A method for realizing high-mobility UMOSFET trenches in SiC

By removing the etching damage of SiC UMOSFET trenches through sacrificial oxidation and interfacial gas passivation, and performing N+ ion implantation at the bottom and corners of the trenches, the problem of high interface state density of SiC UMOSFETs was solved, and the device performance of high mobility and high breakdown voltage was improved.

CN123124422APending Publication Date: 2026-11-17WUHU RES INST OF XIAN UNIV OF ELECTRONIC SCI & TECH +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611329647.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-31
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

During the manufacturing process of SiC UMOSFETs, physical impacts and chemical corrosion damage to the trench sidewalls lead to increased interface state density and decreased mobility, making them unsuitable for high-frequency and high-power-density applications.

Method used

Etching damage was removed by sacrificial oxidation and interfacial gas passivation, and a high-quality second P-type epitaxial layer was grown. N+ ion implantation was performed at the bottom and corners of the trench to form amorphous SiC regions to improve the oxidation rate and interfacial states and reduce the channel resistance.

Benefits of technology

It significantly improves the electron mobility of the SiC/gate oxide interface, reduces the channel resistance, and enhances the overall performance and breakdown voltage of the device, making it suitable for high-frequency and high-power-density applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124422A_ABST
    Figure CN123124422A_ABST
Patent Text Reader

Abstract

This invention discloses a method for realizing a high-mobility UMOSFET trench on SiC, comprising the following steps: growing a first P-type epitaxial layer (2) on an N-type SiC substrate (1); etching the middle region of the first P-type epitaxial layer (2), with the etching endpoint located on the surface of the N-type SiC substrate (1) to form a trench; performing a sacrificial oxidation process on the etched surface, followed by interface gas passivation; epitaxially growing a second P-type epitaxial layer (3) on the current sample surface; and performing N-type passivation on the second P-type epitaxial layer (3) at the bottom of the trench. + Ion implantation enables N + The implantation region and the N-type SiC substrate (1) form an N-type substrate at the bottom of the trench. + A connecting layer (51) is formed to create a UMOSFET trench. By growing a second P-type epitaxial layer, this invention reduces the interface states, thereby improving electron mobility and enhancing the overall performance of the UMOSFET device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of wide bandgap semiconductor manufacturing technology, specifically relating to a method for realizing a trench in a silicon carbide (SiC) high mobility trench MOSFET (UMOSFET). Background Technology

[0002] In the context of a generally positive outlook for the power electronics industry, power semiconductor devices have become a direct factor affecting the cost and efficiency of power electronic devices. Although silicon-based power devices are already quite mature, as power semiconductors gradually develop towards higher power, higher frequency, and lower power consumption, design limitations of the devices themselves make them increasingly difficult to apply to high-efficiency and high-power-density applications.

[0003] Due to its superior physical properties, SiC material has begun to attract widespread attention from industry professionals, leading to the development of SiC trench MOSFET technology. Compared to silicon-based devices, SiC's high thermal conductivity and large bandgap make it more suitable for operation in scenarios with high current density, high breakdown field strength, and high operating temperature. Compared to comparable Si UMOSFETs, SiCUMOSFETs have lower characteristic on-resistance and switching losses, making them more suitable for high-frequency operation. Furthermore, the high thermal conductivity of SiCUMOSFETs significantly improves the device's high-temperature stability.

[0004] Therefore, given the difficulty of traditional power devices meeting the demands for high efficiency and miniaturization, SiC UMOSFETs, with their advantages of low on-resistance, high voltage withstand, and fast switching speed, are gradually replacing SiC planar MOSFETs, adapting to the high-voltage, high-current requirements of scenarios such as new energy vehicles, photovoltaic energy storage, and smart grids. Meanwhile, the high energy efficiency requirements of 5G base stations and data center power supplies, as well as the performance upgrades of industrial motor drives, are further driving their widespread application.

