Marking adhesive tape and lithium ion battery applying same
By optimizing the structure in the label tape, the marking layer is spaced and connected to the substrate layer and connected to the base layer, the problem of information failure caused by swelling of the commercial labeling tape is solved, and the information traceability and vibration resistance of lithium batteries are improved.
Patent Information
- Application Number
- CN202323624506.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-28
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2033-12-28
AI Technical Summary
The traceability information is invalid due to deformation after swelling, and the production information of lithium batteries cannot be effectively managed and identified, which in turn affects the safety and information traceability of lithium batteries.
Design a marking tape including a swelling layer, a composite layer and a marking layer. By optimizing the structure, there is a space between the marking layer and the swelling layer and is connected to a substrate layer that is not easily swellable, reducing the deformation of the marking layer due to swelling of the swelling layer. , ensure the integrity and recognizability of identification information.
It achieves a good swelling fixation effect in the electrolyte while maintaining the clarity and integrity of the identification information, improves the vibration resistance and information traceability of lithium batteries, and ensures the traceability of production information.
Smart Images

Figure CN221940364U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the field of marking tapes, and in particular relates to a marking tape and a lithium ion battery using the marking tape. Background Art
[0002] During daily use, when lithium batteries vibrate or fall, there is a certain gap between the bare cells and the outer shell of the lithium battery, and there is a relative displacement between the bare cells and the outer shell, which can easily lead to problems such as electrode damage, battery short circuit, and increased resistance. In order to solve the above problems, marking tape is used to bond the bare cells and cylindrical shells of lithium batteries, and the characteristic of the marking tape to expand in the electrolyte is used to fill the gaps in the lithium battery. In the cell manufacturing process, in order to trace the raw materials, production process and other information and avoid the generation of abnormal batteries, the cells need to be coded and bound. There is traceable information in the battery shell, but there is no traceable performance inside the bare cells, and the bare cells need to have identifiable traceability information at different times before and after the shell is filled for easy traceability.
[0003] Therefore, it is possible to consider setting traceability information on the identification tape. However, the commercially available identification tape will become invalid due to the deformation of the tape after swelling, making it impossible to trace the production information of the battery cell, and further making it impossible to trace the information of the lithium battery to achieve effective management and safe identification of the lithium battery.
[0004] Therefore, it is necessary to develop an identifiable and traceable marking tape, which can provide complete, clear and traceable marking information while providing good swelling and fixing effects. Utility Model Content
[0005] The utility model aims to provide a marking tape and a lithium ion battery using the marking tape. The marking tape can provide a good swelling and fixing effect and can also provide complete and clear marking information.
[0006] The utility model provides a marking tape, which includes a swelling layer, a composite layer and a marking layer, wherein the swelling layer and the composite layer are connected, the composite layer includes a substrate layer, and the composite layer includes two first surfaces and a second surface that are arranged back to back, wherein the first surface is composited with the swelling layer; the marking layer simultaneously satisfies: a. the marking layer is arranged inside the composite layer and / or on the second surface; b. the marking layer is connected to the substrate layer; c. a gap is formed between the marking layer and the first surface. The marking tape provided by the utility model optimizes the structure so that there is a gap between the marking layer and the swelling layer, and the marking layer is connected to the substrate layer that is not easy to swell in an electrolyte or a carbonate solvent, thereby reducing the probability of deformation of the marking layer due to the swelling of the swelling layer, thereby improving the recognition rate of identification information in the marking tape and the manufacturing yield of the battery cell. When the marking tape is used to fix the battery cell, the swelling layer in the marking tape can swell in volume in the electrolyte, fill the gap between the battery shell and the battery cell, and improve the anti-vibration effect of the battery; and the swelling rate of the substrate layer in the electrolyte is small, even if the swelling layer swells, the marking layer connected to the substrate layer is not easy to deform, so that complete and clear marking information can be provided. Therefore, when the marking tape contacts the electrolyte, the marking layer can still provide marking information that is easy to be scanned and identified by the equipment, so as to realize the traceability of the production batch number, production machine, production process, etc. involved in the target product, and achieve the purpose of identification and traceability.
[0007] Preferably, the composite layer further includes a first adhesive layer, and the first adhesive layer is bonded to the swelling layer.
[0008] Preferably, at least one surface of the substrate layer is used as the identification surface, and the identification surface is composited with the surface of the identification layer. Compared with the identification tape in which the identification layer is arranged inside the substrate layer, the identification tape in which the identification layer is directly composited with the identification surface of the substrate layer has a simple production process and is more conducive to mass production.
