Frame for flip chip packaging structure and chip packaging structure thereof

By designing grooves on the frame to correspond one-to-one with chip bumps, reflow soldering technology is used to solve the problems of offset and virtual soldering in flip-chip packaging, improving the reliability and product quality of the package.

CN221805522UActive Publication Date: 2024-10-01JIANGSU SILICON INTEGRITY SEMICON TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323499007.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-21
Publication Date
2024-10-01
Estimated Expiration
2033-12-21

AI Technical Summary

Technical Problem

During the flip-chip packaging process, the chip may be deflected during the transfer process, resulting in inaccurate bonding positions of bumps and pins, affecting packaging reliability. Existing solutions such as frame electroplating increase bonding strength, but are difficult to produce and prone to defects. Welding.

Method used

The grooves on the main body of the design frame are used to bond with the chip bumps. The outer dimensions of the grooves are larger than the bumps and are formed by etching, laser or mechanical drilling. The tips of the bumps are dipped in flux and reflowed at high temperatures to ensure a solid bond. Prevent offset and false soldering.

Benefits of technology

Effectively prevent chip offset and false soldering, improve the reliability and yield rate of flip-chip packaging products, and reduce production risks and abnormal situations.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221805522U_ABST
    Figure CN221805522U_ABST
Patent Text Reader

Abstract

The utility model discloses a frame for a flip chip packaging structure and a chip packaging structure thereof, the frame is provided with a frame main body and a pin, the front surface of the frame main body is used for flip chip, the flip chip is provided with a bump used for bonding with the frame, the tip of the bump forms a tin cap, and the tin cap is provided with a plurality of pins. A groove is formed in the position, needing to be bonded with the protruding block of the chip, of the front face of the frame, when the chip is inversely installed, the front end of the protruding block is inversely buckled into the groove, the boundary dimension of the groove is not smaller than that of the protruding block, the depth of the groove ranges from 50% of the height of the tin cap to 50% of the height of the protruding block, and the tip end of the protruding block is dipped in scaling powder and inversely buckled into the groove. During reflow soldering, the tin cap is melted to be combined with the groove, and the frame is combined with the chip through the plastic package material. According to the utility model, the process difficulty is reduced, the production risk of the frame is reduced, the problems of chip bump offset and pseudo soldering are improved, and the reliability of flip chip packaging products is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of semiconductor packaging, and more specifically to a frame for a flip chip packaging structure and a chip packaging structure thereof. Background Art

[0002] With the continuous development of packaging technology integration, flip-chip packaging products have greatly improved the integration of electronic devices. In recent years, flip-chip packaging has become an interconnection method for high-performance packaging, and its application has been widely and rapidly developed.

[0003] Flip chip packaging, such as Figure 1 As shown in the figure, the components and their reference numerals are: chip 100, copper pillar planting ball 101, frame pin 102, plastic encapsulation material 103, there is a copper pillar planting ball on the front of the chip (which can be called a bump, and the bump at the tip of the bump can be called a tin cap), after the chip is flipped, the bump on the surface of the chip is dipped in flux and then mounted on the frame, and the bump is directly bonded to the pin on the surface of the frame. In conventional flip chip packaging, the conveyor belt is driven to the reflow furnace for curing. During the transmission process, the chip may be offset, thereby affecting the combination position of the chip bump and the pin, affecting the reliability of the chip.

[0004] The reliability of the chip packaging structure is very important. The existing way to improve product reliability is to roughen the frame and electroplate the copper pillars at the positions corresponding to the combination with the frame to increase the bonding strength between the copper pillars and the frame. Figure 2 As shown in the figure, the components and their reference numerals are: chip 100, copper pillar planting ball 101, frame pin 102, plastic encapsulation material 103, electroplating 104 at the copper pillar planting ball and the frame pin. However, the production of the electroplated frame is difficult, the electroplating area is small, the electroplating tolerance is difficult to control during production, and cold solder joints are prone to occur.

[0005] Therefore, it is necessary to provide a frame design solution that can meet high reliability requirements and can be manufactured at the current production level to solve the above problems. Utility Model Content

[0006] In order to solve the above problems, the utility model provides a frame for a flip chip packaging structure and a chip packaging structure thereof, which can reduce the production risk of the frame while improving the problems of chip bump offset and cold solder joints, thereby improving the reliability of flip chip packaging products.

[0007] According to one aspect of the utility model, a frame for a flip chip packaging structure is provided, the frame having a frame body and pins, the front side of the frame body is used for flipping the chip, the flipped chip has a bump for bonding to the frame, the tip of the bump forms a tin cap, the front side of the frame is provided with a groove at a position where the bump of the chip needs to be bonded, when the chip is flipped, the front end of the bump is buckled into the groove, the outer dimensions of the groove are not less than the outer dimensions of the bump, and the depth of the groove is 50% of the height of the tin cap to 50% of the height of the bump.

