Switch panel punching die
By using embedded punching and cutting tool molds made of plastic materials and steel, the problem of low production efficiency of traditional tool molds is solved, achieving a more efficient production process and cost-reducing effect.
Patent Information
- Application Number
- CN202421373358.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-17
- Publication Date
- 2025-04-11
- Estimated Expiration
- 2034-06-17
AI Technical Summary
The traditional switch panel punching and cutting tool die is made of pure steel, which takes a long time to form a tool die at multiple punching and cutting points, resulting in low production efficiency.
The punching and cutting tool mold is made of plastic material and steel. By opening an annular groove and a clamping groove on the main board, the first blade, the second blade and the punching module are embedded to realize the embedded tool mold design.
It effectively improves the production efficiency of the tool mold, reduces the use of milling materials, reduces the production cost, and improves the overall production efficiency of the panel.
Smart Images

Figure CN222741630U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of switch panel processing tools, and in particular to a switch panel punching die. Background Art
[0002] Membrane switch is an operating system that integrates key functions, indicating elements, and instrument panels. It consists of four parts: panel, upper circuit, isolation layer, and lower circuit. When the membrane switch is pressed, the contact of the upper circuit deforms downward and contacts the plate of the lower circuit. When the finger is released, the contact of the upper circuit rebounds, the circuit is disconnected, and the loop triggers a signal. The membrane switch has a rigorous structure, beautiful appearance, and good sealing. It is moisture-proof and has a long service life. It is widely used in electronic communications, electronic measurement instruments, industrial control, medical equipment, automotive industry, smart toys, household appliances and other fields.
[0003] During the processing and production of the panel, since it has different components and the panel itself has a certain shape, it is necessary to punch the panel to make it punched into a specified shape; the traditional switch panel punching die is made of pure steel material, and the steel raw material is processed by a milling cutter to finally form a specified shape; in actual applications, the switch panel often has multiple points that need to be punched, such as the punching of the outer frame shape, some circular through-hole punching, and even some special shapes that need to be punched. It often takes a long time to form a matching die from steel raw materials, which is very unfavorable to production efficiency. Utility Model Content
[0004] The purpose of this application is to provide a switch panel punching die to solve at least one of the above-mentioned technical problems.
[0005] In order to solve the above technical problems, the present application provides a switch panel punching die, including a main board, on which a first annular groove, a plurality of second annular grooves and a clamping groove are formed, and the second annular groove and the clamping groove are located within the annular range of the first annular groove;
[0006] a first blade strip, wherein the first blade strip is embedded in the first annular groove;
[0007] a second blade strip, wherein the second blade strip is embedded in the second annular groove;
[0008] A punching module, the punching module comprising a main body and a blade, the punching module being embedded in the clamping slot;
[0009] Wherein, the main board is made of plastic material, and the first blade, the second blade and the punching module are made of steel;
[0010] In the above implementation process, the punching die provided by the present scheme is composed of a composite of plastic material and steel, wherein the first blade is used to form the outer contour of the panel, the second blade can be used to form some conventionally shaped through holes, and the punching module is used to form some special shaped through holes; it is understandable that, compared with the traditional punching die, if it is necessary to form a die with multiple punching points, it takes a lot of time to mill off a large amount of steel to form the corresponding knife positions, and in the present scheme, the main board is used as the main body of the board, and the corresponding first annular groove and other groove structures are further opened thereon, and the corresponding blade and punching module are embedded in an embedded manner, which can be directly embedded and then used through a certain position adjustment, or it can be embedded in the steel block and then the point is concentratedly milled without large-scale milling; it can be seen that the present scheme effectively improves the production efficiency of the die and thus improves the overall production efficiency of the panel. In addition, this method can also effectively reduce production costs.