[0005] However, the fabrication of SiC UMOSFETs is highly dependent on deep trench etching, a process that inevitably introduces physical impacts and chemical corrosion damage to the trench sidewalls. Immediately depositing gate oxide after sacrificial oxidation cannot completely repair this damage; a large accumulation of dangling bonds and micro-defects remains at the SiC / gate oxide interface, leading to a significant increase in interface state density and a severe degradation of the effective channel electron mobility. This decrease in mobility increases the actual on-resistance and dynamic losses of the device, weakening the intrinsic electrical advantages of SiC material and becoming a key technological bottleneck restricting the expansion of SiC UMOSFETs to higher frequency and higher power density applications. Summary of the Invention

[0006] To address the aforementioned problems in the prior art, this invention provides a method for implementing high-mobility UMOSFET trenches in SiC. The technical problem to be solved by this invention is achieved through the following technical solution: In a first aspect, the present invention provides a method for realizing a SiC high-mobility UMOSFET trench, comprising the following steps: Step 1: Grow a first P-type epitaxial layer 2 on an N-type SiC substrate 1; Step 2: Etch the middle region of the first P-type epitaxial layer 2, with the etching endpoint located on the surface of the N-type SiC substrate 1, to form a trench; Step 3: Perform sacrificial oxidation on the etched surface from Step 2, followed by interfacial gas passivation. Step 4: Epitaxially grow a second P-type epitaxial layer 3 on the surface of the current sample; Step 5: Perform N-type extrusion on the second P-type epitaxial layer 3 at the bottom of the trench. + Ion implantation enables N + The implantation region and the N-type SiC substrate 1 form an N-type substrate at the bottom of the trench. + The connecting layer 51 forms a UMOSFET trench.

[0007] In one embodiment of the present invention, the method further includes: Step 6: Deposit gate oxide 6 on the surface of the current sample; Step 7: Continue to deposit polycrystalline silicon on the inner wall of the trench as the conductive layer 7 of the gate electrode.

[0008] In one embodiment of the present invention, step 5 further includes: N-type epitaxial layer 3 at the bottom of the trench is subjected to N-type extrusion. + During ion implantation, N220N2 is applied to the corners of the trench openings. + Ion implantation to form N + Source area 52.

[0009] In one embodiment of the present invention, growing a first P-type epitaxial layer 2 on an N-type SiC substrate 1 includes growing a first P-type epitaxial layer 2 with a thickness of 3~20μm on the N-type SiC substrate 1.

[0010] In one embodiment of the present invention, step 2 involves performing a sacrificial oxidation process on the etched surface, including: oxidizing the etched surface for 5 to 120 minutes at a temperature of 850 to 1150°C under a pure oxygen or oxygen-nitrogen mixed atmosphere to form a 10 to 100 nm sacrificial oxide layer on the etched surface; and then stripping the sacrificial oxide layer using a fluorine-containing etching solution.

[0011] In one embodiment of the present invention, step 2, performing interface gas passivation treatment on the etched surface, includes: evacuating the process chamber to a vacuum level of ≤10. - After 3 Pa, an interface treatment gas is introduced; thermal activation treatment is carried out at 1000~1650℃ for 1~40 min to chemically passivate and volatilize impurities on the SiC surface of the trench sidewalls and bottom; after the treatment is completed, an inert atmosphere is maintained for purging and cooling. The interface treatment gas includes: A SiH4 / Ar mixed gas with a volume fraction of 3-5%, or... A mixture of HCl / equilibrium gas with a volume fraction of 0.1% to 5%, or, Pure Ar gas, or, A mixture of H2 carrier gas with a volumetric flow rate of 5000~10000 sccm and SiH4 gas with a volumetric flow rate of 20~60 sccm, or... Pure H2 gas with a volumetric flow rate of 20~2000 sccm; The balance gas is at least one of nitrogen, argon, helium and hydrogen. In the HCl / balance gas mixture, the volume fraction of HCl is calculated based on the total flow rate of the mixture, and the remainder is the balance gas.

[0012] In one embodiment of the present invention, the epitaxial growth of the second P-type epitaxial layer 3 on the surface of the current sample includes: epitaxially growing the second P-type epitaxial layer with a thickness of 0.1~1μm on the surface of the current sample; the material of the second P-type epitaxial layer is any one of 4H-SiC, 3C-SiC and 6H-SiC.

[0013] In one embodiment of the present invention, step 5 specifically includes: A thick implantation mask layer 41 is grown on the second P-type epitaxial layer 3, and the thick implantation mask layer 41 inside the trench and at the corners on both sides of the trench is etched using photolithography to expose the surface of the second P-type epitaxial layer 3. A thin injection mask layer 42 is grown on the surface of the current sample. Based on the thin injection mask layer 42, N is performed at the bottom of the trench and the corner of the opening. + Ion implantation; The thick injection mask layer 41 and the thin injection mask layer 42 are stripped off.

