Laminated paper box capable of preventing glue failure in low-temperature environment

Through the design of modified PET film and easy-to-tear wire, the problem of coating paper boxes being opened in low-temperature environments is solved, and the stability and convenience of coating paper boxes being achieved under low-temperature conditions are achieved.

CN223132628UActive Publication Date: 2025-07-22SHANGHAI YOUNG SUN PRINTING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202421699731.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-07-18
Publication Date
2025-07-22
Estimated Expiration
2034-07-18

AI Technical Summary

Technical Problem

Existing coated paper boxes are prone to abnormal glue opening problems during low-temperature processing, low-temperature transport and low-temperature use.

Method used

The modified PET film and easy-to-tear wire design was adopted, and the component content of the modified PET film was adjusted to 10-25% aqueous acrylic resin and 50-75% acrylic ester copolymer. The knife plate parameters of the modified PET film were adjusted to 23.5mm in height, 0.71mm in thickness and 18mm in thickness. They were fixed on the top plate through a press, combined with the use of easy-to-tear wire to prevent glue opening.

Benefits of technology

It improves the viscosity and stability of the coated paper box in low temperature environments, prevents glue from being opened at the living room, increases the practicality and convenience of the device, and facilitates opening and removal of internal items.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN223132628U_ABST
    Figure CN223132628U_ABST
Patent Text Reader

Abstract

The utility model discloses a film-coated paper box capable of preventing glue failure in a low-temperature environment. The film-coated paper box comprises a first main board which is of a square paper board structure, and one side of the surface of the first main board is fixedly connected with a first side board; a second side plate is fixedly connected to one side of the surface of the first main plate, first top plates are symmetrically arranged on the surface of the first main plate, an easy-to-tear line is arranged on the surface of the first top plate on one side, baffles are fixedly connected to the surfaces of the first side plate and the second side plate, and a second main plate is connected to the other end of the second side plate. A second top plate is fixedly connected to the surface of the second main plate in a stacked mode. According to the film-coated paper box capable of preventing glue failure in the low-temperature environment, the modified PET film is arranged, the viscosity between the film-coated paper boxes can be improved, the content of components in the modified PET film can be changed, the pasting stability between the second top plate and the first top plate can be improved, glue failure at a pasted opening can be prevented, meanwhile, the shape of a transverse cutter plate of the modified PET film is changed, and the performance of the modified PET film can be improved; the practicability of the device is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of coated paper boxes, in particular to a coated paper box for preventing glue opening in a low-temperature environment. Background Art

[0002] A paper box is a three-dimensional shape, which is composed of a polyhedron formed by the movement, stacking, folding, and surrounding of several component faces. The faces in the three-dimensional composition play a role in dividing space in the space. By cutting, rotating, and folding the faces in different parts, different emotional expressions can be obtained for the faces. A coating film is provided on the surface of the paper box. In the market, existing frozen products have high requirements for the moisture-proof and anti-fouling properties of paper outer packages. Coating is the best method to enhance the moisture-proof and anti-fouling properties of paper outer packages. The commonly used paperboard coating material is polyethylene terephthalate PET. However, when the existing coated paper boxes are used in low-temperature processing, low-temperature transportation, and low-temperature use, there are abnormal problems of inability to break the material. Content of the Utility Model

[0003] The purpose of the utility model is to provide a coated paper box for preventing glue opening in a low-temperature environment, so as to solve the problem that when the existing coated paper boxes are used in low-temperature processing, low-temperature transportation, and low-temperature use, there are abnormal problems of inability to break the material as mentioned in the above background art.

[0004] To achieve the above purpose, the utility model provides the following technical solution: A coated paper box for preventing glue opening in a low-temperature environment, including a main board one which is set as a square cardboard structure, and one side of the surface of the main board one is fixedly connected with a side board one;

[0005] One side of the surface of the main board one is fixedly connected with a side board two, and the surface of the main board one is symmetrically provided with a top board one, and an easy tear line is arranged on the surface of one of the top board ones. The surfaces of the side board one and the side board two are both fixedly connected with baffles, and the other end of the side board two is connected with a main board two. The surface of the main board two is symmetrically and fixedly connected with a top board two, and a modified PET film is fixedly connected to the surface of each of the top board two. One side of the main board two is connected with a combined board.

[0006] Preferably, the main board one and the main board two are symmetrically arranged on both sides of the side board two, and the positions of the side board two and the main board one are correspondingly arranged.

[0007] Adopting the above technical solution, the main board one and the main board two can be bent to form the whole paper box.

[0008] Preferably, the side board one and the side board two are correspondingly arranged, and the inner wall of the combined board is attached to the outer surface of the side board one.

[0009] Adopting the above technical solution, at the same time, the side board one, the side board two, the main board one, and the main board two are connected to form a whole.

[0010] Preferably, a pair of the top plates are symmetrically arranged on both sides of the main board one, and the end of the side board one is attached to the surface of the main board two.