[0008] In some embodiments, the groove includes a bottom wall, and the bottom wall is arc-shaped.

[0009] In some embodiments, the groove includes a bottom wall and a side wall connected to the bottom wall, the bottom wall is a flat bottom, the bottom wall and the side wall are vertically arranged, and the bottom wall and the side wall are transitioned by an arc.

[0010] In some embodiments, the groove includes a bottom wall and a side wall connected to the bottom wall, the bottom wall is a flat bottom, the angle formed between the bottom wall and the side wall is an obtuse angle, and the bottom wall and the side wall are transitioned through an arc.

[0011] According to another aspect of the utility model, a chip packaging structure is provided, including a chip and a frame for the above-mentioned flip chip packaging structure, the chip has a bump for bonding to the frame, the tip of the bump forms a tin cap, the surface of the tin cap is dipped in flux, the chip is flipped on the front side of the frame, the front end of the bump is buckled into the groove, the tin cap melts and combines with the groove during reflow soldering, and when the chip is packaged, the frame and the chip are combined through the plastic packaging material.

[0012] In some embodiments, the bump is a copper pillar, and the material of the tin cap is tin or tin-silver.

[0013] Compared with the prior art, the beneficial effects of the utility model are as follows: the utility model provides a frame for a flip chip packaging structure and a chip packaging structure having the frame, on the frame, grooves are made at positions where the bumps of the chip need to be bonded, when the chip is flip-bonded, the bumps are directly embedded in the grooves on the frame, the bumps of the chip correspond one-to-one with the grooves of the frame, to prevent the chip from shifting, before embedding the bumps, flux is dipped on the tin caps at the tips of the chip bumps, and reflow soldering is performed at high temperature, so that the tin caps at the tips of the bumps on the chip melt, and after cooling, they are more firmly bonded to the recessed holes, thereby stabilizing the combination of the chip bumps and the frame, and grooves are formed on the frame by etching, laser or mechanical drilling, and the bump tips are melted by reflow soldering, thereby reducing the production operation risks in terms of process, reducing the abnormal operation of the production line, preventing the problems of flip chip bump shifting and cold soldering, improving the reliability of flip chip packaging products, and being able to effectively improve the product yield. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1It is a schematic diagram of the structure of a conventional flip chip packaging product design;

[0015] Figure 2 This is a schematic diagram of the structure of the electroplating of the pins and chip positions of conventional flip chip packaging products;

[0016] Figure 3 It is a structural schematic diagram of an embodiment of a frame for a flip chip packaging structure of the utility model;

[0017] Figure 4 It is a structural schematic diagram of an implementation method of a chip packaging structure of the utility model;

[0018] Figure 5 It is a structural schematic diagram of a groove implementation method;

[0019] Figure 6 It is a structural schematic diagram of another embodiment of the concave groove;

[0020] Figure 7 It is a schematic structural diagram of another embodiment of the groove. DETAILED DESCRIPTION

[0021] The utility model is further described below in conjunction with specific implementation methods.

[0022] Example 1

[0023] like Figure 3 and 4 As shown, a frame for a flip chip packaging structure according to one embodiment of the utility model has a frame body 11 and pins 12. The front of the frame body 11 is used for a flip chip 2. The flip chip 2 has a bump 3 for bonding with the frame. The top of the bump 3 is planted with a ball so that the tip forms a tin cap 31. The material of the tin cap 31 can be tin or tin-silver. On the front of the frame, a groove 13 is processed by etching, laser or mechanical drilling at the position to be bonded with the bump 3 of the chip 2. The outer dimensions of the groove 13 are not less than the outer dimensions of the bump 3, and the depth of the groove 13 is at least half of the height of the tin cap 31 and the deepest does not exceed half of the total height of the bump 3. When the chip 2 is flipped, the tip of the bump 3 (that is, the tin cap 31) is dipped in flux (not shown) in advance, and then the front end of the bump 3 is turned upside down into the groove 13. The bump 3 corresponds to the groove 13 one by one to prevent the chip 2 from shifting. When the product passes through high-temperature reflow soldering, the tip of the bump 3 on the chip 2 (that is, the tin cap 31) will melt, and after cooling, it will be more firmly combined with the groove 13, thereby stabilizing the combination of the chip bump 3 and the frame.

[0024] In some applications, the bump 3 is a copper column, and a tin cap 31 is implanted on the copper column. The end of the tin cap 31 is arc-shaped, so the groove 13 is designed as an arc-shaped bottom wall 131. Figure 5 shown.

