Double-sided passivation contact crystalline silicon solar cell

By using local passivation contact areas on both the front and back of the crystalline silicon solar cell and connecting the electrode units with transparent conductive electrodes, the problems of low conversion efficiency and optical parasitic absorption of doped polycrystalline silicon are solved, and high-efficiency photoelectricity is achieved Convert and low cost production.

CN221994479UActive Publication Date: 2024-11-12JIANGSU YIJING OPTOELECTRONICS TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420600832.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-27
Publication Date
2024-11-12
Estimated Expiration
2034-03-27

AI Technical Summary

Technical Problem

The existing TOPCon passivation contact crystalline silicon solar cells have low back conversion efficiency in the double-sided structure, and cannot fully exert the double-sided power generation characteristics. The optical parasitic absorption of doped polysilicon leads to high manufacturing costs, and the improvement of photoelectric conversion efficiency requires sacrificing optics. performance.

Method used

Local hole or electron passivation contact areas are used on the front and back of the battery, and the electrode units distributed in periodic dot matrix are connected through transparent conductive electrodes to avoid the entire surface passivation of the contact structure, reduce the electrode light shading rate, and improve the photoelectric conversion efficiency.

Benefits of technology

It realizes high-efficiency photoelectric conversion on both sides of the battery, reduces the light shading rate of the electrode, significantly improves the photoelectric conversion efficiency and production cost, and is suitable for industrial applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221994479U_ABST
    Figure CN221994479U_ABST
Patent Text Reader

Abstract

The utility model provides a double-sided passivation contact crystalline silicon solar cell, which is characterized in that doped p-n junctions or high-low junctions are adopted in non-electrode contact areas on the front surface and the back surface of the cell, and local hole or electron passivation contact structures are adopted in electrode contact areas; the local hole or electron passivation contact region (and the electrode region) has a periodic lattice structure on two surfaces of the cell; and the electrode units which are distributed on the two surfaces of the cell in a dot matrix manner are connected through the transparent conductive electrode, so that the convergence of photon-generated carriers is realized. According to the utility model, the whole light receiving surface of the cell can be prevented from adopting a passivation contact structure, so that the defects of high optical parasitic absorption coefficient and high optical loss of doped (boron or phosphorus) polycrystalline silicon are overcome; and meanwhile, on the basis of keeping efficient photon-generated carrier extraction, transmission and collection, the electrode shading rate is greatly reduced, so that excellent photoelectric conversion efficiency can be realized on two surfaces of the cell, and efficient double-surface power generation can be realized in application.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the field of solar cells, and mainly provides a double-sided passivation contact crystalline silicon solar cell. Background Art

[0002] Photovoltaic power generation is green and environmentally friendly, can be sustainable, can solve the energy and environmental crisis of mankind, and has an important strategic position in the future energy development. The development of high-efficiency, low-cost solar cells is the key to promoting the stable and rapid development of the photovoltaic power generation industry. Among various types of solar cells, crystalline silicon solar cells (referred to as crystalline silicon cells) have the fastest development in research and application due to their high photoelectric conversion efficiency, stable performance and low manufacturing cost. The industrialization technology is the most mature and the market share is the highest. Crystalline silicon solar cells with passivated contact structure (referred to as passivated contact cells) can achieve extremely excellent surface passivation, selective passage of photogenerated carriers and one-dimensional efficient collection through tunneling silicon oxide and doped polycrystalline silicon, and have very high photoelectric conversion efficiency.

[0003] At present, TOPCon (Tunnel Oxide and Passivated Contact) passivated contact cells with n-type silicon as substrate have become popular in the industry. The n region of this type of cell is an electronic passivated contact region, and the p region still uses a boron-doped pn junction. For passivated contact cells with n-type silicon as substrate, the role of the hole passivated contact region in improving the photoelectric conversion efficiency is significantly higher than that of the electron passivated contact layer. Therefore, the current industrial TOPCon cells cannot give full play to the maximum advantages of passivated contact structure cells. The main reason that restricts the use of passivated contact structures on both sides of the cell is the high optical parasitic absorption coefficient of doped (boron or phosphorus) polycrystalline silicon, which will make the excellent electrical (passivation) performance improvement that can be obtained on the light-receiving side of the cell after the passivated contact structure is adopted at the expense of significantly sacrificing optical performance. Therefore, how to apply both hole and electron passivated contact technologies to crystalline silicon cells is the key to improving the photoelectric conversion efficiency of passivated contact cells and reducing their manufacturing costs. In addition, although the current industrial TOPCon cells are bifacial, the conversion efficiency on the back of the cells is not high and cannot give full play to their bifacial power generation characteristics. Therefore, improving the conversion efficiency on the back of the cells can enable the passivated contact cells to perform bifacial power generation more efficiently in applications and reduce the cost per kilowatt-hour. Utility Model Content

