Die for detecting ring stiffness of in-situ curing pipeline

By designing a mold for detecting solidified-in-situ pipelines, using a biaxial motor and a threaded rod to drive the extruded detection plate, combined with a magnesium alloy positioning thorn and position-adjusting structure, it solves the problem of fixation and troubleshooting of existing equipment when detecting solidified-in-situ pipelines. Adaptation issues, enabling robust ring stiffness detection.

CN221860126UActive Publication Date: 2024-10-18XIAMEN JIEHANG ENG TESTING TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323401771.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-13
Publication Date
2024-10-18
Estimated Expiration
2033-12-13

AI Technical Summary

Technical Problem

The existing pipe ring stiffness testing equipment is inconvenient to fix when testing in-situ cured pipes, and the up-and-down direction extrusion detection method is not suitable for underground pipes, resulting in limitations and shaking problems in the mold during use.

Method used

A mold is designed that includes a detection box, a control panel, a deformation sensor and a driving structure. The mutual movement of the extrusion detection plate is realized through a biaxial motor, a threaded rod and a movable block. Combined with a magnesium alloy positioning thorn and an adjustment structure, it can be stable Fixed above the pipe, and adapted to the pipe by squeezing the detection plate and pressure sensing plate for detection.

Benefits of technology

The mold can be firmly fixed on the in-situ cured pipeline and adapted to underground pipelines for ring stiffness testing, which improves the accuracy and convenience of testing and overcomes the instability and unsuitability problems of existing equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221860126U_ABST
    Figure CN221860126U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of in-situ curing pipeline detection, and discloses a mold for detecting the ring stiffness of an in-situ curing pipeline, which comprises a detection box, a control panel fixed on the front surface of the detection box, a deformation sensor fixed at the bottom of the detection box, and a driving structure arranged in the detection box, fixing grooves are formed in the left side and the right side of the bottom of the detection box, extrusion detection plates are slidably connected to the left side and the right side of the bottom of the detection box, and pressure sensing plates are embedded in the surfaces of the opposite sides of the extrusion detection plates; the mold has a positioning function, can adapt to a construction site of an in-situ curing pipeline, can stably fix the mold above the pipeline so as to facilitate subsequent detection work, can be matched with the actual condition of the in-situ curing pipeline, and can detect the two sides of the pipeline by extruding the two sides of the pipeline, so that the detection efficiency is greatly improved. Therefore, the worker can conveniently carry out subsequent detection work on the in-situ curing pipeline.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of in-situ cured pipeline detection, in particular to a mold used for detecting the ring stiffness of an in-situ cured pipeline. Background Art

[0002] In-situ pipe curing is a trenchless method for repairing underground pipes. It is widely used in the maintenance of urban underground pipe facilities. The basic principle is to place the resin-impregnated liner pipe into the original pipe by flipping or pulling, and cure the resin by heating (using ultraviolet light, hot water, hot steam) to form a pipe lining repair method. After the pipe is repaired, the staff needs to inspect and evaluate the pipe to ensure that its quality and performance meet the requirements. During the inspection, the ring stiffness of the pipe needs to be tested. The ring stiffness is an indicator of the pipe's ability to withstand external pressure loads. The larger the value, the stronger the pipe's ability to withstand external pressure loads.

[0003] After searching, the pipeline ring stiffness testing equipment, application number: CN201921736605.1, when performing ring stiffness testing on the pipeline, it is tested by squeezing in the up and down directions. However, when testing in-situ cured pipelines, most of the pipelines are buried underground, which makes it inconvenient for the mold to fix itself when testing in-situ cured pipelines. The mold itself is prone to shaking during testing, and the method of testing by squeezing in the up and down directions is not suitable for underground pipelines (there is soil under the pipeline), which makes the mold have certain limitations during use and is inconvenient to use. Utility Model Content

[0004] The utility model aims to provide a mold for detecting the ring stiffness of an in-situ cured pipeline, so as to solve the problems raised in the above background technology.

