A high-strength electrolytic zinc cathode plate

By riveting the connecting plate body and conductive beam, and thickened edge barriers and aluminum strips are provided at the connection, the problem of separation and fall off of traditional cathode plates due to corrosion is solved, and corrosion resistance and service life are improved.

CN222715469UActive Publication Date: 2025-04-04NANHUA MAOSEN REGENERATION TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420465609.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-11
Publication Date
2025-04-04
Estimated Expiration
2034-03-11

AI Technical Summary

Technical Problem

In long-term use, traditional electrolytic zinc cathode plates are prone to separation and fall off due to corrosion, affecting the electrolytic efficiency and zinc sheet quality.

Method used

The plate body and the conductive beam are connected by riveting, and thickened edges and aluminum strips are installed at the connection to completely cover the upper part of the cathode plate and an insulating anti-corrosion coating is applied.

Benefits of technology

It improves corrosion resistance of the upper part of the cathode plate, prevents harsh gas corrosion, extends the service life of the cathode plate, and ensures that the connection is firm and does not loosen easily.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222715469U_ABST
    Figure CN222715469U_ABST
Patent Text Reader

Abstract

The utility model discloses a high-strength electrolytic zinc cathode plate, which relates to the technical field of electrolytic equipment accessories. It includes a plate body, a conductive beam, an aluminum strip and an aluminum rivet. Polypropylene insulating strips are hot-pressed on both sides of the plate body. A thickened rib is provided on the rear side of the conductive beam, and a positioning column is provided on the inner surface of the thickened rib. A positioning hole is provided on the top of the plate body, and the plate body is installed at the thickened rib through the positioning hole and the positioning column. The aluminum strip is pressed on the top of the plate body. The high-strength electrolytic zinc cathode plate uses riveting to connect the plate body and the conductive beam into one body, and by providing a thickened rib and an aluminum strip at the connection between the two, the upper part of the cathode plate that is exposed to the electrolyte for a long time is completely covered, and an insulating anti-corrosion coating is applied, which can improve the corrosion resistance of the upper part of the cathode plate, so that it will not be damaged by corrosion from harsh gases, and the connection is firm and not easy to loosen and fall off, thereby extending the service life of the cathode plate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of electrolytic equipment accessories, in particular to a high-strength electrolytic zinc cathode plate. Background Art

[0002] Hydrometallurgy uses a lead-silver alloy plate containing about 1% silver as an anode and an industrial pure aluminum plate as a cathode. Zinc is extracted by electrodeposition in a zinc sulfate electrolyte. During the electrolysis process, zinc ions obtain electrons at the cathode and are reduced to zinc and precipitated. After the plate surface accumulates to a certain thickness, it is removed and peeled off to obtain zinc sheets. The aluminum cathode plate is an important component in the electrolytic zinc production facility. The corrosion resistance and service life of the aluminum cathode plate are not only related to the production cost of electrolytic zinc, but also affect the electrolysis efficiency and quality of electrolytic zinc.

[0003] The conductive beam of the traditional cathode plate is manufactured by a separate casting method, and then connected to the electrode plate by welding, or directly cast with the electrode plate without welding. During the production process, most of the cathode plate surface is immersed in the zinc sulfate solution in the electrolytic cell and is poorly corroded and basically intact. However, the portion of the cathode plate surface above the neck where the bridge is connected is exposed to the zinc sulfate solution in the electrolytic cell. It has been working in the acidic environment of the production workshop for a long time and is severely corroded. The conductive beam and the electrode plate are easily separated and fall off after being corroded. Utility Model Content

[0004] The utility model provides a high-strength electrolytic zinc cathode plate to solve the problems in the background technology.

[0005] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a high-strength electrolytic zinc cathode plate, comprising a plate body, a conductive beam, an aluminum strip and aluminum rivets, polypropylene insulating strips are hot-pressed on both sides of the plate body, a thickened rib is provided on the rear side of the conductive beam, and a positioning column is provided on the inner surface of the thickened rib, a positioning hole is provided on the top of the plate body, and the plate body is installed at the thickened rib through the positioning hole and the positioning column, the aluminum strip is pressed on the top of the plate body, and the top of the plate body is riveted to the thickened rib and the aluminum strip respectively through aluminum rivets, the surfaces of the thickened rib and the aluminum strip are coated with an insulating anti-corrosion coating, a conductive clip is provided on the conductive beam, and a conductive head is fixedly installed in the conductive clip.

