Magnesium alloy profile heat treatment straightening device

By designing the traction wheel, pre-pressure wheel, straightening wheel, meter wheel and cutting wheel in the heat treatment and straightening device of the magnesium alloy profile, and using the elastic force of the spring and compression spring, the problem of distance deviation between the meter wheel and the cutting wheel in the device is solved, ensuring the accurate position when the profile is cut, and the strength of the alloy is improved.

CN222842865UActive Publication Date: 2025-05-09JIANGSU ZHONGFU ALUMINUM MAGNESIUM TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202421629825.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-07-10
Publication Date
2025-05-09
Estimated Expiration
2034-07-10

AI Technical Summary

Technical Problem

When the magnesium alloy profile heat treatment straightening device is used, there is a distance offset between the meter wheel and the cutting wheel, resulting in inaccurate position of the profile when cut, resulting in the final length exceeding or not meeting the expected requirements.

Method used

A heat treatment and straightening device for magnesium alloy profiles is designed. By setting up a traction wheel, pre-pressure wheel, calibration wheel, meter wheel and cutting wheel on the main body, and using the elastic force of the stainless steel spring and compression spring, the rollers are made to fit the outer wall of the profile, and the rotation shaft and the clamping shaft are displaced through the compression spring to ensure the accurate position of the profile when cut.

Benefits of technology

It effectively prevents the displacement problem of the profile when it is cut, ensures that the final length of the profile meets the expected requirements, and optimizes the structural structure of the alloy by cooling down in cold water, improving the strength of the alloy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222842865U_ABST
    Figure CN222842865U_ABST
Patent Text Reader

Abstract

The utility model discloses a magnesium alloy profile heat treatment straightening device which comprises a main machine body, a traction wheel used for guiding is arranged at the position, located on the left side, of the upper end of the main machine body, a pre-pressing wheel is arranged at the position, located on the left side, of the front end of the main machine body, and a straightening wheel is arranged in the middle of the front end of the main machine body. A water tank is fixed to the rear end of the water storage tank, a sponge is placed in the water storage tank, a meter counting wheel measures a profile and then penetrates through a fixed cylinder to enter a cutting wheel, the profile enters the inner position of the fixed cylinder to extrude a sleeve and a rotating shaft, a sleeving cylinder and the rotating shaft generate displacement, and the cutting wheel is driven to cut off the profile. And meanwhile, a stainless steel spring and a compression spring release elastic force, so that a roller is attached to the outer wall position of the sectional material, the movement of the sectional material enables the roller to rotate at the outer wall position of a rotating shaft, in this way, the sectional material is conveyed to the inner position of a cutting-off wheel to be cut off, and displacement is prevented.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field related to heat treatment straightening devices for magnesium alloy profiles, and in particular relates to a heat treatment straightening device for magnesium alloy profiles. Background Art

[0002] The heat treatment straightening device for magnesium alloy profiles is a device used to straighten magnesium alloy profiles. During the production process of magnesium alloy profiles, since the shape or size deviation may occur during the manufacturing or processing process, the heat treatment straightening device can adjust the shape and size of the magnesium alloy profile by heating and mechanical correction to meet the design requirements. This device usually includes components such as a heating system, a pressure system, and a control system, which can effectively improve the quality and performance of magnesium alloy profiles.

[0003] When the heat treatment straightening device for magnesium alloy profiles is in use, there is a certain distance between the meter wheel and the cutting wheel, and it is easy to offset when entering the cutting wheel. The offset causes the position of the profile to be inaccurate when cutting, resulting in the final length of the profile exceeding or falling short of the expected requirements. Therefore, the market needs a new device to solve the current problems. Utility Model Content

[0004] The purpose of the utility model is to provide a magnesium alloy profile heat treatment straightening device to solve the problem that when the magnesium alloy profile heat treatment straightening device proposed in the above background technology is in use, the meter wheel and the cutting wheel are at a certain distance, and it is easy to offset when entering the cutting wheel. Due to the offset, the position of the profile is inaccurate when cutting, resulting in the final length of the profile exceeding or falling short of the expected requirements. Therefore, the market needs a new device to solve the current problems.

