By setting a fluoride liquid layer and an anti-fingerprint liquid layer on the glass panel of the gas stove, and using the recesses to increase the contact area, the problem of anti-fingerprint liquid layer is solved, and the good anti-oil and anti-fingerprint effect of the panel is achieved, and the lengthening effect of the panel is extended. It has service life and ease of cleaning.

CN221944293UActive Publication Date: 2024-11-01HISENSE (SHANDONG) KITCHEN & BATHROOM CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323662104.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-29
Publication Date
2024-11-01
Estimated Expiration
2033-12-29

AI Technical Summary

Technical Problem

The anti-fingerprint liquid layer of the existing gas stove glass panel is prone to fall off, resulting in a reduced anti-oil and anti-fingerprint effect, affecting the user experience.

Method used

A fluoride liquid layer is provided on the surface of the glass substrate, and an anti-fingerprint liquid layer is added to the fluoride liquid layer. A solid hydrophobic and oleophobic coating is formed by combining the fluoride liquid layer and the anti-fingerprint liquid layer, and a multiple recesses are used to increase the The contact area between the large fluoride liquid layer and the glass substrate ensures the stability of the fluoride liquid layer and the anti-fingerprint liquid layer.

Benefits of technology

It achieves good anti-glass and anti-fingerprint effects of glass panels, extends the service life of the panels, and maintains easy cleaning.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221944293U_ABST
    Figure CN221944293U_ABST
Patent Text Reader

Abstract

The utility model discloses a stove, relates to the technical field of stoves, and aims to solve the problem that in the prior art, an anti-fingerprint liquid layer is easy to fall off, so that the anti-oil and anti-fingerprint effects of a glass surface are reduced. The cooker comprises a panel, and the panel comprises a glass substrate, a fluorinated liquid layer and an anti-fingerprint liquid layer. The fluorination liquid layer is arranged on the surface of the glass substrate and is connected with the glass substrate, and the fingerprint-proof liquid layer is arranged on the fluorination liquid layer and is connected with the fluorination liquid layer. A plurality of concave parts are arranged on one side, facing the fluorination liquid layer, of the glass substrate, and at least part of the fluorination liquid layer is filled in the plurality of concave parts. Therefore, the contact area between the fluorination liquid layer and the surface of the glass substrate can be increased, so that the fluorination liquid layer and the fingerprint-proof liquid layer are not easy to fall off, and the panel can have good oil stain-proof and fingerprint-proof effects. Therefore, the problem that in the prior art, an anti-fingerprint liquid layer is prone to falling off, so that the oil stain prevention and fingerprint prevention effects of the glass surface are reduced can be solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of stoves, in particular to a stove. Background Art

[0002] A gas stove is a common kitchen appliance used for cooking food. A gas stove usually uses natural gas or liquefied gas as fuel, and heats the bottom of the pot through flames to cook food.

[0003] At present, the panels of household gas stoves in the kitchen are mostly made of tempered glass, mainly because glass panels are more fashionable and beautiful, and are also easy to clean. However, as users cook for a long time, oil smoke and food residues may form grease on the glass surface, and fingers touching the glass panel will also leave fingerprints. These grease and fingerprints may form stains on the glass surface that are difficult to clean, affecting the user experience.

[0004] In the prior art, anti-fingerprint liquid is usually coated on the glass surface to achieve the anti-oil and anti-fingerprint effects, but the anti-fingerprint liquid layer is easy to fall off, thereby greatly reducing the anti-oil and anti-fingerprint effects of the glass surface. Utility Model Content

[0005] The embodiment of the utility model provides a stove, which solves the problem in the prior art that the anti-fingerprint liquid layer is easy to fall off, resulting in reduced anti-oil and anti-fingerprint effects on the glass surface.

[0006] In order to achieve the above object, the embodiment of the utility model adopts the following technical solution:

[0007] The embodiment of the present application provides a stove, the stove includes a panel, the panel includes a glass substrate, a fluorinated liquid layer and an anti-fingerprint liquid layer. The fluorinated liquid layer is arranged on the surface of the glass substrate, and the side of the fluorinated liquid layer facing the glass substrate is connected to the glass substrate, and the anti-fingerprint liquid layer is arranged on the side of the fluorinated liquid layer away from the glass substrate, and is connected to the fluorinated liquid layer. A plurality of recessed portions are provided on the side of the glass substrate facing the fluorinated liquid layer, and at least part of the fluorinated liquid layer is filled in the plurality of recessed portions.

[0008] In the cooker provided in the embodiment of the present application, a fluorinated liquid layer is arranged on a glass substrate, so that the fluorinated liquid layer can be well attached to the glass substrate. After the anti-fingerprint liquid layer is arranged on the fluorinated liquid layer, the fluorinated liquid in the fluorinated liquid layer can be mixed with the anti-fingerprint liquid in the anti-fingerprint liquid layer, so that the fluorinated liquid layer and the anti-fingerprint liquid layer are firmly combined, thereby forming a firm hydrophobic and oleophobic coating on the surface of the glass substrate, so that the static water droplet contact angle on the panel surface is greater than or equal to 100°, oil stains are not easily adhered, and easy cleaning can be maintained at any time.