[0014] In one embodiment of the present invention, the deposition of gate oxide 6 on the surface of the current sample includes: depositing gate oxide 6 with a thickness of 20~80nm by thermal oxidation or CVD.

[0015] Compared with the prior art, the beneficial effects of the present invention are as follows: 1. This invention utilizes sacrificial oxidation to remove defects on the SiC surface and uses interfacial gas passivation to form a smooth surface, so as to epitaxially grow a high-quality second P-type epitaxial layer. By epitaxially growing the second P-type epitaxial layer, the physical impact and chemical corrosion damage caused by etching are significantly reduced, making the interface states of SiC / gate oxide much lower than those formed by traditional etching processes, thereby improving electron mobility, reducing channel resistance, and improving the overall performance of the device.

[0016] 2. This invention involves implanting N2O into the outer surface of SiC at the bottom of the trench. + Ions cause the formation of amorphous SiC in this region. Since the activation energy for Si-C bond breaking in the amorphous SiC layer is reduced, the thermal oxidation rate at the bottom of the trench is accelerated during subsequent gate oxide deposition, thereby increasing the local thickness of the bottom gate oxide, effectively widening the depletion region and reducing the peak electric field at the corner, thus increasing the bottom breakdown voltage.

[0017] The present invention will be further described in detail below with reference to the accompanying drawings and embodiments. Attached Figure Description

[0018] Figure 1 This is a flowchart of a method for implementing a SiC high-mobility UMOSFET trench according to an embodiment of the present invention; Figure 2 This is a schematic diagram of the sample structure in step 1 of a SiC high-mobility UMOSFET trench implementation method provided in an embodiment of the present invention; Figure 3 This is a schematic diagram of the sample structure in step 2 of a SiC high-mobility UMOSFET trench implementation method provided in an embodiment of the present invention; Figure 4 This is a three-dimensional topographic image of the surface of the first P-type epitaxial layer 2 without interface gas passivation treatment provided in an embodiment of the present invention; Figure 5 This is a three-dimensional topographic image of the surface of the first P-type epitaxial layer 2 after interfacial gas passivation treatment provided in an embodiment of the present invention; Figure 6 This is a schematic diagram of the sample structure in step 4 of a SiC high-mobility UMOSFET trench implementation method provided in an embodiment of the present invention; Figures 7(a)-7(e) This is a schematic diagram of the sample structure in step 5 of a SiC high-mobility UMOSFET trench implementation method provided in an embodiment of the present invention; Figure 8 This is a schematic diagram of the sample structure in step 6 of a SiC high-mobility UMOSFET trench implementation method provided in an embodiment of the present invention; Figure 9This is a schematic diagram of the sample structure in step 7 of a SiC high-mobility UMOSFET trench implementation method provided in an embodiment of the present invention; Figure reference numerals: 1-SiC substrate, 2-First P-type epitaxial layer, 3-Second P-type epitaxial layer, 41-Thick implantation mask layer, 42-Thin implantation mask layer, 51-N + Connected layers, 52-N + Source region, 6-gate oxide, 7-conductive layer of gate electrode. Detailed Implementation

[0019] The present invention will be further described in detail below with reference to specific embodiments, but the implementation of the present invention is not limited thereto.

[0020] In a first aspect, embodiments of the present invention provide a method for implementing a SiC high-mobility UMOSFET trench, such as... Figure 1 As shown, it includes the following steps: Step 1: Grow a first P-type epitaxial layer 2 on an N-type SiC substrate 1.

[0021] Specifically, an N-type SiC substrate 1 is placed in an epitaxial growth furnace, and a first P-type epitaxial layer 2 with a thickness of 3~20 μm is grown on the N-type SiC substrate 1 using CVD technology. The sample structure at this point is as follows: Figure 2 As shown.

[0022] For example, in step 1, a first P-type epitaxial layer 2 with a thickness of 12 μm can be grown on an N-type SiC substrate 1, but it is not limited to this.

[0023] Step 2: Etch the middle region of the first P-type epitaxial layer 2, with the etching endpoint located on the surface of the N-type SiC substrate 1, forming a trench.

