Testing device for accelerating corrosion of steel bar structure

By adopting wet and dry cycle corrosion and drying technology in the steel corrosion test device, the problems of single corrosion environment and slow speed in the existing technology are solved, and the efficiency and intuitiveness of the corrosion test are significantly improved.

CN221860234UActive Publication Date: 2024-10-18XIAMEN UNIV OF TECH
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202420268960.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-04
Publication Date
2024-10-18
Estimated Expiration
2034-02-04

AI Technical Summary

Technical Problem

The corrosion environment in the existing steel bar corrosion test is single, resulting in slow corrosion speed, low efficiency, and difficulty in visually judging the corrosion situation.

Method used

Design a test device for accelerated corrosion of steel bar structures. By setting up steel bar clamping components and rotating mechanisms in the test chamber, the wet and dry cycle corrosion test of steel bars is realized. A dryer is used to accelerate the drying process of steel bars, combined with the use of corrosive liquid. function to achieve intermittent reciprocating turning and comprehensive drying of steel bars.

Benefits of technology

It effectively accelerates the efficiency of steel bar corrosion tests, makes corrosion more intuitive through wet and dry cycle corrosion, and significantly improves the speed and efficiency of corrosion tests.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221860234U_ABST
    Figure CN221860234U_ABST
Patent Text Reader

Abstract

The utility model discloses a test device for accelerating corrosion of a reinforcing steel bar structure, which comprises a test box, reinforcing steel bar clamping components, a first rotating mechanism, a dryer and a second rotating mechanism, the two reinforcing steel bar clamping components are respectively arranged in a drying area and a test pool, and are both arranged on a rotating shaft; the first motor drives the rotating shaft to rotate to turn over the two reinforcing steel bar clamping assemblies up and down; a dryer is arranged in the drying area, and the first rotating mechanism drives the dryer to horizontally rotate around the steel bar clamping assembly. The first motor drives the rotating shaft 3 to rotate to discontinuously move the steel bars out of or into the test pool, and the dryer is combined to dry the steel bars, so that the dry-wet circulating corrosion test on the steel bars is facilitated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of steel bar corrosion testing devices, in particular to a testing device for accelerating the corrosion of steel bar structures. Background Art

[0002] Rebar refers to steel used for reinforced concrete and prestressed reinforced concrete, with a circular cross section, sometimes a square with rounded corners. It includes plain round bars, ribbed bars, and twisted bars. Plain round bars are actually small round bars and coils of ordinary low-carbon steel. Deformed bars are ribbed bars on the surface, usually with two longitudinal ribs and evenly distributed transverse ribs along the length. In order to ensure the service life of the steel bars, it is often necessary to conduct corrosion tests on the steel bars;

[0003] When the steel bar is undergoing a corrosion test, the steel bar is generally placed in a test pool filled with a corrosive liquid, and then the steel bar is wet-corroded by the corrosive liquid to observe the corrosion of the steel bar. However, if the corrosion is only tested by the corrosion of the steel bar by the corrosive liquid, the corrosion environment is only carried out in the corrosive liquid and the corrosion environment is relatively simple. Therefore, the reference for judging corrosion is poor, and the steel bar is corroded slowly, which will also affect the efficiency of the steel bar corrosion test. Utility Model Content

[0004] In view of the deficiencies of the prior art, the utility model provides a test device for accelerating the corrosion of a steel bar structure, which effectively accelerates the efficiency of the steel bar corrosion test by repeatedly corroding and drying the steel bars.

[0005] In order to achieve the above object, the utility model is realized by the following technical solutions:

[0006] A test device for accelerating corrosion of a steel bar structure comprises a test box, a steel bar clamping assembly, a first rotating mechanism, a dryer, and a second rotating mechanism. The lower part of the test box is a test pool for containing a corrosive liquid, and the upper part of the test box is a drying area, which is connected to the test pool.

[0007] The first rotating mechanism includes a rotating shaft and a first motor connected to the rotating shaft, the rotating shaft is horizontally arranged in the test box, a steel bar clamping assembly is respectively arranged in the drying area and the test pool, and the two steel bar clamping assemblies are both mounted on the rotating shaft, and the first motor drives the rotating shaft to rotate so as to flip the two steel bar clamping assemblies up and down;

[0008] A dryer is provided in the drying area and is located at one side of the steel bar clamping assembly. The first rotating mechanism drives the dryer to rotate horizontally around the steel bar clamping assembly.

