A stress-relief structural layer, a flexible cover plate, a substrate, and an electronic device.

By employing a design that combines the protrusions and cavities of the first and second stress buffer layers in the flexible cover plate, stress during bending is buffered, solving the problem of wrinkles easily appearing after frequent bending and improving the durability of the flexible cover plate.

CN123124236APending Publication Date: 2026-11-17HEFEI VISIONOX TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510638217.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-16
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Flexible cover plates are prone to wrinkles after frequent bending, making it difficult to release stress.

Method used

The first stress buffer layer and the second stress buffer layer are stacked together. The protrusions and the cavity cooperate to form a stress buffer structure layer. When bending, the protrusions and the cavity fit together to buffer the stress.

Benefits of technology

Effectively buffers the stress of the flexible cover during bending, prevents wrinkles, and improves the durability of the flexible cover.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124236A_ABST
    Figure CN123124236A_ABST
Patent Text Reader

Abstract

This application provides a stress buffer structure layer, a flexible cover plate, a substrate, and an electronic device. The stress buffer structure layer includes a first stress buffer layer and a second stress buffer layer. The side of the first stress buffer layer facing the second stress buffer layer has a plurality of first protrusions arranged in an array, and a first cavity is provided between two adjacent rows of first protrusions. The side of the second stress buffer layer facing the first stress buffer layer has a plurality of second protrusions arranged in an array, and a second cavity is provided between two adjacent rows of second protrusions. The side of the first stress buffer layer facing the second stress buffer layer and the side of the second stress buffer layer facing the first stress buffer layer are in contact with each other so that the first protrusions and the second cavities cooperate to form a stress buffer structure layer. The stress buffer structure layer of this application can buffer the stress generated during the bending process of the flexible cover plate, thereby improving the problem that the flexible cover plate is prone to wrinkling after bending.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application belongs to the field of semiconductor manufacturing technology, and more specifically, relates to a stress-relief structural layer, a flexible cover plate, a substrate, and an electronic device. Background Technology

[0002] Flexible cover glass is a material with flexibility and bendability, widely used in flexible display terminals such as foldable screen phones and wearable devices. As a key protective component of the screen, flexible cover glass needs to have transparency, hardness, scratch resistance, flexibility, and resilience to meet the performance requirements of devices under frequent bending.

[0003] Due to the difficulty in releasing stress, flexible cover plates are prone to wrinkles after frequent bending. Summary of the Invention

[0004] In order to improve or solve the technical problem that flexible cover plates in related technologies are prone to wrinkling after frequent bending, the purpose of this application is to provide a stress buffer structure layer, a flexible cover plate, a substrate, and an electronic device.

[0005] In a first aspect, embodiments of this application provide a stress-buffering structural layer, comprising: a first stress-buffering layer and a second stress-buffering layer; the first stress-buffering layer and the second stress-buffering layer are stacked; the side of the first stress-buffering layer facing the second stress-buffering layer is provided with a plurality of first protrusions arranged in an array, and a first cavity is provided between two adjacent columns of the first protrusions; the side of the second stress-buffering layer facing the first stress-buffering layer is provided with a plurality of second protrusions arranged in an array, and a second cavity is provided between two adjacent columns of the second protrusions; the side of the first stress-buffering layer facing the second stress-buffering layer and the side of the second stress-buffering layer facing the first stress-buffering layer are in contact with each other, so that the first protrusions cooperate with the second cavities, and the second protrusions cooperate with the first cavities to form a stress-buffering structural layer; when the stress-buffering structural layer is bent, the first protrusions at the bend of the stress-buffering structural layer fit into the second cavities at the corresponding positions of the bend of the stress-buffering structural layer, and the second protrusions at the bend of the stress-buffering structural layer fit into the first cavities at the corresponding positions of the bend of the stress-buffering structural layer.

[0006] Furthermore, when the stress buffer structure layer is not bent, the first protrusion at each position of the first stress buffer layer is in movable engagement with the second cavity at the corresponding position of the second stress buffer layer, and the second protrusion at each position of the second stress buffer layer is in movable engagement with the first cavity at the corresponding position of the first stress buffer layer; there is a first space between the first protrusion at each position and the second cavity at the corresponding position, and there is a second space between the second protrusion at each position and the first cavity at the corresponding position.

