Substrate for sand filling method
By arranging concentric holes and triangular rings on the substrate for the sand filling method, combined with guide slopes and positioning holes, the problems of displacement and sand loss on the substrate are solved, ensuring constant size of the test pit and accuracy of test results, achieving a higher operational stability and test accuracy.
Patent Information
- Application Number
- CN202420315940.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-20
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2034-02-20
AI Technical Summary
The substrate used in the sand filling method is prone to displacement on the ground during operation, causing deviations in test pit specifications and affecting the accuracy of test results. In addition, sand easily flows into the gap between the substrate and the ground, causing deviations in test results.
Design a substrate for the sand filling method. Concentric holes and rings are provided at the bottom of the plate. The cross section of the ring is triangular. The guide slope is designed so that it can be quickly inserted into the ground to prevent sand from flowing into the gap. It is also ensured by positioning holes and enclosures. Substrate fixation and test result accuracy.
Ensure the constant size of the test pit, improve the accuracy of test results, prevent sand loss, enhance the fit between the substrate and the ground, reduce base collapse, and improve the reliability of test results.
Smart Images

Figure CN221803735U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of equipment for a sand filling method, and more specifically, to a substrate for a sand filling method. Background Art
[0002] The sand injection method is currently the main method for measuring compaction on many engineering sites. It looks simple on the surface, but it is often difficult to master in actual operation and is prone to cause large errors. It often causes disputes between quality inspection and supervision departments and construction units, so it requires sufficient operational skills. This method is suitable for on-site measurement of the density and compaction of various material compaction layers of base layers (or subbase layers), gravel pavements and roadbed base layers.
[0003] The utility model patent with authorization announcement number CN219641503U discloses a roadbed compaction detection device for road engineering inspection, including a sand filling cylinder and a cross pin, a cross pin is installed inside the sand filling cylinder, and a base plate is arranged below the sand filling cylinder, and a positioning mechanism is arranged on the side of the sand filling cylinder close to the base plate, and the positioning mechanism includes a docking groove, a docking block, a first magnetic ring and a second magnetic ring.
[0004] As shown in the above scheme and its attached drawings, this is the structure of a common sand cylinder and substrate used in the current sand filling method, wherein the bottom surface of the substrate is a plane. When placed on the ground for base layer and sand filling operations, the substrate is easily displaced on the ground, causing deviations between the test pit specifications and the standards, which will have a certain impact on the test results; and in the process of sand filling, part of the sand is easy to flow into the gap between the substrate and the ground, causing a large deviation in the test results. Utility Model Content
[0005] The utility model aims to overcome at least one defect of the above-mentioned prior art and provide a substrate for sand filling method, which is used to solve the technical problem that the substrate is easily displaced on the ground, causing deviations between the test pit specifications and the standards, which will have a certain impact on the test results.
[0006] The technical solution adopted by the utility model is a substrate for sand filling method, comprising a plate body, a circular hole is arranged on the plate body, a circular ring is arranged at the bottom of the plate body, the inner diameter of the circular ring is the same as the inner diameter of the circular hole, the circular ring and the circular hole are arranged concentrically, and the cross section of the circular ring is a triangle.
[0007] This solution sets a circular ring concentric with the circular hole at the bottom of the plate. During the test, the plate is placed on the ground at the test location, and the plate is pressed, and the circular ring is inserted downward into the ground, so that the plate will not move on the ground, ensuring that the size of the test pit is always constant, thereby ensuring the accuracy of the test results; when filling sand, the sand will not flow into the gap between the plate and the ground through the obstruction of the circular ring, which can further improve the accuracy of the test results.
[0008] Furthermore, the cross section of the ring is a right triangle, the inner wall of the circular hole and the inner wall of the ring are in the same vertical cylindrical surface, and the outer wall of the ring is a guide slope that gradually tilts from top to bottom toward the center of the ring. The ring can be quickly and easily inserted into the ground to be tested through the guide slope, and a test pit can be quickly dug on the ground with the inner wall of the ring as a reference, with the guide slope facing outward. During insertion, due to the action of the guide slope, the base layer outside the ring will move outward and be slightly compacted, which can prevent the base layer outside the ring from collapsing into the test pit, while the inner wall of the ring is a vertical cylindrical surface, which will not have an effect on the base layer in the test pit, thereby ensuring that the base layer dug out in the test pit is in a natural state, ensuring the accuracy of the test.
[0009] Furthermore, the ring is integrally formed with the plate body, which is more convenient for production and has better structural strength.
[0010] Furthermore, the plate body is square, and positioning holes are respectively provided at the four corners of the plate body for inserting positioning nails when fixing. When fixing, the plate body is fixed to the ground by the positioning nails, which can further improve the firmness of the plate body, make the plate body fit more closely with the ground, and further promote the accuracy of the test results.
