Stainless steel color-coated sheet capable of being welded

By designing spaced blank areas and coating structures on stainless steel color-coated plates, the problem that traditional connection methods cannot prevent water leakage and wind resistance is solved, and the continuous welding and efficient corrosion and wind resistance of stainless steel color-coated plates are achieved.

CN221941745UActive Publication Date: 2024-11-01RUITONG INFORMATION IND JIANGSU
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323499237.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-21
Publication Date
2024-11-01
Estimated Expiration
2033-12-21

AI Technical Summary

Technical Problem

The connection methods of traditional stainless steel color-coated plates (lap, buckle, and bite) cannot completely prevent water leakage risks and have extremely poor wind resistance, which cannot meet welding requirements.

Method used

A stainless steel color coating board including spaced color coating area and white coating area is designed. The white coating area is used for welding. The coating composed of passivation layer, primer layer and topcoat layer improves corrosion resistance and sealing. Ensure welding quality and wind resistance.

Benefits of technology

Continuous welding of stainless steel color-coated plates is realized, which enhances the corrosion resistance and wind resistance of the roof and curtain walls, prevents water leakage, and improves the adhesion and sealing of the coating.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221941745U_ABST
    Figure CN221941745U_ABST
Patent Text Reader

Abstract

The utility model provides a stainless steel color-coated sheet capable of being welded, which comprises color-coated areas and blank areas which are arranged at intervals, the blank areas are arranged on two sides close to the edge, and the blank areas are stainless steel substrates which are used for welding with adjacent stainless steel color-coated sheets after being bent. The color coating area comprises a stainless steel substrate, passivation layers coated on the two sides of the stainless steel substrate, a primer layer coated on the front passivation layer, and a finish paint layer coated on the primer layer; the blank area is not coated with a coating, and the color coating area is coated with a coating, so that corrosion resistance of a roof and a curtain wall is achieved, water leakage can be prevented, the wind resistance of a building is greatly enhanced, the corrosion resistance of the stainless steel base plate can be improved and the adhesive force performance of the primer layer and the stainless steel base plate can be enhanced due to the arrangement of the passivation layer, and the service life of the stainless steel base plate is prolonged. The primer layer is arranged, so that the sealing performance of the coating can be enhanced, the adhesive force of the finish paint and the stainless steel base material is improved, peeling and falling of the coating in the color coating area are avoided, and the paint color of the finish paint can be selected according to needs.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of stainless steel plates, in particular to a stainless steel color-coated plate capable of being welded. Background Art

[0002] Stainless steel welded color-coated plates have excellent corrosion resistance and are widely used in building roof curtain wall enclosure systems. There are three ways to connect traditional coated color-coated plates: overlap, buckle, and bite, but these three connection methods cannot completely prevent the hidden danger of water leakage, and the wind resistance effect is extremely poor. The use of welded roofs and curtain walls just solves this problem. The welding method is to press and bend the edges of the stainless steel welded color-coated plates, and then weld them continuously with the adjacent stainless steel welded color-coated plates on the installation purlins installed on the roof, and then put on the cap to prevent water vapor from penetrating. For the stainless steel color-coated plates that need to be welded, there must be no coating at the welding point to isolate the conductivity. Therefore, the style of coating both sides of the stainless steel color-coated plates in the existing technology cannot meet the welding requirements of stainless steel color-coated plates. Utility Model Content

[0003] In view of the shortcomings of the prior art mentioned above, the purpose of the utility model is to provide a stainless steel color-coated plate that can be welded, which is used to solve the problem that the traditional connection methods of color-coated plates in the prior art are overlapping, buckling, and biting, but cannot completely prevent the hidden danger of water leakage and have extremely poor wind resistance.

[0004] In order to achieve the above purpose and other related purposes, the utility model provides the following technical solutions:

[0005] A weldable stainless steel color-coated plate comprises a color-coated area and a blank area which are arranged at intervals, and both sides close to the edge are blank areas, the blank area is a stainless steel substrate which is used for welding with adjacent stainless steel welding color-coated plates after being pressed and bent, and the color-coated area comprises a stainless steel substrate, a passivation layer coated on both sides of the stainless steel substrate, a primer layer coated on the passivation layer on the front side, and a topcoat layer coated on the primer layer.