[0007] Furthermore, the first protrusion has a first rectangular structure or a first toothed structure, and the second protrusion has a second rectangular structure or a second toothed structure; when the stress buffer structure layer is not bent, the first space is a first gap for movable engagement with the first rectangular structure or the first toothed structure; the second space is a second gap for movable engagement with the second rectangular structure or the second toothed structure.

[0008] Furthermore, the first protrusion has a first curved surface structure, and the second protrusion has a second curved surface structure; when the stress buffer structure layer is not bent, the first space is a third gap for movable cooperation with the first curved surface structure; the second space is a fourth gap for movable cooperation with the second curved surface structure.

[0009] Furthermore, the first stress buffer layer and the second stress buffer layer are made of flexible glass.

[0010] Secondly, embodiments of this application provide a flexible cover plate, comprising: a first protective layer, the stress buffer structure layer, and a second protective layer; the first protective layer, the first stress buffer layer, the second stress buffer layer, and the second protective layer are stacked.

[0011] Furthermore, the first protective layer, the first stress buffer layer, the second stress buffer layer, and the second protective layer are all made of flexible glass.

[0012] Thirdly, embodiments of this application provide a substrate including the stress buffer structure layer.

[0013] Fourthly, embodiments of this application provide an electronic device having a display screen, the display screen being provided with the flexible cover plate.

[0014] Furthermore, the display screen is a foldable screen.

[0015] This application provides a stress-buffering structural layer, a flexible cover plate, a substrate, and an electronic device. By employing a first stress-buffering layer with one side facing the second stress-buffering layer and a second stress-buffering layer with the other side facing the first stress-buffering layer in contact, a first protrusion engages with a second cavity, and the second protrusion engages with the first cavity to form a stress-buffering structural layer. When the stress-buffering structural layer is bent, the first protrusion at the bend of the stress-buffering structural layer fits into the second cavity at the corresponding position of the bend, and the fit between the second protrusion at the bend and the first cavity at the corresponding position of the bend buffers the stress between the first and second stress-buffering layers. This buffers the stress generated during the bending process of the flexible cover plate, thereby improving or solving the problem of wrinkles easily appearing on the flexible cover plate after frequent bending. Attached Figure Description

[0016] To more clearly illustrate the technical solutions in the embodiments of this application, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0017] Figure 1 This is a schematic diagram of the structure of the first stress buffer layer.

[0018] Figure 2 This is a schematic diagram of the second stress buffer layer.

[0019] Figure 3 This is a schematic diagram of the stress buffer structure layer.

[0020] Figure 4 This is a schematic diagram of the stress buffer structure layer under bending conditions.

[0021] Figure 5 This is a schematic diagram of the stress buffer structure layer in an embodiment when it is not bent.

[0022] Figure 6 This is a schematic diagram of the stress buffer structure layer under bending conditions in one embodiment.

[0023] Figure 7 This is a schematic diagram of the stress buffer structure layer in an unbent state in another embodiment.

[0024] Figure 8 This is a schematic diagram of the stress buffer structure layer under bending conditions in another embodiment.

[0025] Figure 9 This is a schematic diagram of the structure of each layer of the flexible cover plate.

[0026] The attached figures are labeled as follows:

[0027] 1-Stress buffer structure layer, 10-First stress buffer layer, 20-Second stress buffer layer, 11-First cavity, 12-First protrusion, 21-Second protrusion, 22-Second cavity; 100-Bend, 120-First stress buffer layer a, 210-Second stress buffer layer a, 122-First gap, 121-First toothed structure, 211-Second toothed structure, 221-Second gap, 1200-First stress buffer layer b, 2100-Second stress buffer layer b, 1201-First curved surface structure, 1202-Fourth gap, 2101-Third gap, 2102-Second curved surface structure, 2-First protective layer, 3-Second protective layer. Detailed Implementation

[0028] To make the technical problems, technical solutions, and beneficial effects to be solved by this application clearer, the following detailed description is provided in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and are not intended to limit the scope of this application.

[0029] It should be noted that when a component is referred to as being "fixed to" or "set on" another component, it can be directly on or indirectly on that other component. When a component is referred to as being "connected to" another component, it can be directly connected to or indirectly connected to that other component.

[0030] It should be understood that the terms "length", "width", "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this application.

[0031] Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of that feature. In the description of this application, "multiple" means two or more, unless otherwise explicitly specified.

