A heat insulation and heat dissipation plate, a secondary battery and an electrical device.

By embedding a hydrogel phase change heat dissipation layer within the battery insulation layer, the problem of thermal runaway in high-capacity batteries is solved, achieving effective heat isolation and cooling, adapting to changes in cell volume, and improving battery safety and stability.

CN123120972APending Publication Date: 2026-11-17SUCOOL TECH (SHENZHEN) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611514752.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-28
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing high-capacity batteries are prone to thermal runaway under conditions of overcharging, short circuit, compression, and thermal abuse. They lack effective thermal propagation prevention and heat dissipation protection, resulting in insufficient safety and stability.

Method used

A hydrogel phase change heat dissipation layer is set inside the heat insulation layer of inorganic ceramic material, combined with materials such as polyacrylamide, fumed silica, hollow glass microspheres and glass fiber to form a compressible composite material. The phase change heat dissipation layer vaporizes at high temperature and carries away heat, thereby reducing the temperature of the battery cell.

Benefits of technology

It effectively blocks heat transfer at high temperatures, reduces the risk of thermal runaway, adapts to changes in cell volume, provides mechanical strength and flexibility, and improves the safety performance of the battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123120972A_ABST
    Figure CN123120972A_ABST
Patent Text Reader

Abstract

This application discloses a heat insulation and heat dissipation plate, a secondary battery, and an electrical device, relating to the field of new energy technology. The heat insulation and heat dissipation plate is manufactured using an integral molding process, and its structure includes a heat insulation layer and a phase change heat dissipation layer encased inside the heat insulation layer. The heat insulation layer is made of inorganic ceramic material; the phase change heat dissipation layer is made of hydrogel; and the thermal conductivity of the heat insulation and heat dissipation plate at 25℃ is 0.020~0.045 W / (m·K). By setting a hydrogel phase change heat dissipation layer inside the inorganic ceramic material heat insulation layer, the heat insulation plate can be endowed with efficient heat insulation and heat dissipation cooling effects, synergistically improving the safety protection performance of high-capacity battery cells. Due to the flexibility of the internal hydrogel material, the heat insulation and heat dissipation plate also has compressibility, solving the problem of the incompressibility of traditional heat insulation plates and adapting to the volume contraction and expansion during the charging and discharging process of the battery cell.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of new energy technology, and in particular to a heat insulation heat dissipation plate, a secondary battery, and an electrical device. Background Technology

[0002] With the rapid iteration and upgrading of the new energy vehicle and energy storage industries, power batteries are gradually developing towards high capacity, high energy density, high-rate charge and discharge, and integrated packaging. The large-scale application of high-nickel ternary and large-capacity lithium iron phosphate cells has significantly improved the range and energy storage capacity of battery systems. However, the heat storage and heat release rates of individual cells have also increased significantly. Under conditions of overcharging, short circuit, compression, and thermal abuse, batteries are highly susceptible to thermal runaway, which greatly restricts the safety and stability of energy storage and power battery systems. Therefore, building an efficient and reliable cell thermal runaway isolation and protection system to suppress the thermal propagation chain reaction is the core safety guarantee for the large-scale application of high-capacity batteries and a key requirement for industry technological upgrading. Summary of the Invention

[0003] This application provides a heat insulation heat dissipation plate, a secondary battery, and an electrical device. The integrally formed heat insulation heat dissipation plate has the functions of efficient heat insulation and heat dissipation and cooling. Its mechanical compressibility can adapt to the volume contraction and expansion during the charging / discharging process of the battery cell, thus better meeting the long-term normal use and safety protection requirements of high-capacity and high-density power batteries.

[0004] In a first aspect, this application provides a heat-insulating heat dissipation plate, including a heat insulation layer and a phase change heat dissipation layer wrapped inside the heat insulation layer, wherein: The material of the heat insulation layer includes inorganic ceramic materials; The material of the phase change heat dissipation layer includes hydrogel; The thermal conductivity of the heat insulation and heat dissipation plate at 25℃ is 0.020~0.045W / (m·K).

[0005] This application provides a hydrogel phase change heat dissipation layer inside the heat insulation layer of inorganic ceramic material, which can give the heat insulation board the function of heat dissipation and cooling, and improve the overall performance of the material. Due to the flexibility of the hydrogel heat dissipation material, it is compressible, which solves the shortcoming of traditional heat insulation boards that are not compressible and adapts to the contraction and expansion of the battery cell.

[0006] In some embodiments, the phase change heat dissipation layer is made of polyacrylamide, fumed silica, hollow glass microspheres, glass fiber, and water. Polyacrylamide serves as a hydrogel polymer framework, providing space for water retention and structural strength, making the overall heat dissipation material compressible and designable, with pressure deformation to accommodate battery volume expansion. Fumed silica improves the material's thermal insulation performance. Hollow glass microspheres can partially replace silica as a thermal insulation component, reducing raw material costs. Glass fiber improves the material's strength and toughness. Water acts as a phase change material, vaporizing at temperatures above 100°C to carry away heat and reduce the probability of thermal runaway. The hollow glass microspheres have a size of 55 μm to 65 μm. The glass fiber has a size of 6 μm to 10 μm.

