A multi-point COB packaging method, a light-emitting unit housing structure, and a light source module

By setting grooves on the board to fix the light-emitting unit and filling it with fluorescent glue, combined with parabolic reflective surface and high temperature curing, the problem of difficulty in controlling the size and angle accuracy of light-emitting points in multi-point COB packaging is solved, and high-precision lamp light pattern and light efficiency are improved.

CN123124547APending Publication Date: 2026-11-17SHANGHAI SANSI ELECTRONICS ENG +4
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510620223.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-14
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In multi-point COB packaging, the precision error of the dispensing machine and the flowability of the dammed adhesive make it difficult to control the size and angle of the light-emitting points, and the overall light pattern of the lamp is difficult to manage.

Method used

The method involves setting grooves on the board to fix the light-emitting unit and filling the grooves with fluorescent adhesive, omitting the damming step. By combining a parabolic reflective surface and a high-temperature curing process, a stable encapsulation structure is formed using high-refractive-index fluorescent adhesive and protective adhesive.

Benefits of technology

The accuracy of the light-emitting angle and the size of the light-emitting point of the light-emitting unit has been improved, ensuring the stability and luminous efficiency of the overall luminaire light pattern, and enhancing the mechanical strength and optical effect of the packaging structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124547A_ABST
    Figure CN123124547A_ABST
Patent Text Reader

Abstract

This application provides a multi-point COB packaging method, a light-emitting unit housing structure, and a light source module. The light-emitting unit housing structure includes: a board with multiple grooves and corresponding packaging pads arranged on it, wherein all the grooves have the same opening direction; and a groove for housing the light-emitting unit, the inner surface of which is provided with a reflective surface. The light-emitting unit is fixed at the bottom center of the groove, and the light emitted by the light-emitting unit is reflected by the reflective surface and emitted to the outside in the opening direction of the groove. By setting grooves on the board and fixing the light-emitting unit in the grooves, and filling the grooves with fluorescent adhesive, the step of using damming adhesive for damming is eliminated. This avoids the problems of light emission angle and light emission point size accuracy of the light-emitting unit caused by the error of the dispensing machine and the thixotropy and flowability of the damming adhesive, and also avoids the problem of difficulty in controlling the light pattern of the overall lamp.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of multi-point COB packaging method, light-emitting unit housing structure and light source module. Background Technology

[0002] Multi-point COB (Chip-on-Board) packaging involves directly mounting multiple wafers onto a single, unified packaging substrate. The chips are secured to the substrate using soldering or bonding methods, and appropriate optical and thermal management designs enhance the light source's performance and heat dissipation. Unlike traditional SMD packaging, multi-point COB packaging technology is better suited for high-power-density applications, offering higher brightness and luminous efficacy, making it suitable for high-power streetlights, floodlights, industrial lighting, and other fields.

[0003] In multi-point COB packaging, damming refers to the process of forming a physical enclosure around the LED chip using a gel-like material. The most common material is damming adhesive, which mainly provides space for subsequent phosphor filling, ensuring that the phosphor can be evenly covered on the surface of the LED chip.

[0004] However, due to the inherent errors in the precision of dispensing machines, they cannot meet the micron-level precision requirements. Furthermore, due to the fluidity of the damming adhesive itself, the size and position of the resulting dam are usually difficult to strictly control. As a result, it is difficult to control the precision of the size of a single light-emitting point and the precision of the light-emitting angle of a single light-emitting point in the module light source, and the overall light pattern of the lamp is also difficult to control. Summary of the Invention

[0005] In view of the shortcomings of the prior art described above, the purpose of this application is to provide a multi-point COB packaging method, a light-emitting unit housing structure, and a light source module to solve the above problems.

[0006] To achieve the above and other related objectives, a first aspect of this application provides a multi-point COB packaged light-emitting unit housing structure, comprising: a plate having a plurality of grooves and corresponding packaging pads arranged on the plate, wherein all the grooves have the same opening direction; and a groove for housing the light-emitting unit, wherein a reflective surface is provided on the inner surface of the groove, wherein the light-emitting unit is fixed at the bottom center position of the groove, and the light emitted by the light-emitting unit is reflected by the reflective surface and emitted to the outside in the opening direction of the groove.

