Shaping die for VC vapor chamber

By setting up the raised rib strips and hydraulic mechanisms on the VC temperature uniform plate shaping mold, the VC surface of stainless steel is leveled, solving the problem of uneven surfaces after laser welding, and improving the appearance quality and performance stability of the product.

CN222242007UActive Publication Date: 2024-12-27SHENZHEN VC THERMAL TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420989293.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-05-09
Publication Date
2024-12-27
Estimated Expiration
2034-05-09

AI Technical Summary

Technical Problem

After laser welding, stainless steel VC is prone to uneven surfaces, affecting appearance quality and performance stability.

Method used

A VC temperature uniform plate shaping mold is designed, including an upper mold and a lower mold. By setting up a raised rib strip and a hydraulic mechanism on the upper mold, the pressure is applied to cause local depressions on the skirt surface of the VC temperature uniform plate to realize the surface. leveling.

Benefits of technology

It effectively solves the problem of uneven surface of the product after laser welding, improves the appearance quality and performance stability of the product, and avoids effective area crushing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222242007U_ABST
    Figure CN222242007U_ABST
Patent Text Reader

Abstract

The utility model provides a VC vapor chamber shaping die which comprises an upper die, an upper profiling groove matched with a VC vapor chamber in shape is formed in one face of the upper die, a plurality of protruding ribs are fixedly connected to the face, close to the upper profiling groove, of the upper die, and the protruding ribs are arranged around the upper profiling groove. By means of the protruding ribs arranged on the upper die, when the VC vapor chamber is leveled through the upper die under the pressure effect, local recesses can be generated on the skirt edge surface of the VC vapor chamber, a shell on the surface of the VC vapor chamber is stretched towards the skirt edge, the effect of leveling the surface of the VC vapor chamber is achieved, in the action process, the VC vapor chamber is kept empty through an upper profiling groove, and the VC vapor chamber is prevented from falling off. And a working effective area of a product is prevented from being crushed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of temperature equalizing plate shaping, in particular to a VC temperature equalizing plate shaping mould. Background Art

[0002] With the continuous advancement of mobile phone technology, especially the widespread application of 5G technology, the functions of smartphones are becoming increasingly rich and their performance is continuously improving. However, this progress has also brought a problem: the heat dissipation demand of mobile phones is increasing. Although traditional heat dissipation materials such as copper alloys have certain heat dissipation performance, their heat dissipation effect has gradually failed to meet market demand when facing high-performance smartphones. Therefore, the market demand for new heat dissipation materials is becoming increasingly urgent; stainless steel, as a new type of heat dissipation material, has begun to be used in the field of mobile phone heat dissipation due to its excellent thermal conductivity and corrosion resistance.

[0003] However, in the manufacturing process of stainless steel VC, although laser welding technology solves the welding problem, the surface of the product is prone to unevenness after laser welding, which directly affects the appearance quality and performance stability of the product. Therefore, we made improvements and proposed a VC temperature plate shaping mold. Summary of the invention

[0004] The purpose of the utility model is to solve the existing problem that the surface of the product is prone to unevenness after laser welding.

[0005] In order to achieve the above-mentioned purpose of the invention, the utility model provides a VC temperature equalizing plate shaping mold to improve the above-mentioned problem.

[0006] The specific application is as follows:

[0007] The VC temperature equalizer shaping mold comprises an upper mold, one side of which is provided with an upper profiling groove adapted to the shape of the VC temperature equalizer, and a side of the upper mold close to the upper profiling groove is fixedly connected with a plurality of raised ribs, which are arranged around the upper profiling groove.

[0008] As a preferred technical solution of the present application, the raised ribs are used to create a depression on the surface of the VC temperature equalizing plate skirt so that the surface shell of the VC temperature equalizing plate is stretched toward the skirt to achieve leveling of the surface of the VC temperature equalizing plate.

