Light Emitting Diode and its Fabrication Method
By introducing a superlattice structure into the light-emitting diode (LED), the compressive and tensile stresses introduced by Mg and Si doping in the composite semiconductor layer cancel each other out, thus solving the stress imbalance problem in the epitaxial growth process and achieving high-yield and high-efficiency LED fabrication.
Patent Information
- Application Number
- CN202611339266.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-31
- Publication Date
- 2026-11-17
AI Technical Summary
In the prior art, stress imbalance caused by lattice mismatch and thermal mismatch during the epitaxial growth of GaN-based light-emitting diodes leads to epitaxial wafer warping and cracking, affecting product yield.
By employing a superlattice structure, and alternately stacking a first sublayer and a second sublayer doped with different dopants in a composite semiconductor layer, the compressive stress and tensile stress introduced by Mg and Si doping cancel each other out, thus achieving stress self-compensation at the nanoscale.
It effectively reduces the macroscopic warpage of epitaxial wafers, suppresses crack formation, improves epitaxial growth yield, and enhances luminous efficiency and chip integrity.
Smart Images

Figure CN123124524A_ABST
Abstract
Description
Technical Field
[0001] This disclosure belongs to the field of semiconductor fabrication technology, and specifically relates to a light-emitting diode and its fabrication method. Background Technology
[0002] Light-emitting diodes (LEDs), as a new generation of solid-state light sources, have advantages such as high efficiency, energy saving, and long lifespan, and are widely used in display, lighting, and backlighting fields. Gallium nitride (GaN)-based materials are the mainstream system for fabricating blue-green LEDs, which are typically grown epitaxially on heterogeneous substrates using metal-organic chemical vapor deposition (MOCVD) technology.
[0003] Due to significant lattice and thermal mismatches between GaN and conventional substrates (such as sapphire and silicon substrates), enormous stress is generated during epitaxial growth. To relieve this stress and filter dislocations, a three-dimensional growth layer is grown on top of the nucleation layer in related technologies. This layer is typically unintentionally doped GaN or GaN doped with a single silicon Si layer.
[0004] However, in related conventional techniques, single doping or no doping cannot effectively balance the tensile stress accumulated during epitaxial growth, which makes the epitaxial wafer prone to severe warping or even cracking, resulting in low product yield. Summary of the Invention
[0005] This disclosure provides a light-emitting diode and its fabrication method, which can effectively solve problems such as epitaxial cracking and wafer warpage. The technical solution is as follows: In a first aspect, embodiments of this disclosure provide a light-emitting diode, comprising: a composite semiconductor layer, a first semiconductor layer, a light-emitting layer, and a second semiconductor layer stacked sequentially; The first semiconductor layer is doped with a first dopant, and the second semiconductor layer is doped with a second dopant, wherein the first dopant is different from the second dopant; The composite semiconductor layer has a superlattice structure and includes a first sublayer and a second sublayer that are periodically and alternately stacked. The first sublayer is doped with the second dopant, and the second sublayer is doped with the first dopant.
[0006] In one implementation of this disclosure, the second dopant is Mg, and the doping concentration of Mg is 4 × 10⁻⁶. 17 cm -3 ~6×10 17 cm -3 .
[0007] In another implementation of this disclosure, the thickness of the first sublayer is 5-7 nm.
[0008] In another implementation of this disclosure, the first dopant is Si, and the Si doping concentration is 4 × 10⁻⁶. 17 cm -3 ~6×10 17 cm -3 .
[0009] In another implementation of this disclosure, the thickness of the second sublayer is 5-7 nm.
[0010] In another implementation of this disclosure, both the first sub-layer and the second sub-layer are intentionally doped GaN layers.
[0011] In another implementation of this disclosure, the light-emitting diode further includes: a two-dimensional merging layer; The two-dimensional merging layer is located between the composite semiconductor layer and the first semiconductor layer, and the two-dimensional merging layer is an unintentionally doped GaN layer.