[0009] By providing the recessed portion, the contact area between the fluoride liquid layer and the surface of the glass substrate can be increased, so that the fluoride liquid layer can be more firmly attached to the surface of the glass substrate, so that the fluoride liquid layer and the anti-fingerprint liquid layer are not easy to fall off, so that the panel can have good anti-oil and anti-fingerprint effects, and can also protect the glass substrate for a long time, extending its service life.

[0010] In addition, the fluorinated liquid layer also has good anti-fouling properties. If the anti-fingerprint liquid layer on the glass substrate and the portion of the fluorinated liquid layer outside the plurality of recessed portions are destroyed, the fluorinated liquid layer filling the plurality of recessed portions still remains on the surface of the glass substrate, thereby reducing the contact area between oil stains and fingerprints and the glass substrate, achieving anti-fingerprint and anti-oil stain effects.

[0011] Therefore, the stove provided in the embodiment of the present application can solve the problem in the prior art that the anti-fingerprint liquid layer is easy to fall off, resulting in reduced anti-oil and anti-fingerprint effects on the glass surface.

[0012] In some embodiments, the surface of the glass substrate includes a first supporting surface, the first supporting surface is perpendicular to the thickness direction of the glass substrate, at least part of the plurality of recessed portions is disposed on the first supporting surface, and at least part of the fluorinated liquid layer is disposed on the first supporting surface and connected to the first supporting surface.

[0013] In some embodiments, the first supporting surface is parallel to the fluorinated liquid layer, and / or the edge of the first supporting surface coincides with the projection of the side edge of the fluorinated liquid layer in the thickness direction of the glass substrate.

[0014] In some embodiments, the surface of the glass substrate further includes a first decorative surface, which is disposed on a peripheral wall of the glass substrate and connected to an edge of the first supporting surface, a plurality of recessed portions are disposed on the first supporting surface and the first decorative surface, and the fluorinated liquid layer is disposed on the first supporting surface and the first decorative surface and connected to the first supporting surface and the first decorative surface.

[0015] In some embodiments, there are multiple first decorative surfaces, and planes where at least two first decorative surfaces are located are parallel or intersecting.

[0016] In some embodiments, the surface of the glass substrate further includes a second supporting surface and a first decorative surface. The second supporting surface and the first supporting surface are spaced apart in the thickness direction of the glass substrate, the first decorative surface is located on the outer peripheral side of the first supporting surface, two opposite sides of the first decorative surface in the thickness direction of the glass substrate are respectively connected to the edges of the first supporting surface and the second supporting surface, the plane where the first supporting surface is located is parallel to or intersects with the plane where the second supporting surface is located, and the fluorinated liquid layer is disposed on the first supporting surface, the first decorative surface and the second supporting surface, and is connected to the first supporting surface, the first decorative surface and the second supporting surface.

[0017] In some embodiments, the thickness of the fluorinated liquid layer ranges from 6 μm to 12 μm; and / or the thickness of the anti-fingerprint liquid layer ranges from 4 μm to 8 μm.

[0018] In some embodiments, the panel has a static water drop contact angle greater than or equal to 100°.

[0019] In some embodiments, the fluorinated liquid layer includes a layer body and a plurality of protrusions, the plurality of protrusions are located on the side of the layer body facing the glass substrate, one protrusion fits in one recess, and the layer body is connected to the anti-fingerprint liquid layer and the glass substrate.

[0020] In some embodiments, the cooker further comprises a shell and a burner, wherein the shell is arranged below the panel and connected to the panel, the burner is mounted on the panel, the panel is provided with a through hole, and the burner extends out of the through hole. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 This is one of the structural schematic diagrams of the cooker provided in the embodiment of the present application;

[0022] Figure 2 The second structural schematic diagram of the stove provided in the embodiment of the present application;

[0023] Figure 3 One of the structural schematic diagrams of the panel provided in the embodiment of the present application;

[0024] Figure 4 The second structural schematic diagram of the panel provided in the embodiment of the present application;

[0025] Figure 5 The third structural diagram of the panel provided in the embodiment of the present application;

[0026] Figure 6 A fourth structural schematic diagram of a panel provided in an embodiment of the present application;

[0027] Figure 7 A fifth structural diagram of a panel provided in an embodiment of the present application;

[0028] Figure 8 A flow chart of a panel processing method provided in an embodiment of the present application;

[0029] Fig. 9 The sixth structural diagram of the panel provided in the embodiment of the present application;

[0030] Fig.10 The seventh structural diagram of the panel provided in the embodiment of the present application;

[0031] Fig.11 The eighth structural diagram of the panel provided in the embodiment of the present application;

[0032] Fig.12 A ninth structural diagram of a panel provided in an embodiment of the present application;

[0033] Fig.13 The tenth structural diagram of the panel provided in the embodiment of the present application;

[0034] Fig.14 The eleventh structural diagram of the panel provided in the embodiment of the present application;

[0035] Fig.15 The twelfth structural diagram of the panel provided in the embodiment of the present application;

[0036] Fig.16 The thirteenth structural diagram of the panel provided in the embodiment of the present application;

[0037] Fig.17 This is the fourteenth structural schematic diagram of the panel provided in the embodiment of the present application.