[0007] In some embodiments, the mass ratio of polyacrylamide, fumed silica, hollow glass microspheres, glass fiber, and water is 10:(6~10):(10~20):(4~8):(60~75). When the mass ratio of polyacrylamide, fumed silica, hollow glass microspheres, glass fiber, and water is within the above range, they can be uniformly mixed and molded to balance mechanical and thermal insulation properties.

[0008] In some embodiments, the inorganic ceramic material includes nano-silica, an infrared shielding agent, ceramic fibers, and a binder. Nano-silica can improve the material's thermal insulation performance. The infrared shielding agent can reduce high-temperature infrared radiation. Ceramic fibers can improve the material's mechanical strength. The binder can improve the interaction between nanoparticles, which is beneficial for molding. The infrared shielding agent includes, but is not limited to, at least one of silicon carbide, titanium dioxide, and nano-carbon black. The ceramic fibers include, but are not limited to, at least one of alumina ceramic fibers, zirconia ceramic fibers, and mullite ceramic fibers. The binder includes, but is not limited to, at least one of silica sol, water glass, carboxymethyl cellulose, and polyvinyl alcohol.

[0009] In some embodiments, the mass ratio of nano-silica, infrared shading agent, ceramic fiber, and binder is (60~80):(4~8):(5~10):(3~6). Within this range, the mass ratio of nano-silica, infrared shading agent, ceramic fiber, and binder can impart high thermal insulation performance and excellent mechanical strength to the composite material.

[0010] In some embodiments, the phase change heat dissipation layer accounts for 25% to 45% of the thickness of the insulation layer; and / or, The thickness of the phase change heat dissipation layer is 0.8mm to 2.0mm; the thickness of the phase change heat dissipation layer is within this range, which allows for... Suitable for one-piece compression molding processes, the composite material has sufficiently high mechanical strength and thermal insulation properties; and / or, The thickness of the insulation layer is 1.8~6.0mm. Within this range, the thickness of the insulation layer can be adapted to the current spacing between energy storage batteries and power batteries, ensuring sufficient thermal insulation safety redundancy.

[0011] In some embodiments, the hydrogel is encapsulated by an airtight and watertight material to form a phase change heat dissipation layer. During normal use, the encapsulation of the hydrogel by the airtight and watertight material prevents moisture evaporation. Simultaneously, when the temperature rises (>100°C), the water trapped inside undergoes a phase change, turning into water vapor. This vapor breaks through the edges of the encapsulation material (the edges are formed by heat-pressing two pieces of encapsulation material together, which can rupture under vapor pressure), carrying away heat and achieving heat dissipation. The airtight and watertight material can be at least one of aluminum-plastic film, polyester film, and polyimide film.

[0012] In some embodiments, the area ratio of the phase change heat dissipation layer to the heat insulation layer in the length and width directions is (0.7~0.95):1. Within this range, the phase change heat dissipation layer can be encased within the heat insulation layer, adapting to a one-piece molding production process. Multiple functional modules can be integrated, resulting in synergistic enhancement of overall mechanical strength and flexibility, and high production efficiency. In contrast, a simple physical stacked structure of heat insulation layer / intermediate layer / heat insulation layer will have an increased overall thermal conductivity due to the intermediate layer, leading to a decrease in heat insulation performance. Furthermore, the surface of the heat insulation layer has a porous nanostructure, low surface energy, and the presence of loose powder, making it difficult to bond it to the intermediate layer material to form a unified whole.

[0013] Because the phase change heat dissipation layer is wrapped inside the insulation layer, and the insulation material surrounds the phase change heat dissipation layer, the phase change heat dissipation layer is embedded inside the insulation layer like a sandwich. The water inside the phase change heat dissipation layer material, as a phase change component, vaporizes at high temperature (above 100℃ at normal pressure) and carries away a large amount of heat. At the same time, the remaining polymer skeleton and inorganic mixture still have good thermal insulation performance, with a thermal conductivity close to 0.03W / m·K.

[0014] Specifically, a 1mm thick layer of heat insulation powder (containing nano-silica, infrared shielding agent, ceramic fiber, and adhesive in a mass ratio of 72:5:8:5, pre-mixed evenly) can be laid flat in a cuboid mold. Then, a 1mm thick layer of heat dissipation material (containing polyacrylamide, fumed silica, hollow glass microspheres, glass fiber, and water in a mass ratio of 10:6:12:4:68, pre-mixed evenly) can be placed in the aluminum-plastic film-encapsulated heat dissipation material. The thickness of the powder can be controlled by the feeding weight of the mixed powder and the depth of the mold's vertical displacement. Finally, the material is molded into a single piece using a press at a room temperature of 25°C. The sheet is then encapsulated with PET (polyethylene terephthalate) double-sided adhesive, which is the final heat insulation and heat dissipation plate.