[0006] Furthermore, the polypropylene insulation strip is in a U shape and is sandwiched between two side edges of the plate body.

[0007] Furthermore, the thickened retaining edge is provided with a first riveting hole, the top end of the plate body is provided with a second riveting hole, the aluminum pressure strip is provided with a third riveting hole, and the riveting holes among the three correspond to each other.

[0008] Furthermore, the aluminum rivet penetrates the first riveting hole, the second riveting hole and the third riveting hole, so that the thickened retaining edge, the plate body and the aluminum pressure strip are riveted to each other.

[0009] Furthermore, the conductive clip and the conductive head are both provided with threaded holes, and the threaded holes are threadedly connected with threaded heads, and the conductive head is locked and connected to the conductive clip via the threaded heads.

[0010] Furthermore, the conductive beam is provided with hooks, and the hooks are located at both ends of the conductive beam.

[0011] Compared with the prior art, the utility model provides a high-strength electrolytic zinc cathode plate having the following

[0012] Beneficial effects:

[0013] The high-strength electrolytic zinc cathode plate is connected to the plate body and the conductive beam by riveting, and a thickened rib and an aluminum strip are arranged at the connection between the two to completely cover the upper part of the cathode plate exposed to the electrolyte for a long time, and an insulating anti-corrosion coating is applied to improve the corrosion resistance of the upper part of the cathode plate so that it will not be damaged by corrosion from harsh gases. The connection is firm and not easy to loosen or fall off, thereby extending the service life of the cathode plate. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 It is a schematic diagram of the structure of the utility model;

[0015] Figure 2 It is a partial schematic diagram of the utility model;

[0016] Figure 3 It is a side view of the utility model.

[0017] In the figure: 1. plate body; 2. conductive beam; 3. aluminum pressure strip; 4. aluminum rivet; 5. polypropylene insulation strip; 6. thickened rib; 7. positioning column; 8. positioning hole; 9. insulating anti-corrosion coating; 10. conductive clip; 11. conductive head; 12. first riveting hole; 13. second riveting hole; 14. third riveting hole; 15. threaded hole; 16. threaded head; 17. hook. DETAILED DESCRIPTION

[0018] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0019] See also Figure 1-Figure 3The utility model discloses a high-strength electrolytic zinc cathode plate, comprising a plate body 1, a conductive beam 2, an aluminum strip 3 and an aluminum rivet 4. Polypropylene insulating strips 5 are hot-pressed on both sides of the plate body 1. A thickened rib 6 is provided on the rear side of the conductive beam 2, and a positioning column 7 is provided on the inner surface of the thickened rib 6. A positioning hole 8 is provided on the top of the plate body 1, and the plate body 1 is installed at the thickened rib 6 through the positioning hole 8 and the positioning column 7. The aluminum strip 3 is pressed on the top of the plate body 1. The top of the plate body 1 is riveted to the thickened rib 6 and the aluminum strip 3 respectively through the aluminum rivet 4. The thickened rib 6 and the aluminum strip The surface of 3 is coated with an insulating anti-corrosion coating 9. The plate body 1 and the conductive beam 2 are connected into one by riveting, and a thickened retaining edge 6 and an aluminum strip 3 are arranged at the connection between the two to completely cover the upper part of the cathode plate exposed to the electrolyte for a long time, and the insulating anti-corrosion coating 9 is applied to improve the corrosion resistance of the upper part of the cathode plate so that it will not be damaged by corrosion by harsh gases, and the connection is firm and not easy to loosen and fall off, thereby extending the service life of the cathode plate. A conductive clip 10 is provided on the conductive beam 2, and a conductive head 11 is fixedly installed in the conductive clip 10.

[0020] Specifically, the polypropylene insulating strip 5 is in a U shape and is sandwiched between two side edges of the plate body 1 .

[0021] In this embodiment, in order to prevent the cathode from short-circuiting and the deposited zinc from wrapping around the cathode, making zinc stripping difficult, polypropylene insulating strips 5 are installed on the edges of both sides of the electrode plate.

[0022] Specifically, the thickened retaining edge 6 is provided with a first riveting hole 12, the top end of the plate body 1 is provided with a second riveting hole 13, the aluminum pressure strip 3 is provided with a third riveting hole 14, and the riveting holes of the three correspond to each other.

[0023] In this embodiment, the first riveting hole 12 , the second riveting hole 13 and the third riveting hole 14 are provided to cooperate with the aluminum rivet 4 , so that the thickened retaining edge 6 , the plate body 1 and the aluminum pressure strip 3 are connected.