[0012] Secondly, embodiments of this disclosure provide a method for fabricating a light-emitting diode, the method comprising: A composite semiconductor layer, a first semiconductor layer, a light-emitting layer, and a second semiconductor layer are sequentially prepared. The first semiconductor layer is doped with a first dopant, and the second semiconductor layer is doped with a second dopant. The first dopant is different from the second dopant. The composite semiconductor layer is a superlattice structure. The composite semiconductor layer includes a first sublayer and a second sublayer that are periodically and alternately stacked. The first sublayer is doped with the second dopant, and the second sublayer is doped with the first dopant.
[0013] In another implementation of this disclosure, the fabrication of the composite semiconductor layer includes: Set the temperature to 1000~1100℃, the pressure to 200~400 torr, and the V / III ratio to 800~1500; The first sublayer and the second sublayer are grown alternately. When the first sublayer is grown, TMGa, NH3, and Cp2Mg are introduced for a first time. When the second sublayer is grown, TMGa, NH3, and SiH4 are introduced for a second time.
[0014] In another implementation of this disclosure, the first sub-layer and the second sub-layer are grown alternately, including: During the alternating growth of the first and second sublayers, NH3 and carrier gas are introduced to perform a purging operation.
[0015] The beneficial effects of the technical solutions provided in this disclosure are: The light-emitting diode provided in this embodiment effectively improves the stress imbalance and warping problems caused by a single-doped three-dimensional growth layer in related technologies by introducing a superlattice structure composed of a first sublayer and a second sublayer periodically stacked as a composite semiconductor layer.
[0016] In light-emitting diodes (LEDs), the second dopant in the first sublayer and the second semiconductor layer is an acceptor impurity, which causes lattice expansion, introducing compressive stress. Conversely, the first dopant in the second sublayer and the first semiconductor layer is a donor impurity, which causes lattice contraction, introducing tensile stress. These two opposing internal stresses cancel each other out at the alternating interfaces of the superlattice, achieving nanoscale stress self-compensation. This brings the net stress of the entire composite semiconductor layer close to equilibrium, significantly reducing the macroscopic warpage of the epitaxial wafer, suppressing crack formation, and improving the yield of epitaxial growth. Attached Figure Description
[0017] To more clearly illustrate the technical solutions in the embodiments of this disclosure, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of this disclosure. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0018] Figure 1 This is a schematic diagram of the structure of a light-emitting diode provided in an embodiment of this disclosure; Figure 2 This is a flowchart of a method for fabricating a light-emitting diode according to an embodiment of this disclosure; Figure 3 This is a flowchart of another method for fabricating a light-emitting diode provided in this embodiment.
[0019] The symbols in the diagram represent the following meanings: 10. Substrate; 20. Nucleation layer; 30. Composite semiconductor layer; 310, First sublayer; 320, Second sublayer; 40. Two-dimensional merging layer; 50. First semiconductor layer; 60. Emissive layer; 70. P-type electron blocking layer; 80. Second semiconductor layer.
[0020] The accompanying drawings have illustrated specific embodiments of this disclosure, which will be described in more detail below. These drawings and descriptions are not intended to limit the scope of the concept in any way, but rather to illustrate the concepts of this disclosure to those skilled in the art through reference to particular embodiments. Detailed Implementation
[0021] To make the objectives, technical solutions, and advantages of this disclosure clearer, the embodiments of this disclosure will be described in further detail below with reference to the accompanying drawings.
[0022] Figure 1 A schematic diagram of the structure of a light-emitting diode provided in an embodiment of this disclosure is shown below. Figure 1 The light-emitting diode includes a composite semiconductor layer 30, a first semiconductor layer 50, a light-emitting layer 60, and a second semiconductor layer 80 stacked sequentially.
[0023] The first semiconductor layer 50 is doped with a first dopant, and the second semiconductor layer 80 is doped with a second dopant. The first dopant is different from the second dopant. The composite semiconductor layer 30 has a superlattice structure and includes a first sublayer 310 and a second sublayer 320 that are periodically and alternately stacked. The first sublayer 310 is doped with the second dopant, and the second sublayer 320 is doped with the first dopant.