[0032] As a core component of flexible display devices, the performance of flexible cover glass directly impacts the user experience of end products. With the rise of new materials such as UTG and advancements in processing technology, flexible cover glass will play an even more important role in consumer electronics, automotive displays, and smart wearables. Material innovation and process optimization will be key directions for the development of flexible cover glass technology.

[0033] Flexible cover glass is a material with flexibility and bendability, widely used in flexible display terminals such as foldable screen phones and wearable devices. As a key protective component of the screen, flexible cover glass needs to possess transparency, hardness, scratch resistance, flexibility, and resilience to meet the performance requirements of devices under frequent bending. Specifically:

[0034] Flexibility: It can withstand frequent folding and bending without cracking or breaking, ensuring that the screen can easily achieve various bending shapes.

[0035] Hardness and abrasion resistance: It must have a certain degree of hardness to resist scratches and wear during daily use, and prevent scratches from appearing on the screen surface, which would affect the display effect.

[0036] Optical performance: High light transmittance is key to ensure that light can pass through fully and present clear, vivid images and colors. At the same time, it also needs to have low reflectivity to reduce the interference of external light reflection on vision.

[0037] Impact resistance: When subjected to external impact, such as if the mobile phone is accidentally dropped, it can effectively buffer the impact force and protect the screen and internal display components from damage.

[0038] Chemical stability: Resistant to the corrosive effects of chemicals such as sweat, cosmetics, and detergents, preventing chemical reactions that could lead to a decline in material performance or changes in appearance.

[0039] Flexible cover glass is typically made of transparent polyimide film (CPI), ultra-thin flexible glass (UTG), or multifunctional polymer glass film materials (GLAM). The advantages of transparent polyimide film are: excellent flexibility, capable of withstanding numerous folds and bends; lightweight; good high-temperature resistance; mature mass production technology; and relatively low cost. The disadvantages are: it is prone to aging, and its performance may decline after long-term use; insufficient hardness, making the surface easily scratched; poor fingerprint resistance; and absorption of ultraviolet and blue light, resulting in a yellowish tint and affecting display quality. It was initially widely used in flexible display devices such as foldable phones and still retains certain advantages in some large-size flexible display fields, such as foldable laptops and rollable TVs.

[0040] The advantages of ultra-thin flexible glass (UTG) are: high light transmittance, providing a clearer visual effect; high hardness, strong wear and scratch resistance, and a good tactile feel; high temperature resistance, corrosion resistance, high strength, and good resilience, effectively solving problems such as creases and low rebound. The disadvantages are: the glass material itself is fragile, and although it has undergone thinning and flexibility treatment, its toughness is still insufficient, requiring care to avoid strong impacts and collisions with sharp objects during use. With technological advancements, it has gradually become the mainstream flexible cover material for foldable screens, widely used in foldable phones, rollable TVs, automotive displays, and other fields.

[0041] The advantages of multifunctional polymeric glass-like film (GLAM) materials are: combining the hardness of ultra-thin flexible glass (UTG) with the flexibility of transparent polyimide film (CPI), achieving a surface hardness of up to 9H, capable of withstanding millions of dynamic bends with a radius of 1.5mm, and withstanding tens of thousands of abrasion tests with steel wool without scratching. The disadvantages are: as a relatively new material, current production processes may be immature, and costs may be high. Currently, it has been validated by major domestic mobile phone brands in their latest foldable projects, and is expected to be widely used in the field of flexible displays in the future.

[0042] The manufacturing process for flexible covers has different requirements depending on the material. The manufacturing process for flexible covers using transparent polyimide film (CPI) as the raw material includes:

[0043] Raw material preparation: Dianhydrides and diamines are selected as monomer raw materials for the synthesis of polyimide. These raw materials must have high purity to ensure product quality. At the same time, appropriate solvents, such as N,N-dimethylformamide (DMF) and N-methylpyrrolidone (NMP), are prepared to dissolve the raw materials and for subsequent reactions.

[0044] Polymerization reaction: Dianhydride and diamine are added to a solvent in a specific molar ratio, and the polymerization reaction is carried out under specific temperature and stirring conditions to produce a polyamic acid (PAA) solution. During the reaction, parameters such as temperature, reaction time, and stirring speed need to be strictly controlled to obtain PAA with suitable molecular weight and properties.

[0045] Film Formation: The prepared PAA solution is uniformly coated onto a flat substrate, such as a stainless steel plate or silicon wafer, using methods such as casting or spin coating. The viscosity of the solution, coating thickness, and coating speed must be carefully controlled during the coating process to ensure the uniformity of the film.

