Side die structure of precast slab
By designing a prefabricated plate side form structure including a top mold, a bottom mold, a sealing strip and a magnetic seat, the problem of low versatility of the existing side molds was solved, and the adaptability to different exposed steel bars and the improvement of production efficiency were achieved. Improvement ensures the sealing and adhesion of prefabricated panels.
Patent Information
- Application Number
- CN202420246722.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-01
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2034-02-01
AI Technical Summary
The existing prefabricated panel side formwork has low versatility, resulting in increased resource consumption, reduced production efficiency and increased production costs, and cannot adapt to the needs of different exposed steel bar spacing and diameters.
Design a side mold structure including a top mold, a bottom mold, sealing strips, guide pins and magnetic seats. The exposed steel bars are extruded and sealed by the sealing strips. The guide pins and magnetic seats are fixed in the installation position to adapt to different conditions. Rebar parameters, and improve versatility and ease of disassembly through designs such as soft and hard rubber strips, dovetail-shaped protrusions and grooves, rough surfaces and sleeves.
It achieves high versatility of the side mold, reduces resource consumption, improves production efficiency, ensures the side sealing and adhesion of the prefabricated panels, and simplifies the disassembly and installation process of the side mold.
Smart Images

Figure CN221819003U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of prefabricated component production, and further to a side mold structure of a prefabricated panel. Background Art
[0002] At present, prefabricated panels (including prefabricated floor panels, prefabricated wall panels, prefabricated cantilever panels, reinforced prefabricated panels, prefabricated composite panels, etc.) are widely used in prefabricated building projects. In order to strengthen the connection between prefabricated panels and other building parts, reinforced prefabricated panels are generally used. Reinforced prefabricated panels refer to prefabricated panels with exposed steel bars around them. The prefabricated panels are connected to other building parts by pouring concrete at the exposed steel bars of the prefabricated panels. At present, the side molds used in the production of reinforced prefabricated panels are all customized. The steel bar perforations or notches on the side molds are adapted to the spacing and diameter of the exposed steel bars. When the parameters such as the spacing and diameter of the exposed steel bars are adjusted, the original side molds cannot be adapted and the side molds need to be remade. This results in low versatility of such side molds, increased resource consumption, reduced production efficiency, and increased production costs of prefabricated panels.
[0003] Therefore, the market is in urgent need of a highly versatile side mold solution. Utility Model Content
[0004] In order to solve the above problems, the present application provides a side mold structure of a prefabricated panel, which has an ingenious design and a simple structure. The side mold structure has strong versatility, improves the utilization rate of the side mold and the production efficiency of the prefabricated panel, and the top mold and the bottom film in the side mold structure are easy to separate. The technical solution adopted by the present application is as follows:
[0005] A side mold structure of a prefabricated board comprises: a top mold body, the top mold body is provided with a plurality of guide holes; a bottom mold body, the bottom mold body is provided with a plurality of mounting positions; a sealing strip, the sealing strip is respectively clamped on the top mold body and the bottom mold body;
[0006] A plurality of guide pins, one end of each guide pin being provided with a magnetic seat, the end of each guide pin provided with the magnetic seat being suitable for being inserted into the installation position, and the guide pin being suitable for being inserted into the guide hole;
[0007] After the top mold body and the bottom mold body are relatively fixed by the guide pins, the sealing strip clamped to the top mold body and the sealing strip clamped to the bottom mold body are suitable for clamping on both sides of the exposed steel bars of the precast panel to seal the sides of the precast panel.
