Device for accurately detecting Y value of bituminous coal gelatinous layer

Through the combination of the free fall motion of the probe assembly and the non-contact probe position measurement device, the problems of insufficient measurement speed and inaccurate measurement of thin colloid in the existing technology are solved, and the Y value of the bituminous coal colloid layer is determined. High-accuracy measurement, and the measurement process is optimized through neural network, which improves the reliability and accuracy of the measurement results.

CN221826089UActive Publication Date: 2024-10-11ANSHAN S Y D SCI & TECH
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202323567646.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-26
Publication Date
2024-10-11
Estimated Expiration
2033-12-26

AI Technical Summary

Technical Problem

The existing automatic detection device for bituminous coal colloid layer thickness cannot respond quickly when measuring zigzag or zhishan mixed coal samples, resulting in measurement errors; it is difficult to achieve accurate measurement of thin colloid coal types, and the influence of human factors still exists.

Method used

The free fall motion of the probe assembly is used in conjunction with a non-contact probe position measurement device to measure the probe position through laser or ultrasonic waves, reducing the peak point lag time, improving measurement accuracy, and optimizing the measurement process through neural network self-learning.

Benefits of technology

It achieves accurate measurement of thin colloidal coal types, reduces measurement errors, improves measurement speed and accuracy, and improves the reproducibility and accuracy of measurement results through AI intelligent measurement.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221826089U_ABST
    Figure CN221826089U_ABST
Patent Text Reader

Abstract

The utility model relates to a device for accurately detecting the Y value of a bituminous coal gelatinous layer. The device comprises a device bracket, a coal cup, a motor, a screw rod and nut transmission mechanism, a pressure sensor, a probe assembly, a control system, a non-contact probe position measuring device and a locking mechanism, the probe assembly is composed of a probe and a reflecting plate, and the measuring end of the non-contact probe position measuring device acts on the reflecting plate; the locking mechanism can lock the probe assembly to enable the probe assembly to be suspended in the air or release the probe assembly to enable the probe assembly to fall freely. The free falling motion of the probe assembly is matched with the non-contact probe position measuring device, so that the position of the upper layer of the colloid is measured, the delay time (within hundreds of milliseconds) of an X-value peak point is greatly shortened, and the measurement accuracy is improved; meanwhile, the determination of the thin colloid coal type becomes possible; on the basis, optimization of the determination process can be further realized by establishing a database of determined coal types and utilizing neural network self-learning.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of bituminous coal colloid thickness detection, in particular to a device for accurately detecting the Y value of a bituminous coal colloid layer. Background Art

[0002] The method for determining the index of the colloidal layer is designed to simulate the coking conditions of an industrial coke oven. According to the provisions of GB / T 479, the coal sample is placed on a steel cup, a constant pressure is applied on it, and it is heated from one side of the bottom to form a series of isothermal layers. The height increases steadily from top to bottom, so that the coal sample in the coal cup forms a semi-coke layer and a colloidal layer. The thickness of the colloidal body is measured by a probe, and the maximum thickness Y is used as an index to indicate the coking property of the coal. At the end of the experiment, the distance between the final position and the starting position of its volume curve is measured, that is, the final shrinkage X. At the same time, the volume change curve of the coal sample during the heating process is recorded to determine the type of volume curve. The experiment starts from room temperature and the drying and preheating stage is before reaching 250℃. At 300-350℃, the coal sample begins to soften, pyrolyzes to produce colloidal bodies, and gradually begins to expand and shrink. At first, the colloidal layer is from thin to thick. As the temperature continues to rise, the solidification rate of the colloidal layer is greater than the generation rate, so it gradually becomes thinner until it disappears completely. At this time, the coal sample is completely solidified and semi-coke is generated, and the experiment ends.