[0006] By implementing the above technical solution, the stainless steel welded color-coated plate has excellent corrosion resistance and is widely used in building roofs and curtain wall enclosure systems. There are three ways to connect traditional coated color-coated plates: overlap, buckle, and bite, but these three connection methods cannot completely prevent the hidden danger of water leakage, and the wind resistance effect is extremely poor. The use of welded roofs and curtain walls can just solve this problem. The welding method is to press and bend the blank margins of the stainless steel welded color-coated plate, and weld it to the adjacent stainless steel welded color-coated plate on the installation purlin installed on the roof, and then put on the cover cap. If welding is to be done, there must be no coating at the welding point to isolate the conductivity. This is the role of the blank area in this application. The blank area in this application can be bent and connected to the adjacent stainless steel welded color-coated plate The color-coated plates are welded to achieve a continuous welding process, which not only solves the corrosion resistance of the roof and curtain wall, but also prevents water leakage. The roof and curtain wall are relatively integrated, which greatly enhances the building's wind resistance. The setting of the passivation layer can improve the anti-corrosion performance of the stainless steel substrate and enhance the adhesion performance of the coating and the stainless steel substrate. The setting of the primer can enhance the sealing of the coating, improve the adhesion of the topcoat to the stainless steel substrate, and avoid peeling of the coating. The topcoat can be selected from white, red, blue, yellow, green or gray series as needed.

[0007] In an embodiment of the present invention, the width of the blank area is 1-10 cm.

[0008] To implement the above technical solution, the blank area is mainly used for welding. The width of the blank area is set to 1-10 cm as needed, and no primer layer and topcoat layer are provided on the reverse side of the blank area, so as to improve the conductivity and welding quality.

[0009] In an embodiment of the present invention, the thickness of the stainless steel substrate is 0.4-1.2 mm.

[0010] To implement the above technical solution, the stainless steel substrate in the present application is made of stainless steel material that can be continuously welded, and the thickness can be set as needed.

[0011] In one embodiment of the present invention, the passivation layer includes an inner layer composed of chromium oxide and an outer layer composed of chromic acid oxide.

[0012] By implementing the above technical solution, the setting of the passivation layer can improve the corrosion resistance of stainless steel. After the stainless steel is passivated, a dense passivation film (outer layer) can be formed on the surface of the stainless steel substrate to isolate the contact between the stainless steel substrate and the environment, thereby improving the oxidation resistance and corrosion resistance of the stainless steel. The inner layer is composed of chromium oxide of the stainless steel substrate and is integrated with the stainless steel substrate, thereby preventing external oxygen, water and other corrosive media from eroding the stainless steel surface, thereby maintaining good corrosion resistance.

[0013] In an embodiment of the present invention, the thickness of the primer layer is 4-12 μm.

[0014] To implement the above technical solution, the physical properties of the coating composed of the passivation layer, the primer layer, and the topcoat layer in this application are: 00-grid level, T-bend ≦2T, reverse impact ≧12J, MEK ≧120 times. To ensure the quality of the coating, the primer is applied to the stainless steel substrate by a paint roller and the primer is baked in an oven to ensure that the primer is completely cured.

[0015] In one embodiment of the present invention, the thickness of the topcoat layer 6 is 10-25 μm. To implement the above technical solution, the topcoat is reversely coated on the stainless steel using a paint roller, a smoothing roller (or no roller), a paint roller, and a guide roller to ensure the quality of the topcoat coating, and the topcoat is completely cured by baking in an oven, and the topcoat is cooled and rolled up after the curing is completed.

[0016] As described above, the weldable stainless steel color-coated plate of the utility model has the following beneficial effects:

[0017] The blank area in the present application can be welded to the adjacent stainless steel welding color-coated plate after press-forming and bending, which not only solves the corrosion resistance of the roof and curtain wall, but also prevents water leakage, and greatly enhances the wind resistance of the building. The setting of the passivation layer can improve the anti-corrosion performance of the stainless steel plate, and the setting of the primer can enhance the sealing ability and the bonding force with the topcoat, thereby improving the adhesion between the topcoat and the stainless steel substrate and avoiding peeling of the coating. After the stainless steel is passivated, a dense passivation film can be formed on the surface of the stainless steel substrate to isolate the contact between the stainless steel substrate and the environment, thereby improving the oxidation resistance and corrosion resistance of the stainless steel, and preventing external oxygen, water and other corrosive media from eroding the stainless steel surface, so that it maintains good corrosion resistance. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 Shown is a schematic diagram of the structure of the utility model.

[0019] Figure 2 Shown is another structural schematic diagram of the utility model.

[0020] Figure 3 Shown is a cross-section of the painted area.

[0021] Figure 4 Shows the schematic diagram of welding adjacent color-coated plates.

[0022] Component number description

[0023] 1. Color coating area; 2. Blank area; 3. Stainless steel substrate; 4. Passivation layer; 5. Primer layer; 6. Topcoat layer; 7. Capping. DETAILED DESCRIPTION

[0024] The following specific embodiments illustrate the implementation of the present invention, and those familiar with the technology can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. It should be noted that the following embodiments and features in the embodiments can be combined with each other without conflict.