[0007] In one embodiment of the first aspect of this application, the light-emitting unit is a wafer, which is fixed to the bottom center of the groove by a die-bonding material, and the positive and negative electrodes of the wafer are respectively connected to the packaging pads corresponding to the groove where the wafer is located by bonding wires.

[0008] In one embodiment of the first aspect of this application, a plurality of micropores or pits are uniformly provided on the reflective surface of the groove.

[0009] In one embodiment of the first aspect of this application, the reflective surface of the groove is curved and the cross-sectional view of the groove is parabolic, with the opening direction of the parabola being consistent with the opening direction of the groove.

[0010] To achieve the above and other related objectives, a second aspect of this application provides a multi-point COB packaging method, comprising: fixing each light-emitting unit in each groove of the light-emitting unit receiving structure of the multi-point COB package as described in any one of the preceding claims; electrically connecting each light-emitting unit to the packaging pad corresponding to its groove; preparing fluorescent adhesive and filling the fluorescent adhesive in each groove; and placing the multi-point COB package light-emitting unit receiving structure in an oven for high-temperature curing.

[0011] In one embodiment of the second aspect of this application, after the fluorescent adhesive is filled into each of the grooves, and before the multi-point COB-encapsulated light-emitting unit housing structure is placed in an oven for high-temperature curing, a damming adhesive is applied around the perimeter of the plate; after high-temperature curing, protective adhesive is filled into the damming area, and the multi-point COB-encapsulated light-emitting unit housing structure is placed in an oven again for high-temperature curing.

[0012] In one embodiment of the second aspect of this application, the fluorescent adhesive is made by mixing a two-component transparent silicone gel and a fluorescent powder.

[0013] In one embodiment of the second aspect of this application, the fluorescent adhesive, when its color rendering index is 70, comprises: 85.5% of a combined phosphor and 15.5% of an encapsulating adhesive; wherein the combined phosphor comprises: 70% of a green phosphor with an emission peak of 529nm-544nm, 7.5% of a red phosphor with an emission peak of 594nm-678nm, and 22.5% of a red phosphor with an emission peak of 630nm-640nm.

[0014] In one embodiment of the second aspect of this application, the fluorescent adhesive, when its color rendering index is 80, comprises: 85.5% of a combined phosphor and 15.5% of an encapsulating adhesive; wherein the combined phosphor comprises: 64.5% of a green phosphor with an emission peak of 529nm-544nm, 11.5% of a red phosphor with an emission peak of 594nm-678nm, and 24% of a red phosphor with an emission peak of 630nm-640nm.

[0015] To achieve the above and other related objectives, a third aspect of this application provides a multi-point COB packaged light source module, comprising: a multi-point COB packaged light-emitting unit housing structure as described in any one of the preceding claims; a light-emitting unit fixed in the multi-point COB packaged light-emitting unit housing structure; an array lens disposed on one side of the multi-point COB packaged light-emitting unit housing structure; and a heat sink attached and fixed to the other side of the multi-point COB packaged light-emitting unit housing structure.

[0016] As described above, this application has the following beneficial effects:

[0017] This application discloses a multi-point COB packaged light-emitting unit housing structure, comprising: a board body with multiple grooves and corresponding packaging pads arranged on the board body, wherein all the grooves have the same opening direction; and grooves for housing the light-emitting unit, wherein a reflective surface is provided on the inner surface of the groove, wherein the light-emitting unit is fixed at the bottom center position of the groove, and the light emitted by the light-emitting unit is reflected by the reflective surface and emitted to the outside in the opening direction of the groove. By providing grooves on the board body, fixing the light-emitting unit in the grooves, and filling the grooves with fluorescent adhesive, the step of using damming adhesive for damming is omitted, avoiding the problems of light emission angle and light emission point size accuracy of the light-emitting unit caused by the error of the dispensing machine and the thixotropy and flowability of the damming adhesive, and also avoiding the problem of difficulty in controlling the light pattern of the overall lamp. The beneficial effects of the multi-point COB packaging method and light source module disclosed in this application are consistent with the beneficial effects of the light-emitting unit housing structure. Attached Figure Description

[0018] Figure 1 The image shown is a side cross-sectional view of a multi-point COB package containing a light-emitting unit (including a light-emitting unit) according to an embodiment of this application.

