A self-powered optical communication node based on quantum dot fluorescent solar concentrators
By combining quantum dot fluorescent solar concentrators with photodetectors and solar cells, the problems of existing LSC optical receivers being unable to be self-powered and fabricated on a large scale have been solved, achieving efficient and low-cost optical signal reception, suitable for distributed and mobile communication nodes.
Patent Information
- Application Number
- CN202611525069.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-29
- Publication Date
- 2026-11-17
AI Technical Summary
Existing LSC optical receivers cannot achieve self-powered operation and are difficult to fabricate on a large scale at low cost, which limits their application in distributed, mobile, and maintenance-free scenarios.
A quantum dot-based fluorescent solar concentrator is used to absorb and re-emit light signals using quantum dot luminescent materials. Combined with total internal reflection of the polymer waveguide layer and photodetectors and solar cells at the edge, it achieves self-sufficiency in energy and signal reception.
It achieves large-area, high-efficiency, and wide-field-of-view optical signal reception without increasing the area of the receiving device, while reducing system complexity and maintenance costs.
Smart Images

Figure CN123122680A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the fields of visible light communication and optical wireless communication receiving technology, specifically to a quantum dot-based fluorescent solar concentrator optical receiver, a self-powered optical communication node including the optical receiver, and a method for fabricating the optical receiver. Background Technology
[0002] In visible light communication (VLC), high-speed photodetectors require small active area to reduce junction capacitance and increase modulation bandwidth. However, small-area detectors can only receive photons within a narrow receiving cone. Therefore, existing receivers typically rely on bulky optical lens assemblies or complex nanostructures, which limit the field of view and require precise alignment, making them unsuitable for the random, dynamic geometric positions of indoor mobile terminals. Light-sensitive solar concentrators (LSCs) collect and concentrate omnidirectional incident light from a large surface onto a compact device located at the edge of a waveguide plate through an absorption-re-emission-total internal reflection mechanism, achieving large-area, wide-field-of-view light collection without increasing the receiver area. Using colloidal quantum dots as the luminescent material in LSCs leverages their tunable spectral characteristics and high photostability. However, existing LSC optical receivers typically only receive the optical signal; the node itself still relies on an external power source or independent battery, increasing system size, wiring complexity, and maintenance costs, limiting their application in distributed, mobile, and maintenance-free scenarios. Furthermore, the fabrication processes for existing LSC optical receivers still require improvement in terms of large-area, low-cost, and scalable capabilities.
[0003] Therefore, there is an urgent need for an optical communication node capable of self-sufficiency in energy supply using LSC edge-coupled solar cells, as well as a quantum dot-based LSC optical receiver structure and its fabrication method that can be fabricated on a large area at low cost. In summary, developing a large-area, high-efficiency, high-stability, and wide-bandwidth fluorescent solar concentrator optical receiver has significant application value. Summary of the Invention
[0004] This invention aims to solve the technical problems of existing LSC optical receivers being unable to achieve self-powered energy supply and being difficult to fabricate in large areas at low cost, and provides a quantum dot-based LSC optical receiver, a self-powered optical communication node and its fabrication method.
[0005] Based on this, the present invention provides a quantum dot-based LSC optical receiver. It includes a polymer waveguide layer, quantum dot luminescent material dispersed within the polymer waveguide layer, a photodetector disposed at the edge of the polymer waveguide layer, and a solar cell disposed at the edge of the polymer waveguide layer. The quantum dot luminescent material is selected from one or more of group II-VI core-shell nanocrystals, group I-III-VI copper-based ternary quantum dots, and carbon quantum dots. Incident light is absorbed by the quantum dots and re-emitted as fluorescence. The fluorescence is guided to the edge by total internal reflection, converted into a communication electrical signal by the photodetector, and then converted into electrical energy by the solar cell.
[0006] The self-powered optical communication node uses LSC edge-coupled solar cells to convert fluorescence into electrical energy, achieving self-powered energy supply while receiving communication signals. It does not require an external power source or independent battery, which helps reduce system complexity, wiring costs, and maintenance costs.
[0007] The optical receiver uses quantum dots as the light-emitting material, and its absorption and emission spectra can be modulated by selecting group II-VI core-shell nanocrystals, group I-III-VI copper-based ternary quantum dots, and carbon quantum dots to adapt to different light sources and communication bands; among them, carbon dots are free of heavy metals, have a wide range of raw material sources, low cost, and are environmentally friendly.
[0008] This invention provides a self-powered optical communication node, comprising the aforementioned optical receiver, an energy management module connected to a solar cell, and a communication signal processing module connected to a photodetector. The electrical energy output from the solar cell powers the node via the energy management module, and the electrical signal output from the photodetector is demodulated by the communication signal processing module to recover communication data.