[0038] Figure numerals: 1, stove; 10, panel; 11, glass substrate; 111, recessed portion; 112, first supporting surface; 113, first decorative surface; 114, second supporting surface; 115, second decorative surface; 12, fluorinated liquid layer; 121, layer body; 122, protruding portion; 123, connecting portion; 13, anti-fingerprint liquid layer; 20, shell; 30, igniter; 40, burner head; 50, regulator. DETAILED DESCRIPTION

[0039] The embodiments of the utility model are described in detail below with reference to the accompanying drawings.

[0040] In the description of the present invention, it should be understood that the terms "center", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating directions or positional relationships, are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore should not be understood as a limitation on the present invention.

[0041] The terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present utility model, unless otherwise specified, "plurality" means two or more.

[0042] In the description of the present utility model, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be internal communication between two components. For ordinary technicians in this field, the specific meanings of the above terms in the present utility model can be understood according to specific circumstances. In addition, when describing pipelines or channels, the "connected" and "connected" used in this application have the meaning of conduction. The specific meaning needs to be understood in conjunction with the context.

[0043] In the embodiments of the present application, words such as "exemplary" or "for example" are used to indicate examples, illustrations or descriptions. Any embodiment or design described as "exemplary" or "for example" in the embodiments of the present application should not be interpreted as being more preferred or more advantageous than other embodiments or designs. Specifically, the use of words such as "exemplary" or "for example" is intended to present related concepts in a specific way.

[0044] As used herein, "about," "substantially," or "approximately" includes the stated value and an average value that is within an acceptable range of variation from the particular value as determined by one of ordinary skill in the art taking into account the measurements in question and the errors associated with the measurement of the particular quantity (i.e., the limitations of the measurement system).

[0045] refer to Figure 1 The embodiment of the present application provides a stove 1, which includes a panel 10, a shell 20 and a burner 40. The shell 20 is arranged below the panel 10 and connected to the panel 10. The panel 10 is provided with a through hole, through which the burner 40 can extend and be installed on the panel 10, and the burner 40 is used to spray gas.

[0046] refer to Figure 2 The stove 1 further includes an igniter 30 , a gas pipeline (not shown in the figure) and a valve device (not shown in the figure), etc. The burner head 40 is connected to the gas pipeline via the valve device, and the igniter 30 can be arranged close to the burner head 40 .

[0047] Continue to refer Figure 1 or Figure 2The stove also includes a regulator 50, which is installed on the panel 10 and is used to adjust the fire power. When using the stove 1, the regulating knob can be rotated to control the valve device to open, so that the gas flows to the burner 40, and the igniter 30 is controlled to ignite, ignite the gas ejected through the burner 40, and make the mixture of gas and air burn to form a flame for heating the food in the pot and cooking the food. During the operation of the gas stove, the regulating knob can be rotated according to the cooking needs to adjust the opening of the valve device, thereby changing the gas flow delivered to the burner 40, and then realizing the adjustment of the fire power.

[0048] It can be understood that the number of the through holes can be one or more, and the number of the burner heads 40 is set according to the number of the through holes. In the present application, two burner heads 40 are provided.

[0049] refer to Figure 3 The panel 10 includes a glass substrate 11 , a fluorinated liquid layer 12 and an anti-fingerprint liquid layer 13 .

[0050] It can be understood that the panel 10 can be a glass panel. The panel 10 can also include a substrate and a glass substrate 11 disposed on the substrate. The substrate can be made of metal materials such as stainless steel or ceramics.

[0051] The fluoride liquid layer 12 is disposed on the surface of the glass substrate 11 , and the side of the fluoride liquid layer 12 facing the glass substrate 11 is connected to the glass substrate 11 , wherein the surface is the side facing the user when the user uses the cooker 1 .

[0052] Exemplarily, the material of the fluorinated liquid layer 12 may be fluorinated liquid, and specifically, the fluorinated liquid may be a fluorinated liquid series FC60-FC330.

[0053] Exemplarily, the fluorinated liquid may be sprayed onto the surface of the glass substrate 11 . Of course, the fluorinated liquid may also be disposed on the surface of the glass substrate 11 by roll coating or other methods.

[0054] The fluoride liquid layer 12 has good adhesion, and has friction resistance, temperature resistance, acid and alkali resistance, and compactness, so that the fluoride liquid layer 12 and the glass substrate 11 can have a good connection.

[0055] The anti-fingerprint liquid layer 13 is disposed on a side of the fluoride liquid layer 12 away from the glass substrate 11 , and is connected to the fluoride liquid layer 12 .

[0056] Exemplarily, the material of the anti-fingerprint liquid layer 13 may be anti-fingerprint liquid DH320LF. Specifically, the main component of the anti-fingerprint liquid is 99% perfluoropolyether+1% special fluorosilane.

[0057] For example, the anti-fingerprint liquid may be sprayed on the surface of the fluorinated liquid layer 12 . Of course, the anti-fingerprint liquid may also be disposed on the surface of the fluorinated liquid layer 12 by roll coating or other methods.

[0058] The anti-fingerprint liquid layer 13 has low surface free energy and excellent hydrophobicity and oleophobicity, so that the surface of the panel 10 is not easily wetted by water or grease, thereby reducing the residual fingerprints, and can also reduce the adhesion of dust, oil and other stains, making the surface of the panel 10 easier to clean. The anti-fingerprint liquid layer 13 also has a certain wear resistance, which can extend the service life of the surface of the panel 10 and reduce the generation of scratches. In addition, the anti-fingerprint liquid layer 13 usually has good transparency and will not affect the appearance and texture of the glass substrate 11.