[0011] Furthermore, a fence is provided on the top surface of the plate body, and the fence is formed integrally with the plate body. The fence mainly serves as a stopper to block the base layer to be tested dug out from the test pit, making it easier to collect the dug base layer.
[0012] Furthermore, the height of the ring is not less than 20 mm. The depth of 20 mm ensures the firmness during insertion. If it is less than 20 mm, the firmness cannot be guaranteed when used in some roadbeds with loose base materials.
[0013] Furthermore, the thickest part of the ring is not greater than 5 mm. When the thickness of the ring is greater than 5 mm, it is too thick and difficult to insert into the ground. Moreover, because the thickness is too large, the outer base of the ring is over-pressed and easily collapses when digging a test pit.
[0014] Furthermore, when the side length of the plate is 300-400 mm, the diameter of the positioning hole is 10-20 mm. After testing, when the side length of the plate is 300 mm, a 10 mm positioning hole, that is, a 10 mm positioning nail is sufficient to fix it firmly, and when the side length of the plate is 400 mm, a 20 mm positioning hole, that is, a 20 mm positioning nail is sufficient to fix it firmly.
[0015] Compared with the prior art, the beneficial effects of the utility model are as follows: a circular ring concentric with the circular hole is arranged at the bottom of the plate body in this scheme; during testing, the plate body is placed on the ground where the test location is located, and the plate body is pressed, and the circular ring is inserted downward into the ground, so that the plate body will not be displaced on the ground, ensuring that the size of the test pit is always constant, thereby ensuring the accuracy of the test results; when filling with sand, the sand will not flow into the gap between the plate body and the ground through the obstruction of the circular ring, which can further improve the accuracy of the test results. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a schematic diagram of the overall structure of the utility model.
[0017] Figure 2 It is a half-section view of the utility model.
[0018] In the figure: 1. plate body, 2. round hole, 3. round ring, 4. guide slope, 5. positioning hole, 6. enclosure. DETAILED DESCRIPTION
[0019] The drawings of the present invention are only used for illustrative purposes and cannot be construed as limiting the present invention. In order to better illustrate the following embodiments, some parts of the drawings may be omitted, enlarged or reduced, and do not represent the size of the actual product; for those skilled in the art, it is understandable that some well-known structures and their descriptions in the drawings may be omitted.
[0020] The basic process of the sand filling method is as follows: 1. At the test site, first place the substrate on the ground to be tested, then use a shovel to dig a test pit based on the circular hole 2 on the substrate, and then scoop out the base layer generated by the digging of the test pit (different roadbeds use different base layers, such as soil, sand, concrete, etc.) and bag them for weighing.
[0021] 2. Weigh the total weight of the sand cylinder filled with sand and the sand inside as M1, then place the sand cylinder on the circular hole 2 of the base plate, turn on the switch on the sand cylinder, and fill the test pit with sand. When the sand in the sand cylinder no longer flows down, it means that the test pit is full. Turn off the switch on the sand cylinder, remove the sand cylinder and weigh the total weight of the sand cylinder and the remaining sand inside as M2. Use M1-M2 to know the weight of all the sand filled in the test pit.
[0022] 3. The density and compaction degree of the base layer in the test pit can be calculated by digging out the weight of the base layer in the test pit and the weight of the sand filling in the test pit through other steps and methods (which belong to the prior art and will not be elaborated here).
[0023] The above method is the general process of the sand filling method. Among them, ensuring that the volume of the base layer excavated in the test pit is the same as the volume of the sand filled in is the key factor to ensure the accuracy of the test. Although the test requires that the substrate must be placed on a flat ground, in actual operation, the test ground cannot be absolutely flat and the substrate cannot fit perfectly with the ground. Therefore, in the process of sand filling, when the sand fills the test pit, some of the sand will flow into the gap between the substrate and the ground, which will affect the final test results.
[0024] like Figure 1 and 2 As shown, the present scheme discloses a substrate for sand filling method, including a plate body 1, a circular hole 2 is arranged on the plate body 1, a circular ring 3 is arranged at the bottom of the plate body 1, the inner diameter of the circular ring 3 is the same as the inner diameter of the circular hole 2, the circular ring 3 is arranged concentrically with the circular hole 2, and the cross section of the circular ring 3 is a triangle.
[0025] In this solution, a circular ring 3 concentric with the circular hole 2 is set at the bottom of the plate body 1. During the test, the plate body 1 is placed on the ground at the test location, and the plate body 1 is pressed, and the circular ring 3 is inserted downward into the ground. The plate body 1 will not move on the ground, ensuring that the size of the test pit is always constant, thereby ensuring the accuracy of the test results; when filling with sand, the sand will not flow into the gap between the plate body 1 and the ground through the obstruction of the circular ring 3, which can further improve the accuracy of the test results.
