Vacuum brazing structure for dissimilar materials

By using an interference fit front lip and overlapping portion in the vacuum brazing structure of the solenoid, the problems of poor centering effect and solder loss in the prior art are solved, and the coaxiality and coaxiality after welding are improved. Welding quality.

CN221848927UActive Publication Date: 2024-10-18GUANGZHOU HUITONG PRECISION HYDRAULIC CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420339059.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-23
Publication Date
2024-10-18
Estimated Expiration
2034-02-23

AI Technical Summary

Technical Problem

In the existing vacuum brazing structure of the solenoid, the gap between the front lip and the magnetic isolation ring at the front and rear ends reduces the centering effect, makes it difficult to meet the coaxiality requirements, and the solder is easily lost, affecting the welding quality.

Method used

Using a dissimilar material vacuum brazing structure, interference fit is performed between the front lips of the first weldment and the second weldment and the inner hole of the magnetic isolation ring to ensure that the two front lips are centered and the solder is isolated, using a shaft The diameter of the overlapping part and front lip gradually becomes smaller, and the inner hole of the magnetic isolation ring is filled with solder to avoid loss.

Benefits of technology

The coaxiality after brazing is improved, the loss of solder is avoided, and the welding quality is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221848927U_ABST
    Figure CN221848927U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of brazing, in particular to a vacuum brazing structure for dissimilar materials. The dissimilar material vacuum brazing structure comprises a first weldment, a magnetism isolating ring and a second weldment, the rear end of the first weldment is provided with a first lap joint part and a first front lip part with the shaft diameter sequentially decreasing, and the front end of the second weldment is provided with a second lap joint part and a second front lip part with the shaft diameter sequentially decreasing. The magnetism isolating ring is arranged at the rear end of the first weldment and the front end of the second weldment in a sleeving mode, and the first front lip part and the second front lip part are right opposite to each other and arranged in a spaced mode. The first lap joint part and the second lap joint part are both in clearance fit with an inner hole of the magnetism isolating ring, and the first front lip part and the second front lip part are both in interference fit with the inner hole of the magnetism isolating ring; the gap between the magnetism isolating ring and the rear end of the first weldment and the gap between the magnetism isolating ring and the front end of the second weldment are filled with brazing filler metal. And the two front lip parts are in interference fit with the inner hole of the magnetism isolating ring, so that the coaxiality of the brazed first weldment and the brazed second weldment is improved, and meanwhile, the loss of brazing filler metal in the welding process is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of brazing, in particular to a vacuum brazing structure of dissimilar materials. Background Art

[0002] In hydraulic valve products, such as solenoids, metals of different materials need to be connected and sealed, and the connection parts need to meet the processing requirements of high strength and good sealing. The front and rear ends of existing solenoids are processed and manufactured by vacuum brazing. During the vacuum welding process, the mating surface of the front end of the solenoid is coated with brazing material, and a magnetic isolation ring (usually a stainless steel ring) is put on the mating surface of the front end. Then, the mating surface of the rear end of the solenoid is coated with brazing material and then put into the magnetic isolation ring, so that the front and rear ends are aligned through the magnetic isolation ring, and finally the assembled structure is placed vertically in the brazing tooling. The solenoid is heated and insulated in a vacuum environment, so that the brazing material melts within a suitable temperature and time range, and fully infiltrates, dissolves, diffuses, and welds with the solid metal under the action of capillary force to achieve the welding purpose.

[0003] In the above-mentioned brazing structure, the two front lips at the front and rear ends are clearance-fitted with the magnetic isolation ring, which not only reduces the centering effect of the front and rear ends, resulting in the coaxiality of the solenoid after brazing being difficult to meet the requirements, but also the brazing material located above is easy to leak through the gap between the front lip and the magnetic isolation ring, affecting the welding quality. Utility Model Content

[0004] The utility model aims to provide a vacuum brazing structure of dissimilar materials, so as to improve the centering effect of the front end and the rear end of the brazing structure, improve the coaxiality after welding, and avoid the loss of brazing material.

