Extrusion coated gasket
By designing an extruded coating gasket with an inclined structure on the lithium battery electrode coating gasket, the problem of thick edges and thin areas being too wide during the lithium battery coating process is solved, and the battery performance and coating uniformity are improved , a significant reduction in the width of the thin edge is achieved.
Patent Information
- Application Number
- CN202420214305.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-29
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2034-01-29
AI Technical Summary
During the coating process of lithium battery electrodes, there are problems such as thick edges and thinning areas that are too wide, which affects the battery capacity, circulation performance and storage performance.
An extruded coating gasket is designed, including the gasket body, slurry cavity, slurry lip and thinning groove. The thinning groove extends along the length and height of the gasket and gradually decreases in the thickness direction to form a Inclined structure to optimize the flow and distribution of the coating liquid.
It effectively solves the problem of thick edges and thin areas too wide, improves the uniformity of coating effect and battery performance, reduces the thin edge width area, and reaches the top level in the industry.
Smart Images

Figure CN222077074U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of pole piece coating of a lithium battery, in particular to an extrusion coating gasket. Background Art
[0002] With the continuous development of economy and the continuous progress of society, people's production and life are provided with extremely rich material consumer goods, and lithium battery is one of the many material consumer goods.
[0003] At present, the coating process of the pole piece is indispensable in the production process of lithium batteries. The coating die head of the lithium battery coating process needs to be installed with a gasket for production, that is, the corresponding gasket needs to be installed between the upper die head and the lower die head according to the product model specifications. Since the edge of the pole piece has thinning specifications, there must be a certain thickness difference between the edge and the middle of the pole piece, and the opening edge of the gasket needs to be designed with a guide structure to guide the edge slurry to be coated on the substrate. Due to different application scenarios, different capacity or rate lithium-ion products are designed. Different lithium-ion products are made using different material systems to meet customer requirements. At the same time, slurries made from different material systems have different rheological curves, which will have different coating effects during extrusion coating, especially the coating edge. Figure 4 The problem with thick edge 210 is shown.
[0004] Although there are now gaskets that solve the thick edge problem, there are Figure 5 The problem of the thinned area shown by the middle reference number 220 being too large or too thin leads to the loss of battery capacity, and the battery's cycle, rate, and storage performances are all affected to a certain extent.
[0005] Therefore, an extrusion coated gasket is provided to overcome one or more of the above-mentioned disadvantages. Utility Model Content
[0006] The utility model aims to provide an extrusion coating gasket to solve the problem that the thick edge and the thinned area of coating are too wide.
[0007] To achieve the above-mentioned purpose, the extrusion coating gasket of the utility model comprises a gasket body and a pulp outlet cavity, a pulp outlet lip and a thinning groove opened on the gasket body. The pulp outlet lip is connected with the pulp outlet cavity in the height direction of the gasket body. The thinning groove extends along the length direction and the height direction of the gasket body respectively, and the thinning groove also extends to the position connected with the pulp outlet lip and the pulp outlet cavity respectively. The size of the thinning groove in the thickness direction of the gasket body is gradually reduced in the direction close to the pulp outlet lip, so that the corresponding position of the gasket body forms an inclined structure with an inclination.
[0008] Compared with the prior art, with the help of thinning grooves opened on the gasket body and extending along the length and height directions of the gasket body respectively, the thinning grooves also extend to the positions connected with the slurry outlet lip and the slurry outlet cavity respectively. The size of the thinning grooves in the thickness direction of the gasket body is gradually decreasing in the direction close to the slurry outlet lip, so that the corresponding position of the gasket body forms an inclined structure with an inclination. This design solves the problem of thick edges of coating and the problem of too wide thinning area.
[0009] Preferably, the dimension of the inclined structure in the length direction of the gasket body is a, the dimension of the end of the thinning groove away from the slurry discharge lip in the thickness direction of the gasket body is b, and the dimension of the end of the inclined structure facing the slurry discharge lip in the thickness direction of the gasket body is c; wherein, 2mm≤a≤4.5mm; 0.1mm≤b≤0.3mm, 0.1mm≤c≤0.3mm.