[0024] Specifically, a trench pattern is defined in the middle section of the first P-type epitaxial layer 2, and the first P-type epitaxial layer 2 below the pattern is etched. The etching endpoint is located on the upper surface of the N-type SiC substrate 1. At this time, the sample structure is as follows: Figure 3 As shown.

[0025] For example, SiO2 can be deposited using a PECVD system as a mask, and a trench pattern can be formed in the middle section of the first P-type epitaxial layer 2 by photolithography and development. Then, the trench pattern can be etched using an ICP / RIE etching device, with the etching endpoint located on the upper surface of the N-type SiC substrate 1 to form a trench.

[0026] Step 3: Perform sacrificial oxidation on the etched surface from Step 2, followed by interfacial gas passivation.

[0027] Preferably, the etched surface is subjected to a sacrificial oxidation process, including: oxidation at a temperature of 850~1150℃ for 5~120 min in a pure oxygen or oxygen-nitrogen mixed atmosphere to form a 10~100 nm sacrificial oxide layer on the etched surface; and then the sacrificial oxide layer is stripped off using a fluorine-containing etching solution.

[0028] Specifically, firstly, dilute hydrofluoric acid (HF volume fraction 1%~10%) is used to remove the natural oxide layer and residual etching particles on the sample surface; then, deionized water is used for rinsing and nitrogen is used for drying to ensure that the sidewalls and bottom of the trench are exposed to a clean SiC surface.

[0029] Then, the cleaned sample is transferred to an oxidation furnace and pure oxygen or an oxygen-nitrogen mixture (oxygen volume fraction 50%~100%) is introduced at a temperature of 850~1150℃ for 5~120 min. This allows the oxygen to preferentially react with the defect atoms on the trench sidewalls and bottom, as well as the impurities adsorbed on the surface, thus selectively oxidizing the damaged layer and contaminants. This generates SiO2 and carbon oxides, which are then solidified in the sacrificial oxide layer, forming a sacrificial oxide layer with a thickness of 10~100 nm.

[0030] Finally, the sample was immersed in hydrofluoric acid solution and etched at room temperature to completely remove the sacrificial oxide layer. After etching, it was rinsed with deionized water and dried with nitrogen to make the residual SiO2 thickness on the exposed SiC surface <0.5 nm, the dangling bond density was significantly reduced, and the Si:C stoichiometry was restored to the intrinsic range, providing a low-defect substrate for subsequent interfacial gas passivation treatment.

[0031] For example, the wafer is immersed in dilute hydrofluoric acid (HF volume fraction 3%) for 1 min to remove the natural oxide layer and etching residue particles on the wafer surface; then it is rinsed with deionized water for 30 s and dried with nitrogen to ensure that the trench sidewalls and bottom are exposed to a clean SiC surface.

[0032] The cleaned wafers are transferred to an oxidation furnace, where pure oxygen is introduced at 850°C for 5 minutes to form a sacrificial oxide layer with a thickness of 10-30 nm.

[0033] The wafer was immersed in a hydrofluoric acid (HF volume fraction 3%) solution and etched at room temperature for 1 min to completely remove the sacrificial oxide layer. After etching, it was rinsed with deionized water and dried with nitrogen gas to make the residual SiO2 thickness on the exposed SiC surface <0.5 nm, the dangling bond density was significantly reduced, and the Si:C stoichiometry was restored to the intrinsic range, providing a low-defect substrate for subsequent interface gas passivation treatment.

[0034] Thus, through the sacrificial oxidation process, the embodiments of the present invention selectively oxidize and strip the physical damage layer, non-stoichiometric region and adsorbed impurities introduced by etching on the trench surface, thereby initially reducing the interface state density Dit of the etched surface and restoring the Si:C ratio, providing a low-defect substrate for subsequent interface gas passivation treatment.

[0035] Preferably, the etched surface undergoes interfacial gas passivation treatment, including: evacuating the process chamber to a vacuum level of ≤10. - After 3 Pa, an interface treatment gas is introduced; then, a thermal activation treatment is performed at 1000~1650℃ for 1~40 min to chemically passivate and volatilize impurities on the sidewalls and bottom SiC surface of the trench; after the treatment is completed, an inert atmosphere is maintained for purging and cooling.