[0046] Imidization treatment: The PAA-coated substrate is placed in an oven or high-temperature furnace for thermal imidization. At high temperatures, PAA molecules undergo a cyclization and dehydration reaction, transforming into polyimide. The thermal imidization temperature is typically between 200-400℃, with the holding time determined based on the specific material and process requirements. Alternatively, chemical imidization can be used, achieving imidization at lower temperatures by adding dehydrating agents and catalysts.

[0047] Post-processing: The formed polyimide film undergoes post-processing, including stretching and alignment, to improve its mechanical and optical properties. Stretching can be performed at specific temperatures and speeds to orient the molecular chains along the stretching direction, enhancing the film's strength and flexibility. Simultaneously, surface treatments can be applied, such as coating with anti-scratch or anti-reflective layers, to improve the film's surface properties.

[0048] The manufacturing process for flexible cover plates made from ultra-thin flexible glass (UTG) includes:

[0049] Glass substrate preparation: Using the float glass production process, glass raw materials (such as silica sand, soda ash, limestone, etc.) are mixed in a specific ratio, heated to a high-temperature molten state, and then formed onto the surface of molten tin using the float glass process, resulting in a glass substrate of uniform thickness. During this stage, strict control must be maintained over the purity of the raw materials, the melting temperature, and the forming process parameters to ensure the quality and performance of the glass substrate.

[0050] Thinning Process: The prepared glass substrate undergoes thinning treatment, commonly achieved through chemical etching and mechanical polishing. Chemical etching involves immersing the glass substrate in an etching solution, where a chemical reaction removes substances from the glass surface, resulting in thinning. The composition, concentration, temperature, and etching time of the etching solution significantly impact the thinning effect and the glass surface quality. Mechanical polishing utilizes polishing equipment, such as grinders or polishing machines, to mechanically remove the glass layer from the substrate surface, achieving thinning. During polishing, it is crucial to control parameters such as polishing pressure, speed, and polishing media to prevent scratches, cracks, and other defects on the glass surface.

[0051] Chemical strengthening involves immersing the thinned glass substrate in a molten salt containing potassium ions for ion exchange treatment. At high temperatures, sodium ions on the glass surface exchange with potassium ions in the molten salt, forming a compressive stress layer on the glass surface, thus improving its strength and toughness. The parameters for chemical strengthening, such as temperature, time, and molten salt composition, need to be optimized based on the glass's composition and thickness to achieve the best strengthening effect.

[0052] Cleaning and Inspection: The chemically strengthened glass is cleaned to remove residual molten salt and impurities from the surface. After cleaning, optical inspection equipment and mechanical property testing equipment are used to comprehensively test the glass's thickness, flatness, optical properties, strength, etc., and unqualified products are rejected.

[0053] The manufacturing process for flexible cover plates using multifunctional polymer glass film material (GLAM) as raw material includes:

[0054] Raw material synthesis and formulation design: First, polymer materials with specific structures and properties are synthesized. Simultaneously, the formulations of glass components and additives are designed based on product performance requirements. The synthesis of polymer materials typically involves polymerization reactions. By selecting appropriate monomers, initiators, and reaction conditions, the molecular weight, molecular structure, and properties of the polymer are controlled. The design of the glass component must consider the basic properties of glass, such as hardness, light transmittance, and thermal stability, as well as its compatibility and bonding with the polymer materials. The selection and dosage of additives also require precise control to achieve the material's multifunctionality, such as improving flexibility, wear resistance, and UV resistance.

[0055] Composite processes: These involve combining synthesized polymer materials with glass components through specific composite techniques. Common composite methods include solution mixing, co-extrusion, and coating. Solution mixing involves dissolving the polymer material in a suitable solvent, then mixing it uniformly with glass powder or sol, and finally solidifying the mixture by evaporating the solvent. Co-extrusion involves adding the polymer material and glass material separately to different extruders, fusing them together during extrusion to form a composite film. Coating involves applying glass sol or coating materials to the surface of the polymer film, followed by drying and curing to firmly bond the coating to the polymer film.

[0056] Molding and Processing: Based on the shape and size requirements of the final product, the composite material is molded and processed. For example, the material is made into the required film thickness and width through processes such as calendering and stretching; the material is processed into a cover plate with a specific shape through processes such as thermoforming and molding. During the molding and processing, it is necessary to control process parameters such as temperature, pressure, and speed to ensure the material's performance and dimensional accuracy.

