Ceramic repair welding gun head
By adopting the design of a tapered discharge hole and a water-cooling component in the ceramic welding repair gun head, the problems of welding intensity dispersion and heat management during the welding repair process are solved, the welding repair quality and equipment stability are improved, and the service life is extended. And ensure operational safety.
Patent Information
- Application Number
- CN202420118792.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-17
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2034-01-17
AI Technical Summary
The existing ceramic welding repair gun head has problems such as dispersion of welding strength and poor heat management during the welding repair process, which affects the quality of welding repair and the life of the equipment.
A ceramic welding repair gun head is designed, which uses a tapered discharge hole and a water-cooling component. The diameter-reducing structure increases the gathering speed and pressure of the welding repair material, and the water-cooling system reduces the heat of the equipment to increase stability and safety.
It effectively reduces the dispersion of welding repair force, improves the quality of welding repair and the firmness of the welding joint, while extending the service life of the equipment and ensuring operational safety.
Smart Images

Figure CN221854472U_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the technical field of ceramic welding repair, and in particular to a ceramic welding repair gun head. Background Art
[0002] Ceramic welding repair technology is a new hot maintenance technology for industrial furnaces and kilns. It is mainly used to repair refractory materials such as refractory bricks inside industrial furnaces and kilns. This technology uses a mixture of powdered refractory materials and powdered metal combustibles as solder, and uses oxygen as a carrier to transport the solder to the repair area through a welding gun. Under high temperature, the metal and oxygen undergo a violent oxidation exothermic reaction, melting the solder and producing a ceramic bond, which is deposited in the repair area of the base refractory material until the required thickness is reached. Ceramic welding repair technology has the characteristics of compact structure and strong seismic resistance, and can form an overall dense structure with stable volume.
[0003] In ceramic welding repair technology, the ceramic welding gun is an important tool in ceramic welding repair technology, which is used to deliver the solder to the repair area. This welding gun has a unique design that can achieve independent movement relative to the welding gun and can simultaneously monitor the position of the welding gun outlet and the reaction zone. Another feature of the ceramic welding gun is that the ceramic welding material it sprays out has a high temperature, which allows it to form a strong bond with the refractory brick wall to be welded.
[0004] In the prior art, a Chinese patent with authorization announcement number CN206375830U discloses a welding gun head for a ceramic welding machine, which includes a horizontal tube and a vertical tube. The upper end of the vertical tube is connected to one end of the horizontal tube through an arc tube, and a T-shaped anchor is fixed on the outer side wall of the lower part of the vertical tube. The inner diameter of the gun head is straight, and the ceramic welding material is transported by the ceramic welding gun and then sprayed onto the refractory bricks on the sprayed surface through the ceramic welding gun head. The force is small and there is a divergence phenomenon, which will affect the quality of the ceramic welding. Utility Model Content
[0005] In order to reduce the divergence of welding repair force and reduce the impact on the quality of ceramic welding repair, the present application provides a ceramic welding gun head.
[0006] The present application provides a ceramic welding gun head, which adopts the following technical solution:
[0007] A ceramic welding gun head, comprising:
[0008] The gun barrel is provided with a straight receiving passage formed inside;
[0009] A feed pipe, which is arranged at one end of the repair gun barrel and is connected to the accommodating channel inside the repair gun barrel, and is used for the entry of ceramic welding repair material;
[0010] The gun head is arranged at the other end of the gun barrel, and has a conical discharge hole formed therein. The discharge hole is connected to the accommodating channel inside the gun barrel, and the cross-sectional area of the discharge hole at one end close to the gun barrel is larger than that at the end far from the gun barrel.
[0011] By adopting the above technical scheme, when ceramic repair welding is performed, the ceramic welding material enters the repair gun tube through the feed pipe, and then is sprayed at the repair position through the repair gun head. The repair gun head is set to reduce the diameter, so that the ceramic solder passing through this point is accelerated, so that it is sprayed onto the sprayed surface of the refractory material with a more concentrated speed, faster speed, greater pressure, and more solid welding, so that the quality of the weld body reaches the ideal effect, thereby reducing the occurrence of divergence of welding force and reducing the impact on the quality of ceramic welding.