[0011] Preferably, the first annular groove and / or the second annular groove comprises a first groove body portion and a second groove body portion that are interconnected;
[0012] The first groove portion is close to the punched front side of the main board, and the second groove portion is close to the punched back side of the main board;
[0013] The first groove body parts are connected without interruption, and the second groove body parts are formed at intervals along the circumferential direction of the first groove body parts;
[0014] In the above implementation process, the first knife strip in this scheme serves as a part for forming the outer shape of the panel, and sometimes its range is large. If a full-through embedding method is adopted, unstable assembly is likely to occur. For this reason, further improvements are made in this scheme, wherein the first groove body part is a completely connected uninterrupted groove body, thereby ensuring the continuity of the entire punching blade surface of the first knife strip, and the second groove body is arranged in an interval manner, which can avoid the first annular groove being fully through, thereby ensuring the embedding stability of the first knife strip, ensuring stability during subsequent punching, and ensuring production quality; the same is true for the second annular groove.
[0015] Preferably, a protruding tooth structure is formed on a side of the first blade and / or the second blade facing away from the cutting surface thereof;
[0016] In the above implementation process, the protruding tooth structure can be understood as being adapted to the second grooves arranged at intervals, thereby achieving sufficient embedding and improving the stability of assembly.
[0017] Preferably, the cross section of the main body of the punching module is rectangular;
[0018] In the above implementation process, the cross-section of the punching module is rectangular, that is, during production, the block of steel can be directly assembled in the corresponding slot of the mainboard, and then the corresponding shape is milled out by a milling cutter to form the blade part.
[0019] Preferably, a protrusion is formed on the outer peripheral wall of the main body of the punching die;
[0020] Preferably, the cross section of the protrusion is trapezoidal;
[0021] Preferably, the cross section of the protrusion is rectangular;
[0022] In the above implementation process, the protrusions formed on the outer peripheral wall of the punching die main body can provide more limiting points between the punching die and the main board, thereby improving the stability of embedded assembly.
[0023] Preferably, the mainboard is made of PVC material;
[0024] In the above implementation process, the mainboard is made of PVC material, which can ensure that the mainboard has sufficient hardness and corresponding wear resistance, thereby effectively extending the service life without the need for frequent mold replacement; further, it also has a certain waterproof performance, which can effectively delay the time when rust appears on the cutting mold.
[0025] Preferably, first mounting holes are provided at positions near the four corners of the main board along the thickness direction thereof;
[0026] Preferably, a first mounting groove is provided on a wall surface surrounding an edge of the mainboard;
[0027] In the above implementation process, the present solution sets a first mounting hole and a first mounting groove, and the user can select corresponding mounting points and mounting methods according to the actual assembly situation to improve its compatibility.
[0028] Compared with the prior art, the beneficial effect of the present application lies in that: the present solution uses the main board as the main body of the board, and further opens the corresponding first annular groove and other groove structures thereon, and embeds the corresponding knife strips and punching modules in an embedded manner. It can be used by directly embedding and adjusting a certain position, or it can be embedded in a steel block and then the point is concentratedly milled without the need for large-scale milling. It can be seen that the present solution effectively improves the production efficiency of the knife mold and thus improves the overall production efficiency of the panel. In addition, this method can also effectively reduce production costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0030] Figure 1 It is a front structural schematic diagram of one embodiment of the present application;
[0031] Figure 2 It is a schematic diagram of the back structure of one embodiment of the present application;
[0032] Figure 3 It is a front structural schematic diagram of one embodiment of the present application;
[0033] Figure 4 It is a structural schematic diagram of a punching module in one embodiment of the present application;
[0034] Figure 5 It is a partial structural schematic diagram of one embodiment of the present application;
[0035] Figure 6 It is a partial structural schematic diagram of one embodiment of the present application;
[0036] Among them: 10, main board; 11, first mounting hole; 12, first mounting slot; 21, first blade; 22, second blade; 30, punching module; 31, main body; 32, blade; 33, protrusion; 40, first annular slot; 41, first slot body; 42, second slot body. DETAILED DESCRIPTION
[0037] The embodiments of the present application are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present application, and cannot be understood as limiting the present application.
[0038] In the description of the present application, it should be understood that the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present application, "plurality" means two or more, unless otherwise clearly and specifically defined.