[0009] Preferably, the first adhesive layer is composited with the identification surface of the substrate layer, and the first adhesive layer wraps the identification layer. The configuration of embedding the identification layer into the first adhesive layer can fully protect the identification layer and ensure the integrity of the identification information in the identification layer.
[0010] Preferably, the thickness of the identification layer is less than the thickness of the first adhesive layer, and the thickness of the identification layer: the thickness of the first adhesive layer = 1 to 3: 1.5 to 5. Under the premise that the identification layer is embedded in the first adhesive layer and a gap is formed between the identification layer and the first surface, by setting the thickness ratio of the first adhesive layer to the identification layer to fall within the above range, the identification information of the identification layer can be clear and easy to identify, and the first adhesive layer can provide better light transmittance and refractive index for identifying and reading the identification information in the identification layer. Moreover, when the thickness ratio of the first adhesive layer to the identification layer is within the above range, the first adhesive layer is not easy to break due to local excessive thinness, thereby improving the structural stability of the first adhesive layer, so that the identification layer can be firmly attached to one side of the substrate layer and is not easily deformed due to the swelling of the identification tape.
[0011] Preferably, the thickness of the first adhesive layer does not exceed 5 μm.
[0012] Preferably, the marking tape further comprises a second adhesive layer, the second adhesive layer is connected to the composite layer, or the second adhesive layer is connected to the swelling layer. The marking tape can utilize the viscosity of the second adhesive layer to fix the marking tape on the object to be attached to the battery cell.
[0013] Preferably, the substrate layer is polypropylene, polyethylene terephthalate, polyethylene, polybutylene terephthalate, polyimide, polycarbonate or a polyolefin copolymer.
[0014] Preferably, the thickness of the marking tape is 20 to 80 μm. When the thickness of the marking tape falls within the above range, the marking tape is light in weight and small in thickness under the premise of being able to swell and fix the object, which is not only beneficial to the subsequent shelling process, but also can improve the safety and energy density of the battery using the marking tape.
[0015] The utility model also provides a lithium ion battery, which comprises a battery shell, a battery core and the above-mentioned marking tape. The battery core is arranged inside the battery shell, and the marking tape is attached to the surface of the battery core.
[0016] Preferably, the marking layer is composed of photocurable ink. The marking layer composed of photocurable ink has the advantages of corrosion resistance and wear resistance. When the marking tape is immersed in the electrolyte, the marking layer is not easily dissolved in the electrolyte, and is conducive to maintaining complete and clear marking information, thereby improving the recognizability of the marking tape.
[0017] Preferably, the thickness of the swelling layer is 18-75 μm.
[0018] Preferably, the thickness of the marking layer is no greater than 3 μm.
[0019] Preferably, the thickness of the substrate layer is 2 to 20 μm.
[0020] Preferably, the substrate layer is polyethylene terephthalate.
[0021] Preferably, the thickness of the first adhesive layer is no greater than 5 μm.
[0022] Preferably, the first adhesive layer is polyacrylic pressure-sensitive adhesive, rubber pressure-sensitive adhesive or polyurethane pressure-sensitive adhesive.
[0023] Preferably, the first adhesive layer is polyacrylate adhesive.
[0024] Preferably, the bonding force of the first adhesive layer is not less than 0.5N / 25mm.
[0025] Preferably, the second adhesive layer is polyacrylic acid pressure-sensitive adhesive, rubber pressure-sensitive adhesive or polyurethane pressure-sensitive adhesive.
[0026] Preferably, the second adhesive layer is polyacrylate adhesive.
[0027] Preferably, the bonding force of the second adhesive layer is not less than 0.5N / 25mm.
[0028] Preferably, the thickness of the second adhesive layer is no greater than 10 μm. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 A schematic diagram of the structure of the marking tape provided in Example 1;
[0030] Figure 2 A schematic diagram of the structure of the marking tape provided in Example 2;
[0031] Figure 3 A schematic diagram of the structure of the marking tape provided in Example 3;
[0032] In the above drawings, the corresponding relationship of the reference numerals is: 1. swelling layer, 2. composite layer, 3. second adhesive layer, 21. first adhesive layer, 22. substrate layer, 4. marking layer. DETAILED DESCRIPTION
[0033] For better understanding and implementation, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the accompanying drawings in the embodiments of the present invention.