[0005] To achieve the above object, the utility model provides the following technical solution: a mold for detecting the ring stiffness of an in-situ cured pipeline, comprising a detection box, a control panel fixed on the front of the detection box, and a deformation sensor fixed on the bottom of the detection box, and also comprising:

[0006] A driving structure is arranged inside the detection box, and the left and right sides of the bottom of the detection box are provided with fixed grooves, the left and right sides of the bottom of the detection box are slidably connected with extrusion detection plates, and the surfaces of the extrusion detection plates facing each other are embedded with pressure sensing plates for direct contact with the surface of the in-situ cured pipe, the driving structure includes a double-axis motor fixed inside the detection box, a first threaded rod rotatably connected to the left and right sides of the detection box, a movable block threadedly connected to the surface of the first threaded rod, and a connecting plate fixed to the bottom of the movable block, one end of the first threaded rod is fixedly connected to the output shaft of the double-axis motor, and the thread directions of the surfaces of the first threaded rods on the left and right sides of the detection box are oppositely arranged, and the bottom of the connecting plate passes through the fixed groove and is fixedly connected to the top of the extrusion detection plate;

[0007] A fixed frame is fixed on the top of the detection box, and an adjustment structure is provided on the surface of the fixed frame. A movable plate is provided on the left and right sides of the top of the detection box, and a positioning thorn is fixed on the surface of one side of the movable plate. The adjustment structure includes a second threaded rod, a lifting plate, a knob and a connecting rod. The second threaded rod is rotatably connected to the top of the detection box, and the second threaded rod passes through the fixed frame and is rotatably connected to the fixed frame. The lifting plate is threadedly connected to the surface of the second threaded rod, and the knob is fixed on the top of the second threaded rod. The connecting rod is hinged at the front and rear of the left and right surfaces of the lifting plate, and the other end of the connecting rod is hinged to the surface of the movable plate, and the connecting rod is arranged obliquely as a whole.

[0008] Preferably, the inner walls of the detection box are provided with limit grooves on both sides, and the front and rear sides of the inner walls are provided with limit blocks slidably connected to the inner walls of the limit grooves.

[0009] Preferably, guide bars are fixed on the left and right sides of the front and rear sides of the top of the detection box, and guide grooves are opened on the surfaces of the guide bars. Guide blocks are fixed on the surfaces of the front and rear sides of the movable plate, and the guide blocks penetrate the guide grooves and are slidably connected to the inner walls of the guide grooves.

[0010] Preferably, the number of the positioning thorns is several, and the spacings between the positioning thorns are the same, and the material of the positioning thorns is magnesium alloy.

[0011] Compared with the prior art, the beneficial effects of the utility model are as follows:

[0012] The utility model has a positioning function. The mold can adapt to the construction site of the in-situ cured pipeline and can stably fix the mold itself above the pipeline to facilitate subsequent detection work. Moreover, the mold can be adapted to the actual situation of the in-situ cured pipeline and can be detected by squeezing both sides of the pipeline, so that the staff can perform subsequent detection work on the in-situ cured pipeline. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 It is a three-dimensional structural schematic diagram of the utility model;

[0014] Figure 2 It is a three-dimensional structural schematic diagram of another viewing angle of the utility model;

[0015] Figure 3 It is a cross-sectional view of the detection box in the utility model;

[0016] Figure 4 It is a three-dimensional schematic diagram of the fixing frame in the utility model;

[0017] Figure 5 For this utility model Figure 4 A partial enlarged view of point A in the middle.

[0018] In the figure: 1. detection box; 2. control panel; 3. deformation sensor; 4. driving structure; 41. dual-axis motor; 42. first threaded rod; 43. movable block; 44. connecting plate; 5. fixing groove; 6. extrusion detection plate; 7. pressure sensing plate; 8. fixing frame; 9. adjustment structure; 91. second threaded rod; 92. lifting plate; 93. knob; 94. connecting rod; 10. movable plate; 11. positioning thorn; 12. limit groove; 13. limit block; 14. guide strip; 15. guide groove; 16. guide block. DETAILED DESCRIPTION