[0003] Initially, the experimenter needs to master the correct feel to measure the upper and lower layers, otherwise it will have a great impact on the experiment. When measuring the upper layer, the probe can be inserted with resistance, and no force should be used, otherwise the upper layer will be dented and the measured value will be low. When measuring the lower layer, it is necessary to ensure that the probe penetrates the colloid to reach the semi-coke surface. When the colloid is very thin, the probe should be inserted slowly and with light force. When a slight resistance is felt, it is the upper layer. Then add a little force to slowly penetrate it. When a slightly larger resistance is felt, it stops, which is the lower layer. When the colloid is very viscous, after measuring the upper layer, a larger force must be used to penetrate the colloid, but the force must be uniform and vertical, otherwise it will not be able to penetrate, and the probe will be bent or even broken. When the colloid is penetrated to the point where the resistance is significantly increased, it reaches the semi-coke surface. This situation is generally encountered in zigzag, mountain or mixed zigzag volume curves. In addition, for large zigzag coal samples, when measuring the values ​​of the upper and lower layers, it is necessary to measure slightly before the recording pen reaches the top and bottom, otherwise the recording pen will fall and rise immediately, missing the opportunity for accurate measurement.

[0004] In order to avoid the influence of the experimental personnel's operating factors on the results, a variety of automatic detection devices for the thickness of the colloid layer have been developed; however, at present, almost all automatic detection devices for the thickness of the bituminous coal colloid layer (Y value) use the motor to drive the screw rod to move vertically up and down in the forward and reverse rotation, and use the pressure sensor to drive the probe to measure. For example, the "bituminous coal colloid layer automatic detection device" disclosed in the Chinese utility model patent with the authorization announcement number CN 2144293Y uses a DC motor and a screw rod as a transmission device, and uses a force-sensitive sensor to collect the force signal when the probe touches the surface of each material, and directly obtains the maximum colloid layer through computer processing. The "colloid layer measuring instrument" disclosed in the Chinese utility model patent with the authorization announcement number CN 201034575Y uses a probe control component composed of a stepping motor and a screw rod, and a probe sensing device composed of a pressure sensor and a probe.

[0005] The principle of the above-mentioned colloid thickness detection device is: the feedback force when the probe end contacts different layers of the colloid is different, and the pressure sensor detects the change in feedback force, thereby judging whether the probe contacts the surface of the colloid or the semi-coke layer. The typical feature of the above-mentioned colloid layer Y value determination device is that the probe and the pressure sensor are inseparable during detection, and the layer must be judged by the direct feedback of the pressure sensor force on the probe force. This type of device has the following problems:

[0006] 1. For zigzag or mixed coal samples, due to the very fast changes in their characteristic properties, that is, the X value has a high frequency of fluctuation and a large change in the upper and lower amplitudes, the probe for detecting the Y value cannot respond quickly, resulting in a lag in the time node of the peak or valley point of the X value. This is because the above-mentioned transmission device converts the rotary motion of the motor into the linear motion of the probe, and the speed of the mechanical motion cannot meet the higher speed requirements. At the same time, too fast a speed will cause a force impact when contacting the colloid layer, or even directly penetrate the surface. As a result, the time node of the Y value detection cannot correspond to the X value one by one, which will inevitably cause errors or even measurement failures.

[0007] 2. The colloid produced by lean coal and lean coking coal is very thin, and the colloid layer is thin and soft. It will be deformed or even punctured by a slight external force. When the probe reaches the colloid layer, it must generate a force sufficient for the pressure sensor to get feedback. At this time, the response time and force sensitivity of the pressure sensor will cause a large deviation in the measurement result, or even fail to measure normally. For example, when the probe reaches the colloid layer, because the colloid surface is very thin and soft, even if the probe has touched the surface, it does not generate enough force for the pressure sensor to feedback. Then the probe can only continue to move downward until there is enough force feedback at a certain depth to trigger the pressure sensor to respond. This will inevitably cause the thin and soft colloid layer to sag or even be punctured under the pressure of the probe. At this time, the detection position has deviated from the true colloid layer, and the obtained measurement data is also wrong. Therefore, it is difficult for the above-mentioned automatic colloid layer measurement device to accurately measure the colloid of lean coal or lean coking coal.

[0008] 3. Another method is to input the type of coal to be measured into the computer system in advance when detecting the thickness of the colloid layer, and then measure it based on previous empirical data. However, the problem of the detection process being affected by human factors cannot be solved.