[0009] The optical receiver utilizes total internal reflection within the polymer waveguide layer to concentrate a large area of wide-field incident light onto a small area of high-speed photodetector, achieving wide-field reception while ensuring high modulation bandwidth.
[0010] The present invention provides a method for fabricating the above-mentioned optical receiver, wherein a polymer waveguide layer is formed by a blade coating method and a UV polymerization method, and a photodetector and a solar cell are disposed at the edge of the waveguide layer.
[0011] The optical receiver is fabricated using a combination of blade coating and ultraviolet polymerization, which is a simple and highly scalable process that facilitates the realization of large-area, low-cost LSC optical receivers.
[0012] The properties of some of the materials and devices involved in this invention are as follows: Figure 1 This is a schematic diagram of the structure of the quantum dot-based fluorescent solar concentrator optical receiver of the present invention.
[0013] Figure 2 This is a block diagram of the self-powered optical communication node of the present invention.
[0014] Figure 3 The images show the absorption and emission spectra of the quantum dots of this invention.
[0015] Figure 4 This is a fluorescence lifetime diagram of the quantum dot material of the present invention.
[0016] Figure 5 This is a graph showing the photoelectric conversion efficiency of the fluorescent solar concentrator of the present invention.
[0017] Figure 6 This is the frequency response diagram of the light receiver end of the fluorescent solar concentrator based on the present invention. Detailed Implementation
[0018] To elaborate on the technical implementation path of the present invention, the following will further describe the implementation methods of the present invention in conjunction with specific embodiments. It should be noted that the selection of the following embodiments is intended to illustrate the technical solution of the present invention in a verifiable manner, and its core function is to provide clear technical understanding and application guidance for those skilled in the art, rather than to limit the scope of protection of the claims of the present invention through enumeration.
[0019] It should be particularly noted that, unless otherwise specified, the process methods, testing procedures, or experimental operations cited in the embodiments and comparative examples of this invention refer to common technical means known in the art; the names of process steps, abbreviations of materials, and other expressions involved are all standard terms widely recognized in this technical field. Relevant practitioners can accurately call upon known technical paths based on the above-mentioned common names and complete specific implementations according to industry standard operating procedures or guidance parameters provided by equipment suppliers.
[0020] The present invention will be further described in detail below with reference to the accompanying drawings and embodiments. The following embodiments are for illustrative purposes only and should not be construed as limiting the scope of protection of the present invention. Example Example 1
[0021] Step 1: Preparation of Group II-VI: CdSe / CdZnS core-shell nanocrystals: A mixture of CdO (1 mmol), TOPO (8 mmol), ODPA (1 mmol), and HPA (1 mmol) was placed in a three-necked round-bottom flask and degassed at 150 °C for 1 h. Under a nitrogen atmosphere, the mixture was heated to 300 °C and held for 10 min to dissolve CdO. The temperature was then lowered to 280 °C–350 °C, and a selenium precursor solution (1 mmol Se powder dissolved in 0.5 mL TOP and 0.1 mL DPP) was rapidly injected. After stirring for 1.5 min, the solution was cooled to 50 °C and diluted with hexane (3 mL). After further cooling to room temperature, the product was precipitated with ethanol. Finally, the CdSe NRs dissolved in TOP to obtain a clear stock solution (0.1 mg / mL), which was stored in the dark under nitrogen. CdO (0.24 mmol), TOPO (8 mmol), ODPA (0.8 mmol), and HPA (0.48 mmol) were mixed in a flask and degassed at 150°C for 60 min with vigorous stirring. The suspension was then heated to 350°C under N2. TOP (1.8 mL) was injected, and the temperature was allowed to return to 350°C. Then, the S precursor solution (2.1 mmol of sulfur powder dissolved in 2.5 mL of TOP) and the CdSeNRs seed solution (0.1 mL) were rapidly injected. Immediately afterwards, the Zn-OA solution (5 mmol of Zn(Ac)2 dissolved in 5 mL of ODE and 5 mL of OA) was added at a rate of 0.2 mL / min. After the addition was complete, the reaction was allowed to continue for 40 min. The flask was then cooled to room temperature. The resulting mixture was diluted with hexane (5 mL), and the product was precipitated by adding ethanol, followed by centrifugation. Finally, the CdSe / CdZnS nanocrystals were redissolved in hexane. The prepared nanocrystals have a fluorescence quantum efficiency of 99.7% and a fluorescence lifetime of 14.18 ns.