[0005] To achieve this purpose, the technical solution adopted by the utility model is:

[0006] A vacuum brazing structure of dissimilar materials, comprising a first weldment, a magnetic isolation ring, and a second weldment, wherein the rear end of the first weldment has a first overlap portion and a first front lip portion with successively smaller shaft diameters, and the front end of the second weldment has a second overlap portion and a second front lip portion with successively smaller shaft diameters;

[0007] The magnetic isolation ring is sleeved on the rear end of the first weldment and the front end of the second weldment, and the first front lip and the second front lip are opposite and spaced apart; the first overlapping portion and the second overlapping portion are both gap-fitted with the inner hole of the magnetic isolation ring, and the first front lip and the second front lip are both interference-fitted with the inner hole of the magnetic isolation ring; the gap between the magnetic isolation ring and the rear end of the first weldment and the gap between the magnetic isolation ring and the front end of the second weldment are both filled with solder.

[0008] As a preferred solution, the inner hole of the magnetic isolation ring includes a first hole, a second hole and a third hole which are connected in sequence, and the inner diameter of the second hole is smaller than the inner diameters of the first hole and the third hole;

[0009] The outer diameters of the first front lip and the second front lip are equal, the first overlap portion is clearance-fitted with the first hole, the first front lip and the second front lip are interference-fitted with the second hole, and the second overlap portion is clearance-fitted with the second hole.

[0010] As a preferred embodiment, a first transition surface is provided between the first overlapping portion and the first front lip portion, a second transition surface is provided between the second overlapping portion and the second front lip portion, a third transition surface is provided between the first hole and the second hole, and a fourth transition surface is provided between the second hole and the third hole. The first transition surface and the third transition surface are arranged opposite to each other and are clearance-matched, and the second transition surface and the fourth transition surface are arranged opposite to each other and are clearance-matched.

[0011] As a preferred solution, the angle between the first transition surface and the outer peripheral surface of the first overlap portion is α1, the filling thickness of the solder between the first transition surface and the third transition surface is w1, and the length of the first front lip portion is H1=w1 / sinα1;

[0012] The included angle between the second transition surface and the outer peripheral surface of the second overlapping portion is α2, the filling thickness of the solder between the second transition surface and the fourth transition surface is w2, and the length of the second front lip portion is H2=w2 / sinα2.

[0013] As a preferred embodiment, an inwardly recessed material storage trough is provided at the intersection of the first hole and the third transition surface, and at the intersection of the third hole and the fourth transition surface.

[0014] As a preferred solution, the gap between the first overlapping portion and the first hole is δ1, then δ1=K(D0-D1), the gap between the second overlapping portion and the third hole is δ2, then δ2=K(D0-D2), K is the filling coefficient, D0 is the outer diameter of the magnetic isolation ring, D1 is the inner diameter of the first hole, and D2 is the inner diameter of the second hole.

[0015] As a preferred solution, the outer diameters of the first overlapping portion and the second overlapping portion are equal, and the inner diameter of the first hole and the inner diameter of the third hole are equal.

[0016] As a preferred solution, the outer diameter of the magnetic isolation ring is D0, the length of the magnetic isolation ring is L, and L>0.2D0.

[0017] As a preferred solution, the magnetic isolation ring is a stainless steel ring.

[0018] As a preferred solution, the solder is a copper-based solder, a nickel-based solder or a silver-based solder.

[0019] The beneficial effects of the utility model are:

[0020] The vacuum brazing structure of dissimilar materials proposed by the utility model has a good centering effect because the first front lip and the second front lip are both interference-fitted with the inner hole of the magnetic isolation ring, thereby improving the coaxiality of the first weldment and the second weldment after brazing. At the same time, the interference fit between the two front lips and the magnetic isolation ring can isolate the brazing material at the rear end of the first weldment from the brazing material at the front end of the second weldment, thereby avoiding the loss of brazing material during welding and improving the welding quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 It is a schematic diagram of the structural decomposition of a dissimilar material vacuum brazing structure provided by an embodiment of the utility model;

[0022] Figure 2 It is a structural schematic diagram of a dissimilar material vacuum brazing structure provided by an embodiment of the utility model;

[0023] Figure 3 yes Figure 2 A partial enlarged view of point A in the middle.

[0024] The names and numbers of the components in the figure are as follows:

[0025] 1. first weldment; 11. first overlap portion; 12. first front lip portion; 13. first transition surface;

[0026] 2. Magnetic isolation ring; 21. First hole; 22. Second hole; 23. Third hole; 24. Third transition surface; 25. Fourth transition surface; 26. Material storage trough;

[0027] 3. Second weldment; 31. Second overlapping portion; 32. Second front lip portion; 33. Second transition surface. DETAILED DESCRIPTION

[0028] In order to make the technical problems solved by the present invention, the technical solutions adopted and the technical effects achieved clearer, the technical solutions of the present invention are further described below in conjunction with the accompanying drawings and through specific implementation methods. It is understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for the convenience of description, only the parts related to the present invention are shown in the accompanying drawings, rather than all of them.