[0012] Optionally, a connecting piece is further included, and the connecting piece is arranged at one end of the replenishing gun barrel away from the feeding pipe, and the discharge hole realizes a smooth transition with the storage channel in the replenishing gun barrel through the connecting piece.
[0013] By adopting the above technical solution and setting the connecting piece, a smooth transition between the repair gun head and the repair gun barrel accommodating channel is achieved, which reduces the obstruction of the ceramic welding material, allows the ceramic welding material to flow smoothly, and maintains the welding effect and welding quality.
[0014] Optionally, the connecting piece is a connecting straight pipe welded to the gun barrel, a connecting straight pipe is formed inside the connecting straight pipe, and the connecting hole is connected to the accommodating channel and is opened with the same diameter.
[0015] By adopting the above technical solution, the sealing connection of the connecting piece is achieved by welding the straight pipe and the supplementary gun pipe, and the installation is convenient.
[0016] Optionally, a sink groove connected to the connecting hole is formed at one end of the connecting straight tube away from the replenishing gun tube, and the replenishing gun head can be detachably connected to the sink groove and sunk into the sink groove.
[0017] By adopting the above technical solution, the repair gun head is sunk into the sinking groove, which reduces the impact of the external environment on the repair gun head. At the same time, the rotation of the repair gun head can be reduced and its stability can be improved.
[0018] Optionally, the gun head is threadedly connected to the sink.
[0019] By adopting the above technical solution and using a threaded connection method, the tightening degree of the gun head can be adjusted. At the same time, the connection is stable, not easy to disengage, easy to replace, quick to replace, and easy to install.
[0020] Optionally, a rotating groove for facilitating rotation is provided at the end of the repair gun head.
[0021] By adopting the above technical solution, when replacing the repair gun head, the rotary wrench is inserted into the rotary slot and rotated. The setting of the rotary slot facilitates the replacement of the repair gun head.
[0022] Optionally, a water cooling component is provided on the outer side of the gun barrel, and the water cooling component includes:
[0023] A water cooling main pipe is sleeved on the gun supply pipe and forms a water cooling cavity between the main pipe and the gun supply pipe;
[0024] A water cooling inlet pipe is arranged on the water cooling main pipe, is connected with the water cooling cavity and is used for water replenishment;
[0025] The water cooling outlet pipe is arranged on the water cooling main pipe, is communicated with the water cooling cavity and is used for water drainage.
[0026] By adopting the above technical solution, when the ceramic welding gun is working, water is supplied to the water cooling chamber through the water cooling inlet pipe, and then drained through the water cooling outlet pipe, so that the ceramic welding gun can work normally, so as to ensure the normal operation of the equipment and protect the safety of the operator, and effectively reduce the heat generated by the ceramic welding gun during operation, thereby extending the service life of the equipment.
[0027] Optionally, the water cooling main pipe extends to the connecting piece.
[0028] By adopting the above technical solution, the water-cooling main pipe cools the entire welding gun, thereby improving the durability of the overall equipment and extending its service life.
[0029] Optionally, a stop block is provided on the repair gun head, a first slide groove is opened on the connecting hole, the first slide groove is opened along the length direction of the connecting straight tube, a stop groove connected with the first slide groove is opened in the connecting hole, the stop groove is opened along the circumference of the connecting hole, and the end away from the first slide groove approaches the repair gun barrel.
[0030] By adopting the above technical solution, when replacing the repair gun head, first rotate the repair gun head so that the stop block slides along the stop groove into the first slide groove, and then pull the repair gun head outward, so that the repair gun head drives the stop block to slide out along the first slide groove, and then insert the new repair gun head into the sink groove, the stop block slides along the first slide groove into the stop groove, and then rotate the repair gun head so that the stop block presses against the stop groove to complete the replacement of the repair gun head; the above connection method has a simple structure, is easy to operate, and shortens the replacement time, can reduce damage to the thread, and can reduce the loosening of the thread caused by temperature increase.
[0031] Optionally, a locking bolt is threadedly connected to the connecting straight pipe, and the locking bolt abuts against the repair gun head and limits its rotation.
[0032] By adopting the above technical solution and setting the locking bolt, the connection stability of the repair gun head is further improved, which can effectively reduce the leakage of ceramic welding materials, improve safety, and enable the welding work to be carried out in an orderly manner.