[0036] The interface treatment gas includes: A SiH4 / Ar mixed gas with a volume fraction of 3-5%, or... A mixture of HCl / equilibrium gas with a volume fraction of 0.1% to 5%, or, Pure Ar gas, or, A mixture of H2 carrier gas with a volumetric flow rate of 5000~10000 sccm and SiH4 gas with a volumetric flow rate of 20~60 sccm, or... Pure H2 gas with a volumetric flow rate of 20~2000 sccm; The balance gas is at least one of nitrogen, argon, helium and hydrogen. In the HCl / balance gas mixture, the volume fraction of HCl is calculated based on the total flow rate of the mixture, and the remainder is the balance gas.

[0037] For example, the process chamber is evacuated to ≤10 - After 3 Pa, pure H2 gas with a volumetric flow rate of 40~100 slm is introduced; thermal activation treatment is performed at 1400℃ for 20 min to chemically passivate and volatilize impurities on the SiC surface of the trench sidewalls and bottom; after treatment, an inert atmosphere is maintained for purging and cooling. At this time, the root mean square surface roughness R of the first P-type epitaxial layer 2 is... q ≤0.3nm.

[0038] Please compare. Figure 4 and Figure 5 ,in, Figure 4 This is a three-dimensional morphology image of the surface of the first P-type epitaxial layer 2 without interfacial gas passivation treatment (i.e., prepared by conventional process methods) provided in an embodiment of the present invention. Figure 5 This is a three-dimensional morphology image of the surface of the first P-type epitaxial layer 2 after interface gas passivation treatment according to an embodiment of the present invention. The specific process parameters for interface passivation are as follows: the process chamber is evacuated to ≤10... -After 3 Pa, pure H2 gas with a volumetric flow rate of 40 slm was introduced; then, thermal activation treatment was performed at 1400℃ for 20 min, followed by purging and cooling under an inert atmosphere after treatment. The test conditions were as follows: the sample surface was scanned using a Bruker Dimension Icon atomic force microscope with a silicon probe having a radius of curvature ≤ 5 nm, the scanning range was 5 × 5 μm², and the scanning rate was 1.0 Hz.

[0039] It can be seen that the surface of the first P-type epitaxial layer 2 prepared by the traditional process has significant micro-undulations and surface protrusions, and the root mean square surface roughness R of the first P-type epitaxial layer 2 is... q With a thickness of 1.2 nm, direct deposition of gate oxide 6 will result in a SiC / gate oxide interface with a high interface state density. The surface of the first P-type epitaxial layer 2, after interface gas passivation, is smooth, without periodic etching streaks or local depressions, and the root mean square roughness R of the first P-type epitaxial layer 2 is [value missing]. q With a wavelength of 0.23 nm, it provides a passivation state interface with low defects and high chemical stability for growing a high-quality second P-type epitaxial layer 3.

[0040] Thus, through interfacial gas passivation treatment, the SiC crystal bulk structure is not changed, and the surface is reconstructed at the atomic level. This solves the problems of unsaturated atomic-level dangling bonds and interface trap states, making the interface state density Dit of the etched surface stable. This provides a passivated interface with low defects and high chemical stability for the subsequent epitaxial growth of the second P-type epitaxial layer 3.

[0041] Step 4: Epitaxially grow a second P-type epitaxial layer 3 on the surface of the current sample.

[0042] Preferably, the second P-type epitaxial layer 3 with a thickness of 0.1~1μm is grown using an epitaxial growth furnace, and the sample structure is as follows. Figure 6 As shown. The material of the second P-type epitaxial layer 3 is any one of 4H-SiC, 3C-SiC, and 6H-SiC.

[0043] For example, an epitaxial growth furnace is used to grow a second P-type epitaxial layer 3 with a thickness of 0.5 μm on the surface of the current sample. The material of the second P-type epitaxial layer 3 is 4H-SiC.

[0044] Understandably, the surface formed by etching in existing technologies is rough. In this embodiment, based on sacrificial oxidation and interface gas passivation, the surface roughness is further reduced by epitaxially growing a second P-type epitaxial layer 3, resulting in a planar epitaxial layer. This planar epitaxial layer reduces the interface states of SiC / gate dielectric, thereby improving electron mobility, reducing channel resistance, and enhancing the overall performance of the device.