[0008] In the present application, a sealing strip is used to squeeze the exposed steel bars to seal the side of the precast panel to prevent concrete (casting material) from leaking out from the exposed steel bars or to prevent slurry leakage. This design does not require perforations or notches on the side mold, nor does it require slurry blocking parts. It can adapt to precast panels with different exposed steel bar spacings and various exposed steel bar diameters, thereby improving the versatility of the side mold structure. In addition, a magnetic seat is provided on the guide pin, and the magnetic attraction between the magnetic seat and the bottom mold body or the precast panel mold base is utilized to fix the guide pin in the installation position to prevent the guide pin from falling off from the installation position when the precast panel mold base vibrates. The guide pin is not only firmly fixed and not easy to fall off, but also easy to pull out from the guide hole, which is beneficial to the rapid disassembly of the top mold body and the bottom mold body.
[0009] In some embodiments, the sealing strip includes a soft strip portion and a hard strip portion, the soft strip portion and the hard strip portion of the sealing strip are made by a two-color extrusion process, and the soft strip portion is suitable for gripping the exposed steel bars.
[0010] By setting a soft rubber strip part and a hard rubber strip part, the soft rubber strip part is softer than the hard rubber strip part and has better filling performance, which is conducive to tightly wrapping around the exposed steel bar periphery and improving the sealing of the side of the precast panel, while the hard rubber strip part is harder and stronger than the soft rubber strip part, which can provide strong support for the soft rubber strip part and ensure the ability of the sealing strip to recover from deformation. At the same time, the hard rubber strip part also plays a buffering role to prevent the direct action between the soft rubber strip part and the top mold body (or bottom mold body), thereby reducing the risk of damage to the soft rubber strip part.
[0011] In some embodiments, the top mold body and the bottom mold body are both provided with a card slot, and both side walls of the card slot are provided with a long first protrusion, and the sealing strip is provided with a first groove adapted to the first protrusion, so that the sealing strip can be clamped in the card slot through the cooperation of the first protrusion and the first groove.
[0012] By setting the first protrusion and the first groove, not only is it easy to install the sealing strip on the top mold body (or bottom mold body), but the sealing strip is also stably connected to the top mold body (or bottom mold body) and is not easy to separate from the top mold body (or bottom mold body).
[0013] In some embodiments, the cross-section of the first protrusion is dovetail-shaped, and the first groove is a dovetail groove.
[0014] By designing the cross-section of the first protrusion to be in a dovetail shape and the first groove to be in a dovetail groove, the connection strength between the sealing strip and the top mold body (or the bottom mold body) can be improved, reducing the risk of the sealing strip returning to the slot when squeezed by exposed steel bars, thereby improving the gripping effect of the sealing strip on the exposed steel bars.
[0015] In some embodiments, at least one of a side of the top mold body close to the prefabricated panel and a side of the bottom mold body close to the prefabricated panel is provided with a rough surface.
[0016] By providing a rough surface, an uneven structure (rough surface) can be formed on the side of the precast panel after the side form is removed, thereby improving the bonding strength between the precast panel and concrete (casting material).
[0017] In some embodiments, at least one of a side of the top mold body close to the precast panel and a side of the bottom mold body close to the precast panel is provided with a plurality of second protrusions or second grooves to form the rough surface.
[0018] In some embodiments, a sleeve is further included, which is installed in the installation position, and one end of the guide pin provided with the magnetic seat is suitable for being inserted into the sleeve, and one end of the sleeve away from the bottom mold body is suitable for abutting against the top mold body.
[0019] By setting the sleeve, the abutment between the sleeve and the top mold body can be utilized to control the distance between the top mold body and the bottom mold body, thereby controlling the overall thickness of the side mold structure, so that the overall thickness of the side mold structure is not less than the thickness of the prefabricated board.
[0020] In some embodiments, the side wall of the sleeve is provided with an opening.
[0021] By setting an opening on the side wall of the sleeve, the inner wall of the sleeve can be easily cleaned, reducing the risk of debris in the sleeve affecting the magnetic attraction of the magnetic seat. At the same time, the depth of the guide pin inserted into the sleeve can be observed through the opening to determine whether the guide pin is inserted into place.
