Packaging structure capable of reducing thickness of flip-chip product

By using transparent protective glue and electroplating layers in flip chip packaging, the uneven flow of plastic sealing materials and the matching of frame semi-etching is solved, and the thinning packaging structure is achieved, the integration and operating efficiency are improved, and the product thickness is reduced. Directly check the packaging effect through transparent protective adhesive, improving product stability.

CN221947135UActive Publication Date: 2024-11-01JIANGSU SILICON INTEGRITY SEMICON TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202322628825.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-09-26
Publication Date
2024-11-01
Estimated Expiration
2033-09-26

AI Technical Summary

Technical Problem

In flip chip packaging, due to uneven flow of plastic seal material and matching of the semi-etched frame area, the product thickness increases, the integration decreases, and the internal cavity filling is not satisfactory, affecting product quality.

Method used

Use transparent protective glue instead of plastic sealing layer. By flipping the chip inverted and inverted, the protective glue is brushed or dipped on the frame, and cured at high temperature to fix the chip and frame, eliminating the plastic sealing process, thinning the packaging structure, and using electroplating. The layer is connected to other components.

Benefits of technology

It has achieved the reduction of production processes, improved product integration, facilitated internal abnormality checks, reduced product thickness, improved operating efficiency, and directly checked the packaging effect through transparent protective adhesives to improve product stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221947135U_ABST
    Figure CN221947135U_ABST
Patent Text Reader

Abstract

The utility model discloses a packaging structure for reducing the thickness of a flip-chip product, which comprises a chip, protective glue, bumps, a frame and an electroplated layer, the bottom of the chip is connected with the frame through the plurality of bumps, the protective glue covers the top of the frame and the chip, and the electroplated layer is arranged at the bottom of the frame. According to the packaging structure for thinning the thickness of the flip-chip product, a plastic packaging layer in the prior art is replaced by the protection glue, the overall thickness of the packaging structure is further reduced, and the packaging structure for thinning the thickness of the flip-chip product has the advantages that the production process is reduced, the integration level of the product is improved, internal abnormity of the product is conveniently checked, the operation efficiency is improved, and the thickness of the product is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of semiconductor packaging, and more specifically to a packaging structure for reducing the thickness of a flip-chip product. Background Art

[0002] With the continuous development of packaging technology integration, flip chip packaging products have greatly improved the integration of electronic devices. In recent years, the flip chip packaging structure has become a high-performance packaging interconnection method, and its application has been widely and rapidly developed. However, in flip chip packaging, there is a bump on the front of the chip. After the chip flips, the bump and the pin are bonded to form a space with a certain height. The plastic encapsulation product needs to cover the chip frame and other parts to form a certain height, which reduces the integration of the product. In addition, when the product is plastic encapsulated, the plastic encapsulation material flows unevenly between the chip and the frame. At the same time, the half-etched pins of the frame need to match the position of the bump on the chip, so there will be a large half-etched area on the frame as a whole. When the product is plastic encapsulated, there will also be problems such as insufficient filling of internal voids, which will cause various abnormalities in the package and affect product quality.

[0003] A process method for thinning the packaging structure of a flip-chip product is proposed. After the chip is flipped and mounted on a frame, a transparent protective glue is brushed or dipped on the entire surface. After the protective glue is cured, it can protect the product surface and fix the chip and the frame. The plastic sealing process is omitted, and the product can be protected and the operation of the product can be stabilized while reducing the overall thickness of the product. At the same time, the internal situation of the product can be directly checked through the transparent protective glue, and the product packaging effect can be tested. While improving the product integration, it is convenient to internally check for internal abnormalities of the product and improve operating efficiency. Utility Model Content

[0004] In order to solve the above problems, the purpose of the utility model is to provide a packaging structure for thinning flip-chip products, which reduces production processes, improves product integration, facilitates internal troubleshooting of product abnormalities, improves operating efficiency and reduces product thickness.

[0005] According to one aspect of the utility model, a packaging structure for reducing the thickness of a flip-chip product is provided, comprising: a chip, a protective glue, a bump, a frame, and an electroplating layer, wherein the bottom of the chip is connected to the frame via a plurality of bumps, the protective glue covers the top of the frame and the chip, and the bottom of the frame is provided with an electroplating layer. By using the protective glue to replace the plastic sealing layer in the prior art, the overall thickness of the packaging structure is reduced.

[0006] In some embodiments, the thickness of the frame is a minimum of 0.1 mm.

[0007] In some embodiments, the chip thickness is at least 70 um to 90 um.

[0008] In some embodiments, the height of the bump is at least 90 um.

[0009] In some embodiments, the thickness of the protective glue is 25um-50um.

[0010] In some embodiments, the protective glue is a mixture of one or more of epoxy resin, silicone, polyurethane, polyimide, and acrylic resin. Compared with plastic sealing materials, the protective glue has a lower filler content and a higher transparency coefficient, and has a better protective effect.

[0011] In some embodiments, the working temperature of the protective glue is less than 200 degrees Celsius.

[0012] In some embodiments, the electroplating layer is nickel-palladium-gold or tin, with a thickness of 0.531um-20um. The electroplating layer is used to facilitate connection with other components.