[0022] Step 2: Preparation of CdSe / CdZnS core-shell structured nanocrystalline fluorescent solar concentrator: First, CdSe / CdZnS quantum dots dispersed in n-hexane were evaporated to a dry powder state. Then, lauryl methacrylate and ethylene glycol dimethacrylate were mixed at a mass ratio of 4:1. A photoinitiator (0.5 wt%) was added to this solution, and the mixture was sonicated until a clear solution was obtained. This solution was then injected into a flask containing 50 mg of CdSe / CdZnS quantum dot dry powder, and the mixture was sonicated to ensure uniform dispersion, followed by continuous stirring for 6 hours to ensure complete homogenization. The mixture was then injected into a mold consisting of two glass plates (with approximately 1 mm thick rubber blocks at the four corners of the glass plates for spacing). Photopolymerization was performed under 365 nm ultraviolet light for 30 minutes, followed by a 3-hour dark curing treatment to obtain the CdSe / CdZnS fluorescent solar concentrator.
[0023] Step 3: Couple solar cells to the four side edges of the prepared fluorescent solar concentrator, and leave a small portion of the side edges to couple photodetectors. Use NOA68 refractive index matching glue for coupling. The back-end module of the photodetector is powered by the coupled solar cells, ultimately realizing a large-area visible light communication receiving node with "net zero energy consumption". Example 2
[0024] Step 1: Preparation of Group I-III-VI copper-based ternary quantum dots CuInS2 / ZnS: First, 1 mmol of zinc acetate, 2 ml of dodecyl mercaptan, and 8 ml of oleic acid were placed in a three-necked flask, heated to 70°C, and evacuated for 20 minutes. The temperature was then slowly increased to 110°C, and nitrogen gas was introduced to maintain the solution at 110°C, thus completing the preparation of the precursor solution. Separately, 1 mmol of cuprous iodide, 1 mmol of indium acetate, and 10 ml of dodecyl mercaptan were placed in a three-necked flask, evacuated at room temperature for 30 minutes, and slowly heated to 110°C. After purging with nitrogen gas, the temperature was rapidly increased to 230°C. Once the temperature reached 230°C, the incubated precursor solution was rapidly injected, and the solution was maintained at 230°C for one hour. After cooling, the resulting solution was centrifuged to obtain CuInS2 / ZnS quantum dots, which were then dissolved in hexane to obtain a CuInS2 / ZnS quantum dot hexane solution. The prepared quantum dots have a fluorescence quantum efficiency of 98.8% and a fluorescence lifetime of 343 ns.
[0025] Step 2: Preparation of CuInS2 / ZnS fluorescent solar concentrator: First, CuInS2 / ZnS quantum dots dispersed in n-hexane were evaporated to a dry powder state. Then, lauryl methacrylate and ethylene glycol dimethacrylate were mixed at a mass ratio of 4:1. A photoinitiator (0.5 wt%) was added to this solution, and the mixture was sonicated until a clear solution was obtained. This solution was then injected into a flask containing 50 mg of CuInS2 / ZnS quantum dot dry powder, and the mixture was sonicated to ensure uniform dispersion, followed by continuous stirring for 12 hours to ensure complete homogenization. The mixture was then injected into a mold consisting of two glass plates (with approximately 1 mm thick rubber blocks at the four corners of the glass plates for spacing). Photopolymerization was performed under 365 nm UV light for 30 minutes, followed by a 3-hour dark curing treatment to obtain the CuInS2 / ZnS fluorescent solar concentrator.
[0026] Step 3: Couple solar cells to the four side edges of the prepared fluorescent solar concentrator, and leave a small portion of the side edges to couple photodetectors. Use NOA68 refractive index matching glue for coupling. The back-end module of the photodetector is powered by the coupled solar cells, ultimately realizing a large-area visible light communication receiving node with "net zero energy consumption". Example 3
[0027] Step 1: Preparation of carbon quantum dots: 0.03g of PDA molecules, 1.2g of urea, and 0.6g of boric acid were placed in a beaker and mixed thoroughly. The beaker was then placed in an oven and heated to 200℃ for six hours. After cooling, a large amount of ultrapure water was added to the beaker. The resulting solution was centrifuged to obtain an aqueous solution of carbon quantum dots. The aqueous solution of carbon quantum dots was dialyzed to obtain an impurity-free aqueous solution of carbon quantum dots, which was then lyophilized to obtain carbon quantum dot powder. The prepared carbon quantum dots had a fluorescence quantum efficiency of 99.3% and a fluorescence lifetime of 5.54 ns.