[0022] In some embodiments, a sealing rubber ring is provided at the guide hole, and the guide pin is suitable for sealingly cooperating with the sealing rubber ring.
[0023] By providing a sealing rubber ring, the risk of slurry contaminating the surface of the guide pin, entering the installation position or entering the sleeve during the pouring of concrete (pouring material) can be reduced, thereby avoiding affecting the smooth extraction and insertion of the guide pin.
[0024] In some embodiments, a magnetic block and / or a pinching portion is provided at one end of the guide pin away from the magnetic seat.
[0025] When a magnetic block is provided, the guide pin can be pulled out by utilizing the mutual magnetic attraction between the magnetic device and the magnetic block, and the pulling-out method of the guide pin is convenient and quick; when a pinching portion is provided, the pinching portion provides a force-carrying part for the fingers, which facilitates the pulling-out of the guide pin.
[0026] The side mold structure of a prefabricated panel provided in the present application has at least one of the following beneficial effects:
[0027] 1. The application provides a side mold structure of a prefabricated panel, which uses a sealing strip to squeeze the exposed steel bars to seal the side of the prefabricated panel, thereby preventing concrete (casting material) from leaking out from the exposed steel bars or preventing slurry leakage. This design does not require perforations or notches on the side mold, nor does it require slurry blocking parts, and can adapt to prefabricated panels with different exposed steel bar spacings and various exposed steel bar diameters, thereby improving the versatility of the side mold structure. In addition, a magnetic suction seat is provided on the guide pin, and the magnetic suction of the magnetic suction seat and the bottom mold body or the prefabricated panel mold base is used to fix the guide pin in the installation position, thereby preventing the guide pin from falling off from the installation position when the prefabricated panel mold base vibrates. The guide pin is not only firmly fixed and not easy to fall off, but also easy to be pulled out from the guide hole, which is conducive to the rapid disassembly of the top mold body and the bottom mold body.
[0028] 2. The application provides a side mold structure of a prefabricated panel, which is provided with a soft rubber strip part and a hard rubber strip part. The soft rubber strip part is softer than the hard rubber strip part and has better filling performance, which is conducive to tightly wrapping around the outer periphery of the exposed steel bar, thereby improving the sealing performance of the side of the prefabricated panel. The hard rubber strip part is harder and stronger than the soft rubber strip part, which can provide strong support for the soft rubber strip part, thereby ensuring the ability of the sealing strip to recover deformation. At the same time, the hard rubber strip part also plays a buffering role, thereby preventing the direct action between the soft rubber strip part and the top mold body (or the bottom mold body), thereby reducing the risk of damage to the soft rubber strip part.
[0029] 3. The side mold structure of a prefabricated panel provided by the present application, by providing the first protrusion and the first groove, not only facilitates the installation of the sealing strip to the top mold body (or the bottom mold body), but also the sealing strip is stably connected to the top mold body (or the bottom mold body) and is not easy to be separated from the top mold body (or the bottom mold body);
[0030] 4. The side mold structure of a prefabricated panel provided by the present application can improve the connection firmness between the sealing strip and the top mold body (or bottom mold body) by designing the cross section of the first protrusion to be dovetail-shaped and the first groove to be dovetail groove, thereby reducing the risk of the sealing strip returning to the slot when being squeezed by the exposed steel bars, and improving the gripping effect of the sealing strip on the exposed steel bars;
[0031] 5. The side mold structure of a prefabricated panel provided in the present application can form an uneven structure (rough surface) on the side of the prefabricated panel after the side mold is disassembled by setting a rough surface, thereby improving the bonding strength between the prefabricated panel and concrete (casting material);
[0032] 6. The side mold structure of a prefabricated panel provided by the present application can control the distance between the top mold body and the bottom mold body by setting a sleeve, thereby controlling the overall thickness of the side mold structure, so that the overall thickness of the side mold structure is not less than the thickness of the prefabricated panel;