[0019] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0020] See also Figure 1-5As shown, a mold for detecting the ring stiffness of an in-situ cured pipeline comprises a detection box 1, a control panel 2 is fixed on the front of the detection box 1, and a plurality of control buttons are arranged on the surface of the control panel 2, a deformation sensor 3 is installed in the middle of the bottom of the detection box 1, a driving structure 4 is arranged inside the detection box 1, and a fixing groove 5 is opened on the left and right sides of the bottom of the detection box 1, an extrusion detection plate 6 is slidably connected to the left and right sides of the bottom of the detection box 1, and a pressure sensing plate 7 is embedded on the surface of the extrusion detection plate 6 facing each other, the driving structure 4 comprises a double-axis motor 41 fixed inside the detection box 1, a first threaded rod 42 rotatably connected to the left and right sides of the detection box 1, a movable block 43 threadedly connected to the surface of the first threaded rod 42, and a connecting plate 44 fixed to the bottom of the movable block 43, one end of the first threaded rod 42 is fixedly connected to the output shaft of the double-axis motor 41, and the thread directions of the surfaces of the first threaded rod 42 on the left and right sides of the detection box 1 are opposite The bottom of the connecting plate 44 passes through the fixing groove 5 and is fixedly connected to the top of the extrusion detection plate 6. A fixing frame 8 is fixed to the top of the detection box 1. The fixing frame 8 is U-shaped as a whole, and slots are provided on the left and right sides of the fixing frame 8. A positioning structure 9 is provided on the surface of the fixing frame 8. A movable plate 10 is provided on the left and right sides of the top of the detection box 1, and a positioning thorn 11 is fixed on the surface of one side of the movable plate 10. The positioning structure 9 includes a second threaded rod 91, a lifting plate 92, a knob 93 and a connecting rod 94. The second threaded rod 91 is rotatably connected to the top of the detection box 1, and the second threaded rod 91 passes through the fixing frame 8 and is rotatably connected between the fixing frame 8. The lifting plate 92 is threadedly connected to the surface of the second threaded rod 91, and the knob 93 is fixed to the top of the second threaded rod 91. The connecting rod 94 is hinged at the front and rear of the left and right side surfaces of the lifting plate 92, and the other end of the connecting rod 94 is hinged to the surface of the movable plate 10, and the connecting rod 94 is tilted as a whole.

[0021] Limiting grooves 12 are provided on the left and right sides of the front and back sides of the inner wall of the detection box 1, and limiting blocks 13 are fixed on the front and back sides of the movable block 43, and one side of the limiting block 13 extends to the inside of the limiting groove 12 and is slidably connected to the inner wall of the limiting groove 12. When the mold is installed, the staff can turn on the dual-axis motor 41, so that the first threaded rods 42 on the left and right sides rotate synchronously, and the movable blocks 43 on the left and right sides move toward each other, so that the extrusion detection plates 6 on both sides below extrude the in-situ cured pipe, and then detect its ring stiffness. During the movement of the movable block 43, the limiting blocks 13 on both sides will guide the movable block 43, so that the movable block 43 can only move horizontally left and right.

[0022] Guide strips 14 are fixed to the left and right sides of the front and rear sides of the top of the detection box 1, and guide grooves 15 are provided on the surface of the guide strips 14. Guide blocks 16 are fixed to the surfaces of the front and rear sides of the movable plate 10, and the guide blocks 16 penetrate the guide grooves 15 and are slidably connected to the inner walls of the guide grooves 15. When the connecting rod 94 moves to move the movable plate 10, the guide blocks 16 on both sides can guide the movable plate 10, so that the movable plate 10 can only move horizontally left and right, which is convenient for the subsequent fixation of the mold.

[0023] There are several positioning spikes 11, and the spacing between the positioning spikes 11 is the same. The material of the positioning spikes 11 is magnesium alloy. When the movable plate 10 pushes the positioning spikes 11 out, the positioning spikes 11 made of magnesium alloy have high strength, so that they can be inserted into the soil on both sides. Moreover, the magnesium alloy material is light, which is convenient for the staff to move the mold.

