Hot stamping anti-oxidation anodized aluminum
By setting protective layer and connection mechanism on the outside of the hot stamped antioxidant electrochemical aluminum, the problem of lack of side protection is solved, and higher antioxidant performance and service life are achieved.
Patent Information
- Application Number
- CN202421598795.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-08
- Publication Date
- 2025-04-01
- Estimated Expiration
- 2034-07-08
AI Technical Summary
The existing hot stamping antioxidant electrochemical aluminum lacks side protection, which makes it easy for air to enter from the side, affecting service life.
The bonding area and air permeation path are increased by providing a protective layer, including a waterproof layer, a sealing layer and a wear-resistant layer, and annular grooves and annular sealing blocks are provided on the outside of the electrochemical aluminum film body.
Effectively isolate and protect the sides of the electrochemical aluminum, preventing air from entering, thereby improving antioxidant performance and service life.
Smart Images

Figure CN222698168U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of hot stamping, in particular to hot stamping anti-oxidation electrochemical aluminum. Background Art
[0002] Hot stamping paper is commonly known as electroplated aluminum in northern my country. It is composed of polyester film (PET) and multiple layers of chemical coatings coated on its surface. The polyester film is usually 12 microns thick, and some of the coatings are used to produce decorative effects, while some coatings are used to control the performance of hot stamping paper. Different coatings are suitable for different substrates. After searching, the Chinese patent publication number CN217705245U discloses a hot stamping anti-oxidation type electroplated aluminum hot stamping foil, including a hot stamping foil body, a strengthening mechanism and a paper tube, and the hot stamping foil body is wrapped on the surface of the paper tube. By connecting the anti-magnetic attraction coating and the sealing film on the side of the electroplated aluminum layer, the influence of magnetic force on the hot stamping foil is reduced, which is not conducive to its connection and use, and the sealing film is used for sealing and isolation, and the high temperature resistant layer and the anti-oxidation layer are connected on the side of the electroplated aluminum layer to reduce the deformation of the hot stamping foil during the hot stamping process and ensure the anti-oxidation effect of the hot stamping foil.
[0003] In the above technical solution, the high temperature resistant layer and the anti-oxidation layer are connected to the side of the electroplated aluminum layer, which reduces the deformation of the hot stamping foil during the hot stamping process and ensures the anti-oxidation effect of the hot stamping foil. However, there is no side protection, and air can easily enter the interior of the electroplated aluminum from the side, and the air penetration path cannot be increased to slow down the internal oxidation rate, thereby affecting the service life. Utility Model Content
[0004] In view of the deficiencies in the prior art, the utility model provides hot stamping anti-oxidation electrochemical aluminum, which solves the problems raised in the background technology.
[0005] To achieve the above purpose, the utility model is implemented by the following technical solutions: hot stamping anti-oxidation electrochemical aluminum, including an electrochemical aluminum film body, the electrochemical aluminum film body includes a base layer, the lower surface of the base layer is fixedly connected with a first anti-oxidation layer, the outer surface of the base layer is fixedly connected with a coloring layer, the outer surface of the coloring layer is fixedly connected with a second anti-oxidation layer, the outer surface of the second anti-oxidation layer is fixedly connected with a protective layer, and a connecting mechanism is provided inside the protective layer;
[0006] The protective layer comprises a waterproof layer fixedly connected to the outer surface of the second anti-oxidation layer, a sealing layer fixedly connected to the outer surface of the waterproof layer, and a wear-resistant layer fixedly connected to the outer surface of the sealing layer.
[0007] Preferably, the protective layer is coated on the outside of the base layer, and can cover and protect the inner base layer, thereby protecting the side of the base layer.
[0008] Preferably, the connecting mechanism includes an annular groove, the upper surface and lower surface of the waterproof layer, the upper surface and lower surface of the sealing layer, and the lower surface of the wear-resistant layer are all provided with annular grooves, an annular sealing block is embedded and fixedly connected inside the annular groove, and the lower surfaces of the waterproof layer, the sealing layer and the wear-resistant layer are all bonded with a first adhesive layer. The provision of the annular groove and the annular sealing block can increase the bonding area, which can not only increase the structural strength but also increase the air inlet path, thereby delaying the oxidation time and increasing the service life.
[0009] Preferably, the first adhesive layer and the adjacent annular sealing block are integrally formed, and the first adhesive layer enters the annular groove in a softened state and becomes an annular sealing block after solidification.
[0010] Preferably, the lower surface of the waterproof layer is flush with the lower surface of the first anti-oxidation layer, and the lower surface of the inner first anti-oxidation layer is bonded with a second adhesive layer, and the lower surface of the second adhesive layer is flush with the lower surface of the first adhesive layer at the bottom of the waterproof layer, so as to facilitate the pasting of the electrochemical aluminum film body.
[0011] Preferably, the lower surfaces of the second adhesive layer and the adjacent first adhesive layer are both bonded with release paper, so as to facilitate isolation of the second adhesive layer and the first adhesive layer when not in use.