[0004] In order to solve the above problems, the utility model provides a double-sided passivated contact crystalline silicon solar cell (referred to as double-sided passivated contact cell), wherein the double-sided passivated contact cell adopts doped pn junctions or high-low junctions in the non-electrode contact areas on the front and back sides of the cell, and adopts a local hole (or electron) passivation contact structure in the electrode contact area; the local hole (or electron) passivation contact area (and the electrode area) have a periodic lattice distribution structure on both sides of the cell; and the electrode units with periodic lattice distribution in the metal electrode areas on the two sides of the cell are connected by transparent conductive electrodes to realize the convergence of photogenerated carriers. Based on the above-mentioned battery structure design, it is possible to avoid using a passivated contact structure on the entire light-receiving surface of the battery, thereby solving the disadvantages of high optical parasitic absorption coefficient and high optical loss of doped (boron or phosphorus) polycrystalline silicon, so that a passivated contact structure can be used on both sides of the battery; it is also possible to greatly reduce the electrode shading rate while maintaining efficient photogenerated carrier extraction, transmission and collection, and significantly increase the area ratio of the battery that receives photons, thereby achieving excellent photoelectric conversion efficiency on both sides of the battery, and achieving efficient double-sided power generation in applications.

[0005] The technical solution of the utility model is as follows:

[0006] The utility model discloses a double-sided passivation contact crystalline silicon solar cell, comprising a silicon substrate;

[0007] A local hole passivation contact region is formed on the first surface of the silicon substrate, wherein the local hole passivation contact region has a plurality of hole passivation contact units distributed in a periodic lattice;

[0008] A pn junction or a high-low junction using acceptor doping formed on the first surface of the silicon substrate and arranged staggered with the local hole passivation contact area;

[0009] A first passivation layer for passivating the first surface of the silicon substrate;

[0010] A first metal electrode formed on the first surface of the silicon substrate, the first metal electrode having a plurality of first electrode units distributed in a periodic lattice, the first electrode units being arranged correspondingly to the hole passivation contact units;

[0011] A local electronic passivation contact region is formed on the second surface of the silicon substrate, wherein the local electronic passivation contact region has a plurality of electronic passivation contact units distributed in a periodic lattice;

[0012] A donor-doped pn junction or a high-low junction formed on the second surface of the silicon substrate and arranged staggered with the local electronic passivation contact region;

[0013] A second passivation layer for passivating the second surface of the silicon substrate;

[0014] A second metal electrode is formed on the second surface of the silicon substrate, wherein the second metal electrode has a plurality of second electrode units distributed in a periodic lattice, and the second electrode units are arranged correspondingly to the hole passivation contact units.

[0015] Optionally, the first electrode unit coincides with the geometric center of the hole passivation contact unit, and the outer contour is less than or equal to the outer contour of the hole passivation contact unit; the second electrode unit coincides with the geometric center of the electron passivation contact unit, and the outer contour is less than or equal to the outer contour of the electron passivation contact unit.

[0016] Optionally, the local hole passivation contact region is composed of tunneling silicon oxide and boron-doped or gallium-doped polysilicon; the local electron passivation contact region is composed of tunneling silicon oxide and phosphorus-doped polysilicon; the tunneling silicon oxide has a thickness of 1.2-1.6nm and a refractive index of 1.45-1.5; the boron-doped or gallium-doped polysilicon has a thickness of 5-500nm; and the phosphorus-doped polysilicon has a thickness of 5-500nm.

[0017] Optionally, the shape of the hole passivation contact unit is any one of circular, rectangular, diamond, and elliptical; the arrangement period of the hole passivation contact unit is 100-5000 microns; the area percentage of the local hole passivation contact area is 0.05%-2.5%; the shape of the electron passivation contact unit is any one of circular, rectangular, diamond, and elliptical; the arrangement period of the electron passivation contact unit is 100-5000 microns; the area percentage of the local electron passivation contact area is 0.05%-2.5%.

[0018] Optionally, the shapes of the first electrode unit and the second electrode unit are respectively the same as the hole passivation contact unit and the electron passivation contact unit.

[0019] Optionally, the shading rate of the first metal electrode and the second metal electrode is 0.05%-0.75%.

[0020] Optionally, the first passivation layer and the second passivation layer are both silicon nitride; the thickness of the silicon nitride is 70-80 nm, and the refractive index is 1.9-2.1.

[0021] Optionally, the double-sided passivated contact crystalline silicon solar cell also includes a transparent conductive electrode, which is used to connect the first electrode unit in the first metal electrode and the second electrode unit in the second metal electrode; the transparent conductive electrode is a gate line type, and its axis line coincides with the line connecting the center point of the electrode unit in the y direction or the x direction.

[0022] Optionally, the light transmittance of the transparent conductive electrode is not less than 90%; the material of the transparent conductive electrode is silver nanowire, copper nanowire, transparent conductive oxide, or the transparent conductive electrode is a transparent conductive electrode based on graphene and carbon nanotubes.

[0023] Optionally, a transparent conductive electrode is provided in each column of the first metal electrode in the y direction; a transparent conductive electrode is provided in each column of the second metal electrode in the y direction; a transparent conductive electrode is provided in every M rows of the first metal electrode in the x direction; a transparent conductive electrode is provided in every M rows of the second metal electrode in the x direction; M is a natural number greater than 1.