[0025] The groove 13 can also be designed as a structure of a bottom wall 131 and a side wall 132 connected to the bottom wall 131, the bottom wall 131 is a flat bottom, and the bottom wall 131 and the side wall 132 are arranged vertically (such as Figure 6 As shown in FIG. 1 , the bottom wall 131 and the side wall 132 are connected by an arc transition 133. Alternatively, the angle A formed between the bottom wall 131 and the side wall 132 is an obtuse angle (as shown in FIG. Figure 7 As shown), the bottom wall 131 and the side wall 132 are connected by an arc-shaped transition 133.

[0026] Example 2

[0027] like Figure 3 and 4 As shown, a chip packaging structure according to another embodiment of the present invention includes a chip 2 and the frame described in the above embodiment 1.

[0028] The chip 2 has a bump 3 for bonding with the frame, and the tip of the bump 3 forms a tin cap 31. The bump 3 is a copper column, and the material of the tin cap 31 is tin or tin-silver.

[0029] Dip the soldering flux on the surface of the tin cap 31, flip the chip 2 on the front side of the frame, and buckle the front end of the bump 3 into the groove 13. During reflow soldering, the tin cap 31 melts and combines with the groove 13, which can stabilize the combination of the chip copper column and the frame. When the chip 2 is packaged, the frame and the chip 2 are combined with the plastic packaging material 4.

[0030] The utility model provides a frame for a flip chip packaging structure and a chip packaging structure with the frame. A groove 13 is made on the frame at a position where the bump 3 of the chip 2 needs to be bonded. When the chip 2 is flip-bonded, the bump 3 is directly embedded in the groove 13 on the frame. The bump 3 of the chip 2 corresponds to the groove 13 of the frame one by one to prevent the chip 2 from shifting. Before the bump 3 is embedded, soldering flux is dipped on a tin cap 31 at the tip of the bump 3 of the chip 2, and reflow soldering is performed at high temperature. The tin cap 31 at the tip of the bump 3 on the chip 2 melts and is more firmly bonded to the groove 13 after cooling, thereby stabilizing the bond between the bump 3 of the chip 2 and the frame.

[0031] A groove 13 is formed on the frame by etching, laser or mechanical drilling, and the tip of the bump 3 is melted by reflow soldering. This process can be completed based on current technology, which reduces production operation risks, reduces production line operation abnormalities, prevents flip chip bump offset and cold soldering, improves the reliability of flip chip packaging products, and can effectively improve the product yield to meet production needs.

[0032] The above are only some embodiments of the present invention. It should be pointed out that for ordinary technicians in this field, other modifications and improvements can be made without departing from the creative concept of the present invention, which all belong to the protection scope of the present invention.

Claims

1. A frame for a flip chip packaging structure, the frame comprising a frame body (11) and pins (12), the front side of the frame body (11) being used for flipping a chip (2), the flipped chip (2) having a bump (3) for bonding with the frame, the tip of the bump (3) forming a tin cap (31), It is characterized in that A groove (13) is provided on the front side of the frame at a position where the protrusion (3) of the chip (2) needs to be bonded. When the chip (2) is flipped, the front end of the protrusion (3) is buckled into the groove (13). The outer dimensions of the groove (13) are not less than the outer dimensions of the protrusion (3). The depth of the groove (13) is 50% of the height of the tin cap to 50% of the height of the protrusion.

2. The flip chip packaging structure frame according to claim 1, It is characterized in that The groove (13) comprises a bottom wall (131), and the bottom wall (131) is arc-shaped.

3. The flip chip packaging structure frame according to claim 1, It is characterized in that The groove (13) comprises a bottom wall (131) and a side wall (132) connected to the bottom wall (131); the bottom wall (131) is a flat bottom; the bottom wall (131) and the side wall (132) are vertically arranged; and an arc-shaped transition (133) is formed between the bottom wall (131) and the side wall (132).

4. According to the frame for flip chip packaging structure according to claim 1, the groove (13) comprises a bottom wall (131) and a side wall (132) connected to the bottom wall (131), the bottom wall (131) is a flat bottom, the angle formed between the bottom wall (131) and the side wall (132) is an obtuse angle, and the bottom wall (131) and the side wall (132) are connected by an arc transition (133).

5. A chip packaging structure, It is characterized in that The invention comprises a chip (2) and a frame for a flip chip packaging structure as claimed in any one of claims 2 to 4, wherein the chip (2) has a bump (3) for bonding with the frame, the tip of the bump (3) forms a tin cap (31), the surface of the tin cap (31) is dipped with solder flux, the chip (2) is flipped on the front side of the frame, the front end of the bump (3) is buckled into a groove (13), the tin cap (31) melts and combines with the groove (13) during reflow soldering, and when the chip is packaged, the frame and the chip (2) are combined through a plastic packaging material (4).

6. The chip packaging structure according to claim 5, It is characterized in that The bump (3) is a copper column, and the tin cap (31) is tin or tin-silver.