[0033] 7. The side mold structure of a prefabricated panel provided by the present application can facilitate cleaning of the inner wall of the sleeve by setting an opening on the side wall of the sleeve, thereby reducing the risk of debris in the sleeve affecting the magnetic attraction of the magnetic suction seat. At the same time, the depth of the guide pin inserted into the sleeve can be observed through the opening to facilitate judgment of whether the guide pin is inserted in place;
[0034] 8. The application provides a side mold structure of a prefabricated panel, which can reduce the risk of slurry contaminating the surface of the guide pin, entering the installation position or entering the sleeve during the pouring of concrete (casting material) by setting a sealing rubber ring, thereby avoiding affecting the smooth extraction and insertion of the guide pin;
[0035] 9. The present application provides a side mold structure for a prefabricated panel. When a magnetic block is provided, the guide pin can be pulled out by utilizing the mutual magnetic attraction between the magnetic device and the magnetic block, and the method for pulling out the guide pin is convenient and quick. When a pinching portion is provided, the pinching portion provides a force point for the fingers, which facilitates the pulling out of the guide pin. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] The following will explain the preferred implementation mode in a clear and understandable manner with reference to the accompanying drawings, and further explain the above characteristics, technical features, advantages and implementation methods of a side form structure of a prefabricated panel:
[0037] Figure 1 It is a schematic diagram of the overall structure after the embodiment of the present application is assembled;
[0038] Figure 2 It is an exploded diagram of the overall structure of the embodiment of the present application;
[0039] Figure 3 This is a schematic diagram of the structure of the top mold body and the sealing strip after being assembled in the embodiment of the present application;
[0040] Figure 4 This is a schematic diagram of the structure of the bottom mold body and the sealing strip after being assembled in the embodiment of the present application;
[0041] Figure 5 is a schematic diagram of the guide pin and the sleeve after being assembled in the embodiment of the present application;
[0042] Figure 6 is a schematic diagram of the guide pin after being pulled out from the sleeve in the embodiment of the present application;
[0043] Figure 7 is a schematic diagram of a guide pin and a sleeve after being assembled in another embodiment of the present application;
[0044] Figure 8 is a schematic diagram of another embodiment of the present application after the guide pin is pulled out from the sleeve;
[0045] Fig. 9 It is a schematic diagram of the overall structure after assembling various embodiments of the present application.
[0046] Description of Figure Numbers:
[0047] Top mold body 1, guide hole 2, bottom mold body 3, mounting position 4, sealing rubber strip 5, soft rubber strip part 51, hard rubber strip part 52, guide pin 6, magnetic seat 7, slot 8, first protrusion 9, first groove 10, second protrusion 11, second groove 12, sleeve 13, opening 14, sealing rubber ring 15, pinching part 16, magnetic block 17. DETAILED DESCRIPTION
[0048] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the specific implementation methods of the present application will be described below with reference to the accompanying drawings. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings and other implementation methods can be obtained based on these drawings without creative work.
[0049] In order to simplify the drawings, only the parts related to the present application are schematically shown in each figure, and they do not represent the actual structure of the product. In addition, in order to simplify the drawings and facilitate understanding, in some figures, only one of the parts with the same structure or function is schematically drawn or marked. In this article, "one" not only means "only one", but also means "more than one".
[0050] It should be further understood that the term “and / or” used in the specification and appended claims refers to any combination and all possible combinations of one or more of the associated listed items, and includes these combinations.
[0051] In this document, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0052] In addition, in the description of the present application, the terms "first", "second", etc. are only used to distinguish the description and cannot be understood as indicating or implying relative importance.