[0009] Furthermore, the steel bar clamping assembly includes a support rod, one side of the support rod is connected to a mesh bag and a mesh sleeve, the synchronization rod is located on the other side of the support rod, the mesh bag and the mesh sleeve are provided with a splint, the side of the synchronization rod close to the support rod is connected to two pressure rods passing through the support rod, the splint is fixedly connected to the synchronization rod through the pressure rod, the synchronization rod is provided with a threaded hole, the threaded locking rod passes through the threaded hole on the synchronization rod and is connected to the support rod.

[0010] Furthermore, the mesh pocket is located at one end of the support rod close to the rotating shaft, and the mesh pocket corresponds to the mesh sleeve in upper and lower parts and has the same inner diameter.

[0011] Furthermore, the second rotating mechanism includes a second motor, a drive shaft, and an L-shaped fixed rod, the lower end of the vertical section of the L-shaped fixed rod is connected to the dryer, the upper end of the vertical section of the L-shaped fixed rod is connected to one end of the horizontal section, the other end of the horizontal section is connected to a vertically arranged drive shaft, and one end of the drive shaft extends out of the top surface of the test box and is connected to the output shaft of the second motor.

[0012] Furthermore, an exhaust pipe is provided on one side of the upper end of the test box, and an air filter is installed in the exhaust pipe.

[0013] Furthermore, a drain valve connected to the test pool is installed on one side of the lower end of the test pool.

[0014] Furthermore, an opening is provided at the upper front portion of the test box, and a box door is provided at the opening.

[0015] The utility model has the following beneficial effects:

[0016] 1. Two steel bar clamping assemblies are set up, one of which is inserted into the corrosive liquid in the test tank, and the other is close to the dryer. Then the motor drives the steel bars in the two steel bar clamping assemblies to turn back and forth intermittently, so as to facilitate the dry-wet cycle corrosion test of the steel bars. Compared with the prior art that only conducts wet corrosion test, the dry-wet cycle corrosion test is more intuitive for the corrosion of steel bars.

[0017] 2. The steel bars are dried by the dryer. The dryer dries the steel bars comprehensively, which is beneficial to improve the drying speed of the steel bars. Since the steel bars are dried quickly, the speed of the dry-wet cycle corrosion test is also improved, thereby effectively accelerating the efficiency of the steel bar corrosion test. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a schematic diagram of the overall structure of the test device for accelerating corrosion of steel bar structure of the utility model;

[0019] Figure 2 This is a schematic diagram of the structure of the steel bar clamping assembly of the utility model;

[0020] Figure 3 It is the working state after the steel bars are loaded into the test device for accelerated corrosion of steel bar structure;

[0021] Figure 4 It is a front view of the test device for accelerating corrosion of steel bar structure of the utility model.

[0022] Explanation of the numbers: 1. Test chamber; 2. Test pool; 3. Rotating shaft; 4. First motor; 5. Support rod; 6. Mesh bag; 7. Mesh sleeve; 8. Synchronous rod; 9. Threaded locking rod; 10. Pressure rod; 11. Clamp; 12. Second motor; 13. Drive shaft; 14. L-shaped fixing rod; 15. Dryer; 16. Exhaust pipe; 17. Air filter element; 18. Box door; 19. Drain valve. DETAILED DESCRIPTION

[0023] The utility model is further described below in conjunction with the accompanying drawings and embodiments.

[0024] In the description of the present invention, it should be understood that the terms "upper", "lower", "front", "back", "left", "right", "top", "bottom", "inside", "outside", etc., indicating directions or positional relationships, are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore should not be understood as a limitation on the present invention.

[0025] like Figures 1 to 4 As shown, this embodiment discloses a test device for accelerating corrosion of a steel bar structure, comprising a test box 1, a steel bar clamping assembly, a first rotating mechanism, a dryer 15, and a second rotating mechanism. The lower part of the test box 1 is a test pool 2 for containing a corrosive liquid, and the upper part of the test box 1 is a drying area, which is connected to the test pool 2; the first rotating mechanism comprises a rotating shaft 3 and a first motor 4 connected to the rotating shaft 3, the rotating shaft 3 is transversely arranged in the test box 1, a steel bar clamping assembly is respectively arranged in the drying area and the test pool 2, and the two steel bar clamping assemblies are both installed on the rotating shaft 3, and the first motor 4 drives the rotating shaft 3 to rotate to flip the two steel bar clamping assemblies up and down; a dryer 15 is arranged in the drying area, and the dryer 15 is located on one side of the steel bar clamping assembly, and the first rotating mechanism drives the dryer 15 to rotate horizontally around the steel bar clamping assembly.