[0028] Step 2: Preparation of the carbon quantum dot fluorescent solar concentrator: First, take an appropriate amount of carbon quantum dot powder, dissolve it in a methanol solution, and sonicate it to obtain a transparent solution. Take 10 ml of the carbon quantum dot methanol solution, add 1600 mg of polyvinylpyrrolidone mixture to the solution, and stir continuously for 24 hours to ensure complete dissolution and mixing to obtain the appropriate solution. Use a blade coating method to evenly coat the solution onto a glass substrate. After the solvent has completely evaporated, the carbon quantum dot fluorescent solar concentrator is obtained.
[0029] Step 3: Couple solar cells to the four side edges of the prepared fluorescent solar concentrator, and leave a small portion of the side edges to couple photodetectors. Use NOA68 refractive index matching glue for coupling. The back-end module of the photodetector is powered by the coupled solar cells, ultimately realizing a large-area visible light communication receiving node with "net zero energy consumption".
[0030] Performance testing: Under AM 1.5G standard sunlight, the 5×5 cm sample prepared in Example 1... 2 The photoelectric conversion efficiency of the fluorescent solar concentrator reaches 3.69%; 15×15 cm 2 The photoelectric conversion efficiency of the fluorescent solar concentrator reaches 2.18%. The frequency response of the device can reach 5 MHz, with a theoretical limit of 27 MHz. It exhibits stable performance in accelerated aging tests and has great potential for large-scale practical applications in the field.
[0031] While the invention has been described herein with reference to specific embodiments, it should be understood that these embodiments are merely examples of the principles and applications of the invention. Therefore, it should be understood that many modifications can be made to the exemplary embodiments, and other arrangements can be designed without departing from the spirit and scope of the invention as defined by the appended claims. It should be understood that different dependent claims and features described herein can be combined in ways different from those described in the original claims. It is also understood that features described in conjunction with individual embodiments can be used in other described embodiments.
Claims
1. A quantum dot-based fluorescent solar concentrator optical receiver, characterized in that, include: Polymer waveguide layer; quantum dot luminescent material dispersed within the polymer waveguide layer; A photodetector located at the edge of the polymer waveguide layer; A solar cell disposed at the edge of the polymer waveguide layer; wherein the quantum dot luminescent material absorbs incident light and re-emits it as fluorescence, and the fluorescence undergoes total internal reflection within the polymer waveguide layer due to the refractive index difference between the polymer waveguide layer and the external environment and is guided to the edge of the polymer waveguide layer; The photodetector is used to convert fluorescence guided to the edge into communication electrical signals, and the solar cell is used to convert fluorescence guided to the edge into electrical energy.
2. The optical receiver according to claim 1, characterized in that, The quantum dot luminescent material is selected from one or more of the following: group II-VI core-shell nanocrystals, group I-III-VI copper-based ternary quantum dots, and carbon quantum dots.
3. The optical receiver according to claim 2, characterized in that, The quantum dot luminescent material is a II-VI core-shell structured nanocrystal.
4. The optical receiver according to claim 2, characterized in that, The quantum dot luminescent material is a group I-III-VI copper-based ternary quantum dot.
5. The optical receiver according to claim 2, characterized in that, The quantum dot luminescent material is a carbon quantum dot.
6. The optical receiver according to claim 1, characterized in that, The photodetector is a high-speed photodetector, and the solar cell is a photovoltaic cell; the photodetector and the solar cell are located at different edges of the polymer waveguide layer, or in different regions of the same edge.
7. The optical receiver according to claim 1, characterized in that, The polymer waveguide layer is obtained by coating quantum dot luminescent material and polymer precursor into a film using a blade coating method and curing it using an ultraviolet polymerization method.
8. A self-powered optical communication node, characterized in that, include: A quantum dot-based fluorescent solar concentrator light receiver as described in any one of claims 1 to 7; and an energy management module connected to the solar cell; A communication signal processing module connected to the photodetector; wherein the solar cell converts fluorescence into electrical energy and outputs it to the energy management module, the energy management module is used to store the electrical energy and supply power to the self-powered optical communication node; the photodetector converts fluorescence into communication electrical signals and outputs them to the communication signal processing module, the communication signal processing module is used to demodulate the communication electrical signals to recover communication data.
9. The self-powered optical communication node according to claim 8, characterized in that, The energy management module includes an energy storage unit and a power management circuit. The energy storage unit is used to store the electrical energy output by the solar cell, and the power management circuit is used to supply power to the communication signal processing module.
10. The self-powered optical communication node according to claim 8, characterized in that, The incident light is visible light, and the self-powered optical communication node is a visible light communication node.