Extruded plastic pallet (1)

By using a glue-bonded design with two types of reinforcing elements and ribs, combined with extrusion and load-bearing press manufacturing, the high carbon footprint and high cost of pallets are solved, enabling low-carbon, low-cost, and repairable pallet manufacturing, reducing storage and transportation space.

CN123125153APending Publication Date: 2026-11-17AHIA WASTE TREATMENT PLANT
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202580003061.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-07-23
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing pallet manufacturing technologies suffer from high carbon footprints, are irreparable, costly, and require significant storage and transportation space.

Method used

The design employs two types of reinforcing elements and ribs connected by adhesive, combined with extrusion and load-bearing press manufacturing, to replace rotational molding and allow for on-site assembly.

Benefits of technology

It enables low-carbon footprint, repairable, and low-cost pallet manufacturing, reducing storage and transportation space requirements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FT_1
    Figure FT_1
  • Figure FT_2
    Figure FT_2
  • Figure FT_3
    Figure FT_3
Patent Text Reader

Abstract

Traditional wooden pallets contribute to deforestation, are less sustainable, easily absorb bacteria, and pose risks of chemical contamination, splinters, and damage. Wooden pallets must comply with ISPM 15 (International Standard for Phytosanitary Measures 15) for food packaging materials. Rotomolded plastic pallets are difficult to repair when damaged. Plastic pallets are more expensive than wooden pallets. Plastic pallets increase carbon footprint. Extruded plastic sand pallets are durable, repairable, and not subject to ISPM 15. This invention consists of two components glued together to form a pallet: a reinforcing member (2) and a rib (3). Extruded pallets require no mechanical fasteners.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The extruded plastic pallet (1) of the present invention consists of only two components, namely a reinforcing member (2) and a rib (3), which are connected by glue without mechanical fasteners, to manufacture a pallet for handling, storing and moving packaged materials. Technical Field

[0002] The process steps for manufacturing the extruded plastic tray (1) of the present invention are as follows.

[0003] According to the proportions in Table (1) of Figure 4, the mixture (4) is prepared with the following components: plastic (5), sand (6) and pigment (7).

[0004] The mixture is heated by means of an extruder (28) and the temperature is maintained at 270 degrees Celsius to 320 degrees Celsius. The molten mixture (4) is poured into the mold cavity (30) and the upper part of the mold press (31) is pressed down to reinforce the reinforcing member (2) or the rib (3).

[0005] Allow to cool for 60 to 120 seconds, then lift the top of the press (31). Remove the molded reinforcement (2).

[0006] Repeat the same process for the second mold to manufacture the rib (3).

[0007] If a sufficient number of reinforcing members (2) and ribs (3) are manufactured, then according to Figure 1 Assemble it by gluing the reinforcing member (2) and the rib (3) together to obtain the desired size and shape (rectangular or square). Background Technology

[0008] Standard pallets can be used to manipulate materials by inserting fork arms into the channels provided by the pallet.

[0009] Wooden pallets are simple, but they contribute to deforestation and need to meet ISPM 15 requirements.

[0010] Rotationally molded plastic pallets have a high carbon footprint and are irreparable.

[0011] There are a wide variety of molded pallets on the market, made from virgin or recycled plastic pellets and using fiber adhesives.

[0012] The manufacture of plastic pallets generates a higher carbon footprint, is more expensive, and is irreparable, leading to the need to invent a more durable, low-cost, low-carbon footprint circular economy model pallet that is easier to manufacture. Summary of the Invention

[0013] The present invention addresses the need for a low-cost, repairable, ISPM 15-compliant inspection-free pallet and a method for manufacturing the pallet (1).

[0014] The present invention consists of multiple sets of only two types of elements (reinforcing member (2) and rib (3)) to manufacture a tray.

[0015] This invention provides better industrial applicability than the prior art patent US 2008 / 0110377 A1 (stevens), which contains three elements (see patent figures), namely a lower part (914), an upper part (910), and a separate middle square block (912) for manufacturing a pallet.

[0016] The pallet reinforcements and ribs are manufactured by extrusion and load press, unlike the rotational molding process used in FR3149877A3 (Flexipal As) and US 2008 / 0110377 A1 (Stevens).

[0017] This invention offers better industrial applicability than the prior art patent US 2008 / 0110377 A1 (stevens), which manufactures a tray into two identical halves that are fixed together in a reverse-overlapping manner.

[0018] The moldable mixture is a blend of 26% to 40% by weight of plastic and 60% to 74% by weight of sand.

[0019] The moldable mixture may contain 0.5% by weight of pigment additives to obtain the preferred color.

[0020] The proportions of the plastic-sand mixture (4) are the same, while the percentages of sand (6) and plastic (5) can vary; the maximum plastic content can be 90% by weight, while the minimum plastic content can be 26% by weight; similarly, the maximum sand content can be 74% by weight, while the minimum content can be 10% by weight.