[0011] With the above technical solution, the main board one is arranged at both ends of the top board one. At this time, the side board one is connected to the main board two, and the main board one and the main board two can be fixed.

[0012] Preferably, the inner wall baffle of the top board two is attached to the surface, and the baffle is arranged on both sides inside the top board two.

[0013] With the above technical solution, the top board two is attached to the baffle. At this time, both ends of the main board one and the main board two can be closed.

[0014] Preferably, the positions of the two modified PET films are symmetrically arranged on both sides of the main board two.

[0015] With the above technical solution, at the same time, the modified PET film can connect the top board two and the combined board.

[0016] Preferably, the modified PET films are symmetrically arranged on both sides of the main board two. The inner wall of the top board one corresponds to the surface of the top board two, and the end of the modified PET film corresponds to the position of the top board one.

[0017] With the above technical solution, the modified PET film can improve the adhesiveness and prevent the glue from coming off at the glued part.

[0018] Compared with the prior art, the beneficial effects of the present utility model are as follows: The film-coated paper box for preventing glue from coming off in a low-temperature environment:

[0019] 1. A modified PET film is provided, which can improve the adhesiveness between the film-coated paper boxes. By changing the component content inside the modified PET film, the adhesion stability between the top board two and the top board one can be improved, preventing the glue from coming off at the glued part. At the same time, by changing the shape of the cross-cutting die plate of the modified PET film, the performance of the modified PET film can be improved, enhancing the practicability of the device;

[0020] 2. An easy-to-tear line is provided. The top board one can be torn open through the easy-to-tear line. At this time, the top board one is torn and disconnected. One end of the top board one is attached to the modified PET film, which can prevent the broken top board one from falling off. At this time, the top board two can be opened, facilitating the removal of the items inside the paper box and increasing the convenience of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 is a three-dimensional structural schematic diagram of the present utility model;

[0022] Figure 2 is a schematic diagram of the flat structure of the main board one of the present utility model;

[0023] Figure 3Schematic three-dimensional structure diagram for the installation of the second side plate of the present utility model;

[0024] Figure 4 Schematic three-dimensional structure diagram for the installation of the combined plate of the present utility model;

[0025] Figure 5 Schematic three-dimensional structure diagram for the installation of the tear line of the present utility model.

[0026] In the figure: 1, the first main board; 2, the first side plate; 3, the second side plate; 4, the first top plate; 5, the baffle; 6, the second main board; 7, the second top plate; 8, the modified PET film; 9, the combined plate; 10, the tear line. Specific embodiments

[0027] Next, the technical solutions in the embodiments of the present utility model will be clearly and completely described in conjunction with the accompanying drawings in the embodiments of the present utility model. Obviously, the described embodiments are only a part of the embodiments of the present utility model, rather than all the embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those of ordinary skill in the art without creative efforts shall fall within the protection scope of the present utility model.

[0028] Please refer to Figures 1-5 , the present utility model provides a technical solution: a film-coated paper box for preventing glue opening in a low-temperature environment, including the first main board 1, the first side plate 2, the second side plate 3, the first top plate 4, the baffle 5, the second main board 6, the second top plate 7, the modified PET film 8, the combined plate 9 and the tear line 10;

[0029] For this film-coated paper box, the properties of the modified PET film 8 are improved to prevent the paper shell from opening. The specific implementation method is as follows:

[0030] The main board 1 is set as a square cardboard structure, and one side of the surface of the main board 1 is fixedly connected with a first side plate 2; one side of the surface of the main board 1 is fixedly connected with a second side plate 3, and a first top plate 4 is symmetrically arranged on the surface of the main board 1, and a tear line 10 is arranged on the surface of one of the first top plates 4. The surfaces of the first side plate 2 and the second side plate 3 are both fixedly connected with baffles 5, and the other end of the second side plate 3 is connected with a second main board 6. The surface of the second main board 6 is symmetrically and fixedly connected with a second top plate 7, and modified PET films 8 are fixedly connected to the surfaces of the second top plates 7. One side of the second main board 6 is connected with a combined board 9. The main board 1 and the second main board 6 are symmetrically arranged on both sides of the second side plate 3, and the positions of the second side plate 3 and the main board 1 are correspondingly arranged. The positions of the first side plate 2 and the second side plate 3 are correspondingly arranged, and the inner wall of the combined board 9 is attached to the outer surface of the first side plate 2. The first top plates 4 are symmetrically arranged on both sides of the main board 1. The end of the first side plate 2 is attached to the surface of the second main board 6. The inner wall of the second top plate 7 is attached to the surface of the baffle 5, and the baffle 5 is arranged on both sides inside the second top plate 7. The positions of the two modified PET films 8 are symmetrically arranged on both sides of the second main board 6. The modified PET films 8 are symmetrically arranged on both sides of the second main board 6. The inner wall of the first top plate 4 is correspondingly arranged with the surface of the second top plate 7, and the end of the modified PET film 8 is correspondingly arranged with the position of the first top plate 4.

