UV attenuation testing device
By designing a UV attenuation test device and using a ring structure and copper foil fixings, the problem of easy damage and corrosion of battery cells during UV testing was solved, faster and more accurate test results were achieved, and the effects of oxidation and water vapor were reduced.
Patent Information
- Application Number
- CN202420449575.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-07
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2034-03-07
AI Technical Summary
In traditional cell UV attenuation tests, cells are easily scratched, damaged by oxidation under long-term high temperatures, and water vapor corrosion and dirt are difficult to solve.
Design a UV attenuation test device, including a front panel, a back panel, a packaging strip and a fixing piece. The battery piece is between the packaging film and the back panel. The packaging strip forms a ring structure. The fixing piece is copper foil. The test is performed in a nitrogen environment. It is carried out in medium to reduce the influence of oxidation and water vapor.
It improves the test speed and accuracy, reduces the wear and tear of battery cells, reduces oxidation and water mist corrosion, and protects the battery cells.
Smart Images

Figure CN221900844U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of photovoltaics, in particular to a UV attenuation testing device. Background Art
[0002] In the photovoltaic field, in the UV attenuation test of solar cells, the attenuation of solar cells under different film packaging is different. When the solar cells are packaged at the module end, a specific film is used. When the module is used for testing, the time and cycle are long. Using the cell test can speed up the test cycle. In traditional technology, when the cell is used for UV attenuation testing, the cell is directly encapsulated in two glass plates. The cell is directly sandwiched between the glass plates, which can easily cause scratches on the back glass of the cell. The cell is easily oxidized and damaged under long-term high temperature. In addition, water vapor is easy to corrode and dirty the surface of the cell during testing, or it is easy to get dirty during the process of taking the cell. Utility Model Content
[0003] Based on this, it is necessary to provide a UV attenuation testing device. When the UV attenuation testing device of the utility model is used for UV attenuation testing of solar cells and packaging films, the testing speed is fast and the testing results are more accurate.
[0004] An embodiment of the present application provides a UV attenuation testing device.
[0005] A UV attenuation test device comprises a front panel, a back panel, a packaging strip, a packaging film and a fixing part, wherein the packaging film is laminated and connected to one surface of the front panel, the packaging strip is arranged between the packaging film and the back panel to form a ring structure, the battery cell to be tested is used to be packaged between the packaging film and the back panel and is located in the ring structure formed by the packaging strip, and the fixing part fixes the front panel and the back panel.
[0006] In some embodiments, there is a gap between the inner edge of the packaging strip and the battery cell to be tested.
[0007] In some embodiments, the spacing distance between the inner edge of the packaging strip and the battery cell to be tested is 3 mm to 5 mm.
[0008] In some embodiments, the front panel is a glass panel;
[0009] And / or, the back panel is a glass panel or a PET panel.
[0010] In some embodiments, the front panel and the back panel are respectively in a square shape;
[0011] The side lengths of the front panel and the back panel are 200 mm to 400 mm respectively.
[0012] In some embodiments, the thickness of the front panel is 0.2 mm to 5 mm;
[0013] And / or, the thickness of the back panel is 0.2 mm~5 mm.
[0014] In some embodiments, the packaging strip is in the shape of a long strip, and the width of the packaging strip is 50 mm to 100 mm.
[0015] In some embodiments, the packaging strip has a thickness of 0.1 mm to 1 mm.
[0016] In some embodiments, the fixing member is in a U-shaped structure, and the fixing member is clamped on at least a portion of the edges of the front panel and the back panel.
[0017] In some embodiments, the fixing member is a copper foil.
[0018] The UV attenuation test device of the utility model has a fast test speed when used for UV attenuation test of solar cells and packaging films. After the test, it is easier to separate the cells from the packaging materials such as packaging films and packaging strips used for auxiliary tests, reduce the wear of the cells, and make the test results more accurate. After the test sample is placed in a nitrogen environment, the oxygen content is reduced, the oxidation effect of air on the grid lines of the cells at high temperatures is reduced, and the corrosion of the cells by water mist is reduced. In addition, the use of copper foil edge sealing in one embodiment of the present application also reduces the influence of water vapor condensed by air on the cells in the test sample during the test. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present application, and those skilled in the art can obtain other drawings based on these drawings without creative work.