[0009] The "coal colloid layer thickness detection device" disclosed in the Chinese utility model patent with the authorization announcement number CN 211121140U includes a heating furnace, a coal cup, a bracket, a lifting motor, a pressure sensor and a probe; it also includes a translation mechanism and a balance frame, the pressure sensor is composed of a large-range pressure sensor and a small-range pressure sensor, and the probe is composed of a first probe and a second probe; the middle part of the balance frame is connected to the output shaft of the lifting motor, and the two ends of the balance frame are respectively connected to the first probe through a large-range pressure sensor and connected to the second probe through a small-range pressure sensor; the lifting motor is connected to the bracket through a translation mechanism. Two ranges of pressure sensors are used to measure the bottom and top of the colloid layer respectively, in order to solve the problem of inaccurate measurement caused by the large range span of the pressure sensor. Although the use of a small-range pressure sensor can improve the measurement accuracy to a certain extent, it does not fundamentally solve the above-mentioned problems.

[0010] The Chinese patent application with publication number CN 116448668 A discloses "a handheld SLP probe for measuring the Y value of the colloid layer", which includes a furnace body mainframe, a button panel, a PC terminal, a wireless SLP probe, and a mobile terminal. The furnace body mainframe is connected to the control panel and the PC terminal respectively by cables, and is connected to the wireless SLP probe by wireless or wired means, and the wireless SLP probe communicates wirelessly with the mobile terminal. It uses non-contact laser detection distance to accurately read the probe measurement reading, and uses the wireless communication module in the digital module to achieve remote communication with the mobile terminal. The probe can also be connected to a digital sharing tool and added to the Internet of Things, which not only retains the advantages of manual measurement but also avoids the disadvantages of manual detection readings, and can also achieve remote observation readings. It realizes non-contact reading of probe readings, but this measurement method is only designed for manual replacement of traditional mechanical probes, and is not compatible with the automatic measurement of the utility model. Summary of the invention

[0011] The utility model provides a device for accurately detecting the Y value of a bituminous coal colloid layer. The free-fall motion of a probe assembly cooperates with a non-contact probe position measuring device to achieve the measurement of the position of the upper surface of the colloid, greatly reducing the lag time of the X-value peak point (within 100 milliseconds), thereby improving the accuracy of the measurement; at the same time, the measurement of thin colloid coal types becomes possible; on this basis, the measurement process can be optimized by further establishing a database for measuring coal types and utilizing neural network self-learning.

[0012] In order to achieve the above purpose, the utility model adopts the following technical solutions:

[0013] A device for accurately detecting the Y value of a bituminous coal colloid layer, comprising a device support, a coal cup, a motor, a screw-nut transmission mechanism and a pressure sensor; further comprising a probe assembly, a control system, a non-contact probe position measuring device and a locking mechanism; the probe assembly consists of a probe and a reflector, the reflector being placed on the top of the probe; the measuring end of the non-contact probe position measuring device acts on the reflector; the motor is arranged on the device support, the motor shaft is connected to the upper end of the screw, and the nut is transmission-connected to the screw; the pressure sensor and the locking mechanism are respectively fixedly connected to the nut, and the measuring end of the pressure sensor is located directly above the probe; the locking mechanism can lock the probe assembly so that it is suspended in the air, or release the probe assembly so that it falls freely; the coal cup is located below the probe assembly; the driving end of the motor, the signal output end of the pressure sensor, the driving end and the signal output end of the non-contact probe position measuring device, and the driving end of the locking mechanism are respectively connected to the control system.

[0014] Furthermore, the motor is a servo motor.

[0015] Furthermore, the non-contact probe position measuring device is a laser, and the laser beam emitted by the laser acts vertically downward on the top surface of the reflective plate.

[0016] Furthermore, the non-contact probe position measuring device is an ultrasonic sensor, and the ultrasonic signal emitted by the ultrasonic sensor acts on the top surface of the reflector.

[0017] Furthermore, the locking mechanism is an electromagnet; the electromagnet is connected to the nut through a fixed connecting plate; and one side of the reflector is magnetically connected to the iron core of the electromagnet.

[0018] Furthermore, the locking mechanism is a mechanical clamping mechanism, which is provided with an openable and closable clamp, and one side of the reflective plate is clamped in the openable and closable clamp.

[0019] Furthermore, the probe is composed of a needle body and a needle cap, the diameter of the needle cap is larger than the diameter of the needle body, and the pressure sensor acts on the needle cap; a guide rail is provided on one side of the probe falling path.

[0020] Furthermore, the reflective plate is made of aluminum or aluminum alloy, stainless steel, non-metallic material, or a composite plate of non-metallic material and metal material, and has a thickness of 0.2 to 1 mm.