[0059] When anti-fingerprint liquid is sprayed on the fluorinated liquid, the components of the anti-fingerprint liquid match the components of the fluorinated liquid, making the interaction between them closer, thereby achieving better bonding.

[0060] In this way, the fluorinated liquid layer 12 can not only adhere well to the glass substrate 11, but also better bond with the anti-fingerprint liquid layer 13, so that the fluorinated liquid layer 12 and the anti-fingerprint liquid layer 13 can be firmly attached to the glass substrate 11, and a strong hydrophobic and oleophobic coating is formed on the surface of the glass substrate 11, so that the surface of the panel 10 is not easy to adhere to oil stains and can be kept easy to clean at any time.

[0061] In addition, since the surface of the panel 10 is not easily corroded by oil stains and water drops, the service life of the panel 10 will be extended, and the panel 10 can also maintain a good appearance.

[0062] In some embodiments, the static water drop contact angle of the panel 10 is greater than or equal to 100°. The static water drop contact angle refers to the angle formed when a water drop or an oil drop contacts the surface of the panel 10. When a water drop or an oil drop forms a large contact angle on the surface of the panel 10, it indicates that the surface of the panel 10 has strong hydrophobicity and oleophobicity, and the water drop or the oil drop will appear spherical or rapidly rolling. In this case, the adhesion between the water drop or the oil drop and the surface of the panel 10 is very weak, so that the surface of the panel 10 is not easy to adhere to oil stains, and can be kept easy to clean at any time.

[0063] refer to Figure 4 and Figure 5 A plurality of recessed portions 111 are provided on the side of the glass substrate 11 facing the fluoride liquid layer 12 , and at least a portion of the fluoride liquid layer 12 is filled in the plurality of recessed portions 111 , that is, a portion of the fluoride liquid layer 12 is filled in the plurality of recessed portions 111 , or the entire fluoride liquid layer 12 is filled in the plurality of recessed portions 111 .

[0064] In this way, by providing the recessed portion 111, the contact area between the fluoride liquid layer 12 and the surface of the glass substrate 11 can be increased, so that the fluoride liquid layer 12 can be more firmly attached to the surface of the glass substrate 11, so that the fluoride liquid layer 12 and the anti-fingerprint liquid layer 13 are not easy to fall off, so that the panel 10 can have good anti-oil and anti-fingerprint effects, and can also protect the glass substrate 11 for a long time, extending its service life.

[0065] In addition, the fluorinated liquid layer 12 has good anti-fouling properties. When the anti-fingerprint liquid layer 13 on the glass substrate 11 and the portion of the fluorinated liquid layer 12 outside the plurality of recessed portions 111 are destroyed, the fluorinated liquid layer 12 filled in the plurality of recessed portions 111 still remains on the surface of the glass substrate 11, thereby reducing the contact area between oil stains and fingerprints and the glass substrate 11, thereby achieving anti-fingerprint and anti-oil stain effects.

[0066] Therefore, the stove provided in the embodiment of the present application can solve the problem in the prior art that the anti-fingerprint liquid layer is easy to fall off, resulting in reduced anti-oil and anti-fingerprint effects on the glass surface.

[0067] Continue to refer Figure 4 and Figure 5 , and combined with Figure 6 The spacing between the multiple recessed portions 111 can be set as needed, and the spacing between two adjacent recessed portions 111 can be 0 or not 0, which is not limited in this embodiment.

[0068] like Figure 5 and Figure 6 As shown, when the distance between two adjacent recesses 111 is 0, that is, when a plurality of continuous recesses 111 are provided on the surface of the glass substrate 11 , the fluoride liquid layer 12 may be completely filled in the plurality of recesses 111 or may be partially filled in the plurality of recesses 111 .

[0069] like Figure 4 As shown, when the distance between two adjacent recesses 111 is not 0, that is, when a plurality of recesses 111 are spaced apart on the surface of the glass substrate 11 , a portion of the fluoride liquid layer 12 can be filled in the plurality of recesses 111 , and another portion can be located outside the plurality of recesses 111 .

[0070] It is understandable that the plurality of recessed portions 111 may be selectively disposed at positions of the glass substrate 11 that are prone to oil dripping, water dripping, and touching. Of course, the plurality of recessed portions 111 may also be disposed on the entire surface of the glass substrate 11 .

[0071] Continue to refer Figure 4 , and combined with Figure 7For example, the plurality of recessed portions 111 may be a plurality of micro grooves disposed on the surface of the glass substrate 11 . The shape of the grooves may be set as required. The shape of the grooves may be triangular, semicircular, etc. This embodiment does not specifically limit this.

[0072] Continue to refer Figure 4 In some embodiments, the fluorinated liquid layer 12 includes a layer body 121 and a plurality of protrusions 122 , the plurality of protrusions 122 are located on a side of the layer body 121 facing the glass substrate 11 , one protrusion 122 fits in one recess 111 , and the layer body 121 is connected to the anti-fingerprint liquid layer 13 and to the glass substrate 11 .

[0073] In this way, the layer body 121 can well bond the glass substrate 11 and the anti-fingerprint liquid layer 13 together, and when the anti-fingerprint liquid layer 13 and the layer body 121 are destroyed, the surface of the glass substrate 11 still has the protrusions 122 filled in the multiple recesses 111, thereby reducing the contact area between oil stains and fingerprints and the glass substrate 11, achieving the effect of anti-fingerprint and anti-oil stains.