[0045] Step 5: Perform N-type extrusion on the second P-type epitaxial layer 3 at the bottom of the trench. + Ion implantation enables N + The implantation region and the N-type SiC substrate 1 form an N-type substrate at the bottom of the trench. + The connecting layer 51 forms a UMOSFET trench.

[0046] Optionally, step 5 may also include: N-type epitaxial layer 3 at the bottom of the trench is subjected to N-type epitaxial layer 3. + During ion implantation, N2200N2 is applied to the corners of the trench opening. + Ion implantation to form N + Source area 52.

[0047] Specifically, step 5 includes: First, a thick implantation mask layer 41 is grown on the second P-type epitaxial layer 3. The sample structure is shown in Figure 7(a). The thick implantation mask layer 41 in the trench and on both sides of the trench is etched by photolithography to expose the surface of the second P-type epitaxial layer 3. The sample structure is shown in Figure 7(b).

[0048] Then, a thin injection mask layer 42 is grown on the surface of the current sample, and the sample structure is shown in Figure 7(c). This thin injection mask layer 42 is used to prevent injection damage.

[0049] Next, N is performed at the bottom of the trench and the corner of the opening based on the thin injection mask layer 42. + Ion implantation was performed, and the sample structure at this point is shown in Figure 7(d).

[0050] Finally, the thick injection mask layer 41 and the thin injection mask layer 42 are peeled off, and the sample structure is shown in Figure 7(e).

[0051] For example, firstly, a 2 μm thick implantation mask layer 41 is grown on the second P-type epitaxial layer 3 using PECVD. An etching pattern is defined in the middle section of the thick implantation mask layer 41, including the trenches and the corners on both sides of the trenches. The thick implantation mask layer 41 within the etching pattern is removed using photolithography to expose the surface of the second P-type epitaxial layer 3.

[0052] Then, a thin injection mask layer 42 with a thickness of 0.01~0.1 μm was grown on the current sample surface using PECVD.

[0053] Next, N is performed at the bottom of the trench and the corner of the opening. + Injection: Injection energy is 10~150 keV, and the dose is 1×10¹ 4 ~5×10¹ 5 cm -², with an injection angle of 7°. Annealing at 1700℃ in an inert atmosphere for 30 min activates nitrogen atoms, forming N atoms embedded beneath the P-type body region. + Connecting layers and N covering the edge of the P-type body region + Edge modulation layer; the N + All layers pass through N - Epitaxial layer and top N + The source region is electrically connected.

[0054] Finally, the thick implantation mask layer 41 and the thin implantation mask layer 42 are removed by HF pickling.

[0055] Ultimately N + The surface doping concentration of the implanted region ranges from 5 × 10⁻⁶. 19 cm -3 ~2×10 20 cm -3 .

[0056] This invention embodiment utilizes high-energy N + An amorphous damage layer is introduced into the bottom region of trench S. This region has a lower Si-C bond breaking activation energy and a significantly higher micro-defect density than the intact lattice, leading to enhanced thermal oxidation reactivity. In subsequent thermal oxidation processes, the amorphous SiC region exhibits a faster oxidation rate, resulting in a thicker SiO2 dielectric layer than the surrounding crystalline region. This locally thickened SiO2 layer effectively enhances the electric field blocking capability at the bottom of the trench, causing the depletion region to smoothly widen into the dielectric layer, significantly weakening the peak electric field, and thus effectively improving the overall breakdown voltage of the device.

[0057] Compared with the prior art, the beneficial effects of the embodiments of the present invention are as follows: 1. This invention utilizes sacrificial oxidation to remove defects on the SiC surface and uses interfacial gas passivation to form a smooth surface, so as to epitaxially grow a high-quality second P-type epitaxial layer 3. By epitaxially growing the second P-type epitaxial layer 3, the physical impact and chemical corrosion damage caused by etching are significantly reduced, making the interface states of SiC / gate oxide much lower than those formed by traditional etching processes, thereby improving electron mobility, reducing channel resistance, and improving the overall performance of the device.

[0058] 2. This invention involves implanting N2O into the outer surface of SiC at the bottom of the trench, the corner area, and the lower section of the sidewall. + This causes the formation of amorphous SiC in the region. Since the activation energy for Si-C bond breaking in the amorphous SiC layer is reduced, the thermal oxidation rate at the bottom of the trench is accelerated during subsequent gate oxide deposition, thereby increasing the local thickness of the bottom gate oxide, effectively widening the depletion region and reducing the peak electric field at the corner, thus increasing the bottom breakdown voltage.