[0021] Compared with the prior art, the beneficial effects of the utility model are:

[0022] 1) The free fall motion of the probe assembly cooperates with the non-contact probe position measurement device to measure the position of the upper layer of the colloid, and the measurement process is not affected by the motor, screw transmission mechanism and pressure sensor;

[0023] 2) The probe assembly is locked and released by a locking mechanism. After the probe is released, it falls freely along the guide rail and rises with the locking mechanism after the measurement is completed. The device has a simple structure;

[0024] 3) Apply downward pressure to the probe assembly through the combined mechanism of motor-screw nut transmission-pressure sensor, and measure the position of the lower layer of the colloid;

[0025] 4) Since the probe assembly (probe and reflector) is very light, the external force exerted on the colloid when it reaches the upper layer of the colloid after free fall has little effect, which greatly reduces the lag time of the peak point of the X value (within 100 milliseconds), thereby improving the accuracy of the measurement;

[0026] 5) The free fall motion of the probe assembly and the non-contact probe position measurement device make it possible to accurately detect the colloid of thin colloid coal. It has been verified in practice that the flocculent coal produced by some lean coal with a Y value thickness of less than 4mm can be accurately measured with good reproducibility.

[0027] 6) Establish a database for measuring coal types through edge computing, use neural networks to achieve self-learning measurement of Y values, and then realize AI intelligent measurement. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 It is a structural schematic diagram of a device for accurately detecting the Y value of a bituminous coal colloid layer according to the utility model.

[0029] Figure 2 It is a schematic diagram of the probe assembly of the utility model being located at an initial position before measurement.

[0030] Figure 3 It is a schematic diagram of the measurement of the upper layer of the colloid described in the present invention (the probe is in contact with the upper layer of the colloid).

[0031] Figure 4 It is a schematic diagram of the measurement of the lower layer of the colloid described in the present invention (the probe is in contact with the lower layer of the colloid).

[0032] Figure 5 This is an illustration of the probe response lag when using a conventional automatic colloid thickness detection device. Figure 1 .

[0033] Figure 6 This is an illustration of the probe response lag when using a conventional automatic colloid thickness detection device. Figure 2 .

[0034] In the figure: 1. Laser 1.1. Laser beam 2. Pressure sensor 3. Servo motor 4. Screw 5. Screw nut 6. Fixed connecting plate 7. Electromagnet 7.1. Iron core 8. Guide rail 9. Probe assembly 9.1. Needle body 9.2. Needle cap 9.3. Reflector 10. Control system 11. Cigarette paper tube 12. Coal cup 13. Colloid 14. Semi-coke layer 15. Probe DETAILED DESCRIPTION

[0035] The specific implementation of the utility model is further described below in conjunction with the accompanying drawings:

[0036] like Figure 1As shown, the utility model discloses a device for accurately detecting the Y value of a bituminous coal colloid layer, comprising a device support, a coal cup 12, a motor, a screw-nut transmission mechanism and a pressure sensor 2; it also comprises a probe assembly 9, a control system 10, a non-contact probe position measuring device and a locking mechanism; the probe assembly 9 is composed of a probe and a reflector 9.3, and the reflector 9.3 is placed on the top of the probe; the measuring end of the non-contact probe position measuring device acts on the reflector 9.3; the motor is arranged on the device support, the motor shaft is connected to the upper end of the screw 4, and the nut 5 is transmission-connected to the screw 4; the pressure sensor 2 and the locking mechanism are respectively fixedly connected to the nut 5, and the measuring end of the pressure sensor 2 is located directly above the probe; the locking mechanism can lock the probe assembly 9 so that it is suspended in the air, or release the probe assembly 9 so that it falls freely; the coal cup 12 is located below the probe assembly 9; the driving end of the motor, the signal output end of the pressure sensor 2, the driving end and the signal output end of the non-contact probe position measuring device, and the driving end of the locking mechanism are respectively connected to the control system 10.

[0037] Furthermore, the motor is a servo motor 3 .

[0038] Furthermore, the non-contact probe position measuring device is a laser 1, and the laser beam 1.1 emitted by the laser 1 acts vertically downward on the top surface of the reflective plate 9.3.

[0039] Furthermore, the non-contact probe position measuring device is an ultrasonic sensor, and the ultrasonic signal emitted by the ultrasonic sensor acts on the top surface of the reflector.