[0057] Surface Treatment and Performance Optimization: The molded GLAM flexible cover plate undergoes surface treatments, such as coating with anti-scratch, oleophobic, and anti-fingerprint layers, to further improve its surface and performance characteristics. Simultaneously, by adjusting process parameters and adding appropriate additives, the optical, mechanical, and thermal properties of the material are optimized to meet the requirements of different application scenarios. Finally, comprehensive quality inspections are conducted on the product, including visual inspection, dimensional measurement, and performance testing, to ensure that the product quality meets standards.

[0058] Flexible cover plates are commonly used in smartphones, tablets, laptops, smart wearable devices, and automotive displays. Details are as follows.

[0059] The rise of foldable phones has led to the widespread application of flexible cover plates, providing users with larger screen display areas and unique user experiences. Some foldable tablets also utilize flexible cover plate technology, offering better portability and flexible usage modes. Some foldable laptops are also equipped with flexible cover plates, enabling screen folding and deformation to meet user needs in different usage scenarios. Some smart wearable devices, such as smartwatches and smart bracelets, also use flexible cover plates, which can adapt to the bending of the wrist, providing better wearing comfort and screen durability. Flexible cover plates are also commonly used in automotive display devices such as central control displays and dashboards; the bendable flexible cover plate can better adapt to the design of gaps within the vehicle, providing a wider display area and better visual effects.

[0060] Because the flexibility of flexible cover materials such as transparent polyimide film (CPI), ultra-thin flexible glass (UTG), or multifunctional polymer glass film materials (GLAM) is limited by the properties of the material itself, wrinkles are likely to appear after repeated folding.

[0061] Therefore, current flexible cover plates have problems such as difficulty in releasing stress and wrinkles after repeated folding.

[0062] To address the technical problem of flexible cover plates easily developing wrinkles after frequent bending in related technologies, refer to... Figure 1-3As shown, this application embodiment provides a stress buffer structure layer, including: a first stress buffer layer 10 and a second stress buffer layer 20; the first stress buffer layer 10 and the second stress buffer layer 20 are stacked; the side of the first stress buffer layer 10 facing the second stress buffer layer 20 is provided with a plurality of first protrusions 12 arranged in an array, and a first cavity 11 is provided between two adjacent columns of the first protrusions 12; the side of the second stress buffer layer 20 facing the first stress buffer layer 10 is provided with a plurality of second protrusions 21 arranged in an array, and a second cavity 22 is provided between two adjacent columns of the second protrusions 21; the side of the first stress buffer layer 10 facing the second stress buffer layer 20... The sides of the second stress buffer layer 20 facing the first stress buffer layer 10 are in contact with each other, so that the first protrusion 12 engages with the second cavity 22, and the second protrusion 21 engages with the first cavity to form a stress buffer structure layer 1; when the stress buffer structure layer 1 is bent, the first protrusion 12 at the bend of the stress buffer structure layer fits into the second cavity 22 at the corresponding position of the bend of the stress buffer structure layer 100, and the second protrusion 21 at the bend of the stress buffer structure layer 100 fits into the first cavity at the corresponding position of the bend of the stress buffer structure layer 100 to buffer the stress between the first stress buffer layer 10 and the second stress buffer layer 20.

[0063] See Figure 1-3 As shown, the first stress buffer layer 10 and the second stress buffer layer 20 are fastened together to form an integrally formed or non-integrated stress buffer structure layer 1. A plurality of first protrusions 12 on the first stress buffer layer 10 are arranged in a rectangular array, with a first cavity 11 between two adjacent columns of opposing first protrusions 12. All the first cavities between adjacent columns of the rectangular array are arranged linearly. A plurality of second protrusions 21 on the second stress buffer layer 20 are arranged in a rectangular array, with a second cavity 22 between two adjacent columns of opposing second protrusions 21. The position of the first protrusion 12 in each column of the first stress buffer layer is opposite to the position of the second cavity 22 in each column of the second stress buffer layer, and the position of the first cavity 11 in each column of the first stress buffer layer is opposite to the position of the second protrusion 21 in each column of the second stress buffer layer.