[0024] Specifically, the aluminum rivet 4 penetrates the first riveting hole 12 , the second riveting hole 13 and the third riveting hole 14 , so that the thickened retaining edge 6 , the plate body 1 and the aluminum pressure strip 3 are riveted to each other.

[0025] In this embodiment, the plate body 1 and the conductive beam 2 are connected to each other by riveting. Specifically, the conductive clip 10 and the conductive head 11 are both provided with a threaded hole 15, and a threaded head 16 is threadedly connected in the threaded hole 15, and the conductive head 11 is locked and connected to the conductive clip 10 through the threaded head 16.

[0026] In this embodiment, the conductive head 11 is fixed on the conductive clip 10 by the cooperation between the threaded head 16 and the threaded hole 15 .

[0027] Specifically, the conductive beam 2 is provided with hooks 17 , and the hooks 17 are located at both ends of the conductive beam 2 .

[0028] In this embodiment, the hook 17 is mainly used to hang the cathode plate so that it can be hung in the electrolytic cell.

[0029] When in use, the plate body 1 and the conductive beam 2 are connected into one by riveting, and a thickened rib 6 and an aluminum strip 3 are provided at the connection between the two to completely cover the upper part of the cathode plate exposed to the electrolyte for a long time, and an insulating anti-corrosion coating 9 is applied to improve the corrosion resistance of the upper part of the cathode plate so that it will not be damaged by corrosion from harsh gases, and the connection is firm and not easy to loosen or fall off, thereby extending the service life of the cathode plate.

[0030] In summary, the high-strength electrolytic zinc cathode plate is connected as a whole by riveting between the plate body 1 and the conductive beam 2, and a thickened rib 6 and an aluminum strip 3 are provided at the connection between the two, so that the upper part of the cathode plate exposed to the electrolyte for a long time is completely covered, and an insulating anti-corrosion coating 9 is applied, which can improve the corrosion resistance of the upper part of the cathode plate so that it will not be damaged by corrosion from harsh gases, and the connection is firm and not easy to loosen and fall off, thereby extending the service life of the cathode plate.

[0031] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A high-strength electrolytic zinc cathode plate, comprising a plate body (1), a conductive beam (2), an aluminum pressure strip (3) and an aluminum rivet (4), characterized in that: Polypropylene insulating strips (5) are hot-pressed on both sides of the plate body (1); a thickened retaining edge (6) is provided on the rear side of the conductive beam (2); a positioning column (7) is provided on the inner surface of the thickened retaining edge (6); a positioning hole (8) is provided on the top of the plate body (1); and the plate body (1) is installed at the thickened retaining edge (6) through the positioning hole (8) and the positioning column (7); the aluminum pressure strip (3) is pressed on the top of the plate body (1); the top of the plate body (1) is riveted to the thickened retaining edge (6) and the aluminum pressure strip (3) respectively through aluminum rivets (4); the surfaces of the thickened retaining edge (6) and the aluminum pressure strip (3) are both coated with an insulating anti-corrosion coating (9); a conductive clip (10) is provided on the conductive beam (2); and a conductive head (11) is fixedly installed in the conductive clip (10).

2. The high-strength electrolytic zinc cathode plate according to claim 1, characterized in that: The polypropylene insulating strip (5) is in a U shape and is sandwiched between the two side edges of the plate body (1).

3. The high-strength electrolytic zinc cathode plate according to claim 1, characterized in that: The thickened retaining edge (6) is provided with a first riveting hole (12), the top end of the plate body (1) is provided with a second riveting hole (13), the aluminum pressure strip (3) is provided with a third riveting hole (14), and the riveting holes of the three correspond to each other.

4. The high-strength electrolytic zinc cathode plate according to claim 3, characterized in that: The aluminum rivet (4) penetrates the first riveting hole (12), the second riveting hole (13) and the third riveting hole (14), so that the thickened retaining edge (6), the plate body (1) and the aluminum pressure strip (3) are riveted to each other.

5. The high-strength electrolytic zinc cathode plate according to claim 1, characterized in that: The conductive clip (10) and the conductive head (11) are both provided with a threaded hole (15), and a threaded head (16) is threadedly connected in the threaded hole (15), and the conductive head (11) is locked and connected to the conductive clip (10) via the threaded head (16).

6. The high-strength electrolytic zinc cathode plate according to claim 1, characterized in that: The conductive beam (2) is provided with a hook (17), and the hook (17) is located at both ends of the conductive beam (2).