[0015] The thermal insulation layer and phase change heat dissipation layer materials have extremely low thermal conductivity, effectively blocking heat transfer. When heat is transferred to the heat dissipation material, the temperature reaches 100℃~110℃. The water in the intermediate gel undergoes a phase change, vaporizing and breaking through the aluminum-plastic film from the edges, carrying away a large amount of heat and cooling the heat source of the device. Simultaneously, the remaining polymer and inorganic components still have good thermal insulation properties (the thermal conductivity of the dry phase change heat dissipation layer is 0.03 W / (m·K)), having a limited impact on the overall high thermal insulation performance of the material. Based on the thermal insulation board, a composite material with thermal insulation and heat dissipation functions is integrally molded. This design not only endows the thermal insulation material with heat dissipation performance, but also breaks through the barrier limit of existing thermal insulation boards under the same thickness conditions, further reducing the heat source temperature and shortening the duration of higher temperatures through phase change heat dissipation, protecting adjacent devices; at the same time, due to the flexibility of the intermediate hydrogel material, the thermal insulation and heat dissipation material as a whole has a certain degree of compressibility, mechanically adapting to the contraction and expansion changes during the battery structure's cyclic charging and discharging, thus protecting the battery cell.

[0016] Secondly, this application provides a secondary battery, including a plurality of cells and a heat-insulating heat dissipation plate as described in the first aspect, disposed between adjacent cells.

[0017] Thirdly, this application provides an electrical device including the secondary battery described in the second aspect. Attached Figure Description

[0018] To more clearly illustrate the technical solutions in the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0019] Figure 1 This is a cross-sectional view of a heat insulation and heat dissipation plate according to an embodiment of this application in the thickness direction.

[0020] Figure 2 This is a cross-sectional view of a heat-insulating heat dissipation plate according to an embodiment of this application in the direction of the heat insulation surface.

[0021] Figure 3 This is a schematic diagram of the position and structure of the heat insulation plate and the battery cell in a secondary battery according to an embodiment of this application.

[0022] Explanation of icon numbers: 100 heat insulation heat dissipation plate; 1 heat insulation layer; 2 phase change heat dissipation layers; 200 battery cells. Detailed Implementation

[0023] To make the objectives, technical solutions, and advantages of this application clearer, the technical solutions of this application will be clearly and completely described below in conjunction with the embodiments of this application. Obviously, the described embodiments are only some, not all, of the embodiments of this application. Based on the embodiments of this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.

[0024] With the rapid iteration and upgrading of the new energy vehicle and energy storage industries, power batteries are gradually developing towards high capacity, high energy density, high-rate charge and discharge, and integrated packaging. The large-scale application of high-nickel ternary and large-capacity lithium iron phosphate cells has significantly improved the range and energy storage capacity of battery systems. However, the heat storage and heat release rates of individual cells have also increased significantly. Under conditions of overcharging, short circuit, compression, and thermal abuse, batteries are highly susceptible to thermal runaway, which greatly restricts the safety and stability of energy storage and power battery systems. Therefore, building an efficient and reliable cell thermal runaway isolation and protection system to suppress the thermal propagation chain reaction is the core safety guarantee for the large-scale application of high-capacity batteries and a key requirement for industry technological upgrading.

[0025] Currently, mainstream materials for thermal protection of high-capacity batteries include aerogel thermal insulation composites, ceramic fibers, insulation boards, and mica composite panels. While these materials exhibit high-temperature insulation and flame-retardant protection in specific scenarios, they generally suffer from technical bottlenecks, such as difficulty in balancing insulation performance, thickness, and mechanical strength, and lack heat dissipation capabilities. For example, aerogel materials, based on a porous structure, have high porosity, low thermal conductivity, and excellent insulation performance. However, their loose and fragile framework makes them prone to cracking, pulverization, and collapse under battery cyclic expansion and compression, as well as vehicle vibration and impact conditions, leading to a rapid decline in protective performance. Insulation boards, with their dense structure, lack sufficient mechanical toughness and cannot adapt to the normal charging and discharging contraction and deformation of the battery. Once the internal microporous structure of the material is damaged, the thermal conductivity increases significantly, and the thermal insulation barrier capability decreases markedly. Furthermore, these insulation materials lack heat dissipation and cooling functions. To ensure sufficiently high safety protection, sufficiently thick insulation materials are usually chosen, increasing material costs and installation space while sacrificing the energy density of the battery system. Therefore, developing novel composite protective materials with low thermal conductivity, heat dissipation, and adjustable mechanical properties is essential to better meet the long-term safety protection requirements of high-capacity, high-density power batteries.