[0026] The steel bar clamping assembly includes a support rod 5, one side of the support rod 5 is connected to a mesh bag 6 and a mesh sleeve 7, a synchronization rod 8 is located on the other side of the support rod 5, a clamping plate 11 is provided in the mesh bag 6 and the mesh sleeve 7, and the synchronization rod 8 is connected to two pressure rods 10 passing through the support rod 5 on the side close to the support rod 5, the clamping plate 11 is fixedly connected to the synchronization rod 8 through the pressure rod 10, and a threaded hole is provided on the synchronization rod 8, and a threaded locking rod 9 passes through the threaded hole on the synchronization rod 8 and is connected to the support rod 5.

[0027] In the figure, the pressure rod 10 is fixed to the left side of the splint 11, and the pressure rod 10 passes through the support rod 5 to the left, the synchronization rod 8 is arranged on the left side of the support rod 5, the left end of the pressure rod 10 is fixed to the synchronization rod 8, the threaded locking rod 9 is rotatably connected to the left side of the support rod 5, and the threaded locking rod 9 passes through the synchronization rod 8 to the left, and the mesh pocket 6 corresponds to the mesh sleeve 7 up and down and has the same inner diameter.

[0028] The front upper part of the test box 1 is provided with an opening, and a box door 18 is provided at the opening. The mesh bag 6 corresponds to the mesh sleeve 7 in the upper and lower parts and has the same inner diameter. The mesh bag 6 is located at the end of the support rod 5 close to the rotating shaft 3, so that the steel bar can be passed through the mesh sleeve 7 at the opening of the test box 1 and held by the mesh bag 6, and then the pressure plate can be adjusted to clamp the steel bar. By opening the box door 18, new corrosive liquid can be easily added to the test pool 2, and it is convenient to replace the steel bar to be tested.

[0029] The second rotating mechanism includes a second motor 12, a driving shaft 13, and an L-shaped fixing rod 14. The lower end of the vertical section of the L-shaped fixing rod 14 is connected to the dryer 15, the upper end of the vertical section of the L-shaped fixing rod 14 is connected to one end of the horizontal section, and the other end of the horizontal section is connected to the vertically arranged driving shaft 13. One end of the driving shaft 13 extends out of the top surface of the test box 1 and is connected to the output shaft of the second first motor 4.

[0030] When the corrosion test of the steel bars is carried out by the test device, the steel bars are inserted into the mesh sleeve 7 and the mesh pocket 6, and then the threaded locking rod 9 is turned to drive the synchronization rod 8, the pressure rod 10 and the clamping plate 11 to move right until the clamping plate 11 clamps the steel bars in the mesh sleeve 7 and the mesh pocket 6. Therefore, after the steel bars are clamped and fixed by the steel bar clamping assembly, one of the steel bars extends into the corrosive liquid in the test tank 2, and the other steel bar is close to the dryer 15. Then, the rotating shaft 3 is driven to rotate by the operation of the first motor 4, and at the same time, the rotating shaft 3 drives the steel bar clamping assembly and the steel bars to rotate together.

[0031] When the steel bars move to the upper position in the test box 1, the dryer 15 is started to dry the steel bars. At the same time, the second motor 12 is driven to drive the drive shaft 13, the L-shaped fixing rod 14 and the dryer 15 to rotate together. Therefore, the dryer 15 will perform comprehensive drying treatment around the outer periphery of the steel bars, which is beneficial to improve the drying speed of the steel bars. Since the steel bar drying speed is fast, the speed of the dry-wet cycle corrosion test is also improved, thereby effectively accelerating the efficiency of the steel bar corrosion test.

[0032] In summary, the first motor 4 drives the steel bars at the upper and lower ends of the rotating shaft 3 to intermittently flip back and forth, and the steel bars will intermittently move out of or enter the test pool 2, so the corrosion environment will be constantly changed. The steel bars are dried in combination with the dryer 15, which is conducive to the dry-wet cycle corrosion test of the steel bars. Compared with the prior art that only conducts wet corrosion tests, the dry-wet cycle corrosion test is more intuitive for the corrosion of the steel bars.

