Impeller sealing element mold
Through mold design, the impeller seal is divided into the left mold and the right mold. The die core partition is used to separate the mold core into half a seal cavity, which solves the problem of many overall casting defects and achieves the production of seals with lower cost and higher efficiency.
Patent Information
- Application Number
- CN202420682561.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-03
- Publication Date
- 2025-04-25
- Estimated Expiration
- 2034-04-03
AI Technical Summary
The overall casting defects of existing impeller seals have many, resulting in high mass production costs, and scrapping one defect will lead to the problem of scrapping the other.
Using mold design, the mold is divided into the left mold and the right mold, and separated from the mold core into two half-seal cavity through the mold core partition, so as to simultaneously process two half-seal seals to reduce overall casting defects.
It reduces the cost of seal production, reduces overall casting defects, and improves production efficiency and material utilization.
Smart Images

Figure CN222790567U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of mold processing, and in particular relates to an impeller sealing component mold. Background Art
[0002] In various mechanical, chemical, metallurgical and pharmaceutical equipment, in order to prevent the leakage of liquids and gases, it is necessary to provide effective seals between the equipment interfaces, and the impeller shaft is usually sealed by mechanical seals or packing seals, and the sealing and buffering are achieved by filling auxiliary seals in the aluminum seal. The existing impeller seals are usually made by pouring aluminum liquid to achieve the complete production of a seal, but in the production process, the whole is generally cast, and after rough processing, it is cut into two halves by wire cutting, and then the mating surface is finely processed. There are too many overall casting defects, and the cost of the subsequent process is high. If one half is scrapped due to casting defects, the other will also be scrapped. This results in high parts cost, which is not conducive to mass production. Utility Model Content
[0003] Based on the problems mentioned in the above background technology, the utility model provides an impeller seal mold.
[0004] The technical solution adopted by the utility model is as follows: an impeller seal mold, comprising a base, a mold is installed on the base, the mold comprises a left mold and a right mold, a mold core is arranged between the left mold and the right mold, the mold core side wall is provided with two oppositely arranged shaping grooves, a mold core partition is arranged in the shaping groove, two side walls of the mold core partition are respectively connected to the left mold and the right mold side walls, the mold core partition and the mold core respectively form half a seal cavity with the left mold or the right mold.
[0005] Furthermore, a heightening plate is provided on the base, and a limiting groove matching the position of the mold core and the mold core partition is opened on the heightening plate.
[0006] Furthermore, a connecting plate is provided on the side of the left mold and the right mold away from the mold core partition.
[0007] Furthermore, a push rod plate is provided below the base, a plurality of push rods are connected to the push rod plate, a plurality of push holes are provided in the sealing cavity, a plurality of separation holes are provided on the mold core, and the push rods pass through the push holes and are inserted into the separation holes.
[0008] Furthermore, a pressure plate is arranged below the push rod plate, a countersunk hole is arranged on the pressure plate, a connecting hole corresponding to the countersunk hole is arranged on the push rod plate, and the push rod plate and the pressure plate are connected by bolts.
[0009] Furthermore, pouring gates are provided on the left mold and the right mold, and liquid inlets connected to the pouring gates are provided on the inner side walls of the left mold and the right mold, and the inner walls of the pouring gates are inclined toward the liquid inlets.
[0010] Furthermore, a heat dissipation cavity is provided in the middle of the mold core.
[0011] Beneficial effects of the utility model:
[0012] By dividing the mold into a left mold and a right mold and separating them with a core partition and a core, two half seal cavities are obtained, so that two halves of the impeller seal can be processed simultaneously. Since half of the seal is combined into one seal, the overall casting defects are fewer and no further cutting is required. Even if one half is defective and scrapped, the other half can be easily retained, and the production cost is lower. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] The present invention can be further described by the non-limiting embodiments given in the accompanying drawings;
[0014] Figure 1 It is a schematic diagram of the utility model;
[0015] Figure 2 This is an explosion diagram of the utility model;
[0016] The attached drawings are marked as follows:
[0017] Base 1, left mold 11, right mold 12, heightening plate 13, limiting groove 14, pouring port 15, liquid inlet 16, mold core 2, shaping groove 21, mold core partition 22, heat dissipation cavity 23, separation hole 24, half sealing cavity 3, top hole 31, connecting plate 4, ejector plate 5, ejector 51, connecting hole 52, pressing plate 53, countersunk hole 54. DETAILED DESCRIPTION
[0018] like Figure 1-2 As shown, an impeller seal mold comprises a base 1, on which a mold is installed, and the mold comprises a left mold 11 and a right mold 12, a core 2 is arranged between the left mold 11 and the right mold 12, and two oppositely arranged shaping grooves 21 are opened on the side wall of the core 2, and a core partition 22 is arranged in the shaping groove 21, and two side walls of the core partition 2 are respectively connected to the side walls of the left mold 11 and the right mold 12, and the core partition 22 and the core 2 respectively form a half seal cavity 3 with the left mold 11 or the right mold 12.