[0029] In the description of the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", and "fixed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0030] In the present utility model, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.

[0031] In the description of this embodiment, the terms "upper", "lower", "right", "left" and other directions or positional relationships are based on the directions or positional relationships shown in the drawings, and are only for the convenience of description and simplified operation, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation of the present invention. In addition, the terms "first" and "second" are only used to distinguish in the description and have no special meaning.

[0032] The technical solution of the utility model is further explained below with reference to the accompanying drawings and through specific implementation methods.

[0033] The front and rear ends of existing solenoids are processed and manufactured by vacuum brazing. In the vacuum brazing structure of the solenoid, the front lips and the magnetic isolation rings of the front and rear ends are both in a gap fit, which not only reduces the centering effect of the front and rear ends, resulting in the coaxiality of the solenoid after brazing being difficult to meet the requirements, but also the assembly structure of the solenoid is placed vertically in the brazing tooling, and the brazing material at the top is easy to flow through the gap between the front lip and the magnetic isolation ring, affecting the welding quality.

[0034] To solve the above problems, Figure 1 to Figure 3As shown, this embodiment also proposes a vacuum brazing structure of dissimilar materials, which includes a first welding piece 1, a magnetic isolation ring 2 and a second welding piece 3. The rear end of the first welding piece 1 has a first overlap portion 11 and a first front lip portion 12 whose axial diameters decrease successively, and the front end of the second welding piece 3 has a second overlap portion 31 and a second front lip portion 32 whose axial diameters decrease successively. The magnetic isolation ring 2 is sleeved on the rear end of the first welding piece 1 and the front end of the second welding piece 3, and the first front lip portion 12 and the second front lip portion 32 are opposite and spaced apart; the first overlap portion 11 and the second overlap portion 31 are both in clearance fit with the inner hole of the magnetic isolation ring 2, and the first front lip portion 12 and the second front lip portion 32 are both interference fit with the inner hole of the magnetic isolation ring 2. The gap between the magnetic isolation ring 2 and the rear end of the first welding piece 1 and the gap between the magnetic isolation ring 2 and the front end of the second welding piece 3 are filled with brazing material. Since the first front lip 12 and the second front lip 32 are both interference fit with the inner hole of the magnetic isolation ring 2, the two front lips have a good centering effect, which improves the coaxiality of the first weldment 1 and the second weldment 3 after brazing. At the same time, the interference fit between the two front lips and the magnetic isolation ring 2 can isolate the brazing material at the rear end of the first weldment 1 from the brazing material at the front end of the second weldment 3, avoiding the loss of brazing material during welding and improving the welding quality.

[0035] In this embodiment, the first weldment 1 and the second weldment 3 are aligned and then welded into a solenoid through the magnetic isolation ring 2. In other embodiments, the first weldment 1 and the second weldment 3 can also be welded assembly structural parts of other products, which are not specifically limited here.

[0036] It should be noted that the magnetic isolation ring 2 is a stainless steel ring, which is easy to process and manufacture and has a good magnetic isolation effect. In other embodiments, the magnetic isolation ring 2 can also be made of other metal materials with magnetic isolation properties, as long as it can be welded with the first weldment 1 and the second weldment 3. The solder can be a copper-based solder, a nickel-based solder or a silver-based solder to ensure good welding quality between the magnetic isolation ring 2 and the two weldments.

[0037] Specifically, Figure 1As shown, the inner hole of the magnetic isolation ring 2 includes a first hole 21, a second hole 22 and a third hole 23 which are connected in sequence, and the inner diameter of the second hole 22 is smaller than the inner diameters of the first hole 21 and the third hole 23. The outer diameters of the first front lip 12 and the second front lip 32 are equal, the first overlap portion 11 and the first hole 21 are clearance-matched, the first front lip 12 and the second front lip 32 are interference-fitted with the second hole 22, and the second overlap portion 31 and the second hole 22 are clearance-matched. The outer diameters of the first overlap portion 11 and the second overlap portion 31 are equal, and the inner diameter of the first hole 21 and the inner diameter of the third hole 23 are equal. In other embodiments, the outer diameters of the first overlap portion 11 and the second overlap portion 31 may also be unequal, and the inner diameter of the first hole 21 and the inner diameter of the third hole 23 are adaptively adjusted so that the gap between the first overlap portion 11 and the first hole 21 and the gap between the second overlap portion 31 and the third hole 23 are within an appropriate range.