[0024] The light-emitting diode provided in this embodiment effectively improves the stress imbalance and warping problems caused by a single-doped three-dimensional growth layer in related technologies by introducing a superlattice structure composed of a first sublayer 310 and a second sublayer 320 periodically and alternately stacked on the nucleation layer 20 as a composite semiconductor layer 30.
[0025] In a light-emitting diode (LED), the second dopant in the first sublayer 310 and the second semiconductor layer 80 is an acceptor impurity, which causes lattice expansion, i.e., introduces compressive stress. Conversely, the first dopant in the second sublayer 320 and the first semiconductor layer 50 is a donor impurity, which causes lattice contraction, i.e., introduces tensile stress. These two opposing internal stresses cancel each other out at the alternating interfaces of the superlattice, achieving nanoscale stress self-compensation. This brings the net stress of the entire composite semiconductor layer 30 close to equilibrium, significantly reducing the macroscopic warpage of the epitaxial wafer, suppressing crack formation, and improving the yield of epitaxial growth.
[0026] In this embodiment, the second dopant in the first sublayer 310 is at least one of Mg, Zn, and Cd.
[0027] In the above implementation, by selecting at least one of Mg, Zn or Cd as the doping source, these impurity atoms can increase the local lattice constant when they substitute into the GaN lattice.
[0028] For example, Mg, as a shallow acceptor, can provide stable and controllable compressive stress and hole carriers. Zn, as a deep-level acceptor, can induce significant local lattice distortion and expansion without causing excessive free carriers to interfere with specific electrical designs. Cd, due to its larger atomic radius than the former two, can provide a good lattice expansion effect even at lower concentrations. In other words, regardless of which element or combination of elements is used, a clear compressive stress component can be stably injected into the first sublayer 310. This actively introduced compressive stress can reliably neutralize the tensile stress that naturally accumulates during growth.
[0029] In this embodiment, when the second dopant is Mg, the doping concentration of Mg is 4 × 10⁻⁶. 17 cm -3 ~6×10 17 cm -3 The thickness of the first sublayer 310 is 5~7nm.
[0030] In the above implementation, the Mg doping concentration is controlled within the aforementioned range, and the thickness of the first sublayer 310 is controlled within the range of 5~7 nm, so that the first sublayer 310 maintains good crystal quality while providing sufficient compressive stress. If the doping concentration is lower than 4×10⁻⁶, 17 cm -3 If the thickness is less than 5 nm, the total amount of compressive stress introduced is insufficient to completely neutralize the tensile stress of adjacent sublayers, and the epitaxial wafer will still experience indentation and warping due to residual tensile stress. If the doping concentration is higher than 6 × 10⁻⁶, the epitaxial wafer will still warp due to residual tensile stress. 17 cm -3 If the thickness is greater than 7nm, excessive Mg atoms will aggregate or precipitate in the crystal lattice, destroying the single crystal structure of GaN and increasing non-radiative recombination defects, thus affecting the chip's luminous efficiency.
[0031] In this embodiment, the first dopant is at least one of Si, Ge, and O.
[0032] In the above implementation, by selecting at least one of Si, Ge or O as the doping source, these atoms can cause effective local lattice contraction when they enter the crystal lattice.
[0033] For example, Si, as a shallow donor, can provide uniform lattice contraction (i.e., tensile stress) and good conductivity when substituting Ga atoms. Ge also substitutes Ga atoms, but at high doping concentrations, it is less likely to induce surface roughening. O achieves lattice contraction by substituting N atoms, providing an alternative crystallographic stress control method for technical solutions that do not wish to excessively interfere with Ga atom lattice sites. In other words, any of the above elements can steadily construct a tensile stress field within the material. This tensile stress field, together with the compressive stress field of the aforementioned first sublayer 310, forms a strong alternating "tensile stress" and "compressive stress" fluctuation, forcing bottom penetrating dislocations to bend at large angles and annihilate each other when passing through the interface, ensuring stress balance and improving dislocation filtering efficiency.