[0010] Preferably, the thinning grooves are symmetrically arranged with the pulp outlet lip as the center.
[0011] Preferably, center lines of the pulp outlet lip and the pulp outlet cavity coincide with each other in the height direction of the gasket body.
[0012] Preferably, the size of the pulp outlet lip in the length direction of the gasket body is smaller than the size of the pulp outlet cavity in the length direction of the gasket body.
[0013] Preferably, the gasket body is provided with a plurality of mounting holes arranged around the pulp outlet cavity.
[0014] Preferably, a lug is provided on one side of the gasket body away from the pulp outlet cavity and the pulp outlet lip, the lug protruding outward and extending along the length direction of the gasket body.
[0015] Preferably, the lugs are symmetrically arranged with the center line of the gasket body in the height direction as the center.
[0016] Preferably, the gasket body includes an elongated base, a height body bent in the same direction from two opposite ends of the elongated base, and a folded body parallel to the elongated base folded back in directions facing each other from the end of each height body, the height body and the elongated base jointly define the pulp outlet cavity, the folded bodies jointly define the pulp outlet lip, and the thinning groove is opened on the folded body.
[0017] Preferably, the elongated base and the height body are each provided with a plurality of mounting holes, and the mounting holes on the elongated base and the height body are arranged together around the pulp outlet cavity. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1It is a plan view of the extrusion coated gasket of the utility model viewed in its thickness direction.
[0019] Figure 2 yes Figure 1 The position indicated by arrow B is an enlarged view viewed along the direction indicated by arrow B.
[0020] Figure 3 yes Figure 2 An enlarged view of the corresponding size is shown in FIG.
[0021] Figure 4 This is a structural diagram showing that there is a thick edge at the edge of the existing coating.
[0022] Figure 5 It is a structural diagram showing that the existing coating edge has a thinning area that is too large and too thin. DETAILED DESCRIPTION
[0023] Embodiments of the present invention will now be described with reference to the accompanying drawings, in which like reference numerals represent like elements.
[0024] See also Figure 1 The extrusion coating gasket 100 of the present invention is applied to a coating die and is disposed between an upper die and a lower die of the coating die. Since the structure of the coating die is well known in the art, and the positional relationship between the extrusion coating gasket 100 of the present invention and the upper die and the lower die of the coating die is well known in the art, it will not be described in detail here.
[0025] Recombination Figure 2 The extrusion coating gasket 100 of the utility model includes a gasket body 10 and a slurry discharge cavity 20, a slurry discharge lip 30 and a thinning groove 40 opened on the gasket body 10. The slurry discharge lip 30 is connected with the slurry discharge cavity 20 in the height direction of the gasket body 10 to meet the need that the coating liquid in the slurry discharge cavity 20 flows along the height direction of the gasket body 10 to the slurry discharge lip 30, and then passes through the slurry discharge lip 30 to be coated on the pole piece. The thinning groove 40 extends along the length direction and the height direction of the gasket body 10 respectively, and the thinning groove 40 extends to a position connected with the slurry discharge lip 30, and the thinning groove 40 also extends to a position connected with the slurry discharge cavity 20 to meet the need that the coating liquid in the slurry discharge cavity 20 flows along the height direction of the gasket body 10 to the thinning groove 40, and then passes through the thinning groove 40 to be coated on the pole piece. The size of the thinning groove 40 in the thickness direction of the gasket body 10 is gradually reduced in the direction close to the lip 30, so that the corresponding position of the gasket body 10 forms an inclined structure 11 with an inclination. Figure 2 and Figure 3 Specifically, Figure 3As an example, the dimension of the inclined structure 11 in the length direction of the gasket body 10 is a, the dimension of the end of the thinning groove 40 away from the lip 30 in the thickness direction of the gasket body 10 is b, and the dimension of the end of the inclined structure 11 facing the lip 30 in the thickness direction of the gasket body 10 is c; wherein, 2mm≤a≤4.5mm; 0.1mm≤b≤0.3mm, 0.1mm≤c≤0.3mm, for example, a is 2mm, 2.5mm, 3mm, 3.5mm, 4mm or 4.5mm, b is 0.1mm, 0.2mm or 0.3mm, c is 0.1mm, 0.2mm or 0.3mm, such a design can further make the thinning area narrower and solve the thick edge better. More specifically, as follows:
[0026] like Figure 1 As shown, the thinning grooves 40 are symmetrically arranged with the slurry outlet lip 30 as the center, so as to ensure the consistency of the effect of solving the thick edges and thinning areas on both sides of the electrode coating. In addition, the center lines of the slurry outlet lip 30 and the slurry outlet cavity 20 in the height direction of the gasket body 10 coincide with each other, and the coincident center lines can be seen indicated by the label L, so as to effectively ensure the uniformity of the coating effect. In addition, the size of the slurry outlet lip 30 in the length direction of the gasket body 10 is smaller than the size of the slurry outlet cavity 20 in the length direction of the gasket body 10, so as to control the size of the slurry outlet lip 30 to be smaller than the size of the slurry outlet cavity 20. Specifically, at Figure 1 In the embodiment, as an example, a plurality of mounting holes 12 are provided on the gasket body 10 and arranged around the pulp outlet cavity 20, so that the gasket body 10 can be assembled and connected with the upper die head and the lower die head respectively by means of the mounting holes 12. In addition, the gasket body 10 is away from the pulp outlet cavity 20 and the pulp outlet lip 30 on one side (i.e. Figure 1 The lower side of the gasket body 10 is provided with a lug 13 which protrudes outward and extends along the length direction of the gasket body 10. Figure 1 As an example, the lugs 13 are symmetrically arranged with the center line of the gasket body 10 in the height direction (as indicated by the label L) as the center, so as to facilitate the manufacturing and processing of the lugs 13 on the gasket body 10, and to facilitate the assembly operation of the gasket body 10 with the upper die head and the lower die head respectively; obviously, in other embodiments, the lugs 13 can be deleted, so it is not limited to this.
[0027] like Figure 1 As shown, the gasket body 10 comprises an elongated base 10a, a height body 10b bent in the same direction from opposite ends of the elongated base 10a, and a folded body 10c parallel to the elongated base 10a folded back in the direction facing each other from the ends of each height body 10b. The height body 10c and the elongated base 10a jointly define the aforementioned pulp outlet cavity 20, the folded body 10c jointly define the aforementioned pulp outlet lip 30, and the thinning groove 40 is opened in the folded body 10c. Figure 1As shown. This design facilitates the extrusion coating gasket 100 of the utility model to be manufactured by punching and simplifies its manufacturing process. Specifically, combined with Figure 1 and Figure 2 As an example, the thinning groove 40 is opened on the gasket body 10 (specifically, on one side of the folded body 10c) in the thickness direction of the gasket body 10. It should be noted that when the gasket body 10 includes an elongated base 10a, a height body 10b and a folded body 10c, at this time, the mounting holes 12 on the aforementioned gasket body 10 are respectively located on the elongated base 10a and the height body 10b, that is, the elongated base 10a and the height body 10b are each provided with a plurality of mounting holes 12, so that the mounting holes 12 on both the elongated base 10a and the height body 10b are arranged together around the pulp outlet cavity 20. This design is to increase the reliability of fixing the gasket body 10 to the upper die head and the lower die head respectively; in addition, the lug 13 is located on the elongated base 10a.
[0028] Compared with the prior art, with the help of a thinning groove 40 opened on the gasket body 10 and extending along the length direction and the height direction of the gasket body 10, the thinning groove 40 also extends to the position connected with the pulp outlet lip 30 and the pulp outlet cavity 20, and the size of the thinning groove 40 in the thickness direction of the gasket body 10 is gradually decreased along the direction close to the pulp outlet lip 30, so that the corresponding position of the gasket body 10 forms an inclined structure 11 with an inclination. This design solves the problem of thick edges of coating and the problem of too wide thinning area.