[0038] like Figure 1 and Figure 3 As shown, there is a first transition surface 13 between the first overlap portion 11 and the first front lip portion 12, a second transition surface 33 between the second overlap portion 31 and the second front lip portion 32, a third transition surface 24 between the first hole 21 and the second hole 22, a fourth transition surface 25 between the second hole 22 and the third hole 23, the first transition surface 13 and the third transition surface 24 are arranged opposite to each other and have clearance fit, and the second transition surface 33 and the fourth transition surface 25 are arranged opposite to each other and have clearance fit. Through the clearance fit between the first hole 21 and the first overlap portion 11, the clearance fit between the first transition surface 13 and the third transition surface 24, the clearance fit between the second overlap portion 31 and the third hole 23, and the clearance fit between the second transition surface 33 and the fourth transition surface 25, a filling space for solder is formed between the first hole 21 and the first overlap portion 11, between the first transition surface 13 and the third transition surface 24, between the second overlap portion 31 and the third hole 23, and between the second transition surface 33 and the fourth transition surface 25.

[0039] like Figure 3 As shown, the angle between the first transition surface 13 and the outer peripheral surface of the first lap joint 11 is α1, the filling thickness of the solder between the first transition surface 13 and the third transition surface 24 is w1, and the length of the first front lip 12 is H1=w1 / sinα1. The angle between the second transition surface 33 and the outer peripheral surface of the second lap joint 31 is α2, the filling thickness of the solder between the second transition surface 33 and the fourth transition surface 25 is w2, and the length of the second front lip 32 is H2=w2 / sinα2. By setting the length of the first front lip 12 to H1 and the length of the second front lip 32 to H2, the first front lip 12 and the second front lip 32 can contact the inner wall of the second hole 22, ensuring the interference fit between the second hole 22 and the two front lips. It should be noted that the volume of the filled solder is more than 1.2 times the filling space to ensure sufficient filling of the solder and improve the welding quality.

[0040] Furthermore, if Figure 3 As shown, the gap between the first overlap portion 11 and the first hole 21 is δ1, then δ1=K(D0-D1), the gap between the second overlap portion 31 and the third hole 23 is δ2, then δ2=K(D0-D2), K is the filling factor, D0 is the outer diameter of the magnetic isolation ring 2, D1 is the inner diameter of the first hole 21, and D2 is the inner diameter of the second hole 22. The above gaps δ1 and δ2 are the gap values ​​after welding. The value of K is related to the size of w1 and w2, and the larger w1 and w2 are, the smaller the K value is. The value of K can be an empirical value obtained through multiple tests. By setting δ1 and δ2 to the above values, the thermal stress and contact stress of the two overlap edges of the magnetic isolation ring 2 (the hole walls of the first hole 21 and the third hole 23) during the welding process are reduced, and the stress deformation of the two overlap edges is reduced.

[0041] It should be noted that the outer diameter of the magnetic isolation ring 2 is D0, and the length of the magnetic isolation ring 2 in this embodiment is L, L>0.2D0, so that the two overlapping edges have sufficient length, increasing the filling space, ensuring the use of solder, and facilitating the solder to be fully filled in the filling space.

[0042] like Figure 2 and Figure 3 As shown, the intersection of the first hole 21 and the third transition surface 24, and the intersection of the third hole 23 and the fourth transition surface 25 are both provided with an inwardly recessed material storage groove 26. The provision of the material storage groove 26 can not only guide and buffer the flow of the solder, but also allow the heated and molten solder to flow smoothly in the filling space, thereby improving the filling effect. At the same time, the inwardly recessed material storage groove 26 can also store excess solder to prevent the solder from overflowing the filling space.