[0040] Furthermore, the locking mechanism is an electromagnet 7; the electromagnet 7 is connected to the nut 5 via a fixed connecting plate 6; one side of the reflector 9.3 is magnetically connected to the iron core 7.1 of the electromagnet 7.

[0041] Furthermore, the locking mechanism is a mechanical clamping mechanism, which is provided with an openable and closable clamp, and one side of the reflective plate 9.3 is clamped in the openable and closable clamp.

[0042] Furthermore, the probe is composed of a needle body 9.1 and a needle cap 9.2, the diameter of the needle cap 9.2 is larger than the diameter of the needle body 9.1, and the pressure sensor 2 acts on the needle cap 9.2; a guide rail 8 is provided on one side of the probe falling path.

[0043] Furthermore, the reflector 9.3 is made of aluminum or aluminum alloy, stainless steel, non-metallic material, or a composite plate of non-metallic material and metal material, with a thickness of 0.2-1 mm.

[0044] The method for using the device for accurately detecting the Y value of a bituminous coal colloid layer described in the utility model is as follows:

[0045] 1) The coal cup 12 is placed on a heating furnace, and a coal sample is placed in the coal cup 12 and heated;

[0046] 2) If Figure 1 , Figure 2 As shown, the probe assembly 9 is suspended above the coal cup 12 by a locking mechanism, and the non-contact probe position measuring device is started by the control system 10 so that its measuring end acts on the reflective plate 9.3;

[0047] 3) When measuring the upper surface of the colloid of the coal sample, the control system 10 controls the locking mechanism to loosen the probe assembly 9; the probe assembly 9 falls vertically along the guide rail 8, passes through the cigarette tube 11 and stays on the upper surface of the colloid 13 (such as Figure 3 The non-contact probe position measuring device measures the vertical distance between it and the reflector 9.3, and transmits the measured data to the control system 10;

[0048] 4) When measuring the lower surface of the colloid of the coal sample, the control system 10 controls the motor to start, and the motor shaft drives the screw 4 to rotate, so that the nut 5 moves downward along the screw 4; the pressure sensor 2 obtains force feedback after contacting the needle cap 9.2 of the probe; the pressure sensor 2 applies pressure to the probe so that the probe pierces the colloid 13, and when the probe head reaches the surface of the semi-coke layer 14 (such as Figure 4 As shown), the control system 10 makes a judgment according to the change of the feedback value of the force, and then the control system 10 stops the motor from moving, and the non-contact probe position measuring device measures the vertical distance between it and the reflective plate 9.3 again, and transmits the measured data to the control system 10;

[0049] 5) The control system 10 calculates the maximum thickness of the colloid layer, i.e., the value Y, according to the data measured in step 3) and step 4);

[0050] 6) After the measurement is completed, the control system 10 controls the locking mechanism to re-lock the reflector 9.3, and the motor rotates in the reverse direction, driving the pressure sensor 2 and the probe assembly 9 to move upward synchronously and return to the initial position, waiting for the next measurement.

[0051] Furthermore, the control system 10 includes an edge computer, which establishes a database based on the measured data and forms a self-learning mode based on the neural network. In subsequent measurements, the neural network calculation is automatically performed according to the type of coal and a prediction is made in advance to optimize the measurement process.

[0052] Normally, when measuring colloid, the distance between the lower end of the probe and the bottom of the coal cup is about 50 mm or less. Calculated based on the distance of 50 mm, the time taken for the probe to fall vertically within this distance is about 0.1 s. When colloid is produced in the coal sample, as the thickness of the colloid increases, the distance between the upper layer of the colloid and the lower end of the probe will gradually decrease. Then the time for the probe to freely fall from the initial position to the upper layer of the colloid will be much less than 0.1 s.

[0053] When a certain type of bituminous coal is in a certain shape and changes very quickly, the Y value should be measured at the peak point of the X value curve according to the provisions of GB / T 479. As mentioned above, the conventional bituminous coal colloid thickness automatic detection device uses a motor screw drive to drive the probe downward. If the downward speed is too fast, the inertia force when the probe hits the upper layer of the colloid will be too large, resulting in measurement failure or large deviation in the measurement data. Therefore, the speed when the motor drives the probe downward cannot be too fast, but this will cause the probe to lag behind seriously when measuring the upper layer of the colloid, that is, the point where the Y value is measured has deviated from the peak point of the X value. Figure 5 As shown, point A is the peak point of the X value. From the start of the motor movement to the arrival of the probe at the upper layer of the colloid, the actual measurement point is point B. The time delay between point A and point B may be more than a few seconds. It can be seen that point B lags behind point A seriously.