[0024] The utility model has the following beneficial effects:

[0025] (1) The double-sided passivated contact crystalline silicon solar cell provided by the present invention can obtain high photoelectric conversion efficiency on the front and back sides of the cell based on the following cell structure design, and can realize efficient double-sided power generation.

[0026] By using a periodic lattice-distributed local hole (or electron) passivation contact structure (typically, the area ratio of the local hole or electron passivation contact area is less than 1%) in the electrode contact area on the front and back of the battery, it is possible to avoid using a passivation contact structure on the entire light-receiving surface of the battery, thereby solving the drawbacks of high optical parasitic absorption coefficient and high optical loss of doped (boron or phosphorus) polycrystalline silicon, so that both sides of the battery can use a passivation contact structure. On this basis, on the two sides of the battery, the photogenerated carriers are guided out through the corresponding periodic lattice-distributed electrode units, and these lattice-distributed electrode units are connected by transparent conductive electrodes, thereby realizing the convergence of photogenerated carriers. Through optimized design, the electrode shading rate can be greatly reduced (typically less than 0.2%), and the area ratio of the battery receiving photons can be significantly increased. The above is the optical basis for the battery to achieve high double-sided photoelectric conversion efficiency.

[0027] Doped pn junctions or high-low junctions are used in the non-electrode contact area on the front or back of the battery, local hole (or electron) passivation contact structure is used in the electrode contact area, and transparent conductive electrodes are used to connect these dot-matrix distributed electrode units. Through optimized design, efficient and low-loss photogenerated carrier extraction, transmission and collection can be achieved, which is the electrical basis for achieving high double-sided photoelectric conversion efficiency.

[0028] Because the front and back sides of the battery use similar structural designs, both the front and back sides of the battery can achieve high photoelectric conversion efficiency, which is the basis for achieving bifacial and high-efficiency photovoltaic power generation.

[0029] (2) The double-sided passivated contact crystalline silicon solar cell can use a transparent conductive electrode based on copper nanowires, which can greatly save the amount of silver used in the cell metallization and significantly reduce the cell production cost.

[0030] (3) The double-sided passivated contact crystalline silicon solar cell has a simple structure and a simple preparation method, can achieve high photoelectric conversion efficiency, has low production cost, and is very suitable for industrialization. In application, it can perform efficient double-sided photovoltaic power generation, and has a wide range of flexible application scenarios: including distributed photovoltaics, ground power stations, and building photovoltaics. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Figure 1 .Structural schematic diagram of the double-sided passivated contact crystalline silicon solar cell. In practical applications, both the front and back sides of the cell can receive solar photons, and generate electricity efficiently on both sides.

[0032] Among them, 1 is an n-type or p-type single crystal silicon substrate, 2 is a boron-doped junction, and 3 is a phosphorus-doped junction. 4 is a tunneling silicon oxide, 5 is a boron-doped polysilicon, and 6 is a phosphorus-doped polysilicon; 4 and 5 form a local hole passivation contact area, and 4 and 6 form a local electron passivation contact area. 7 is the silicon nitride on the front of the battery, 8 is the silicon nitride on the back of the battery, 9 is the electrode corresponding to the local hole passivation contact area on the front of the battery, and 10 is the electrode corresponding to the local electron passivation contact area on the back of the battery.

[0033] Figure 2 The electrode units of the double-sided passivated contact crystalline silicon solar cell are periodically distributed on the front (or back) side, and are connected by transparent conductive electrodes to achieve the convergence of photogenerated carriers. The cell area directly below the transparent conductive electrode can still receive photons for photovoltaic power generation.

[0034] Among them, 1 is one side of the battery; 2 is the local hole (or electron) passivation contact area; 3 is the electrode (shading) corresponding to the local hole (or electron) passivation contact area; 4 is the transparent conductive electrode in the y direction, connecting the electrode units, and there is a transparent conductive electrode for connection on each y column where the electrode unit is located; 5 is the transparent conductive electrode in the x direction, connecting the electrode units, and here the 4 y values ​​corresponding to the y-division into three equal parts are connected in the x direction to enhance the convergence. DETAILED DESCRIPTION

[0035] In order to better understand the utility model, the utility model will be further described below in conjunction with specific embodiments and drawings. Obviously, the embodiments described are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0036] The utility model provides a double-sided passivated contact crystalline silicon solar cell, which has the following characteristics:

[0037] The substrate material used in the double-sided passivated contact cell is silicon material (referred to as silicon substrate or silicon wafer), and single crystal silicon or polycrystalline silicon can be selected, and the substrate doping type can be n-type (phosphorus-doped) or p-type (boron-doped or gallium-doped).

[0038] For one side of the battery (either the front or the back), the non-electrode contact area adopts a pn junction or a high-low junction (p + -p), and its electrode contact area adopts a hole passivation contact structure (referred to as a local hole passivation contact area). The local hole passivation contact area is composed of tunneling silicon oxide and boron-doped polysilicon. The thickness of the tunneling silicon oxide is 1.2-1.6nm, and the refractive index is 1.45-1.5; the thickness of the boron-doped polysilicon is 5-500nm.