[0026] For example, one method for preparing a high-insulation nanoporous thermal insulation board involves mixing fumed silica, fumed alumina, a light-blocking agent, and fibers in a specific mass ratio, and then pressing the mixture into a nanoporous thermal insulation board at room temperature in a mold, resulting in a board with low thermal conductivity. While this method produces insulation boards with excellent thermal barrier properties and avoids dust pollution in the production environment, the materials are prone to cracking, lack proper encapsulation, and easily shed powder. In practical applications, this can easily contaminate other devices and the environment.

[0027] In view of this, this application provides a heat insulation heat dissipation plate, a secondary battery, and an electrical device to better meet the long-term safety protection requirements of high-capacity, high-density power batteries.

[0028] Firstly, such as Figure 1 and Figure 2 As shown, this application provides a heat insulation and heat dissipation plate 100, including a heat insulation layer 1 and a phase change heat dissipation layer 2 wrapped inside the heat insulation layer 1, wherein: The material of the heat insulation layer 1 includes inorganic ceramic materials; The material of the phase change heat dissipation layer 2 includes hydrogel; The thermal conductivity of the heat insulation and heat dissipation plate 100 at 25℃ is 0.020~0.045W / (m·K).

[0029] This application provides a hydrogel phase change heat dissipation layer 2 inside the heat insulation layer 1 of inorganic ceramic material, which can give the heat insulation board the function of heat dissipation and cooling, and improve the overall performance of the material. Due to the presence of the hydrogel heat dissipation material, it is compressible, which solves the problem of the incompressibility of traditional heat insulation boards and adapts to the contraction and expansion of the battery cell.

[0030] The thermal insulation heat dissipation plate 100 has a thermal conductivity within this range at 25℃, which can effectively block the diffusion of heat from the thermal runaway cell to adjacent cells and prevent the spread of thermal runaway.

[0031] In conjunction with the first aspect, in some embodiments provided in this application, the phase change heat dissipation layer 2 is made of polyacrylamide, fumed silica, hollow glass microspheres, glass fiber, and water. Polyacrylamide serves as a hydrogel polymer framework, providing space for water retention and structural strength, making the overall heat dissipation material compressible and designable, with pressure deformation to accommodate battery volume expansion. Fumed silica improves the material's thermal insulation performance. Hollow glass microspheres can partially replace silica as a thermal insulation component, reducing raw material costs. Glass fiber improves the material's strength and toughness. Water acts as a phase change material, vaporizing at temperatures above 100°C to carry away heat and reduce the probability of thermal runaway. The hollow glass microspheres have a size of 55 μm to 65 μm. The glass fiber has a size of 6 μm to 10 μm.

[0032] In conjunction with the first aspect, in some embodiments provided in this application, the mass ratio of polyacrylamide, fumed silica, hollow glass microspheres, glass fiber, and water is 10:(6~10):(10~20):(4~8):(60~75). When the mass ratio of polyacrylamide, fumed silica, hollow glass microspheres, glass fiber, and water is within the above range, they can be uniformly mixed and molded, balancing mechanical and thermal insulation properties.

[0033] In conjunction with the first aspect, in some embodiments provided in this application, the inorganic ceramic material includes nano-silica, an infrared shielding agent, ceramic fibers, and a binder. Nano-silica can improve the material's thermal insulation performance. The infrared shielding agent can reduce high-temperature infrared radiation. Ceramic fibers can improve the material's mechanical strength. The binder can improve the interaction between nanoparticles, which is beneficial for molding. The infrared shielding agent includes, but is not limited to, at least one of silicon carbide, titanium dioxide, and nano-carbon black. The ceramic fibers include, but are not limited to, at least one of alumina ceramic fibers, zirconia ceramic fibers, and mullite ceramic fibers. The binder includes, but is not limited to, at least one of silica sol, water glass, carboxymethyl cellulose, and polyvinyl alcohol.

[0034] In conjunction with the first aspect, in some embodiments provided in this application, the mass ratio of nano-silica, infrared shading agent, ceramic fiber, and adhesive is (60~80):(4~8):(5~10):(3~6). Within this range, the mass ratio of nano-silica, infrared shading agent, ceramic fiber, and adhesive can impart excellent thermal insulation properties and mechanical strength to the composite material.

[0035] In conjunction with the first aspect, in some embodiments provided in this application, the phase change heat dissipation layer 2 accounts for 25% to 45% of the thickness of the heat insulation layer 1.

[0036] In conjunction with the first aspect, in some embodiments provided in this application, the thickness of the phase change heat dissipation layer 2 is 0.8mm to 2.0mm; the thickness of the phase change heat dissipation layer 2 is within this range, which can be adapted to the integral molding process, and the composite material has sufficiently high mechanical strength and thermal insulation performance.