[0009] As a preferred technical solution of the present application, it also includes a lower mold used in conjunction with the upper mold, and a lower contoured groove adapted to the shape of the VC temperature equalizing plate is provided on a side of the lower mold close to the upper mold.

[0010] As a preferred technical solution of the present application, a side of the lower mold close to the upper mold is fixedly installed with a plurality of positioning pins, and the plurality of positioning pins are arranged around the lower profiling groove; a side of the upper mold close to the lower mold is provided with a plurality of pin grooves, and the plurality of pin grooves are arranged around the upper profiling groove, and the positions of the plurality of pin grooves correspond to the positions of the plurality of positioning pins respectively.

[0011] As a preferred technical solution of the present application, a plurality of positioning posts are fixedly mounted on a side of the lower mold close to the upper mold, and a plurality of positioning grooves for the positioning posts to be inserted are provided on the upper mold.

[0012] As a preferred technical solution of the present application, a hydraulic mechanism is provided between the upper mold and the lower mold, and the hydraulic mechanism is used to drive the upper mold and the lower mold to close and separate the molds.

[0013] As a preferred technical solution of the present application, the hydraulic mechanism includes a base, a plurality of columns are fixedly installed on the top of the base, a fixed platform is fixedly connected between the plurality of columns, a first hydraulic cylinder is fixedly installed on the top of the fixed platform, a telescopic end of the first hydraulic cylinder passes through the fixed platform and is fixedly connected with a lifting plate, the upper mold is installed at the bottom of the lifting plate, and the lifting plate is interlaced and connected with the outer surface of the column;

[0014] Both sides of the top of the lifting plate are fixedly connected with limit rods, and the top ends of the limit rods pass through the fixing platform and extend to above the fixing platform.

[0015] As a preferred technical solution of the present application, two slide rails are fixedly installed on the top of the base, and the outer surfaces of the two slide rails are slidably connected to a plurality of slide seats, and the lower mold is installed between the tops of the plurality of slide seats.

[0016] As a preferred technical solution of the present application, a second hydraulic cylinder is fixedly installed on the top of the base, and the telescopic end of the second hydraulic cylinder is connected to the lower mold.

[0017] As a preferred technical solution of the present application, an air hole is opened through the bottom of the inner cavity of the lower contoured groove, a sleeve is fixedly installed on the top of the base, an air cavity is arranged in the sleeve, a hollow piston is slidably connected in the air cavity, a center hole tube is fixedly connected to one side of the hollow piston, and one end of the center hole tube away from the hollow piston is fixedly connected to the bottom of the upper mold and is connected to the air hole.

[0018] Compared with the prior art, the utility model has the following beneficial effects:

[0019] In the scheme of this application:

[0020] In order to solve the problem that the product surface is prone to unevenness after laser welding in the prior art, the present application provides raised ribs on the upper mold so that when the upper mold flattens the VC temperature equalizing plate under pressure, it can produce local depressions on the skirt surface of the VC temperature equalizing plate, stretch the surface shell of the VC temperature equalizing plate toward the skirt, and achieve the effect of leveling the surface of the VC temperature equalizing plate. During this action, the VC temperature equalizing plate avoids air through the upper contoured groove to avoid crushing the effective working area of ​​the product. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 A schematic diagram of the structure of the VC temperature equalizer shaping mold provided in this application;

[0022] Figure 2 A schematic diagram of the structure of the lower contour groove of the VC temperature plate shaping mold provided in this application;

[0023] Figure 3 A schematic diagram of the structure of the upper mold of the VC temperature plate shaping mold provided in this application from a bottom view;

[0024] Figure 4 A schematic diagram of the structure of the hydraulic mechanism of the VC temperature plate shaping mold provided in this application;

[0025] Figure 5 This is a schematic diagram of the partial cross-sectional structure of the sleeve of the VC temperature equalizer shaping mold provided in this application.