[0039] For the other side of the battery (back or front), its non-metallic electrode contact area adopts a donor (mainly phosphorus) doped pn junction or high-low junction (n + -n), and its electrode contact area adopts an electronic passivation contact structure (referred to as a local electronic passivation contact area). The local electronic passivation contact area is composed of tunneling silicon oxide and phosphorus-doped polysilicon. The thickness of the tunneling silicon oxide is 1.2-1.6nm, and the refractive index is 1.45-1.5; the thickness of the phosphorus-doped polysilicon is 5-500nm.

[0040] The pattern design of the local hole passivation contact region or the local electron passivation contact region (collectively referred to as the local passivation contact region) is as follows:

[0041] 1) A minimum graphic unit with periodic distribution, and the minimum graphic unit is arranged in a periodic lattice distribution form on the front or back of the battery. The specific lattice distribution pattern is not limited, and typically can be in the form of a rectangle or a diamond. Among them, the minimum graphic unit of the local hole passivation contact area is referred to as a hole passivation contact unit, and the minimum graphic unit of the local electron passivation contact area is referred to as an electron passivation contact unit, and the two are collectively referred to as passivation contact units.

[0042] 2) The shape of the smallest unit pattern is not limited, and can be a circle, rectangle, diamond, ellipse, etc. The size of the smallest unit pattern, that is, its diameter, side length, or the length of the major and minor axes of the ellipse, etc., is not limited; typically, taking a circle as an example, its diameter is 5-500 microns; taking a square as an example, its side length is 5-500 microns.

[0043] 3) The spacing (i.e., period) between the center points of each adjacent minimum unit pattern is 100-5000 microns.

[0044] 4) The percentage of the total area of ​​the hole passivation contact unit or the electron passivation contact unit to the front area of ​​the battery is referred to as the local passivation contact area area percentage. Generally, the local passivation contact area area percentage is between 0.05% and 2.5% (inclusive), and typically less than 1%. Due to the high optical parasitic absorption coefficient of doped polysilicon, this value is a direct reflection of the area with poor optical performance of the battery.

[0045] Both sides of the double-sided passivated contact cell have a layer of silicon nitride as an anti-reflection film with a thickness of 70-80nm and a refractive index of 1.9-2.1.

[0046] The front and back sides of the double-sided passivated contact battery have corresponding electrode units (i.e., the smallest graphic unit of the electrode) arranged directly above each passivated contact unit, and both have the same geometric center. From a horizontal perspective, the graphic area of ​​each electrode unit cannot exceed the area of ​​its corresponding local passivated contact unit.

[0047] The shape of the electrode unit can be designed to be the same as or different from the shape of the corresponding passivation contact unit. Generally, they are selected to be the same in shape; based on this, it is only necessary to design the size of the electrode unit to be smaller than or equal to the size of the corresponding passivation contact unit, that is, the outer contour of the electrode unit should be smaller than or equal to the outer contour of the corresponding electron passivation contact unit or hole passivation contact unit.

[0048] For the electrodes corresponding to the local passivation contact area, generally, they are light-shielding from the material selection, so the area percentage of such electrodes is the electrode light-shielding rate of the battery. Generally, the electrode light-shielding rate is between 0.05% and 0.75% (inclusive), and typically less than 0.2%.

[0049] For the front and back sides of the double-sided passivated contact cell, transparent conductive electrodes are used to connect the electrode units distributed in the dot matrix on each side to achieve the convergence of photogenerated carriers, such as Figure 2 As shown. The pattern of the transparent conductive electrode is a grid line type, and its axis line coincides with the line connecting the center point of the electrode unit in the y direction or the x direction. The transparent conductive electrode needs to have high transmittance while having good conductivity (to ensure efficient transmission and collection of photogenerated carriers). Generally, the transmittance exceeds 90%. Therefore, the battery area directly below the transparent conductive electrode can still receive solar photons for photovoltaic power generation.

[0050] For the design of a technical solution for connecting a transparent conductive electrode to an electrode unit directly above a passivation contact unit (hereinafter referred to as a transparent conductive electrode connection solution), as follows Figure 2 As shown ( Figure 2A typical representative solution is given in the specific embodiments below), there can be many different types of design solutions for the transparent conductive electrode connection methods in the x and y directions including the horizontal plane, as well as the transparent conductive electrode line width and aspect ratio, which need to be designed in conjunction with the battery structure parameters and the silicon wafer size, without specific limitation.

[0051] The material selection of the transparent conductive electrode is not limited, and silver nanowires or copper nanowires, transparent conductive oxides (TCO), or transparent conductive electrodes based on graphene and carbon nanotubes can be used. Preferably, nano silver wires or nano copper wires with higher transmittance, conductivity and aspect ratio and lower cost can be used. In particular, copper nanowires can greatly save the amount of silver used in battery metallization and significantly reduce the cost of battery production.