[0064] Optionally, when the first stress buffer layer 10 and the second stress buffer layer 20 are in contact with each other in an unbent state, the first protrusion 12 at each position is in movable engagement with the second cavity 22 at the corresponding position, and the second cavity 22 at the corresponding position is located on the second stress buffer layer 20 opposite to the first protrusion 12 at each position; similarly, the first cavity 11 at each position is in movable engagement with the second protrusion 21 at the corresponding position, and the second protrusion 21 at the corresponding position is located on the second stress buffer layer 20 opposite to the first cavity 11 at each position.

[0065] See Figure 4 As shown, when the stress buffer structure layer 1 is bent, the first cavity 11 at each position of the bend 100 and the corresponding second protrusion 21 change from a movable fit to a fitted fit under the stress generated during the bending process. That is, during this process, the second protrusion 21 gradually fills the first cavity 11. Similarly, the first protrusion 12 at each position and the corresponding second cavity 22 change from a movable fit to a fitted fit under the stress generated during the bending process. That is, during this process, the first protrusion 12 gradually fills the second cavity 22. This buffers the stress generated during the bending process, thereby improving the structural damage to the materials of the first and second stress buffer layers caused by the stress during bending. This improves the wrinkles caused by material structural damage in the first and second stress buffer layers during bending. Therefore, when this stress buffer structure layer 1 is applied to a flexible cover plate, it can improve or solve the wrinkles caused by repeated bending of the flexible cover plate.

[0066] Therefore, in this embodiment of the stress buffer structure layer, the side of the first stress buffer layer facing the second stress buffer layer and the side of the second stress buffer layer facing the first stress buffer layer are in contact with each other, so that the first protrusion and the second cavity cooperate, and the second protrusion and the first cavity cooperate to form a stress buffer structure layer; when the stress buffer structure layer is bent, the first protrusion at the bend of the stress buffer structure layer fits into the second cavity at the corresponding position of the bend of the stress buffer structure layer, and the second protrusion at the bend of the stress buffer structure layer fits into the first cavity at the corresponding position of the bend of the stress buffer structure layer to buffer the stress between the first stress buffer layer and the second stress buffer layer, thereby buffering the stress generated by the flexible cover plate during bending, thereby improving or solving the problem that the flexible cover plate is prone to wrinkles after frequent bending.

[0067] In some embodiments, when the stress buffer structure layer is not bent, the first protrusion at each position of the first stress buffer layer is in movable engagement with the second cavity at the corresponding position of the second stress buffer layer, and the second protrusion at each position of the second stress buffer layer is in movable engagement with the first cavity at the corresponding position of the first stress buffer layer; there is a first space between the first protrusion at each position and the second cavity at the corresponding position, and there is a second space between the second protrusion at each position and the first cavity at the corresponding position.

[0068] The presence of a first space and a second space between the first stress buffer layer and the second stress buffer layer can enhance the stress buffering effect between the first stress buffer layer and the second stress buffer layer, and increase the buffer space between the first stress buffer layer and the second stress buffer layer.

[0069] The stress-relief structural layer can be made of ultra-thin flexible glass or transparent polyimide film, etc. No limitation is made here. Optionally, the first stress-relief layer and the second stress-relief layer can be made of flexible glass.

[0070] In some embodiments of this application, the first protrusion has a first rectangular structure or a first toothed structure, and the second protrusion has a second rectangular structure or a second toothed structure; when the stress buffer structure layer is not bent, the first space is a first gap for movable engagement with the first rectangular structure or the first toothed structure; the second space is a second gap for movable engagement with the second rectangular structure or the second toothed structure.

[0071] Taking a toothed structure as an example. In one embodiment of this application, the stress buffer structure layer 1 includes a first stress buffer layer a 120 and a second stress buffer layer a 210; the first protrusion 12 of the first stress buffer layer a 120 is a first toothed structure 121; the second protrusion of the second stress buffer layer a 210 is a second toothed structure 211, see reference. Figure 5 As shown, when the stress buffer structure layer 1 is not bent, the second toothed structure 211 is in movable engagement with the first gap 122 of the first cavity, and the first toothed structure 121 is in movable engagement with the second gap 221 of the second cavity. The first gap 122 and the second gap 221 can provide more stress buffering gaps for stress buffering.

[0072] See Figure 4 and Figure 6 As shown, when the stress buffer structure layer 1 is bent, the stress buffer structure layer 1 at the bend 100 exhibits... Figure 6 In the state where the first and second gaps disappear, the second toothed structure 211 moves and engages with the first cavity, and the first toothed structure 121 moves and engages with the second cavity. As the stress changes during the bending process, the first toothed structure 211 fills the first cavity and fits against the inner wall of the first cavity, and the second toothed structure fills the second cavity and fits against the inner wall of the second cavity, thus completing the stress buffering process.