[0019] Figure 2 Displayed as Figure 1 Region A in the text.

[0020] Figure 3 The image shown is a top view of a multi-point COB packaged light-emitting unit housing structure (including light-emitting units) according to an embodiment of this application.

[0021] Figure 4 Displayed as Figure 1 Region B in the text.

[0022] Figure 5 The diagram shown is a structural schematic of a multi-point COB packaged light source module in one embodiment of this application.

[0023] Component designation explanation

[0024] Multi-point COB packaged light-emitting single unit

[0025] Meta-accommodation structure

[0026] Board 11

[0027] Groove 12

[0028] Package pad 13

[0029] Light-emitting unit 2

[0030] Wire bonding 3

[0031] Protective adhesive 4

[0032] Array lens 5

[0033] Radiator 6 Detailed Implementation

[0034] The following specific examples illustrate the implementation of this application. Those skilled in the art can easily understand other advantages and effects of this application from the content disclosed in this specification. This application can also be implemented or applied through other different specific embodiments, and various details in this specification can also be modified or changed based on different viewpoints and applications without departing from the spirit of this application. It should be noted that, unless otherwise specified, the following embodiments and features in the embodiments can be combined with each other.

[0035] In the embodiments of this application, terms such as "first" and "second" are used to distinguish identical or similar items with essentially the same function and effect. For example, "first XX" and "second XX" are merely used to distinguish different XXs and do not limit their order. Those skilled in the art will understand that terms such as "first" and "second" do not limit the quantity or execution order, and that "first" and "second" do not necessarily imply that they are different.

[0036] It should be noted that, in the embodiments of this application, the words "exemplary" or "for example" indicate examples, illustrations, or descriptions. Any embodiment or design described as "exemplary" or "for example" in this application should not be construed as being more preferred or advantageous than other embodiments or designs. Specifically, the use of words such as "exemplary" or "for example" is intended to present the relevant concepts in a concrete manner.

[0037] In this application embodiment, "at least one" refers to one or more, and "more than one" refers to two or more. "And / or" describes the relationship between related objects, indicating that three relationships can exist. For example, A and / or B can represent: A alone, A and B simultaneously, or B alone, where A and B can be singular or plural. The character " / " generally indicates that the preceding and following related objects are in an "or" relationship. "At least one of the following" or similar expressions refer to any combination of these items, including any combination of single or plural items. For example, at least one of a, b, or c can represent: a, b, c, ab, ac, bc, or abc, where a, b, and c can be single or multiple.

[0038] To achieve the above and other related objectives, a first aspect of this application provides a multi-point COB packaged light-emitting unit 2 accommodating structure 1, comprising: a plate 11, wherein a plurality of grooves 12 and corresponding packaging pads 13 are arranged on the plate 11, wherein the opening direction of all the grooves 12 is consistent; a groove 12, wherein the groove 12 is used to accommodate the light-emitting unit 2, and a reflective surface is provided on the inner surface of the groove 12, wherein the light-emitting unit 2 is fixed at the bottom center position of the groove 12, and the light emitted by the light-emitting unit 2 is reflected by the reflective surface and emitted to the outside in the opening direction of the groove 12.

[0039] In traditional multi-point COB packaging, a planar plate 11 is used, with multiple wafers directly fixed on the plane of the substrate. When using phosphor adhesive for dispensing, it is necessary to first create a dam around each wafer, and then fill the dam with phosphor adhesive. The planar plate 11 has been widely used in electronic packaging, with a stable structure and mature manufacturing process. The plate 11 itself is usually used to provide support, connection and heat dissipation functions. Those skilled in the art are accustomed to arranging multiple LED chips evenly on the planar substrate, because this method is simple and easy to implement and can meet most application requirements. However, the present invention omits the damming step by setting multiple grooves 12 on the plate 11 to fix each wafer separately. It also avoids the problems of the emission angle and emission point size accuracy of the light-emitting unit 2 caused by the error of the dispensing machine and the thixotropy and flowability of the damming adhesive, and also avoids the problem of difficulty in controlling the light pattern of the overall lamp.

[0040] In one embodiment of the first aspect of this application, the light-emitting unit 2 is a wafer, which is fixed to the bottom center of the groove 12 by a die-bonding material, and the positive and negative electrodes of the wafer are respectively connected to the encapsulation pads 13 corresponding to the groove 12 where the wafer is located via bonding wires 3.