[0037] In conjunction with the first aspect, in some embodiments provided in this application, the thickness of the heat insulation layer 1 is 1.8~6.0mm. The thickness of the heat insulation layer 1 within this range can adapt to the current spacing between energy storage batteries and power batteries, ensuring sufficient heat insulation safety redundancy.

[0038] In conjunction with the first aspect, in some embodiments provided in this application, the hydrogel is encapsulated by a gas- and water-resistant material to form a phase change heat dissipation layer 2. Encapsulating the hydrogel with a water-resistant material prevents moisture evaporation during normal use, while allowing internal water vapor to break through the edges of the encapsulation material (which are formed by two pieces of encapsulation material heat-pressed together and can rupture under steam pressure) when the temperature rises (>100°C), thus achieving heat dissipation. The gas- and water-resistant material can be at least one of aluminum-plastic film, polyester film, and polyimide film.

[0039] In conjunction with the first aspect, in some embodiments provided in this application, the area ratio of the phase change heat dissipation layer 2 to the heat insulation layer 1 in the length and width directions is (0.7~0.95):1. Within this range, the phase change heat dissipation layer can be encased within the heat insulation layer, adapting to an integrated molding process. Multiple functional modules can be integrated, resulting in enhanced overall mechanical strength and flexibility, and high production efficiency. In contrast, a simple physical stacking structure of heat insulation layer / intermediate layer / heat insulation layer will have its overall thermal conductivity increased due to the intermediate layer, reducing its heat insulation performance. Furthermore, the surface of the heat insulation layer has a porous nanostructure, low surface energy, and the presence of loose powder, making it difficult to bond with the intermediate layer material to form a unified whole.

[0040] Because the phase change heat dissipation layer 2 is wrapped inside the insulation layer 1, and the phase change heat dissipation layer 2 is surrounded by the material of the insulation layer 1, the phase change heat dissipation layer 2 is embedded inside the insulation layer 1 like a sandwich. The water inside the phase change heat dissipation layer 2 material, as a phase change component, vaporizes at high temperature (above 100℃ at normal pressure) and carries away a large amount of heat. At the same time, the remaining polymer skeleton and inorganic mixture still have good thermal insulation performance, and its thermal conductivity is close to 0.03W / m·K.

[0041] Specifically, a 1mm thick layer of heat insulation layer 1 powder (containing nano-silica, infrared shielding agent, ceramic fiber and adhesive in a mass ratio of 72:5:8:5, pre-mixed evenly) can be laid flat in a cuboid mold. Then, a 1mm thick layer of phase change heat dissipation material (containing polyacrylamide, fumed silica, hollow glass microspheres, glass fiber and water in a mass ratio of 10:6:12:4:68, pre-mixed evenly) can be placed in the aluminum-plastic film-encapsulated layer. Then, a 1mm thick layer of heat insulation layer 1 powder can be laid flat on the surface of the heat dissipation material. The thickness of the powder can be controlled by the feeding weight of the mixed powder and the depth of the vertical displacement of the mold. Finally, the material is molded into a single piece using a press at a room temperature of 25℃. The sheet is then encapsulated with PET double-sided adhesive to form the final heat insulation heat dissipation plate.

[0042] Both the insulation layer 1 and the phase change heat dissipation layer 2 (after phase change) have extremely low thermal conductivity, effectively blocking heat transfer. When heat is transferred to the phase change heat dissipation material, the temperature reaches 100℃~110℃. The water in the intermediate gel undergoes a phase change, vaporizes, and breaks through the aluminum-plastic film from the edges, carrying away a large amount of heat and cooling the heat source of the device. Simultaneously, the remaining polymer and inorganic components still have good thermal insulation properties (the thermal conductivity of the dry phase change heat dissipation layer is 0.03 W / (m·K)), having a limited impact on the overall high thermal insulation performance of the material. Based on the insulation board, a composite material with thermal insulation and heat dissipation functions is integrally molded. This design not only endows the insulation material with heat dissipation performance, but also breaks through the barrier limit of existing insulation boards under the same thickness conditions, further reducing the heat source temperature and shortening the duration of higher temperatures through heat dissipation, protecting adjacent devices. Furthermore, due to the flexibility of the intermediate hydrogel material, the overall thermal insulation and heat dissipation material has a certain degree of compressibility, mechanically adapting to the contraction and expansion changes during battery cycle charging and discharging, thus protecting the battery cell.

[0043] Secondly, this application provides a secondary battery, such as Figure 3 The diagram shows a plurality of battery cells 200 and a heat-insulating heat dissipation plate 100 as described in the first aspect, disposed between adjacent battery cells 200.

[0044] Thirdly, this application provides an electrical device including the secondary battery described in the second aspect.