[0039] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installation" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or mutual communication; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0040] In the description of the present application, it should be understood that the terms "upper", "lower", "side", "front", "rear", etc. indicate orientations or positional relationships based on the installation, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0041] In the description of this application, it should be noted that the term "and / or" is merely a description of the association relationship between associated objects, indicating that three relationships may exist. For example, A and / or B can mean: A exists alone, A and B exist at the same time, and B exists alone.
[0042] It should also be noted that, in the embodiments of the present application, the same figure mark is used to represent the same component or the same part. For the same parts in the embodiments of the present application, the figure may only mark one of the parts or components as an example. It should be understood that the figure mark also applies to other identical parts or components.
[0043] In order to further understand the content, features and effects of the utility model of the present application, the following embodiments are given as examples and described in detail with reference to the accompanying drawings:
[0044] Example
[0045] During the processing and production of the panel, since it has different components and the panel itself has a certain shape, it is necessary to punch the panel to make it punched into a specified shape; the traditional switch panel punching die is made of pure steel material, and the steel raw material is processed by a milling cutter to finally form a specified shape; in actual applications, the switch panel often has multiple points that need to be punched, such as punching of the outer frame shape, punching of some circular through holes, and even some special shapes that need to be punched. It often takes a long time to form a matching die from the steel raw material, which is very unfavorable to production efficiency; in order to solve the above technical problems, this embodiment provides the following technical solutions:
[0046] For details, see Figure 1-6, this embodiment provides a switch panel punching die, including a main board 10, a first blade 21, a second blade 22, that is, a punching module 30;
[0047] Specifically, a first annular groove 40, a plurality of second annular grooves and a clamping groove are formed on the main board 10, and the second annular groove and the clamping groove are located within the annular range of the first annular groove 40;
[0048] Specifically, the first blade 21 is embedded in the first annular groove 40;
[0049] Specifically, the second blade 22 is embedded in the second annular groove;
[0050] Specifically, the punching module 30 includes a main body 31 and a blade 32, and the punching module 30 is embedded in the clamping groove;
[0051] The main board 10 is made of plastic material, and the first blade 21, the second blade 22 and the punching module 30 are made of steel;
[0052] In the above scheme, the punching die provided by the present scheme is composed of a composite of plastic material and steel, wherein the first blade 21 is used to form the outer contour of the panel, and the second blade 22 can be used to form some conventionally shaped through holes, and the punching module 30 is used to form some specially shaped through holes; it is understandable that, compared with the traditional punching die, if it is necessary to form a die with multiple punching points, it takes a lot of time to mill off a large amount of steel to form the corresponding knife positions, and in the present scheme, the main board 10 is used as the main body of the board, and the corresponding first annular groove 40 and other groove structures are further opened thereon, and the corresponding blade and punching module 30 are embedded in an embedded manner, which can be directly embedded and then used through a certain position adjustment, or it can be embedded in the steel block and then the point is concentratedly milled without large-scale milling; it can be seen that the present scheme effectively improves the production efficiency of the die and thus improves the overall production efficiency of the panel. In addition, this method can also effectively reduce production costs.
[0053] For details, see 2 and Figure 5 , the first annular groove 40 and / or the second annular groove includes a first groove body 41 and a second groove body 42 that communicate with each other;
[0054] Furthermore, the first slot body 41 is close to the punched front side of the main board 10, and the second slot body 42 is close to the punched back side of the main board 10;
[0055] Specifically, the first slot body 41 is connected without interruption, and the second slot body 42 is formed at intervals along the circumferential direction of the first slot body 41;
[0056] In the above scheme, the first blade strip 21 in this scheme is used as a component for forming the outer shape of the panel, and sometimes its range is relatively large. If a full-through embedding method is adopted, unstable assembly is likely to occur. For this reason, further improvements are made in this scheme, wherein the first groove body 41 is a completely connected groove body without interruption, thereby ensuring the continuity of the entire punching blade surface of the first blade strip 21, and the second groove body 42 is arranged in an interval manner, which can avoid the first annular groove 40 being fully through, thereby ensuring the embedding stability of the first blade strip 21, ensuring stability during subsequent punching, and ensuring production quality; the same is true for the second annular groove.