[0073] The toothed structure allows the first stress buffer layer a and the second stress buffer layer a to have strong mutual support when bent, thus avoiding excessive local stress on the first stress buffer layer a or the second stress buffer layer a at the bend, which could lead to structural damage.

[0074] Similarly, when the first protrusion is a first rectangular structure and the second protrusion is a second rectangular structure, both the first cavity and the second cavity can be rectangular cavities that match the first protrusion and the second protrusion. Thus, when the stress buffer structure layer transitions from an unbent state to a bent state, the first protrusion and the second cavity change from a movable fit to a close fit, and the second protrusion and the first cavity change from a movable fit to a close fit, thereby playing a role in buffering and releasing the stress.

[0075] In some embodiments of this application, the first protrusion has a first curved surface structure, and the second protrusion has a second curved surface structure; when the stress buffer structure layer is not bent, the first space is a third gap for movable engagement with the first curved surface structure; and the second space is a fourth gap for movable engagement with the second curved surface structure.

[0076] See Figure 7 and Figure 8 As shown, in another embodiment of this application, the first protrusion has a first curved surface structure 1202, and the second protrusion has a second curved surface structure 2102; the first space is a third gap 2101 for movable cooperation with the first curved surface structure; and the second space is a fourth gap 1201 for movable cooperation with the second curved surface structure.

[0077] See Figure 7 As shown, the stress buffer structure layer 1 includes a first stress buffer layer b 1200 and a second stress buffer layer b 2100. The first cavity has a third gap 2101, and the second cavity has a fourth gap 1201. When the stress buffer structure layer 1 is not bent, the second curved surface structure 2102 is in movable fit with the fourth gap 1201; the first curved surface structure 1202 is in movable fit with the third gap 2101. Optionally, the first and second curved surface structures are spherical or ellipsoidal structures.

[0078] When the stress buffer structure layer 1 is bent, refer to the structural reference of the stress buffer structure layer 1 at the bend 100. Figure 8 As shown, during the transition from an unbent state to a bent state, the first curved surface structure 1202 on the first stress buffer layer gradually fills the third gap 2101, and the second curved surface structure 2102 on the second stress buffer layer gradually fills the fourth gap 1201, thereby playing a role in mitigating the stress generated in the stress buffer layer 1 during the bending process.

[0079] The curved surface structure of the first and second protrusions helps to make the contact surface between the first curved surface structure 1202 and the third gap 2101 more smoothly and evenly subjected to force. The contact surface between the second curved surface structure 2102 and the fourth gap 1201 on the second stress buffer layer is also more smoothly and evenly subjected to force. Thus, the stress buffer layer 1 is more evenly buffered during the transition from the unbent state to the bent state.

[0080] Therefore, the stress buffer structure layer adopts a hollowed-out staggered design. Through the different modes of action of the first protrusion, the first cavity, the second protrusion, and the second cavity in the bent and unbent states, that is, in the unbent state, the first protrusion and the second cavity are in movable cooperation, and the second protrusion and the first cavity are in movable cooperation. In the bent state, the first protrusion and the second cavity at the bend gradually change from movable cooperation to close contact, and the second protrusion and the first cavity gradually change from movable cooperation to close contact. This achieves the buffering effect of stress generated in the stress buffer structure layer during bending, thereby improving or solving the problem that flexible cover plates are prone to wrinkles after bending.

[0081] Secondly, embodiments of this application provide a flexible cover plate, see [link to relevant documentation]. Figure 9 As shown, it includes: a first protective layer 2, the stress buffer structure layer and a second protective layer 3; the first protective layer 2, the first stress buffer layer 10, the second stress buffer layer 20 and the second protective layer 3 are stacked.

[0082] In some embodiments of this application, the first protective layer 2, the first stress buffer layer 10, the second stress buffer layer 20, and the second protective layer 3 are all made of flexible glass.

[0083] The use of the aforementioned stress-buffering structural layer in the flexible cover plate allows for a more moderate and sufficient buffering and release of stress generated during the transition from an unbent to a bent state. This improves or solves the wrinkling problem caused by stress damaging the material structure of the flexible cover plate during bending.