[0025] See also Figures 1 to 4 The utility model provides a stainless steel color-coated plate capable of being welded, comprising a color-coated area 1 and a blank area 2 arranged at intervals, and both sides close to the edge are blank areas 2, the blank area 2 is a stainless steel substrate 3 used for welding with adjacent stainless steel welding color-coated plates after bending, the color-coated area 1 comprises a stainless steel substrate 3, a passivation layer 4 coated on both sides of the stainless steel substrate 3, a primer layer 5 coated on the front side of the passivation layer 4, and a topcoat layer 6 coated on the primer layer 5.

[0026] Stainless steel welded color-coated plates have excellent corrosion resistance and are widely used in building roof curtain walls and enclosure systems. There are three ways to connect traditional coated color-coated plates: overlap, buckle, and bite, but these three connection methods cannot completely prevent the hidden danger of water leakage, and the wind resistance effect is extremely poor. The use of welded roofs and curtain walls just solves this problem. The welding method is to press and bend the edge of the stainless steel welded color-coated plate, and weld it against the installation purlin installed on the roof, and then put on the cap 7. If you want to weld, there must be no coating to isolate the conductivity at the welding point. This is the role of the blank area 2 in this application. The blank area 2 in this application can be welded with the adjacent stainless steel welded color-coated plate after bending. This not only solves the corrosion resistance of the roof and curtain wall, but also prevents water leakage, and greatly enhances the wind resistance of the building. The setting of the passivation layer 4 can improve the anti-corrosion performance of the stainless steel plate, and the setting of the primer can enhance the sealing degree of the coating, improve the adhesion of the topcoat to the stainless steel substrate, and avoid peeling of the coating. The topcoat can be selected according to needs. The color is white series, red series, blue series, yellow series, purple series, black series, green series or gray series and other paint colors.

[0027] The width of the blank area 2 is 1-10 cm. The blank area 2 is mainly used for welding, and the width of the blank area 2 is set to 1-10 cm as required, and the other side of the blank area 2 is not provided with a primer layer 5 and a topcoat layer 6.

[0028] The thickness of the stainless steel substrate 3 is 0.4-1.2 mm. The stainless steel substrate 3 in the present application is a common stainless steel material that can be welded, and the thickness can be set as required.

[0029] The passivation layer 4 comprises a dense passivation film (outer layer) formed on the surface of the stainless steel substrate after the stainless steel passivation treatment to isolate the contact between the stainless steel substrate and the environment, thereby improving the anti-oxidation and anti-corrosion capabilities of the stainless steel. The inner layer is composed of chromium oxide brought by the stainless steel substrate 3, which can prevent external oxygen, water and other corrosive media from eroding the stainless steel surface, thereby maintaining good corrosion resistance.

[0030] The thickness of the primer layer 5 is 4-12 μm. The physical properties of the coating composed of the passivation layer 4, the primer layer 5, and the topcoat layer in the present application are: 100-grid level 0, T bend ≦2T, reverse impact ≧12J, MEK ≧120 times. To ensure the quality of the coating, the primer is applied to the stainless steel substrate by a paint roller and then baked in an oven to ensure that the primer is completely cured.

[0031] The thickness of the topcoat layer 6 is 10-25 μm. The topcoat is reversely coated on the stainless steel by rotating a paint roller, a smoothing roller (or no roller), a paint roller, and a guide roller, and is completely cured by an oven baking method. After the topcoat is cured, it is cooled and rolled up.

[0032] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. All equivalent modifications or changes made by those skilled in the art without departing from the spirit and technical ideas disclosed in the present invention shall still be covered by the claims of the present invention.

Claims

1. A weldable color-coated stainless steel plate, characterized by: The invention comprises a color-coated area (1) and a blank area (2) arranged at intervals, and both sides close to the edge are blank areas (2), the blank areas (2) located on both sides are stainless steel substrates (3) for welding with adjacent stainless steel color-coated plates after being press-formed and bent, and the color-coated area (1) comprises a stainless steel substrate (3), a passivation layer (4) coated on both sides of the stainless steel substrate (3), a primer layer (5) coated on the passivation layer (4) on the front side, and a topcoat layer (6) coated on the primer layer (5).

2. The weldable color-coated stainless steel sheet according to claim 1, characterized in that: The width of the blank area (2) is 1-10 cm.

3. The weldable color-coated stainless steel sheet according to claim 1, characterized in that: The thickness of the stainless steel substrate (3) is 0.4-1.2 mm.

4. The weldable color-coated stainless steel sheet according to claim 1, characterized in that: The thickness of the primer layer (5) is 4-12 μm.

5. The weldable color-coated stainless steel sheet according to claim 1, characterized in that: The thickness of the topcoat layer (6) is 10-25 μm.