[0034] In this embodiment, when the first dopant is Si, the Si doping concentration is 4 × 10⁻⁶. 17 cm -3 ~6×10 17 cm -3 The thickness of the second sublayer 320 is 5~7nm.
[0035] In the above implementation, the Si doping concentration is controlled within the aforementioned range, and the thickness of the second sublayer 320 is controlled within the range of 5~7 nm, so that the tensile stress level generated by it exactly matches the compressive stress generated by the first sublayer 310. If the doping concentration is lower than 4×10⁻⁶, 17 cm -3 If the thickness is less than 5 nm, the tensile stress is insufficient, and the overall structure will exhibit bulging and warping dominated by compressive stress. If the doping concentration is higher than 6 × 10⁻⁶, the tensile stress will be insufficient, and the overall structure will exhibit bulging and warping dominated by compressive stress. 17 cm -3 If the thickness is greater than 7nm, it will not only cause excessive tensile stress leading to epitaxial cracking, but also cause severe surface roughening due to excessive Si concentration.
[0036] See also Figure 1 In this embodiment, the first semiconductor layer 50 is a Si-doped GaN layer with a thickness of 1.5 μm, and the light-emitting layer 60 is a multi-quantum-well layer, which is composed of periodically alternating layers of In. 0.15 Ga 0.85 Composed of N-layers and GaN-layers, In 0.15 Ga 0.85 The N layer has a thickness of 3 nm, the GaN layer has a thickness of 10 nm, and the second semiconductor layer 80 is a Mg-doped GaN layer with a thickness of 150 nm.
[0037] In the above implementation, electrons and holes can achieve efficient recombination and light emission in the light-emitting layer 60, thus completing the efficient conversion of electrical energy into light energy.
[0038] See also Figure 1In this embodiment, the light-emitting diode further includes a substrate 10 and a nucleation layer 20 stacked on the substrate 10.
[0039] In this embodiment, the light-emitting diode further includes a two-dimensional merging layer 40. The two-dimensional merging layer 40 is located on the side of the composite semiconductor layer 30 facing away from the nucleation layer 20, that is, between the composite semiconductor layer 30 and the first semiconductor layer 50. The two-dimensional merging layer 40 is an unintentionally doped GaN layer.
[0040] In the above implementation, the two-dimensional merging layer 40 fills in the pits and depressions left by the underlying composite semiconductor layer 30. Since the penetrating dislocations in the underlying layer are largely bent and annihilated when passing through the superlattice interface, the two-dimensional merging layer 40 can obtain a high-quality single-crystal surface with low dislocation density, thus providing a smooth and low-defect-density high-quality platform for the subsequent growth of the core light-emitting active region.
[0041] It is worth noting that, compared to the two-dimensional merging layer 40, the composite semiconductor layer 30 is a three-dimensional growth layer.
[0042] See also Figure 1 In this embodiment, the light-emitting diode further includes a P-type electron blocking layer 70, which is located between the light-emitting layer 60 and the second semiconductor layer 80.
[0043] Among them, the P-type electron blocking layer 70 is Al 0.2 Ga 0.8 The N-layer has a thickness of 20nm.
[0044] The light-emitting diodes provided in this disclosure have at least the following technical effects: (1) Stress self-compensation.
[0045] By utilizing the compressive stress introduced by Mg and the tensile stress introduced by Si to cancel each other out at the nanoscale, near-zero net stress of the composite semiconductor layer 30 is achieved, which significantly reduces epitaxial wafer warpage, suppresses crack formation, and improves yield by more than 2%.
[0046] (2) High efficiency in filtering dislocations.
[0047] The periodic stress field of the composite semiconductor layer 30 forces through dislocations to bend and annihilate at multiple Mg / Si superlattice interfaces, reducing the dislocation density of the upper GaN layer to less than 2 × 10⁻⁶. 8 cm -2 The crystal quality has been significantly improved.
[0048] (3) Enhance hole injection.