[0041] Wafers are the most basic and critical semiconductor material in modern electronic and optoelectronic devices. Made from high-purity semiconductor single-crystal materials, they are the foundational material for manufacturing various LEDs. The quality and processing technology of wafers directly affect the performance, efficiency, and reliability of the final electronic components. After the overall wafer is cut into smaller wafers, a metal layer is typically deposited on the back of the smaller wafers to form electrodes. Preferably, the die-bonding material includes die-bonding adhesive or die-bonding film. The die-bonding adhesive has high viscosity, high temperature resistance, and vibration resistance, and is relatively inexpensive. Existing processes are mature, but it requires high-temperature curing, which may cause stress damage to the heat-sensitive devices inside the lamp. Die-bonding film, also known as DAF film, has good thermal conductivity and corrosion resistance. Using die-bonding film instead of die-bonding adhesive can reduce thermal stress, thereby improving heat dissipation efficiency. Preferably, the bonding wire 3 connecting the wafer and the packaging pad 13 includes gold wire, copper wire, or aluminum wire. The gold wire has good conductivity and strong oxidation resistance, making it suitable for high-frequency, high-reliability applications. The copper wire has a lower cost and better current carrying capacity, but poorer oxidation resistance, making it suitable for high-current applications. The aluminum wire has the lowest cost, but weaker mechanical strength.

[0042] Preferably, each pair of the package pads 13 is symmetrically distributed on both sides of each groove 12 with the groove 12 as the center. Due to the difference in the coefficients of thermal expansion between the wafer and the substrate 11, tensile or compressive stress will be generated when the temperature changes. In addition, the electromagnetic force or vibration generated by the current passing through the bonding wire 3 during operation can be mitigated by the symmetrical distribution of the positive and negative package pads 13, which can uniformize the stress and prevent the bonding wire 3 on one side from bearing excessive tensile or bending loads. Furthermore, the symmetrical layout can offset the local deformation caused by the difference in CTE.

[0043] In one embodiment of the first aspect of this application, a plurality of micro-holes or pits are uniformly disposed on the reflective surface of the groove 12. The micro-holes or pits alter the light propagation path, causing multiple reflections on the surface. Due to the variability of the reflection angle and path, light scattering and loss are reduced, allowing more light rays to be ultimately guided to the desired direction, thereby improving the brightness and luminous efficacy of the light source. Furthermore, the uniform distribution of the micro-holes or pits helps to form a more uniform light field, avoiding bright spots or shadows, which is particularly important in applications requiring wide-angle lighting.

[0044] In one embodiment of the first aspect of this application, the reflective surface of the groove 12 is curved and the cross-sectional view of the groove 12 is parabolic, with the opening direction of the parabola being consistent with the opening direction of the groove 12.

[0045] It should be understood that when light from a light source strikes a parabolic reflective surface, all incident rays are reflected to the same focal point according to the geometric properties of a parabola. Therefore, designing the reflective surface as a parabola significantly improves light concentration, avoiding scattering and dispersion. Compared to traditional planar reflective surfaces, parabolic reflective surfaces can concentrate more light into a specific direction, thereby improving the optical efficiency of the light-emitting unit 2. Furthermore, by precisely designing the opening direction and reflection angle of the parabola, the directional output of light can be better controlled. In certain applications, such as those requiring highly efficient directional light sources, this design ensures the directionality and focus of the beam, further improving the lighting effect and light source utilization.

[0046] To achieve the above and other related objectives, a second aspect of this application provides a multi-point COB packaging method, comprising: fixing each light-emitting unit 2 in each groove 12 of the light-emitting unit 2 receiving structure 1 of the multi-point COB package as described in any one of the preceding claims; electrically connecting each light-emitting unit 2 to the packaging pad 13 corresponding to its groove 12; preparing fluorescent adhesive and filling the fluorescent adhesive in each groove 12; and placing the multi-point COB package light-emitting unit 2 receiving structure 1 in an oven for high-temperature curing.