[0020] In order to more completely understand the present application and its beneficial effects, the following description will be given in conjunction with the accompanying drawings. In the following description, the same reference numerals represent the same parts.
[0021] FIG1 is a schematic side view of a UV attenuation testing device according to an embodiment of the present invention;
[0022] FIG. 2 is a front schematic diagram of a UV attenuation testing device according to an embodiment of the present invention.
[0023] Description of Reference Numerals
[0024] 10. UV attenuation test device; 100. front panel; 200. back panel; 300. packaging strip; 400. packaging film; 500. fixing part; 20. battery cell. DETAILED DESCRIPTION
[0025] In order to make the above-mentioned purposes, features and advantages of the utility model more obvious and easy to understand, the specific implementation methods of the utility model are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the utility model. However, the utility model can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the utility model, so the utility model is not limited by the specific embodiments disclosed below.
[0026] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.
[0027] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0028] In the present utility model, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.
[0029] In the description of the present utility model, "several" means more than one, "many" means more than two, "greater than", "less than", "exceed" etc. are understood to exclude the number itself, and "above", "below", "within" etc. are understood to include the number itself. If there is a description of "first" or "second", it is only used to distinguish the technical features, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features or implicitly indicating the order of the indicated technical features.
[0030] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art in the technical field of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.
[0031] The embodiment of the present application provides a UV attenuation test device 10 to solve the problem that when a cell is subjected to a UV attenuation test in the conventional technology, the cell is easily scratched, the cell is easily oxidized and damaged under long-term high temperature, and the cell surface is easily corroded and contaminated by water vapor during the test, or the cell surface is easily dirty during the process of removing the cell. The UV attenuation test device 10 will be described below in conjunction with the accompanying drawings.
[0032] The UV attenuation test device 10 provided in the embodiment of the present application is exemplified in FIG1 , which is a schematic diagram of the structure of the UV attenuation test device 10 provided in the embodiment of the present application. The UV attenuation test device 10 of the present application can be used for UV attenuation testing of solar cells and packaging films 400.
[0033] In order to more clearly illustrate the structure of the UV attenuation testing device 10 , the UV attenuation testing device 10 will be introduced below with reference to the accompanying drawings.
[0034] Exemplarily, referring to FIG. 1 , a UV attenuation testing device 10 includes a front panel 100 , a back panel 200 , a packaging strip 300 , a packaging film 400 , and a fixing member 500 .
[0035] The packaging film 400 is laminated and connected to one surface of the front panel 100. The packaging strip 300 is arranged between the packaging film 400 and the back panel 200 to form a ring structure. The battery cell 20 to be tested is used to be packaged between the packaging film 400 and the back panel 200 and is located in the ring structure surrounded by the packaging strip 300. The fixing member 500 fixes the front panel 100 and the back panel 200.
[0036] When the UV attenuation test device 10 of the utility model is used for the UV attenuation test of solar cells, the test speed is fast, and it is easier to separate the cell 20 and the packaging materials for auxiliary testing such as the packaging film 400 and the packaging strip 300 after the test, thereby reducing the wear of the cell 20 and making the test result more accurate. After the test sample is placed in a nitrogen environment, the oxygen content is reduced, the oxidation effect of the air on the grid line of the cell 20 at high temperature is reduced, and the corrosion of the cell 20 by water mist is reduced.
[0037] In some embodiments, as shown in FIG. 2 , there is a gap between the inner edge of the packaging strip 300 and the battery cell 20 to be tested.
[0038] In some embodiments, the distance between the inner edge of the packaging strip 300 and the battery cell 20 to be tested is 3 mm to 5 mm.
[0039] In some embodiments, the front panel 100 is a glass plate.
[0040] In some embodiments, the back panel 200 is a glass panel or a PET panel.