[0049] Two-dimensional holes are generated at the Mg / Si superlattice interface due to the polarization effect, providing an additional lateral hole injection path for the active region and improving the luminous efficiency by 3% to 5%. Furthermore, the Si-doped second sublayer 320 provides a highly conductive channel, while the ultrathin Mg-doped first sublayer 310 does not increase the vertical resistance, thus reducing the forward operating voltage by approximately 0.01 to 0.02 V.
[0050] (4) Optimize the laser ablation process.
[0051] In the superlattice structure of the composite semiconductor layer 30, the defect levels and periodic interfaces introduced by Mg doping can enhance the absorption of exfoliation lasers (such as 248nm and 355nm), enabling precise energy deposition at the target interface and avoiding exfoliation failure due to insufficient absorption. The multilayer heterogeneous interface can act as a "stress buffer spring," absorbing and dispersing the stress waves generated by thermal shock during exfoliation, preventing cracking of the epitaxial layer.
[0052] Experiments show that using the light-emitting diodes provided in this disclosure, the chip integrity after laser lift-off can be improved to over 95%. After lift-off, the stress compensation mechanism of the Mg / Si superlattice in the epitaxial layer continues to function, reducing residual stress in the thin film by more than 50%, which is beneficial for subsequent bonding, photolithography, and other processes. For AlGaN-based UVC-LEDs, the AlN buffer layer is transparent to lasers, while the Mg / Si superlattice can effectively absorb laser light, providing a feasible solution for substrate lift-off of UVC-LEDs.
[0053] Figure 2 This is a flowchart illustrating a method for fabricating a light-emitting diode (LED) according to an embodiment of the present disclosure, in conjunction with... Figure 2 In this embodiment, the preparation method includes: Step 201: Prepare composite semiconductor layer 30.
[0054] Step 202: Prepare the first semiconductor layer 50.
[0055] Step 203: Prepare the light-emitting layer 60.
[0056] Step 204: Prepare the second semiconductor layer 80.
[0057] The first semiconductor layer 50 is doped with a first dopant, and the second semiconductor layer 80 is doped with a second dopant. The first dopant is different from the second dopant. The composite semiconductor layer 30 has a superlattice structure and includes a first sublayer 310 and a second sublayer 320 that are periodically and alternately stacked. The first sublayer 310 is doped with a second dopant, and the second sublayer 320 is doped with a first dopant.
[0058] In the fabrication method provided in this disclosure, the light-emitting diode obtained by introducing a superlattice structure composed of a first sublayer 310 and a second sublayer 320 periodically and alternately stacked on the nucleation layer 20 as a composite semiconductor layer 30 effectively improves the stress imbalance and warping problems caused by a single doped three-dimensional growth layer in related technologies.
[0059] In a light-emitting diode (LED), the second dopant in the first sublayer 310 and the second semiconductor layer 80 is an acceptor impurity, which causes lattice expansion, i.e., introduces compressive stress. Conversely, the first dopant in the second sublayer 320 and the first semiconductor layer 50 is a donor impurity, which causes lattice contraction, i.e., introduces tensile stress. These two opposing internal stresses cancel each other out at the alternating interfaces of the superlattice, achieving nanoscale stress self-compensation. This brings the net stress of the entire composite semiconductor layer 30 close to equilibrium, significantly reducing the macroscopic warpage of the epitaxial wafer, suppressing crack formation, and improving the yield of epitaxial growth.
[0060] Figure 3 A flowchart illustrating another method for fabricating a light-emitting diode provided in this disclosure, in conjunction with... Figure 3 In this embodiment, the preparation method includes: Step 301: Provide a substrate 10.
[0061] For example, substrate 10 is a sapphire substrate or a silicon substrate.
[0062] Step 302: Pre-treat the substrate 10.
[0063] For example, the substrate 10 is placed in the reaction chamber, heated to 1050°C~1100°C, and heat-treated in H2 atmosphere for 5~10 minutes to remove oxides that may exist on the surface of the substrate 10.
[0064] Step 303: Prepare a core layer 20 on one side of the substrate 10.