[0047] In the multi-point COB packaging process, each light-emitting unit 2 is first precisely placed into the recess 12, ensuring its correct position within the housing structure. Preferably, the design of each recess 12 can be customized according to the size and shape of the light-emitting unit 2 to ensure a stable fixation and provide sufficient space for subsequent electrical connections. Next, each light-emitting unit 2 is electrically connected to the pads on the packaging substrate by soldering. This process ensures that the light-emitting unit 2 can correctly receive current and emit light stably. The soldering method typically employs high-precision automated equipment to ensure soldering quality and electrical performance stability. Phosphor adhesive is an important component in COB packaging, mainly used to modify or homogenize the light emitted by the light source. A suitable phosphor adhesive can perform color conversion or improve the luminous efficiency of the light emitted by the light-emitting unit 2. When filling with phosphor adhesive, it is necessary to ensure that the phosphor adhesive layer is evenly distributed within each recess 12 to ensure maximum optical effect. High-temperature curing is a key step to ensure that the fluorescent adhesive is uniformly cured and tightly bonded to the substrate during encapsulation. This process is usually carried out in an oven. By controlling the temperature and time, the fluorescent adhesive reaches the optimal curing state, enhancing its mechanical strength and anti-aging properties, and ensuring that the light-emitting unit 2 does not experience fluorescent adhesive peeling or performance degradation during long-term operation.

[0048] In one embodiment of the second aspect of this application, after the fluorescent adhesive is filled into each of the grooves 12, and before the multi-point COB-encapsulated light-emitting unit 2 housing structure 1 is placed in an oven for high-temperature curing, a damming adhesive is applied around the perimeter of the plate 11. After high-temperature curing, protective adhesive 4 is filled into the dammed area, and the multi-point COB-encapsulated light-emitting unit 2 housing structure 1 is placed in an oven again for high-temperature curing. The function of the damming adhesive is to form a dammed area around the entire plate 11 to limit the flow range of the subsequent protective adhesive 4, ensuring that the protective adhesive 4 is only filled in the required locations. The damming adhesive generally has high adhesion and a certain degree of flexibility, forming a solid closed area to prevent the protective adhesive 4 from flowing to undesirable areas during curing. After the damming adhesive is set, the entire multi-point COB-encapsulated light-emitting unit 2 housing structure 1 is placed in an oven for the first high-temperature curing. This step ensures that the fluorescent adhesive and the damming adhesive are cured at a suitable temperature to increase mechanical strength and ensure that all materials are firmly bonded. After the first curing, the protective adhesive 4 is then filled. Protective adhesive 4 is a specially designed adhesive typically used to encapsulate the entire light-emitting unit 2 and its related components. Protective adhesive 4 provides additional protection and enhances the overall structure's resistance to shock and pressure. Protective adhesive 4 is usually filled within the containment area to further seal and protect the light-emitting unit 2. After filling with protective adhesive 4, the multi-point COB-encapsulated light-emitting unit 2 housing structure 1 is placed in an oven for a second high-temperature curing. The purpose of this second curing is to ensure that the protective adhesive 4 is fully cured at the appropriate temperature, forming a robust and stable encapsulation structure capable of withstanding the physical pressure, temperature changes, and long-term optical loads from the external environment.

[0049] Preferably, the damming adhesive is made of epoxy resin and silicone. Epoxy resin has good thermosetting properties, adhesion, and strength. Silicone has good high-temperature resistance and flexibility. Preferably, the protective adhesive 4 is made of epoxy resin, silicone, and polyurethane resin. The polyurethane resin has good impact resistance and abrasion resistance. It should be understood that the damming adhesive is used to form a physical isolation zone, control the flow range of the protective adhesive 4, and enhance the stability of the encapsulation structure. The protective adhesive 4 is an adhesive used to fill and seal the entire light-emitting unit 2 during the encapsulation process. It not only protects the light-emitting unit 2 from external influences but also enhances the mechanical strength and optical effect of the encapsulation.

[0050] In one embodiment of the second aspect of this application, the fluorescent adhesive is made by mixing a two-component transparent silicone gel and a fluorescent powder.