[0045] The present application will be described below with reference to specific embodiments.

[0046] Example 1 A heat-insulating and heat-dissipating panel includes a heat-insulating layer and a phase-change heat-dissipating layer encased within the heat-insulating layer, wherein: The heat insulation layer is made of nano-silica, infrared shading agent (silicon carbide), ceramic fiber (alumina ceramic fiber) and adhesive (silica sol) in a mass ratio of 60:8:10:6, and has a thickness of 1.8 mm. The phase change heat dissipation layer is made of polyacrylamide, fumed silica, hollow glass microspheres, glass fiber and water in a mass ratio of 10:6:15:6:63, with a thickness of 0.8 mm, and is encapsulated by a 0.2 mm thick aluminum-plastic film. The ratio of the area of ​​the phase change heat dissipation layer to that of the insulation layer on the insulation surface is 0.7:1.

[0047] Example 2 A heat-insulating and heat-dissipating panel includes a heat-insulating layer and a phase-change heat-dissipating layer encased within the heat-insulating layer, wherein: The heat insulation layer is made of nano-silica, infrared shading agent (titanium dioxide), ceramic fiber (zirconia ceramic fiber), and adhesive (water glass) in a mass ratio of 80:4:5:3, and has a thickness of 6.0 mm. The phase change heat dissipation layer is made of polyacrylamide, fumed silica, hollow glass microspheres, glass fiber and water in a mass ratio of 10:10:10:4:60, with a thickness of 2.0 mm, and is encapsulated by a 0.3 mm thick polyimide film. The ratio of the area of ​​the phase change heat dissipation layer to that of the heat insulation layer on the heat insulation surface is 0.95:1.

[0048] Example 3 A heat-insulating and heat-dissipating panel includes a heat-insulating layer and a phase-change heat-dissipating layer encased within the heat-insulating layer, wherein: The heat insulation layer is made of nano-silica, infrared shading agent (nano-carbon black), ceramic fiber (mullite ceramic fiber) and adhesive (water glass) in a mass ratio of 70:5:8:5, and has a thickness of 3.6 mm. The phase change heat dissipation layer is made of polyacrylamide, fumed silica, hollow glass microspheres, glass fiber and water in a mass ratio of 10:8:15:5:70, with a thickness of 1.8 mm, and is encapsulated by a 0.25 mm thick polyester film. The ratio of the area of ​​the phase change heat dissipation layer to that of the insulation layer on the insulation surface is 0.8:1.

[0049] Example 4 A heat-insulating and heat-dissipating panel includes a heat-insulating layer and a phase-change heat-dissipating layer encased within the heat-insulating layer, wherein: The heat insulation layer is made of nano-silica, infrared shading agent (silicon carbide), ceramic fiber (alumina ceramic fiber) and adhesive (silica sol) in a mass ratio of 55:10:15:10, and has a thickness of 0.5 mm. The phase change heat dissipation layer is made of polyacrylamide, fumed silica, hollow glass microspheres, glass fiber and water in a mass ratio of 10:5:8:2:55, with a thickness of 1.5 mm, and is encapsulated by a 0.2 mm thick aluminum-plastic film. The ratio of the area of ​​the phase change heat dissipation layer to that of the insulation layer on the insulation surface is 0.6:1.

[0050] Example 5 A heat-insulating and heat-dissipating panel includes a heat-insulating layer and a phase-change heat-dissipating layer encased within the heat-insulating layer, wherein: The heat insulation layer is made of nano-silica, infrared shading agent (silicon carbide), ceramic fiber (alumina ceramic fiber) and adhesive (silica sol) in a mass ratio of 85:3:3:2, and has a thickness of 4.0 mm. The phase change heat dissipation layer is made of polyacrylamide, fumed silica, hollow glass microspheres, glass fiber and water in a mass ratio of 10:15:25:10:80, with a thickness of 1.0 mm, and is encapsulated by a 0.2 mm thick aluminum-plastic film. The ratio of the area of ​​the phase change heat dissipation layer to that of the insulation layer on the insulation surface is 0.99:1.

[0051] Comparative Example 1 Similar to Example 4, except that it does not contain a phase change heat dissipation layer.

[0052] Comparative Example 2 Similar to Example 4, the difference is that the internal phase change heat dissipation layer is made of aerogel (specifically, a ceramic fiber aerogel plate), which does not contain water.

[0053] Comparative Example 3 Similar to Example 4, the difference is that the phase change heat dissipation layer is a single piece disposed on one side of the heat insulation plate.