[0041] In some embodiments, the front panel 100 and the back panel 200 are respectively in a square shape. The front panel 100 and the back panel 200 have the same size. The side lengths of the front panel 100 and the back panel 200 are 200 mm to 400 mm, respectively. For example, in one specific example, the side lengths of the front panel 100 and the back panel 200 are 200 mm, respectively. In another specific example, the side lengths of the front panel 100 and the back panel 200 are 400 mm, respectively. It is not difficult to understand that in other specific examples, the side lengths of the front panel 100 and the back panel 200 can also be 250 mm, 300 mm, 350 mm or other parameters, respectively.
[0042] In some embodiments, the thickness of the front panel 100 is 0.2 mm to 5 mm. For example, in one specific example, the thickness of the front panel 100 is 0.2 mm. In another specific example, the thickness of the front panel 100 is 5 mm. It is not difficult to understand that in other specific examples, the thickness of the front panel 100 can also be 1 mm, 2 mm, 3 mm, 4 mm or other parameters.
[0043] In some embodiments, the thickness of the back panel 200 is 0.2 mm to 5 mm. For example, in one specific example, the thickness of the back panel 200 is 0.2 mm. In another specific example, the thickness of the back panel 200 is 5 mm. It is not difficult to understand that in other specific examples, the thickness of the back panel 200 can also be 1 mm, 2 mm, 3 mm, 4 mm or other parameters.
[0044] In some embodiments, the packaging strip 300 is in the shape of a long strip, and the width of the packaging strip 300 is 50 mm to 100 mm. Preferably, the width of the packaging strip is 1 cm.
[0045] In some embodiments, the thickness of the packaging strip 300 is 0.1 mm to 1 mm. For example, in one specific example, the thickness of the packaging strip 300 is 0.1 mm. In another specific example, the thickness of the packaging strip 300 is 1 mm. It is not difficult to understand that in other specific examples, the thickness of the packaging strip 300 can also be 0.2 mm, 0.3 mm, 0.4 mm, 0.5 mm, 0.6 mm, 0.7 mm, 0.8 mm, 0.9 mm or other parameters.
[0046] In some embodiments, the fixing member 500 is in a U-shaped structure, and the fixing member 500 is clamped on at least part of the edges of the front panel 100 and the back panel 200. During the test, the fixing member 500 first fixes three edges of the front panel 100 and the back panel 200, and then fixes the remaining edge after being protected by inert gas.
[0047] In some embodiments, the fixing member 500 is a copper foil. The present application uses the copper foil as the fixing member 500 for edge sealing to reduce the influence of the water vapor condensed by the air on the battery cell 20 in the test sample during the test.
[0048] When the UV attenuation test device 10 of the utility model is used for the UV attenuation test of the battery cell 20, the steps include:
[0049] (1) Testing the initial electrical performance data of the battery cell 20.
[0050] (2) The front panel 100 and the packaging film 400 to be tested are laminated together using a photovoltaic module laminator.
[0051] (3) Place the packaging strip 300 on the back panel 200 to form a ring structure and fix it with tape. No lamination is required between the packaging strip 300 and the back panel 200.
[0052] (4) Place the battery cell 20 to be tested in the annular structure of the packaging strip 300 so that the gap between the inner wall of the annular structure and the battery cell 20 is 3-5 mm.
[0053] (5) Stack the front panel 100, the packaging film 400 to be tested, the battery cell 20, the packaging strip 300, and the back panel 200 together.
[0054] (6) Fix three edges of the front panel 100 and the back panel 200 with copper foil.
[0055] (7) Place the intermediate from step (6) horizontally in a nitrogen cabinet for 1 hour.
[0056] (8) The remaining edge of the intermediate in step (7) is fixed with copper foil to form a UV testable sample, and a UV test is performed on the UV testable sample.
[0057] (9) After side viewing, the edge copper foil of the UV testable sample is cut open, and the battery cell 20 is taken out to test the electrical performance data of the battery cell 20 after the UV attenuation experiment.