[0021] The mixture (4) above is extruded in an extruder and heated to 278°C to 320°C to produce a moldable mixture. Technical issues

[0022] The published patent US 2008 / 0110377 A1 (stevens) includes three elements (see patent diagrams): a lower part (914), an upper part (910), and a separate middle square block (912) for manufacturing a tray fastened together with a removable device.

[0023] Patent FR3149877A3 (Flexipal As) also has three elements: an upper part, a lower part, and a hollow square block connecting the upper and lower parts.

[0024] The present invention has only two elements, namely a reinforcing member (2) and a rib (3), to manufacture plastic-sand trays of various sizes and shapes that are fastened by glue.

[0025] Earlier pallet models required more storage space, and logistics and transportation also required more space because only assembled pallets could be transported; in this invention, components can be packaged in cartons and transported to the site, and assembled on-site by gluing. Problem Solution

[0026] A new design was developed to manufacture extruded trays using only two components (1).

[0027] The new manufacturing method uses extrusion and load-bearing presses instead of rotational molding.

[0028] The reinforcing member (2) and the rib (3) are glued together for assembly, which allows disassembled parts to be transported and reduces storage space.

[0029] This special design helps to manufacture pallets that are more robust than other types on the market. Beneficial effects of the invention

[0030] Extruded trays are durable, repairable, and not subject to ISPM 15.

[0031] Extruded pallets can be packaged individually in 1.3*0.5 meter cartons and can be assembled on-site; this helps reduce logistics and transportation space.

[0032] Increase the use of recycled plastics and recycled sand from construction demolition waste to reduce carbon footprint impact. Attached Figure Description

[0033] The invention will be readily understood from the following description and accompanying drawings. Figure 1

[0034] [ Figure 1 A view illustrating an extruded tray (1) assembled according to the present invention is shown. Figure 2

[0035] Figure 2 The reinforcing member (2) of the plastic-sand tray (1) is illustrated, and the workflow is illustrated in the flowchart. Figure 3

[0036] Figure 3 Examples of multiple ribs (3) used for the top and bottom of the reinforcement to manufacture the extruded tray (1) are shown. Figure 4

[0037] [Figure 4] Table-1 illustrates various compositions of plastic-sand mixture (4) used to manufacture extruded trays (1). Figure 5

[0038] [ Figure 5 An example is a pulverized high-density polyethylene (5) plastic waste used to manufacture a plastic-sand mixture (4) for extruding a tray (1). Figure 6

[0039] [ Figure 6 The sand (6) is illustrated in the composition of the plastic-sand mixture (4) used to manufacture the extruded pallet (1) or the sand recovered from construction demolition waste. Figure 7

[0040] Figure 7 An example of a basic extruder (28) for heating the blend (4) is shown. Figure 8

[0041] Figure 8 An example is shown: a base press (32) and a dye mold cavity (30) for manufacturing reinforcement (2) and rib (3). Detailed Implementation

[0042] The manufacturing details of the tray used in this invention have been given below. Figure 1 Assembly view of plastic-sand tray (1)

[0043] Figure 1 An assembly view of the assembled extruded tray of the present invention is shown. Only two types of components are used to manufacture this type of tray; one is a reinforcing member (2), and the other is a rib (3).

[0044] The tray has a plurality of ribs (3), preferably six at the top of the reinforcing member (2) and four at the bottom of the reinforcing member (2). The ribs are made of the plastic-sand mixture (4) described in this invention.

[0045] The extruded tray (1) has multiple reinforcing members (2), preferably four, in the middle of the tray, which helps to distribute the load evenly to all the ribs (3). The load-bearing reinforcing members (2) are made of the plastic-sand mixture (4) described in this invention.

[0046] The reinforcement (2) is designed to have a minimum leg height of 55 mm, which will be raised by the bottom rib (3) to have a maximum space of 74 mm to accommodate various types of lifting mechanisms, such as forklifts or pallet trolleys.

[0047] The rib (3) is glued to the reinforcing member (3) to assemble the tray (1). Figure 2 Reinforcing component (2)

[0048] Figure 2 Details of the reinforcing member (2) used in the manufacture of the plastic-sand tray (1) are illustrated. The reinforcing member (2) is made of the plastic-sand mixture (4) described in this invention. The reinforcing member (2) is a molded single piece and is pressed using a 200-ton press (32). The extruded plastic-sand mixture (4) is poured into the mold cavity and pressed using a 200-ton press (32) to reinforce the reinforcing member (2).

[0049] The reinforcing member has a channel designed in the center, which connects to the internal ridge to reinforce the formed reinforcing member (2).