[0059] In one embodiment, in the SiC high-mobility UMOSFET trench implementation method provided by the present invention, step 5 further includes: N-type epitaxial layer 3 at the bottom of the trench is subjected to N-type epitaxial layer 3. + During ion implantation, N2200N2 is applied to the corners of the trench opening. + Ion implantation to form N + Source area 52.

[0060] This invention embodiment utilizes high-energy N + An amorphous damage layer is introduced into the upper surface at the corner of the opening. This region has a lower Si-C bond breaking activation energy and a significantly higher micro-defect density than the intact lattice, leading to enhanced thermal oxidation reactivity. In subsequent thermal oxidation processes, the amorphous SiC region exhibits a faster oxidation rate, resulting in a thicker SiO2 dielectric layer than the surrounding crystalline region. This locally thickened SiO2 layer smooths the lateral electric field distribution at the gate edge, effectively improving the device's local electric field suppression capability.

[0061] In one embodiment, the SiC high-mobility UMOSFET trench implementation method provided by the present invention further includes the following steps: Step 6: Deposit gate oxide 6 on the surface of the current sample.

[0062] Specifically, a gate oxide film with a thickness of 20-80 nm is deposited via thermal oxidation or CVD. The gate oxide material can be elemental SiO2, SiN, Al2O3, AlN, or HfO2, or a composite film. The sample structure at this point is as follows: Figure 8 As shown.

[0063] It is worth mentioning that during the thermal oxidation process, since the activation energy of the amorphous SiC oxidation at the bottom of the trench is lower than that of the complete lattice, the oxidation rate at the bottom is faster than that at the sidewall, which naturally increases the SiO2 thickness at that location. That is, the thickness of the gate oxide 6 at the bottom of the trench is higher than that at the sidewall.

[0064] For example, the thermal oxidation growth of gate oxide step specifically involves: loading the wafer, after interface gas passivation and nitrogen ion implantation annealing, into a tube oxidation furnace and evacuating it to ≤10 °C. - After passing through a pressure of 3 Pa, high-purity oxygen (purity ≥99.999%) is introduced; dry thermal oxidation is then performed at 1200~1400℃ for 5~30 min, exposing the SiC surface on the inner wall, bottom, and top of the trench to grow SiO2 gate oxide 6 with a thickness of 20~80 nm. For example, when dry thermal oxidation is performed at 1250℃ for 17 min, the thickness of the gate oxide 6 at the bottom of the trench is 51~60 nm, and the thickness of the gate oxide 6 on the sidewall of the trench is 50 nm.

[0065] Understandably, thermal oxidation directly nucleates on a low-interfacial-state substrate, avoiding isolated oxidation nuclei and interfacial micropores caused by carbon residues in traditional processes. This results in a dense, low-stress dielectric layer, ensuring that the interfacial state density Dit is consistently ≤1×10¹¹ cm⁻¹. - ²·eV - ¹, The peak electric field at the bottom of the trench is reduced by ≥15%, and the device breakdown voltage is increased by ≥10%.

[0066] Step 7: Continue to deposit polycrystalline silicon on the inner wall of the trench as the conductive layer 7 of the gate electrode.

[0067] Specifically, polycrystalline silicon with a thickness of 0.4~0.8 μm is deposited in the trench using CVD, resulting in a sample structure as shown below. Figure 9 As shown.

[0068] It is understandable that this embodiment completes the fabrication of the trench structure in the SiC UMOSFET, and subsequent electrode fabrication can yield a complete UMOSFET.

[0069] For example, the effective electron mobility of the device channel is ≥80 cm⁻¹. 2 / V·s.

[0070] The SiC high-mobility UMOSFET trench implementation method provided by this invention is simple in process, compatible with standard semiconductor processes, suitable for mass production, and has good prospects for industrial application.

[0071] The above description, in conjunction with specific preferred embodiments, provides a further detailed explanation of the present invention. It should not be construed that the specific implementation of the present invention is limited to these descriptions. For those skilled in the art, various simple deductions or substitutions can be made without departing from the concept of the present invention, and all such modifications and substitutions should be considered within the scope of protection of the present invention.