[0033] An exhaust pipe 16 is provided on one side of the upper end of the test box 1, and an air filter 17 is installed in the exhaust pipe 16. When odorous gas is generated during the corrosion test, the odorous gas will be discharged through the exhaust pipe 16. During this process, the air filter 17 in the exhaust pipe 16 will filter the odorous gas, thereby making the gas discharge more environmentally friendly.

[0034] A drain valve 19 connected to the test pool 2 is installed at one side of the lower end of the test pool 2. When the corrosive liquid needs to be discharged, the drain valve 19 can be opened to conveniently discharge the waste corrosive liquid.

[0035] As described above, the embodiments are only used to illustrate the technical solutions of the utility model, rather than to limit it. Although the utility model has been described in detail with reference to the aforementioned embodiments, ordinary technicians in the field should understand that they can still modify the technical solutions recorded in the aforementioned embodiments, or replace some of the technical features therein with equivalents. These modifications or replacements do not make the corresponding technical solutions deviate from the spirit and scope of the technical solutions of the embodiments of the utility model. Therefore, all other embodiments obtained by ordinary technicians in the field without making creative work belong to the protection scope of the utility model.

Claims

1. A test device for accelerating corrosion of steel bar structures, characterized in that: It includes a test box, a steel bar clamping assembly, a first rotating mechanism, a dryer, and a second rotating mechanism. The lower part of the test box is a test pool for containing corrosive liquid, and the upper part of the test box is a drying area, which is connected to the test pool. The first rotating mechanism includes a rotating shaft and a first motor connected to the rotating shaft, the rotating shaft is horizontally arranged in the test box, a steel bar clamping assembly is respectively arranged in the drying area and the test pool, and the two steel bar clamping assemblies are both mounted on the rotating shaft, and the first motor drives the rotating shaft to rotate so as to flip the two steel bar clamping assemblies up and down; A dryer is provided in the drying area and is located at one side of the steel bar clamping assembly. The first rotating mechanism drives the dryer to rotate horizontally around the steel bar clamping assembly.

2. The test device for accelerated corrosion of steel bar structure according to claim 1, characterized in that: The steel bar clamping assembly includes a support rod, one side of the support rod is connected to a mesh bag and a mesh sleeve, a synchronization rod is located on the other side of the support rod, a clamping plate is provided in the mesh bag and the mesh sleeve, and the side of the synchronization rod close to the support rod is connected to two pressure rods passing through the support rod, the clamping plate is fixedly connected to the synchronization rod through the pressure rod, a threaded hole is provided on the synchronization rod, and a threaded locking rod passes through the threaded hole on the synchronization rod and is connected to the support rod.

3. The test device for accelerating corrosion of steel bar structure according to claim 2, characterized in that: The mesh pocket is located at one end of the support rod close to the rotating shaft, and the mesh pocket corresponds to the mesh sleeve up and down and has the same inner diameter.

4. The test device for accelerating corrosion of steel bar structure according to claim 1, characterized in that: The second rotating mechanism includes a second motor, a drive shaft, and an L-shaped fixed rod. The lower end of the vertical section of the L-shaped fixed rod is connected to the dryer, the upper end of the vertical section of the L-shaped fixed rod is connected to one end of the horizontal section, and the other end of the horizontal section is connected to a vertically arranged drive shaft. One end of the drive shaft extends out of the top surface of the test box and is connected to the output shaft of the second motor.

5. The test device for accelerating corrosion of steel bar structure according to claim 1, characterized in that: An exhaust pipe is arranged on one side of the upper end of the test box, and an air filter element is installed in the exhaust pipe.

6. The test device for accelerating corrosion of steel bar structure according to claim 1, characterized in that: A drain valve connected to the test pool is installed on one side of the lower end of the test pool.

7. The test device for accelerating corrosion of steel bar structure according to claim 1, characterized in that: An opening is arranged at the upper front part of the test box, and a box door is arranged at the opening.

Citation Information

Cited By

  • Device and method for testing corrosion resistance of pavement steel for bridge and method for evaluating corrosion resistance

    CN120404549A