[0051] It should be understood that a higher refractive index allows more light to enter the protective adhesive 4 from the surface of the light-emitting unit 2 and be effectively emitted to the outside, thus reducing light loss. Therefore, using silicone with a high refractive index can maximize the light output efficiency of the entire encapsulation system. Furthermore, transparency is crucial for light propagation; a transparent colloid ensures that the optical fiber emitted by the light-emitting unit 2 is not blocked or discolored, thus maintaining high-quality light output. In addition, a highly transparent colloid can maximize the utilization of the light source's luminous efficiency, ensuring stable color and brightness of the light output. Silicone has good stability at high temperatures, thus it can withstand the heat generated by the light-emitting unit 2 during operation, avoiding deformation, aging, or performance degradation of the colloid due to temperature changes, thereby improving the lifespan of the entire light source module. The two-component silicone provides good mechanical strength after curing, while also possessing sufficient flexibility to adapt to thermal expansion and contraction during the operation of the light source module, thus preventing cracking of the encapsulation material or glass, enhancing structural stability. The role of phosphor is to convert the blue or ultraviolet light emitted by the wafer into the desired visible light. High-efficiency phosphor can absorb the light emitted by the emitter to the maximum extent and convert it into visible light with higher intensity and more uniform color.

[0052] In one embodiment of the second aspect of this application, the fluorescent adhesive, when its color rendering index is 70, comprises: 85.5% of a combined phosphor and 15.5% of an encapsulating adhesive; wherein the combined phosphor comprises: 70% of a green phosphor with an emission peak of 529nm-544nm, 7.5% of a red phosphor with an emission peak of 594nm-678nm, and 22.5% of a red phosphor with an emission peak of 630nm-640nm.

[0053] The Color Rendering Index (CRI) measures a light source's ability to reproduce the true colors of objects. A maximum score of 100 indicates that the color of an object under illumination is closer to its true color under natural light. Light sources with a CRI greater than 80 are typically used in office and indoor lighting, where certain color reproduction requirements exist. CRIs greater than 90 are typically used in demanding environments such as medical, photography, and precision manufacturing. CRIs around 70 are generally used in outdoor lighting and some industrial and mining lighting scenarios, balancing brightness and cost while emphasizing luminous efficiency. Preferably, in this embodiment, a CRI of 70 is set to maximize luminous efficiency and cost control while ensuring a certain level of color reproduction capability. This is ideal for applications requiring high brightness and long lifespan but with moderate color reproduction requirements, such as road lighting and warehouse lighting.

[0054] Preferably, the composition of the encapsulating adhesive is the same as that of the protective adhesive 4 filled within the dam, both being two-component transparent silicone rubber. The encapsulating adhesive is used here to coat and fix the phosphor onto the surface of the light-emitting chip, providing mechanical protection and promoting optical and thermal stability. Preferably, when the encapsulating adhesive accounts for 15.5% of the phosphor, it ensures uniform dispersion of the phosphor while providing a good supporting structure and preventing light decay or powder sedimentation. The 529–544nm wavelength range is a bright and clear mid-green band, where the human eye has the highest sensitivity (peak value approximately 555nm), resulting in the strongest visual brightness. This band provides dominant brightness output, significantly increasing luminous flux and compensating for the shortcomings of blue chips in the green portion, enhancing overall light sensitivity. The green phosphor with a emission peak of 529nm-544nm accounts for as much as 70% to maximize the human eye's high perception of green and achieve maximum luminous efficiency. Red phosphors with an emission wavelength of 594nm-678nm cover the orange-red to deep red region, offering broad coverage and encompassing the reflected colors of most common objects. They provide broad-spectrum compensation, enhancing color rendering in the red region and improving the realism of objects such as faces, wood, and skin under illumination. They also contribute to improving the color rendering index. Although their proportion is relatively low, they have a significant effect on completing the spectrum. When the proportion of red phosphors with an emission wavelength of 594nm-678nm is 7.5%, the conversion efficiency is relatively low, thus allowing for better control of energy consumption and heat load. Red phosphors with an emission peak of 630nm-640nm are located in the deep red light range and are an important source of visual warmth. They can enhance the warmth of the color temperature, adjust the overall light color to lean towards natural light (neutral white or warm white), avoid a cool light source, and also enhance the recognition of red details. This formulation ratio allows green phosphor to dominate the output, making it suitable for energy-saving lighting with high luminous efficacy. It also uses red phosphor for adjustment, mixing warm tones to output neutral to warm white light, enabling color temperature control. Furthermore, it uses broadband and narrowband red light to complete the red end of the spectrum, achieving a color rendering index of 70, thus meeting the needs of most application scenarios.