[0054] The total weight of the probe assembly described in the utility model is only a few grams. When measuring the upper layer of the colloid, the force exerted by the overall weight of the probe assembly on the upper layer of the colloid is very small, especially when measuring lean coal, lean coke and other coal samples with extremely thin colloids. The probe assembly has little effect on the upper layer of the colloid. However, when using a conventional automatic detection device for the thickness of the bituminous coal colloid layer, the judgment condition can only be met when the probe passes through the cigarette paper tube 11 and contacts the upper layer of the colloid and the feedback force is large enough, causing the probe to continue to move downward to cause the upper layer of the colloid to deform. Figure 6 As shown in the figure, the measurement position should be point a, but in actual measurement, the probe 15 causes the upper surface of the colloid 13 to deform and sink, and the measurement point changes from point a to point b, resulting in a height error value H between the measured value and the true value. Since the colloids of different types of coal have different degrees of thinness, the H value cannot be compensated at all, resulting in a loss of accuracy in the measurement result. The probe may even directly pierce the colloid, resulting in the inability to measure the upper surface of the colloid normally.

[0055] However, the method of pre-inputting the type of coal or the built-in coal data characteristics before measurement cannot accurately obtain the data characteristics of all types of coal due to the large batch differences caused by the natural properties of coal. Therefore, this simple human intervention method is not feasible. An edge computer is provided in the control system described in the utility model, which not only controls various moving parts such as probe assemblies, motors, locking mechanisms, and receives and stores measurement data, but also establishes a database based on all measurement data and forms a self-learning mode based on neural networks. In subsequent measurements, neural network calculations can be automatically performed according to the type of coal, and pre-judgment can be performed in advance to optimize the detection process. The more types of coal measured, the richer the database, and the more accurate the optimized measurement. Finally, AI intelligent measurement is achieved through the self-learning process.

[0056] The non-contact probe position measurement device described in the present invention can be a laser, or an ultrasonic sensor, etc. As long as it is a device that can use non-contact measurement of probe displacement, it is within the protection scope of the present invention. Similarly, the locking mechanism described in the present invention has the function of locking (magnetic attraction or clamping) and releasing (demagnetizing or loosening) the probe assembly. The locking mechanism can use an electromagnet or a mechanical clamping mechanism, and can also use a linear motor, a linear guide slider and a baffle. In addition, the probe assembly described in the present invention is only a basic structure. Other forms of changes that occur on this basis are within the protection scope of the present invention as long as they use free fall motion.

[0057] The material of the reflector is preferably aluminum or aluminum alloy, ultra-thin stainless steel, non-metallic material, or a composite plate of non-metallic material and metal material. The smaller the dead weight, the better, and the thickness can be controlled at 0.2-1 mm.

[0058] The following examples are implemented based on the technical solution of the utility model, and provide detailed implementation methods and specific operation processes, but the protection scope of the utility model is not limited to the following examples. The methods used in the following examples are conventional methods unless otherwise specified.

[0059] [Example]

[0060] like Figure 1-Figure 4 As shown, in this embodiment, the device for accurately detecting the Y value of the bituminous coal colloid layer is composed of a device bracket, a coal cup, a servo motor, a screw rod, a nut, a pressure sensor, a probe assembly, a control system, a laser and an electromagnet.

[0061] The probe in the probe assembly can slide freely up and down along the guide rail. During measurement, the laser beam emitted by the laser acts vertically downward on the reflective plate to measure the real-time position of the probe, realizing non-contact measurement of the probe displacement data.

[0062] The locking mechanism is an electromagnet. Before and after the measurement, the probe assembly is attracted and locked by the iron core of the electromagnet. The electromagnet can be driven to move up and down through the motor and the screw-nut transmission mechanism.

[0063] When measuring the upper surface of the colloid, the electromagnet is activated, the electromagnet core retracts, and the probe assembly falls vertically along the guide rail in a free-falling manner under the action of its own gravity. In a very short time, the probe falls on the upper surface of the colloid and stops. The current position information of the probe can be obtained through the cooperation of the laser and the reflector and transmitted to the control system, thereby obtaining the position of the upper surface of the colloid.