[0005] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a heat treatment straightening device for magnesium alloy profiles, comprising a main body, the upper end of the main body is provided with a traction wheel for guiding at a left position, the front end of the main body is provided with a pre-pressing wheel at a left position, a straightening wheel is provided at the middle position of the front end of the main body, a meter wheel is provided at the right position of the front end of the main body, a cutting wheel for cutting is installed at the right end of the main body, a fixing cylinder is fixed at the left position of the front end of the cutting wheel, a fixing column is fixed on the inner wall of the fixing cylinder at the upper and lower positions, and the other end of the fixing column is provided with a fixing cylinder at the upper and lower positions. A stainless steel spring is fixed at the position, a sleeve tube is fixed at the other end of the stainless steel spring, a clamping shaft is fixed at the left and right end positions of the sleeve tube, a rotating shaft is installed at the left and right end positions of the sleeve tube, a groove is provided at the inner position of the rotating shaft, a compression spring is provided at the inner position of the groove, a roller is sleeved at the outer wall position of the rotating shaft, a fixing rod is installed at the other end position of the rotating shaft, and the other end position of the fixing rod is fixed to the fixing tube, a water storage tank is fixed at the front end of the cutting wheel at the right position, a water tank is fixed at the rear end position of the water storage tank, and a sponge is placed at the inner position of the water storage tank.

[0006] Preferably, the traction wheel conveys the heat-treated magnesium alloy profile to the pre-pressing wheel.

[0007] Preferably, the pre-pressing wheel applies pressure to deform and soften the magnesium alloy profile.

[0008] Preferably, the straightening wheel applies force to straighten the magnesium alloy profile.

[0009] Preferably, the meter wheel measures the length of the corrected magnesium alloy profile, and the cutting wheel cuts the corrected profile.

[0010] Preferably, the profile measured by the meter wheel passes through a fixed cylinder and enters the cutting wheel, and the interior of the fixed cylinder squeezes the sleeve cylinder and the rotating shaft when the profile enters.

[0011] Preferably, the roller contacts the profile at the outer wall position of the rotating shaft and rotates, and the rotating shaft and another rotating shaft are displaced by a compression spring, a clamping shaft and a groove.

[0012] Preferably, the clamping shaft is fixed to a compression spring, and the rotating shaft is squeezed so that the clamping shaft moves at an inner position of the groove.

[0013] Preferably, cold water is added to the inner position of the water tank and flows into the inner position of the water storage tank.

[0014] Compared with the prior art, the utility model provides a magnesium alloy profile heat treatment straightening device, which has the following beneficial effects:

[0015] 1. After measuring the profile, the meter wheel passes through the fixed cylinder and enters the cutting wheel. The profile enters the internal position of the fixed cylinder, which squeezes the sleeve and the rotating shaft, causing the sleeve and the rotating shaft to displace. At the same time, the stainless steel spring and the compression spring release the elastic force, so that the roller fits the outer wall of the profile. The movement of the profile causes the roller to rotate at the outer wall of the rotating shaft, so that the profile is transported to the internal position of the cutting wheel for cutting, thereby preventing displacement.

[0016] 2. Move the cut profile with the sponge, add cold water through the water tank, let the cold water enter the inner position of the water tank, immerse the inner position of the sponge in the cold water, and cool the profile when fitting with the profile. This can optimize the organizational structure of the alloy to a certain extent and improve the strength of the alloy. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 The utility model is a schematic diagram of the structure of a magnesium alloy profile heat treatment straightening device.

[0018] Figure 2 The utility model is a schematic diagram of the structure of a fixed cylinder of a magnesium alloy profile heat treatment straightening device.