[0074] refer to Figure 8 In some embodiments, the present application also provides a method for processing a panel, the method comprising:

[0075] Step S100: Substrate treatment: remove oil stains from the surface of the glass substrate, and then let it stand or dry it after cleaning.

[0076] Step S200: fluoride liquid spraying: under the conditions of temperature 23°C ± 2°C and relative humidity 55% ± 5%, spray fluoride liquid series FC60-FC330 at an amount of 20g / ㎡-30g / ㎡ onto the surface of the glass substrate, dry for 2min-4min, and then cure at 120°C-160°C for 20min-30min to form a fluoride liquid layer on the surface of the glass substrate.

[0077] Step S300: Anti-fingerprint liquid spraying: Under the conditions of temperature 23°C ± 2°C and relative humidity 55% ± 5%, spray the anti-fingerprint liquid DH320LF at an amount of 10g / ㎡ to 20g / ㎡ onto the surface of the fluorinated liquid, dry the surface for 2min to 4min, and then cure at 120°C to 160°C for 20min to 30min to form an anti-fingerprint liquid layer on the surface of the fluorinated liquid layer.

[0078] The performance parameters of the panel 10 after the fluorinated liquid layer 12 and the anti-fingerprint liquid layer 13 are provided on the glass substrate 11 and the performance parameters of the ordinary glass panel are shown in Table 1 below.

[0079] Table 1

[0080] category Ordinary glass panel Panel of this application Surface free energy 30-35mN / m 8-10mN / m Water drop contact angle 50-60° 100-120° Easy to clean generally Easy to clean Easy to clean life none 3 years

[0081] It can be seen from Table 1 above that by setting the fluorinated liquid layer 12 and the anti-fingerprint liquid layer 13 on the glass substrate 11, the surface free energy of the panel 10 of the present application is smaller and the water droplet contact angle is larger, indicating that the panel 10 of the present application has better hydrophobicity and oleophobicity. In addition, compared with ordinary glass panels, the panel 10 of the present application is easy to clean and has a longer service life.

[0082] Different ratios between the fluorinated liquid content and the anti-fingerprint liquid content result in different performances of the panel 10 formed in the end. The present application prepares samples through the following different ratios and conducts reliability tests on each panel 10 sample under the same conditions.

[0083] Embodiment 1: 80% fluorinated liquid + 20% anti-fingerprint liquid.

[0084] Embodiment 2: 70% fluorinated liquid + 30% anti-fingerprint liquid.

[0085] Embodiment 3: 60% fluorinated liquid + 40% anti-fingerprint liquid.

[0086] Embodiment 4: 50% fluorinated liquid + 50% anti-fingerprint liquid.

[0087] Embodiment 5: 40% fluorinated liquid + 60% anti-fingerprint liquid.

[0088] Among them, the content of fluorinated liquid in Example 1 accounts for the largest proportion, and the content of anti-fingerprint liquid in Example 5 accounts for the largest proportion.

[0089] The test samples of Examples 1 to 5 were subjected to reliability tests under the same conditions, and the test method was as follows:

[0090] (1) Friction resistance test: Use 0000# steel wool, with a force of 10N, a stroke of 40mm, 40 times / min, and wipe 2000 times in total.

[0091] (2) Acid resistance test: Use 10% acetic acid solution to corrode the coating surface at room temperature for 24 hours, then rinse it with clean water.

[0092] (3) Alkali resistance test: Use 5% sodium carbonate solution to corrode the coating surface at room temperature for 24 hours, then rinse it with clean water.

[0093] (4) High temperature resistance test: Place the sample in a 200°C environment for 8 hours, take it out, cool it for 60 minutes, and rinse it with clean water.

[0094] The water drop contact angle results after the reliability test and the initial water drop contact angle are shown in Table 2 below.

[0095] Table 2

[0096] sample Initial water drop contact angle After friction Acid resistance After alkali resistance After high temperature Embodiment 1 80°-90° 75°-85° 75°-85° 75°-85° 75°-85° Embodiment 2 90°-95° 80°-85° 80°-85° 80°-85° 80°-85° Embodiment 3 105°-115° 85°-100° 85°-100° 85°-100° 85°-100° Embodiment 4 115°-120° 75°-85° 75°-85° 75°-85° 75°-85° Embodiment 5 >120° 60°-70° 60°-70° 60°-70° 60°-70°

[0097] It can be seen from Table 2 above that the greater the proportion of the anti-fingerprint liquid, the greater the initial water drop contact angle. However, as the proportion of the fluorinated liquid decreases, the adhesion of the fluorinated liquid and the anti-fingerprint liquid on the glass substrate 11 becomes weaker. After the reliability test, the damage to the anti-fingerprint liquid layer 13 becomes more serious, and the water drop contact angle shows a rapid downward trend.

[0098] After comprehensive consideration, when the anti-fingerprint liquid content is designed to be 35% to 45% and the fluorinated liquid content is designed to be 55% to 65%, it can not only ensure an excellent initial water droplet contact angle, have good anti-fingerprint and anti-fouling effects, but also maintain good coating integrity after reliability testing and still be easy to clean.