[0034] In the description of the present invention, it should be noted that the terms "upper", "lower", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" etc. indicating directions or positional relationships are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on the present invention.
[0035] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention.
[0036] Example 1
[0037] This embodiment provides a marking tape. The structure of the marking tape is as follows: Figure 1 shown.
[0038] In the thickness direction, the marking tape comprises a swelling layer 1, a first adhesive layer 21, a substrate layer 22, and a second adhesive layer 3 which are compounded in sequence. The first adhesive layer 21 and the substrate layer 22 together constitute a composite layer 2. The first adhesive layer 21 comprises a first surface and a third surface which are arranged back to back, and the substrate layer 22 comprises a second surface and a fourth surface which are arranged back to back. The first surface of the first adhesive layer 21 is compounded with the swelling layer 1, and the third surface of the first adhesive layer 21 is compounded with the fourth surface of the substrate layer 22. The fourth surface of the substrate layer 22 is used as the identification surface, and a marking layer 4 is provided on the identification surface of the substrate layer 22. The surface of the marking layer 4 is compounded with the identification surface, so that the identification surface is embedded in the first adhesive layer 21 on the third surface of the first adhesive layer 21, thereby making the marking layer 4 arranged inside the composite layer 2. Among them, the marking tape is attached to the surface of the battery cell and then placed in the battery shell, and the marking tape is immersed in the electrolyte. The swelling layer 1 in the marking tape will swell in the electrolyte, fill the gap between the battery cell and the battery shell, and improve the shockproof stability of the battery. The swelling rate of the substrate layer 22 in the marking tape in the electrolyte is small, so the marking layer 4 connected to the substrate layer 22 is not easily deformed, thereby being able to provide complete and clear marking information.
[0039] Furthermore, the identification layer 4 is composed of light-curable ink, and includes identification information of numbers and two-dimensional codes in the identification layer 4. In other embodiments, the identification information in the identification layer 4 can be adjusted according to different identification requirements.
[0040] Furthermore, the substrate layer 22 is made of a polyethylene terephthalate (PET) film with a thickness of 10 μm. The first adhesive layer 21 is made of a polyacrylate adhesive with a thickness of 4 μm and an adhesive force of not less than 0.5 N / 25 mm. The swelling layer 1 is made of the base film in patent CN114213983B, the volume swelling rate of the swelling layer 1 is greater than 200%, and the thickness of the swelling layer 1 is 50 μm. The second adhesive layer 3 is made of a polyacrylate adhesive with a thickness of 8 μm and an adhesive force of not less than 0.5 N / 25 mm. The thickness of the logo layer 4 is 2 μm, so that the thickness ratio of the logo layer 4 to the first adhesive layer 21 is 2:4, thereby forming a gap between the logo layer 4 and the first surface.
[0041] In other embodiments, the materials and thicknesses of the swelling layer 1, the first adhesive layer 21, the substrate layer 22, the second adhesive layer 3, and the marking layer 4 can be adjusted according to different requirements, provided that the normal use of the marking tape is not affected, the marking effect of the marking layer 4 is not affected, and a gap is formed between the marking layer 4 and the first surface.
[0042] Example 2
[0043] This embodiment provides a marking tape based on the embodiment 1. The structure of the marking tape is as follows: Figure 2 The difference between this embodiment and the first embodiment is that the second surface of the substrate layer 22 is used as the identification surface, and a logo layer 4 is provided on the identification surface of the substrate layer 22. The surface of the logo layer 4 is composited with the identification surface, so that the identification surface is embedded in the first adhesive layer 21, thereby the logo layer 4 is provided on the second surface. The rest of the film material, film position relationship, and film thickness are strictly consistent with those of the first embodiment.
[0044] Example 3
[0045] This embodiment provides a marking tape based on the embodiment 1. The structure of the marking tape is as follows: Figure 3 As shown. The difference between this embodiment and embodiment 1 is that: in the thickness direction, the marking tape includes a substrate layer 22, a first adhesive layer 21, a swelling layer 1, and a second adhesive layer 3 that are compounded in sequence. The first adhesive layer 21 and the substrate layer 22 together constitute a composite layer 2. The first adhesive layer 21 includes a first surface and a third surface that are arranged back to back, and the substrate layer 22 includes a second surface and a fourth surface that are arranged back to back. The first surface of the first adhesive layer 21 is compounded with the swelling layer 1, and the third surface of the first adhesive layer 21 is compounded with the fourth surface of the substrate layer 22. The fourth surface of the substrate layer 22 is used as the identification surface, and a marking layer 4 is provided on the identification surface of the substrate layer 22. The surface of the marking layer 4 is compounded with the identification surface, so that the identification surface is embedded in the first adhesive layer 21 on the third surface of the first adhesive layer 21, thereby making the marking layer 4 arranged inside the composite layer 2. The material and thickness of the remaining film layers are strictly consistent with those of embodiment 1, so that a gap is formed between the marking layer 4 and the first surface.