[0053] refer to Figure 1-Figure 9The present application provides a side mold structure of a prefabricated board, comprising: a top mold body 1, the top mold body 1 is provided with a plurality of guide holes 2; a bottom mold body 3, the bottom mold body 3 is provided with a plurality of mounting positions 4; a sealing strip 5, the sealing strip 5 is respectively clamped on the top mold body 1 and the bottom mold body 3; a plurality of guide pins 6, one end of the guide pin 6 is provided with a magnetic seat 7, the end of the guide pin 6 provided with the magnetic seat 7 is suitable for being inserted into the mounting position 4, and the guide pin 6 is suitable for being inserted into the guide hole 2;
[0054] After the top mold body 1 and the bottom mold body 3 are relatively fixed by the guide pins 6, the sealing strip 5 clamped on the top mold body 1 and the sealing strip 5 clamped on the bottom mold body 3 are suitable for clamping on both sides of the exposed steel bars of the prefabricated panel to seal the sides of the prefabricated panel.
[0055] Specifically, the top mold body 1 and the bottom mold body 3 can be obtained by extrusion molding of aluminum, or by welding of patterned plates, or by extrusion molding of FRP glass fiber reinforced plastics, or by extrusion molding of materials such as polyurethane. The present application does not impose any restrictions on the specific manufacturing materials and processes of the top mold body 1 and the bottom mold body 3. Specifically, the bottom mold body 3 is fixed on the prefabricated plate mold platform by a magnetic box, and the top mold body 1 is also restricted by the magnetic box in the vertical movement relative to the bottom mold body 3. The relative movement of the top mold body 1 and the bottom mold body 3 in the horizontal direction is restricted by the guide pin 6.
[0056] In this embodiment, the exposed steel bars are squeezed by the sealing strip 5, that is, the exposed steel bars extend from between the sealing strip 5 of the top mold body 1 and the sealing strip 5 of the bottom mold body 3 to seal the side of the precast panel to prevent concrete (casting material) from leaking out from the exposed steel bars or to prevent slurry leakage. This design does not require perforations or notches on the side mold, nor does it require slurry blocking parts. It can adapt to precast panels with different exposed steel bar spacings and various exposed steel bar diameters, thereby improving the versatility of the side mold structure. In addition, by providing a magnetic seat 7 on the guide pin 6, the magnetic seat 7 and the bottom mold body 3 or the precast panel mold base and other parts are used to fix the guide pin 6 in the installation position 4 to prevent the guide pin 6 from falling off from the installation position 4 when the precast panel mold base vibrates. The guide pin 6 is not only firmly fixed and not easy to fall off, but also easy to be pulled out from the guide hole 2, which is conducive to the rapid disassembly of the top mold body 1 and the bottom mold body 3. In this embodiment, the mounting position 4 can be a through hole penetrating the bottom mold body 3, or a non-penetrating groove. When the mounting position 4 is a through hole, the magnetic seat 7 on the guide pin 6 can be directly magnetically attracted to the prefabricated board mold platform.
[0057] refer to Figure 1 , Figure 2 , Fig. 9In one embodiment, the sealing strip 5 includes a soft strip portion 51 and a hard strip portion 52. The soft strip portion 51 and the hard strip portion 52 of the sealing strip 5 are made by a two-color extrusion process, and the soft strip portion 51 is suitable for gripping exposed steel bars.
[0058] It is worth noting that by providing the soft rubber strip portion 51 and the hard rubber strip portion 52, the soft rubber strip portion 51 is softer than the hard rubber strip portion 52 and has better filling performance, which is conducive to tightly wrapping around the exposed steel bar periphery and improving the sealing of the side of the precast panel, while the hard rubber strip portion 52 is harder and stronger than the soft rubber strip portion 51, which can provide strong support for the soft rubber strip portion 51 and ensure the ability of the sealing strip 5 to recover from deformation. At the same time, the hard rubber strip portion 52 also plays a buffering role to prevent the direct interaction between the soft rubber strip portion 51 and the top mold body 1 (or the bottom mold body 3), thereby reducing the risk of damage to the soft rubber strip portion 51.