[0050] The reinforcement (2) has a maximum height of 100 mm, a width of 30 mm, and a length of 1200 mm. The length and width may vary depending on the size requirements of the pallet (1), while the height will always be 100 mm. The reinforcement (2) has a notch with a height of 55 mm, which will be raised to 74 mm by assembling the bottom rib (3). This notch will be used to insert the forks of a two-way forklift or a pallet trolley. Figure 3 Rib-shaped component (3)

[0051] Figure 3 An example is shown of a rib (3) made from the plastic-sand mixture (4) described in this invention.

[0052] The ribs (3) are designed identically, with a width of 70 mm, a height or thickness of 19 mm, and a length of 1200 mm. All pallets will have the same width and thickness, regardless of whether the length varies according to the size requirements of the pallet (1).

[0053] The rib (3) is made of three raised surfaces and two channels. Each raised surface has a width of 14 mm and a thickness of 19 mm, and each channel is arranged on the raised surfaces from the top and bottom, with a width of 14 mm and a depth of 3 mm. This design will provide the rib (3) with additional strength to withstand more loads.

[0054] Figure 4, Table 1. Formulation of plastic-sand mixture (4) for extrusion molding tray (1).

[0055]

[0056] The proportions of the plastic-sand mixture (4) in the table above are the same, while the percentages of plastic (5) and sand (6) can vary; the maximum plastic (5) content can be 90% by weight, while the minimum plastic (5) content can be 26% by weight; similarly, the maximum sand (6) content can be 74% by weight, while the minimum sand (6) content can be 10% by weight.

[0057] The pigment (7) may be 0.25% by weight and may be any color, preferably green. Figure 5 Plastic (5)

[0058] Post-consumer HDPE plastic waste (5) must be crushed to a size of 5 mm to 8 mm to prepare a mixture (4).

[0059] PET, LDPE, and ABS plastic waste should also be crushed to a size of 5 mm before use. Figure 6 Sand(6)

[0060] Sand (6) or sand recovered from building demolition waste can be used to make the mixture (4), and sand (6) with a minimum size of 0.15 mm to a maximum size of 1.5 mm, preferably 0.6 mm, must be used. Figure 7 Extruder (28)

[0061] A simplified drawing of the extruder used for heating and blending the mixture (4) is provided.

[0062] The extruder is driven to rotate by a motor, and the powdered mixture is injected into it and heated by the extruder's heating coil. Figure 8 Press (32)

[0063] Traditional hydraulic presses are used to compress molten mixtures to reinforce stiffeners (2) and ribs (3). Industrial applicability

[0064] The extrusion-molded tray (1) of the present invention can be applied to mass production.

[0065] Due to its unique structure and ease of on-site assembly, the component reinforcements (2) and ribs (3) of the extruded pallet (1) can be packed in cardboard boxes and transported anywhere in the world.

[0066] Storage in warehouses or containers requires less space.

[0067] The inventors and the applicant have begun manufacturing extruded pallets at the applicant's factory. Reference List

[0068] The first pallet patent was invented in 1925 by a gentleman named Howard T. Hallowell, who named it the "lift truck platform".

[0069] Since then, it has undergone numerous improvements and innovations around the world, some of which are documents listed in the citation list. Declaration of Preservation of Biological Materials

[0070] This invention does not involve biological materials, therefore the biological materials declaration clause does not apply. Sequence List Exemption Declaration

[0071] Since no biological materials are used in this invention, the sequence listing clause does not apply to this patent application. Citation List

[0072] The list of citations is as follows: FR3149877A3 (Flexipal AS) US 2178646A – Pallet US 2008 / 0110377 A1 (Stevens) US2372055A 1945-03-20 pallet Patent documents

[0073] No patent documents related to pallet manufacturing were obtained. Non-patent literature

[0074] Non-patent literature can be cross-validated with existing patents in the citation lists for wooden pallets and plastic pallets.

Claims

1. An extruded tray (1) comprising multiple groups consisting of only two elements—a reinforcing rib (2) and a rib (3)—which are assembled by adhesive bonding to form various sizes and square or rectangular structures.

2. According to claim 1, the two elements—the reinforcing member (2) and the rib (3)—are made by an extruder (28) and a load press (32).

3. The extruded tray (1) according to claim 1, wherein the extruded tray is made of a combination of only two components: a reinforcing member (2) and a rib (3).

4. The extruded tray (1) according to any one of the preceding claims, wherein the extruded tray is joined by gluing.

5. The extruded pallet (1) according to any one of the preceding claims, wherein the extruded pallet is made of the reinforcing member (2) of various sizes (length and width) and the rib (3) of various sizes (length and width) to meet the needs of pallets (1) of various sizes worldwide.

6. The extruded tray (1) according to claim 1, wherein the extruded tray is made by a special design of the reinforcing member (2) as shown in FIG2 and the rib (3) as shown in FIG4 to enhance the structural strength of the reinforcing rib (2) and the rib (3).

Citation Information

Patent Citations

  • Load-Carrying Apparatus and Methods of Manufacture

    US20080110377A1

  • Pallet

    US2178646A