[0046] Example 4
[0047] This embodiment provides a marking tape based on the embodiment 1. The structure of the marking tape is as follows: Figure 1 The difference between this embodiment and embodiment 1 is that the substrate layer 22 is a polyethylene (PE) film with a thickness of 10 μm.
[0048] Test Case
[0049] Test subjects: the marking tapes provided in Examples 1 to 4.
[0050] Test items and test methods:
[0051] (1) Scanning yield: Use the second adhesive layer 3 in the test object to stick the test object on the battery cell, and put the battery cell into the battery shell, inject the electrolyte to make the test object swell, and make a lithium-ion battery. After the lithium-ion battery is left to stand at 60°C for 30 days, remove the battery cell from the lithium-ion battery and scan the code. Use an A140 laser logistics scanning gun and place it 20 cm above the logistics conveyor belt. The conveyor belt conveys the battery cell at a speed of 10m / min and scans the code vertically at an angle of 90°. The calculation formula for the scanning yield is (number of cells with identified QR codes / total number of scanned cells)*100%.
[0052] Table 1. Test results of marking tapes
[0053] Group Scanning yield (%) Example 1 99.8 Example 2 99.8 Example 3 99.8 Example 4 99.8
[0054] Result analysis: From Table 1, it can be seen that the marking tapes of Examples 1 to 4 can provide a good scanning yield for lithium-ion batteries, and can trace the information of lithium batteries to achieve effective management and safe identification of lithium batteries. It can be seen that the marking tape provided by this method improves the recognition rate of identification information in the marking tape and the traceability of the battery cell by optimizing the structure.
[0055] The above embodiments are only used to illustrate the technical solution of the utility model rather than to limit the protection scope of the utility model. Although the utility model is described in detail with reference to the preferred embodiments, ordinary technicians in this field should understand that the technical solution of the utility model can be modified or replaced by equivalents without departing from the essence and scope of the technical solution of the utility model.
Claims
1. A marking tape, characterized in that: The invention comprises a swelling layer, a composite layer and a marking layer, wherein the swelling layer and the composite layer are connected, the composite layer comprises a substrate layer, and the composite layer comprises a first surface and a second surface disposed back to back, wherein the first surface is composited with the swelling layer; The identification layer also satisfies: a. The identification layer is disposed inside the composite layer and / or on the second surface; b. The identification layer is connected to the substrate layer; c. A gap is formed between the identification layer and the first surface.
2. The marking tape according to claim 1, wherein: The composite layer further includes a first adhesive layer, and the first adhesive layer is bonded to the swelling layer.
3. The marking tape according to claim 2, wherein: At least one surface of the substrate layer is used as an identification surface, and the identification surface is composited with the surface of the marking layer.
4. The marking tape according to claim 3, wherein: The first adhesive layer is compounded with the identification surface of the base material layer, and the first adhesive layer wraps the identification layer.
5. The marking tape according to claim 4, wherein: The thickness of the marking layer is smaller than that of the first adhesive layer, and the thickness of the marking layer: the thickness of the first adhesive layer = 1-3: 1.5-5.
6. The marking tape according to claim 2, wherein: The thickness of the first adhesive layer does not exceed 5 μm.
7. The marking tape according to claim 1, wherein: The marking tape further includes a second adhesive layer, and the second adhesive layer is connected to the composite layer, or the second adhesive layer is connected to the swelling layer.
8. The marking tape according to claim 1, wherein: The substrate layer is polypropylene, polyethylene terephthalate, polyethylene, polybutylene terephthalate, polyimide, polycarbonate or polyolefin copolymer.
9. The marking tape according to claim 1, wherein: The thickness of the marking tape is 20 to 80 μm.
10. A lithium-ion battery, characterized in that: The battery comprises a battery shell, a battery cell and the identification tape according to any one of claims 1 to 9, wherein the battery cell is arranged inside the battery shell, and the identification tape is attached to the surface of the battery cell.