[0029] It is worth noting that the direction indicated by the arrow A in the drawings and the opposite direction are the height direction of the gasket body 10, the direction indicated by the arrow B in the drawings and the opposite direction are the length direction of the gasket body 10, and the direction indicated by the arrow C in the drawings and the opposite direction are the thickness direction of the gasket body 10. Figure 1 In the figure, for the left thinning groove 40, the direction indicated by arrow B is the direction in which the thinning groove 40 approaches the lip 30; and for the right thinning groove 40, the opposite direction indicated by arrow B is the direction in which the thinning groove 40 approaches the lip 30. In addition, it is optional that, except for the inclined structure 11, the thickness dimensions of the other positions of the folded body 10c, the elongated base 10a and the height body 10b are the same to ensure the flatness of the other positions of the folded body 10c, the elongated base 10a and the height body 10b in the thickness direction. In addition, for "2mm≤a≤4.5mm, 0.1mm≤b≤0.3mm, and 0.1mm≤c≤0.3mm", "mm" is expressed as millimeter, and through the size control and the coordination of the inclined structure 11 formed at the corresponding position of the gasket body 10 by the thinning groove 40, the thin edge width area is reduced to the top level in the industry, from the current industry width of 5~12mm to within 3mm.
[0030] The above disclosure is only a preferred embodiment of the present invention, and certainly cannot be used to limit the scope of rights of the present invention. Therefore, equivalent changes made according to the scope of the patent application of the present invention are still within the scope covered by the present invention.
Claims
1. An extrusion coating gasket, comprising a gasket body, a pulp outlet cavity and a pulp outlet lip opened on the gasket body, wherein the pulp outlet lip is connected to the pulp outlet cavity in the height direction of the gasket body, It is characterized in that The extrusion coated gasket also includes a thinning groove opened on the gasket body and extending along the length direction and height direction of the gasket body respectively. The thinning groove also extends to the position connected with the pulp outlet lip and the pulp outlet cavity respectively. The size of the thinning groove in the thickness direction of the gasket body is gradually reduced in the direction close to the pulp outlet lip, so that the corresponding position of the gasket body forms an inclined structure with an inclination.
2. The extrusion coated gasket according to claim 1, It is characterized in that The dimension of the inclined structure in the length direction of the gasket body is a, the dimension of the end of the thinning groove away from the slurry discharge lip in the thickness direction of the gasket body is b, and the dimension of the end of the inclined structure facing the slurry discharge lip in the thickness direction of the gasket body is c; wherein, 2mm≤a≤4.5mm; 0.1mm≤b≤0.3mm, 0.1mm≤c≤0.3mm.
3. The extrusion coated gasket according to claim 1, It is characterized in that The thinning grooves are symmetrically arranged with the pulp outlet lip as the center.
4. The extrusion coated gasket according to claim 1, It is characterized in that The center lines of the pulp outlet lip and the pulp outlet cavity in the height direction of the gasket body coincide with each other.
5. The extrusion coated gasket according to claim 1, It is characterized in that The size of the pulp outlet lip in the length direction of the gasket body is smaller than the size of the pulp outlet cavity in the length direction of the gasket body.
6. The extrusion coated gasket according to claim 1, It is characterized in that The gasket body is provided with a plurality of mounting holes arranged around the pulp outlet cavity.
7. The extrusion coated gasket according to claim 1, It is characterized in that A lug which protrudes outward and extends along the length direction of the gasket body is arranged on one side of the gasket body away from the pulp outlet cavity and the pulp outlet lip.
8. The extrusion coated gasket according to claim 7, It is characterized in that The lugs are symmetrically arranged with the center line of the gasket body in the height direction as the center.
9. The extrusion coated gasket according to claim 1, It is characterized in that The gasket body includes an elongated base, a height body bent in the same direction from the opposite ends of the elongated base, and a folded body parallel to the elongated base folded back in directions facing each other from the end of each height body, the height body and the elongated base jointly define the pulp outlet cavity, the folded bodies jointly define the pulp outlet lip, and the thinning groove is opened on the folded body.
10. The extrusion coated gasket according to claim 9, It is characterized in that The elongated base and the height body are each provided with a plurality of mounting holes, and the mounting holes on the elongated base and the height body are arranged together around the pulp outlet cavity.