[0084] The functions and effects of the technical features in this technical solution that are similar to or related to the aforementioned technical solution are similar to those in the aforementioned technical solution, and the inventive concept and beneficial effects of this technical solution are similar to those in the aforementioned technical solution, so they will not be repeated here.

[0085] Thirdly, embodiments of this application provide a substrate including the stress buffer structure layer.

[0086] The flexible cover plate is produced by using the stress buffer structure layer mentioned above on the substrate, which can make the flexible cover plate obtained by using the substrate have a better anti-wrinkle effect.

[0087] The functions and effects of the technical features in this technical solution that are similar to or related to the aforementioned technical solution are similar to those in the aforementioned technical solution, and the inventive concept and beneficial effects of this technical solution are similar to those in the aforementioned technical solution, so they will not be repeated here.

[0088] Fourthly, embodiments of this application provide an electronic device having a display screen, the display screen being provided with the flexible cover plate.

[0089] Furthermore, the display screen is a foldable screen.

[0090] The functions and effects of the technical features in this technical solution that are similar to or related to the aforementioned technical solution are similar to those in the aforementioned technical solution, and the inventive concept and beneficial effects of this technical solution are similar to those in the aforementioned technical solution, so they will not be repeated here.

[0091] The above description is merely a preferred embodiment of this application and is not intended to limit this application. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of this application should be included within the protection scope of this application.

Claims

1. A stress buffer structure layer, characterized by, The system includes a first stress buffer layer and a second stress buffer layer; the first stress buffer layer and the second stress buffer layer are stacked; the side of the first stress buffer layer facing the second stress buffer layer has a plurality of first protrusions arranged in an array, and a first cavity is provided between two adjacent rows of first protrusions; the side of the second stress buffer layer facing the first stress buffer layer has a plurality of second protrusions arranged in an array, and a second cavity is provided between two adjacent rows of second protrusions; the side of the first stress buffer layer facing the second stress buffer layer and the side of the second stress buffer layer facing the first stress buffer layer are in contact with each other, so that the first protrusions and the second cavities cooperate, and the second protrusions and the first cavities cooperate to form a stress buffer structure layer; When the stress buffer structure layer is bent, the first protrusion at the bend of the stress buffer structure layer fits into the second cavity at the corresponding position of the bend of the stress buffer structure layer, and the second protrusion at the bend of the stress buffer structure layer fits into the first cavity at the corresponding position of the bend of the stress buffer structure layer.

2. The stress buffer structure layer of claim 1, wherein, When the stress buffer structure layer is not bent, the first protrusion at each position of the first stress buffer layer is in movable engagement with the second cavity at the corresponding position of the second stress buffer layer, and the second protrusion at each position of the second stress buffer layer is in movable engagement with the first cavity at the corresponding position of the first stress buffer layer; there is a first space between the first protrusion at each position and the second cavity at the corresponding position, and there is a second space between the second protrusion at each position and the first cavity at the corresponding position.

3. The stress buffer structure layer of claim 2, wherein, The first protrusion has a first rectangular structure or a first toothed structure, and the second protrusion has a second rectangular structure or a second toothed structure; when the stress buffer structure layer is not bent, the first space is a first gap for movable engagement with the first rectangular structure or the first toothed structure; the second space is a second gap for movable engagement with the second rectangular structure or the second toothed structure.

4. The stress buffer structure layer according to claim 1 or 2, wherein, The first protrusion has a first curved surface structure, and the second protrusion has a second curved surface structure; when the stress buffer structure layer is not bent, the first space is a third gap for movable cooperation with the first curved surface structure; the second space is a fourth gap for movable cooperation with the second curved surface structure.

5. The stress buffer structure layer of claim 1, wherein, The first stress buffer layer and the second stress buffer layer are made of flexible glass.

6. A flexible cover sheet characterized by include: The first protective layer, the stress buffer structure layer as described in any one of claims 1-4, and the second protective layer; the first protective layer, the first stress buffer layer, the second stress buffer layer, and the second protective layer are stacked.

7. The flexible cover sheet of claim 6, wherein, The first protective layer, the first stress buffer layer, the second stress buffer layer, and the second protective layer are all made of flexible glass.

8. A substrate, characterized by, It includes the buffer structure described in any one of claims 1-5 or the flexible cover plate described in any one of claims 6-7.

9. An electronic device, comprising: The electronic device has a display screen, which is provided with the flexible cover plate according to any one of claims 6-7.

10. The electronic device of claim 9, wherein, The display screen is a foldable screen.