[0026] The cross section of the ring 3 is a right triangle, the inner wall of the circular hole 2 and the inner wall of the ring 3 are in the same vertical cylindrical surface, and the outer wall of the ring 3 is a guide slope 4 that gradually tilts from top to bottom toward the center of the ring 3. The ring 3 can be quickly and easily inserted into the ground to be tested through the guide slope 4, and a test pit can be quickly dug on the ground with the inner wall of the ring 3 as a reference. The guide slope 4 faces outward. During insertion, due to the action of the guide slope 4, the base layer outside the ring 3 will be slightly compacted by the external extrusion movement, which can prevent the base layer outside the ring 3 from collapsing into the test pit. The inner wall of the ring 3 is a vertical cylindrical surface, which will not affect the base layer that needs to be weighed in the test pit, and will not affect the base layer dug out of the test pit, ensuring the accuracy of the test.
[0027] The ring 3 is integrally formed with the plate body 1. The ring 3 is integrally formed with the plate body 1, which is more convenient for production and manufacturing and has better structural strength.
[0028] The height of the ring 3 is not less than 20 mm. The depth of 20 mm ensures firmness during insertion. If it is less than 20 mm, firmness cannot be guaranteed when used on some soft ground surfaces. The thickest part of the ring 3 is not greater than 5 mm. When the thickness of the ring 3 is greater than 5 mm, it is too thick and difficult to insert into the ground. In addition, the outer base of the ring 3 is over-pressed due to the excessive thickness, and it is easy to collapse downward when digging a test pit.
[0029] The plate body 1 is square. Positioning holes 5 are respectively provided at the four corners of the plate body 1, which are used to insert positioning nails when fixing. When fixing, the plate body 1 is fixed to the ground by the positioning nails, which can further improve the firmness of the plate body 1, make the base plate fit more closely with the ground, and further promote the accuracy of the test results; the top surface of the plate body 1 is provided with a fence 6, and the fence 6 is integrally formed with the plate body 1; the fence 6 mainly plays a stopper role, which is used to block the base layer to be tested dug out from the test pit, making it easier to collect the dug base layer.
[0030] When the side length of the plate body 1 is 300-400mm, the diameter of the positioning hole 5 is 10-20mm. After testing, when the side length of the plate body 1 is 300mm, a 10mm positioning hole 5 is selected, that is, a 10mm positioning nail is sufficient to fix it firmly, and when the side length of the plate body 1 is 400mm, a 20mm positioning hole 5 is selected, that is, a 20mm positioning nail is sufficient to fix it firmly; in practice, the side length of the plate body 1 is 350mm, and the diameter of the positioning hole 5 is 15mm.
[0031] As an example of this solution, in actual use, the size of the substrate can be set as follows: the overall side length is 350mm, the aperture of the positioning hole 5 is 15mm, the aperture of the circular hole 2 is 150mm, the thickness of the ring 3 is 5mm, the height of the ring 3 is 20mm, and a positioning pin of 50mm long and 15mm thick can be used for fixing.
[0032] Obviously, the above embodiments of the utility model are only examples for clearly explaining the technical solution of the utility model, and are not intended to limit the specific implementation methods of the utility model. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the claims of the utility model shall be included in the protection scope of the claims of the utility model.
Claims
1. A substrate for sand filling method, characterized in that: The invention comprises a plate body (1), wherein a circular hole (2) is arranged on the plate body (1), and a circular ring (3) is arranged at the bottom of the plate body (1). The inner diameter of the circular ring (3) is the same as the inner diameter of the circular hole (2), the circular ring (3) and the circular hole (2) are arranged concentrically, and the cross section of the circular ring (3) is triangular.
2. A substrate for sand filling method according to claim 1, characterized in that: The cross section of the circular ring (3) is a right triangle, the inner wall surface of the circular hole (2) and the inner wall surface of the circular ring (3) are in the same vertical cylindrical surface, and the outer wall of the circular ring (3) is a guiding inclined surface (4) which gradually inclines from top to bottom toward the center of the circular ring (3).
3. The substrate for sand filling method according to claim 1, characterized in that: The circular ring (3) and the plate body (1) are integrally formed.
4. The substrate for sand filling method according to claim 1, characterized in that: The height of the ring (3) is not less than 20 mm.
5. The substrate for sand filling method according to claim 1, characterized in that: The thickest part of the ring (3) is no larger than 5 mm.
6. A substrate for sand filling method according to any one of claims 1 to 5, characterized in that: The plate body (1) is square.
7. The substrate for sand filling method according to claim 6, characterized in that: The four corners of the plate body (1) are respectively provided with positioning holes (5) for inserting positioning pins.
8. The substrate for sand filling method according to claim 7, characterized in that: When the side length of the plate body (1) is 300 to 400 mm, the diameter of the positioning hole (5) is 10 to 20 mm.
9. The substrate for sand filling method according to claim 6, characterized in that: The top surface of the plate body (1) is provided with a baffle (6), and the baffle (6) and the plate body (1) are integrally formed.