[0052] Combination Figure 1 and Figure 2 As shown, in a specific embodiment, for the front side of the battery, the hole passivation contact unit is a square with a side length of 90μm; the corresponding electrode unit is also a square with a side length of 40μm. These square minimum area units are distributed in a periodic square lattice, and the spacing between the center points of adjacent minimum units (whether in the x direction or the y direction) is 1250μm. Therefore, the area percentage of the local hole passivation contact area on the front side of the battery is 0.51%, and the electrode shading rate is 0.10%.

[0053] For the back of the battery, the electronic passivation contact unit is a square with a side length of 90μm; the corresponding electrode unit is also a square with a side length of 40μm. These square minimum area units are distributed in a periodic square lattice, and the spacing between the center points of adjacent minimum units (whether in the x direction or the y direction) is 1250μm. Therefore, the area percentage of the local electronic passivation contact area on the back of the battery is 0.51%, and the electrode shading rate is 0.10%.

[0054] The transparent conductive electrode connection scheme on both sides of the battery, such as Figure 2 shown.

[0055] a) On each y column where an electrode unit is located, there is a transparent conductive electrode for connecting the electrode units.

[0056] b) In the x-direction, after dividing the y-direction into three equal parts, one transparent conductive electrode is used to connect the corresponding four y-values ​​in the x-direction. One of the functions of the four transparent conductive electrodes in the x-direction is to enhance the convergence of the collected photogenerated carriers; the second function is to facilitate the subsequent assembly packaging through the technology of shingling combined with small-chip cells, so as to continue to maintain the high-performance optical advantages of the double-sided passivated contact crystalline silicon cells in the components. It should be noted that the four transparent conductive electrodes designed in the x-direction are a comprehensive optimization design based on the battery structure parameters and silicon wafer size. For different battery structure parameters and silicon wafer sizes, the number of transparent conductive electrodes in the x-direction can be flexibly designed.

[0057] Furthermore, the double-sided passivated contact crystalline silicon solar cell disclosed in the embodiment can be prepared by conventional technology, and an example is given as follows:

[0058] Step 1. Select a 182mm*182mm n-type single crystal silicon wafer with a bulk resistivity of 1Ω·cm.

[0059] Step 2. First, use sodium hydroxide solution to polish and etch the n-type silicon wafer to remove the damaged layer on the surface of the silicon wafer. Then, use sodium hydroxide solution combined with a single-sided water-floating wet etching method to perform single-sided texturing on one side of the silicon wafer to form a random pyramid-shaped velvet surface. The surface where this velvet surface is located is defined as the front side of the battery, which will be subsequently doped with boron; accordingly, the other polished surface is defined as the back side of the battery, which will be subsequently doped with phosphorus; it should be noted here that in the subsequent battery preparation process, the back side of the battery will also be texturized at an appropriate step.

[0060] Step 3. Use thermal oxidation technology to prepare tunneling silicon oxide on the front side of the silicon wafer. The thickness is 1.3 nm and the refractive index is 1.46.

[0061] Step 4. Use LPCVD to prepare intrinsic amorphous silicon on the front of the battery with a thickness of 100nm. The LPCVD intrinsic amorphous silicon plated on the back of the battery is very small, mainly produced in a very narrow range at the edge of the back, and this effect can be eliminated by wet chemical etching later.

[0062] Step 5. Use screen printing chemical etching slurry to etch away the intrinsic amorphous silicon and tunneling silicon oxide on the front side of the battery except for the local hole passivation contact design area. For example, Merck's Isishape BES etching slurry contains a certain concentration of phosphate, which can etch amorphous silicon and silicon oxide. After screen printing the slurry, heat it to 350-400℃ on a heating plate and let it stand for 1-2 minutes. The pattern of the screen printing screen is consistent with the design pattern of the local hole passivation contact area on the front of the battery given above. The intrinsic amorphous silicon and tunneling silicon oxide in the printed slurry area are etched away, and the velvet surface prepared on the front of the battery will not be damaged.

[0063] After this step, only the intrinsic amorphous silicon and tunneling silicon oxide in the local hole passivation contact design area are retained on the front of the battery, and the other areas are n-type silicon substrates with velvet morphology. Then, a 40-50°C hydrochloric acid solution combined with ultrasonic cleaning is used to clean the silicon wafer surface to remove the Merck etching slurry involved in the silicon wafer surface and obtain a clean surface.

[0064] Step 6. Use the masked ion implantation method to perform localized boron ion implantation in the non-local hole passivation contact design area and the local hole passivation contact design area on the front of the battery. The process mask pattern of the ion implantation is consistent with the design pattern of the local hole passivation contact area on the front of the battery given above. In the non-local hole passivation contact design area, the boron implantation energy is 5keV and the dose is 1.5·10 15 cm -2 In the local hole passivation contact design area, the boron implantation energy is 10 keV and the dose is 6·10 15 cm -2 The temperature of the silicon wafer substrate during ion implantation is room temperature 25°C.