[0064] When measuring the lower layer of the colloid, the servo motor drives the screw to rotate, so that the nut and the pressure sensor and electromagnet on it move downward synchronously, the measuring end of the pressure sensor contacts the needle cap, and the pressure sensor obtains force feedback. The pressure sensor applies pressure to the probe to pierce the colloid until the end of the needle reaches the surface of the semi-focus layer; the control system determines that the end of the probe has reached the surface of the off-focus layer based on the real-time feedback value of the force, and controls the motor to stop so that the probe no longer moves downward; at the same time, the laser cooperates with the reflector to transmit the current position information of the probe to the control system, and the thickness between the upper and lower layers of the colloid, that is, the Y value, can be calculated.

[0065] When the probe assembly stops moving, the control system controls the core of the electromagnet to extend and relock the probe assembly. Then the servo motor reverses and drives the electromagnet, probe assembly and pressure sensor to move upward synchronously through the screw rod and nut. Depending on the position of the probe, the servo motor uses variable speed operation. During the empty stroke when returning, the probe assembly moves at high speed until it returns to the initial position and stops, waiting for the next measurement process.

[0066] The above is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent substitutions or changes within the technical scope disclosed by the present invention according to the technical solution and inventive concept of the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A device for accurately detecting the Y value of a bituminous coal colloid layer, comprising a device bracket, a coal cup, a motor, a screw-nut transmission mechanism and a pressure sensor; characterized in that: It also includes a probe assembly, a control system, a non-contact probe position measuring device and a locking mechanism; the probe assembly consists of a probe and a reflector, the reflector is placed on the top of the probe; the measuring end of the non-contact probe position measuring device acts on the reflector; the motor is arranged on the device bracket, the motor shaft is connected to the upper end of the screw rod, and the nut is connected to the screw rod by transmission; the pressure sensor and the locking mechanism are fixedly connected to the nut respectively, and the measuring end of the pressure sensor is located directly above the probe; The locking mechanism can lock the probe assembly so that it is suspended in the air, or release the probe assembly so that it falls freely; the coal cup is located below the probe assembly; the driving end of the motor, the signal output end of the pressure sensor, the driving end and signal output end of the non-contact probe position measuring device, and the driving end of the locking mechanism are respectively connected to the control system.

2. The device for accurately detecting the Y value of a bituminous coal colloid layer according to claim 1, characterized in that: The motor is a servo motor.

3. The device for accurately detecting the Y value of a bituminous coal colloid layer according to claim 1, characterized in that: The non-contact probe position measuring device is a laser, and the laser beam emitted by the laser acts vertically downward on the top surface of the reflective plate.

4. The device for accurately detecting the Y value of a bituminous coal colloid layer according to claim 1, characterized in that: The non-contact probe position measuring device is an ultrasonic sensor, and the ultrasonic signal emitted by the ultrasonic sensor acts on the top surface of the reflector.

5. The device for accurately detecting the Y value of a bituminous coal colloid layer according to claim 1, characterized in that: The locking mechanism is an electromagnet; the electromagnet is connected to the nut through a fixed connecting plate; one side of the reflector is magnetically connected to the iron core of the electromagnet.

6. The device for accurately detecting the Y value of a bituminous coal colloid layer according to claim 1, characterized in that: The locking mechanism is a mechanical clamping mechanism, which is provided with an openable and closable clamp, and one side of the reflective plate is clamped in the openable and closable clamp.

7. The device for accurately detecting the Y value of a bituminous coal colloid layer according to claim 1, characterized in that: The probe is composed of a needle body and a needle cap. The diameter of the needle cap is larger than the diameter of the needle body. The pressure sensor acts on the needle cap. A guide rail is arranged on one side of the probe falling path.

8. The device for accurately detecting the Y value of a bituminous coal colloid layer according to claim 1, characterized in that: The reflective plate is made of aluminum or aluminum alloy, stainless steel, non-metallic material, or a composite plate of non-metallic material and metal material, and has a thickness of 0.2-1 mm.

Citation Information

Cited By

  • Device and method for accurately detecting Y value of bituminous coal gelatinous layer