[0019] Figure 3 The utility model is a schematic diagram of the internal structure of a fixed cylinder of a magnesium alloy profile heat treatment straightening device.

[0020] Figure 4 It is a partially enlarged structural schematic diagram of a magnesium alloy profile heat treatment straightening device of the utility model.

[0021] Figure 5 The utility model is a schematic diagram of the cross-sectional structure of a water storage tank of a magnesium alloy profile heat treatment straightening device.

[0022] In the figure: 1. main body; 2. traction wheel; 3. pre-pressure wheel; 4. straightening wheel; 5. meter wheel; 6. fixing cylinder; 7. cutting wheel; 8. water tank; 9. sponge; 10. water storage tank; 11. fixing column; 12. sleeve cylinder; 13. roller; 14. fixing rod; 15. rotating shaft; 16. stainless steel spring; 17. compression spring; 18. clamping shaft; 19. groove. DETAILED DESCRIPTION

[0023] The technical solutions in the embodiments of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, rather than all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the utility model.

[0024] The utility model provides Figure 1-5 The heat treatment straightening device for magnesium alloy profiles shown in the figure comprises a main body 1, wherein the upper end of the main body 1 is provided with a traction wheel 2 for guiding at a left position, the front end of the main body 1 is provided with a pre-pressing wheel 3 at a left position, a straightening wheel 4 is provided at the middle position of the front end of the main body 1, a meter wheel 5 is provided at the right position of the front end of the main body 1, a cutting wheel 7 for cutting is installed at the right end position of the main body 1, a fixing cylinder 6 is fixed at the front end of the cutting wheel 7 at the left position, a fixing column 11 is fixed to the inner wall of the fixing cylinder 6 at the upper and lower positions, a stainless steel spring 16 is fixed at the other end position of the fixing column 11, and the stainless steel spring 1 6 is fixed with a sleeve tube 12, and a clamping shaft 18 is fixed at the left and right ends of the sleeve tube 12. A rotating shaft 15 is installed at the left and right ends of the sleeve tube 12, and a groove 19 is provided at the inner position of the rotating shaft 15. A compression spring 17 is provided at the inner position of the groove 19. A roller 13 is sleeved on the outer wall of the rotating shaft 15, and a fixing rod 14 is installed at the other end of the rotating shaft 15. The other end of the fixing rod 14 is fixed to the fixing tube 6. A water storage tank 10 is fixed to the front end of the cutting wheel 7 at the right position, a water tank 8 is fixed at the rear end of the water storage tank 10, and a sponge 9 is placed inside the water storage tank 10.

[0025] After the magnesium alloy profile is heated, it enters the straightening device. First, it passes through the traction wheel 2, which allows the profile to move smoothly in the straightening device. Then, the profile passes through the pre-pressing wheel 3, which applies a certain force to the profile to deform and soften it, in preparation for the subsequent straightening treatment. Then, the profile passes through the straightening wheel 4, which applies force to correct the profile, adjust its shape and size, and eliminate the deviation generated during the processing. It continues to pass through the meter wheel 5, which is used to measure the length of the profile to ensure that the straightened profile meets the required size requirements. Finally, the profile passes through the cutting wheel 7, which cuts the profile to the required length, completing the final shaping after the straightening treatment.

[0026] like Figure 1 and Figure 5As shown, the traction wheel 2 conveys the heat-treated magnesium alloy profile to the pre-pressing wheel 3, the pre-pressing wheel 3 applies pressure to deform and soften the magnesium alloy profile, the straightening wheel 4 applies force to correct the magnesium alloy profile, the meter wheel 5 measures the length of the corrected magnesium alloy profile, the cutting wheel 7 cuts the corrected profile, the profile measured by the meter wheel 5 passes through the fixed cylinder 6 and enters the cutting wheel 7, the inside of the fixed cylinder 6 squeezes the sleeve cylinder 12 and the rotating shaft 15 when the profile enters, the roller 13 contacts the profile and rotates at the outer wall position of the rotating shaft 15, the rotating shaft 15 and another rotating shaft 15 are displaced by the compression spring 17, the clamping shaft 18 and the groove 19, the clamping shaft 18 is fixed with the compression spring 17, the rotating shaft 15 is squeezed so that the clamping shaft 18 moves at the internal position of the groove 19, and cold water is added to the internal position of the water tank 8 to flow into the internal position of the water storage tank 10.