[0065] Then, furnace tube thermal annealing is performed. During the annealing, the ion-implanted boron in the non-local hole passivation contact design area is activated and redistributed in silicon to form a boron-doped pn junction; the amorphous silicon in the local hole passivation contact design area is fully crystallized into polysilicon, and the ion-implanted boron also completes the impurity activation and redistribution in the polysilicon. The furnace tube annealing temperature is 980°C, the time is 30-40 minutes, and the nitrogen atmosphere.

[0066] After this step, the sheet resistance of the boron-doped junction in the non-local hole passivation contact area on the front side of the cell is 100-120Ω / □. The sheet resistance of the boron-doped polysilicon layer in the local hole passivation contact area is 80-100Ω / □.

[0067] Step 7. Use atmospheric pressure chemical vapor deposition (APCVD) to prepare a layer of silicon oxide on the front of the battery, with a thickness of 30-40nm and a refractive index of 1.46. Using chained in-line APCVD technology, this layer of silicon oxide is only prepared on the front of the battery and used as a protective layer on the front of the battery to effectively block the impact of wet chemical etching in the subsequent step 8 on the front of the battery.

[0068] Step 8. First, use the "single-sided water floating" wet chemical etching method to completely etch away the small amount of boron-doped polysilicon and silicon oxide on the back of the battery (mainly at the edge). Then, use the "single-sided water floating" alkaline solution etching method to texturize the back of the battery. The details are as follows:

[0069] (1) A mixed solution of nitric acid and hydrofluoric acid is used in combination with a single-sided water-floating wet etching method to etch away the boron-doped polysilicon that is plated and doped on the back of the battery. In the mixed solution of nitric acid and hydrofluoric acid, the mass concentration of nitric acid is 40%, the mass concentration of hydrofluoric acid is 4%, the solution temperature is 7° C., and the etching time is 1-2 minutes.

[0070] (2) Etch away the thin silicon oxide on the back of the battery using a hydrofluoric acid solution with one side water floating. The hydrofluoric acid concentration is 1% and the cleaning time is 15-30 seconds.

[0071] (3) The back of the battery is textured by a wet etching method using a KOH solution with a single-sided water float. The KOH solution has a mass concentration of 2%, a temperature of 70° C., and an etching time of 5-6 minutes, so that a random pyramid-shaped texture is formed on the back of the silicon wafer.

[0072] In all wet chemical etchings in this step, the APCVD silicon oxide prepared in step 7 plays a good protective role on the front side of the battery.

[0073] Step 9. Use thermal oxidation technology to prepare tunneling silicon oxide on the back of the silicon wafer. The thickness is 1.3nm and the refractive index is 1.46.

[0074] Step 10. Use LPCVD to prepare intrinsic amorphous silicon on the back of the battery with a thickness of 100nm. The LPCVD intrinsic amorphous silicon that is plated on the front of the battery is very small, mainly produced in a very narrow range at the edge of the front, and this effect can be eliminated by wet chemical etching later.

[0075] Step 11. Use screen printing chemical etching slurry to etch away the intrinsic amorphous silicon and tunneling silicon oxide on the back of the battery except for the local electronic passivation contact design area. BES etching slurry, after screen printing, is heated to 350-400℃ on a heating plate and left to stand for 1-2 minutes. The pattern of the screen printing screen is consistent with the design pattern of the local electronic passivation contact area on the back of the battery given above. The intrinsic amorphous silicon and tunneling silicon oxide in the printing slurry area are etched away without damaging the velvet surface prepared on the back of the battery.

[0076] After this step, only the intrinsic amorphous silicon and tunneling silicon oxide in the local electronic passivation contact design area are retained on the back of the battery, and the other areas are the n-type silicon substrate with a velvet morphology. Then, the surface of the silicon wafer is cleaned with a 40-50°C hydrochloric acid solution combined with ultrasonic cleaning to clean the residual Merck slurry on the surface of the silicon wafer and obtain a clean surface.

[0077] Step 12. Use masked ion implantation to perform localized phosphorus ion implantation in the non-local electronic passivation contact design area and the local electronic passivation contact design area on the back of the battery. The process mask pattern of the ion implantation is consistent with the design pattern of the local electronic passivation contact area on the back of the battery given above. In the non-local electronic passivation contact design area, the phosphorus implantation energy is 7 keV and the dose is 2.10 15 cm -2 In the local electron passivation contact design area, the phosphorus implantation energy is 20keV and the dose is 5·10 15 cm -2 The temperature of the silicon wafer substrate during ion implantation is room temperature 25°C.

[0078] Then, furnace thermal annealing is performed. During the annealing, the ion-implanted phosphorus in the non-local electronic passivation contact design area is activated and redistributed in silicon to form phosphorus-doped n + -n high-low junction. The amorphous silicon in the local electronic passivation contact design area is fully crystallized into polysilicon, and the ion-implanted phosphorus also completes the impurity activation and redistribution in the polysilicon. The furnace tube annealing temperature is 850℃, the time is 30-40min, and the nitrogen atmosphere.