[0043] The above embodiments are only to illustrate the basic principles and characteristics of the present invention. The present invention is not limited by the above embodiments. Without departing from the spirit and scope of the present invention, the present invention may be subject to various changes and modifications, which are within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. Vacuum brazing structure of dissimilar materials, characterized in that: The invention comprises a first weldment (1), a magnetic isolation ring (2) and a second weldment (3), wherein the rear end of the first weldment (1) comprises a first overlap portion (11) and a first front lip portion (12) whose axial diameters decrease successively, and the front end of the second weldment (3) comprises a second overlap portion (31) and a second front lip portion (32) whose axial diameters decrease successively; The magnetic isolation ring (2) is mounted on the rear end of the first weldment (1) and the front end of the second weldment (3), and the first front lip (12) and the second front lip (32) are opposite to each other and spaced apart; the first overlap portion (11) and the second overlap portion (31) are both clearance-matched with the inner hole of the magnetic isolation ring (2), and the first front lip (12) and the second front lip (32) are both interference-fitted with the inner hole of the magnetic isolation ring (2); the gap between the magnetic isolation ring (2) and the rear end of the first weldment (1) and the gap between the magnetic isolation ring (2) and the front end of the second weldment (3) are both filled with solder.

2. The dissimilar material vacuum brazing structure according to claim 1, characterized in that: The inner hole of the magnetic isolation ring (2) comprises a first hole (21), a second hole (22) and a third hole (23) which are connected in sequence, and the inner diameter of the second hole (22) is smaller than the inner diameters of the first hole (21) and the third hole (23); The outer diameters of the first front lip (12) and the second front lip (32) are equal, the first overlapping portion (11) is clearance-fitted with the first hole (21), the first front lip (12) and the second front lip (32) are both interference-fitted with the second hole (22), and the second overlapping portion (31) is clearance-fitted with the second hole (22).

3. The dissimilar material vacuum brazing structure according to claim 2, characterized in that: A first transition surface (13) is provided between the first overlapping portion (11) and the first front lip portion (12), a second transition surface (33) is provided between the second overlapping portion (31) and the second front lip portion (32), a third transition surface (24) is provided between the first hole (21) and the second hole (22), a fourth transition surface (25) is provided between the second hole (22) and the third hole (23), the first transition surface (13) and the third transition surface (24) are arranged opposite to each other and are clearance-matched, and the second transition surface (33) and the fourth transition surface (25) are arranged opposite to each other and are clearance-matched.

4. The dissimilar material vacuum brazing structure according to claim 3, characterized in that: The included angle between the first transition surface (13) and the outer peripheral surface of the first overlap portion (11) is α1, the filling thickness of the solder between the first transition surface (13) and the third transition surface (24) is w1, and the length of the first front lip portion (12) is H1=w1 / sinα1; The included angle between the second transition surface (33) and the outer peripheral surface of the second overlap portion (31) is α2, the filling thickness of the solder between the second transition surface (33) and the fourth transition surface (25) is w2, and the length of the second front lip (32) is H2=w2 / sinα2.

5. The dissimilar material vacuum brazing structure according to claim 3, characterized in that: An inwardly recessed material storage trough (26) is provided at the intersection of the first hole (21) and the third transition surface (24), and at the intersection of the third hole (23) and the fourth transition surface (25).

6. The dissimilar material vacuum brazing structure according to claim 2, characterized in that: The gap between the first overlapping portion (11) and the first hole (21) is δ1, then δ1=K(D0-D1), the gap between the second overlapping portion (31) and the third hole (23) is δ2, then δ2=K(D0-D2), K is the filling factor, D0 is the outer diameter of the magnetic isolation ring (2), D1 is the inner diameter of the first hole (21), and D2 is the inner diameter of the second hole (22).

7. The dissimilar material vacuum brazing structure according to claim 2, characterized in that: The outer diameters of the first overlapping portion (11) and the second overlapping portion (31) are equal, and the inner diameter of the first hole (21) and the inner diameter of the third hole (23) are equal.

8. The dissimilar materials vacuum brazing structure according to any one of claims 1 to 7, characterized in that: The outer diameter of the magnetic isolation ring (2) is D0, and the length of the magnetic isolation ring (2) is L, where L>0.2D0.

9. The dissimilar materials vacuum brazing structure according to any one of claims 1 to 7, characterized in that: The magnetic isolation ring (2) is a stainless steel ring.

10. The dissimilar materials vacuum brazing structure according to any one of claims 1 to 7, characterized in that: The solder is a copper-based solder, a nickel-based solder or a silver-based solder.