[0099] In some embodiments, the thickness of the fluorinated liquid layer 12 is in the range of 6 μm to 12 μm.

[0100] The thickness of the fluorinated liquid layer 12 has an important influence on the performance of the panel 10. If the thickness of the fluorinated liquid layer 12 is too small, its adhesion on the glass substrate 11 will be weaker, and it will not have a good bonding effect. Moreover, after the reliability test, the fluorinated liquid layer 12 and the anti-fingerprint liquid layer 13 will be more seriously damaged. If the thickness of the fluorinated liquid layer 12 is too large, it may cause the transparency of the surface of the glass substrate 11 to decrease, affecting the appearance and texture of the glass substrate 11, while wasting raw materials and increasing costs.

[0101] The thickness of the fluorinated liquid layer 12 is set in the range of 6 μm to 12 μm. On the basis of maintaining good adhesion and reliability, the appearance of the panel 10 can be guaranteed and the resource utilization efficiency can be improved.

[0102] It can be understood that the thickness range of the fluorinated liquid layer 12 is 6 μm to 12 μm, which is the thickness of the layer body 121 . The thickness of the fluorinated liquid layer 12 in the recess 111 can be set according to the depth of the recess 111 , and this embodiment does not specifically limit this.

[0103] For example, the size of the recessed portion 111 can be set as needed, the depth of the recessed portion 111 can be less than the thickness of the fluorinated liquid layer 12, and the opening size of the recessed portion 111 can be greater than or equal to the depth size of the recessed portion 111. Of course, the opening size of the recessed portion 111 can also be less than the depth size of the recessed portion 111, and this embodiment does not specifically limit this.

[0104] In some embodiments, the thickness of the anti-fingerprint liquid layer 13 is in the range of 4 μm to 8 μm.

[0105] The thickness of the anti-fingerprint liquid layer 13 has an important impact on the performance of the panel 10. If the thickness of the anti-fingerprint liquid layer 13 is too small, it may not provide sufficient anti-fingerprint performance, resulting in fingerprints and stains being more likely to remain on the surface. In addition, it may also cause the durability of the anti-fingerprint liquid layer 13 to decrease, making it susceptible to wear and scratches. If the thickness of the anti-fingerprint liquid layer 13 is too large, it may affect the touch of the surface of the glass substrate 11, reduce the transparency of the glass, and affect the user experience.

[0106] The thickness of the anti-fingerprint liquid layer 13 is set to 4 μm to 8 μm, which can maintain good anti-fingerprint and anti-oil effects while ensuring the appearance of the panel 10 and improving resource utilization efficiency.

[0107] refer to Fig. 9 In some embodiments, the surface of the glass substrate 11 includes a first supporting surface 112, which is usually used to place objects. The first supporting surface 112 is perpendicular to the thickness direction of the glass substrate 11, and at least part of the multiple recessed portions 111 is arranged on the first supporting surface 112, that is, part of the multiple recessed portions 111 is arranged on the first supporting surface 112, or all of the multiple recessed portions 111 are arranged on the first supporting surface 112.

[0108] At least part of the fluorinated liquid layer 12 is disposed on the first supporting surface 112, that is, part of the fluorinated liquid layer 12 is disposed on the first supporting surface 112, and at this time, part of the fluorinated liquid layer 12 is filled in the multiple recessed portions 111, or, the fluorinated liquid layer 12 is completely disposed on the first supporting surface 112, and at this time, the fluorinated liquid layer 12 can be partially filled in the multiple recessed portions 111, or can be completely filled in the multiple recessed portions 111, and the fluorinated liquid layer 12 is connected to the first supporting surface 112.

[0109] In this way, a strong hydrophobic and oleophobic coating can be formed on the first supporting surface 112, so that the first supporting surface 112 is not easy to adhere to oil stains and fingerprints, and can be kept easy to clean at any time. In addition, after the hydrophobic and oleophobic coating is located outside the multiple recessed parts 111, the first supporting surface 112 still retains the fluorinated liquid layer 12 filled in the multiple recessed parts 111, thereby reducing the contact area between oil stains and fingerprints and the first supporting surface 112, achieving the effect of anti-fingerprint and anti-oil stain.

[0110] In some embodiments, the first supporting surface 112 is parallel to the fluorinated liquid layer 12 .

[0111] refer to Fig.10In some embodiments, the fluorinated liquid layer 12 includes a plurality of protrusions 122 and a connecting portion 123 connecting two adjacent protrusions 122, the plurality of protrusions 122 cooperate with the plurality of recesses 111, and the protrusions 122 do not fill the corresponding recesses 111, and the distances between the surface of the fluorinated liquid layer 12 away from the glass substrate 11 and the surface facing the glass substrate 11 are equal at all locations.

[0112] refer to Fig.11 In some embodiments, the edge of the first supporting surface 112 coincides with the projection of the side edge of the fluorinated liquid layer 12 in the thickness direction of the glass substrate 11, that is, the fluorinated liquid layer 12 covers the entire first supporting surface 112. In this way, it can be ensured that the entire first supporting surface 112 has good anti-fingerprint and anti-oil effects.