[0079] After this step, the square resistance of the phosphorus-doped junction in the non-local electronic passivation contact area on the back of the cell is 100-120Ω / □. The square resistance of the phosphorus-doped polysilicon layer in the local electronic passivation contact area is 70-90Ω / □.

[0080] Step 13. Use a single-sided water-flooded hydrofluoric acid solution wet etching method to etch away the small amount of phosphorus-silicate glass generated on the back of the battery in step 12. The hydrofluoric acid concentration is 2%, and the cleaning time is 60-90 seconds.

[0081] Step 14. Use the PECVD method to prepare a layer of silicon nitride on the back of the battery with a thickness of 75nm and a refractive index of 2.0. This layer of silicon nitride serves as an auxiliary passivation layer on the back of the battery to enhance the working stability of the battery in extreme applications (especially high humidity and high temperature). In addition, this layer of silicon nitride has two functions. One is to serve as a protective layer on the back of the battery to effectively block the wet chemical etching in the subsequent step 15. The second is to serve as a buffer barrier layer for screen-printed metallization in the subsequent step 17 to ensure that the silver paste can be confined within the phosphorus-doped polysilicon layer after rapid thermal treatment and sintering, and to minimize overdiffusion through the phosphorus-doped polysilicon and tunneling silicon oxide to enter the silicon substrate.

[0082] Step 15. First, use the "single-sided water floating" wet etching method to chemically etch the small amount of phosphorus-doped polysilicon on the front side of the battery (mainly at the edge) and etch it all away. Then, use hydrofluoric acid solution to etch away the APCVD SiO2 deposited on the front side of the battery in step 7 and the small amount of borosilicate glass generated on the front side of the battery in step 6. The details are as follows:

[0083] (1) A mixed solution of nitric acid and hydrofluoric acid is used in combination with a single-sided water-floating wet etching method to etch away the phosphorus-doped polysilicon that is plated and doped around the front edge of the battery. In the mixed solution of nitric acid and hydrofluoric acid, the mass concentration of nitric acid is 40%, the mass concentration of hydrofluoric acid is 4%, the solution temperature is 7° C., and the etching time is 30-60 seconds.

[0084] (2) Using a single-sided water-floating hydrofluoric acid solution etching method, the APCVD SiO2 and a small amount of borosilicate glass on the front of the battery are etched away. The hydrofluoric acid concentration is 5%, and the cleaning time is 5-6 minutes.

[0085] In this step of wet etching, the silicon nitride prepared in step 14 plays a good protective role on the back of the battery. Through this step of chemical etching, electrical insulation isolation is also completed between the front and back of the battery.

[0086] Step 16. A layer of silicon nitride is prepared on the front of the cell by PECVD as a passivation anti-reflection film with a thickness of 75nm and a refractive index of 2.0. This layer of silicon nitride also serves as a buffer barrier layer for the metallization of the screen-printed silver paste in the subsequent step 17 to ensure that the silver paste can be confined within the boron-doped polysilicon as much as possible after rapid thermal treatment and sintering, and as little as possible enter the silicon substrate by diffusing through the boron-doped polysilicon and tunneling silicon oxide.

[0087] Step 17. Metallize the local passivation contact areas on the front and back of the battery by screen printing silver paste and rapid thermal treatment sintering. Alignment technology is required to achieve: alignment of the local hole passivation contact area on the front of the battery and the corresponding metallization area, and alignment of the local electron passivation contact area on the back of the battery and the corresponding metallization area. The electrode units on the front and back of the battery are also square with a side length of 40μm. The electrode units and their corresponding square passivation contact units have the same geometric center. The actual peak temperature of rapid thermal treatment sintering is 720-750℃, the time at the peak temperature is 2-4 seconds, and the atmosphere is compressed air.

[0088] Step 18. Use inkjet printing method to print the silver nanowire ink (ink) to connect the electrode units distributed on both sides of the battery into transparent conductive electrodes ( Figure 2 ). The silver nanowire transparent conductive electrode is a grid line type, and alignment technology is required. Its axis line coincides with the connection line of the center point of the electrode unit in the y direction or x direction. Then the rapid thermal treatment method is used for annealing, the temperature is 175℃, the time is 10-15 minutes, and the atmosphere is nitrogen. The line width of the silver nanowire transparent conductive electrode is 20 microns, the line height is 40 microns, and the transmittance is 97.5%.

[0089] At this point, the preparation of the double-sided passivated contact crystalline silicon solar cell is completed.

[0090] The double-sided passivated contact cell disclosed in the utility model can be prepared into a double-sided passivated contact solar module by using shingle technology, conductive glue (transparent conductive glue), and combining with small-piece cell technology. In actual double-sided photovoltaic power generation applications, the front and back sides of the cell module can be swapped: that is, either side can be used as the main side that receives photons. Specific applications include distributed photovoltaics, ground power stations, and building photovoltaics.