[0059] In this embodiment, the soft rubber strip portion 51 may be a foamed rubber strip, such as an EPDM foamed (sponge) rubber strip, and the hard rubber strip portion 52 may be a hard rubber strip, such as an EPDM rubber strip.
[0060] refer to Figure 1 , Figure 2 , Fig. 9 In one embodiment, the top mold body 1 and the bottom mold body 3 are both provided with a card slot 8, and the two side walls of the card slot 8 are both provided with a long first protrusion 9, and the sealing strip 5 is provided with a first groove 10 adapted to the first protrusion 9, so that the sealing strip 5 is clamped in the card slot 8 through the cooperation of the first protrusion 9 and the first groove 10.
[0061] In this embodiment, by providing the first protrusion 9 and the first groove 10, not only is it convenient to install the sealing strip 5 to the top mold body 1 (or the bottom mold body 3), but the sealing strip 5 is also stably connected to the top mold body 1 (or the bottom mold body 3) and is not easy to separate from the top mold body 1 (or the bottom mold body 3).
[0062] refer to Figure 1 , Figure 2 , Fig. 9 In one embodiment, the cross section of the first protrusion 9 is dovetail-shaped, and the first groove 10 is a dovetail groove.
[0063] It can be understood that by designing the cross-section of the first protrusion 9 to be dovetail-shaped and the first groove 10 to be a dovetail groove, the connection firmness between the sealing strip 5 and the top mold body 1 (or the bottom mold body 3) can be improved, and the risk of the sealing strip 5 returning to the slot 8 when squeezed by the exposed steel bars can be reduced, thereby improving the gripping effect of the sealing strip 5 on the exposed steel bars.
[0064] refer to Figure 1 , Figure 2 , Fig. 9In one embodiment, at least one of the side of the top mold body 1 close to the precast panel and the side of the bottom mold body 3 close to the precast panel is provided with a rough surface. It can be understood that by providing the rough surface, an uneven structure (rough surface) can be formed on the side of the precast panel after the side mold is removed, thereby improving the bonding force between the precast panel and the concrete (casting material).
[0065] refer to Figure 1 , Figure 2 , Fig. 9 In one embodiment, at least one of the side of the top mold body 1 close to the precast panel and the side of the bottom mold body 3 close to the precast panel is provided with a plurality of second protrusions 11 or second grooves 12 to form a rough surface.
[0066] refer to Figure 1 , Figure 2 , Figure 4-Figure 9 In one embodiment, it also includes a sleeve 13, which is installed in the installation position 4, and one end of the guide pin 6 with a magnetic seat 7 is suitable for being inserted into the sleeve 13, and the end of the sleeve 13 away from the bottom mold body 3 is suitable for abutting against the top mold body 1.
[0067] It is worth noting that by setting the sleeve 13, the abutment between the sleeve 13 and the top mold body 1 can be utilized to control the distance between the top mold body 1 and the bottom mold body 3, thereby controlling the overall thickness of the side mold structure, so that the overall thickness of the side mold structure is not less than the thickness of the precast panel.
[0068] refer to Figure 1 , Figure 2 , Figure 4-Figure 8 In one embodiment, the side wall of the sleeve 13 is provided with an opening 14. By providing the opening 14 on the side wall of the sleeve 13, it is convenient to clean the inner wall of the sleeve 13, reducing the risk of debris in the sleeve 13 affecting the magnetic attraction of the magnetic seat 7. At the same time, the depth of the guide pin 6 inserted into the sleeve 13 can be observed through the opening 14, so as to judge whether the guide pin 6 is inserted in place.
[0069] refer to Figure 1-Figure 3 In one embodiment, a sealing rubber ring 15 is provided at the guide hole 2, and the guide pin 6 is adapted to be sealed with the sealing rubber ring 15. It can be understood that the provision of the sealing rubber ring 15 can reduce the risk of slurry contaminating the surface of the guide pin 6, entering the installation position 4 or entering the sleeve 13 during the pouring of concrete (casting material), thereby avoiding affecting the smooth extraction and insertion of the guide pin 6.