[0026] Indicated in the figure:

[0027] 1. Upper mold; 101. Upper profiling groove; 102. Raised rib; 2. Lower mold; 201. Lower profiling groove; 3. Positioning column; 301. Positioning groove; 4. Positioning pin; 401. Pin groove; 5. Hydraulic mechanism; 501. Base; 502. Column; 503. Fixed table; 504. First hydraulic cylinder; 505. Lifting plate; 506. Limit rod; 507. Slide rail; 508. Slide seat; 509. Second hydraulic cylinder; 6. Sleeve; 601. Air cavity; 602. Hollow piston; 603. Middle hole tube; 604. Air hole. DETAILED DESCRIPTION

[0028] In order to enable those skilled in the art to better understand the solution of the utility model, the technical solution in the embodiment of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiment of the utility model. Obviously, the described embodiment is only a part of the embodiment of the utility model, not all of the embodiments. Based on the embodiment of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the utility model.

[0029] As described in the background technology, during the manufacturing process of stainless steel VC, although laser welding technology solves the welding problem, the surface of the product is prone to unevenness after laser welding, which directly affects the appearance quality and performance stability of the product.

[0030] In order to solve this technical problem, the utility model provides a VC temperature equalizing plate shaping mold, which is used for leveling the skirt of the stainless steel VC temperature equalizing plate after laser welding.

[0031] Specifically, please refer to Figure 1-Figure 3 VC temperature plate shaping mold specifically includes:

[0032] The upper mold 1 has an upper contoured groove 101 on one side thereof which matches the shape of the VC temperature equalizing plate, and a plurality of raised ribs 102 are fixedly connected to a side of the upper mold 1 close to the upper contoured groove 101 , and the plurality of raised ribs 102 are arranged around the upper contoured groove 101 .

[0033] The VC temperature equalizing plate shaping mold provided by the utility model has raised ribs 102 arranged on the upper mold 1, so that when the upper mold 1 flattens the VC temperature equalizing plate under the action of pressure, a local depression can be produced on the skirt surface of the VC temperature equalizing plate, and the surface shell of the VC temperature equalizing plate is stretched toward the skirt, so as to achieve the effect of flattening the surface of the VC temperature equalizing plate. During this action, the VC temperature equalizing plate is avoided by the upper profiling groove 101 to avoid crushing the effective working area of ​​the product.

[0034] In order to enable those skilled in the art to better understand the solution of the utility model, the technical solution in the embodiments of the utility model will be clearly and completely described below in conjunction with the accompanying drawings.

[0035] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features and technical solutions in the embodiments may be combined with each other.

[0036] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.

[0037] Example 1, please refer to Figure 1-Figure 3The VC temperature equalizing plate shaping mold comprises an upper mold 1, one side of the upper mold 1 is provided with an upper profiling groove 101 adapted to the shape of the VC temperature equalizing plate, and a side of the upper mold 1 close to the upper profiling groove 101 is fixedly connected with a plurality of raised ribs 102, and the plurality of raised ribs 102 are arranged around the upper profiling groove 101. By means of the raised ribs 102 arranged on the upper mold 1, when the upper mold 1 flattens the VC temperature equalizing plate under pressure, a local depression can be generated on the skirt surface of the VC temperature equalizing plate, and the surface shell of the VC temperature equalizing plate is stretched toward the skirt to realize the flattening of the surface of the VC temperature equalizing plate. During this action, the VC temperature equalizing plate is avoided through the upper profiling groove 101 to avoid crushing of the effective working area of ​​the product.