[0054] Performance testing The heat insulation and heat dissipation plates of Examples 1 to 5 and Comparative Examples 1 to 3 were subjected to performance tests. The test methods were as follows: Thermal conductivity measurement: A 10W constant-temperature heating element was used to test the room-temperature thermal insulation performance. The heating element was horizontally attached to the heat insulation and heat dissipation plate (10...). 10 0.25cm), with a room-temperature aluminum block (with 25℃ circulating water inside) attached to the other side, and left to stand until the temperature and heat reach a steady state. Thermocouples were used to track and record the temperatures of the hot and cold sides of the heat insulation board. Using Fourier's law, the overall thermal conductivity λ of the heat insulation board was calculated. The formula is λ = (Q / Q) d) / (A (T1-T2)), where Q is the heat flow rate, d is the material thickness, A is the cross-sectional area of ​​the material in the direction of heat flow, T1 is the surface temperature of the hot side of the material, and T2 is the surface temperature of the cold side of the material.

[0055] Material compression properties: The self-made heat insulation and heat dissipation plate (100...) 100 A 2.5mm thick insulation board served as the experimental group, while a commercially available insulation board of the same size served as the standard control group. A universal testing machine was used to vertically compress the specimens at a constant speed of 2 mm / min, ensuring the pressure contact surface was flat and aligned to avoid eccentric force errors. Load and deformation data for both groups of specimens were collected synchronously throughout the process. The deformation changes of the two groups of samples at compressive stresses of 1 MPa and 3 MPa were compared, and the calculation formula was ε = L1 / L0, where L1 is the compression amount of the material under a fixed pressure, and L0 is the initial thickness of the material.

[0056] Simulated battery thermal runaway hot bench test: The temperature of the heating plate was raised to 650℃, and then the heat insulation plate (286) was placed on the heat dissipation plate. 216 A 2.5 mm sample was placed on a heating plate and compressed using a press to maintain a pressure of 1 MPa. Heating of the heating plate was then stopped. Thermocouples were placed at the center of the top and bottom of the insulation plate to track and record the temperature changes on both sides of the sample. After stabilization for 10 minutes, the temperature difference ΔT between the top and bottom surfaces was recorded, representing the material's insulation effect under high-temperature conditions. Commercially available insulation boards and aerogel of the same size were selected as control groups. The calculation formula was ΔT = T1 - T2, where T1 and T2 were the temperatures of the hot and cold sides of the material after 10 minutes of stabilization, respectively.

[0057] The test results are shown in Table 1.

[0058] Table 1. Performance of the heat insulation panels in Examples 1 to 5 and Comparative Examples 1 to 3

[0059] As shown in Table 1, Examples 1 to 5 exhibit significant advantages in overall performance, including low thermal conductivity, compressibility, and a large thermal insulation temperature difference. Example 3, due to the moderate thickness of its insulation and phase change heat dissipation layers, demonstrates low thermal conductivity and balanced compressibility at room temperature, resulting in slightly better overall thermal insulation performance than Examples 1 to 2. Example 5, with its lower thickness of the phase change heat dissipation layer, has slightly worse compressibility and thermal insulation performance than Examples 1 to 4, but its overall performance is still superior to Comparative Examples 1 to 3.

[0060] It should be noted that the hydrogel phase change heat dissipation layer in this application has an extremely low thermal conductivity (close to 0.03 W / m·K) at room temperature, and it is also an excellent heat insulation material. Its heat dissipation function is not achieved through high thermal conductivity, but through the latent heat of phase change of internal moisture at high temperature. During normal battery operation at room temperature, the outer inorganic ceramic insulation layer effectively blocks the lateral transfer of heat from the battery cell due to its extremely low thermal conductivity. At the same time, the moisture encapsulated in the inner hydrogel by the gas- and water-barrier material is completely locked in, preventing moisture loss due to evaporation under normal operating conditions. However, when the battery cell experiences thermal runaway and the temperature rises above 100°C, heat penetrates the insulation layer and is transferred to the hydrogel phase change heat dissipation layer. This triggers a phase change from liquid to gas in the water inside the hydrogel, absorbing a large amount of latent heat. The resulting water vapor breaks through the edges of the encapsulation material and is released directionally, thus rapidly carrying the heat away from the heat source area in the form of latent heat, providing active cooling for the thermally runaway battery cell. During this process, the polymer skeleton and inorganic mixture remaining in the hydrogel maintain structural integrity and continue to play an insulating role, preventing heat from spreading further to adjacent battery cells. Due to the inherent flexibility and compressibility of hydrogel materials, the entire heat insulation and heat dissipation plate possesses a certain elastic deformation capability in the thickness direction, which can adaptively match the contraction and expansion of the battery cell during cyclic charging and discharging, thereby providing buffer protection for the battery cell at the mechanical level. The heat insulation layer, phase change heat dissipation layer, encapsulation structure, material composition, and the resulting triple functions of heat insulation, heat dissipation, and compressive deformation form a synergistic relationship.

[0061] Comparative Example 1 lacks a phase change heat dissipation layer, therefore the material has no toughness and is almost incompressible.