[0033] In summary, this application includes the following beneficial technical effects:
[0034] 1. When performing ceramic repair welding, the ceramic welding material enters the repair gun tube through the feed pipe, and then is sprayed at the repair position through the repair gun head. The repair gun head is set to reduce the diameter, so that the ceramic welding material passing through here is accelerated, so that it is sprayed onto the sprayed surface of the refractory material with more concentration, faster speed, greater pressure, and more solid welding, so that the quality of the weld body reaches the ideal effect, thereby reducing the divergence of the welding force and reducing the impact on the quality of ceramic welding;
[0035] 2. When the ceramic welding gun is working, water is supplied to the water cooling chamber through the water cooling inlet pipe, and then drained through the water cooling outlet pipe, so that the ceramic welding gun can work normally, to ensure the normal operation of the equipment and protect the safety of the operator, and effectively reduce the heat generated by the ceramic welding gun during operation, and extend the service life of the equipment;
[0036] 3. The setting of the locking bolt further improves the connection stability of the repair gun head, which can effectively reduce the leakage of ceramic welding materials, improve safety, and enable the welding work to proceed in an orderly manner. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] Figure 1 This is a schematic diagram of the structure of the gun barrel in Example 1 of the present application.
[0038] Figure 2 This is a schematic diagram of the structure of the gun head and the connecting piece in Example 1 of the present application.
[0039] Figure 3 This is a schematic diagram of the structure of the rotating tank in Example 1 of the present application.
[0040] Figure 4 This is a schematic diagram of the structure of the stop groove in Example 2 of the present application.
[0041] Attached figures: 100, gun barrel; 110, accommodating channel; 200, feed pipe; 300, gun head; 310, discharge hole; 320, rotating groove; 400, connecting piece; 410, connecting hole; 420, sinking groove; 430, first slide groove; 440, stop groove; 500, water-cooling assembly; 510, water-cooling main pipe; 511, water-cooling chamber; 520, water-cooling inlet pipe; 530, water-cooling outlet pipe; 600, locking bolt; 700, stop block. DETAILED DESCRIPTION
[0042] The following is combined with Figure 1-Figure 4This application is described in further detail.
[0043] The embodiment of the present application discloses a ceramic welding gun head.
[0044] Embodiment 1:
[0045] refer to Figure 1 and Figure 2 The ceramic welding gun head includes a gun barrel 100, a gun head 300 disposed at one end of the gun barrel 100, connected to the gun barrel 100 and used for gathering welding materials, a feed pipe 200 disposed at the other end of the gun barrel 100 and connected to the gun barrel 100, and a water cooling component 500 disposed outside the gun barrel 100. The gun barrel 100 has a straight accommodating channel 110, and the diameter of each part of the accommodating channel 110 is consistent, thereby improving the transportation stability of the solder. When performing ceramic welding, the ceramic welding material enters the accommodating channel 110 through the feed pipe 200, and then is coated on the welding position through the gun head 300.
[0046] refer to Figure 1 , Figure 2 and Figure 3 The end of the supplementary gun barrel 100 close to the supplementary gun head 300 is bent at a right angle, and the bend can be chamfered or smoothly transitioned according to needs; the accommodating channel 110 in the supplementary gun barrel 100 changes direction according to the bending of the supplementary gun barrel 100, and the feeding pipe 200 can be fixed to the straight pipe section of the supplementary gun barrel 100 by welding or threaded connection; the end of the supplementary gun barrel 100 away from the feeding pipe 200 is provided with a connecting piece 400, and the connecting piece 400 is a connecting straight pipe, which is welded and fixed to the supplementary gun barrel 100, and a connecting hole 410 is formed in the connecting straight pipe, and the aperture of the connecting hole 410 is consistent with the aperture of the accommodating channel 110 ; A sink 420 connected to the connecting hole 410 is provided at the end of the connecting straight tube away from the supplementary gun tube 100, and the sink 420 is a cylindrical groove. The supplementary gun head 300 can be detachably connected in the sink 420, and the supplementary gun head 300 is sunk into the sink 420. A conical discharge hole 310 is provided in the supplementary gun head 300, and the cross-section of the discharge hole 310 is truncated cone-shaped, and the diameter of the end of the supplementary gun head 300 away from the connecting straight tube gradually decreases, so that the cross-sectional area of the end of the supplementary gun head 300 away from the connecting straight tube is smaller than the cross-sectional area of the end close to the connecting straight tube, and the end of the supplementary gun head 300 with a larger cross-sectional area is consistent with the diameter of the connecting hole 410 to achieve a smooth transition.