[0055] In one embodiment of the second aspect of this application, the fluorescent adhesive, when its color rendering index is 80, comprises: 85.5% of a combined phosphor and 15.5% of an encapsulating adhesive; wherein the combined phosphor comprises: 64.5% of a green phosphor with an emission peak of 529nm-544nm, 11.5% of a red phosphor with an emission peak of 594nm-678nm, and 24% of a red phosphor with an emission peak of 630nm-640nm.

[0056] Preferably, the green phosphor with an emission peak of 529nm–544nm accounts for 64.5% of the formulation. This proportion is moderately reduced while ensuring high luminous efficacy, allowing for better color rendering performance. The red phosphor with an emission peak of 594nm–678nm accounts for 11.5%. This proportion is moderately increased to compensate for the output gap of low-efficiency red light under high CRI requirements, achieving comprehensive color reproduction. The red phosphor with an emission peak of 630nm–640nm accounts for 24%, a further increase compared to the CRI 70 formulation, significantly enhancing red performance and providing key support for achieving a CRI of 80. This formulation ratio ensures that the green phosphor still dominates the output, thus preventing the overall luminous efficacy from being significantly weakened by CRI adjustment. Simultaneously, by appropriately increasing the proportion of broadband and deep red phosphors, the red end of the spectrum is effectively completed, giving the light source superior color reproduction capabilities and a CRI of 80. This makes it suitable for applications with higher requirements for light color quality, such as indoor office, commercial, and educational lighting.

[0057] To achieve the above and other related objectives, a third aspect of this application provides a multi-point COB packaged light source module, comprising: a multi-point COB packaged light-emitting unit 2 accommodating structure 1 as described in any one of the preceding claims; a light-emitting unit 2, the light-emitting unit 2 being fixed in the multi-point COB packaged light-emitting unit 2 accommodating structure 1; an array lens 5, the array lens 5 being disposed on one side of the multi-point COB packaged light-emitting unit 2 accommodating structure 1; and a heat sink 6, the heat sink 6 being attached and fixed to the other side of the multi-point COB packaged light-emitting unit 2 accommodating structure 1.

[0058] It should be understood that the principle and technical effect of the multi-point COB packaged light-emitting unit 2 accommodating structure 1 included in the multi-point COB packaged light source module are as described above, and will not be repeated here.

[0059] Preferably, the radiator 6 includes a finned heatsink 6, a heat pipe composite heatsink 6, or a one-piece die-cast aluminum heatsink 6. The finned heatsink 6 increases the heat exchange area by setting multiple sets of vertical fins on a metal base (such as aluminum or copper), suitable for natural convection or forced convection cooling with a fan. The heat pipe composite heatsink 6 integrates a heat pipe structure on the basis of a traditional finned structure, utilizing phase change heat transfer characteristics to rapidly guide heat from the heat source to a low-temperature region, improving overall thermal conductivity. The one-piece die-cast aluminum heatsink 6 has a compact structure and simplified manufacturing process, suitable for applications with limited space or high structural strength requirements.

[0060] Preferably, the array lens 5 includes a convex lens array, a freeform lens array, or a composite optical structure. A convex lens array refers to each light-emitting unit 2 corresponding to an independent micro-convex lens, which can achieve collimation, focusing, or diffusion, suitable for high-brightness projection or track lighting applications. A freeform lens array is an aspherical profile customized according to the spatial layout of the light-emitting unit 2 and the optical target, improving optical shaping capabilities and light energy utilization. A composite optical structure involves integrating microstructures (such as light diffusion textures, prism etching, etc.) into some of the array lenses 5 to achieve composite effects such as soft light, anti-glare, and uniform light.

[0061] The above description is merely a specific embodiment of this application, but the scope of protection of this application is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the technical scope disclosed in this application should be included within the scope of protection of this application. Therefore, the scope of protection of this application should be determined by the scope of the claims.

[0062] In summary, this application effectively overcomes the various shortcomings of the prior art and has high industrial application value.

[0063] The above embodiments are merely illustrative of the principles and effects of this application and are not intended to limit this application. Any person skilled in the art can modify or alter the above embodiments without departing from the spirit and scope of this application. Therefore, all equivalent modifications or alterations made by those skilled in the art without departing from the spirit and technical concept disclosed in this application should still be covered by the claims of this application.