[0057] Specifically, a protruding tooth structure is formed on a side of the first blade 21 and / or the second blade 22 facing away from the cutting surface thereof;
[0058] In the above solution, the protruding tooth structure can be understood as being adapted to the second grooves arranged at intervals, thereby achieving sufficient embedding and improving the stability of assembly.
[0059] Specifically, the cross section of the main body 31 of the punching module 30 is rectangular;
[0060] In the above solution, the cross section of the punching module 30 is rectangular, that is, during production, the block of steel material can be directly assembled into the corresponding slot of the main board 10, and then the corresponding shape is milled out by a milling cutter to form the blade portion 32.
[0061] For details, see Figure 3-4 A protrusion 33 is formed on the outer peripheral wall of the main body 31 of the punching die;
[0062] In one embodiment, the cross section of the protrusion 33 is trapezoidal;
[0063] In one embodiment, the cross section of the protrusion 33 is rectangular;
[0064] In the above solution, the protrusions 33 formed on the outer peripheral wall of the punching die body 31 can provide more limiting points between the punching die and the main board 10, thereby improving the stability of the embedded assembly.
[0065] Specifically, the main board 10 is made of PVC material;
[0066] In the above scheme, the main board 10 is made of PVC material, which can ensure that the main board 10 has sufficient hardness and corresponding wear resistance, thereby effectively extending the service life without the need for frequent mold replacement; further, it also has a certain waterproof performance, which can effectively delay the time when rust appears on the cutting mold.
[0067] For details, see Figure 6 First mounting holes 11 are provided near the four corners of the main board 10 along the thickness direction thereof;
[0068] In another embodiment, a first mounting groove 12 is provided on a wall surface of the main board 10 surrounding its edge;
[0069] In the above solution, the first mounting hole 11 and the first mounting groove 12 are provided in this solution, and the user can select the corresponding mounting point and mounting method according to the actual assembly situation to improve its compatibility.
[0070] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application may be combined with each other.
[0071] The above description is only a preferred embodiment of the present application and does not constitute any form of limitation to the present application. Any simple modification, equivalent changes and modifications made to the above embodiments based on the technical essence of the present application are within the scope of the technical solution of the present application.
Claims
1. A switch panel punching die, characterized in that: include A main board, on which a first annular groove, a plurality of second annular grooves and a clamping groove are formed, wherein the second annular groove and the clamping groove are located within the annular range of the first annular groove; a first blade strip, wherein the first blade strip is embedded in the first annular groove; a second blade strip, wherein the second blade strip is embedded in the second annular groove; A punching module, the punching module comprising a main body and a blade, the punching module being embedded in the clamping slot; The main board is made of plastic material, and the first blade, the second blade and the punching module are made of steel.
2. The switch panel punching die according to claim 1, characterized in that: The first annular groove includes a first groove body portion and a second groove body portion that are interconnected; The first groove portion is close to the punched front side of the main board, and the second groove portion is close to the punched back side of the main board; The first groove body parts are connected without interruption, and the second groove body parts are formed at intervals along the circumferential direction of the first groove body parts.
3. The switch panel punching die according to claim 2, characterized in that: A protruding tooth structure is formed on a side of the first blade strip and / or the second blade strip facing away from the cutting surface thereof.
4. The switch panel punching die according to claim 1, characterized in that: The cross section of the main body of the punching module is rectangular.
5. The switch panel punching die according to claim 1, characterized in that: A protrusion is formed on the outer peripheral wall of the main body of the punching die.
6. The switch panel punching die according to claim 5, characterized in that: The cross section of the protrusion is trapezoidal.
7. The switch panel punching die according to claim 5, characterized in that: The cross section of the protrusion is rectangular.
8. The switch panel punching die according to any one of claims 1 to 7, characterized in that: The main board is made of PVC material.
9. The switch panel punching die according to claim 8, characterized in that: First mounting holes are provided at positions near the four corners of the main board along the thickness direction thereof.
10. The switch panel punching die according to claim 8, characterized in that: A first mounting groove is provided on a wall surface surrounding the edge of the main board.