[0091] Finally, it should be noted that, although the implementation scheme of the utility model is described above in conjunction with the accompanying drawings, the utility model is not limited to the above-mentioned specific implementation scheme and application field. The above-mentioned specific implementation scheme is only illustrative and instructive, and is used to help understand the method and its core idea of ​​the utility model, but is not restrictive. Under the enlightenment of this specification, ordinary technicians in this field can make many forms of changes, improvements and equivalent implementations in the specific implementation scheme and application scope without departing from the scope of protection of the principles of the utility model and the claims, which should also be regarded as the protection scope of the utility model.

Claims

1. A double-sided passivated contact crystalline silicon solar cell, It is characterized in that including a silicon substrate; A local hole passivation contact region is formed on the first surface of the silicon substrate, wherein the local hole passivation contact region has a plurality of hole passivation contact units distributed in a periodic lattice; A pn junction or a high-low junction using acceptor doping formed on the first surface of the silicon substrate and arranged staggered with the local hole passivation contact area; A first passivation layer for passivating the first surface of the silicon substrate; A first metal electrode formed on the first surface of the silicon substrate, the first metal electrode having a plurality of first electrode units distributed in a periodic lattice, the first electrode units being arranged correspondingly to the hole passivation contact units; A local electronic passivation contact region is formed on the second surface of the silicon substrate, wherein the local electronic passivation contact region has a plurality of electronic passivation contact units distributed in a periodic lattice; A donor-doped pn junction or a high-low junction formed on the second surface of the silicon substrate and arranged staggered with the local electronic passivation contact region; A second passivation layer for passivating the second surface of the silicon substrate; A second metal electrode is formed on the second surface of the silicon substrate, wherein the second metal electrode has a plurality of second electrode units distributed in a periodic lattice, and the second electrode units are arranged correspondingly to the hole passivation contact units.

2. The double-sided passivated contact crystalline silicon solar cell according to claim 1, It is characterized in that The first electrode unit coincides with the geometric center of the hole passivation contact unit, and the outer contour is less than or equal to the outer contour of the hole passivation contact unit; the second electrode unit coincides with the geometric center of the electron passivation contact unit, and the outer contour is less than or equal to the outer contour of the electron passivation contact unit.

3. The double-sided passivated contact crystalline silicon solar cell according to claim 1, It is characterized in that The local hole passivation contact area is composed of tunneling silicon oxide and boron-doped or gallium-doped polysilicon; the local electron passivation contact area is composed of tunneling silicon oxide and phosphorus-doped polysilicon; the tunneling silicon oxide has a thickness of 1.2-1.6nm and a refractive index of 1.45-1.5; the boron-doped or gallium-doped polysilicon has a thickness of 5-500nm; and the phosphorus-doped polysilicon has a thickness of 5-500nm.

4. The double-sided passivated contact crystalline silicon solar cell according to claim 1, It is characterized in that The shape of the hole passivation contact unit is any one of a circle, a rectangle, a diamond, and an ellipse; the arrangement period of the hole passivation contact unit is 100-5000 microns; the area percentage of the local hole passivation contact area is 0.05%-2.5%; The shape of the electronic passivation contact unit is any one of a circle, a rectangle, a diamond, and an ellipse; the arrangement period of the electronic passivation contact unit is 100-5000 microns; and the area percentage of the local electronic passivation contact region is 0.05%-2.5%.

5. The double-sided passivated contact crystalline silicon solar cell according to claim 1, It is characterized in that The shapes of the first electrode unit and the second electrode unit are respectively the same as those of the hole passivation contact unit and the electron passivation contact unit.

6. The double-sided passivated contact crystalline silicon solar cell according to claim 1, It is characterized in that The light shielding rate of the first metal electrode and the second metal electrode is 0.05%-0.75%.

7. The double-sided passivated contact crystalline silicon solar cell according to claim 1, It is characterized in that The first passivation layer and the second passivation layer are both silicon nitride; the thickness of the silicon nitride is 70-80 nm, and the refractive index is 1.9-2.

1.

8. The double-sided passivated contact crystalline silicon solar cell according to any one of claims 1 to 7, It is characterized in that It also includes transparent conductive electrodes, which are used to connect the first electrode unit in the first metal electrode and the second electrode unit in the second metal electrode; the transparent conductive electrode is a grid line type, and its axis line coincides with the line connecting the center point of the electrode unit in the y direction or the x direction.

9. The double-sided passivated contact crystalline silicon solar cell according to claim 8, It is characterized in that The light transmittance of the transparent conductive electrode is not less than 90%; the material of the transparent conductive electrode is silver nanowire, copper nanowire, transparent conductive oxide, or the transparent conductive electrode is a transparent conductive electrode based on graphene and carbon nanotubes.

10. The double-sided passivated contact crystalline silicon solar cell according to claim 8, It is characterized in that Each column of the first metal electrode in the y direction is provided with a transparent conductive electrode; each column of the second metal electrode in the y direction is provided with a transparent conductive electrode; each M-row of the first metal electrode in the x direction is provided with a transparent conductive electrode; each M-row of the second metal electrode in the x direction is provided with a transparent conductive electrode; M is a natural number greater than 1.