[0031] Lay the cardboard flat and cut the whole paper box so that the cardboard forms the finished product of the required paper box after cutting, such as Figure 2 , at this time, work on the cut cardboard by a scoring machine to produce indentations between adjacent cardboards, which is convenient for bending them. At the same time, process one of the first top plates 4 through laser technology to form a tear line 10 on the surface of the first top plate 4. At the same time, it is necessary to adjust the modified PET film 8 so that the content of the water-based acrylic resin in the modified PET film 8 reaches 10 - 25%, and the content of the acrylate copolymer reaches 50 - 75%, and the content of other primer components remains unchanged, so as to form a new modified PET film 8. When the modified PET film 8 is formed, it needs to be die-cut, and the die-cutting plate parameters of the modified PET film 8 are modified to a knife height of 23.5 mm, a knife thickness of 0.71 mm, and a die-cutting plate thickness of 18 mm. Then, fix the produced modified PET film 8 on the surface of the second top plate 7 through a laminating machine;

[0032] Bend the creases of the adjacent cardboard sheets. At this time, position the first side plate 2 and the second side plate 3 correspondingly, make the outer surface of the first side plate 2 fit the surface of the composite board 9. At this time, the first side plate 2 and the second side plate 3 are respectively perpendicular to the first side plate 2 and the second side plate 3. Then bend the baffle 5 inward so that the ends of the baffle 5 are correspondingly arranged. Bend the second top plate 7 so that the bottom of the second top plate 7 fits the bent baffle 5. At this time, bend the first top plate 4 so that the bottom of the first top plate 4 fits the surface of the second top plate 7. At this time, one end of the first top plate 4 fits the surface of the modified PET film 8. At this time, the modified PET film 8 and the tear line 10 are arranged in an alternating position. After the paper box is installed, by pulling the tear line 10, the two ends of the tear line 10 lose contact with the first top plate 4. At this time, the tear line 10 is torn off from the surface of the first top plate 4. At this time, one side of the first top plate 4 is fixedly connected to the modified PET film 8, and the other side of the first top plate 4 is connected to the main board 1. At this time, the remaining first top plate 4 and the second top plate 7 can be opened to take out the things inside the paper box.

[0033] Working principle: When using this film-coated paper box for preventing glue opening in a low-temperature environment, the modified PET film 8, the composite board 9 and the tear line 10 are provided to improve the properties of the modified PET film 8, prevent the paper shell from opening glue, and increase the overall practicability.

[0034] Although the embodiments of the present invention have been shown and described, for those of ordinary skill in the art, it can be understood that various changes, modifications, substitutions and variations can be made to these embodiments without departing from the principle and spirit of the present invention. The scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A film-coated paper box for preventing glue separation in a low-temperature environment, including a main board one (1) which is set as a square cardboard structure, and a side board one (2) is fixedly connected to one side of the surface of the main board one (1); It is characterized in that: A side board two (3) is fixedly connected to one side of the surface of the main board one (1), and a top board one (4) is symmetrically arranged on the surface of the main board one (1), and a tear line (10) is arranged on the surface of one of the top boards one (4). Baffles (5) are fixedly connected to the surfaces of the side board one (2) and the side board two (3), and the other end of the side board two (3) is connected to a main board two (6). A top board two (7) is symmetrically and fixedly connected to the surface of the main board two (6), and a modified PET film (8) is fixedly connected to the surface of the top board two (7). A combined board (9) is connected to one side of the main board two (6).

2. The film-coated paper box for preventing glue opening in a low-temperature environment according to claim 1, wherein: The main board one (1) and the main board two (6) are symmetrically arranged on both sides of the side board two (3), and the positions of the side board two (3) and the main board one (1) are correspondingly arranged.

3. A film-coated paper box for preventing glue opening in a low-temperature environment according to claim 1, characterized in that: The side board one (2) and the side board two (3) are correspondingly arranged, and the inner wall of the combined board (9) is attached to the outer surface of the side board one (2).

4. The film-coated paper box for preventing glue opening in a low-temperature environment according to claim 1, wherein: The top board one (4) is symmetrically arranged on both sides of the main board one (1), and the end of the side board one (2) is attached to the surface of the main board two (6).

5. The film-coated paper box for preventing glue opening in a low-temperature environment according to claim 1, wherein: The inner wall of the top board two (7) is attached to the surface of the baffle (5), and the baffle (5) is arranged on both sides inside the top board two (7).

6. The laminated paper box for preventing glue opening in a low-temperature environment according to claim 1, characterized in that: The positions of the two modified PET films (8) are symmetrically arranged on both sides of the main board two (6).

7. A film-coated paper box for preventing glue opening in a low-temperature environment according to claim 1, wherein: The modified PET films (8) are symmetrically arranged on both sides of the main board two (6). The inner wall of the top board one (4) and the surface of the top board two (7) are correspondingly arranged, and the end of the modified PET film (8) is correspondingly arranged with the position of the top board one (4).