[0027] The cut profile is moved with the sponge 9, and cold water is added through the water tank 8 so that the cold water enters the inner position of the water storage tank 10. The inner position of the sponge 9 is immersed in the cold water, and the profile is cooled when it is fitted with the profile. This can optimize the organizational structure of the alloy to a certain extent and improve the strength of the alloy.

[0028] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A magnesium alloy profile heat treatment straightening device, characterized in that: The invention comprises a main body (1), wherein a traction wheel (2) for guiding is arranged at the upper end of the main body (1) at the left position, a pre-pressing wheel (3) is arranged at the front end of the main body (1) at the left position, a straightening wheel (4) is arranged at the middle position of the front end of the main body (1), a meter wheel (5) is arranged at the front end of the main body (1) at the right position, a cutting wheel (7) for cutting is installed at the right end of the main body (1), a fixing cylinder (6) is fixed at the front end of the cutting wheel (7) at the left position, a fixing column (11) is fixed to the inner wall of the fixing cylinder (6) at the upper and lower positions, a stainless steel spring (16) is fixed at the other end of the fixing column (11), and a sleeve is fixed at the other end of the stainless steel spring (16). The sleeve tube (12) is provided with a clamping shaft (18) fixed at the left and right ends of the sleeve tube (12), a rotating shaft (15) is installed at the left and right ends of the sleeve tube (12), a groove (19) is provided at the inner position of the rotating shaft (15), a compression spring (17) is provided at the inner position of the groove (19), a roller (13) is sleeved at the outer wall position of the rotating shaft (15), a fixing rod (14) is installed at the other end position of the rotating shaft (15), and the other end position of the fixing rod (14) is fixed to the fixing tube (6), a water storage tank (10) is fixed at the front end of the cutting wheel (7) at the right position, a water tank (8) is fixed at the rear end position of the water storage tank (10), and a sponge (9) is placed at the inner position of the water storage tank (10).

2. A magnesium alloy profile heat treatment straightening device according to claim 1, characterized in that: The traction wheel (2) transports the heat-treated magnesium alloy profile to the pre-pressing wheel (3).

3. A magnesium alloy profile heat treatment straightening device according to claim 2, characterized in that: The pre-pressing wheel (3) applies pressure to cause the magnesium alloy profile to deform and soften.

4. A magnesium alloy profile heat treatment straightening device according to claim 3, characterized in that: The straightening wheel (4) applies force to straighten the magnesium alloy profile.

5. The magnesium alloy profile heat treatment straightening device according to claim 1, characterized in that: The meter wheel (5) measures the length of the corrected magnesium alloy profile, and the cutting wheel (7) cuts the corrected profile.

6. The magnesium alloy profile heat treatment straightening device according to claim 5, characterized in that: The profile measured by the meter wheel (5) passes through the fixed cylinder (6) and enters the cutting wheel (7). The interior of the fixed cylinder (6) squeezes the sleeve cylinder (12) and the rotating shaft (15) when the profile enters.

7. The magnesium alloy profile heat treatment straightening device according to claim 6, characterized in that: The roller (13) contacts the profile and rotates at the outer wall position of the rotating shaft (15), and the rotating shaft (15) and another rotating shaft (15) are displaced through a compression spring (17), a clamping shaft (18) and a groove (19).

8. The magnesium alloy profile heat treatment straightening device according to claim 7, characterized in that: The clamping shaft (18) is fixed to the compression spring (17), and the rotating shaft (15) is squeezed so that the clamping shaft (18) moves at an inner position of the groove (19).