[0038] Furthermore, the raised ribs 102 are used to make the surface of the VC temperature averaging board skirt concave, so that the surface shell of the VC temperature averaging board is stretched toward the skirt, so as to achieve the flattening of the surface of the VC temperature averaging board;

[0039] Specifically, the raised ribs 102 will produce local depressions on the surface of the skirt of the stainless steel VC temperature-averaging plate in the shaping mold, but this design is to achieve the effect of surface leveling; first of all, it should be understood that the design purpose of the shaping mold is to correct the unevenness of the surface of the stainless steel VC temperature-averaging plate by applying precise and controlled pressure. When the shaping mold applies pressure, the raised ribs 102 will apply greater force to specific areas of the surface of the skirt of the stainless steel VC temperature-averaging plate, thereby producing local depressions on the surface of the skirt; this local depression is not a side effect of shaping, but a key step in achieving surface leveling. Through the local depressions produced by the raised ribs 102, the shaping mold can stretch the shell of the surface of the stainless steel VC temperature-averaging plate toward the skirt. This stretching effect is actually correcting the unevenness of the surface of the stainless steel VC temperature-averaging plate, making it smoother.

[0040] Further, such as Figure 1-Figure 2 As shown, it also includes a lower mold 2 used in conjunction with the upper mold 1. The lower mold 2 is provided with a lower contoured groove 201 that is adapted to the shape of the VC temperature equalizing plate on one side close to the upper mold 1. The lower contoured groove 201 is used to cooperate with the upper contoured groove 101 to avoid crushing the effective working area of ​​the VC temperature equalizing plate.

[0041] Further, such as Figure 1-Figure 3 As shown, a plurality of positioning pins 4 are fixedly installed on one side of the lower mold 2 close to the upper mold 1, and the plurality of positioning pins 4 are arranged around the lower profiling groove 201, and a plurality of pin grooves 401 are opened on one side of the upper mold 1 close to the lower mold 2, and the plurality of pin grooves 401 are arranged around the upper profiling groove 101, and the positions of the plurality of pin grooves 401 correspond to the positions of the plurality of positioning pins 4 respectively. In the process of placing the VC temperature equalizing plate into the lower profiling groove 201, the VC temperature equalizing plate can be positioned by the positioning pins 4, so as to improve the accuracy of the placement of the VC temperature equalizing plate.

[0042] Further, such as Figure 1-Figure 3 As shown, a plurality of positioning posts 3 are fixedly installed on one side of the lower mold 2 close to the upper mold 1, and a plurality of positioning grooves 301 for inserting the positioning posts 3 are opened on the upper mold 1. The positioning posts 3 and the positioning grooves 301 are used together for positioning during the mold closing process of the upper mold 1 and the lower mold 2, thereby improving the accuracy of the mold closing between the upper mold 1 and the lower mold 2.

[0043] Further, such as Figure 4 As shown, a hydraulic mechanism 5 is provided between the upper mold 1 and the lower mold 2. The hydraulic mechanism 5 is used to drive the upper mold 1 and the lower mold 2 to close and separate the molds. The hydraulic mechanism 5 can provide pressure to the upper mold 1 during closing the molds, so as to achieve the leveling of the surface of the VC temperature equalizing plate by the upper mold 1.

[0044] Example 2, the VC temperature plate shaping mold provided in Example 1 is further optimized, specifically, as follows Figure 4 As shown, the hydraulic mechanism 5 includes a base 501, a plurality of columns 502 are fixedly installed on the top of the base 501, a fixed platform 503 is fixedly connected between the plurality of columns 502, a first hydraulic cylinder 504 is fixedly installed on the top of the fixed platform 503, the telescopic end of the first hydraulic cylinder 504 passes through the fixed platform 503 and is fixedly connected with a lifting plate 505, the upper mold 1 is installed at the bottom of the lifting plate 505, the lifting plate 505 is connected with the outer surface of the column 502, the first hydraulic cylinder 504 can drive the lifting plate 505 to move up and down through the lifting plate 505, and the upper mold 1 can be driven to move up and down through the lifting plate 505, so as to realize mold closing and mold separation;

[0045] Limit rods 506 are fixedly connected to both sides of the top of the lifting plate 505. The top of the limit rods 506 passes through the fixed platform 503 and extends above the fixed platform 503. The limit rods 506 can limit the lifting process of the lifting plate 505 to improve the stability of the lifting process of the lifting plate 505.