[0024] Working principle: At the construction site, after the staff has carried out in-situ solidification treatment on the underground pipeline, the staff can take out the mold and place the mold above the repaired pipeline. At this time, the staff will place the mold flat and then turn the knob 93 on the top to move the movable plates 10 on both sides, and the positioning spikes 11 will be inserted into the soil on both sides to complete the fixation of the mold. When the fixation is completed, the staff can turn on the dual-axis motor 41 to make the extrusion detection plates 6 on both sides move toward each other to extrude the repaired pipeline. During the extrusion process, the pressure sensing plate 7 and the deformation sensor 3 transmit the detected data to the inside of the control panel 2, and then the staff reads the obtained data to analyze whether the ring stiffness of the repaired pipeline meets the standard, so as to complete the ring stiffness detection operation of the in-situ cured pipeline.

[0025] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A mold for detecting the ring stiffness of an in-situ cured pipeline, comprising a detection box (1), a control panel (2) fixed to the front of the detection box (1), and a deformation sensor (3) fixed to the bottom of the detection box (1), characterized in that: Also includes: A driving structure (4) is arranged inside the detection box (1), and the left and right sides of the bottom of the detection box (1) are provided with fixing grooves (5), the left and right sides of the bottom of the detection box (1) are slidably connected with extrusion detection plates (6), and the surfaces of the extrusion detection plates (6) facing each other are embedded with pressure sensing plates (7) for directly contacting the surface of the in-situ cured pipe. The driving structure (4) comprises a double-axis motor (41) fixed inside the detection box (1), a first threaded rod (42) rotatably connected to the left and right sides of the detection box (1), a movable block (43) threadedly connected to the surface of the first threaded rod (42), and a connecting plate (44) fixed to the bottom of the movable block (43), one end of the first threaded rod (42) is fixedly connected to the output shaft of the double-axis motor (41), and the threads of the surfaces of the first threaded rods (42) on the left and right sides of the detection box (1) are arranged in opposite directions, and the bottom of the connecting plate (44) passes through the fixing groove (5) and is fixedly connected to the top of the extrusion detection plate (6); A fixing frame (8) is fixed to the top of the detection box (1), and a positioning structure (9) is arranged on the surface of the fixing frame (8). A movable plate (10) is arranged on both the left and right sides of the top of the detection box (1), and a positioning spike (11) is fixed on the surface of one side of the movable plate (10). The positioning structure (9) comprises a second threaded rod (91), a lifting plate (92), a knob (93) and a connecting rod (94). The second threaded rod (91) is rotatably connected to the top of the detection box (1), and the second threaded rod (91) passes through the fixing frame (8) and is rotatably connected to the fixing frame (8). The lifting plate (92) is threadedly connected to the surface of the second threaded rod (91), and the knob (93) is fixed to the top of the second threaded rod (91). The connecting rod (94) is hinged to the front and rear sides of the left and right side surfaces of the lifting plate (92), and the other end of the connecting rod (94) is hinged to the surface of the movable plate (10). The connecting rod (94) is arranged in an inclined manner as a whole.

2. A mold for detecting the ring stiffness of an in-situ cured pipeline according to claim 1, characterized in that: Limiting grooves (12) are provided on both the left and right sides of the front and rear sides of the inner wall of the detection box (1), and limiting blocks (13) slidably connected to the inner wall of the limiting grooves (12) are fixed on both the front and rear sides of the movable block (43).

3. A mold for detecting the ring stiffness of an in-situ cured pipeline according to claim 1, characterized in that: Guide bars (14) are fixed on the left and right sides of both front and rear sides of the top of the detection box (1), and guide grooves (15) are provided on the surface of the guide bars (14). Guide blocks (16) are fixed on the surfaces of both front and rear sides of the movable plate (10), and the guide blocks (16) penetrate the guide grooves (15) and are slidably connected to the inner wall of the guide grooves (15).

4. A mold for detecting the ring stiffness of an in-situ cured pipeline according to claim 1, characterized in that: The number of the positioning thorns (11) is several, and the spacings between the positioning thorns (11) are the same; the material of the positioning thorns (11) is magnesium alloy.