[0047] An internal thread is formed on the inner wall of the sink 420, and an external thread is formed on the outer side of the repair gun head 300. The external thread of the repair gun head 300 is threadedly connected with the internal thread of the connecting straight pipe.
[0048] In order to facilitate the disassembly of the repair gun head 300 , a rotation groove 320 is formed at one end of the repair gun head 300 away from the repair gun barrel 100 , and the rotation groove 320 is a straight groove.
[0049] The water cooling assembly 500 includes a water cooling main pipe 510 which is sleeved on the outside of the replenishing gun barrel 100. The water cooling main pipe 510 is bent along the replenishing gun barrel 100 and extends to a connection straight pipe. A water cooling cavity 511 is formed between the water cooling main pipe 510 and the replenishing gun barrel 100. A water cooling inlet pipe 520 and a water cooling outlet pipe 530 are fixedly connected to the water cooling main pipe 510. Both the water cooling inlet pipe 520 and the water cooling outlet pipe 530 are connected to the water cooling cavity 511, and the water cooling inlet pipe 520 is used for water intake, and the water cooling outlet pipe 530 is used for water discharge.
[0050] In order to further improve the water cooling effect, one or more water cooling components 500 can be installed on the outside of the water cooling main pipe 510 to perform multiple water cooling and cooling, and the multiple water cooling components 500 can be interconnected for circulation cooling; in other embodiments, a ring pipe can also be coiled on the gun barrel 100 for cooling and cooling.
[0051] The implementation principle of Example 1 of the present application is: when performing ceramic repair welding, firstly, the repair gun head 300 is threadedly connected to the connecting straight pipe, and then the connecting straight pipe is welded to the repair gun barrel 100. Alternatively, the connecting straight pipe may be welded first and then the repair gun head 300 is installed, and then cold water is supplied to the water cooling inlet pipe 520, and then the cold water is discharged through the water cooling outlet pipe 530; the ceramic welding repair material enters the repair gun barrel 100 through the feed pipe 200, and then is sprayed at the repair position through the reducer on the repair gun head 300, and the repair gun head 300 is set to reduce the diameter so that the ceramic solder passing through here is accelerated, so that it is sprayed onto the sprayed surface of the refractory material and is more concentrated; the water cooling component 500 cools the repair gun barrel 100 to improve safety and extend service life.
[0052] Embodiment 2:
[0053] refer to Figure 4 The difference between this embodiment and embodiment 1 is that a first slide groove 430 is provided on the sink 420, and the first slide groove 430 is provided along the length direction of the connecting straight pipe and extends to the end away from the connecting straight pipe; a stopping groove 440 is provided on the inner wall of the sink 420, and the stopping groove 440 is provided in an arc shape and is located near the end of the connecting straight pipe, and one end of the stopping groove 440 is connected to the first slide groove 430, and the end of the stopping groove 440 away from the first slide groove 430 approaches the replenishing gun barrel 100, and a stopping block 700 is fixedly connected to the outer wall of the replenishing gun head 300, and the stopping block 700 can slide along the first slide groove 430, and can slide into the stopping groove 440 along the first slide groove 430, and as the stop block 700 slides along the stopping groove 440, the replenishing gun head 300 is pressed against the connecting straight pipe.
[0054] In order to enhance the stability of the repair gun head 300 , a locking bolt 600 is threadedly connected to the connecting straight pipe. The locking bolt 600 extends into the sink 420 to abut against the repair gun head 300 and limit the rotation of the repair gun head 300 , and the locking bolt 600 is located on the opposite side of the first slide groove 430 .