[0113] refer to Fig.12 In some embodiments, the surface of the glass substrate 11 includes a first decorative surface 113 in addition to the first supporting surface 112. The first decorative surface 113 is disposed on the peripheral wall of the glass substrate 11 and connected to the edge of the first supporting surface 112. A plurality of recessed portions 111 are disposed on the first supporting surface 112 and the first decorative surface 113. The fluorinated liquid layer 12 is disposed on the first supporting surface 112 and the first decorative surface 113 and connected to the first supporting surface 112 and the first decorative surface 113.

[0114] The first decorative surface 113 is the side surface of the edge of the glass substrate 11 . When water or oil flows on the first supporting surface 112 , it may drip along the first decorative surface 113 . In addition, users cannot avoid touching the first decorative surface 113 , thereby leaving fingerprints on the first decorative surface 113 .

[0115] In this way, by providing the fluorinated liquid layer 12 and the anti-fingerprint liquid layer 13 on both the first supporting surface 112 and the first decorative surface 113, fingerprint residue can be prevented more comprehensively and the first supporting surface 112 and the first decorative surface 113 can be kept easy to clean, so that the entire panel 10 has good anti-fingerprint and anti-oil effects, thereby improving the user experience.

[0116] refer to Fig.13 In some embodiments, there are multiple first decorative surfaces 113, and the planes where at least two first decorative surfaces 113 are located are parallel.

[0117] Of course, the planes where at least two first decorative surfaces 113 are located may also intersect.

[0118] Taking the glass substrate 11 as a rectangular parallelepiped as an example, some users' glass substrates 11 are against the wall on three sides, which involves one first decorative surface 113; some users' glass substrates 11 are against the wall on two sides, which involves two first decorative surfaces 113; some users' glass substrates 11 are not set against the wall, which involves four first decorative surfaces 113. The fluoride liquid layer 12 and the anti-fingerprint liquid layer 13 can be set on one or more first decorative surfaces 113 as needed.

[0119] When the two first decorative surfaces 113 are adjacent surfaces, the planes where the two first decorative surfaces 113 are located intersect; when the two first decorative surfaces 113 are opposite surfaces, the planes where the two first decorative surfaces 113 are located are parallel.

[0120] Of course, the shape of the glass substrate 11 can be set as needed. In addition to being a rectangular parallelepiped, it can also be an ellipse, a prism, etc., which is not specifically limited in this embodiment.

[0121] refer to Fig.14 In some embodiments, the surface of the glass substrate 11 includes, in addition to the first supporting surface 112, a second supporting surface 114 and a first decorative surface 113. The second supporting surface 114 and the first supporting surface 112 are spaced apart in the thickness direction of the glass substrate 11, the first decorative surface 113 is located on the outer peripheral side of the first supporting surface 112, and two opposite sides of the first decorative surface 113 in the thickness direction of the glass substrate 11 are connected to the edges of the first supporting surface 112 and the second supporting surface 114, respectively.

[0122] That is, there is a height difference between the first supporting surface 112 and the second supporting surface 114 , and the first decorative surface 113 is located between the first supporting surface 112 and the second supporting surface 114 , and respectively connects the first supporting surface 112 and the second supporting surface 114 .

[0123] Exemplarily, the first supporting surface 112 may be located above the second supporting surface 114 . Of course, the first supporting surface 112 may also be located below the second supporting surface 114 .

[0124] The first decorative surface 113 and the second supporting surface 114 are both located at the edge of the glass substrate 11 , and the first supporting surface 112 , the first decorative surface 113 and the second supporting surface 114 may form a step shape.

[0125] The plane where the first support surface 112 is located is parallel to the plane where the second support surface 114 is located, and the fluorinated liquid layer 12 is disposed on the first support surface 112, the first decorative surface 113 and the second support surface 114, and is connected to the first support surface 112, the first decorative surface 113 and the second support surface 114. Of course, the plane where the first support surface 112 is located and the plane where the second support surface 114 is located may also intersect.

[0126] In this way, by providing the fluorinated liquid layer 12 and the anti-fingerprint liquid layer 13 on the first supporting surface 112, the first decorative surface 113 and the second supporting surface 114, fingerprint residue can be prevented more comprehensively and the first supporting surface 112, the first decorative surface 113 and the second supporting surface 114 can be kept easy to clean, so that the entire panel 10 has good anti-fingerprint and anti-oil effects, thereby improving the user experience.

[0127] refer to Fig.15 In some other embodiments, the second supporting surface 114 and the first decorative surface 113 are both provided with multiple planes, at least two planes where the first decorative surfaces 113 are located are parallel or intersecting, and at least two planes where the second supporting surfaces 114 are located are also parallel or intersecting.

[0128] The first decorative surface 113 may be perpendicular to the first supporting surface 112, or may not be perpendicular to the first supporting surface 112. Similarly, the first decorative surface 113 may be perpendicular to the second supporting surface 114, or may not be perpendicular to the second supporting surface 114.

[0129] refer to Fig.16 In some other possible embodiments, the surface of the glass substrate 11 includes, in addition to the first supporting surface 112, the first decorative surface 113 and the second supporting surface 114, a second decorative surface 115. The second decorative surface 115 is located on the outer peripheral side of the second supporting surface 114 and is connected to the edge of the second supporting surface 114. The plane where the second supporting surface 114 is located intersects with the plane where the second supporting surface 114 is located.