[0019] By adopting the above technical scheme, the mold is divided into a left mold 11 and a right mold 12, which are separated from the mold core 2 by a core partition 22 to obtain two half seal cavities 3, so that two halves of the impeller seal can be processed simultaneously. Since half a seal is synthesized into one seal, the overall casting defects are fewer and the production cost is lower.
[0020] As a preferred solution, a heightening plate 13 is provided on the base 1, and a limiting groove 14 matching the position of the mold core 2 and the mold core partition 22 is provided on the heightening plate 13. The setting of the limiting groove 14 facilitates the determination of the installation position of the mold core 2 and the partition, and facilitates subsequent replacement and maintenance.
[0021] As a preferred solution, a connecting plate 4 is provided on the side of the left mold 11 and the right mold 12 away from the mold core partition 22. A push rod plate 5 is provided below the base 1, and a plurality of push rods 51 are connected to the push rod plate 5. A plurality of push holes 31 are provided in the sealing cavity, and a plurality of separation holes 24 are provided on the mold core 2. The push rods 51 pass through the push holes 31 and are arranged in the separation holes 24. A pressing plate 53 is provided below the push rod plate 5, and a countersunk hole 54 is provided on the pressing plate 53. A connecting hole 52 corresponding to the countersunk hole 54 is provided on the push rod plate 5, and the push rod plate 5 is connected to the pressing plate 53 by bolts.
[0022] The entire mold is hoisted by the connection plate 4 and connected to an extrusion device, such as a cylinder, through the pressing plate 53, and the mold core 2 and the mold that have been cooled are ejected by the ejector rod 51.
[0023] As a preferred solution, a pouring port 15 is provided on both the left mold 11 and the right mold 12, and a liquid inlet 16 connected to the pouring port 15 is provided on the inner side walls of the left mold 11 and the right mold 12, and the inner wall of the pouring port 15 is inclined toward the liquid inlet 16. Through the arrangement of the liquid inlet 16 and the pouring port 15, aluminum liquid pouring is achieved, and the liquid inlet 16 is narrow, which is convenient for uniform liquid inlet.
[0024] As a preferred solution, a heat dissipation cavity 23 is provided in the middle of the mold core 2. The mold core 2 is provided with the heat dissipation cavity 23 to reduce the wall thickness and facilitate heat dissipation.
[0025] The utility model is described in detail above. The description of the specific embodiments is only used to help understand the method and core idea of the utility model. It should be pointed out that for ordinary technicians in this technical field, without departing from the principle of the utility model, the utility model can also be improved and modified, and these improvements and modifications also fall within the scope of protection of the claims of the utility model.
Claims
1. An impeller seal mold, characterized in that: include A base (1) is provided on which a mold is mounted. The mold comprises a left mold (11) and a right mold (12). A mold core (2) is arranged between the left mold (11) and the right mold (12). The side wall of the mold core (2) is provided with two oppositely arranged shaping grooves (21). A mold core partition (22) is arranged in the shaping groove (21). The two side walls of the mold core partition (22) are respectively connected to the side walls of the left mold (11) and the right mold (12). The mold core partition (22) and the mold core (2) respectively form a half sealing cavity (3) with the left mold (11) or the right mold (12).
2. The impeller seal mold according to claim 1, characterized in that: A heightening plate (13) is provided on the base (1), and a limiting groove (14) matching the position of the mold core (2) and the mold core partition plate (22) is provided on the heightening plate (13).
3. The impeller seal mold according to claim 1, characterized in that: A connecting plate (4) is provided on the side of the left mold (11) and the right mold (12) away from the mold core partition plate (22).
4. The impeller seal mold according to claim 3, characterized in that: A push rod plate (5) is provided below the base (1), a plurality of push rods (51) are connected to the push rod plate (5), a plurality of push holes (31) are provided in the sealing component cavity, a plurality of separation holes (24) are provided on the mold core (2), and the push rods (51) pass through the push holes (31) and are arranged in the separation holes (24).
5. The impeller seal mold according to claim 4, characterized in that: A pressing plate (53) is arranged below the push rod plate (5), a countersunk hole (54) is arranged on the pressing plate (53), a connecting hole (52) corresponding to the countersunk hole (54) is arranged on the push rod plate (5), and the push rod plate (5) and the pressing plate (53) are connected by bolts.
6. The impeller seal mold according to claim 1, characterized in that: The left mold (11) and the right mold (12) are both provided with a pouring port (15), and the inner side walls of the left mold (11) and the right mold (12) are both provided with a liquid inlet (16) connected with the pouring port (15) and the half sealing cavity (3), and the inner wall of the pouring port (15) is inclined toward the liquid inlet (16).
7. The impeller seal mold according to claim 1, characterized in that: A heat dissipation cavity (23) is provided in the middle of the mold core (2).