Claims

1. A method for realizing a SiC high-mobility UMOSFET trench, characterized in that, Includes the following steps: Step 1: Grow a first P-type epitaxial layer (2) on an N-type SiC substrate (1); Step 2: Etch the middle region of the first P-type epitaxial layer (2), with the etching endpoint located on the surface of the N-type SiC substrate (1) to form a trench; Step 3: Perform sacrificial oxidation on the etched surface from Step 2, followed by interfacial gas passivation. Step 4: Epitaxially grow a second P-type epitaxial layer on the surface of the current sample (3); Step 5, N + ion implantation, so that N + the implanted region and the N-type SiC substrate (1) form N + the communication layer (51) forms the UMOSFET trench.

2. The method for realizing a SiC high-mobility UMOSFET trench according to claim 1, characterized in that, The method further includes: Step 6: Deposit gate oxide on the surface of the current sample (6); Step 7: Continue to deposit polysilicon on the inner wall of the trench as a conductive layer for the gate electrode (7).

3. The method for realizing a SiC high-mobility UMOSFET trench according to claim 1, characterized in that, Step 5 also includes: N-implanting the second P-type epitaxial layer (3) at the bottom of the trench + N-implanting the corners of the trench opening at the same time as the ion implantation + N-implanting, forming N + source regions (52).

4. The method for realizing a SiC high-mobility UMOSFET trench according to claim 1, characterized in that, The growth of the first P-type epitaxial layer (2) on the N-type SiC substrate (1) includes: growing a first P-type epitaxial layer (2) with a thickness of 3~20μm on the N-type SiC substrate (1).

5. The method for realizing a SiC high-mobility UMOSFET trench according to claim 1, characterized in that, In step 2, the etched surface is subjected to a sacrificial oxidation process, including: oxidizing the etched surface for 5 to 120 minutes at a temperature of 850 to 1150°C in a pure oxygen or oxygen-nitrogen mixed atmosphere to form a 10 to 100 nm sacrificial oxide layer on the etched surface; and then using a fluorine-containing etching solution to remove the sacrificial oxide layer.

6. The method for realizing a SiC high-mobility UMOSFET trench according to claim 1, characterized in that, In step 2, the interface gas passivation treatment is performed on the etched surface, including: vacuumizing the process cavity to ≤10 - Pa, then introducing the interface treatment gas; performing the thermal activation treatment at 1000-1650 ℃ for 1-40 min to cause the chemical passivation and impurity volatilization of the SiC surface of the groove sidewall and bottom; and maintaining the inert atmosphere to perform the cooling down by blowing. The interface treatment gas includes: A SiH4 / Ar mixed gas with a volume fraction of 3-5%, or... A mixture of HCl / equilibrium gas with a volume fraction of 0.1% to 5%, or, Pure Ar gas, or, A mixture of H2 carrier gas with a volumetric flow rate of 5000~10000 sccm and SiH4 gas with a volumetric flow rate of 20~60 sccm, or... Pure H2 gas with a volumetric flow rate of 20~2000 sccm; The balance gas is at least one of nitrogen, argon, helium and hydrogen. In the HCl / balance gas mixture, the volume fraction of HCl is calculated based on the total flow rate of the mixture, and the remainder is the balance gas.

7. The method for realizing a SiC high-mobility UMOSFET trench according to claim 1, characterized in that, The epitaxial growth of the second P-type epitaxial layer (3) on the surface of the current sample includes: epitaxially growing the second P-type epitaxial layer with a thickness of 0.1~1μm on the surface of the current sample; the material of the second P-type epitaxial layer is any one of 4H-SiC, 3C-SiC and 6H-SiC.

8. The method for realizing a SiC high-mobility UMOSFET trench according to claim 3, characterized in that, Step 5 specifically includes: A thick implantation mask layer (41) is grown on the second P-type epitaxial layer (3), and the thick implantation mask layer (41) inside the trench and at the corners on both sides of the trench is etched by photolithography to expose the surface of the second P-type epitaxial layer (3); A thin injection mask layer is grown on the surface of the current sample (42); N is performed at the bottom of the trench and at the corners of the opening based on a thin implantation mask layer (42) + Ion implantation; The thick injection mask layer (41) and the thin injection mask layer (42) are stripped off.