[0130] The fluorinated liquid layer 12 is disposed on the first supporting surface 112 , the first decorative surface 113 , the second supporting surface 114 and the second decorative surface 115 , and is connected to the first supporting surface 112 , the first decorative surface 113 , the second supporting surface 114 and the second decorative surface 115 .

[0131] In this way, by providing the fluorinated liquid layer 12 and the anti-fingerprint liquid layer 13 on the first supporting surface 112, the first decorative surface 113, the second supporting surface 114 and the second decorative surface 115, fingerprint residue can be prevented more comprehensively and the first supporting surface 112, the first decorative surface 113, the second supporting surface 114 and the second decorative surface 115 can be kept easy to clean, so that the entire panel 10 has good anti-fingerprint and anti-oil effects, thereby improving the user experience.

[0132] refer to Fig.17 In some other embodiments, the second supporting surface 114, the first decorative surface 113 and the second decorative surface 115 are each provided in plurality.

[0133] Although the present application is described herein in conjunction with various embodiments, in the process of implementing the claimed application, those skilled in the art may understand and implement other changes to the disclosed embodiments by viewing the drawings, the disclosure, and the appended claims. In the claims, the word "comprising" does not exclude other components or steps, and "one" or "an" does not exclude multiple situations. A single processor or other unit may implement several functions listed in the claims. Certain measures are recorded in different dependent claims, but this does not mean that these measures cannot be combined to produce good results.

[0134] Although the present application has been described in conjunction with specific features and embodiments thereof, it is obvious that various modifications and combinations may be made thereto without departing from the spirit and scope of the present application. Accordingly, this specification and the drawings are merely exemplary illustrations of the present application as defined by the appended claims, and are deemed to have covered any and all modifications, variations, combinations or equivalents within the scope of the present application. Obviously, those skilled in the art may make various modifications and variations to the present application without departing from the spirit and scope of the present application. Thus, if these modifications and variations of the present application fall within the scope of the claims of the present application and their equivalents, the present application is also intended to include these modifications and variations.

[0135] The above is only a specific implementation of the utility model, but the protection scope of the utility model is not limited thereto. Any technician familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed by the utility model, which should be included in the protection scope of the utility model. Therefore, the protection scope of the utility model should be based on the protection scope of the claims.

Claims

1. A cooking appliance, characterized in that: The cooker comprises a panel, and the panel comprises: Glass substrate; A fluorinated liquid layer, wherein the fluorinated liquid layer is disposed on the surface of the glass substrate, and a side of the fluorinated liquid layer facing the glass substrate is connected to the glass substrate; an anti-fingerprint liquid layer, the anti-fingerprint liquid layer being disposed on a side of the fluorinated liquid layer away from the glass substrate and connected to the fluorinated liquid layer; A plurality of recessed portions are provided on a side of the glass substrate facing the fluoride liquid layer; At least a portion of the fluorinated liquid layer fills the plurality of recessed portions.

2. The cooker according to claim 1, characterized in that: The surface of the glass substrate comprises a first supporting surface, the first supporting surface is perpendicular to the thickness direction of the glass substrate, and at least part of the plurality of recessed portions is disposed on the first supporting surface; At least a portion of the fluorinated liquid layer is disposed on the first supporting surface and connected to the first supporting surface.

3. The cooker according to claim 2, characterized in that: The first supporting surface is parallel to the fluorinated liquid layer, and / or the edge of the first supporting surface coincides with the projection of the side edge of the fluorinated liquid layer in the thickness direction of the glass substrate.

4. The cooker according to claim 2, characterized in that: The surface of the glass substrate further includes a first decorative surface, which is disposed on the peripheral wall of the glass substrate and connected to the edge of the first supporting surface, and the plurality of recessed portions are disposed on the first supporting surface and the first decorative surface; The fluorinated liquid layer is disposed on the first supporting surface and the first decorative surface, and is connected to the first supporting surface and the first decorative surface.

5. The cooker according to claim 4, characterized in that: There are multiple first decorative surfaces, and planes where at least two of the first decorative surfaces are located are parallel or intersecting.

6. The cooker according to claim 2, characterized in that: The surface of the glass substrate further includes: a second supporting surface, the second supporting surface being spaced apart from the first supporting surface along a thickness direction of the glass substrate; A first decorative surface, located at the outer peripheral side of the first supporting surface, wherein two opposite sides of the first decorative surface in the thickness direction of the glass substrate are respectively connected to the edges of the first supporting surface and the second supporting surface; The plane where the first supporting surface is located is parallel to or intersects with the plane where the second supporting surface is located, and the fluorinated liquid layer is arranged on the first supporting surface, the first decorative surface and the second supporting surface, and is connected to the first supporting surface, the first decorative surface and the second supporting surface.

7. The cooker according to claim 1, characterized in that: The thickness of the fluorinated liquid layer ranges from 6 μm to 12 μm; and / or the thickness of the anti-fingerprint liquid layer ranges from 4 μm to 8 μm.

8. The cooker according to claim 1, characterized in that: The static water drop contact angle of the panel is greater than or equal to 100°.

9. The cooker according to any one of claims 1 to 8, characterized in that: The fluorinated liquid layer includes a layer body and a plurality of protrusions, wherein the plurality of protrusions are located on a side of the layer body facing the glass substrate, one of the protrusions fits in one of the recessed portions, and the layer body is connected to the anti-fingerprint liquid layer and the glass substrate.