[0065] For example, an AlN layer is deposited as a nucleation layer 20 using an MOCVD (Metal-Organic Chemical Vapor Deposition) apparatus.
[0066] For example, the temperature is set to 750~850℃, TMGa and NH3 are introduced, the pressure is 100~300 torr, and the growth thickness is 15~30nm.
[0067] For example, the nucleation layer 20 is annealed by turning off TMGa, raising the temperature to 1000℃~1050℃, and annealing in an NH3 atmosphere for 30~60 seconds to recrystallize the nucleation layer 20.
[0068] Step 304: Prepare a composite semiconductor layer 30 on one side of the nucleation layer 20.
[0069] For example, the temperature is set to 1000~1100℃, the pressure is set to 200~400 torr, and the V / III ratio is set to 800~1500. Steps 3041 and 3042 are performed alternately.
[0070] Step 3041: Grow the first sublayer 310.
[0071] For example, TMGa, NH3, and Cp2Mg are introduced continuously for a first time to grow a Mg-doped GaN layer with a thickness of 1~10 nm. That is, the first sublayer 310 uses Mg as the second dopant.
[0072] Step 3042: Grow the second sublayer 320.
[0073] For example, TMGa, NH3, and SiH4 are introduced and the process is continued for a second time to grow a Si-doped GaN layer with a thickness of 1-10 nm. That is, the second sublayer 320 uses Si as the first dopant.
[0074] It is worth noting that after step 3041 is completed, the introduction of Cp2Mg is stopped, and after step 3042 is completed, the introduction of SiH4 is stopped.
[0075] In addition, to further prevent Mg and Si from undergoing pre-reaction in the gas phase, NH3 and carrier gas can be introduced into the gap between steps 3041 and 3042 to perform a purging operation.
[0076] The carrier gases are H2 and N2.
[0077] Step 305: Grow a two-dimensional merging layer 40 on one side of the composite semiconductor layer 30.
[0078] For example, the temperature is raised to 1100°C~1150°C and the pressure is 200 torr to grow an unintentionally doped GaN layer with a thickness of 1~2 μm as a two-dimensional merging layer 40.
[0079] In other embodiments, a lightly Si-doped GaN layer may also be grown as a two-dimensional merging layer 40.
[0080] Step 306: Prepare the first semiconductor layer 50.
[0081] For example, a Si-doped GaN layer with a thickness of 1-2 μm is grown by introducing SiH4 while maintaining a temperature of 1050℃~1100℃ as the first semiconductor layer 50. The Si doping concentration is 1.5 × 10⁻⁶. 19 2.5×1019 cm -3 .
[0082] Step 307: Prepare the light-emitting layer 60.
[0083] For example, the temperature is lowered to 700℃~780℃, the pressure is 200 torr, and N2 is used as the carrier gas for periodic alternating growth of In. 0.15 Ga 0.85 N quantum well layer and GaN quantum barrier layer.
[0084] Among them, In 0.15 Ga 0.85 The thickness of the N quantum well layer is 2~4nm, the thickness of the GaN quantum barrier layer is 8~12nm, and the number of alternating periods is 8~13.
[0085] Step 308: Prepare a P-type electron blocking layer 70.
[0086] For example, the temperature is raised to 950℃~1000℃ to grow a P-type AlGaN layer with a thickness of 10~30nm as a P-type electron blocking layer 70, with an Al composition of 0.15~0.25.
[0087] Step 309: Prepare the second semiconductor layer 80.
[0088] For example, a P-type GaN layer with a thickness of 100-200 nm is grown at a temperature of 950°C to 1000°C as the second semiconductor layer 80, with a Mg doping concentration of 1×10⁻⁶. 19 ~1×10 20 cm -3 .
[0089] After step 309 is completed, the epitaxial wafer is removed after cooling to room temperature under NH3 protection.