[0070] refer to Figure 1 , Figure 2 , Figure 5-Figure 9 In one embodiment, a magnetic block 17 and / or a pinching portion 16 is provided at one end of the guide pin 6 away from the magnetic seat 7 .
[0071] It is understandable that when the magnetic block 17 is provided, the guide pin 6 can be pulled out by utilizing the mutual magnetic attraction between the magnetic device and the magnetic block 17, and the pulling out method of the guide pin 6 is convenient and quick; when the pinching portion 16 is provided, the pinching portion 16 provides a force point for the finger, which facilitates the pulling out of the guide pin 6. It is understandable that only one of the magnetic block 17 and the pinching portion 16 can be provided, or both can be provided at the same time.
[0072] It should be noted that the above embodiments can be freely combined as needed. The above are only preferred implementations of the present application. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principles of the present application, and these improvements and modifications should also be regarded as the protection scope of the present application.
Claims
1. A side mold structure of a prefabricated panel, characterized in that: include: A top mold body, wherein the top mold body is provided with a plurality of guide holes; A bottom mold body, wherein the bottom mold body is provided with a plurality of mounting positions; Sealing strips, the sealing strips are respectively clamped on the top mold body and the bottom mold body; A plurality of guide pins, one end of each guide pin being provided with a magnetic seat, the end of each guide pin provided with the magnetic seat being suitable for being inserted into the installation position, and the guide pin being suitable for being inserted into the guide hole; After the top mold body and the bottom mold body are relatively fixed by the guide pins, the sealing strip clamped to the top mold body and the sealing strip clamped to the bottom mold body are suitable for clamping on both sides of the exposed steel bars of the precast panel to seal the sides of the precast panel.
2. A side form structure of a prefabricated panel according to claim 1, characterized in that: The sealing strip comprises a soft strip portion and a hard strip portion, the soft strip portion and the hard strip portion of the sealing strip are made by a two-color extrusion process, and the soft strip portion is suitable for gripping the exposed steel bars.
3. The side form structure of a prefabricated panel according to claim 1, characterized in that: The top mold body and the bottom mold body are both provided with a card slot, and both side walls of the card slot are provided with a long first protrusion, and the sealing strip is provided with a first groove adapted to the first protrusion, so that the sealing strip can be clamped in the card slot through the cooperation of the first protrusion and the first groove.
4. A side form structure of a prefabricated panel according to claim 3, characterized in that: The cross section of the first protrusion is dovetail-shaped, and the first groove is a dovetail groove.
5. The side form structure of a prefabricated panel according to claim 1, characterized in that: At least one of a side of the top mold body close to the prefabricated board and a side of the bottom mold body close to the prefabricated board is provided with a rough surface.
6. A side form structure of a prefabricated panel according to claim 5, characterized in that: At least one of the side of the top mold body close to the prefabricated board and the side of the bottom mold body close to the prefabricated board is provided with a plurality of second protrusions or second grooves to form the rough surface.
7. A side form structure of a prefabricated panel according to any one of claims 1 to 6, characterized in that: It also includes a sleeve, which is installed in the installation position. The end of the guide pin provided with the magnetic seat is suitable for being inserted into the sleeve, and the end of the sleeve away from the bottom mold body is suitable for abutting against the top mold body.
8. The side form structure of a prefabricated panel according to claim 7, characterized in that: The side wall of the sleeve is provided with an opening.
9. A side form structure of a prefabricated panel according to any one of claims 1 to 6 and 8, characterized in that: A sealing rubber ring is provided at the guide hole, and the guide pin is suitable for sealingly cooperating with the sealing rubber ring.
10. A side form structure of a prefabricated panel according to claim 9, characterized in that: The end of the guide pin away from the magnetic seat is provided with a magnetic block and / or a pinching portion.