[0062] Comparative Example 2 shows that since the phase change heat dissipation layer is made of aerogel (specifically, ceramic fiber aerogel board), it does not contain water and cannot dissipate heat. Therefore, the material's compressibility is significantly reduced. Due to the lack of heat dissipation performance, the overall heat insulation effect of the aerogel material is worse than that of the heat dissipation insulation board.

[0063] In Comparative Example 3, the phase change heat dissipation layer is located on one side of the heat insulation plate, thus retaining the compression performance. However, the heat dissipation plate will immediately burst when it comes into direct contact with the heat source (working prematurely), making heat insulation and heat dissipation uncontrollable, and the overall heat dissipation and cooling results are low.

[0064] In summary, by setting a hydrogel phase change heat dissipation layer inside the heat insulation layer of inorganic ceramic materials, the heat insulation board can be endowed with heat dissipation and cooling functions, improving the overall performance of the material. Due to the presence of hydrogel heat dissipation material, it is compressible, solving the problem of the incompressibility of traditional heat insulation boards and adapting to the contraction and expansion of the battery cell.

[0065] The terms "comprising" and "having," and any variations thereof, in the specification and claims of this application are intended to cover non-exclusive inclusion. For example, a process, method, apparatus, product, or device that includes a series of steps or units is not limited to the listed steps or units, but may optionally include steps or units not listed, or may optionally include other steps or units inherent to such process, method, product, or device. The terms "first," "second," and "third," etc., are used to distinguish different objects, etc., and do not indicate a sequence, nor do they limit "first," "second," and "third" to different types.

[0066] In the description of the embodiments of this application, terms such as "exemplary," "for example," or "for instance" are used to indicate examples, illustrations, or explanations. Any embodiment or design described as "exemplary," "for example," or "for instance" in the embodiments of this application should not be construed as being more preferred or advantageous than other embodiments or designs. Specifically, the use of terms such as "exemplary," "for example," or "for instance" is intended to present the relevant concepts in a concrete manner.

[0067] In the description of the embodiments of this application, unless otherwise stated, " / " means "or". For example, A / B can mean A or B. The "and / or" in the text is merely a description of the relationship between related objects, indicating that there can be three relationships. For example, A and / or B can mean: A exists alone, A and B exist simultaneously, and B exists alone. In addition, in the description of the embodiments of this application, "multiple" means two or more.

[0068] The above are merely preferred embodiments of this application and do not limit the patent scope of this application. Any equivalent structural or procedural transformations made using the content of this application's specification, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of this application.

Claims

1. A heat-insulating and heat-dissipating plate, characterized in that, It includes a heat insulation layer and a phase change heat dissipation layer wrapped inside the heat insulation layer, wherein: The material of the heat insulation layer includes inorganic ceramic materials; The material of the phase change heat dissipation layer includes hydrogel; The thermal conductivity of the heat insulation and heat dissipation plate at 25℃ is 0.020~0.045W / (m·K).

2. The heat insulation and heat dissipation plate as described in claim 1, characterized in that, The phase change heat dissipation layer is made of polyacrylamide, fumed silica, hollow glass microspheres, glass fiber, and water.

3. The heat insulation and heat dissipation plate as described in claim 2, characterized in that, The mass ratio of polyacrylamide, fumed silica, hollow glass microspheres, glass fiber and water is 10:(6~10):(10~20):(4~8):(60~75).

4. The heat insulation and heat dissipation plate as described in claim 1, characterized in that, The inorganic ceramic material includes nano-silica, infrared shielding agent, ceramic fiber and adhesive.

5. The heat insulation and heat dissipation plate as described in claim 4, characterized in that, The mass ratio of nano-silica, infrared shading agent, ceramic fiber and adhesive is (60~80): (4~8): (5~10): (3~6).

6. The heat insulation and heat dissipation plate as described in claim 1, characterized in that: The phase change heat dissipation layer accounts for 25% to 45% of the thickness of the insulation layer; and / or, The thickness of the phase change heat dissipation layer is 0.8mm~2.0mm; and / or, The thickness of the insulation layer is 1.8~6.0mm.

7. The heat insulation and heat dissipation plate as described in claim 1, characterized in that, The hydrogel is encapsulated by an air- and water-proof material to form a phase change heat dissipation layer.

8. The heat insulation and heat dissipation plate as described in claim 7, characterized in that, The hydrogel phase change heat dissipation layer and the inorganic ceramic material are integrally molded, and the area ratio of the phase change heat dissipation layer to the heat insulation layer in the length and width directions is (0.7~0.95):

1.

9. A secondary battery, characterized in that, It includes multiple battery cells and a heat-insulating heat dissipation plate as described in any one of claims 1 to 8 disposed between adjacent battery cells.

10. An electrical device, characterized in that, Includes the secondary battery as described in claim 9.