[0090] Unless otherwise defined, the technical or scientific terms used herein shall have the ordinary meaning understood by one of ordinary skill in the art to which this disclosure pertains. The terms “first,” “second,” “third,” and similar terms used in this patent application specification and claims do not indicate any order, quantity, or importance, but are merely used to distinguish different components. Similarly, the terms “an” or “a” and similar terms do not indicate a quantity limitation, but rather indicate the presence of at least one. The terms “comprising” or “including” and similar terms mean that the elements or objects preceding “comprising” or “including” encompass the elements or objects listed following “comprising” or “including” and their equivalents, and do not exclude other elements or objects. The terms “connected” or “linked” and similar terms are not limited to physical or mechanical connections, but can include electrical connections, whether direct or indirect. The terms “upper,” “lower,” “left,” “right,” etc., are used only to indicate relative positional relationships; when the absolute position of the described objects changes, the relative positional relationship may also change accordingly.
[0091] The above description is merely an optional embodiment of this disclosure and is not intended to limit this disclosure. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this disclosure should be included within the protection scope of this disclosure.
Claims
1. A light-emitting diode, characterized in that, include: A composite semiconductor layer (30), a first semiconductor layer (50), a light-emitting layer (60), and a second semiconductor layer (80) are stacked sequentially. The first semiconductor layer (50) is doped with a first dopant, and the second semiconductor layer (80) is doped with a second dopant, wherein the first dopant is different from the second dopant; The composite semiconductor layer (30) is a superlattice structure. The composite semiconductor layer (30) includes a first sublayer (310) and a second sublayer (320) that are periodically and alternately stacked. The first sublayer (310) is doped with the second dopant, and the second sublayer (320) is doped with the first dopant.
2. The light-emitting diode according to claim 1, characterized in that, The second dopant is Mg, and the Mg doping concentration is 4 × 10⁻⁶. 17 cm -3 ~6×10 17 cm -3 .
3. The light-emitting diode according to claim 1, characterized in that, The thickness of the first sublayer (310) is 5~7nm.
4. The light-emitting diode according to claim 1, characterized in that, The first dopant is Si, and the Si doping concentration is 4 × 10⁻⁶. 17 cm -3 ~6×10 17 cm -3 .
5. The light-emitting diode according to claim 1, characterized in that, The thickness of the second sublayer (320) is 5~7nm.
6. The light-emitting diode according to any one of claims 1 to 5, characterized in that, Both the first sublayer (310) and the second sublayer (320) are intentionally doped GaN layers.
7. The light-emitting diode according to any one of claims 1 to 5, characterized in that, Also includes: Two-dimensional merging layer (40); The two-dimensional merging layer (40) is located between the composite semiconductor layer (30) and the first semiconductor layer (50), and the two-dimensional merging layer (40) is an unintentionally doped GaN layer.
8. A method for fabricating a light-emitting diode, characterized in that, include: A composite semiconductor layer (30), a first semiconductor layer (50), a light-emitting layer (60), and a second semiconductor layer (80) are sequentially prepared. The first semiconductor layer (50) is doped with a first dopant, and the second semiconductor layer (80) is doped with a second dopant. The first dopant is different from the second dopant. The composite semiconductor layer (30) is a superlattice structure. The composite semiconductor layer (30) includes a first sublayer (310) and a second sublayer (320) that are periodically and alternately stacked. The first sublayer (310) is doped with the second dopant, and the second sublayer (320) is doped with the first dopant.
9. The preparation method according to claim 8, characterized in that, The preparation of the composite semiconductor layer (30) includes: Set the temperature to 1000~1100℃, the pressure to 200~400 torr, and the V / III ratio to 800~1500; The first sublayer (310) and the second sublayer (320) are grown alternately. When the first sublayer (310) is grown, TMGa, NH3 and Cp2Mg are introduced for a first time. When the second sublayer (320) is grown, TMGa, NH3 and SiH4 are introduced for a second time.
10. The preparation method according to claim 9, characterized in that, Alternating growth of the first sublayer (310) and the second sublayer (320) includes: During the alternating growth of the first sublayer (310) and the second sublayer (320), NH3 and carrier gas are introduced to perform a purging operation.