[0012] The utility model provides hot stamping anti-oxidation electrochemical aluminum, which has the following beneficial effects:
[0013] 1. The hot stamping anti-oxidation electroplated aluminum has a protective layer which covers the entire base layer, the first anti-oxidation layer, the coloring layer and the second anti-oxidation layer when in use, thereby isolating and protecting the sides of the base layer, the first anti-oxidation layer, the coloring layer and the second anti-oxidation layer, preventing air from entering from the sides, thereby further improving the anti-oxidation performance, thereby solving the problem that the existing electroplated aluminum has no side protection and air can easily enter the inside of the electroplated aluminum from the sides, thus affecting its service life.
[0014] 2. The hot stamping anti-oxidation electroplated aluminum has a connecting mechanism set up so that the first adhesive layer will enter the corresponding annular groove during coating, and will form an annular sealing block after solidification, which can not only increase the adhesion area and improve the structural strength, but also increase the air penetration path, thereby delaying the internal oxidation rate and further improving the service life, thereby solving the problem that the existing electroplated aluminum cannot increase the air penetration path to delay the internal oxidation rate. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a schematic diagram of the overall structure of the utility model;
[0016] Figure 2 It is a schematic diagram of the internal structure of the utility model;
[0017] Figure 3 For the utility model Figure 2 Enlarged view of point A in the middle.
[0018] In the figure, 1. electrochemical aluminum film body; 11. base layer; 12. first anti-oxidation layer; 13. coloring layer; 14. second anti-oxidation layer; 15. protective layer; 151. waterproof layer; 152. sealing layer; 153. wear-resistant layer; 16. connecting mechanism; 161. annular groove; 162. annular sealing block; 163. first adhesive layer; 17. second adhesive layer; 18. release paper. DETAILED DESCRIPTION
[0019] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0020] Example 1: Figure 1 and Figure 2 As shown, the hot stamping anti-oxidation type electrochemical aluminum includes an electrochemical aluminum film body 1, and the electrochemical aluminum film body 1 includes a base layer 11, the lower surface of the base layer 11 is fixedly connected with a first anti-oxidation layer 12, the outer surface of the base layer 11 is fixedly connected with a coloring layer 13, and the outer surface of the coloring layer 13 is fixedly connected with a second anti-oxidation layer 14. The first anti-oxidation layer 12 and the second anti-oxidation layer 14 can be provided with anti-oxidation protection for the bottom and the top of the base layer 11 respectively, thereby improving the service life.
[0021] Example 2: Figure 2 and Figure 3 As shown, the outer surface of the second anti-oxidation layer 14 is fixedly connected with a protective layer 15, and the protective layer 15 includes a waterproof layer 151 fixedly connected to the outer surface of the second anti-oxidation layer 14, and the outer surface of the waterproof layer 151 is fixedly connected with a sealing layer 152, and the outer surface of the sealing layer 152 is fixedly connected with a wear-resistant layer 153. The protective layer 15 is coated on the outside of the base layer 11. When in use, the protective layer 15 is coated on the outside of the entire base layer 11, the first anti-oxidation layer 12, the coloring layer 13 and the second anti-oxidation layer 14, so that the sides of the base layer 11, the first anti-oxidation layer 12, the coloring layer 13 and the second anti-oxidation layer 14 can be isolated and protected to prevent air from entering from the side, thereby further improving the anti-oxidation performance, thereby solving the problem that the existing electroplated aluminum has no side protection, and air easily enters the inside of the electroplated aluminum from the side and affects the service life.
[0022] Example 3: Figure 2 and Figure 3 As shown, the protective layer 15 is provided with a connecting mechanism 16 inside, and the connecting mechanism 16 includes an annular groove 161. The upper surface and lower surface of the waterproof layer 151, the upper surface and lower surface of the sealing layer 152, and the lower surface of the wear-resistant layer 153 are all provided with an annular groove 161. An annular sealing block 162 is embedded and fixedly connected inside the annular groove 161. The lower surfaces of the waterproof layer 151, the sealing layer 152, and the wear-resistant layer 153 are all bonded with a first adhesive layer 163. The first adhesive layer 163 and the adjacent annular sealing blocks 162 are integrally formed. The lower surface of the waterproof layer 151 around is flush with the lower surface of the first anti-oxidation layer 12. The lower surface of the inner first anti-oxidation layer 12 is bonded with a second adhesive layer 17, and the lower surface of the second adhesive layer 17 is flush with the lower surface of the first adhesive layer 163 at the bottom of the waterproof layer 151. The second adhesive layer 17 and the lower surface of the adjacent first adhesive layer 163 are both bonded with release paper 18. Annular grooves 161 are provided on the upper and lower surfaces of the waterproof layer 151, the upper and lower surfaces of the sealing layer 152, and the lower surface of the wear-resistant layer 153. During production, the first adhesive layer 163 is coated between each layer. The first adhesive layer 163 will enter the corresponding annular groove 161 during coating, and an annular sealing block 162 will be formed after solidification, which can not only increase the adhesion area and improve the structural strength, but also increase the path of air penetration, thereby delaying the internal oxidation rate and further improving the service life, thereby solving the problem that the existing electroplated aluminum cannot increase the path of air penetration to delay the internal oxidation rate.