[0046] Further, such as Figure 4 As shown, two slide rails 507 are fixedly installed on the top of the base 501, and the surfaces of the two slide rails 507 are slidably connected with a plurality of slide seats 508. The lower mold 2 is installed between the tops of the plurality of slide seats 508. The slide seats 508 and the slide rails 507 cooperate with each other to support the lower mold 2 and enable the lower mold 2 to move horizontally. After the lower mold 2 is removed from under the upper mold 1 and then the VC temperature equalizing plate is driven, the safety of the process of taking and placing the VC temperature equalizing plate can be improved, and the operating space can be increased, which is convenient for operation.

[0047] Further, such as Figure 4As shown, a second hydraulic cylinder 509 is fixedly installed on the top of the base 501 , and the telescopic end of the second hydraulic cylinder 509 is connected to the lower mold 2 , and the lower mold 2 can be driven to move horizontally through the second hydraulic cylinder 509 .

[0048] Example 3, the VC temperature plate shaping mold provided in Example 2 is further optimized, specifically, as follows Figure 5 As shown, an air hole 604 is provided through the bottom of the inner cavity of the lower profiling groove 201, a sleeve 6 is fixedly installed on the top of the base 501, an air cavity 601 is provided in the sleeve 6, a hollow piston 602 is slidably connected in the air cavity 601, a middle hole tube 603 is fixedly connected to one side of the hollow piston 602, and one end of the middle hole tube 603 away from the hollow piston 602 is fixedly connected to the bottom of the upper mold 1 and communicated with the air hole 604. After the VC temperature averaging plate is placed in the lower profiling groove 201, when the lower mold 2 moves to the bottom of the upper mold 1, the middle hole tube 603, the hollow piston 602 and the air cavity 601 can cooperate to generate negative pressure between the air hole 604 and the lower mold 2 to suck the VC temperature averaging plate, thereby fixing the VC temperature averaging plate, and further improving the stability of the VC temperature averaging plate processing process. When the lower mold 2 is moved away from the bottom of the upper mold 1, the air pressure between 604 and the lower mold 2 is restored, thereby releasing the fixation of the VC temperature averaging plate.

[0049] The use process of the VC temperature plate shaping mold provided by the utility model is as follows:

[0050] The second hydraulic cylinder 509 pushes the lower mold 2 to move toward the sleeve 6, so that the lower mold 2 moves away from directly below the upper mold 1, and the VC temperature-averaging plate is placed in the lower contoured groove 201. The second hydraulic cylinder 509 pushes the lower mold 2 to move away from the sleeve 6. At this time, the middle hole tube 603, the hollow piston 602 and the air cavity 601 cooperate to generate negative pressure between the air hole 604 and the lower mold 2 to suck the VC temperature-averaging plate tightly, thereby fixing the VC temperature-averaging plate. The first hydraulic cylinder 504 pushes the upper mold 1 down through the lifting plate 505 so that the upper mold 1, the raised ribs 102 and the lower mold 2 level the VC temperature-averaging plate.

[0051] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection, an electrical connection, or communication with each other; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0052] Obviously, the embodiments described above are only some embodiments of the utility model, rather than all embodiments. The preferred embodiments of the utility model are given in the accompanying drawings, but they do not limit the patent scope of the utility model. The utility model can be implemented in many different forms. On the contrary, the purpose of providing these embodiments is to make the understanding of the disclosure of the utility model more thorough and comprehensive. Although the utility model is described in detail with reference to the aforementioned embodiments, for those skilled in the art, it is still possible to modify the technical solutions recorded in the aforementioned specific implementation methods, or to replace some of the technical features therein with equivalents. Any equivalent structure made using the contents of the utility model specification and the accompanying drawings, directly or indirectly used in other related technical fields, is also within the scope of patent protection of the utility model.