Claims

1. A multi-point COB packaged light-emitting unit (2) accommodating structure (1), characterized in that, include: A board body (11) is provided with a plurality of grooves (12) and corresponding encapsulation pads (13) arranged on the board body (11), wherein all the grooves (12) have the same opening direction; A groove (12) is provided to accommodate the light-emitting unit (2). A reflective surface is provided on the inner surface of the groove (12). The light-emitting unit (2) is fixed at the bottom center of the groove (12). The light-emitting unit (2) is connected to the encapsulation pad (13) corresponding to the groove (12) by a bonding wire (3). The light emitted by the light-emitting unit (2) is reflected by the reflective surface and emitted to the outside in the opening direction of the groove (12).

2. The light-emitting unit (2) accommodating structure (1) of a multi-point COB package according to claim 1, characterized in that, The light-emitting unit (2) is a wafer, which is fixed to the bottom center of the groove (12) by a die-bonding material. The positive and negative electrodes of the wafer are respectively connected to the encapsulation pads (13) corresponding to the groove (12) where the wafer is located through bonding wires (3).

3. The light-emitting unit (2) accommodating structure (1) of a multi-point COB package according to claim 1, characterized in that, The reflective surface of the groove (12) is uniformly provided with multiple micropores or pits.

4. The light-emitting unit (2) accommodating structure (1) of a multi-point COB package according to claim 1, characterized in that, The reflective surface of the groove (12) is curved, and the cross-sectional view of the groove (12) is parabolic, with the opening direction of the parabola being consistent with the opening direction of the groove (12).

5. A multi-point COB packaging method, characterized in that, include: Each light-emitting unit (2) is fixed in each groove (12) of the multi-point COB package light-emitting unit (2) receiving structure (1) as described in any one of claims 1-4; Each light-emitting unit (2) is electrically connected to the encapsulation pad (13) corresponding to its groove (12); Prepare fluorescent adhesive and fill each of the grooves (12) with the fluorescent adhesive; The light-emitting unit (2) housing structure (1) of the multi-point COB package is placed in an oven for high-temperature curing.

6. A multi-point COB packaging method according to claim 5, characterized in that, After filling each of the grooves (12) with the fluorescent adhesive, and before placing the multi-point COB-encapsulated light-emitting unit (2) housing structure (1) into the oven for high-temperature curing, a ring of damming adhesive is applied around the plate (11); after high-temperature curing, protective adhesive (4) is filled in the damming area, and the multi-point COB-encapsulated light-emitting unit (2) housing structure (1) is placed into the oven again for high-temperature curing.

7. A multi-point COB packaging method according to claim 5, characterized in that, The fluorescent adhesive is made from a mixture of two-component transparent silicone and fluorescent powder.

8. A multi-point COB packaging method according to claim 6, characterized in that, The components of the fluorescent adhesive with a color development index of 70 include: 85.5% combined phosphor and 15.5% encapsulating adhesive; The components of the combined phosphor include: 70% green phosphor with emission peak of 529nm-544nm, 7.5% red phosphor with emission peak of 594nm-678nm, and 22.5% red phosphor with emission peak of 630nm-640nm.

9. A multi-point COB packaging method according to claim 6, characterized in that, The components of the fluorescent adhesive with a color development index of 80 include: 85.5% combined phosphor and 15.5% encapsulating adhesive; The components of the combined phosphor include: 64.5% green phosphor with emission peak of 529nm-544nm, 11.5% red phosphor with emission peak of 594nm-678nm, and 24% red phosphor with emission peak of 630nm-640nm.

10. A multi-point COB packaged light source module, characterized in that, include: The light-emitting unit (2) housing structure (1) of the multi-point COB package as described in any one of claims 1-4; Multiple light-emitting units (2) are fixed in the multi-point COB packaged light-emitting unit (2) accommodating structure (1); An array lens (5) is disposed on one side of the light-emitting unit (2) receiving structure (1) of the multi-point COB package, wherein the opening direction of the groove (12) of the light-emitting unit (2) receiving structure is facing; Heat sink (6) is attached and fixed to the other side of the housing structure (1) of the multi-point COB packaged light-emitting unit (2).