[0055] The implementation principle of Example 2 of the present application is as follows: when performing ceramic repair welding, first insert the stop block 700 of the repair gun head 300 into the first slide groove 430, then slide the repair gun head 300 so that the stop block 700 slides to the stop groove 440, and then rotate the repair gun head 300 so that the repair gun head 300 drives the stop block 700 to slide into the stop groove 440 until the repair gun head 300 is pressed against the bottom of the sink groove 420 of the connecting straight pipe, and then fix the repair gun head 300 with the locking bolt 600, and then weld the connecting straight pipe to the repair gun barrel 100. , you can also weld and connect the straight pipes first and then install the repair gun head 300, then supply cold water to the water cooling inlet pipe 520, and then discharge the cold water through the water cooling outlet pipe 530; the ceramic welding material enters the repair gun barrel 100 through the feed pipe 200, and then is sprayed at the repair position through the reducer on the repair gun head 300. The repair gun head 300 is set to reduce the diameter so that the ceramic solder passing through here is accelerated, so that it is sprayed onto the sprayed surface of the refractory material and is more concentrated; the water cooling component 500 cools the repair gun barrel 100 to improve safety and extend service life.
[0056] The above-mentioned related explanations and descriptions of the embodiments are for the convenience of ordinary technicians in the technical field to understand and apply the utility model. It is obvious that those familiar with the technology in the field can easily make various modifications to these contents and apply the general principles described here to other embodiments without creative work. Therefore, the utility model is not limited to the above-mentioned related explanations and descriptions of the embodiments. Improvements and modifications made by technicians in the field based on the disclosure of the utility model without departing from the scope of the utility model should be within the scope of protection of the utility model.
Claims
1. A ceramic welding gun head, It is characterized in that include: A gun barrel (100) is formed with a straight receiving passage (110) inside; A feed pipe (200) is arranged at one end of the repair gun barrel (100) and is connected to the accommodating channel (110) inside the repair gun barrel (100) and is used for the entry of ceramic welding repair material; The gun head (300) is arranged at the other end of the gun barrel (100), and has a conical discharge hole (310) formed therein, the discharge hole (310) is connected to the accommodating channel (110) inside the gun barrel (100), and the cross-sectional area of the discharge hole (310) at one end close to the gun barrel (100) is larger than that at the other end away from the gun barrel (100); It also includes a connecting piece (400), wherein the connecting piece (400) is arranged at one end of the replenishing gun barrel (100) away from the feeding pipe (200), and the discharge hole (310) is smoothly transitioned to the storage channel (110) in the replenishing gun barrel (100) through the connecting piece (400); The connecting piece (400) is a connecting straight pipe welded to the gun barrel (100), a connecting hole (410) is formed in the connecting straight pipe, and the connecting hole (410) is connected to the accommodating channel (110) and has the same diameter; A sink (420) connected to the connecting hole (410) is formed at one end of the connecting straight tube away from the gun-repairing tube (100), and the gun-repairing head (300) is detachably connected to the sink (420) and sunk into the sink (420).
2. The ceramic welding gun head according to claim 1, It is characterized in that The gun head (300) is threadedly connected to the sink (420).
3. The ceramic welding gun head according to claim 2, It is characterized in that The end of the gun head (300) is provided with a rotation groove (320) for easy rotation.
4. The ceramic welding gun head according to claim 1, It is characterized in that A water cooling assembly (500) is arranged outside the gun barrel (100), and the water cooling assembly (500) comprises: A water cooling main pipe (510) is sleeved on the supplementary gun pipe (100) and forms a water cooling chamber (511) between the main pipe and the supplementary gun pipe (100); A water cooling inlet pipe (520) is arranged on the water cooling main pipe (510), is connected to the water cooling chamber (511) and is used for water replenishment; The water cooling outlet pipe (530) is arranged on the water cooling main pipe (510), is connected with the water cooling chamber (511) and is used for water discharge.
5. The ceramic welding gun head according to claim 4, It is characterized in that The water cooling main pipe (510) extends to the connecting piece (400).
6. The ceramic welding gun tip according to claim 1, It is characterized in that A stop block (700) is provided on the repair gun head (300), a first slide groove (430) is provided on the connecting hole (410), the first slide groove (430) is provided along the length direction of the connecting straight tube, a stop groove (440) connected to the first slide groove (430) is provided in the connecting hole (410), the stop groove (440) is provided along the circumference of the connecting hole (410), and the end away from the first slide groove (430) approaches the repair gun barrel (100).
7. The ceramic welding gun tip according to claim 6, It is characterized in that A locking bolt (600) is threadedly connected to the connecting straight pipe, and the locking bolt (600) abuts against the repair gun head (300) and restricts its rotation.