[0013] The utility model brushes or dips transparent protective glue on the entire surface of the chip after it is flipped and mounted on the frame. After the protective glue is cured, it can protect the product surface and fix the chip and the frame, and the plastic sealing process is omitted. It can protect the product and stabilize the operation of the product while reducing the overall thickness of the product. At the same time, the internal situation of the product can be directly checked through the transparent protective glue, and the product packaging effect can be tested. While improving the product integration, it is convenient to check the internal abnormality of the product and improve the operation efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 It is a schematic diagram of the structure of the packaging structure of the utility model for reducing the thickness of the flip-chip product;

[0015] Figure 2 It is a processing step diagram of the packaging structure of the utility model for reducing the thickness of the flip-chip product. DETAILED DESCRIPTION

[0016] The present invention is described in detail below in conjunction with the various embodiments shown in the accompanying drawings, but it should be noted that these embodiments are not limitations of the present invention, and any equivalent transformations or substitutions in functions, methods or structures made by ordinary technicians in the field based on these embodiments are all within the scope of protection of the present invention.

[0017] In the description of the present utility model, it should be noted that, unless otherwise specified and limited, the terms "installation", "connection" and "connection" should be understood in a broad sense. For example, it can be a mechanical connection or an electrical connection, or it can be the internal connection of two components. It can be a direct connection or an indirect connection through an intermediate medium. For ordinary technicians in this field, the specific meaning of the terms can be understood according to the specific circumstances.

[0018] like Figure 1 As shown, the packaging structure for reducing the thickness of flip-chip products described in the utility model includes: a chip 1, a protective glue 2, bumps 3, a frame 4 and an electroplating layer 5. The bottom of the chip 1 is connected to the frame 4 through a number of bumps 3. The protective glue 2 covers the top of the frame 4 and the chip 1. The bottom of the frame 4 is provided with an electroplating layer 5. By using the protective glue 2 to replace the plastic sealing layer in the prior art, the overall thickness of the packaging structure is reduced.

[0019] The thickness of the frame 4 is at least 0.1 mm.

[0020] The minimum thickness of chip 1 is 70um-90um.

[0021] The minimum height of the bump 3 is 90 um.

[0022] The thickness of the protective glue 2 is 25um-50um.

[0023] The protective glue 2 is a mixture of one or more of epoxy resin, silicone, polyurethane, polyimide, and acrylic resin. Compared with the plastic sealing material, the protective glue 2 has a low filler content and a high transparency coefficient, and has a better protective effect.

[0024] The thickness of the existing packaging technology is 0.37mm, 0.4mm, 0.45mm, 0.55mm, 0.75mm, 0.85mm, etc. Take the conventional product of 0.75mm as an example: the frame thickness is 0.203mm, the plastic packaging material thickness is 0.55mm, and the total product thickness is 0.75mm;

[0025] If protective glue 2 is used: the frame thickness is 0.203mm, the minimum thickness of chip 1 is 70um~90um, the bump height is 90um, the glue thickness can be controlled to 25~50um, and the maximum total product thickness is 0.433mm;

[0026] Compared with plastic packaging materials, protective glue 2 has a low filler content and a high transparency coefficient, and the total thickness of the product can be reduced by more than 42.2%.

[0027] The working temperature of the protective glue 2 is less than 200 degrees Celsius. Generally speaking, standard epoxy resin AB glue can reach a temperature resistance range of about 150°C to 200°C at high temperatures. However, some specially formulated epoxy resins may have higher temperature resistance and can withstand higher temperatures, even exceeding 200°C. Such working temperatures can safely meet the working temperatures of the usage scenarios.

[0028] The electroplating layer 5 is nickel-palladium-gold or tin, with a thickness of 0.531um-20um. The electroplating layer 5 is used to facilitate connection with other components.

[0029] like Figure 2As shown, the processing of the packaging structure for thinning the thickness of the flip-chip product includes the following steps:

[0030] S1: After the chip 1 on the incoming wafer is diced, a single chip 1 is taken out and flipped upside down on the frame;

[0031] S2: brush or dip a layer of transparent protective glue 2 on the entire surface of the product with the chip 1 installed, and solidify the protective glue 2 by baking once, so that the protective glue 2 fixes the chip 1 and the frame;

[0032] S3: The product is reflowed at high temperature to stabilize the connection between the chip 1 bump and the frame, while the protective glue 2 is softened and cooled for secondary curing;

[0033] S4: The back of the product is electroplated to form an electroplating layer 5. The electroplated product is cut into individual pieces to form an independent single-piece packaging structure, which can be used for welding on a PCB board.

[0034] The above are only some embodiments of the present invention. It should be pointed out that for ordinary technicians in this field, other modifications and improvements can be made without departing from the creative concept of the present invention, which all belong to the protection scope of the present invention.

Claims

1. A packaging structure with reduced thickness of flip-chip products, characterized in that: include: A chip, protective glue, bumps, a frame and an electroplating layer, wherein the bottom of the chip is connected to the frame via a plurality of bumps, the protective glue covers the top of the frame and the chip, and an electroplating layer is provided at the bottom of the frame; the protective glue is one of epoxy resin, silicone, polyurethane, polyimide and acrylic resin; the electroplating layer is nickel palladium gold or tin, with a thickness of 0.531um.

2. The packaging structure for reducing the thickness of flip-chip products according to claim 1, characterized in that: The thickness of the frame is at least 0.1 mm.

3. The packaging structure for reducing the thickness of flip-chip products according to claim 2, characterized in that: The minimum thickness of the chip is 70um-90um.

4. The packaging structure for reducing the thickness of flip-chip products according to claim 2, characterized in that: The minimum height of the bump is 90 um.

5. The packaging structure for reducing the thickness of flip-chip products according to claim 4, characterized in that: The thickness of the protective glue is 25um-50um.

6. The packaging structure for reducing the thickness of flip-chip products according to claim 1, characterized in that: The working temperature of the protective glue is less than 200 degrees Celsius.