Claims

1. VC temperature plate shaping mold, characterized by: The invention comprises an upper mould (1), wherein one side of the upper mould (1) is provided with an upper profiling groove (101) adapted to the shape of a VC temperature equalising plate, and a side of the upper mould (1) close to the upper profiling groove (101) is fixedly connected with a plurality of raised ribs (102), and the plurality of raised ribs (102) are arranged around the upper profiling groove (101).

2. The VC temperature plate shaping mold according to claim 1, characterized in that: The raised ribs (102) are used to cause a depression on the surface of the skirt edge of the VC temperature averaging plate, so that the surface shell of the VC temperature averaging plate is stretched toward the skirt edge, thereby achieving flattening of the surface of the VC temperature averaging plate.

3. The VC temperature plate shaping mold according to claim 2, characterized in that: It also comprises a lower mould (2) for use in conjunction with the upper mould (1); a lower contoured groove (201) matching the shape of the VC temperature equalising plate is provided on a side of the lower mould (2) close to the upper mould (1).

4. The VC temperature plate shaping mold according to claim 3, characterized in that: A plurality of positioning pins (4) are fixedly mounted on a side of the lower mold (2) close to the upper mold (1), and the plurality of positioning pins (4) are arranged around the lower profiling groove (201); a plurality of pin grooves (401) are opened on a side of the upper mold (1) close to the lower mold (2), and the plurality of pin grooves (401) are arranged around the upper profiling groove (101); and the positions of the plurality of pin grooves (401) respectively correspond to the positions of the plurality of positioning pins (4).

5. The VC temperature plate shaping mold according to claim 4, characterized in that: A plurality of positioning posts (3) are fixedly mounted on a surface of the lower mould (2) close to the upper mould (1), and a plurality of positioning grooves (301) for the positioning posts (3) to be inserted are provided on the upper mould (1).

6. The VC temperature plate shaping mold according to claim 5, characterized in that: A hydraulic mechanism (5) is provided between the upper mold (1) and the lower mold (2), and the hydraulic mechanism (5) is used to drive the upper mold (1) and the lower mold (2) to close and separate the molds.

7. The VC temperature plate shaping mold according to claim 6, characterized in that: The hydraulic mechanism (5) comprises a base (501), a plurality of columns (502) are fixedly mounted on the top of the base (501), a fixed platform (503) is fixedly connected between the plurality of columns (502), a first hydraulic cylinder (504) is fixedly mounted on the top of the fixed platform (503), a telescopic end of the first hydraulic cylinder (504) passes through the fixed platform (503) and is fixedly connected to a lifting plate (505), the upper mold (1) is mounted on the bottom of the lifting plate (505), and the lifting plate (505) is interlacedly connected to the outer surfaces of the columns (502); Both sides of the top of the lifting plate (505) are fixedly connected to limit rods (506), and the top ends of the limit rods (506) pass through the fixed platform (503) and extend above the fixed platform (503).

8. The VC temperature plate shaping mold according to claim 7, characterized in that: Two slide rails (507) are fixedly mounted on the top of the base (501), and the outer surfaces of the two slide rails (507) are slidably connected to a plurality of slide seats (508), and the lower mold (2) is mounted between the tops of the plurality of slide seats (508).

9. The VC temperature plate shaping mold according to claim 8, characterized in that: A second hydraulic cylinder (509) is fixedly mounted on the top of the base (501), and a telescopic end of the second hydraulic cylinder (509) is connected to the lower mold (2).

10. The VC temperature plate shaping mold according to claim 9, characterized in that: An air hole (604) is formed through the bottom of the inner cavity of the lower profiling groove (201); a sleeve (6) is fixedly mounted on the top of the base (501); an air cavity (601) is arranged in the sleeve (6); a hollow piston (602) is slidably connected in the air cavity (601); a middle-hole tube (603) is fixedly connected to one side of the hollow piston (602); an end of the middle-hole tube (603) away from the hollow piston (602) is fixedly connected to the bottom of the upper mold (1) and communicates with the air hole (604).