained based on the above teachings. The selection and description of the above embodiments are for the purpose of better explaining the contents of this disclosure, thereby enabling those skilled in the art to better utilize the embodiments.

Claims

1. A method for optimizing sintering ore blending, characterized in that, The method includes: Obtain data on moisture content, loss on ignition, chemical composition, and price of each iron-containing raw material; Calculate the dry weight coefficient and residual weight coefficient of each material based on the moisture content and loss on ignition. The wet proportions of each material are correlated with an intermediate variable, and the variable is transformed; the intermediate variable is the reciprocal of the total calcination residue. A linear programming model is constructed using the transformed variables and the intermediate variables as decision variables; the model includes residual constraints, wet ratio constraints, upper and lower limits constraints of chemical composition, and alkalinity linearization constraints. The linear programming model is solved with the objective function of minimizing the cost per ton of sinter. The wet proportions of each material are calculated back based on the transformed variables and intermediate variables obtained from the solution.

2. The sintering ore blending optimization method according to claim 1, characterized in that, The alkalinity linearization constraint includes: The first linear constraint is used to ensure that the result of subtracting the lower limit of alkalinity from the calcium oxide content and multiplying the silica content is greater than or equal to zero. The second linear constraint is used to ensure that the result of multiplying the upper limit of alkalinity by the silica content minus the calcium oxide content is greater than or equal to zero.

3. The sintering ore blending optimization method according to claim 1, characterized in that, The upper and lower limits of the chemical composition include sulfur content constraints, which are corrected for sulfur content using a preset conversion factor.

4. The sintering ore blending optimization method according to claim 1, characterized in that, After calculating the wet mix ratio, the method further includes: Secondary verification was performed using a precise formula calculator; the secondary verification included calculating the dry weight ratio, dry weight ratio, calcination residue, unit consumption, price per ton, sulfur dioxide emissions from flue gas, and iron loss indicators.

5. The sintering ore blending optimization method according to claim 1, characterized in that, The objective function is to minimize the sum of the products of the transformed variables of each material and their prices, plus the processing cost.

6. The sintering ore blending optimization method according to claim 1, characterized in that, The linear programming model is solved using the GLOP solver.

7. The sintering ore blending optimization method according to claim 1, characterized in that, The iron-containing raw materials include iron ore powder, recycled ore, and flux; the chemical composition includes at least one of iron, silicon dioxide, calcium oxide, magnesium oxide, aluminum oxide, sulfur, and phosphorus.

8. The sintering ore blending optimization method according to claim 1, characterized in that, The acquisition of moisture, loss on ignition, chemical composition, and price data for each iron-containing raw material includes: Read pre-stored iron-containing raw material composition and price data from the database; the database supports the import and maintenance of the composition of purchased raw materials.

9. A sintering ore blending optimization system, said system being used to execute the sintering ore blending optimization method according to any one of claims 1 to 8, characterized in that, The system includes: A data acquisition module is configured to acquire data on moisture content, loss on ignition, chemical composition, and price of each iron-containing raw material. The coefficient calculation module is configured to calculate the dry coefficient and the residual coefficient of each material based on the moisture content and loss on ignition, respectively. The variable transformation module is configured to associate the wet ratio of each material with an intermediate variable and perform variable transformation; the intermediate variable is the reciprocal of the total residual calcination. The model building module is configured to construct a linear programming model using the transformed variables and the intermediate variables as decision variables; the model includes residual constraints, wet ratio constraints, upper and lower limits constraints of chemical composition, and alkalinity linearization constraints. The solution module is configured to solve the linear programming model with the objective function of minimizing the cost per ton of sinter. The inverse calculation module is configured to inversely calculate the wet ratio of each material based on the transformed variables and intermediate variables obtained from the solution.