[0023] Working principle: During production, annular grooves 161 are opened on the upper and lower surfaces of the waterproof layer 151, the upper and lower surfaces of the sealing layer 152, and the lower surface of the wear-resistant layer 153. During production, a first viscose layer 163 is coated between each layer. The first viscose layer 163 will enter the corresponding annular groove 161 during coating, and an annular sealing block 162 will be formed after solidification, which can not only increase the adhesion area and improve the structural strength, but also increase the air penetration path, thereby delaying the internal oxidation rate and further improving the service life, thereby solving the problem that the existing electrochemical aluminum cannot increase the air penetration path to delay the internal oxidation rate.
[0024] When in use, the protective layer 15 covers the outside of the entire base layer 11, the first anti-oxidation layer 12, the coloring layer 13 and the second anti-oxidation layer 14, so that the sides of the base layer 11, the first anti-oxidation layer 12, the coloring layer 13 and the second anti-oxidation layer 14 can be isolated and protected to prevent air from entering from the sides, thereby further improving the anti-oxidation performance, thereby solving the problem that the existing electrochemical aluminum has no side protection and air can easily enter the interior of the electrochemical aluminum from the sides and affect the service life. The first anti-oxidation layer 12 and the second anti-oxidation layer 14 can be set to provide anti-oxidation protection for the bottom and top of the base layer 11 respectively, thereby improving the service life.
[0025] The above shows and describes the basic principles and main features of the utility model and the advantages of the utility model. For those skilled in the art, it is obvious that the utility model is not limited to the details of the above exemplary embodiments, and can be implemented in other specific forms without departing from the spirit or basic features of the utility model. Therefore, no matter from which point of view, the embodiments should be regarded as exemplary and non-restrictive. The scope of the utility model is defined by the attached claims rather than the above description, and it is intended to include all changes within the meaning and scope of the equivalent elements of the claims. Any figure mark in the claims should not be regarded as limiting the claims involved.
[0026] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.
Claims
1. Hot stamping anti-oxidation type electroplated aluminum, comprising an electroplated aluminum film body (1), characterized in that: The electrochemical aluminum film body (1) comprises a base layer (11), the lower surface of the base layer (11) is fixedly connected to a first anti-oxidation layer (12), the outer surface of the base layer (11) is fixedly connected to a coloring layer (13), the outer surface of the coloring layer (13) is fixedly connected to a second anti-oxidation layer (14), the outer surface of the second anti-oxidation layer (14) is fixedly connected to a protective layer (15), and a connecting mechanism (16) is provided inside the protective layer (15); The protective layer (15) comprises a waterproof layer (151) fixedly connected to the outer surface of the second anti-oxidation layer (14), the outer surface of the waterproof layer (151) is fixedly connected to a sealing layer (152), and the outer surface of the sealing layer (152) is fixedly connected to a wear-resistant layer (153).
2. The hot stamping anti-oxidation electrochemical aluminum according to claim 1, characterized in that: The protective layer (15) is coated on the outside of the base layer (11).
3. The hot stamping anti-oxidation electrochemical aluminum according to claim 1, characterized in that: The connecting mechanism (16) comprises an annular groove (161); the upper surface and the lower surface of the waterproof layer (151), the upper surface and the lower surface of the sealing layer (152), and the lower surface of the wear-resistant layer (153) are all provided with an annular groove (161); an annular sealing block (162) is embedded and fixedly connected inside the annular groove (161); and the lower surfaces of the waterproof layer (151), the sealing layer (152), and the wear-resistant layer (153) are all bonded with a first adhesive layer (163).
4. The hot stamping anti-oxidation electrochemical aluminum according to claim 3, characterized in that: The first adhesive layer (163) and the adjacent annular sealing block (162) are integrally formed.
5. The hot stamping anti-oxidation electrochemical aluminum according to claim 4, characterized in that: The lower surface of the waterproof layer (151) is flush with the lower surface of the first anti-oxidation layer (12); the lower surface of the inner first anti-oxidation layer (12) is bonded with a second adhesive layer (17); the lower surface of the second adhesive layer (17) is flush with the lower surface of the first adhesive layer (163) at the bottom of the waterproof layer (151).
6. The hot stamping anti-oxidation electrochemical aluminum according to claim 5, characterized in that: Release paper (18) is bonded to the lower surfaces of the second adhesive layer (17) and the adjacent first adhesive layer (163).
Citation Information
Patent Citations
Anti-oxidation alumite hot stamping foil for hot stamping images and texts
CN217705245U