[0058] (10) The difference in electrical performance of the battery cell 20 before and after the experiment is calculated to obtain the corresponding attenuation rate of the battery cell 20 under the packaging film 400.
[0059] In summary, the UV attenuation testing device 10 of the present application has the following beneficial effects compared with the conventional technology:
[0060] (1) The packaging film 400 and the packaging strip 300 in the present application are easily separated from the battery cell 20. There is a gap between the packaging strip 300 and the battery cell 20, and there is no packaging film 400 between the back side of the battery cell 20 and the back panel 200. Therefore, the battery cell 20 can be easily separated after testing without causing damage to the battery cell 20.
[0061] (2) Compared with the component testing in the traditional technology, the battery cell 20 of the present application has a faster testing speed.
[0062] (3) Adding the packaging strip 300 can reduce the wear between the battery cell 20 and the glass plate, making the test result more accurate.
[0063] (4) During the test, one side of the front panel 100 and the back panel 200 is not packaged. After being placed in a nitrogen environment for a predetermined period of time, the oxygen content in the area between the front panel 100 and the back panel 200 is reduced, and the oxidation effect of the air on the grid lines of the battery cell 20 under high temperature is reduced. Finally, the unpackaged edge is packaged to effectively protect the grid lines of the battery cell 20.
[0064] (5) The present application uses copper foil as the fixing member 500 for edge sealing, thereby reducing the influence of water vapor condensed from air on the battery cell 20 in the small sample during the test, and reducing water mist corrosion on the battery cell 20.
[0065] In the above embodiments, the description of each embodiment has its own emphasis. For parts that are not described in detail in a certain embodiment, reference can be made to the relevant descriptions of other embodiments.
[0066] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0067] The above-mentioned embodiments only express several implementation methods of the utility model, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the patent of the utility model. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the utility model, and these all belong to the protection scope of the utility model. Therefore, the protection scope of the utility model patent shall be based on the attached claims.
Claims
1. A UV attenuation testing device (10), characterized in that: The invention comprises a front panel (100), a back panel (200), a packaging strip (300), a packaging film (400) and a fixing member (500), wherein the packaging film (400) is laminated and connected to one surface of the front panel (100), the packaging strip (300) is arranged between the packaging film (400) and the back panel (200) to form an annular structure, a battery cell (20) to be tested is used to be packaged between the packaging film (400) and the back panel (200) and is located in the annular structure formed by the packaging strip (300), and the fixing member (500) fixes the front panel (100) and the back panel (200).
2. The UV attenuation testing device (10) according to claim 1, characterized in that: There is a gap between the inner edge of the packaging strip (300) and the battery cell (20) to be tested.
3. The UV attenuation testing device (10) according to claim 2, characterized in that: The spacing distance between the inner edge of the packaging strip (300) and the battery cell (20) to be tested is 3 mm to 5 mm.
4. The UV attenuation testing device (10) according to claim 1, characterized in that: The front panel (100) is a glass plate; And / or, the back panel (200) is a glass panel or a PET panel.
5. The UV attenuation testing device (10) according to any one of claims 1 to 4, characterized in that: The front panel (100) and the back panel (200) are respectively in a square shape; The side lengths of the front panel (100) and the back panel (200) are respectively 200 mm to 400 mm.
6. The UV attenuation testing device (10) according to any one of claims 1 to 4, characterized in that: The thickness of the front panel (100) is 0.2 mm to 5 mm; And / or, the thickness of the back panel (200) is 0.2 mm to 5 mm.
7. The UV attenuation testing device (10) according to any one of claims 1 to 4, characterized in that: The packaging strip (300) is in the shape of a long strip, and the width of the packaging strip (300) is 50 mm to 100 mm.
8. The UV attenuation testing device (10) according to any one of claims 1 to 4, characterized in that: The packaging strip (300) has a thickness of 0.1 mm to 1 mm.
9. The UV attenuation testing device (10) according to any one of claims 1 to 4, characterized in that: The fixing member (500) is in a U-shaped structure, and the fixing member (500) is clamped on at least part of the edge of the front panel (100) and the back panel (200).